Machining method for aluminum casting sand casting piece of automobile testing fixture
By determining the reference and removing the sand holes in cast aluminum turning parts, eliminating internal stress, and using insert knife and white steel knife for finishing, the reference difficulties and poor performance in cast aluminum parts are solved, and the product is improved Plasticity and welding performance reduce the defective rate.
Patent Information
- Application Number
- CN202411204252.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-30
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2044-08-30
AI Technical Summary
During the processing of cast aluminum parts, there are problems such as difficulty in setting the reference, many sand holes, uneven cooling of the functional curved surface, difficulty in removing internal residual stress, and poor processing performance, resulting in high defect rate, low plasticity, poor corrosion resistance and welding performance.
A processing method for cast aluminum sand turning parts of automobile inspection tools is proposed. By opening the reverse and front, the reference is determined and the sand hole is removed. The insert knife is used to open the reference to ensure consistency and plane verification, and the natural aging is placed to eliminate the internal content. Stress, use contour clamping parts and white steel knives for finishing.
The accuracy of reference positioning and plane verification are achieved, which reduces the difficulty of removing sand holes and internal stresses, and improves processing performance. The cast aluminum turning sand parts produced have high plasticity, corrosion resistance and welding performance, which reduces the number of times. Rate rate.
Smart Images

Figure CN118893475A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of aluminum casting processing methods, and in particular to a processing method for an aluminum casting foundry part of an automobile inspection tool. Background Art
[0002] Cast aluminum parts are widely used in aviation, aerospace, automobile, machinery and other industries due to their low density, high specific strength, corrosion resistance and other excellent properties. Especially in the automotive industry, a large number of cast aluminum parts are used to reduce fuel consumption, improve energy utilization and save manufacturing costs.
[0003] As one of the most commonly used cast aluminum parts, cast aluminum foundry parts encounter many difficulties in their actual processing: (1) It is difficult to determine the reference during processing, and plane alignment is time-consuming and laborious; (2) There are many pinholes, and the uneven cooling of aluminum water on complex functional curved surfaces leads to a high defective rate; (3) It is difficult to remove the residual stress inside the workpiece. The residual stress can cause deformation and cracking of the parts, affect the size of the parts, and reduce fatigue strength; (4) The processing performance is poor, and the cast aluminum foundry parts produced have low plasticity, poor corrosion resistance and poor welding performance. Summary of the invention
[0004] In order to overcome the above-mentioned defects of the existing aluminum casting foundry parts processing method, the present invention proposes a new aluminum casting foundry parts processing method for automobile inspection fixtures.
[0005] Specifically, the present invention provides a method for processing an automobile inspection fixture cast aluminum foundry part, such as Fig.14 As shown, the method comprises the following steps:
[0006] S1. Roughen the reverse side of the aluminum casting and confirm the roughing datum: determine the X, Y datum and Z margin of the aluminum casting, leave 10mm margin for each X and Y, drill the hoisting holes, and then select 5 times the height block to clamp the parts according to the height difference of the bracket;
[0007] S2. Test cutter and roughing on the front of cast aluminum foundry parts: repair X and Y datums on the front of cast aluminum foundry parts, check X and Y datums and test Z value to ensure that X and Y datums are consistent with the front station processing datums. During processing, firstly roughen 8mm locally, then use insert cutter to remove 0.5mm, and after confirming that there are no sand holes in the local roughing position, use insert cutter to continue roughing to 3mm; after roughing is completed, drill the hoisting holes, and then use equal height blocks to clamp the parts according to the height difference of the scaffold;
[0008] S3. Test and roughen the back of cast aluminum foundry parts: Use X, Y, and Z datums as the processing datums of the back station, test X, Y, and Z margins of 15mm to ensure that they are consistent with the processing datums of the front station; use a insert cutter to roughen to 3mm; remove the blank, process the back exhaust gate and process columns, and finally roughen the surface;
[0009] S4. After roughing, place it in a natural aging place for 24 hours to eliminate internal stress.
[0010] Furthermore, the processing method of the automobile inspection fixture cast aluminum foundry part of the present invention comprises step S1:
[0011] S11. According to the height of the scaffold, pad the cast aluminum foundry parts, find two scaffolds as the rough reference, use the dial indicator to level the straight line, and then choose one of the scaffolds as the reference;
[0012] S12. Roughly set the X and Y references of the aluminum casting: Press the workpiece with a pressure plate, use a sharp needle to determine the X and Y reference edges, and input them into the machine tool coordinate system;
[0013] S13. Determine the X and Y references of the aluminum casting;
[0014] S14. Determine the Z-direction allowance of the cast aluminum foundry parts, use a sharp needle to test the Z value, level the regular plane and the saddle, and then make the saddle a plane or mill it to a multiple of 5 according to the drop;
[0015] S15. Select a Φ16 processing reference, leave a 10mm margin on X and Y, drill the lifting holes, and then use equal height blocks to clamp the parts according to the height difference of the bracket.
[0016] Furthermore, the processing method of the automobile inspection fixture cast aluminum foundry part of the present invention comprises step S13:
[0017] S131. Use a Φ32 stainless steel knife to test the inner and outer contours and regular joints of the aluminum casting. Move the workpiece according to the test knife to re-determine the linear test workpiece margin. Reserve a 15mm margin on each side of the aluminum casting.
[0018] S132. When the test tool workpiece margin is more than 8mm, proceed with processing;
[0019] S133. When the workpiece allowance is less than 8mm during the test, adjust the workpiece until the workpiece allowance reaches more than 8mm for processing.
[0020] Furthermore, in the step S15 of the processing method for the automotive inspection fixture cast aluminum foundry part of the present invention, the depth of the hoisting hole is not less than 20 mm.
[0021] Furthermore, the processing method of the automobile inspection fixture cast aluminum foundry part of the present invention comprises step S2:
[0022] S21. Set the processing reference on the front of the cast aluminum foundry, and use the X and Y references as the processing references for the front station program;
[0023] S22. Use a Φ16 cutter to repair the straight line and X, Y datums, use the cutter to produce the auxiliary datum, and verify whether the repaired edge is correct to the test tool datum; use a dial indicator to verify the straight edge, record the deviation from the X, Y edge to the test tool datum, and input it into the machine tool coordinate system;
[0024] S23. Check the X and Y benchmarks, the inner and outer contours of the test workpiece and the regular laps. Use a Φ32 white steel knife and use a sharp needle to test the Z value to ensure that it is consistent with the front station benchmark;
[0025] S24. When processing the front side, first use a Φ63R6 insert cutter to roughen the area by 8mm, then use a Φ16R8 insert cutter to remove 0.5mm, and continue processing after confirming that there are no sand holes in the roughened area;
[0026] S25. Use Φ63R6 insert cutter to continue roughing to 3mm, feed 4000m / min;
[0027] S26. After the roughing is completed, the plane height difference of the light scaffold is a multiple of 5;
[0028] S27. Drill lifting holes, and then use equal height blocks to clamp the parts according to the height difference of the rack.
[0029] Furthermore, in the processing method of the automotive inspection fixture cast aluminum foundry part of the present invention, during the roughing process in step S25, check whether the blade is loose, worn, or the margin is too large, and if the above situation occurs, handle it immediately;
[0030] In step S27, the depth of the lifting hole is not less than 20 mm.
[0031] Furthermore, the processing method of the automobile inspection fixture cast aluminum foundry part of the present invention comprises step S3:
[0032] S31. Set the processing reference on the front of the cast aluminum foundry, and use the X, Y, and Z references as the processing references for the reverse station program;
[0033] S32. Test the cutter again, test the X, Y, and Z margins to 15 mm, and make sure they are consistent with the front station processing benchmark;
[0034] S33. Use Φ63R6 insert cutter to roughen to 3mm, feed 4000m / min;
[0035] S34. Remove the blank, first process the back exhaust gate, then process the process column, and finally open the rough surface.
[0036] Furthermore, the processing method of the automobile inspection fixture cast aluminum foundry part of the present invention adopts strong pressure to flatten the hoisting plane when performing front roughing, and after the roughing is completed, the reference bracket and the reference plane are repaired in the hoisting and pressing state.
[0037] Furthermore, the processing method of the automobile inspection fixture cast aluminum foundry parts of the present invention roughens the cast aluminum foundry parts on the front and back sides with a single side margin of 3mm, and roughens the semi-finished cast aluminum foundry parts on the front and back sides with a single side margin of 1mm, and then fine-processes them to zero position.
[0038] In summary, the processing method of the automobile inspection fixture cast aluminum foundry parts of the present invention can accurately and effectively perform benchmark positioning and plane verification, and can timely detect sand holes and remove residual stress inside the workpiece. The method has excellent processing performance and low defective rate. The cast aluminum foundry parts produced by the method have high plasticity, good corrosion resistance and welding performance. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments of the present invention. Obviously, the following drawings are only some embodiments recorded in the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative work.
[0040] Figure 1 The figure is a schematic diagram of a rough reference frame according to an embodiment of the present invention.
[0041] Figure 2 The figure is a schematic diagram of roughly determining X and Y references according to an embodiment of the present invention.
[0042] Figure 3 This is a schematic diagram of determining the X and Y references of a cast aluminum foundry part according to an embodiment of the present invention.
[0043] Figure 4 A schematic diagram of a processing and hoisting plane according to an embodiment of the present invention Figure 1 .
[0044] Figure 5 It is a schematic diagram of the depth (20mm) of the lifting hole of an embodiment of the present invention.
[0045] Figure 6 A schematic diagram of determining a machining reference for a trial shape according to an embodiment of the present invention.
[0046] Figure 7 It is a partially rough schematic diagram of an embodiment of the present invention.
[0047] Figure 8 This is a schematic diagram of determining whether a part has sand holes according to an embodiment of the present invention.
[0048] Fig. 9 The figure is a schematic diagram of a roughing tool path according to an embodiment of the present invention.
[0049] Fig.10 A schematic diagram of a processing and hoisting plane according to an embodiment of the present invention Figure 2 .
[0050] Fig.11 A schematic diagram of the processing hole depth according to an embodiment of the present invention.
[0051] Fig.12 A schematic diagram of a gate according to an embodiment of the present invention.
[0052] Fig.13 The figure is a schematic diagram of a back-side roughing tool path of an embodiment of the present invention.
[0053] Fig.14 The figure is a flow chart of the overall implementation of the method of the present invention. DETAILED DESCRIPTION
[0054] In order to make the purpose, technical solution and advantages of the present invention clearer, the technical solution of the present invention will be clearly and completely described below in conjunction with specific embodiments and corresponding drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. The present invention can also be implemented or applied through other different specific implementation methods. The details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.
[0055] At the same time, it should be understood that the protection scope of the present invention is not limited to the specific embodiments described below; it should also be understood that the terms used in the embodiments of the present invention are for describing specific embodiments rather than for limiting the protection scope of the present invention.
[0056] Embodiment: A method for processing aluminum castings of automobile inspection tools
[0057] 1. Roughing test on the reverse side of the cast aluminum foundry to confirm the roughing benchmark
[0058] 1. According to the height of the scaffold, pad the cast aluminum foundry parts, find two scaffolds as the rough reference, and use the dial indicator to level the straight line ( Figure 1 ), and then choose one of the pairs as the benchmark.
[0059] 2. Roughly set the X and Y references of cast aluminum foundry parts: Press the workpiece with the pressure plate, use a sharp needle to roughly determine the X and Y reference edges, and input them into the machine tool coordinate system ( Figure 2 ).
[0060] 3. Determine the X and Y references of the cast aluminum foundry parts and determine the Z value
[0061] (1) Determine the X and Y references of the cast aluminum foundry parts: Use a Φ32 white steel knife to test the inner and outer contours and regular laps of the cast aluminum foundry parts. Move the workpiece according to the test knife to re-determine the linear test workpiece allowance. A 15mm allowance is reserved on each side of the cast aluminum foundry parts ( Figure 3 ).
[0062] (2) If the workpiece margin is more than 8mm, it can be processed.
[0063] (3) If the workpiece allowance is less than 8 mm, adjust the workpiece until the workpiece allowance is more than 8 mm and then continue processing.
[0064] (4) If the adjustment is not done properly, the error will be too large and the workpiece will easily move and the tool will break during roughing. If the design model allows, the allowance that can be processed can be within 5mm.
[0065] 4. Determine the Z-direction allowance of the cast aluminum foundry parts, use a sharp needle to test the Z value, level the regular plane and the saddle, and then make the saddle a plane or mill it to a multiple of 5 according to the drop ( Figure 4 ).
[0066] 5. Select the Φ16 processing base, put 10mm margin on X and Y, and drill the M10 lifting hole with a depth of no less than 20mm ( Figure 5 ), and then select 5 times the height blocks to clamp the parts according to the height difference of the frame.
[0067] 2. Frontal testing and roughing of cast aluminum castings
[0068] 1. The datum is set on the front side. The X and Y datums are the processing datums of a station (front station) program.
[0069] 2. Use a Φ16 cutter to trim the straight line and X, Y datums, use the cutter to make the auxiliary datum, and check whether the trimmed edge is correct to the test tool datum. Use a dial indicator to check the straight edge, record the deviation from the X, Y edge to the test tool datum, and input it into the machine tool coordinate system.
[0070] 3. Check the benchmark, the inner and outer contours of the test workpiece and the regular laps. Use a Φ32 white steel knife and use a sharp needle to test the Z value to ensure that it is consistent with the benchmark of a station ( Figure 6 ).
[0071] 4. During front processing, determine whether the parts meet the requirements, check whether the parts have sand holes, and use a Φ63R6 insert cutter to perform local roughing 8mm ( Figure 7 ), then use a Φ16R8 insert knife to remove 0.5mm, if there is no sand hole in the local roughening position ( Figure 8 ), continue processing, otherwise return to the foundry.
[0072] 5. Use Φ63R6 insert cutter to roughen to 3mm ( Fig. 9 ), feed 4000m / min, check whether the blade is loose, worn, or the excess is too large during the roughing process. If any of the above conditions occur, deal with them immediately.
[0073] 6. After the roughing is completed, the plane height difference of the light scaffold is a multiple of 5 ( Fig.10).
[0074] 7. The depth of the M10 lifting hole should be no less than 20mm ( Fig.11 ), and then select equal height blocks to clamp the parts according to the height difference of the frame.
[0075] 3. Reverse cutting and roughing of cast aluminum castings
[0076] 1. The datum is set on the front side, and the X, Y, and Z datums are the datums for the second station (back station) program processing.
[0077] 2. Test the knife again, and try the X, Y, and Z margins of 15mm to ensure they are consistent with the front reference.
[0078] 3. Use Φ63R6 insert cutter to roughen to 3mm, feed 4000m / min.
[0079] 4. Maximize the removal of blanks and first process the exhaust gate on the reverse side ( Fig.12 ), then process the column to prevent uneven cutting and finally open the rough surface ( Fig.13 ).
[0080] 4. Process Optimization Results
[0081] 1. When roughing the front surface, do not manually pad or trim the hoisting surface, but use strong pressure to flatten it. After the roughing is completed, repair the reference bracket and reference plane under the hoisting and pressing state.
[0082] 2. After roughing, place it in a natural aging place for 24 hours to eliminate internal stress.
[0083] 3. Large aluminum castings follow the 3-1-0 principle. For aluminum castings, the first and second stations should leave a 3mm margin on one side for roughing. For semi-finished aluminum castings, the first and second stations should leave a 1mm margin on one side for roughing. Finishing to zero position can meet product quality requirements.
[0084] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Any technician familiar with the profession can make some changes or modifications to the technical contents disclosed above without departing from the scope of the technical solution of the present invention to obtain equivalent embodiments of equivalent changes. However, any simple modification, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention should be included in the scope of protection of the claims of the present invention.
Claims
1. A processing method for aluminum casting parts of automobile inspection fixtures. It is characterized in that The method comprises: S1. Roughen the reverse side of the aluminum casting and confirm the roughing datum: determine the X, Y datum and Z margin of the aluminum casting, leave 10mm margin for each X and Y, drill the hoisting holes, and then select 5 times the height block to clamp the parts according to the height difference of the bracket; S2. Test cutter and roughing on the front of cast aluminum foundry parts: repair X and Y datums on the front of cast aluminum foundry parts, check X and Y datums and test Z value to ensure that X and Y datums are consistent with the front station processing datums. During processing, firstly roughen 8mm locally, then use insert cutter to remove 0.5mm, and after confirming that there are no sand holes in the local roughing position, use insert cutter to continue roughing to 3mm; after roughing is completed, drill the hoisting holes, and then use equal height blocks to clamp the parts according to the height difference of the scaffold; S3. Test and roughen the back of cast aluminum foundry parts: Use X, Y, and Z datums as the processing datums of the back station, test X, Y, and Z margins of 15mm to ensure that they are consistent with the processing datums of the front station; use a insert cutter to roughen to 3mm; remove the blank, process the back exhaust gate and process columns, and finally roughen the surface; S4. After roughing, place it in a natural aging place for 24 hours to eliminate internal stress.
2. The method for processing the aluminum casting of automobile inspection fixture according to claim 1, It is characterized in that Step S1 includes: S11. According to the height of the scaffold, pad the cast aluminum foundry parts, find two scaffolds as the rough reference, use the dial indicator to level the straight line, and then choose one of the scaffolds as the reference; S12. Roughly set the X and Y references of the aluminum casting: Press the workpiece with a pressure plate, use a sharp needle to determine the X and Y reference edges, and input them into the machine tool coordinate system; S13. Determine the X and Y references of the aluminum casting; S14. Determine the Z-direction allowance of the cast aluminum foundry parts, use a sharp needle to test the Z value, level the regular plane and the saddle, and then make the saddle a plane or mill it to a multiple of 5 according to the drop; S15. Select a Φ16 processing reference, leave a 10mm margin on X and Y, drill the lifting holes, and then use equal height blocks to clamp the parts according to the height difference of the bracket.
3. The method for processing the aluminum casting of automobile inspection fixture according to claim 2, It is characterized in that Step S13 includes: S131. Use a Φ32 stainless steel knife to test the inner and outer contours and regular joints of the aluminum casting. Move the workpiece according to the test knife to re-determine the linear test workpiece margin. Reserve a 15mm margin on each side of the aluminum casting. S132. When the test tool workpiece margin is more than 8mm, proceed with processing; S133. When the workpiece allowance is less than 8mm during the test, adjust the workpiece until the workpiece allowance reaches more than 8mm for processing.
4. The method for processing the aluminum casting of automobile inspection fixture according to claim 2, It is characterized in that In step S15, the depth of the lifting hole is not less than 20 mm.
5. The method for processing the aluminum casting of automobile inspection fixture according to claim 1, It is characterized in that Step S2 includes: S21. Set the processing reference on the front of the cast aluminum foundry, and use the X and Y references as the processing references for the front station program; S22. Use a Φ16 cutter to repair the straight line and X, Y datums, use the cutter to produce the auxiliary datum, and verify whether the repaired edge is correct to the test tool datum; use a dial indicator to verify the straight edge, record the deviation from the X, Y edge to the test tool datum, and input it into the machine tool coordinate system; S23. Check the X and Y benchmarks, the inner and outer contours of the test workpiece and the regular laps. Use a Φ32 white steel knife and use a sharp needle to test the Z value to ensure that it is consistent with the front station benchmark; S24. When processing the front side, first use a Φ63R6 insert cutter to roughen the area by 8mm, then use a Φ16R8 insert cutter to remove 0.5mm, and continue processing after confirming that there are no sand holes in the roughened area; S25. Use Φ63R6 insert cutter to continue roughing to 3mm, feed 4000m / min; S26. After the roughing is completed, the plane height difference of the light scaffold is a multiple of 5; S27. Drill lifting holes, and then use equal height blocks to clamp the parts according to the height difference of the rack.
6. The method for processing the aluminum casting of automobile inspection fixture according to claim 5, It is characterized in that During the roughing process in step S25, check whether the blade is loose, worn, or has too much excess. If any of the above conditions are found, handle them immediately; In step S27, the depth of the lifting hole is not less than 20 mm.
7. The method for processing the aluminum casting of automobile inspection fixture according to claim 1, It is characterized in that Step S3 includes: S31. Set the processing reference on the front of the cast aluminum foundry, and use the X, Y, and Z references as the processing references for the reverse station program; S32. Test the cutter again, test the X, Y, and Z margins to 15 mm, and make sure they are consistent with the front station processing benchmark; S33. Use Φ63R6 insert cutter to roughen to 3mm, feed 4000m / min; S34. Remove the blank, first process the back exhaust gate, then process the process column, and finally open the rough surface.
8. The method for processing the aluminum casting of automobile inspection fixture according to claim 1, It is characterized in that The method adopts strong pressure to flatten the hoisting plane when performing front roughing, and after the roughing is completed, the reference bracket and the reference plane are repaired in the hoisting and pressing state.
9. The method for processing the aluminum casting of automobile inspection fixture according to claim 1, It is characterized in that The method comprises the following steps: roughing the front and back surfaces of the cast aluminum foundry piece with a single side margin of 3 mm, roughing the front and back surfaces of the semi-finished aluminum foundry piece with a single side margin of 1 mm, and finishing the work to zero position.
Citation Information
Patent Citations
Design of tool for machining cast-in rib plate
CN105666188A
Machining deformation control method for weakly-rigid aviation structure members
CN108214002A
Metal middle frame processing method and metal middle frame
CN110369951A
Frame section part machining method
CN116021234A
Work finishing device
JP1998058283A