Magnesium alloy wire capable of being differentially degraded and preparation method
By adjusting the composition and structure of the magnesium alloy wire, combined with the multi-physics control process, the differential degradation of the magnesium alloy wire is achieved, which solves the problem of accelerated degradation rate of the magnesium alloy wire after plastic deformation and improves its durability. Corrosion resistance and mechanical properties to meet the stability and performance requirements of clinical applications.
Patent Information
- Application Number
- CN202411069355.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-06
- Publication Date
- 2024-10-01
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The degradation rate of magnesium alloy wire accelerates during the plastic deformation process, resulting in its strength and toughness being affected, and it cannot meet the requirements for the mechanical properties of implants in clinical applications.
By adjusting the composition of the Mg-Zn-Ca rare earth magnesium alloy, controlling its microstructure and surface treatment, and combining multi-physical field control such as magnetic fields and ultrasonic waves to optimize the drawing process parameters, differential degradation of magnesium alloy wires can be achieved.
The corrosion resistance and mechanical properties of magnesium alloy wire are improved, the degradation rate can be controlled in specific environments, the degradation can be delayed or accelerated, and the stability and performance requirements of clinical applications can be met.
Smart Images

Figure CN118726809A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of alloy wires, and in particular to a magnesium alloy wire capable of differential degradation and a preparation method thereof. Background Art
[0002] Alloy wire refers to a filamentous material made by mixing two or more metal elements (or non-metallic elements and metal elements) through processes such as drawing or forging. Magnesium alloy wire is an alloy wire composed of magnesium and other elements. It has the characteristics of light weight, high strength, good corrosion resistance, and high plasticity and toughness. It is used in 3D printing, wire, metal processing, biomedicine and other fields.
[0003] For clinical applications of degradable magnesium alloy wires, plastic deformation is often performed on the wires. However, tensile stress is generated in the plastic deformation area, which accelerates the degradation rate of the magnesium alloy, affects its mechanical properties such as strength and toughness, and causes the material to be unable to maintain sufficient stability during service. With the acceleration of degradation, the material's bearing capacity gradually decreases, and may not meet the requirements for mechanical properties of implants in clinical applications. Therefore, a magnesium alloy wire that can be differentially degraded and a preparation method are proposed to solve the above problems. Summary of the invention
[0004] The object of the present invention is to provide a magnesium alloy wire capable of differential degradation and a preparation method thereof, so as to solve the problems raised in the above-mentioned background technology.
[0005] In order to solve the above technical problems, the present invention provides the following technical solutions: a magnesium alloy wire capable of differential degradation, the magnesium alloy wire being made of a Mg-Zn-Ca rare earth magnesium alloy, and comprising the following components: Zn in an amount of 1.0-3.0 parts by weight;
[0006] 0.5-2.0 parts by weight of Ca;
[0007] Including but not limited to rare earth elements such as Gd, Y, Na, etc. with a total content of 0.5-3.0 parts by weight;
[0008] The balance is Mg and unavoidable impurities;
[0009] By adding different types and contents of alloying elements, adjusting the composition of magnesium alloys, changing the corrosion properties of magnesium alloys, and thus achieving differentiated degradation, the corrosion resistance of magnesium alloys can be improved, and the degradation rate of magnesium alloys in specific environments can be slowed down, or other alloying elements can be used to accelerate the corrosion of magnesium alloys and achieve faster degradation;
[0010] By controlling the microstructure of magnesium alloy wire, such as grain size and texture, its degradation behavior can be affected. The corrosion resistance of magnesium alloy can be improved by refining the grains, while the specific texture may affect the directionality and rate of corrosion.
[0011] By surface treatment of magnesium alloy wire, including chemical conversion film and coating, the chemical properties and physical structure of its surface are changed, thereby adjusting the degradation rate;
[0012] Some coatings can act as a barrier to slow down the corrosion of magnesium alloys, or other bioactive coatings can promote cell growth and tissue repair while controlling the degradation rate;
[0013] The performance of magnesium alloy wire is affected by different processing techniques, thereby affecting its degradation behavior. By optimizing the processing parameters, including drawing speed and annealing temperature, the microstructure and properties of magnesium alloy wire are improved to achieve differentiated degradation.
[0014] A method for preparing a magnesium alloy wire capable of differential degradation, S1: firstly, Mg, Zn, Ca, rare earth elements and necessary additives in a predetermined ratio are placed in a resistance furnace for smelting, and stirred during the smelting process;
[0015] S2: After smelting is completed, the molten metal is poured into a mold and cooled to obtain a magnesium alloy ingot;
[0016] S3: the magnesium alloy ingot is then preheated;
[0017] S4: then, under the control of an external field such as a magnetic field, the preheated magnesium alloy ingot is placed in an extruder for extrusion deformation, and heat treatment is immediately performed after the extrusion deformation is completed;
[0018] S5: then placing the heat-treated magnesium alloy ingot in an aging furnace for aging treatment under the control of an external field such as a magnetic field;
[0019] S6: Finally, under the control of multi-physical fields, the magnesium alloy ingot after aging treatment is drawn into wire form by a wire drawing machine.
[0020] Preferably, Mg, Zn, Ca, rare earth elements and necessary additives in a predetermined ratio are placed in a resistance furnace, heated to 700-750° C., and kept warm for 2-4 hours to ensure that the alloy elements are completely melted.
[0021] Preferably, electromagnetic stirring is used during the smelting process at a stirring speed of 300-500 r / min to promote uniform distribution of alloy elements.
[0022] Preferably, the magnesium alloy ingot is heated to 400-500° C. and kept warm for 1-2 hours to achieve a preheating effect.
[0023] Preferably, during the extrusion molding process, it is necessary to carry out under a constant magnetic field of 0.5-1.5 Tesla, with an extrusion ratio of 4:1-10:1 and an extrusion speed of 1-5 mm / s.
[0024] Preferably, heat treatment is performed immediately after extrusion molding, the heat treatment temperature is 350-400° C., and the heat is kept for 2-4 hours to enhance the mechanical properties of the material and the distribution of the precipitated phase.
[0025] Preferably, the aging treatment is carried out in a weak magnetic field of 0.1-0.5 Tesla, the aging temperature is 200-250° C., and the temperature is kept at 8-24 hours.
[0026] Preferably, during the wire drawing process, a weak magnetic field of 0.1-0.3 Tesla is applied in combination with ultrasonic vibration, and the frequency of the ultrasonic wave is 20-40 KHz.
[0027] Preferably, during the wire drawing process, the wire drawing speed is controlled at 10-30 m / min, and the drawing passes are adjusted according to the required wire diameter until the target diameter is reached.
[0028] Compared with the prior art, the beneficial effects achieved by the present invention are:
[0029] Based on the high-strength and tough biodegradable magnesium alloy of Mg-Zn-Ca-rare earth, the present invention adds external field regulation such as a magnetic field during the aging treatment and drawing process to change the composition of the magnesium alloy wire and the distribution of the precipitated phase, thereby achieving differentiated degradation. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 A flow chart for the overall preparation of the present invention;
[0031] Figure 2 This is a smelting and casting flow chart of the present invention;
[0032] Figure 3 This is a flow chart of the extrusion deformation heat treatment of the present invention;
[0033] Figure 4 This is a flow chart of the aging treatment of the present invention;
[0034] Figure 5 This is a flow chart of the wire drawing process of the present invention. DETAILED DESCRIPTION
[0035] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0036] The present invention provides the following technical solutions:
[0037] Embodiment 1
[0038] A magnesium alloy wire capable of differential degradation and a preparation method thereof, wherein the magnesium alloy wire is made of a Mg-Zn-Ca rare earth magnesium alloy and comprises the following components: Zn in an amount of 1.0-3.0 parts by weight;
[0039] 0.5-2.0 parts by weight of Ca;
[0040] Including but not limited to rare earth elements such as Gd, Y, Na, etc. with a total content of 0.5-3.0 parts by weight;
[0041] The balance is Mg and unavoidable impurities;
[0042] By adding different types and contents of alloying elements, adjusting the composition of magnesium alloys, changing the corrosion properties of magnesium alloys, and thus achieving differentiated degradation, the corrosion resistance of magnesium alloys can be improved, and the degradation rate of magnesium alloys in specific environments can be slowed down, or other alloying elements can be used to accelerate the corrosion of magnesium alloys and achieve faster degradation;
[0043] By controlling the microstructure of magnesium alloy wire, such as grain size and texture, its degradation behavior can be affected. The corrosion resistance of magnesium alloy can be improved by refining the grains, while the specific texture may affect the directionality and rate of corrosion.
[0044] By surface treatment of magnesium alloy wire, including chemical conversion film and coating, the chemical properties and physical structure of its surface are changed, thereby adjusting the degradation rate;
[0045] Some coatings can act as a barrier to slow down the corrosion of magnesium alloys, or other bioactive coatings can promote cell growth and tissue repair while controlling the degradation rate;
[0046] The performance of magnesium alloy wire is affected by different processing techniques, thereby affecting its degradation behavior. By optimizing the processing parameters, including drawing speed and annealing temperature, the microstructure and properties of magnesium alloy wire are improved to achieve differentiated degradation.
[0047] Embodiment 2
[0048] A method for preparing a magnesium alloy wire capable of differential degradation:
[0049] S1: First, Mg, Zn, Ca, rare earth elements and necessary additives in a predetermined ratio are placed in a resistance furnace for smelting, and stirred during the smelting process;
[0050] S2: After smelting is completed, the molten metal is poured into a mold and cooled to obtain a magnesium alloy ingot;
[0051] S3: the magnesium alloy ingot is then preheated;
[0052] S4: then, under the control of an external field such as a magnetic field, the preheated magnesium alloy ingot is placed in an extruder for extrusion deformation, and heat treatment is immediately performed after the extrusion deformation is completed;
[0053] S5: then placing the heat-treated magnesium alloy ingot in an aging furnace for aging treatment under the control of an external field such as a magnetic field;
[0054] S6: Finally, under the control of multi-physical fields, the magnesium alloy ingot after aging treatment is drawn into wire form by a wire drawing machine.
[0055] Specifically, Mg, Zn, Ca, rare earth elements and necessary additives in a predetermined ratio are placed in a resistance furnace, heated to 700-750° C., and kept warm for 2-4 hours to ensure that the alloy elements are completely melted.
[0056] Through the above technical scheme, the additive can be Zr, which can form a large number of fine crystal nuclei during the reaction process of the magnesium alloy, thereby refining the grains and improving the strength and toughness of the magnesium alloy; the additive can also be Mn, which can also play a role in refining the grains during the reaction process of the magnesium alloy, and at the same time improve the corrosion resistance and creep resistance of the magnesium alloy; during the entire heating and melting process, in order to prevent the severe oxidation of magnesium, inert gases such as argon need to be continuously introduced into the furnace to remove oxygen and other harmful gases in the furnace and protect the magnesium alloy from oxidation and pollution.
[0057] Specifically, electromagnetic stirring is used during the smelting process at a stirring speed of 300-500 r / min to promote uniform distribution of alloy elements.
[0058] Through the above technical solution, electromagnetic stirring uses the principle of electromagnetic induction to generate a rotating magnetic field in the smelting furnace. When this rotating magnetic field acts on the molten metal in the molten pool, an induced current is generated in the molten metal. These induced currents interact with the rotating magnetic field to generate Lorentz force, thereby driving the molten metal to form a rotating flow in the molten pool; for magnesium alloys, within the stirring speed range of 300-500r / min, it can not only ensure that the magnesium alloy liquid forms an effective rotating flow in the molten pool and promote the uniform distribution of magnesium alloy elements, but also avoid excessive fluctuations on the surface of the molten pool and reduce the occurrence of oxidation and air inhalation.
[0059] Specifically, the magnesium alloy ingot is heated to 400-500° C. and kept warm for 1-2 hours to achieve a preheating effect.
[0060] Through the above technical scheme, internal stress may be generated in the magnesium alloy ingot during the solidification process. Preheating can partially eliminate or alleviate these stresses and reduce the risk of cracking caused by stress concentration. Appropriate preheating can soften the structure of the magnesium alloy ingot to a certain extent, improve the plasticity of the material, and facilitate subsequent plastic deformation processing. Through insulation, the overall temperature of the ingot can be ensured to be uniform, providing stable initial conditions for subsequent extrusion molding processing and avoiding processing defects caused by uneven temperature.
[0061] Specifically, during the extrusion molding process, it is necessary to carry out the process under a constant magnetic field of 0.5-1.5 Tesla, with an extrusion ratio of 4:1-10:1 and an extrusion speed of 1-5 mm / s.
[0062] Through the above technical solution, the magnetic field can promote the grain refinement, increase of dislocation density and phase change of the magnesium alloy ingot, which helps to improve the strength and toughness of the magnesium alloy ingot.
[0063] Specifically, heat treatment is performed immediately after extrusion molding, and the heat treatment temperature is 350-400° C., and then kept warm for 2-4 hours to enhance the mechanical properties of the material and the distribution of the precipitated phase.
[0064] Through the above technical scheme, heat treatment can improve the internal structure of magnesium alloy ingots, such as refining grains, eliminating internal stress and promoting the formation of precipitation phases, thereby improving the mechanical properties of magnesium alloy ingots such as tensile strength, yield strength, hardness and toughness.
[0065] Specifically, during the aging treatment process, it is necessary to carry out the treatment under a weak magnetic field of 0.1-0.5 Tesla, with an aging temperature of 200-250°C and keep the temperature for 8-24 hours.
[0066] Through the above technical scheme, the weak magnetic field can affect the formation and distribution of the precipitation phase inside the magnesium alloy during the aging process. Through the action of the weak magnetic field, the precipitated phase can be more evenly distributed in the matrix. Combined with appropriate aging temperature and holding time, the performance of the magnesium alloy ingot can be further optimized, and its mechanical properties, corrosion resistance and differentiated degradation performance can be improved.
[0067] Specifically, during the wire drawing process, a weak magnetic field of 0.1-0.3 Tesla is applied and combined with ultrasonic vibration, and the frequency of the ultrasonic wave is 20-40KHz.
[0068] Through the above technical scheme, the weak magnetic field can improve the fluidity of the magnesium alloy ingot, making the wire drawing process smoother; reduce the stress concentration generated by the magnesium alloy ingot during the wire drawing process, and reduce the risk of cracks and fractures; ultrasonic vibration can significantly reduce the drawing force during the wire drawing process, so that the magnesium alloy ingot can pass through the mold more easily, reducing mold wear and energy consumption; ultrasonic vibration can also cause grain refinement inside the magnesium alloy ingot, thereby improving the mechanical properties and surface quality of the magnesium alloy ingot.
[0069] Specifically, during the wire drawing process, the wire drawing speed is controlled at 10-30 m / min, and the drawing passes are adjusted according to the required wire diameter until the target diameter is reached.
[0070] Through the above technical solution, wire drawing is carried out under the control of multiple physical fields, which can ensure that the precipitated phase of the magnesium alloy wire is evenly distributed during the stretching process and achieve differentiated degradation.
[0071] Although the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit thereof, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A magnesium alloy wire capable of differential degradation, Features: The magnesium alloy wire is made of Mg-Zn-Ca rare earth magnesium alloy and includes the following components: Zn in an amount of 1.0-3.0 parts by weight; Ca in an amount of 0.5-2.0 parts by weight; Including but not limited to rare earth elements such as Gd, Y, Na, etc. with a total content of 0.5-3.0 parts by weight; The balance is Mg and unavoidable impurities; By adding different types and contents of alloying elements, adjusting the composition of magnesium alloys, changing the corrosion properties of magnesium alloys, and thus achieving differentiated degradation, the corrosion resistance of magnesium alloys can be improved, and the degradation rate of magnesium alloys in specific environments can be slowed down, or other alloying elements can be used to accelerate the corrosion of magnesium alloys and achieve faster degradation; By controlling the microstructure of magnesium alloy wire, such as grain size and texture, its degradation behavior can be affected. The corrosion resistance of magnesium alloy can be improved by refining the grains, while the specific texture may affect the directionality and rate of corrosion. By surface treatment of magnesium alloy wire, including chemical conversion film and coating, the chemical properties and physical structure of its surface are changed, thereby adjusting the degradation rate; Some coatings can act as a barrier to slow down the corrosion of magnesium alloys, or other bioactive coatings can promote cell growth and tissue repair while controlling the degradation rate; The performance of magnesium alloy wire is affected by different processing techniques, thereby affecting its degradation behavior. By optimizing the processing parameters, including drawing speed and annealing temperature, the microstructure and properties of magnesium alloy wire are improved to achieve differentiated degradation.
2. A method for preparing a magnesium alloy wire capable of differential degradation, Features: S1: First, Mg, Zn, Ca, rare earth elements and necessary additives in a predetermined ratio are placed in a resistance furnace for smelting, and stirred during the smelting process; S2: After smelting is completed, the molten metal is poured into a mold and cooled to obtain a magnesium alloy ingot; S3: the magnesium alloy ingot is then preheated; S4: then, under the control of an external field such as a magnetic field, the preheated magnesium alloy ingot is placed in an extruder for extrusion deformation, and heat treatment is immediately performed after the extrusion deformation is completed; S5: then placing the heat-treated magnesium alloy ingot in an aging furnace for aging treatment under the control of an external field such as a magnetic field; S6: Finally, under the control of multi-physical fields, the magnesium alloy ingot after aging treatment is drawn into wire form by a wire drawing machine.
3. A method for preparing a differentially degradable magnesium alloy wire according to claim 2, Features: Mg, Zn, Ca, rare earth elements and necessary additives in a predetermined ratio are placed in a resistance furnace, heated to 700-750°C, and kept warm for 2-4 hours to ensure that the alloy elements are completely melted.
4. The method for preparing a differentially degradable magnesium alloy wire according to claim 2, Features: Electromagnetic stirring is used during the smelting process with a stirring speed of 300-500r / min to promote the uniform distribution of alloy elements.
5. The method for preparing a differentially degradable magnesium alloy wire according to claim 2, Features: Heat the magnesium alloy ingot to 400-500°C and keep it warm for 1-2 hours to achieve the preheating effect.
6. The method for preparing a differentially degradable magnesium alloy wire according to claim 2, Features: During the extrusion molding process, it is necessary to carry out the process under a constant magnetic field of 0.5-1.5 Tesla, with an extrusion ratio of 4:1-10:1 and an extrusion speed of 1-5 mm / s.
7. The method for preparing a differentially degradable magnesium alloy wire according to claim 2, Features: After extrusion molding, heat treatment is immediately carried out at a temperature of 350-400°C and then kept warm for 2-4 hours to enhance the mechanical properties of the material and the distribution of the precipitated phase.
8. The method for preparing a differentially degradable magnesium alloy wire according to claim 2, Features: During the aging treatment process, it is necessary to carry out the treatment under a weak magnetic field of 0.1-0.5 Tesla, with an aging temperature of 200-250°C and keep warm for 8-24 hours.
9. The method for preparing a differentially degradable magnesium alloy wire according to claim 2, Features: During the wire drawing process, a weak magnetic field of 0.1-0.3 Tesla is applied, combined with ultrasonic vibration, and the frequency of the ultrasonic wave is 20-40KHz.
10. The method for preparing a differentially degradable magnesium alloy wire according to claim 2, Features: During the wire drawing process, the wire drawing speed is controlled at 10-30m / min, and the drawing passes are adjusted according to the required wire diameter until the target diameter is reached.