Processing technology of launch canister

By combining the hat-shaped composite longitudinal bars with the aluminum alloy lining, combined with the laying of multi-layer materials and optimizing the thickness and angle, the problem of insufficient bonding strength of the composite launch tube is solved, and a high-performance and low-weight launch tube design is achieved to meet the needs of Meet the multiple performance requirements of the launch tube.

CN118769574AActive Publication Date: 2024-10-15江苏昌力科技股份有限公司
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202410988303.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-23
Publication Date
2024-10-15
Estimated Expiration
2044-07-23

AI Technical Summary

Technical Problem

The bonding strength of the existing composite launch tube is insufficient and cannot withstand the specified stress value, causing the launch tube to explode prematurely. The impact of the material winding direction on performance is not considered, resulting in an increase in overall quality and cost.

Method used

The hat-shaped composite longitudinal bars are combined with the aluminum alloy lining, and the composite reinforcement is formed by winding carbon fiber composite materials, and multiple layers of insulation and protective materials are laid on its surface. Combined with the shielding net and outer skin layer, the material thickness and laying angle are optimized to ensure Improve structural strength and performance.

Benefits of technology

It achieves high mechanical properties, penetration protection performance, electromagnetic shielding performance and thermal insulation performance of the launch tube. The overall weight is low, which meets the working requirements of the launch tube and improves the reliability and stress resistance of the structure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118769574A_ABST
    Figure CN118769574A_ABST
Patent Text Reader

Abstract

The invention discloses a processing technology of a launch canister. The processing technology comprises the following steps: S1, processing an aluminum alloy lining and composite longitudinal bars; composite longitudinal bars are processed through carbon fiber composite materials, the cross sections of the composite longitudinal bars are in a cap shape, and the concave positions of the composite longitudinal bars are sequentially filled with first heat preservation layers and first anti-penetration protection layers to form composite reinforcing bodies. S2, winding a carbon fiber composite material on the surface of the aluminum alloy lining to serve as a composite middle lining; and S3, the multiple composite reinforcing bodies are glued to the surface of the composite middle lining. And S4, a second heat preservation layer and a second anti-penetration protection layer are sequentially laid on the surface of the cylinder formed in the step S3. And S5, laying a shielding net on the surface of the cylinder body formed in the step S4. And S6, a carbon fiber composite material is laid on the surface of the cylinder formed in the step S5. The prepared launch canister has the advantages of being high in mechanical property, penetration protection performance, electromagnetic shielding performance and heat preservation and heat insulation performance, and the basic performance requirements and function requirements of storage, hoisting, transportation, erecting, launching and other work of the launch canister are met.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of launch tubes, and in particular to a processing technology for launch tubes. Background Art

[0002] As modern military operations place increasingly higher demands on weapon systems, composite launch tubes that combine mechanical properties, thermal insulation properties, and electromagnetic shielding properties have been gradually developed and applied.

[0003] However, the composite material launch tube in the prior art (such as patent number CN103322854B) is just laying multiple layers of materials in sequence, and then fixing them through conventional curing processes, without considering the bonding strength of the composite multi-layer structure. Due to the different thermal expansion coefficients of different materials, the method of laying each functional layer in sequence will have the problem of insufficient bonding strength on the one hand, and different shrinkage rates caused by environmental influences between different functional layers on the other hand, which will affect the connection between different functional layers and cause the launch tube to explode prematurely. In addition, the prior art does not consider the impact of different winding directions of materials on their performance, and often only improves the performance of each functional layer by increasing the thickness, which leads to an increase in the overall quality and cost of the launch tube.

[0004] The launch tube disclosed in patent No. CN202010824801.5 consists of an inner tube and an outer tube. In order to take into account the requirements of low weight and connection between the inner and outer tubes, it is proposed to use longitudinal ribs to co-solidify the inner and outer tubes. However, the launch tube is not designed for thermal insulation, penetration protection, etc., nor does it point out how to achieve effective performance of various functions through reasonable layer distribution and thickness distribution. Summary of the invention

[0005] In order to solve the technical problem in the prior art that the bonding strength of the launch tube is insufficient and cannot withstand the specified stress value, resulting in premature explosion of the launch tube, the present invention provides a processing technology for a launch tube to solve the above problem.

[0006] The technical solution adopted by the present invention to solve its technical problems is: a processing technology for a launch tube, including S1: processing an aluminum alloy lining and composite longitudinal reinforcement; using carbon fiber composite materials to process the composite longitudinal reinforcement, the cross-section of the composite longitudinal reinforcement is a hat-shaped, and the recessed parts of the composite longitudinal reinforcement are filled with a first thermal insulation layer and a first anti-penetration protection layer in sequence to form a composite reinforcement body.

[0007] S2: Carbon fiber composite material is wound on the surface of aluminum alloy liner as a composite middle liner.

[0008] S3: Multiple composite reinforcements are bonded to the surface of the composite middle lining, and the bottom of the first anti-penetration protection layer and the composite longitudinal reinforcement are bonded to the composite middle lining.

[0009] S4: The second thermal insulation layer and the second anti-penetration protection layer are sequentially laid on the surface of the cylinder formed in step S3 in the area outside the composite reinforcement body.

[0010] S5: Lay a shielding net on the surface of the cylinder formed in step S4.

[0011] S6: laying a carbon fiber composite material as an outer skin layer on the surface of the cylinder formed in step S5.

[0012] S7: The top of the composite longitudinal reinforcement is bonded to the shielding mesh and the outer skin.

[0013] Furthermore, the first thermal insulation layer and the second thermal insulation layer are both laminated aerogels, and the first anti-penetration protection layer and the second anti-penetration protection layer are both laminated UHMWPE composite materials.

[0014] Furthermore, the inner surface of the first anti-penetration protection layer and the bottom surface of the composite longitudinal reinforcement are on the same arc surface.

[0015] Furthermore, the thickness of the aluminum alloy lining is 7mm to 8mm, the thickness of the composite middle lining is 4mm to 6mm, the thickness of the composite longitudinal reinforcement is 4mm to 6mm, the thickness of the first thermal insulation layer and the second thermal insulation layer is 15mm to 18mm, the thickness of the first anti-penetration protection layer and the second anti-penetration protection layer is 15mm to 18mm, the thickness of the shielding net is 0.095mm to 0.097mm, and the thickness of the outer skin layer is 4mm to 6mm.

[0016] Furthermore, the angle between the outermost laying angle of the composite middle liner and the central axis of the launch tube is 45° to 60°, and the angle between the outermost laying angle of the outer skin layer and the central axis of the launch tube is 80° to 90°.

[0017] Furthermore, a glass fiber middle liner is laid between the aluminum alloy inner liner and the composite middle liner, and the glass fiber middle liner is formed of glass fiber or glass fiber felt.

[0018] Furthermore, the thickness of the glass fiber lining is 0.3 mm to 0.5 mm.

[0019] Furthermore, a plurality of annular ribs are wound around the outer surface of the outer skin layer, and the annular ribs are made of the same material as the outer skin layer, and any one or more of the annular ribs serve as erection fulcrums or rotation fulcrums.

[0020] Furthermore, the exterior of the outer skin layer is coated with a reflective heat-insulating and hydrophobic coating, and the inner surface of the aluminum alloy lining is coated with a heat-insulating and friction-reducing coating.

[0021] The beneficial effects of the present invention are:

[0022] (1) The launch tube prepared by the processing technology of the launch tube described in the present invention has the characteristics of high mechanical properties, strong penetration protection performance, electromagnetic shielding performance and thermal insulation performance, and the overall weight is less than 7 tons, which meets the basic performance requirements and functional requirements of the launch tube for storage, lifting, transportation, erection, and launching.

[0023] (2) The processing technology of the launch tube described in the present invention connects the inner and outer layers of the tube body through hat-shaped composite longitudinal reinforcements, and at the same time combines the laying method of each layer of material and the reasonable configuration of material thickness to make the launch tube structure more reliable. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] The present invention is further described below in conjunction with the accompanying drawings and embodiments.

[0025] Figure 1 It is a flow chart of the processing technology of the launch tube of the present invention;

[0026] Figure 2 is a stereoscopic view of a launch tube prepared using the process of the present invention;

[0027] Figure 3 is a cross-sectional view of the end face of a launch tube prepared using the process of the present invention;

[0028] Figure 4 yes Figure 3 Enlarged view of point a in the middle.

[0029] In the figure, 1. aluminum alloy lining, 2. composite longitudinal reinforcement, 201. raised part, 202. flange, 3. first thermal insulation layer, 4. first anti-penetration protection layer, 5. composite middle lining, 6. second thermal insulation layer, 7. second anti-penetration protection layer, 8. shielding net, 9. outer skin layer, 10. glass fiber middle lining, 11. ring reinforcement, 12. reflective thermal insulation and hydrophobic coating, 13. thermal insulation and friction reducing coating. DETAILED DESCRIPTION

[0030] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.

[0031] like Figure 1 As shown, a processing technology for a launch tube includes the following steps:

[0032] S1: Processing aluminum alloy lining 1 and composite longitudinal reinforcement 2; using carbon fiber composite material to process composite longitudinal reinforcement 2, the cross section of composite longitudinal reinforcement 2 is hat-shaped, and the concave part of composite longitudinal reinforcement 2 is filled with first thermal insulation layer 3 and first anti-penetration protection layer 4 in sequence to form a composite reinforcement body. That is, composite longitudinal reinforcement 2 has a convex part 201 and a flange 202, and first thermal insulation layer 3 and first anti-penetration protection layer 4 are located in convex part 201.

[0033] S2: Winding a carbon fiber composite material on the surface of the aluminum alloy liner 1 as a composite middle liner 5.

[0034] S3: Multiple composite reinforcement bodies are bonded to the surface of the composite middle liner 5, and the first anti-penetration protection layer 4 and the bottom of the composite longitudinal reinforcement 2 are bonded to the composite middle liner 5. That is, in the raised portion 201, the first thermal insulation layer 3 is located outside the first anti-penetration protection layer 4.

[0035] S4: The second thermal insulation layer 6 and the second anti-penetration protection layer 7 are sequentially laid on the surface of the cylinder formed in step S3 in the outer area of ​​the composite reinforcement body, that is, outside the raised part 201, and the second protection layer is located inside the second anti-penetration protection layer 7.

[0036] S5: Lay a shielding net 8 on the surface of the cylinder formed in step S4.

[0037] S6: laying carbon fiber composite material as the outer skin layer 9 on the surface of the cylinder formed in step S5.

[0038] S7: The top of the composite longitudinal reinforcement 2 is bonded to the shielding mesh 8 and the outer skin layer 9.

[0039] The difference between the present invention and the prior art is that: Figure 3 and Figure 4 As shown, multiple composite longitudinal bars 2 are used to connect the inner and outer layers of the launch tube. The composite longitudinal bars 2 are made of the same material as the composite middle liner 5 and the outer skin layer 9 (the shielding net 8 is a mesh structure and will not affect the connection between the outer skin layer 9 and the composite longitudinal bars 2). The connection strength of the three is higher and is not easily affected by the thermal expansion coefficient and causes the connection relationship to break. The provision of the composite longitudinal bars 2 can also improve the stress resistance and bending resistance of the tube. Second: inside and outside the composite longitudinal bars 2, the laying positions of the thermal insulation layer and the anti-penetration protection layer are opposite, that is, the two are laid in an offset manner, so that they are no longer a single material in the circumferential direction, and the composite longitudinal bars 2 divide the tube into multiple sections in the circumferential direction. When the temperature suddenly changes and the expansion amount of different materials changes, each layer of material can adjust the radial deformation on the inside and outside of the composite longitudinal bars 2 to reduce the circumferential dislocation, thereby reducing the influence of different material parameters on the structural strength. Solving this technical problem can greatly improve the internal pressure resistance and bending resistance of the launch tube.

[0040] In addition to solving the stress problems at the connection points of the above-mentioned layers, the launch tube also needs to solve the stress concentration problem of the overall structure. The more serious the stress concentration phenomenon is, the greater the possibility of explosion of the launch tube. The internal pressure and bending force of the launch tube as a whole under the same working condition are mainly related to the thickness distribution and material selection of each layer of materials. The launch tube designed below meets the following performance requirements put forward by the customer: (1) Mechanical properties: It can withstand a peak internal pressure of 0.8MPa and a temperature peak of 1000℃. It can bear a projectile weight of 50t, and the peak load of the erection support is not more than 70t. (2) Penetration protection performance: The overall structure can resist the normal angle of 0° at a distance of 100 from ordinary rifle bullets. (3) Electromagnetic shielding performance: The electromagnetic interference shielding effectiveness for low-frequency and high-frequency bands is not less than 40dB. (4) Thermal insulation performance: The launch tube can withstand the specified sunlight intensity conditions (total radiation intensity is 1120W / m 2 ) after continuous irradiation for 4 hours, the temperature inside the cylinder does not exceed 35℃.

[0041] The first insulation layer 3 and the second insulation layer 3 are preferably aerogels laid in layers. Aerogels have the characteristics of low density and ultra-low thermal conductivity, are completely hydrophobic and have good fire retardant properties. The insulation layer can be made of aerogel felt. The material can be cut at will. The aerogel can be laid and cut along the surface and can be fixed with pressure-sensitive tape. The first anti-penetration protection layer 4 and the second anti-penetration protection layer 7 are both UHMWPE composite materials laid in layers. UHMWPE composite materials are ultra-high molecular weight polyethylene fiber materials that can be machined into a specified arc shape for laying and fixing. The shielding net 8 can be two layers of copper nets.

[0042] The inner surface of the first anti-penetration protection layer 4 and the bottom surface of the composite longitudinal reinforcement 2 are preferably on the same arc surface, so that the bonding area between the entire composite longitudinal reinforcement 2 and the composite middle liner 5 can be increased. When fixed, the inner surface of the flange 202 of the composite longitudinal reinforcement 2 is directly bonded to the composite middle liner 5. The bottom surface of the composite longitudinal reinforcement 2 is the inner surface of the flange 202.

[0043] The thickness of each material has a certain influence on the mechanical properties, functionality and quality of the launch tube. In the preferred embodiment of the present invention, the thickness of the aluminum alloy lining 1 is 7mm~8mm, the thickness of the composite middle lining 5 is 4mm~6mm, the thickness of the composite longitudinal reinforcement 2 is 4mm~6mm, the thickness of the first thermal insulation layer 3 and the second thermal insulation layer 6 is 15mm~18mm, the thickness of the first anti-penetration protection layer 4 and the second anti-penetration protection layer 7 is 15mm~18mm, the thickness of the shielding net 8 is 0.095mm~0.097mm, and the thickness of the outer skin layer 9 is 4mm~6mm.

[0044] The influence of thickness change of each layer on the internal pressure resistance of the cylinder is: composite middle liner 5 = outer skin layer 9 > aluminum alloy inner liner 1, and the influence of thickness change of each layer on the bending resistance of the cylinder is: outer skin layer 9 > composite middle liner 5 > aluminum alloy inner liner 1. The thickness change of other functional layers has the weakest influence on the mechanical properties. When the composite middle liner 5, outer skin layer 9 and composite longitudinal reinforcement 2 of the same material are selected with a thickness of 4mm to 6mm, the mechanical properties of the cylinder can meet the specified requirements while ensuring that the quality of the cylinder is at a lower value.

[0045] For the aluminum alloy lining 1, its metal material can ensure good mechanical properties. Through simulation experiments, it is found that the lower the thickness of the aluminum alloy lining 1, the greater the stress on the aluminum alloy lining 1, and the increase in the thickness of the aluminum alloy lining 1 will increase the cost. Combined with the data in Table 1, comparing Scheme 1 and Scheme 3, when the thickness of other layers is consistent and the internal pressure or bending force is consistent, when the aluminum alloy lining 1 is 5mm, the maximum stress on the cylinder and the corresponding stress deformation are greatly improved compared with when the thickness of the aluminum alloy lining 1 is 7mm, and the possibility of explosion is greater. The same is true for Scheme 2 and Scheme 4. Comparing Scheme 1 and Scheme 2, since the composite middle lining 5 and the outer skin layer 9 are made of the same material, the outer skin layer 9 is thickened while the composite middle lining 5 is thinned, which has little effect on the mechanical properties of the cylinder.

[0046] Table 1 Simulation results of different launch tube structure schemes

[0047]

[0048] For the composite middle liner 5 and outer skin layer 9, which have a greater impact on the mechanical properties, the laying angle of the material also has a certain influence on the stress. When the angle between the outermost laying angle of the composite middle liner 5 and the central axis of the launch tube is 45°, the bending performance of the launch tube is optimal. When the angle between the outermost laying angle of the composite middle liner 5 and the outer skin layer 9 and the central axis of the launch tube is 80°~90°, the internal pressure resistance of the launch tube is optimal. The present invention combines the two and selects the angle between the outermost laying angle of the outer skin layer 9 and the central axis of the launch tube to be 80°~90° to ensure better resistance to internal pressure. At the same time, the angle between the outermost laying angle of the composite middle liner 5 and the central axis of the launch tube is 45°~60°, so as to coordinate the bending performance and internal pressure resistance of the launch tube.

[0049] For the aluminum alloy liner 1 made of metal and the composite middle liner 5 made of composite material, considering the different thermal expansion coefficients between the two, there is a phenomenon of heteroelectric corrosion. In the present invention, a glass fiber middle liner 10 is preferably laid between the aluminum alloy liner 1 and the composite middle liner 5. The glass fiber middle liner 10 is formed of glass fiber or glass fiber felt. The thickness of the glass fiber middle liner 10 is 0.3mm to 0.5mm. The glass fiber middle liner 10 uses high-toughness resin to isolate the heteroelectric corrosion between the carbon fiber and the metal liner to avoid delamination of the two.

[0050] like Figure 2 As shown, the outer surface of the outer skin layer 9 can also be wrapped with multiple annular ribs 11, which are made of the same material as the outer skin layer 9, and any one or more annular ribs 11 serve as erection fulcrums or rotation fulcrums. The annular ribs 11 can improve the overall mechanical properties of the launch tube on the one hand, and on the other hand, they are specially strengthened at the erection fulcrums and rotation fulcrums to ensure the bending and torsional rigidity and strength of the overall structure.

[0051] For the heat insulation of the launch tube, the present invention has a triple heat insulation setting, such as Figure 4 As shown:

[0052] The first insulation setting is that the outer skin layer 9 is coated with a reflective heat-insulating hydrophobic coating 12, which effectively reflects more than 85% of solar radiation energy and plays a certain heat barrier role in external hot air conduction, reducing the impact of solar radiation from the outermost side.

[0053] The second insulation setting is the first insulation layer 3 and the second insulation layer 6 in the internal structure, and its principle has been explained above.

[0054] The third insulation setting is to coat the inner surface of the aluminum alloy liner 1 with a heat-insulating and friction-reducing coating 13 to minimize the heat transfer and heat radiation effects of the high-temperature gas on the aluminum alloy liner 1 and the composite middle liner 5 during the launch process, thereby avoiding the performance degradation of metal materials and composite materials caused by high temperature.

[0055] This triple insulation setting provides insulation protection from the inside, middle and outside to ensure that the temperature of the cylinder itself is minimally affected by the environment.

[0056] In the description of the present invention, it is necessary to understand that the orientations or positional relationships indicated by the terms "thickness", "inside", "outside", "axial", "radial", "circumferential", etc. are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.

[0057] In addition, the terms "first", "second", etc. are used for descriptive purposes only and should not be understood as indicating or implying relative importance. In the description of the present invention, unless otherwise specified, "plurality" means two or more.

[0058] In this specification, the schematic representation of the terms does not necessarily refer to the same embodiment. Moreover, the specific features, structures, materials or characteristics described can be combined in any suitable manner in one or more embodiments.

[0059] Based on the above ideal embodiments of the present invention, the relevant staff can make various changes and modifications without departing from the technical concept of the present invention through the above description. The technical scope of the present invention is not limited to the contents of the specification, and its technical scope must be determined according to the scope of the claims.

Claims

1. A processing technology for a launch tube, characterized in that: include: S1: Processing aluminum alloy lining (1) and composite longitudinal reinforcement (2); A composite longitudinal rib (2) is processed using a carbon fiber composite material, wherein the cross section of the composite longitudinal rib (2) is a hat shape, and a first thermal insulation layer (3) and a first anti-penetration protection layer (4) are sequentially filled in the concave portion of the composite longitudinal rib (2) to form a composite reinforcement body; S2: Winding a carbon fiber composite material on the surface of the aluminum alloy liner (1) as a composite middle liner (5); S3: a plurality of composite reinforcement bodies are bonded to the surface of the composite middle lining (5), and the bottom of the first anti-penetration protection layer (4) and the composite longitudinal reinforcement (2) are bonded to the composite middle lining (5); S4: laying a second thermal insulation layer (6) and a second anti-penetration protection layer (7) in sequence on the surface of the cylinder formed in step S3 and located outside the composite reinforcement body; S5: Laying a shielding net (8) on the surface of the cylinder formed in step S4; S6: laying a carbon fiber composite material as an outer skin layer (9) on the surface of the cylinder formed in step S5; S7: The top of the composite longitudinal reinforcement (2) is bonded to the shielding mesh (8) and the outer skin layer (9).

2. The processing technology of the launch tube according to claim 1 is characterized in that: The first thermal insulation layer (3) and the second thermal insulation layer (6) are both aerogels laid in layers, and the first anti-penetration protection layer (4) and the second anti-penetration protection layer (7) are both UHMWPE composite materials laid in layers.

3. The processing technology of the launch tube according to claim 1 is characterized in that: The inner surface of the first anti-penetration protective layer (4) and the bottom surface of the composite longitudinal reinforcement (2) are on the same arc surface.

4. The processing technology of the launch tube according to claim 1 is characterized in that: The thickness of the aluminum alloy lining (1) is 7 mm to 8 mm, the thickness of the composite middle lining (5) is 4 mm to 6 mm, the thickness of the composite longitudinal reinforcement (2) is 4 mm to 6 mm, the thickness of the first thermal insulation layer (3) and the second thermal insulation layer (6) are 15 mm to 18 mm, the thickness of the first anti-penetration protection layer (4) and the second anti-penetration protection layer (7) are 15 mm to 18 mm, the thickness of the shielding net (8) is 0.095 mm to 0.097 mm, and the thickness of the outer skin layer (9) is 4 mm to 6 mm.

5. The processing technology of the launch tube according to claim 2 is characterized in that: The angle between the outermost laying angle of the composite middle liner (5) and the central axis of the launch tube is 45° to 60°, and the angle between the outermost laying angle of the outer skin layer (9) and the central axis of the launch tube is 80° to 90°.

6. The processing technology of the launch tube according to claim 1 is characterized in that: A glass fiber middle liner (10) is also laid between the aluminum alloy inner liner (1) and the composite middle liner (5), and the glass fiber middle liner (10) is formed of glass fiber or glass fiber felt.

7. The processing technology of the launch tube according to claim 6 is characterized in that: The thickness of the glass fiber middle liner (10) is 0.3 mm to 0.5 mm.

8. The processing technology of the launch tube according to claim 1 is characterized in that: The outer surface of the outer skin layer (9) is wound with a plurality of annular ribs (11), the annular ribs (11) being made of the same material as the outer skin layer (9), and any one or more of the annular ribs (11) serving as an erection fulcrum or a rotation fulcrum.

9. The processing technology of the launch tube according to claim 1 is characterized in that: The exterior of the outer skin layer (9) is coated with a reflective heat-insulating and hydrophobic coating (12), and the inner surface of the aluminum alloy lining (1) is coated with a heat-insulating and friction-reducing coating (13).

Citation Information

Patent Citations

  • A composite material launch tube and its preparation method

    CN103322854B

  • Composite material concentric launch canister forming method

    CN112026199A

  • Lightweight heat preservation device of composite material cylinder and manufacturing method thereof

    CN110986673A

  • Guided missile launching canister and manufacturing method thereof

    CN111023894A

  • Cylinder body structure of hollow multi-cavity composite material launching cylinder and forming method of cylinder body structure

    CN113432486A