Combined type rapid annealing device and method

By combining induction heating and dielectric heating mechanisms during the annealing process of silicon carbide wafers, the problems of slow heating speed and uneven heating in traditional annealing technology are solved, and the rapid and uniform annealing effect is achieved, and the equipment cost is reduced.

CN118737877APending Publication Date: 2024-10-01FINESSE TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310326736.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-03-30
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

Traditional annealing technology heats the silicon carbide wafer too slowly, resulting in an increase in surface roughness and inability to fully activate the implanted ions. In addition, microwave annealing has problems of uneven heating and high equipment costs.

Method used

A composite rapid annealing device is adopted, combining an induction heating mechanism and a dielectric heating mechanism, and heating is carried out simultaneously or alternately by induction magnetic field and electric field, and intermediate frequency and radio frequency electromagnetic waves are used to achieve rapid and uniform heating.

Benefits of technology

Fast and even heating of silicon carbide wafers is achieved, high heating rates are maintained, equipment costs are reduced, and diffusion pollution is prevented.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118737877A_ABST
    Figure CN118737877A_ABST
Patent Text Reader

Abstract

The invention relates to a combined type rapid annealing device and method, which comprises two electrodes, a heating cavity, an induction heating device and a dielectric heating device, and at least one object to be processed is placed between the two electrodes and is positioned in a cavity of the heating cavity. In the combined type rapid annealing method, an induction heating device of the combined type rapid annealing device carries out an induction heating step on a to-be-processed object. When the electric conductivity of the to-be-processed object is reduced due to temperature rise, the two electrodes can heat the to-be-processed object, and the dielectric heating device can also carry out a dielectric heating step on the to-be-processed object, so that the to-be-processed object can maintain a certain heating rate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to an annealing device and method, and in particular to a composite rapid annealing device and method. Background Art

[0002] Silicon carbide (SiC) has a wide bandgap, high breakdown electric field, high thermal conductivity and excellent chemical inertness, making it an important semiconductor material for manufacturing high-temperature, high-power and high-frequency devices. Ion implantation is an indispensable technology for manufacturing SiC semiconductor components. At the same time, annealing is a necessary step after ion implantation to remove lattice damage and activate implanted ions. For silicon carbide, annealing after ion implantation is required at a temperature greater than 1,500°C to achieve the process effect.

[0003] Conventional annealing is usually performed in a ceramic furnace with resistance heating or low-frequency induction heating. However, the heating / cooling rate of the ceramic furnace is slow (20°C / min), which makes it difficult to anneal silicon carbide at temperatures above 1,500°C. Because if silicon carbide is exposed to temperatures above 1,400°C for a long time, the components on the surface of the substrate will sublimate and redeposit (commonly known as step bunching), causing the surface roughness of the silicon carbide wafer to increase, which limits the maximum annealing temperature. This limitation on the annealing temperature may result in an inability to fully activate the implanted ions, resulting in higher contact and channel region resistance.

[0004] Therefore, in order to avoid the problem of surface degradation of silicon carbide wafers caused by slow heating speed in traditional annealing technology, the development of rapid annealing technology becomes the key. Although halogen lamp and laser technology can achieve rapid thermal processing, there are still some problems, such as the maximum achievable annealing temperature, surface melting, high residual defect density and redistribution of implants.

[0005] On the other hand, silicon carbide can effectively absorb microwave energy. With a properly designed annealing system, microwaves can provide very fast heating and cooling rates for silicon carbide wafers and good control of annealing time. Microwaves have the characteristics of selective heating, because microwaves are only absorbed by semiconductor wafers and not by the surrounding environment, and the annealing heating rate is very fast. At the same time, during the annealing process, the temperature of the environment around the silicon carbide wafer is limited, and the cooling rate of the silicon carbide wafer can be very high when the microwave source is turned off. Compared with traditional annealing technology, the heating results of small-area silicon carbide wafers using microwaves for silicon carbide annealing show that the heating rate can exceed 600℃ / s and the temperature can be as high as 2,000℃.

[0006] However, microwaves have a short wavelength, and the energy distribution in the heating reaction chamber is uneven, which causes the problem of uneven heating of the silicon carbide wafer. Especially when the area of ​​the silicon carbide wafer increases, the volume of the heating reaction chamber increases, and the problem of uneven heating during annealing heating will become more serious. At the same time, the required microwave energy is also greatly increased, making the equipment more expensive. Summary of the invention

[0007] In view of this, one or more objects of the present invention is to provide a composite rapid annealing device and method to solve the problems of the above-mentioned conventional technology.

[0008] When the silicon carbide wafer is heated by electromagnetic waves that generate an alternating magnetic field, eddy currents can be generated to provide an induction heating (or induction heating) effect. However, when the temperature exceeds 500 degrees K, the conductivity of the silicon carbide wafer will drop rapidly, causing its resistivity to increase. Moreover, since electromagnetic waves with an alternating electric field can also heat the silicon carbide wafer by generating a dielectric heating mechanism (or dielectric heating mechanism), the dielectric loss tangent of the silicon carbide wafer will increase as the temperature rises. When the temperature rises to more than about 1,000 degrees Celsius, the dielectric loss tangent will increase rapidly and significantly. Therefore, the present invention proposes a composite heating mechanism that combines an induction heating mechanism and a dielectric heating mechanism to heat a workpiece, such as a silicon carbide wafer.

[0009] To achieve the above-mentioned purpose, the present invention provides a composite rapid annealing device, comprising: two electrodes, wherein at least one object to be processed is placed between the two electrodes; a heating chamber having a chamber for at least accommodating the object to be processed; an induction heating device for performing an induction heating step on the object to be processed in the heating chamber, wherein the induction heating device generates an eddy current in the object to be processed by generating an induced magnetic field, thereby heating the object to be processed; and a dielectric heating device for performing a dielectric heating step on the object to be processed in the heating chamber, wherein the dielectric heating device generates an electric field on the two electrodes, thereby heating the object to be processed between the two electrodes.

[0010] The induction heating device performs the induction heating step on the object to be processed and the two electrodes in the heating chamber, so as to heat the object to be processed and the two electrodes.

[0011] The induction heating device and the dielectric heating device respectively perform the induction heating step and the dielectric heating step simultaneously, sequentially, intermittently or alternately.

[0012] The composite rapid annealing device of the present invention further comprises a Faraday shielding layer disposed on the heating chamber, and the induction heating device penetrates through the Faraday shielding layer to form the induced magnetic field in the chamber of the heating chamber.

[0013] The Faraday shielding layer is a metal tube with a plurality of openings.

[0014] The metal tube has a reflective surface to reduce the radiation heat loss of the heating chamber.

[0015] Wherein, the reflective surface of the metal tube is also covered with a reflective layer.

[0016] There is at least one barrier layer between the two electrodes and the object to be processed.

[0017] There are a plurality of objects to be processed, and at least one barrier layer is disposed between the objects to be processed.

[0018] Wherein, one of the barrier layer and the object to be processed is a polycrystalline structure, and the other of the barrier layer and the object to be processed is a single crystal structure.

[0019] The induction heating device and the dielectric heating device perform the induction heating step and the dielectric heating step on the object to be processed and the barrier layer, so as to heat the object to be processed and the barrier layer.

[0020] The object to be processed is a wafer.

[0021] The object to be processed is selected from a group consisting of a conductive object and a non-conductive object.

[0022] Wherein, the material of the two electrodes is graphite.

[0023] The induction heating device comprises an induction coil wound around the heating chamber, wherein the induction heating device applies a first alternating electromagnetic signal with a first predetermined frequency to the induction coil to generate the induced magnetic field on the object to be processed and the two electrodes.

[0024] The first predetermined frequency ranges from 50 kHz to 200 kHz.

[0025] The dielectric heating device applies a second alternating electromagnetic signal with a second predetermined frequency to generate the electric field on the two electrodes located on both sides of the object to be processed.

[0026] The second predetermined frequency ranges from 10 MHz to 900 MHz.

[0027] The dielectric heating device includes a radio frequency power supply and a matcher. The radio frequency power supply provides the second alternating electromagnetic signal with the second predetermined frequency. The matcher is electrically connected between the radio frequency power supply and the two electrodes to reduce reflection of the second alternating electromagnetic signal.

[0028] The composite rapid annealing device of the present invention further comprises a gas input unit and a gas extraction unit respectively connected to the chamber of the heating chamber, so as to keep the chamber of the heating chamber at a predetermined pressure.

[0029] Wherein, the predetermined pressure of the heating chamber ranges from 0.1 atm to 10 atm.

[0030] Among them, the composite rapid annealing device of the present invention also includes a measurement and control system, including a pressure detection unit and a controller. The pressure detection unit is used to measure the gas pressure of the chamber of the heating chamber, and the controller controls the operation of the gas input unit and / or the exhaust unit accordingly according to the value of the gas pressure.

[0031] The measurement and control system further comprises a pyrometer for measuring the temperature of the chamber of the heating chamber.

[0032] The heating chamber comprises a chamber body, an upper cover and a lower cover, and the chamber body is connected between the upper cover and the lower cover, so as to form the chamber between the chamber body, the upper cover and the lower cover.

[0033] The heating chamber is made of a quartz tube or a ceramic tube.

[0034] To achieve the aforementioned objective, the present invention further proposes a composite rapid annealing method, comprising: performing an induction heating step on at least one object to be processed by an induction heating device, wherein the induction heating device generates an eddy current in the object to be processed by generating an induced magnetic field, thereby heating the object to be processed; and performing a dielectric heating step on the object to be processed by a dielectric heating device, wherein the dielectric heating device generates an electric field to heat the object to be processed.

[0035] The object to be processed is carried between two electrodes, the induction heating device performs the induction heating step on the object to be processed and the two electrodes to heat the object to be processed and the two electrodes, and the dielectric heating device generates the electric field on the two electrodes to heat the object to be processed.

[0036] As described above, the composite rapid annealing device and method according to the present invention has one or more advantages or technical effects:

[0037] (1) By combining the induction heating mechanism and the dielectric heating mechanism, it can be used to heat both conductive and non-conductive objects at the same time. For example, the temperature of a silicon carbide wafer can be increased by the induction heating mechanism, and when the conductivity of the silicon carbide wafer decreases due to the increase in temperature, the temperature of the silicon carbide wafer can be increased by the dielectric heating mechanism, so that the wafer maintains a certain heating rate.

[0038] (2) The induction heating mechanism can also increase the temperature of the electrode. When the conductivity of the SiC wafer decreases due to the increase in temperature, the SiC wafer can be continuously heated by the heating electrode, so that the SiC wafer maintains a certain heating rate.

[0039] (3) The electrode can be used as a bearing base and a heating base.

[0040] (4) The heating chamber has a metal tube that can serve as a reflective layer and a Faraday shielding layer, which can not only reduce the radiation heat dissipation loss of the heating chamber, but also allow the AC magnetic field to enter the heating chamber to generate eddy currents in the wafer.

[0041] (5) A barrier layer is located between the electrode and the wafer or between the wafers to prevent diffusion contamination. The barrier layer can also be used as a supporting base and a heating base.

[0042] In order to enable you to have a further understanding and recognition of the technical features and technical effects of the present invention, preferred embodiments and detailed descriptions are provided as follows. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] Figure 1 It is a schematic cross-sectional structure diagram of one embodiment of the composite rapid annealing device of the present invention.

[0044] Figure 2 It is a schematic diagram of the three-dimensional structure of the Faraday shielding layer of the composite rapid annealing device of the present invention.

[0045] Figure 3 FIG. 1 is a schematic diagram of the operation of the dielectric heating mechanism of the composite rapid annealing device of the present invention, wherein Figure 3 (A), (B) and (C) respectively show the state of multiple wafers, single wafer and no barrier layer used.

[0046] Figure 4 It is a schematic diagram of the operation of the induction heating mechanism of the composite rapid annealing device of the present invention.

[0047] Figure 5 It is a schematic flow chart of the composite heating procedure of the composite rapid annealing method of the present invention.

[0048] Figure 6 It is a schematic cross-sectional structure diagram of another embodiment of the composite rapid annealing device of the present invention.

[0049] Description of reference numerals:

[0050] 10: Composite rapid annealing device

[0051] 20: Electrode

[0052] 22: Wafer

[0053] 24: Barrier layer

[0054] 30: Heating chamber

[0055] 32: Chamber

[0056] 34: Cavity

[0057] 35: Metal layer

[0058] 36: Upper cover

[0059] 37: Insulation material layer

[0060] 38: Lower cover

[0061] 40: Induction heating device

[0062] 42: Inductor

[0063] 50: Dielectric heating device

[0064] 52: RF power supply

[0065] 54: Matcher

[0066] 60: Metal cylinder

[0067] 62: Reflection layer

[0068] 64: Opening

[0069] 66: Faraday Shield

[0070] 70: Measurement and control systems

[0071] 72: Gas input unit

[0072] 73: Intake pipe fittings

[0073] 74: Exhaust unit

[0074] 75: Exhaust pipe fittings

[0075] 76: Pressure detection unit

[0076] 78: Controller

[0077] 79: Pyrometer

[0078] AC: alternating current electromagnetic signal

[0079] Φ: Magnetic flux

[0080] I EC : Eddy current

[0081] S10, S20: Steps DETAILED DESCRIPTION

[0082] In order to facilitate understanding of the technical features, contents and advantages of the present invention and the effects that can be achieved, the present invention is hereby described in detail in the form of embodiments in conjunction with the drawings. The drawings used therein are only for illustration and auxiliary description purposes, and may not be the actual proportions and precise configurations after the implementation of the present invention. Therefore, the proportions and configurations of the attached drawings should not be interpreted or limited to the scope of rights of the present invention in actual implementation. In addition, for ease of understanding, the same elements in the following embodiments are described with the same symbols.

[0083] In addition, the words used throughout the specification and claims generally have the ordinary meaning of each word used in this field, in the content disclosed herein, and in the specific content, unless otherwise noted. Certain words used to describe the present invention will be discussed below or elsewhere in this specification to provide additional guidance to those skilled in the art in the description of the present invention.

[0084] The use of “first”, “second”, “third”, etc. in this document does not specifically refer to the order or sequence, nor is it used to limit the present invention. It is only used to distinguish components or operations described with the same technical terms.

[0085] Secondly, the words "include", "including", "have", "contain" and the like used in this article are open terms, which mean including but not limited to.

[0086] The present invention is a composite rapid annealing device and method. Taking the object to be processed as a wafer (such as a silicon carbide wafer) as an example, the physical property of silicon carbide is that during the heating process and other processing procedures, the conductivity drops rapidly at high temperature, but the dielectric absorption rate of electromagnetic waves rises rapidly. In addition, other wafer materials also have similar or similar characteristics. Therefore, the present invention adopts a composite heating mechanism, including the use of a medium frequency induction heating (Induction Heating) mechanism to quickly increase the temperature of the wafer. For a doped wafer, when its temperature rises rapidly to a value, its conductivity drops rapidly, and its conductivity will change differently with the temperature change of the wafer due to different doping concentrations or types. Therefore, the present invention adopts a composite heating mechanism, and also includes using a radio frequency power source to perform a dielectric heating (Dielectric Heating) mechanism on a wafer whose conductivity drops rapidly, so as to achieve the effect of rapid wafer annealing.

[0087] See also Figures 1 to 5 , Figure 1 It is a schematic cross-sectional structure diagram of one embodiment of the composite rapid annealing device of the present invention. Figure 2 It is a schematic diagram of the three-dimensional structure of the Faraday shielding layer of the composite rapid annealing device of the present invention. Figure 3 It is a schematic diagram of the operation of the dielectric heating mechanism of the composite rapid annealing device of the present invention. Figure 4 It is a schematic diagram of the operation of the induction heating mechanism of the composite rapid annealing device of the present invention. Figure 5 FIG. 1 is a flow chart of a composite heating process of the composite rapid annealing method of the present invention. The composite rapid annealing device 10 of the present invention comprises two electrodes 20, a heating chamber 30, an induction heating device 40 and a dielectric heating device 50, such as Figure 1 As shown. The object to be processed is placed between two electrodes 20. For example, the electrode 20 is used to carry the object to be processed, and the object to be processed is, for example, a material whose conductivity decreases as the temperature increases, or a material whose conductivity changes as the temperature changes, such as a wafer 22. The object to be processed may be, for example, a silicon carbide wafer 22 or a wafer 22 of other materials (such as Si, SiGe, Ge, GaAs, GaN or InP), and may be a wafer at any stage in any semiconductor manufacturing process, and regardless of whether the object to be processed has doped substances or what substances are doped, it belongs to the scope of protection requested by the present invention. However, the present invention is not limited to this, and the object to be processed may also be, for example, other materials or objects, such as an ingot or any other object that needs to be heated. The material of the electrode 20 is, for example, graphite, whereby when the wafer 22 is placed between the two electrodes 20, the electrode 20 can be used as a supporting base for the wafer 22, and at the same time as a heatable electrode (or heating base). Therefore, the electrode 20 may also be made of other materials with similar or identical effects. Although the present invention uses the workpiece whose conductivity decreases with increasing temperature or changes with temperature as an illustrative example, it is not intended to limit the scope of the present invention. In other words, any object, regardless of whether its conductivity (or conductivity) changes with temperature, as long as it can be heated using the composite rapid annealing device 10 of the present invention, falls within the scope of the present invention.

[0088] The composite rapid annealing device 10 of the present invention performs a composite heating process on the wafer 22 in the heating chamber 30. The composite heating process includes using an induction heating mechanism (such as Figure 4 ) and dielectric heating mechanisms (as shown Figure 3 The heating chamber 30 has a chamber 32 for accommodating the two electrodes 20 and the wafer 22. In the combined heating process, the induction heating device 40 of the combined rapid annealing device of the present invention performs an induction heating step (such as Figure 5The induction heating device 40 generates an alternating magnetic field (Magnetic Field) by a first alternating electromagnetic signal (AC), and generates an induced magnetic field (Induced Magnetic Field) with a magnetic flux (Magnetic Flux, Φ) variation to generate an eddy current (Eddy Current, I EC ) in the wafer 22 and the two electrodes 20 (such as Figure 4 As shown), the wafer 22 and the two electrodes 20 are heated.

[0089] In the induction heating mechanism, the heating energy generated per unit volume of the object to be processed can be expressed by the following equation: Among them, σ m is the conductivity of the material to be processed, ω = 2πf, f = electromagnetic wave frequency, B is the strength of the alternating magnetic field. For doped silicon carbide wafers, the conductivity (i.e., 1 / resistivity) will increase with the increase of heating temperature, but when the temperature exceeds 500 degrees K, the conductivity will drop rapidly (i.e., the resistivity will increase).

[0090] In the combined heating process of the combined rapid annealing device 10 of the present invention, the dielectric heating device 50 performs a dielectric heating step (such as Figure 5 The dielectric heating device 50 generates an electric field on the two electrodes 20 to heat the wafer 22 between the two electrodes 20. The number of wafers 22 can be one (eg Figure 3 (B) and (C)) or multiple (such as Figure 3 (A)). In addition, at least one barrier layer 24 (such as Figure 3 (A) and (B)), or omitting the barrier layer 24 (as shown in Figure 3(C)), and a barrier layer 24 may be selectively provided between two adjacent wafers 22. The purpose of the barrier layer 24 is to prevent contamination such as cross-border diffusion of doping components between the wafers 22 or between the wafer 22 and the electrode 20 due to temperature increase. The barrier layer 24 may also be used as a supporting base and a heating base for the wafer 22. The barrier layer 24 may also be selectively made of a material that can be heated by the induction heating device 40 and the dielectric heating device 50. Thus, the induction heating device 40 and the dielectric heating device 50 may, for example, simultaneously perform an induction heating step (S10) and a dielectric heating step (S20) on the wafer 22 and the barrier layer 24 to heat the wafer 22 and the barrier layer 24. For example, if the material of the wafer 22 is a single crystal structure (e.g., single crystal silicon carbide), the component of the barrier 24 is, for example, a polycrystalline structure (e.g., polycrystalline silicon carbide), and vice versa. That is, the wafer 22 and the barrier 24 are, for example, made of different materials. However, the present invention is not limited thereto, and as long as the barrier layer 24 can exert a barrier effect, such as a diffusion barrier effect, no matter what material it is made of or whether it can be heated, it should fall within the scope of protection requested by the present invention. In order to facilitate the description of the technical means and technical effects of the present invention, the present invention takes the object to be processed as a wafer 22 (such as a silicon carbide wafer) and the electrode 20 as an example of a graphite electrode, but any substance, object or structure as long as it can be heated by the composite rapid annealing device of the present invention falls within the scope of protection requested by the present invention. In the composite heating process, the induction heating device 40 and the dielectric heating device 50 are not limited to performing the induction heating step (step S10) and the dielectric heating step (step S20) simultaneously, sequentially, intermittently or alternately.

[0091] The heating mechanism of the composite rapid annealing device of the present invention adopts the medium frequency induction heating mechanism. The reason is that there are two aspects to consider when using the heating power supply of high and low frequency electromagnetic fields. The first aspect is that the efficiency of dielectric heating is more effective in the effect of high frequency electromagnetic waves. The second aspect is to consider the penetration depth of electromagnetic waves. In addition to being the base of the silicon carbide wafer 22, the graphite electrode 20 is also a heating electrode. It is mainly used to use its penetration depth of electromagnetic waves less than 400μm when it is greater than 10MHz. It can be used as an electrode material to generate an AC electric field between the upper and lower electrodes 20 without attenuating too much. For low frequency electromagnetic waves, its penetration depth is greater than the entire heating base composed of the graphite electrode 20 and the silicon carbide wafer 22. In other words, the first AC electromagnetic signal of the medium frequency can effectively heat the whole. In particular, graphite can withstand high temperatures and its induction heating mechanism is highly efficient, so the temperature of the heating base composed of the graphite electrode 20 and the silicon carbide wafer 22 can be quickly increased. However, although the present invention uses a medium frequency electromagnetic field as an example, the scope of rights of the present invention is not limited thereto. Any frequency of electromagnetic field, as long as it can be applied to the present invention to generate inductive heating of the graphite electrode 20 and the silicon carbide wafer 22, falls within the scope of protection requested by the present invention.

[0092] For example, in the early stage of the heating reaction, the present invention can quickly increase the temperature of the graphite electrode 20 and the silicon carbide wafer 22 by the induction heating mechanism. When the temperature of the silicon carbide wafer 22 is higher than 500 degrees K, for example, the conductivity of silicon carbide decreases and the heating effect becomes worse, but the graphite electrode 20 is still heated by induction, and its temperature can still maintain a certain heating rate. During the temperature rise process, the dielectric loss tangent of silicon carbide continues to increase, improving the efficiency of dielectric heating. When the temperature rises to about 1,000 degrees Celsius, the dielectric loss tangent increases significantly, so the effect of dielectric heating can be accelerated.

[0093] In detail, the induction heating device 40 includes, for example, an inductance coil 42 wound around the heating chamber 30. The induction heating device 40 generates an induced magnetic field on the wafer 22 and the two electrodes 20 by applying a first alternating electromagnetic signal of a first predetermined frequency to the inductance coil 42. The inductance coil 42 is driven by a medium frequency AC power source, and the first predetermined frequency ranges from about 50kHz to 200kHz, but is not limited thereto. In this embodiment, the heating chamber 30 may include, for example, a cavity 34, an upper cover 36 and a lower cover 38, and the cavity 34 is connected between the upper cover 36 and the lower cover 38, so as to form a chamber 32 between the cavity 34, the upper cover 36 and the lower cover 38. The inductance coil 42 is wound around the cavity 34 of the heating chamber 30. In order to perform the induction heating mechanism, the cavity 34 of the heating chamber 30 is made of, for example, quartz or ceramic. The radio frequency power source 52 of the dielectric heating device 50 applies a second alternating electromagnetic signal of a second predetermined frequency to the two electrodes 20 via the upper cover 36 and the lower cover 38. The upper cover 36 and the lower cover 38 are, for example, composed of a metal layer 35 and a heat insulating material layer 37. However, the present invention is not limited thereto. In other feasible aspects, the heating chamber 30 of the present invention may also be entirely composed of quartz, ceramic or other materials.

[0094] The present invention can selectively add a reflective design to the heating chamber 30 to increase the reflectivity of infrared light to minimize radiation loss. For example, the present invention can set a metal cylinder 60 outside the cavity 34 of the heating chamber 30, such as Figure 1 and Figure 2 As shown, the metal cylinder 60 is, for example, an optically polished metal cylinder, which can be used as a reflective surface and can be selectively coated with a reflective layer (e.g., gold) 62 to increase the reflectivity of infrared light, thereby reducing the radiation heat dissipation loss generated by the heating base composed of the graphite electrode 20 and the silicon carbide wafer 22 under extremely high temperature conditions. In addition, the present invention can also selectively add a plurality of openings 64 on the metal cylinder 60, and the openings 64 are, for example, longitudinal openings (e.g., long strips) and are distributed around the metal cylinder 60, whereby the metal cylinder 60 can be used as a Faraday shield layer 66 to facilitate the AC magnetic field generated by the induction heating device 40 to pass through the Faraday shield layer 66 and enter the chamber 32 of the heating chamber 30, so that the electrode 20 and the wafer 22 generate an eddy current I EC ,like Figure 4 shown.

[0095] The dielectric heating device 50 is a radio frequency dielectric heating device (or radio frequency heating device), such as Figure 1 and Figure 3As shown, a second AC electromagnetic signal having a second predetermined frequency is applied to generate an electric field between the two electrodes 20 located on both sides of the wafer 22, so as to perform a dielectric heating step on the wafer 22 in the heating chamber 30, thereby maintaining a certain heating rate of the wafer 22. For example, the dielectric heating device 50 includes a radio frequency power source 52, and optionally further includes a matcher 54, the radio frequency power source 52 provides the second AC electromagnetic signal of the second predetermined frequency. The radio frequency power source 52 is, for example, directly electrically connected to the two electrodes 20 or electrically connected to the two electrodes 20 via a wire (not shown). The matcher 54 is electrically connected between the radio frequency power source 52 and the two electrodes 20 to reduce the reflection of the second AC electromagnetic signal. That is, the matching circuit of the matcher 54 is specially designed to adjust the impedance of the heating chamber 30 to match the radio frequency power source 52 (e.g., RF / microwave power source) to reduce the reflection of electromagnetic waves (such as RF or microwave). The frequency of the RF power supply 52 is selected to be greater than 10 MHz. Considering the uniformity of the electromagnetic field distribution, the frequency used is less than 900 MHz. That is, the range of the second predetermined frequency is from 10 MHz to 900 MHz, but not limited thereto, for example, from 10 MHz to 400 MHz, and the output power is adjusted within the range of 1 kilowatt and above, which can be any numerical interval or upper and lower limit endpoints in the above frequency range and power range. The inductance L and capacitance C parameters in the matching circuit of the matcher 54 can change with the change of operating conditions to maintain good coupling conditions. The existing L and C components in the matching circuit of the matcher 54 can be electronically tuned, so there is no delay in the tuning response time, and a higher heating rate can be achieved. Impedance matching is essential for achieving rapid heating. The optimal design of the matching network varies depending on the application. Since those with ordinary knowledge in the technical field to which the present invention belongs should be able to understand how to implement the dielectric heating device 50 and how to use the corresponding matching circuit of the matcher 54 and the RF power supply 52 based on the disclosure of the present invention, it is not further described here.

[0096] Since the present invention has both an induction heating mechanism and a dielectric heating mechanism, it can perform rapid annealing on wafers selected from a group consisting of conductive materials (such as conductive wafers) and non-conductive materials (such as non-conductive wafers). Although the present invention uses non-conductive and conductive silicon carbide wafers as examples, it is not limited to this. Moreover, because the electromagnetic field distribution of the present invention is easy to control and adjust, it can be applied to the annealing of multiple wafers. For large-sized silicon carbide wafers (for example, larger than 8 inches), the design of the annealing system can also be modified accordingly according to the operating principle and structure of the composite rapid annealing device of the present invention. In addition, it should be specially stated that although the present invention uses the example that the electrode 20 can carry the wafer 22 and can be heated by the induction magnetic field, the scope of rights of the present invention is not limited to this. For example, the electrode 20 of the present invention may also be for example not used to carry the wafer 22, for example, it is located on both sides of the wafer 22, such as on the upper cover 36 and the lower cover 38 of the heating chamber 30 (such as Figure 6 Although this modified design cannot heat the silicon carbide wafer 22 by heating the electrode 20, it still belongs to the feasible aspects of the present invention and thus still belongs to the scope of protection claimed by the present invention. That is, as long as the electrode 20 can function when the dielectric heating device 50 applies an alternating electric field, it can be applied to the present invention and falls within the scope of protection claimed by the present invention.

[0097] The composite rapid annealing device 10 of the present invention may selectively include a gas input unit 72 and an exhaust unit 74 connected to the chamber 32 of the heating chamber 30 via an air inlet pipe 73 and an exhaust pipe 75, respectively, so as to maintain the chamber 32 of the heating chamber 30 at a predetermined pressure. Similarly, the composite rapid annealing device 10 of the present invention further selectively includes a measurement and control system 70, which is a gas pressure and gas flow control system, including a pressure detection unit 76 and a controller 78, the pressure detection unit 76 is used to measure the gas pressure of the chamber 32 of the heating chamber 30, and the controller 78 controls the operation of the gas input unit 72 and / or the exhaust unit 74 according to the above-mentioned gas pressure value.

[0098] For example, the operating range of the above-mentioned air pressure and airflow control system is, for example, from 0.1 atmosphere to 10 atmospheres. The pressure of the gas is monitored by the pressure detection unit 76. In addition, the gas input unit 72 injects the gas into the chamber 32 of the heating chamber 30 through the air inlet pipe 73 according to the gas flow setting, and uses the exhaust unit 74 to exhaust the gas from the chamber 32 of the heating chamber 30 through the exhaust pipe 75, wherein the exhaust unit 74 is, for example, a vacuum pump. In detail, before the gas is input into the chamber 32 of the heating chamber 30, the present invention can first evacuate the chamber 32 of the heating chamber 30 with the exhaust unit 74, and after the chamber 32 of the heating chamber 30 is in a vacuum state, the gas is introduced into the chamber 32 of the heating chamber 30 with the gas input unit 72 until the chamber 32 of the heating chamber 30 reaches a predetermined pressure. The predetermined pressure of the chamber 32 of the heating chamber 30 ranges from 0.1 atm to 10 atm, and can be any numerical interval or upper and lower end points in this predetermined pressure range. The above-mentioned gas can be, for example, pure gas such as nitrogen or argon, but any gas that can make the chamber 32 of the heating chamber 30 reach the set gas and its predetermined pressure range belongs to the scope of protection requested by the present invention. In addition, the present invention can control and set the flow rate of the gas input unit 72 input gas through the controller 78, and cooperate with the operation of the exhaust unit 74 to keep the chamber 32 of the heating chamber 30 at the above-mentioned predetermined pressure.

[0099] In addition, the measurement and control system further selectively includes a pyrometer 79 for measuring the temperature of the chamber 32 of the heating chamber 30. The pyrometer 79 is, for example, an infrared pyrometer, but is not limited thereto. The emissivity of the wafer (such as silicon carbide material) measured by the present invention using a black body radiation source is 0.74, and this emissivity value is input into the pyrometer 79, which can be used for all temperature measurements in the technology disclosed by the present invention.

[0100] In summary, the composite rapid annealing device and method of the present invention has the following effects and advantages:

[0101] (1) By combining the induction heating mechanism and the dielectric heating mechanism, it can be used to heat both conductive and non-conductive objects at the same time. For example, the temperature of a silicon carbide wafer can be increased by the induction heating mechanism, and when the conductivity of the silicon carbide wafer decreases due to the increase in temperature, the temperature of the silicon carbide wafer can be increased by the dielectric heating mechanism.

[0102] (2) The induction heating mechanism can also increase the temperature of the electrode. When the conductivity of the SiC wafer decreases due to the increase in temperature, the SiC wafer can be continuously heated by the heating electrode, so that the SiC wafer maintains a certain heating rate.

[0103] (3) The electrode can be used as a bearing base and a heating base.

[0104] (4) The heating chamber has a metal tube that can serve as a reflective layer and a Faraday shielding layer, which can not only reduce the radiation heat dissipation loss of the heating chamber, but also allow the AC magnetic field to enter the heating chamber to generate eddy currents in the wafer.

[0105] (5) A barrier layer is located between the electrode and the wafer or between the wafers to prevent diffusion contamination. The barrier layer can also be used as a supporting base and a heating base.

[0106] The above description is for illustrative purposes only and is not intended to be limiting. Any equivalent modifications or changes made thereto without departing from the spirit and scope of the present invention shall be included in the appended claims.

Claims

1. A composite rapid annealing device, characterized in that: At least: Two electrodes, wherein at least one object to be processed is placed between the two electrodes; A heating chamber having a chamber for at least accommodating the object to be processed; an induction heating device for performing an induction heating step on the object to be processed in the heating chamber, wherein the induction heating device generates an eddy current in the object to be processed by generating an induced magnetic field, thereby heating the object to be processed; and A dielectric heating device is used to perform a dielectric heating step on the object to be processed in the heating chamber, wherein the dielectric heating device generates an electric field on the two electrodes to heat the object to be processed between the two electrodes.

2. The composite rapid annealing device as claimed in claim 1, characterized in that: The induction heating device performs the induction heating step on the object to be processed and the two electrodes in the heating chamber, so as to heat the object to be processed and the two electrodes.

3. The composite rapid annealing device as claimed in claim 1, characterized in that: The induction heating device and the dielectric heating device respectively perform the induction heating step and the dielectric heating step simultaneously, sequentially, intermittently or alternately.

4. The composite rapid annealing device as claimed in claim 1, characterized in that: The invention also comprises a Faraday shielding layer arranged on the heating cavity, and the induction heating device penetrates through the Faraday shielding layer to form the induction magnetic field in the chamber of the heating cavity.

5. The composite rapid annealing device as claimed in claim 4, characterized in that: The Faraday shielding layer is a metal tube with a plurality of openings.

6. The composite rapid annealing device as claimed in claim 5, characterized in that: The metal tube has a reflective surface to reduce the radiation heat dissipation loss of the heating chamber.

7. The composite rapid annealing device as claimed in claim 6, characterized in that: The reflective surface of the metal tube is also covered with a reflective layer.

8. The composite rapid annealing device as claimed in claim 1, characterized in that: There is at least one barrier layer between the two electrodes and the object to be processed.

9. The composite rapid annealing device as claimed in claim 1, characterized in that: There are a plurality of objects to be processed, and at least one barrier layer is disposed between the objects to be processed.

10. The composite rapid annealing device according to claim 8 or 9, characterized in that: One of the barrier layer and the object to be processed is a polycrystalline structure, and the other of the barrier layer and the object to be processed is a single crystal structure.

11. The composite rapid annealing device according to claim 8 or 9, characterized in that: The induction heating device and the dielectric heating device perform the induction heating step and the dielectric heating step on the object to be processed and the barrier layer, so as to heat the object to be processed and the barrier layer.

12. The composite rapid annealing device as claimed in claim 1, characterized in that: The object to be processed is selected from a group consisting of a conductive object and a non-conductive object.

13. The composite rapid annealing device as claimed in claim 1, characterized in that: The object to be processed is a wafer.

14. The composite rapid annealing device as claimed in claim 1, characterized in that: The two electrodes are made of graphite.

15. The composite rapid annealing device as claimed in claim 1, characterized in that: The induction heating device comprises an induction coil wound around the heating chamber, wherein the induction heating device applies a first alternating electromagnetic signal with a first predetermined frequency to the induction coil to generate the induced magnetic field on the object to be processed and the two electrodes.

16. The composite rapid annealing device according to claim 15, characterized in that: The first predetermined frequency ranges from 50 kHz to 200 kHz.

17. The composite rapid annealing device as claimed in claim 1, characterized in that: The dielectric heating device applies a second alternating electromagnetic signal with a second predetermined frequency to generate the electric field on the two electrodes located on both sides of the object to be processed.

18. The composite rapid annealing device according to claim 17, characterized in that: The second predetermined frequency ranges from 10 MHz to 900 MHz.

19. The composite rapid annealing device according to claim 17, characterized in that: The dielectric heating device includes a radio frequency power supply and a matcher. The radio frequency power supply provides the second alternating electromagnetic signal with the second predetermined frequency. The matcher is electrically connected between the radio frequency power supply and the two electrodes to reduce reflection of the second alternating electromagnetic signal.

20. The composite rapid annealing device as claimed in claim 1, characterized in that: The invention also comprises a gas input unit and a gas extraction unit which are respectively connected to the chamber of the heating chamber so as to keep the chamber of the heating chamber at a predetermined pressure.

21. The composite rapid annealing device as claimed in claim 20, characterized in that: The predetermined pressure of the chamber of the heating chamber ranges from 0.1 atm to 10 atm.

22. The composite rapid annealing device as claimed in claim 20, characterized in that: It also includes a measurement and control system, including a pressure detection unit and a controller. The pressure detection unit is used to measure the gas pressure of the chamber of the heating chamber. The controller controls the operation of the gas input unit and / or the exhaust unit accordingly according to the value of the gas pressure.

23. The composite rapid annealing device as claimed in claim 22, characterized in that: The measurement and control system further comprises a pyrometer for measuring the temperature of the chamber of the heating chamber.

24. The composite rapid annealing device as claimed in claim 1, characterized in that: The heating chamber comprises a chamber body, an upper cover and a lower cover. The chamber body is connected between the upper cover and the lower cover to form the chamber between the chamber body, the upper cover and the lower cover.

25. The composite rapid annealing device as claimed in claim 24, characterized in that: The heating chamber is made of a quartz tube or a ceramic tube.

26. A composite rapid annealing method, characterized in that: At least: Performing an induction heating step on at least one object to be processed by an induction heating device, wherein the induction heating device generates an eddy current in the object to be processed by generating an induced magnetic field, thereby heating the object to be processed; and A dielectric heating step is performed on the object to be processed by a dielectric heating device, wherein the dielectric heating device heats the object to be processed by generating an electric field.

27. The composite rapid annealing method according to claim 26, characterized in that: The object to be processed is carried between two electrodes, the induction heating device performs the induction heating step on the object to be processed and the two electrodes to heat the object to be processed and the two electrodes, and the dielectric heating device generates the electric field on the two electrodes to heat the object to be processed.