A production process for automotive wiring harness
By detecting parameters such as conductivity and tensile strength, the production process parameters of automobile wire harnesses are adjusted to solve the problem of production parameter fluctuations in the existing technology, improve product stability and yield, and achieve efficient production of copper-clad aluminum wire harnesses. .
Patent Information
- Application Number
- CN202411061097.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-05
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2044-08-05
AI Technical Summary
The existing automotive wiring harness production process lacks necessary testing, resulting in fluctuations in production parameters and affecting product stability and yield.
By detecting parameters such as conductivity and tensile strength, by adjusting the cross-sectional area ratio of pure copper pipes and pure aluminum core materials and the stress relief annealing time, combined with the adjustment of welding evaluation values and crimping parameters, self-learning optimization of process parameters is realized .
It improves the electrical conductivity and mechanical properties of the wire harness, ensures product stability and yield, and achieves double protection.
Smart Images

Figure CN118588375B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of automobile wiring harness preparation, and in particular to a production process of automobile wiring harness. Background Art
[0002] With the development of new energy vehicles, the existing automotive wiring harnesses are also upgraded. Before the new energy electric vehicles, the common oil vehicle wiring harnesses were mostly low-voltage automotive wiring harnesses, which were needed to adapt to the connection of the electronic components required by the car itself. However, with the development of new energy vehicles, the car is driven by batteries. Compared with oil vehicles, the power and energy consumption of the battery pack are powered by conventional oil vehicle wiring harnesses. The low-voltage automotive wiring harness specifications can no longer meet the requirements. Fixed high-voltage automotive wiring harnesses that are resistant to high temperature, high pressure, can carry large currents, and have better shielding are needed to connect the new energy battery pack to the drive components and for charging.
[0003] Chinese patent publication number: CN116453765A, discloses an automatic production line and processing technology for new energy vehicle wiring harnesses, including the following steps: Step 1: Process two elastic bands; Step 2: Use a wire winder to send multiple wires to the elastic band on one side in a distributed state; Step 3: Control the lower mold II to flip relative to the lower mold I, and buckle the two elastic bands on both sides of the multiple wires; Step 4: The elastic bands on both sides are bonded to each other at both sides of the multiple wires. It can be seen that the above technical solution lacks targeted detection, which greatly reduces the stability and yield of product production when production parameters fluctuate. Summary of the invention
[0004] To this end, the present invention provides a production process for automotive wiring harnesses to overcome the problem in the prior art that the stability and yield of product production do not meet the standards when production parameters fluctuate due to the lack of necessary testing and optimization of production parameters based on the test results.
[0005] To achieve the above object, the present invention provides a production process for an automotive wiring harness, comprising:
[0006] Step S1, interference fitting the degreased and cleaned pure aluminum core material to the degreased and cleaned pure copper tube material to complete the preparation of the wiring harness conductor substrate;
[0007] Step S2, after completing the stretching of the wiring harness conductor substrate according to a preset single deformation rate, performing stress relief annealing, and repeating the stretching and stress relief annealing of the wiring harness conductor substrate until the diameter of the conductor reaches the designed size;
[0008] Step S3, coating the wire with an insulator by extrusion to complete the preparation of the wire harness core wire;
[0009] Step S4, detecting the conductivity coefficient of the wire harness core wire, and when it is preliminarily determined based on the measured conductivity coefficient that the preparation of the wire harness core wire does not meet the preset standard, increasing the cross-sectional area ratio of the pure copper tube to the pure aluminum core material for the preparation of the next batch of wire harness core wires, or increasing the annealing time of the stress relief annealing for the preparation of the next batch of wire harness core wires;
[0010] Step S5, twisting a number of the wire harness core wires that meet the preset standard, and then sequentially coating them with a shielding net and wrapping them with adhesive tape to complete the preparation of the wire harness baseline;
[0011] Step S6, cutting the wire harness base line according to a specified size and then peeling off the winding tape, the shielding net and the insulation layer of each of the wire harness core wires in turn;
[0012] Step S7, after extruding the end of the wire bundle base line after stripping, use brazing to complete welding of the end;
[0013] Step S8, assembling the terminal and the wiring terminal of the wiring harness base line, heating and pressing the terminal and the wiring terminal to complete the crimping;
[0014] Step S9, crimping the shielding ring and the packaging ring respectively to complete the preparation of the wiring harness;
[0015] Step S10, detecting the resistivity of the wiring harness, and determining whether the preparation of the wiring harness meets a preset standard based on the measured resistivity;
[0016] Step S11, packaging the wire harness that meets the preset standard.
[0017] Further, in step S4, when it is preliminarily determined that the preparation of the wire harness core wire meets the preset standard based on the conductivity coefficient, the tensile strength of the wire harness core wire is detected and a secondary determination is made based on the measured tensile strength whether the preparation of the wire harness core wire meets the preset standard.
[0018] Further, in the step S4, the process of preliminarily determining that the preparation of the wire harness core wire does not meet the preset standard according to the conductivity coefficient includes comparing the conductivity coefficient with a first preset conductivity coefficient threshold and a second preset conductivity coefficient threshold, respectively,
[0019] If the conductivity is less than the first preset conductivity threshold, increasing the cross-sectional area ratio of the pure copper tube to the pure aluminum core material for preparing the next batch of wire harness core wires;
[0020] If the conductivity is greater than or equal to the first preset conductivity threshold and less than the second preset conductivity threshold, the annealing time of the stress relief annealing for preparing the next batch of wire harness core wires is increased.
[0021] Furthermore, the increase in the cross-sectional area ratio of the pure copper tube to the pure aluminum core material is positively correlated with the conductivity difference, and the conductivity difference is the difference between the first preset conductivity threshold and the measured conductivity.
[0022] Furthermore, under the first preset condition, several correction methods are provided for the increase of the cross-sectional area ratio, and each correction method has a different correction amplitude for the increase of the cross-sectional area ratio. The first preset condition is that the tensile strength of the wire harness core wire after the cross-sectional area ratio of the pure copper tube and the pure aluminum core material is increased is less than a preset tensile strength threshold.
[0023] Further, when it is determined that the preparation of the wire harness core wires does not meet the preset standard based on the secondary determination of the tensile strength, the annealing temperature of the stress relief annealing for the next batch of wire harness core wires is lowered, or the single deformation rate for the next batch of wire harness core wires is reduced.
[0024] Further, in the step S10, when it is determined based on the resistivity that the preparation of the wire harness does not meet the preset standard, the wire harness that does not meet the preset standard is marked as a first defective product and a welding evaluation value is determined based on the historical first defective product data, and the wire feeding amount for the end welding of the next batch of wire harnesses is increased based on the welding evaluation value, or it is marked as a second defective product and whether the crimping meets the preset standard is determined based on the defective rate and the proportion of the second defective products within a preset period, and the historical first defective product data includes the number of wire harnesses marked as first defective products within the preset period and the resistivity of each wire harness marked as the first defective product.
[0025] Furthermore, the welding evaluation value is obtained by formula (1):
[0026] (1),
[0027] In formula (1), Z is the welding evaluation value, is the resistivity of the wire harness marked as first-class defective products within the preset period, i=1,2,3...m, m is the total number of wire harnesses marked as first-class defective products within the preset period, It is the preset welding evaluation threshold.
[0028] Furthermore, the increase in the wire feeding amount of the end welding is positively correlated with the welding evaluation value.
[0029] Furthermore, when it is determined that the crimping does not meet the preset standard based on the defective rate and the second defective product ratio, the crimping pressure for preparing the next batch of wire harnesses is increased, or the crimping temperature for preparing the next batch of wire harnesses is increased.
[0030] Compared with the prior art, the beneficial effect of the present invention lies in that the core wire of the wiring harness of the process of the present invention is in the form of copper-clad aluminum, which ensures both the conductive performance and the mechanical performance. At the same time, by setting the detection of the wiring harness core wire and the wiring harness, the production of the product is optimized by self-learning, thereby ensuring the stability and yield of the product production.
[0031] Furthermore, when the present invention preliminarily determines that the preparation of the wiring harness core wire meets the preset standard, the tensile strength of the conductor is detected and a secondary determination is made based on the measured tensile strength whether the preparation of the wiring harness core wire meets the preset standard, thereby doubly ensuring the electrical and mechanical properties of the core wire.
[0032] Furthermore, the present invention determines whether the preparation of the wire harness core wire meets the preset standard by comparing the conductivity coefficient with the threshold value, and determines the adjusted process parameters when it does not meet the preset standard, thereby ensuring the stability of the core wire process.
[0033] Furthermore, when the cross-sectional area ratio needs to be adjusted, the present invention constrains the increase in the cross-sectional area ratio by using the conductivity difference, thereby achieving a precise increase in the cross-sectional area ratio.
[0034] Furthermore, after calculating the cross-sectional area ratio, if the tensile strength of the core wire is less than a preset tensile strength threshold, the cross-sectional area ratio is corrected, thereby adjusting the cross-sectional area ratio more accurately.
[0035] Furthermore, when the preparation of the wiring harness is determined to be non-compliant with preset standards based on the resistivity, the present invention marks it as a first defective product, or marks it as a second defective product, and determines through historical data whether the preparation process meets the preset standards, thereby specifically adjusting the parameters of the production process to ensure product stability. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] Figure 1 This is a flow chart of a production process of an automotive wiring harness according to an embodiment of the present invention;
[0037] Figure 2 A flowchart for preliminarily determining whether the preparation of the wire harness core wire meets the preset standard according to an embodiment of the present invention;
[0038] Figure 3 A flow chart of correcting the cross-sectional area ratio according to an embodiment of the present invention;
[0039] Figure 4 The present invention is a flowchart for determining whether the preparation of a wiring harness meets a preset standard. DETAILED DESCRIPTION
[0040] In order to make the objects and advantages of the present invention more clearly understood, the present invention is further described below in conjunction with embodiments; it should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.
[0041] It should be pointed out that the data in this embodiment are obtained by comprehensive analysis and evaluation of the historical detection data of the process of the present invention in the three months before this production and the corresponding historical production results. It can be understood by those skilled in the art that the determination method for the above-mentioned single parameter of the process of the present invention can be to select the value with the highest proportion as the preset standard parameter according to the data distribution, use weighted summation to use the obtained value as the preset standard parameter, substitute each historical data into a specific formula and use the value obtained by the formula as the preset standard parameter or other selection methods, as long as the system of the present invention can clearly define the different specific situations in the single determination process through the obtained values.
[0042] The preferred embodiments of the present invention are described below with reference to the accompanying drawings. It should be understood by those skilled in the art that these embodiments are only used to explain the technical principles of the present invention and are not intended to limit the protection scope of the present invention.
[0043] See also Figure 1 , Figure 2 , Figure 3 as well as Figure 4 As shown, they are respectively a flow chart of a production process of a wiring harness for an automobile according to an embodiment of the present invention; a flow chart of a preliminary determination of whether the preparation of the wiring harness core wire meets the preset standard according to an embodiment of the present invention; a flow chart of correcting the cross-sectional area ratio according to an embodiment of the present invention; and a flow chart of determining whether the preparation of the wiring harness meets the preset standard according to an embodiment of the present invention.
[0044] The present invention provides a production process for an automotive wiring harness, comprising:
[0045] Step S1, interference fit the degreased and cleaned pure aluminum core material into the degreased and cleaned pure copper tube material to complete the preparation of the wiring harness conductor substrate. It can be understood that the wiring harness conductor substrate is assembled in the form of the pure aluminum core material penetrating into the pure copper tube material;
[0046] Step S2, after completing the stretching of the wiring harness conductor substrate according to a preset single deformation rate, performing stress relief annealing, and repeating the stretching and stress relief annealing of the wiring harness conductor substrate until the diameter of the conductor reaches the designed size;
[0047] Step S3, coating the wire with an insulator by extrusion to complete the preparation of the wire harness core wire;
[0048] Step S4, detecting the conductivity coefficient of the wire harness core wire, and when it is preliminarily determined based on the measured conductivity coefficient that the preparation of the wire harness core wire does not meet the preset standard, increasing the cross-sectional area ratio of the pure copper tube to the pure aluminum core material for the preparation of the next batch of wire harness core wires, or increasing the annealing time of the stress relief annealing for the preparation of the next batch of wire harness core wires;
[0049] Step S5, twisting a number of the wire harness core wires that meet the preset standard, and then sequentially coating them with a shielding net and wrapping them with adhesive tape to complete the preparation of the wire harness baseline;
[0050] Step S6, cutting the wire harness base line according to a specified size and then peeling off the winding tape, the shielding net and the insulation layer of each of the wire harness core wires in turn;
[0051] Step S7, after extruding the end of the wire bundle base line after stripping, use brazing to complete welding of the end;
[0052] Step S8, assembling the terminal and the wiring terminal of the wiring harness base line, heating and pressing the terminal and the wiring terminal to complete the crimping;
[0053] Step S9, crimping the shielding ring and the packaging ring respectively to complete the preparation of the wiring harness;
[0054] Step S10, detecting the resistivity of the wiring harness, and determining whether the preparation of the wiring harness meets a preset standard based on the measured resistivity;
[0055] Step S11, packaging the wire harness that meets the preset standard.
[0056] Specifically, the tolerance of the interference fit is referred to GB∕T 5371-2004 Limits and fits - Calculation and selection of interference fits, and is not specifically limited, and only needs to satisfy the assembly of the conductor substrate.
[0057] Specifically, the insulation coating adopts an extruder, which is not specifically limited, and is used to coat the wire with an insulation layer.
[0058] Specifically, the brazing, such as tin wire welding or molten tin welding, is not specifically limited and is used to weld the end caps.
[0059] Specifically, crimping completes the connection between the wire harness base line and the terminal block through a crimping die, and the crimping should meet the requirements of "GB / T18290.2-2000 Solderless Connection Part 2: General Requirements, Test Methods and Usage Guidelines for Solderless Crimping Connections".
[0060] Specifically, in step S4, it is preliminarily determined whether the preparation of the wire harness core wire meets the preset standard according to the conductivity coefficient, wherein:
[0061] If the conductivity is less than the first preset conductivity threshold, it is preliminarily determined that the preparation of the wire harness core wire does not meet the preset standard and the cross-sectional area ratio of the pure copper tube to the pure aluminum core material for the next batch of wire harness core wires is increased, and the first preset conductivity threshold is set to 42.00×10 6 S / m, it can be understood that the cross-sectional area ratio represents the ratio of pure copper to pure aluminum in the wire harness core;
[0062] If the conductivity is greater than or equal to the first preset conductivity threshold and less than the second preset conductivity threshold, it is preliminarily determined that the preparation of the wire harness core wire does not meet the preset standard and the annealing time of the stress relief annealing of the next batch of wire harness core wire preparation is increased, and the second preset conductivity threshold is set to 51.50×10 6 S / m;
[0063] If the conductivity coefficient is greater than or equal to the second preset conductivity coefficient threshold, it is preliminarily determined that the preparation of the wiring harness core wire meets the preset standard, and after the tensile strength of the wiring harness core wire is tested, a secondary determination is made based on the measured tensile strength whether the preparation of the wiring harness core wire meets the preset standard.
[0064] Specifically, the tensile strength test of the wire harness core wire is obtained in accordance with "GB∕T4909.3-2009 Bare Wire Test Method Part 3_Tensile Test".
[0065] Specifically, the increase in the cross-sectional area ratio of the pure copper tube to the pure aluminum core material is positively correlated with the conductivity difference, and the conductivity difference is the difference between the first preset conductivity threshold and the measured conductivity. That is to say, when determining that it is necessary to adjust the cross-sectional area ratio of the pure copper tube to the pure aluminum core material for preparing the next batch of wiring harness core wires, the greater the conductivity difference, the greater the increase in the cross-sectional area ratio of the pure copper tube to the pure aluminum core material.
[0066] Specifically, under the first preset condition, the difference between the preset tensile strength threshold and the tensile strength of the wire harness core wire is calculated, and the difference is recorded as the strength difference, and the correction for the increase of the cross-sectional area ratio is determined based on the strength difference, wherein,
[0067] The first correction method is to use the first preset correction coefficient 0.998 to reduce the increased cross-sectional area ratio to a corresponding value by multiplying it by the increased cross-sectional area ratio; the first correction method satisfies that the strength difference is less than the first preset strength difference, and the first preset strength difference is set to 4.50 MPa;
[0068] The second correction method is to use the second preset correction coefficient 0.996 to reduce the increased cross-sectional area ratio to a corresponding value by multiplying it by the increased cross-sectional area ratio; the second correction method satisfies that the strength difference is greater than or equal to the first preset strength difference and less than the second preset strength difference, and the second preset strength difference is set to 11.25MPa;
[0069] The third correction method is to use the third preset correction coefficient 0.993 to reduce the increased cross-sectional area ratio to a corresponding value by multiplying it by the increased cross-sectional area ratio; the third correction method satisfies that the strength difference is greater than or equal to the second preset strength difference;
[0070] The first preset condition is that the tensile strength of the harness core wire after the cross-sectional area ratio of the pure copper tube to the pure aluminum core material is increased is less than a preset tensile strength threshold, and the preset tensile strength threshold is set to 110 MPa.
[0071] Specifically, under the condition that the preparation of the wire harness core wire is initially determined to meet the preset standard, a secondary determination is made based on the tensile strength whether the preparation of the wire harness core wire meets the preset standard, wherein:
[0072] If the tensile strength is less than the first preset tensile strength, it is determined that the preparation of the wire harness core wires does not meet the preset standard and the annealing temperature of the stress relief annealing of the next batch of wire harness core wires is reduced, and the first preset tensile strength is set to 95.00 MPa;
[0073] If the tensile strength is greater than or equal to the first preset tensile strength and less than the second preset tensile strength, it is determined that the preparation of the wire harness core wires does not meet the preset standard and the single deformation rate of the next batch of wire harness core wires is reduced, and the second preset tensile strength is set to 115.00 MPa;
[0074] If the tensile strength is greater than or equal to the second preset tensile strength, secondarily determining that the preparation of the wire harness core wire meets the preset standard and continuing to produce the wire harness core wire according to the current parameters;
[0075] It can be understood that the preset tensile strength threshold and the first preset tensile strength and the second preset tensile strength are all preset values. The difference is that the tensile strength threshold is used in the correction for the increase in the cross-sectional area ratio, and the first preset tensile strength and the second preset tensile strength are used to preliminarily determine whether the preparation of the wire harness core wire meets the preset standard under the condition that the preparation of the wire harness core wire meets the preset standard.
[0076] Specifically, in step S10, it is determined whether the preparation of the wiring harness meets the preset standard based on the resistivity, wherein:
[0077] The first preparation determines that the preparation of the wiring harness meets the preset standard and continues to produce the wiring harness according to the current parameters; the first preparation determines that the resistivity is less than the first preset resistivity, and the first preset resistivity is set to 2.55×10 -8 ;
[0078] The second preparation determines that the preparation of the wiring harness does not meet the preset standard, marks it as the first defective product, determines the welding evaluation value according to the historical first defective product data, and increases the wire feeding amount for the end welding of the next batch of wiring harnesses according to the welding evaluation value; the second preparation determines that the resistivity is greater than or equal to the first preset resistivity and less than the second preset resistivity, and sets the second preset resistivity to 9.85×10 -8 ;
[0079] The third preparation determines that the preparation of the wiring harness does not meet the preset standard, marks it as a second defective product, and determines whether the crimping meets the preset standard according to the defective rate and the second defective product ratio within a preset period; the third preparation determines that the resistivity is greater than or equal to the second preset resistivity;
[0080] The historical first defective product data includes the number of wiring harnesses marked as first defective products within a preset period and the resistivity of each wiring harness marked as first defective product, and the duration of the preset period is 24 hours.
[0081] Specifically, the welding evaluation value is obtained by formula (1):
[0082] (1),
[0083] In formula (1), Z is the welding evaluation value, is the resistivity of the wire harness marked as first-class defective products within the preset period, i=1,2,3...m, m is the total number of wire harnesses marked as first-class defective products within the preset period, To preset the welding evaluation threshold, set It can be understood that by comparing the average resistivity of the wire harness marked as first-level defective products within a preset period with the preset welding evaluation threshold, it can be used accurately and sensitively to evaluate the welding quality.
[0084] Specifically, the increase in the wire feeding amount for the end welding of the next batch of wire harnesses is positively correlated with the welding evaluation value, that is, the greater the comparison value between the average resistivity of the wire harness marked as a first-level defective product within the preset period and the preset welding evaluation threshold, the greater the increase in the wire feeding amount for the end welding.
[0085] Specifically, whether the crimping meets the preset standard is determined based on the defective rate and the proportion of the second defective products, wherein:
[0086] The first crimping judgment is that the crimping process meets the preset standard, and the terminal is continued to be crimped according to the current parameters; the first crimping judgment satisfies that the defective rate is less than the preset defective rate threshold, and the preset defective rate threshold is set to 3.52%;
[0087] The second crimping judgment is that the crimping process does not meet the preset standard, and the crimping pressure of the next batch of wiring harnesses is increased based on the difference between the preset proportion and the second defective product proportion; the second crimping judgment satisfies that the defective rate is greater than or equal to the preset defective rate threshold and the second defective product proportion is less than the preset proportion, and the preset proportion is set to 42.50%;
[0088] The third crimping judgment is that the crimping process does not meet the preset standard, and the crimping temperature for preparing the next batch of wire harnesses is increased based on the difference between the second defective product ratio and the preset ratio; the third crimping judgment satisfies that the defective rate is greater than or equal to the preset defective rate threshold and the second defective product ratio is greater than or equal to the preset ratio.
[0089] So far, the technical solutions of the present invention have been described in conjunction with the preferred embodiments shown in the accompanying drawings. However, it is easy for those skilled in the art to understand that the protection scope of the present invention is obviously not limited to these specific embodiments. Without departing from the principle of the present invention, those skilled in the art can make equivalent changes or substitutions to the relevant technical features, and the technical solutions after these changes or substitutions will fall within the protection scope of the present invention.
[0090] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A production process for automotive wiring harness, characterized in that: include: Step S1, interference fitting the degreased and cleaned pure aluminum core material to the degreased and cleaned pure copper tube material to complete the preparation of the wiring harness conductor substrate; Step S2, after completing the stretching of the wiring harness conductor substrate according to a preset single deformation rate, performing stress relief annealing, and repeating the stretching and stress relief annealing of the wiring harness conductor substrate until the diameter of the conductor reaches the designed size; Step S3, coating the wire with an insulator by extrusion to complete the preparation of the wire harness core wire; Step S4, detecting the conductivity coefficient of the wire harness core wire, and when it is preliminarily determined based on the measured conductivity coefficient that the preparation of the wire harness core wire does not meet the preset standard, increasing the cross-sectional area ratio of the pure copper tube to the pure aluminum core material for the preparation of the next batch of wire harness core wires, or increasing the annealing time of the stress relief annealing for the preparation of the next batch of wire harness core wires, and, when it is preliminarily determined based on the conductivity coefficient that the preparation of the wire harness core wire meets the preset standard, detecting the tensile strength of the wire harness core wire and secondarily determining whether the preparation of the wire harness core wire meets the preset standard based on the measured tensile strength; Step S5, twisting a number of the wire harness core wires that meet the preset standard, and then sequentially coating them with a shielding net and winding them with adhesive tape to complete the preparation of the wire harness baseline; Step S6, cutting the wire harness base line according to a specified size and then peeling off the winding tape, the shielding net and the insulation layer of each of the wire harness core wires in turn; Step S7, after extruding the end of the wire bundle base line after stripping, use brazing to complete welding of the end; Step S8, assembling the terminal and the wiring terminal of the wiring harness base line, heating and pressing the terminal and the wiring terminal to complete the crimping; Step S9, crimping the shielding ring and the packaging ring respectively to complete the preparation of the wiring harness; Step S10, detecting the resistivity of the wiring harness, and determining whether the preparation of the wiring harness meets a preset standard based on the measured resistivity; Step S11, packaging the wire harness that meets the preset standard.
2. The production process of automobile wiring harness according to claim 1, characterized in that: In step S4, the process of preliminarily determining that the preparation of the wire harness core wire does not meet the preset standard according to the conductivity coefficient includes comparing the conductivity coefficient with a first preset conductivity coefficient threshold and a second preset conductivity coefficient threshold, respectively. If the conductivity is less than the first preset conductivity threshold, then increasing the cross-sectional area ratio of the pure copper tube to the pure aluminum core material for preparing the next batch of wire harness core wires; If the conductivity is greater than or equal to the first preset conductivity threshold and less than the second preset conductivity threshold, the annealing time of the stress relief annealing for preparing the next batch of wire harness core wires is increased.
3. The production process of automobile wiring harness according to claim 2, characterized in that: The increase in the cross-sectional area ratio of the pure copper tube to the pure aluminum core material is positively correlated with the conductivity difference, and the conductivity difference is the difference between the first preset conductivity threshold and the measured conductivity.
4. The production process of automobile wiring harness according to claim 3, characterized in that: Under the first preset condition, several correction methods are provided for the increase of the cross-sectional area ratio, and each correction method has a different correction range for the increase of the cross-sectional area ratio. The first preset condition is that the tensile strength of the wire harness core wire after the cross-sectional area ratio of the pure copper tube and the pure aluminum core material is increased is less than a preset tensile strength threshold.
5. The production process of automobile wiring harness according to claim 4, characterized in that: When it is determined based on the tensile strength that the preparation of the wire harness core wires does not meet the preset standard, the annealing temperature of the stress relief annealing for the next batch of wire harness core wires is lowered, or the single deformation rate for the next batch of wire harness core wires is reduced.
6. The production process of automobile wiring harness according to claim 5, characterized in that: In the step S10, when it is determined based on the resistivity that the preparation of the wiring harness does not meet the preset standard, the wiring harness that does not meet the preset standard is marked as a first defective product and a welding evaluation value is determined according to the historical first defective product data, and the wire feeding amount for the end welding of the next batch of wiring harnesses is increased according to the welding evaluation value, or it is marked as a second defective product and whether the crimping meets the preset standard is determined according to the defective rate and the proportion of the second defective products within a preset period, and the historical first defective product data includes the number of wiring harnesses marked as first defective products within a preset period and the resistivity of each wiring harness marked as the first defective product; The welding evaluation value is obtained by formula (1): (1), In formula (1), Z is the welding evaluation value, is the resistivity of the wire harness marked as first-class defective products within the preset period, i=1,2,3...m, m is the total number of wire harnesses marked as first-class defective products within the preset period, It is the preset welding evaluation threshold.
7. The production process of automobile wiring harness according to claim 6, characterized in that: The increase in the wire feeding amount of the end welding is positively correlated with the welding evaluation value.
8. The production process of automobile wiring harness according to claim 7, characterized in that: When it is determined based on the defective rate and the second defective product ratio that the crimping does not meet the preset standard, the crimping pressure for preparing the next batch of wire harnesses is increased, or the crimping temperature for preparing the next batch of wire harnesses is increased.
Citation Information
Patent Citations
Automatic production line and processing technology of new energy automobile wire harness
CN116453765A
Copper aluminum alloy wire and manufacturing technology thereof
CN104575693A
Production process of special wire harness for new energy automobile
CN111489866A
New energy automobile battery wire harness production process
CN111969384A
Anti-siphon wire harness
CN208873914U