Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-01
Estimated Expiration
2043-03-31

AI Technical Summary

Technical Problem

The existing chromium drainage sand causes secondary oxidation of the molten steel during the automatic opening and pouring of the ladle, affecting the quality of the steel billet. Moreover, because it contains Cr2O3, SiO2 and Fe2O3, it increases the inclusions of the molten steel and causes environmental pollution, and the cost is high.

Method used

Calcium titanium aluminate is used as the main raw material, combined with potassium feldspar or silica powder as the sintering agent, to prepare chromium-free drainage sand, which improves its sintering performance and fluidity at high temperatures and reduces the impact on the purity of molten steel.

Benefits of technology

It significantly reduces the influence of the purity of molten steel, reduces production costs, avoids environmental pollution by chromium diversion sand, and improves the self-opening rate of the diversion sand and the natural opening rate of the ladle nozzle.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004155675640000051
    Figure BDA0004155675640000051
  • Figure BDA0004155675640000061
    Figure BDA0004155675640000061
Patent Text Reader

Abstract

The invention relates to steel ladle chromium-free stuffing sand which comprises the following components in percentage by weight: 97.5-98.5% of titanium calcium aluminate with the particle size of 1.2-0.1 mm; and 1.5-2.5% of a sintering agent, namely potassium feldspar and / or silica powder. According to the chromium-free ladle filler sand for the steel ladle, the titanium calcium aluminate is adopted as the main raw material to produce the ladle filler sand, and compared with chromium ladle filler sand, the influence of the ladle filler sand on the purity of tundish molten steel can be greatly reduced; moreover, the titanium calcium aluminate is an industrial by-product, the price is lower than that of the main raw material chromite of the current chrome stuffing sand, and the cost advantage is achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of steelmaking, in particular to a chromium-free drainage sand for a ladle. Background Art

[0002] Automatic ladle pouring refers to the process in which the molten steel can automatically flow out of the ladle through the upper water inlet, the upper slide steel hole, the lower slide, and the lower water inlet after the sliding water inlet is opened, and then flow into the tundish through the water inlet. If automatic pouring cannot be performed and the method of burning oxygen for drainage is adopted, the molten steel will be poured openly, causing secondary oxidation of the molten steel and affecting the quality of the steel billet.

[0003] Drainage sand is added to the ladle nozzle, from top to bottom, they are the base brick, upper nozzle, and upper slide hole. Drainage sand is a granular high-temperature resistant material with a certain heat insulation effect, so the temperature gradually decreases from top to bottom. The drainage sand added to the nozzle forms a three-layer structure. The drainage sand in contact with the high-temperature molten steel forms a melting layer, the lower part of the melting layer forms a solid phase sintering layer, and the bottom is the unsintered granular drainage sand.

[0004] When the ladle is opened for pouring, the loose drainage sand under the sintering layer flows out by gravity, and then the strong static pressure of the molten steel breaks the drainage sand sintering layer, allowing the molten steel to automatically flow out of the water outlet. The sintering layer plays a vital role in the automatic opening of the ladle. If the sintering layer is too thin or too thick, it is not conducive to automatic opening.

[0005] The quality of drainage sand mainly depends on the material, particle size, flowability, sintering performance and thermal expansion performance. The better the flowability of the drainage sand, the higher the self-opening rate of the ladle. The sintering performance of the drainage sand requires that the surface layer of the material can be lightly sintered and have a certain strength to prevent the penetration of molten steel, while at the same time requiring that the strength of the sintered layer cannot be too high to be destroyed by the static pressure of the molten steel. The thermal expansion rate of the drainage sand should be small, because a large expansion rate will increase the internal stress of the drainage sand, squeeze each other and increase the adhesion to the inner wall of the nozzle, which is not conducive to the free fall of the drainage sand during pouring, and even serious "bridging" phenomenon will occur.

[0006] As the purity requirements for high-quality steel such as automobile plates become higher and higher, higher requirements are placed on the quality of drainage sand. In addition to the function of drainage and pouring, drainage sand also needs to reduce the impact on the purity of molten steel. Therefore, it poses a challenge to traditional chromium drainage sand.

[0007] For example, Chinese patent application No. 201710843919.0 discloses a chromium drainage sand for refined ladle and its preparation method, which is used to solve the problems of low automatic pouring rate, high production cost and large environmental impact of drainage sand. A chromium drainage sand for refined ladle includes the following raw materials by mass percentage: 1-20% chromium ore, 40-60% calcium titanate fused balls, 30-40% fracturing quartz sand and 0.6-1% carbon additive, wherein the carbon additive carbon is a mixture of carbon black and graphite. The calcium titanate introduced in the invention is used as industrial waste slag for steelmaking, and it is applied to the drainage sand, which is effectively recycled and reused, greatly reducing the production cost. The calcium titanate fused balls are used to partially replace the chromium ore, reduce pollution, clean the molten steel, and solve the problems of dependence on imported raw materials and high cost. However, since it is equipped with a certain amount of chromium ore, it still contains a certain amount of Cr2O3, SiO2 and Fe2O3, which affects the purity of the molten steel.

[0008] Chrome sand has the characteristics of high self-opening rate and low cost. Currently, most steel mills use chrome sand as ladle drainage sand. However, chrome sand contains a large amount of Cr2O3 (30-35%), Fe2O3 (18-24%) and SiO2 (20-24%). These oxides cause secondary oxidation of molten steel, increase molten steel inclusions, and aggravate the blockage of stopper rods and submerged nozzles. In addition, chromium-containing materials have an impact on the environment.

[0009] The following types of chromium-free drainage sands are used and reported publicly:

[0010] 1) Silica sand. Low cost, wide source, and good self-opening rate. For example, Chinese patent application No. 201610490918.8 discloses a siliceous drainage sand and a preparation method thereof, wherein the siliceous drainage sand comprises: silica sand; carbon powder; and vegetable oil. Compared with the prior art using water as a binder, vegetable oil itself has better adhesion, and can well bond the lighter carbon powder to the surface of silica sand, effectively preventing the carbon powder in the drainage sand from flying; at the same time, when vegetable oil meets high-temperature molten steel or steel slag, it will not produce a single hydrogen element, thereby effectively avoiding the deficiency of using water as a binder in the prior art, where water decomposes at high temperature to produce hydrogen elements and affects the cleanliness of the molten steel.

[0011] However, silica sand is generally only used for steel grades that require less than 45 minutes from tapping to pouring, and is not suitable for high-grade steel grades that require a long smelting time. In addition, the main component of silica sand is SiO2, which will increase oxygen when entering the molten steel, which is not conducive to the purity of the molten steel.

[0012] 2) Forsterite. The basic properties of forsterite can meet the requirements of drainage sand, and it is a cheap drainage sand. However, in actual use, the automatic pouring rate of mold casting can reach 95%, but the automatic pouring rate of continuous casting is low, and steel mills have rarely used it.

[0013] 3) Zircon sand. The melting point of zircon sand is higher than 1800℃, and it is valued in steel mills with high tapping temperature and long tapping to pouring time. However, due to its high price, zircon sand is not widely used.

[0014] 4) Magnesium drainage sand. This is a patent report. Although magnesium materials are resistant to high temperatures, they have a large expansion coefficient and expand more at high temperatures, which is not conducive to the self-opening rate of drainage sand.

[0015] 5) Corundum drainage sand. For example, Chinese patent application No. 201410380216.5 discloses a plate-like corundum drainage sand and a preparation method thereof, wherein the plate-like corundum drainage sand is composed of the following raw materials by weight: 83-95 plate-like corundum sand; 0.5-10 magnesia sand; 0.2-5 graphite; 1-5 high-temperature sintering agent; 0.2-2 low-temperature sintering agent. The particle size of the plate-like corundum sand is 0.15-2 mm. The particle size of the magnesia sand is 0.088-1 mm. The particle size of the graphite is ≤0.088 mm. The high-temperature sintering agent is at least one of metal silicon, boron carbide, and metal aluminum. The low-temperature sintering agent is borax or boric acid. The plate-like corundum drainage sand provided by the invention does not contain chromium oxide and SiO2, does not pollute the molten steel and the environment, and can achieve a higher natural pouring rate of the ladle nozzle. Although the main raw material, plate-shaped corundum, is resistant to high temperatures and does not expand much, its disadvantage is that it is expensive. The auxiliary raw material, magnesia, expands greatly, which is not conducive to the self-opening rate of drainage sand. Summary of the invention

[0016] The purpose of the present invention is to provide a chromium-free drainage sand for a ladle. The drainage sand is produced by using calcium titanate as a main raw material. Compared with chromium drainage sand, the influence of the drainage sand on the purity of molten steel in the tundish can be greatly reduced. Moreover, calcium titanate is an industrial by-product, and its price is lower than chromite, the main raw material of the current chromium drainage sand, and it has a cost advantage.

[0017] To achieve the above object, the technical solution of the present invention is:

[0018] A chromium-free ladle drainage sand comprises the following components by weight: calcium aluminate titanate, 97.5-98.5%, with a particle size of 1.2-0.1 mm; and a sintering agent, potassium feldspar and / or silicon micropowder, 1.5-2.5%.

[0019] Preferably, in the calcium aluminate titanate, the particle size of 1.2 to 0.1 mm accounts for 30 to 50%, and the particle size of 0.5 to 0.1 mm accounts for 45 to 70%.

[0020] Preferably, the sintering agent is 1.5-2.5% potassium feldspar, or a combination of 0.5-1.2% potassium feldspar and 0.5-1.5% silicon powder.

[0021] Preferably, the SiO2 content of the silicon micropowder is not less than 92% and the particle size is less than 1 μm.

[0022] The present invention uses calcium aluminate as the main raw material to produce drainage sand. Calcium aluminate is a byproduct produced during the smelting process of titanium-iron alloy. It is a high-melting-point complex phase material with calcium aluminate and calcium hexaaluminate as the main materials and calcium dialumate and calcium titanate as the secondary materials. Its refractoriness can reach above 1790°C and has good utilization value in high-temperature industries.

[0023] The composition of calcium aluminotitanate is as follows: Al2O3: 74-76%, TiO2: 13-15%, CaO: 9-11%, MgO: 1.5-1.7%, Fe2O3: 0.6-0.8%, SiO2: 0.2-0.5%, K2O: 0.06-0.07%, Na2O: 0.1-0.2%.

[0024] It can be seen that the main components of calcium titanate are Al2O3, TiO2 and CaO, with a small amount of MgO, Fe2O3, SiO2 and other impurities. Calcium titanate has a high melting point and can be used as a raw material for drainage sand. In addition, calcium titanate does not contain Cr2O3, Fe2O3 and SiO2 components in chromium drainage sand, which is beneficial to improving the purity of molten steel in the tundish. In addition, calcium titanate is an industrial by-product, and its price is lower than chromite, the main raw material of chromium drainage sand, which has a cost advantage.

[0025] In addition, the particle size of the drainage sand is very important. If the particle size is large, it is not easy to sinter. If the particle size is coarse, the gaps between the particles are large, and molten steel can easily penetrate, affecting the self-opening of the drainage sand. If the particle size is fine, the fluidity of the particles is poor. After the drainage sand is added, the filling property in the water inlet is not good. Moreover, if the particle size is fine, over-sintering may occur at high temperature, which also affects the self-opening of the drainage sand. Therefore, the particle size of the main raw material calcium aluminate of the present invention is 1.2-0.1mm. In this particle size range, the particle fluidity is better. Preferably, the particle size is 1.2-0.5mm, accounting for 30-50%, and the particle size is 0.5-0.1mm, accounting for 45-70%.

[0026] Calcium aluminate titanate itself will not sinter at high temperatures, so a sintering agent needs to be added. Potassium feldspar or sodium feldspar or a small amount of silicon powder is added as a sintering agent to make calcium aluminate titanate sinter to a certain extent at high temperatures. Potassium feldspar has a low melting point and can aid sintering at high temperatures. The particle size of potassium feldspar is required to be less than 0.1mm. If the particle size is greater than 0.1mm, the sintering effect is poor. By adding a small amount of SiO2 powder, a CaO-Al2O3-SiO2 glass phase is formed with CaO and Al2O3 in calcium aluminate titanate, promoting the high-temperature sintering of calcium aluminate titanate. The purity of SiO2 powder is required to be not less than 92%, and the particle size is less than 1μm.

[0027] Beneficial effects of the present invention:

[0028] When continuous casting begins, all the drainage sand in the water inlet and the base brick will enter the tundish. Most of the drainage sand will float up after entering the tundish, but a small part will not float up. Assuming that 10% of the drainage sand cannot float up, and some components of the drainage sand react with the acid-molten aluminum in the molten steel, causing secondary oxidation of the molten steel and increasing the inclusions in the molten steel.

[0029] The chromium-free ladle drainage sand of the present invention is mainly made of calcium aluminotitanate and a certain sintering agent. Compared with the existing chromium sand, Cr2O3, Fe2O3 and SiO2 will react with acid-molten aluminum, and the drainage sand of the present invention only has TiO2 that reacts with acid-molten aluminum. Compared with chromium sand, the impact of the present invention on the purity of molten steel is reduced by 81%. At the same time, calcium aluminotitanate is an industrial by-product, and its price is lower than chromite, the main raw material of the current chromium drainage sand, and it has a cost advantage.

[0030] Compared with Chinese patent application No. 201710843919.0, 1-20% chromium ore sand, 40-60% calcium aluminate titanate, and 30-40% fracturing quartz sand are used. First, chromium sand contains a large amount of Cr2O3 (30-35%), Fe2O3 (18-24%), and SiO2 (20-24%). These oxides cause secondary oxidation of molten steel, increase molten steel inclusions, and aggravate the blockage of stopper rods and submerged nozzles; moreover, chromium-containing materials have an impact on the environment; secondly, there are still certain Cr2O3, SiO2, and Fe2O3, which have an impact on the purity of molten steel. The present invention uses all calcium aluminate titanate, without Cr2O3, SiO2, and Fe2O3, which is conducive to improving the purity of molten steel. DETAILED DESCRIPTION

[0031] The present invention will be further described below in conjunction with the embodiments.

[0032] The examples of the present invention and the comparative examples are shown in Table 1. Table 1 lists the examples of the present invention and the comparative examples. The particle size of calcium aluminotitanate is 1.2-0.5 mm, accounting for 40%, and 0.5-0.1 mm, accounting for 60%.

[0033] In the embodiment of the present invention, calcium aluminotitanate is used as the main raw material, a certain sintering agent is added, drainage sand is placed in a corundum crucible, and high-temperature calcination is performed at 1600° C. for 2 hours, and then the sintering condition of the drainage sand is observed.

[0034] As shown in Table 1, the amount of sintering agent added in the embodiment of the present invention is appropriate, the drainage sand is basically sintered, and it is conducive to self-opening.

[0035] In comparative example 1, the amount of sintering agent added was insufficient, and the drainage sand was partially sintered. In comparative example 2, the amount of sintering agent added was too much, and the drainage sand was over-sintered. Both small amount of sintering and over-sintering will affect the self-opening rate of the drainage sand. Therefore, the present invention adds 1.5-2.5% potassium feldspar, or uses 0.5-1.2% potassium feldspar and 0.5-1.5% silicon powder as a sintering agent, and the drainage sand is basically sintered, which is conducive to self-opening.

[0036] Table 1 Unit: Weight percentage

[0037]

[0038]

Claims

1. A chromium-free ladle drainage sand, characterized in that: The weight percentage of its components is: Calcium aluminate titanate, 97.5-98.5%, particle size 1.2-0.1 mm; Sintering agent, potassium feldspar and / or silica powder, 1.5-2.5%.

2. The chromium-free ladle drainage sand according to claim 1, characterized in that: In the calcium alumino-titanate, the particle size of 1.2-0.1 mm accounts for 30-50%; the particle size of 0.5-0.1 mm accounts for 45-70%.

3. The chromium-free ladle drainage sand according to claim 1, characterized in that: The sintering agent is 1.5-2.5% potassium feldspar, or 0.5-1.2% potassium feldspar + 0.5-1.5% silicon powder.

4. The chromium-free ladle drainage sand according to claim 1, characterized in that: The SiO2 in the silicon micropowder is not less than 92% and the particle size is less than 1 μm.

Citation Information

Patent Citations

  • Plate-shaped corundum ladle filler sand and preparation method thereof

    CN104193353A

  • Siliceous stuffing sand and preparation method thereof

    CN106116603A

  • Chrome stuffing sand for refining ladles, and production method thereof

    CN107651968A

  • Titanium calcium aluminate-silicon carbide complex phase refractory material and preparation method thereof

    CN108484186A

  • Blast furnace permanent ceramic tapping iron ladle and preparation method thereof

    CN108774054A

Cited By

  • Titanium calcium aluminate refractory material taking aluminum titanium slag as raw material and preparation method of titanium calcium aluminate refractory material

    CN121609559A

  • Calcium titan-aluminate refractory material using aluminum titanium slag as raw material and preparation method thereof

    CN121609559B