Manufacturing method of ceramic grinding disc
Through the mixing of ceramic abrasive grains and diamond abrasive grains and the molding and sintering process of composite binders, the problems of fragile and high cost ceramic grinding disc materials are solved, and the uniformity, wear resistance and stability of the ceramic grinding disc are improved. .
Patent Information
- Application Number
- CN202310320359.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-03-28
- Publication Date
- 2024-10-01
AI Technical Summary
The existing ceramic grinding disc material is prone to rust, wear, short life, high cost, and uneven abrasive distribution, which affects the consistency and stability of the grinding tool performance.
Ceramic abrasive grains and diamond abrasive grains are mixed in a ratio of 9.5:0.5, and combined with a composite binder for molding and sintering to make a ceramic grinding disc. The uniformity and hardness are ensured through drying, molding and sintering processes.
It achieves the uniformity, wear resistance, high hardness, and long life of the ceramic grinding disc, improves product consistency and stability, and reduces production costs.
Smart Images

Figure CN118721053A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of semiconductor technology, and in particular to a method for manufacturing a ceramic grinding disc. Background Art
[0002] In the application of high-end ceramic abrasive products, high requirements are placed on the uniformity of abrasive distribution in ceramic abrasives, and the consistency and stability of ceramic grinding tooth performance. Users require such ceramic abrasives to be sharp, stable in performance during use, and consistent between batches. In addition, there is also a demand to improve efficiency and reduce costs during the abrasive manufacturing process.
[0003] With the rapid development of the semiconductor industry, the requirements for the flatness and precision of the surface of electronic components are getting higher and higher, and the material of the grinding disc plays a key role in the performance of the grinding disc. At present, the types of grinding discs mainly include cast iron, tin discs, diamonds, etc., which have problems such as easy rust, easy wear, short life, and high cost. Summary of the invention
[0004] The purpose of the embodiment of the present invention is to provide a method for manufacturing a ceramic grinding disc, which can produce a ceramic grinding disc with good uniformity, wear resistance, high hardness and long service life. The product has high consistency and stability, and the manufacturing method is simple and effective with low cost.
[0005] In order to achieve the above object, an embodiment of the present invention provides a method for manufacturing a ceramic grinding disc, comprising:
[0006] The mixed abrasive grains and the composite binder are uniformly mixed according to a preset mass ratio to obtain a raw material for manufacturing the grinding disc;
[0007] Drying the raw materials;
[0008] The dried raw materials are placed in a mold for a grinding disc and molded to obtain a formed grinding disc;
[0009] The formed grinding disc is sintered to obtain a ceramic grinding disc.
[0010] Furthermore, the mixed abrasive particles include ceramic abrasive particles and diamond abrasive particles.
[0011] Furthermore, the weight ratio of the ceramic abrasive grains to the diamond abrasive grains is 9.5:0.5.
[0012] Furthermore, the particle size of the mixed abrasive is 10-15 μm.
[0013] Furthermore, the composite binder is prepared by mixing a granulating agent and isopropyl alcohol.
[0014] Furthermore, the mass ratio is 5:1.
[0015] Furthermore, the drying process of the manufacturing raw materials specifically includes:
[0016] The manufacturing raw materials are placed in a constant temperature drying oven for drying; wherein the drying temperature is 80° C. to 100° C., and the drying time is 30 min to 50 min.
[0017] Furthermore, the step of placing the dried raw materials into a manufacturing mold for a grinding disc for molding to obtain a molded grinding disc specifically includes:
[0018] The dried raw materials were placed in a mold for a grinding disc for molding, and heated at a constant temperature of 150° C. to obtain a molded grinding disc; wherein the molding pressure was 8T and the molding time was 4 hours.
[0019] Furthermore, before sintering the formed grinding disc, the method further comprises:
[0020] The formed grinding disc is subjected to natural cooling.
[0021] Furthermore, the sintering treatment of the formed grinding disc to obtain the ceramic grinding disc specifically includes:
[0022] The formed grinding disc is placed in a muffle furnace for sintering to obtain a ceramic grinding disc; wherein the sintering temperature is 800° C. to 1000° C., the sintering time is 6 hours, and the Mohs hardness of the ceramic grinding disc is 9.
[0023] Compared with the prior art, the embodiment of the present invention provides a method for manufacturing a ceramic grinding disc. First, the mixed abrasive particles and the composite binder are evenly mixed in a preset mass ratio to obtain a raw material for manufacturing the grinding disc; then, the raw material is dried, and the dried raw material is placed in a manufacturing mold of the grinding disc for molding to obtain a formed grinding disc; finally, the formed grinding disc is sintered to obtain a ceramic grinding disc; the embodiment of the present invention can produce a ceramic grinding disc with good uniformity, wear resistance, high hardness and long service life. The product has high consistency and stability, and the manufacturing method is simple and effective with low cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 It is a flow chart of a preferred embodiment of a method for manufacturing a ceramic grinding disc provided by the present invention. DETAILED DESCRIPTION
[0025] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this technical field without creative work are within the scope of protection of the present invention.
[0026] The present invention provides a method for manufacturing a ceramic grinding disc. Figure 1 FIG. 1 is a flow chart of a preferred embodiment of a method for manufacturing a ceramic grinding disc provided by the present invention, wherein the method comprises steps S11 to S14:
[0027] Step S11, uniformly mixing the mixed abrasive grains and the composite binder according to a preset mass ratio to obtain a raw material for manufacturing a grinding disc;
[0028] Step S12, drying the manufacturing raw materials;
[0029] Step S13, placing the dried raw materials into a manufacturing mold for a grinding disc for molding to obtain a molded grinding disc;
[0030] Step S14: sintering the formed grinding disc to obtain a ceramic grinding disc.
[0031] In the specific implementation, first, the prepared mixed abrasive and composite binder are mixed together according to a preset mass ratio and stirred evenly to obtain the manufacturing raw materials of the grinding disc; then, the manufacturing raw materials of the grinding disc are dried, and the dried manufacturing raw materials are placed in a special manufacturing mold for the grinding disc for molding to fix it into shape, and a molded grinding disc is obtained; finally, the molded grinding disc is sintered to obtain a ceramic grinding disc.
[0032] As a preferred embodiment, the mixed abrasive particles include ceramic abrasive particles and diamond abrasive particles.
[0033] As a preferred embodiment, the weight ratio of the ceramic abrasive grains to the diamond abrasive grains is 9.5:0.5.
[0034] As a preferred solution, the particle size of the mixed abrasive is 10-15 μm.
[0035] Specifically, in combination with the above embodiment, the mixed abrasive grains are prepared by mixing ceramic abrasive grains and diamond abrasive grains in a weight ratio of 9.5:0.5, and the particle sizes of the ceramic abrasive grains and diamond abrasive grains are in the range of 10 μm to 15 μm.
[0036] Exemplarily, the particle size may be 10 μm, 11 μm, 12 μm, 13 μm, 14 μm or 15 μm, and may also be set according to actual needs, which is not specifically limited in the embodiment of the present invention.
[0037] As a preferred solution, the composite binder is prepared by mixing a granulating agent and isopropanol.
[0038] Specifically, in combination with the above embodiment, the composite adhesive is prepared by mixing a granulating agent and isopropyl alcohol, wherein the granulating agent can be WS-120 granulating agent, and the WS-120 granulating agent is added to isopropyl alcohol to dissolve and stir evenly to obtain the composite adhesive.
[0039] For example, 20 kg of WS-120 granulating agent is added to 500 L of isopropanol to dissolve and stir evenly to prepare granulated rubber.
[0040] As a preferred solution, the mass ratio is 5:1.
[0041] Specifically, in combination with the above embodiment, the mass ratio of the mixed abrasive to the composite binder is 5:1, that is, the mixed abrasive and the composite binder are uniformly mixed in a mass ratio of 5:1 to obtain the raw material for manufacturing the grinding disc.
[0042] Exemplarily, in the mixing tank, the mass of the mixed abrasive is 100kg, of which the ceramic abrasive is 95kg, the diamond abrasive is 5g, and the mass of the composite binder is 20kg. The ceramic abrasive and diamond abrasive are first mixed evenly, and then the composite binder is added and stirred evenly to obtain the raw material for the manufacturing of the grinding disc.
[0043] As a preferred solution, the drying process of the manufacturing raw materials specifically includes:
[0044] The manufacturing raw materials are placed in a constant temperature drying oven for drying; wherein the drying temperature is 80° C. to 100° C., and the drying time is 30 min to 50 min.
[0045] Specifically, in combination with the above embodiment, when the raw materials for manufacturing the grinding disc are dried, the raw materials can be placed in a constant temperature drying oven and dried at a temperature of 80°C to 100°C, and the drying process lasts for 30 minutes to 50 minutes.
[0046] Exemplarily, the drying temperature can be 80°C, 81°C, 82°C, 83°C, 84°C, 85°C, 86°C, 87°C, 88°C, 89°C, 90°C, 91°C, 92°C, 93°C, 94°C, 95°C, 96°C, 97°C, 98°C, 99°C or 100°C, and can also be set according to actual needs, which is not specifically limited in the embodiments of the present invention.
[0047] Exemplarily, the drying time can be 30 minutes, 31 minutes, 32 minutes, 33 minutes, 34, 35 minutes, 36 minutes, 37 minutes, 38 minutes, 39 minutes, 40 minutes, 41 minutes, 42 minutes, 43 minutes, 44, 45 minutes, 46 minutes, 47 minutes, 48 minutes, 49 minutes or 50 minutes, and can also be set according to actual needs, which is not specifically limited in the embodiments of the present invention.
[0048] As a preferred embodiment, the step of placing the dried raw materials into a manufacturing mold of a grinding disc for molding to obtain a molded grinding disc specifically includes:
[0049] The dried raw materials were placed in a mold for a grinding disc for molding, and heated at a constant temperature of 150° C. to obtain a molded grinding disc; wherein the molding pressure was 8T and the molding time was 4 hours.
[0050] Specifically, in combination with the above embodiment, when the dried manufacturing raw materials are molded, the dried manufacturing raw materials can be placed in a special manufacturing mold for the grinding disc for molding, and heated at a constant temperature of 150°C, with the pressure set to 8T and the time set to 4 hours to fix the molding, thereby obtaining a molded grinding disc.
[0051] As a preferred embodiment, before sintering the formed grinding disc, the method further comprises:
[0052] The formed grinding disc is subjected to natural cooling.
[0053] Specifically, in combination with the above embodiments, after obtaining the molded grinding disc, before sintering the molded grinding disc, the molded grinding disc can be allowed to cool naturally, and after the temperature of the molded grinding disc is reduced to ambient temperature, the molded grinding disc can be sintered.
[0054] As a preferred embodiment, the sintering treatment of the formed grinding disc to obtain the ceramic grinding disc specifically includes:
[0055] The formed grinding disc is placed in a muffle furnace for sintering to obtain a ceramic grinding disc; wherein the sintering temperature is 800° C. to 1000° C., the sintering time is 6 hours, and the Mohs hardness of the ceramic grinding disc is 9.
[0056] Specifically, in combination with the above embodiment, when the formed grinding disc is sintered, the formed grinding disc can be placed in a muffle furnace for sintering, and the temperature is set within the range of 800°C to 1000°C, and kept warm for 6 hours, thereby obtaining a ceramic grinding disc, and the hardness of the ceramic grinding disc reaches Mohs hardness level 9.
[0057] Exemplarily, the sintering temperature can be 800℃, 810℃, 820℃, 830℃, 840℃, 850℃, 860℃, 870℃, 880℃, 890℃, 900℃, 910℃, 920℃, 930℃, 940℃, 950℃, 960℃, 970℃, 980℃, 990℃ or 1000℃, and can also be set according to actual needs, which is not specifically limited in the embodiments of the present invention.
[0058] It should be noted that the embodiment of the present invention mixes ceramic abrasives and diamond abrasives to make the mixed abrasives evenly distributed, and molds them in a special mold, which is beneficial to the uniform distribution of the material and avoids the problem of uneven material distribution when the grinding disc is molded, thereby obtaining a ceramic grinding disc with excellent properties such as good uniformity, high temperature resistance, wear resistance, high hardness, long life, and no toxic side effects. At the same time, the ceramic grinding disc has good consistency and high stability, and the manufacturing method is simple and effective, and the cost is low.
[0059] In combination with all the above embodiments, the implementation process of the present scheme is described below through the first specific embodiment, including: (1) mixing the prepared mixed abrasive grains and the composite binder in a mass ratio of 5:1, and stirring evenly to obtain the raw materials for manufacturing the grinding disc; wherein the mixed abrasive grains are prepared by mixing ceramic abrasive grains and diamond abrasive grains in a weight ratio of 9.5:0.5, and the particle size of the ceramic abrasive grains and the diamond abrasive grains is 10 μm; the composite binder is prepared by mixing a granulating agent and isopropyl alcohol; (2) placing the raw materials for manufacturing the grinding disc in a constant temperature drying oven to The raw material is dried at 80°C for 30 minutes; (3) the dried raw material is placed in a special manufacturing mold for a grinding disc for molding, and heated at a constant temperature of 150°C, with a pressure of 8T set for 4 hours to fix the shape, thereby obtaining a molded grinding disc; (4) after the molded grinding disc is naturally cooled, the molded grinding disc is placed in a muffle furnace for sintering, and the temperature is set to 800°C for 6 hours to obtain a ceramic grinding disc; wherein the hardness of the ceramic grinding disc reaches Mohs hardness level 9.
[0060] In combination with all the above embodiments, the implementation process of the present scheme is described below through a second specific embodiment, including: (1) mixing the prepared mixed abrasive grains and the composite binder in a mass ratio of 5:1, and stirring evenly, and obtaining the raw materials for manufacturing the grinding disc; wherein the mixed abrasive grains are prepared by mixing ceramic abrasive grains and diamond abrasive grains in a weight ratio of 9.5:0.5, and the particle size of the ceramic abrasive grains and the diamond abrasive grains is 12 μm; the composite binder is prepared by mixing a granulating agent and isopropyl alcohol; (2) placing the raw materials for manufacturing the grinding disc in a constant temperature drying oven to The raw material is dried at 90°C for 40 minutes; (3) the dried raw material is placed in a special manufacturing mold for a grinding disc for molding, and heated at a constant temperature of 150°C, with a pressure of 8T set for 4 hours to fix the shape, thereby obtaining a molded grinding disc; (4) after the molded grinding disc is naturally cooled, the molded grinding disc is placed in a muffle furnace for sintering, and the temperature is set to 900°C for 6 hours to obtain a ceramic grinding disc; wherein the hardness of the ceramic grinding disc reaches Mohs hardness level 9.
[0061] In combination with all the above embodiments, the implementation process of the present solution is described below through a third specific embodiment, comprising: (1) mixing the prepared mixed abrasive grains and the composite binder in a mass ratio of 5:1, and stirring evenly, to obtain the raw materials for manufacturing the grinding disc; wherein the mixed abrasive grains are prepared by mixing ceramic abrasive grains and diamond abrasive grains in a weight ratio of 9.5:0.5, and the particle size of the ceramic abrasive grains and the diamond abrasive grains is 15 μm; the composite binder is prepared by mixing a granulating agent and isopropyl alcohol; (2) placing the raw materials for manufacturing the grinding disc in a constant temperature drying oven at 1 00°C for drying for 50 min; (3) placing the dried raw material into a special manufacturing mold for a grinding disc for molding, and heating it at a constant temperature of 150°C, setting the pressure to 8T for 4 hours to fix it into shape, thereby obtaining a molded grinding disc; (4) after the molded grinding disc is naturally cooled, placing the molded grinding disc in a muffle furnace for sintering, and setting the temperature to 1000°C for 6 hours to obtain a ceramic grinding disc; wherein the hardness of the ceramic grinding disc reaches Mohs hardness level 9.
[0062] In summary, the manufacturing method of a ceramic grinding disc provided in an embodiment of the present invention comprises the following steps: first, the mixed abrasive particles and the composite binder are uniformly mixed in a preset mass ratio to obtain a raw material for the grinding disc; then, the raw material is dried, and the dried raw material is placed in a manufacturing mold of the grinding disc for molding to obtain a formed grinding disc; finally, the formed grinding disc is sintered to obtain a ceramic grinding disc; the embodiment of the present invention can produce a ceramic grinding disc with good uniformity, wear resistance, high hardness and long service life, the product has high consistency and stability, and the manufacturing method is simple and effective with low cost.
[0063] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the technical principles of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. A method for manufacturing a ceramic grinding disc, characterized in that: include: The mixed abrasive grains and the composite binder are uniformly mixed according to a preset mass ratio to obtain a raw material for manufacturing the grinding disc; Drying the raw materials; The dried raw materials are placed in a mold for a grinding disc and molded to obtain a formed grinding disc; The formed grinding disc is sintered to obtain a ceramic grinding disc.
2. The method for manufacturing a ceramic grinding disc according to claim 1, characterized in that: The mixed abrasive grains include ceramic abrasive grains and diamond abrasive grains.
3. The method for manufacturing a ceramic grinding disc according to claim 2, characterized in that: The weight ratio of the ceramic abrasive grains to the diamond abrasive grains is 9.5:0.
5.
4. The method for manufacturing a ceramic grinding disc according to claim 2, characterized in that: The particle size of the mixed abrasive particles is 10-15 μm.
5. The method for manufacturing a ceramic grinding disc according to claim 1, characterized in that: The composite binder is prepared by mixing a granulating agent and isopropyl alcohol.
6. The method for manufacturing a ceramic grinding disc according to claim 1, characterized in that: The mass ratio is 5:
1.
7. The method for manufacturing a ceramic grinding disc according to claim 1, characterized in that: The drying process of the manufacturing raw materials specifically includes: The manufacturing raw materials are placed in a constant temperature drying oven for drying; wherein the drying temperature is 80° C. to 100° C., and the drying time is 30 min to 50 min.
8. The method for manufacturing a ceramic grinding disc according to claim 1, characterized in that: The step of placing the dried raw materials into a manufacturing mold for a grinding disc for molding to obtain a molded grinding disc specifically includes: The dried raw materials were placed in a mold for a grinding disc for molding, and heated at a constant temperature of 150° C. to obtain a molded grinding disc; wherein the molding pressure was 8T and the molding time was 4 hours.
9. The method for manufacturing a ceramic grinding disc according to claim 1, wherein: Before sintering the formed grinding disc, the method further comprises: The formed grinding disc is subjected to natural cooling.
10. The method for manufacturing a ceramic grinding disc according to claim 1, characterized in that: The sintering treatment of the formed grinding disc to obtain the ceramic grinding disc specifically includes: The formed grinding disc is placed in a muffle furnace for sintering to obtain a ceramic grinding disc; wherein the sintering temperature is 800° C. to 1000° C., the sintering time is 6 hours, and the Mohs hardness of the ceramic grinding disc is 9.
Citation Information
Patent Citations
Ceramic bond abrasive disc and preparation method thereof
CN105108665A
Ceramic bonding agent, ceramic bonding agent abrasive disk and preparation method of ceramic bonding agent abrasive disk
CN106737255A
Manufacturing method of ceramic grinding teeth
CN111941299A
Ceramic-based diamond grinding wheel for grinding semiconductor plastic package body and manufacturing method of ceramic-based diamond grinding wheel
CN114393522A
Polycrystalline microcrystal glass ceramic binding agent and preparation method thereof, diamond ceramic grinding wheel and preparation method thereof
CN115351719A