Preparation method of phenethyl silane
By using a composite polymerization inhibitor and a platinum catalyst in the hydrosilylation reaction of styrene and hydrogen-containing silane, the problems of low product yield and environmental pollution in the preparation process of phenethylsilane in the existing technology are solved. Efficient and safe preparation of phenethylsilane was achieved, and the selectivity of β-addition products reached more than 98.5%.
Patent Information
- Application Number
- CN202410786069.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-18
- Publication Date
- 2024-10-15
AI Technical Summary
In the existing technology, during the preparation process of phenethylsilane, the yield of the target product is low and there are environmental pollution problems. The catalyst dosage is large, the reaction is unsafe, and the equipment is complex.
Use styrene and hydrogen-containing silane to carry out hydrosilylation reaction, use complex polymerization inhibitor and platinum complex as catalyst, add cocatalyst, raise the temperature to 30~130℃ under stirring, and carry out normal pressure reaction to avoid the use of additional Solvents to simplify the process.
The yield and selectivity of the target product are improved, environmental pollution is reduced, the process is safe, the catalyst dosage is small, and it meets the requirements of green chemistry. The selectivity of the β-addition product reaches more than 98.5%.
Smart Images

Figure SMS_1
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of organic synthesis, and particularly relates to a method for preparing phenethylsilane. Background Art
[0002] Hydrosilylation is one of the important methods for preparing organosilicon compounds containing C-Si bonds. Hydrosilylation can prepare organosilicon compounds containing different functional groups, such as silanes containing double bonds, epoxy groups, phenylethyl groups, etc. Hydrosilylation of styrene with methyldichlorosilane, trichlorosilane, trimethoxysilane, methyldimethoxysilane, etc. can prepare methylphenethyldichlorosilane, phenethyltrichlorosilane, phenethyltrimethoxysilane, methylphenethyldimethoxysilane, etc., which are important intermediates for synthesizing special polyorganosiloxanes. Phenethylsilane is widely used in the preparation of photoresists, photoinitiators, waveguides, nonlinear optical materials, ceramic precursors and other fields. Therefore, it is particularly important to improve the efficiency, selectivity and conversion rate of hydrosilylation, which is a meaningful work worthy of in-depth research.
[0003] At present, phenylethylsilane is mainly prepared by the hydrosilylation reaction of styrene and hydrogen-containing silane, and the chemical reaction equations are as follows (1) and (2) respectively.
[0004]
[0005] n=0、1、2、3
[0006] m=0、1、2、3
[0007] R=CH3、C2H5 etc.
[0008] R'=CH3O, CH3CH2O, etc.
[0009] U.S. Patent No. 6,054,602 (April 25, 2000) discloses the preparation of aromatic chlorosilanes by hydrosilylation of an aromatic compound having a vinyl group directly bonded to an aromatic ring with a hydrogendichlorosilane compound;
[0010] The present invention relates to a method for preparing a compound, wherein an aromatic vinyl compound is subjected to a hydrosilylation reaction by a hydrochlorosilane compound in the presence of platinum or a platinum compound and a carboxylic acid, thereby increasing the amount of the β-addition product of the aromatic ring, with the purpose of facilitating the formation of the β-addition product of the hydrosilylation reaction. By using carboxylic acid, carboxylic acid derivatives and carboxylate as a promoter, the content of the β-addition product is increased to a certain extent, but the yield of the target product is very low. Summary of the invention
[0011] In order to solve the above problems in the prior art, the present invention aims to provide a method for preparing phenethylsilane.
[0012] The technical solution adopted by the present invention is:
[0013] A method for preparing phenethylsilane comprises the following steps:
[0014] Step S1: Add styrene, polymerization inhibitor, catalyst and co-catalyst into a normal pressure reactor, wherein the mass ratio of styrene, polymerization inhibitor, catalyst and co-catalyst is 1:1.0×10 -6 ~1000×10 -6 : 10×10 -6 ~5000×10 -6 : 10×10 -6 ~5000×10 -6 ;
[0015] The inhibitor is one or more of 2,4-dinitrophenol, hydroquinone, benzoquinone, 2,6-dinitro-p-cresol, 2-sec-butyl-4,6-dinitrophenol, alkylhydroxybenzenesulfonic acids, 1-hydroxy-2,2,6,6-tetramethylpiperidine and its derivatives, hydroxylamine compounds, N,N-diisobutyl-p-phenylenediamine, and p-tert-butylcatechol; the catalyst is one of platinum metal compounds; and the co-catalyst is one of triphenylphosphine, phenothiazine, carbazole, tri-n-butylamine, and 4-methyl-3-penten-2-one;
[0016] Step S2: heating to 30-130° C. under stirring, then adding hydrosilane dropwise to react, maintaining the reaction temperature and stirring;
[0017] The hydrogen-containing silane includes one of trichlorosilane, methyldichlorosilane, trimethoxyhydrogensilane, methyldimethoxysilane, triethoxyhydrogensilane, and methyldiethoxysilane;
[0018] Step S3: After the hydrosilane is dripped, the reaction is completed by stirring at the temperature for 0 to 2 hours to obtain a phenethylsilane synthesis product;
[0019] Step S4: Separate and purify the synthetic product obtained in step S3 to obtain a phenethylsilane product.
[0020] Furthermore, the catalyst is selected from a complex of chloroplatinic acid and its sodium, potassium, ammonium salt and isopropanol, or a complex of chloroplatinic acid and its sodium, potassium, ammonium salt and vinyl silane.
[0021] Furthermore, in step S2, the temperature is raised to 60° C. to 100° C. under stirring.
[0022] Furthermore, the polymerization inhibitor is selected from a compound of 2-sec-butyl-4,6-dinitrophenol, dihydroxypropylhydroxylamine and N,N-diisobutyl-p-phenylenediamine.
[0023] Furthermore, the catalyst is selected from one of the complexes of chloroplatinic acid and its sodium, potassium and ammonium salts with divinyltetramethyldisiloxane, linear vinylpolysiloxane and cyclic vinylpolysiloxane.
[0024] Furthermore, the co-catalyst is selected from one of phenothiazine and carbazole.
[0025] The beneficial effects of the present invention are:
[0026] The present invention uses styrene and hydrogen-containing silane as raw materials, adds a composite inhibitor, uses a platinum complex as a catalyst, adds a co-catalyst, heats to 30-130°C under stirring, and performs a hydrosilylation reaction to obtain phenylethylsilane. The present invention does not require the addition of an additional solvent, avoids the addition of steps due to the use of a solvent, and even causes environmental pollution, and meets the requirements of green chemistry and chemical industry. In addition, the present invention is a normal pressure reaction, the process is safe, the equipment is simple, the catalyst dosage is small, the catalyst has a high reaction selectivity and reaction yield, and the target product phenylethylsilane is easy to separate and has a high content. The selectivity of the β-addition product is above 98.5%. DETAILED DESCRIPTION
[0027] The present invention will be further described below in conjunction with specific embodiments.
[0028] The present invention can be further illustrated by the following examples, but the examples are not intended to limit the scope of protection of the present invention, and all the raw materials used are commercially available.
[0029] Example 1: Preparation of methylphenethyldichlorosilane
[0030] To a 500 mL four-necked flask equipped with a stirrer, a thermometer, a condenser and a dropping funnel, 104.2 g of styrene, 0.03 g of a mixture of 2-sec-butyl-4,6-dinitrophenol, dihydroxypropylhydroxylamine and N,N-diisobutyl-p-phenylenediamine in a ratio of 1:1:1 by mass was used as a polymerization inhibitor, 0.18 g of a complex of chloroplatinic acid and divinyltetramethyldisiloxane was used as a catalyst, and 0.06 g of phenothiazine was used as a co-catalyst;
[0031] Raise the temperature to 70°C, add 117.3 g of methyldichlorosilane dropwise, control the reaction temperature at 70-80°C, add the mixture in 1 hour, and keep the reaction at 70-80°C for 0.5 hour;
[0032] After the reaction was completed, the crude product was subjected to vacuum distillation with a vacuum degree of -0.098 MPa, and the fractions at 130-132°C were collected to obtain 208.5 g of methylphenethyldichlorosilane with a content of 98.5%. The product yield was 95.1% and the β addition selectivity was 99.8%.
[0033] Example 2: Preparation of phenethyltrichlorosilane
[0034] To a 500 mL four-necked flask equipped with a stirrer, a thermometer, a condenser and a dropping funnel, 104.2 g of styrene, 0.03 g of a 1:1:1 mixture of 2-sec-butyl-4,6-dinitrophenol, dihydroxypropylhydroxylamine and N,N-diisobutyl-p-phenylenediamine as an inhibitor, 0.18 g of a complex of chloroplatinic acid and linear vinyl polysiloxane as a catalyst, and 0.06 g of phenothiazine as a co-catalyst;
[0035] The temperature was raised to 60°C, 138.2 g of trichlorosilane was added dropwise, the reaction temperature was controlled at 60-70°C, the addition was completed in 1 hour, and the reaction was kept at 60-70°C for 0.5 hour.
[0036] After the reaction was completed, the crude product was subjected to vacuum distillation with a vacuum degree of -0.098 MPa, and the fraction at 126-127°C was collected to obtain 228.4 g of phenethyltrichlorosilane with a content of 98.7%. The product yield was 95.3% and the β addition selectivity was 99.5%.
[0037] Example 3: Preparation of phenethyltrimethoxysilane
[0038] To a 500 mL four-necked flask equipped with a stirrer, a thermometer, a condenser and a dropping funnel, 104.2 g of styrene, 0.03 g of a 1:1:1 mixture of 2-sec-butyl-4,6-dinitrophenol, dihydroxypropylhydroxylamine and N,N-diisobutyl-p-phenylenediamine as an inhibitor, 0.24 g of a complex of potassium chloroplatinate and cyclic vinyl polysiloxane as a catalyst, and 0.08 g of carbazole as a co-catalyst;
[0039] Raise the temperature to 90°C, add 124.6 g of trimethoxysilane dropwise, control the reaction temperature at 90-100°C, add the mixture in 1 hour, and keep the reaction at 90-100°C for 0.5 hour;
[0040] After the reaction was completed, the crude product was subjected to vacuum distillation with a vacuum degree of -0.098 MPa, and the fraction at 134-135°C was collected to obtain 217.3 g of phenethyltrimethoxysilane with a content of 98%. The product yield was 96% and the β addition selectivity was 98.5%.
[0041] Example 4: Preparation of methylphenethyldimethoxysilane
[0042] To a 500 mL four-necked flask equipped with a stirrer, a thermometer, a condenser and a dropping funnel, 104.2 g of styrene, 0.03 g of a mixture of 2-sec-butyl-4,6-dinitrophenol, dihydroxypropylhydroxylamine and N,N-diisobutyl-p-phenylenediamine in a ratio of 1:1:1 by mass was used as a polymerization inhibitor, 0.21 g of a complex of sodium chloroplatinate and divinyltetramethyldisiloxane was used as a catalyst, and 0.07 g of carbazole was used as a co-catalyst;
[0043] Raise the temperature to 70°C, add 108.3 g of methyldimethoxysilane dropwise, control the reaction temperature at 70-80°C, add the mixture in 1 hour, and keep the reaction at 70-80°C for 0.5 hour;
[0044] After the reaction was completed, the crude product was subjected to vacuum distillation with a vacuum degree of -0.098 MPa, and the fractions at 98-100°C were collected to obtain 201 g of methylphenethyldimethoxysilane with a content of 98.9%. The product yield was 95.5% and the β addition selectivity was 99.3%.
[0045] The present invention uses styrene and hydrogen-containing silane as raw materials, adds a composite inhibitor, uses a platinum complex as a catalyst, adds a co-catalyst, heats to 30-130°C under stirring, and performs a hydrosilylation reaction to obtain phenylethylsilane. The present invention does not require the addition of an additional solvent, avoids the addition of steps due to the use of a solvent, and even causes environmental pollution, and meets the requirements of green chemistry and chemical industry. In addition, the present invention is a normal pressure reaction, the process is safe, the equipment is simple, the catalyst dosage is small, the catalyst has a high reaction selectivity and reaction yield, and the target product phenylethylsilane is easy to separate and has a high content. The selectivity of the β-addition product is above 98.5%.
[0046] The present invention is not limited to the above-mentioned optional implementation modes. Anyone can derive other various forms of products under the inspiration of the present invention. However, no matter what changes are made in the shape or structure, all technical solutions that fall within the scope defined by the claims of the present invention fall within the protection scope of the present invention.
Claims
1. A method for preparing phenethylsilane, characterized in that: The following steps are involved: 1 Step S1: Add styrene, polymerization inhibitor, catalyst and co-catalyst into a normal pressure reactor, wherein the mass ratio of styrene, polymerization inhibitor, catalyst and co-catalyst is 1:1.0×10 -6 ~1000×10 -6 : 10×10 -6 ~5000×10 -6 : 10×10 -6 ~5000×10 -6 ; The inhibitor is one or more of 2,4-dinitrophenol, hydroquinone, benzoquinone, 2,6-dinitro-p-cresol, 2-sec-butyl-4,6-dinitrophenol, alkylhydroxybenzenesulfonic acids, 1-hydroxy-2,2,6,6-tetramethylpiperidine and its derivatives, hydroxylamine compounds, N,N-diisobutyl-p-phenylenediamine, and p-tert-butylcatechol; the catalyst is one of platinum metal compounds; and the co-catalyst is one of triphenylphosphine, phenothiazine, carbazole, tri-n-butylamine, and 4-methyl-3-penten-2-one; Step S2: heating to 30-130° C. under stirring, then adding hydrosilane dropwise to react, maintaining the reaction temperature and stirring; The hydrogen-containing silane includes one of trichlorosilane, methyldichlorosilane, trimethoxyhydrogensilane, methyldimethoxysilane, triethoxyhydrogensilane, and methyldiethoxysilane; Step S3: After the hydrosilane is dripped, the reaction is completed by stirring at the temperature for 0 to 2 hours to obtain a phenethylsilane synthesis product; Step S4: Separate and purify the synthetic product obtained in step S3 to obtain a phenethylsilane product.
2. The method for preparing phenethylsilane according to claim 1, characterized in that: The catalyst is selected from a complex of chloroplatinic acid and its sodium, potassium, ammonium salt and isopropanol, or a complex of chloroplatinic acid and its sodium, potassium, ammonium salt and vinyl silane.
3. The method for preparing phenethylsilane according to claim 1, characterized in that: In step S2, the temperature is raised to 60°C to 100°C while stirring.
4. The method for preparing phenethylsilane according to claim 3, characterized in that: The polymerization inhibitor is selected from a compound of 2-sec-butyl-4,6-dinitrophenol, dihydroxypropylhydroxylamine and N,N-diisobutyl-p-phenylenediamine.
5. The method for preparing phenethylsilane according to claim 2, characterized in that: The catalyst is selected from one of the complexes of chloroplatinic acid and its sodium, potassium and ammonium salts with divinyltetramethyldisiloxane, linear vinylpolysiloxane and cyclic vinylpolysiloxane.
6. The method for preparing phenethylsilane according to claim 1, characterized in that: The co-catalyst is selected from one of phenothiazine and carbazole.