Rust paint preparation and application method and system based on stable rust layer

By preparing stable rust layer rust paint and building an automated application system, the problems of complex processes, high costs and human body hazards in the existing technology are solved, and efficient and low-cost automated rust paint application is realized, which improves the effect of imitating rust Authenticity and consistency.

CN118895059APending Publication Date: 2024-11-05SHENZHEN NO 1 HARDWARE MATERIALS CO LTD

Patent Information

Application Number
CN202410938323.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-13
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

When the prior art achieves the effect of iron rust and aging, the process is complex, high cost and polluted, which is harmful to the human body, and the surface imitation rust effect is unreal, and there is a lack of automated application methods.

Method used

By obtaining aqueous paint solution and iron oxide, combining acetic acid solution, a stable rust layer rust paint is prepared by using stirring, drying and spraying technologies, and building an automated application system to realize automatic coating and spraying of rust paint to ensure the stability of rust layer Sex and consistency.

Benefits of technology

The automated application of rusty paint is realized, which reduces process complexity and cost, improves the authenticity and consistency of the surface imitation rust effect, avoids human body harm, and improves production efficiency and product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118895059A_ABST
    Figure CN118895059A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of rusty paint and application thereof, in particular to a rusty paint preparation and application method and system based on a stable rust layer, and the method comprises the steps of obtaining a water paint solution and ferric oxide, obtaining a first mixed material based on the ferric oxide and the water paint solution, and obtaining an acetic acid solution and a copper sulfate solution; acquiring a second mixed material based on the copper sulfate solution and the acetic acid solution, acquiring a to-be-coated product by utilizing the coating unit, acquiring a coating track according to the to-be-coated product, acquiring a coated product according to the coating track and the first mixed material, and drying the coated product by utilizing the drying unit to obtain a dried product. And a spraying unit and a second mixed material are used for spraying the dried product, a sprayed product is obtained, and preparation and application of the rusty paint with the stable rust layer are completed based on the sprayed product. The preparation method of the rusty paint can be provided, and the rusty paint can be effectively and automatically applied through multiple detection methods.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of rust paint and its application, and in particular to a preparation and application method, system, electronic device and computer-readable storage medium of rust paint based on a stable rust layer. Background Art

[0002] Most of the methods on the market need to achieve the effect of rusting and aging iron. The first kind of real raw iron rust effect is mostly made of iron plates or weathering steel. If a real rust effect is required, it must be made by spraying salt water or special rusting liquid.

[0003] In the above method, the process is complicated, the cost is high, there is pollution, it is harmful to the human body, and the surface has the effect of imitating rust. Therefore, a rust paint with a stable rust layer is needed, and in the spraying process, the degree of automation is increased as much as possible. Summary of the invention

[0004] The present invention provides a method for preparing and applying a rust paint based on a stable rust layer and a computer-readable storage medium, the main purpose of which is to provide a method for preparing a rust paint and enable the rust paint to be effectively and automatically applied through a variety of detection methods.

[0005] To achieve the above-mentioned purpose, the present invention provides a method for preparing and applying a rust-resistant paint based on a stable rust layer, comprising:

[0006] Obtaining a water-based paint solution, wherein the solute in the water-based paint solution is water-based paint, the solution is pure water, and the ratio between the mass of the water-based paint and the mass of the pure water is 2:3;

[0007] Obtaining a solution mass based on a water-based paint solution, obtaining an iron oxide mass based on the solution mass, obtaining iron oxide corresponding to the iron oxide mass based on the iron oxide mass, introducing the iron oxide and the water-based paint solution into a pre-constructed stirring unit to obtain a material to be stirred, and performing a stirring operation on the material to be stirred using a pre-constructed stirring method and a stirring unit to obtain a first mixed material, wherein the iron oxide mass is numerically equal to the solution mass;

[0008] Obtaining an acetic acid solution, obtaining a copper sulfate solution based on a preset copper sulfate mass, and introducing the copper sulfate solution and the acetic acid solution into a stirring unit to obtain a second mixed material, wherein the acetic acid solution includes acetic acid and pure water, the copper sulfate solution includes copper sulfate and pure water, and the mass ratio of the mass of acetic acid, the mass of copper sulfate, and the mass of pure water is 3:5:42;

[0009] Acquire a plurality of first test blocks based on the first mixed material, wherein a pre-constructed test area in the first test block is uniformly coated with the first mixed material of a preset thickness, and construct a first drying scheme using a pre-constructed drying unit and the plurality of first test blocks;

[0010] Using a pre-built coating unit to obtain a product to be coated, obtaining a coating trajectory according to the product to be coated, and performing a coating operation on the object to be coated according to the coating trajectory and the first mixed material to obtain a coated product;

[0011] Performing a drying operation on the coated product using a drying unit and a first drying scheme to obtain a dried product;

[0012] The dried product is sprayed using a pre-built spray unit and a second mixed material to obtain a sprayed product, and the rust paint for stabilizing the rust layer is prepared and applied based on the sprayed product.

[0013] Optionally, the first mixed material is obtained by performing a stirring operation on the material to be stirred using the pre-established stirring method and stirring unit, comprising:

[0014] Acquire a stirring sample set based on the material to be stirred, wherein the stirring sample set includes a plurality of unit sample sets, the unit sample set includes a plurality of unit samples, the ratio of the mass of the material to be stirred to the mass of the tracer corresponding to the unit samples in all the unit sample sets is the same, and the mass of the unit samples in the same unit sample set is the same, while the mass of the unit samples in different unit sample sets is different;

[0015] Extract unit sample sets from the stirred sample set in sequence, and perform the following operations on the extracted unit sample sets:

[0016] Based on the stirring unit, a stirring speed sequence and a stirring time sequence are obtained, wherein the stirring speed sequence is a sequence in which the stirring speeds are arranged from small to large, and the stirring time sequence is a sequence in which the stirring time is arranged from short to long;

[0017] Based on the extracted unit sample set, the stirring speed sequence and the stirring time sequence, multiple stirring schemes are constructed, wherein the stirring scheme includes: unit sample, stirring speed and stirring time, stirring schemes are sequentially extracted from the multiple stirring schemes, and the following operations are performed on the extracted stirring schemes:

[0018] Extracting unit sample, stirring speed and stirring time based on the extracted stirring scheme;

[0019] The extracted unit sample is introduced into the stirring unit, and a pre-built stirrer in the stirring unit is started based on the stirring time and the stirring speed, and the stirrer performs a stirring operation on the unit sample to obtain a sample to be tested;

[0020] Calculating the tracer volume error of the tracer in the test sample based on the test sample and a pre-constructed volume fraction calculation formula, comparing the tracer volume error with a preset tracer error threshold, and confirming that the tracer volume error is less than or equal to the tracer error threshold, confirming that the extracted stirring scheme is a valid stirring scheme;

[0021] Aggregate multiple effective mixing schemes to obtain a unit effective mixing scheme set;

[0022] A plurality of effective stirring scheme sets corresponding to the stirring sample set are summarized to obtain a stirring data set, a stirring model is constructed based on the stirring data set, an optimal stirring scheme is obtained using the stirring model, and a stirring operation is performed on the material to be stirred using the optimal stirring scheme and the stirring unit to obtain a first mixed material.

[0023] Optionally, the step of calculating a tracer volume error of a tracer in the test sample based on the test sample and a pre-constructed volume fraction calculation formula, comparing the tracer volume error with a preset tracer error threshold, and confirming that the tracer volume error is less than or equal to the tracer error threshold, and then confirming that the extracted stirring scheme is a valid stirring scheme comprises:

[0024] Obtaining an initial sample volume and an initial tracer volume based on the extracted unit sample;

[0025] The volume of the sample to be tested and the stirring tracer volume are obtained based on the sample to be tested, and the tracer volume error of the extracted stirring scheme is calculated based on the initial sample volume, the initial tracer volume, the volume of the sample to be tested, the stirring tracer volume and the volume fraction calculation formula, wherein the volume fraction calculation formula is:

[0026]

[0027] Where ΔV represents the tracer volume error of the extracted stirring scheme, V1 represents the initial tracer volume, and V a1 represents the initial sample volume, V2 represents the stirring tracer volume, V a2 Indicates the volume of the sample to be tested, |*| indicates taking the absolute value;

[0028] comparing the tracer volume error with a tracer error threshold;

[0029] If the tracer volume error is greater than the tracer error threshold, the extracted stirring scheme is confirmed to be an invalid scheme, and the extracted stirring scheme is discarded;

[0030] If the tracer volume error is less than or equal to the tracer error threshold, the extracted stirring scheme is confirmed to be a valid scheme, and the extracted stirring scheme is confirmed to be a valid stirring scheme.

[0031] Optionally, constructing a first drying scheme using a pre-built drying unit and a plurality of first test blocks includes:

[0032] Extracting first test blocks from the multiple first test blocks in sequence, and performing the following operations on each of the extracted first test blocks:

[0033] Obtaining the test block mass and the coated test block mass of the extracted first test block, wherein the test block mass is the mass of the test area when it is not coated with the first mixed material, and the coated test block mass is the mass of the test area when it is uniformly coated with the first mixed material of a preset thickness, and calculating the undried material mass according to the test block mass and the coated test block mass, wherein the undried material mass is the difference between the coated test block mass and the test block mass;

[0034] Importing the extracted first test block into a drying unit, and acquiring a drying time based on the drying unit, wherein the drying time includes a first drying time and a second drying time;

[0035] The target time is extracted based on the drying time, and the following operations are performed on the extracted target time:

[0036] Determine a target wind speed according to the extracted target time, and perform a drying operation on the extracted first test block using the target wind speed and the target time to obtain a dried sample;

[0037] The mass of the dried block is obtained based on the dried sample, the drying rate is calculated based on the mass of the dried block, and after confirming that the measured drying rate is within a preset target drying rate range, a surface image of the dried sample is obtained using a pre-constructed image unit, and after confirming that the dried sample is effectively dried based on the surface image, an initial drying scheme corresponding to the extracted first test block is obtained;

[0038] A plurality of initial drying schemes are aggregated to obtain an initial drying scheme set, and a first drying scheme is constructed based on the initial drying scheme set.

[0039] Optionally, obtaining the mass of the dried block based on the drying sample and calculating and measuring the drying rate according to the mass of the dried block include:

[0040] The drying rate is calculated based on the mass of the coated test block and the mass of the dried block, wherein the calculation formula of the drying rate is as follows:

[0041]

[0042] Among them, ΔC represents the measured drying rate, C0 represents the mass of the coated test block, C1 represents the mass of the dried block, and C δ Indicates the mass of undried material.

[0043] Optionally, after confirming that the measured drying rate is within a preset target drying rate range, the method further comprises:

[0044] Obtaining a lower limit and an upper limit of a drying rate based on a target drying rate interval, and determining whether the measured drying rate is within the target drying rate interval;

[0045] If the measured drying rate is less than the target drying rate lower limit, the extended drying time is obtained, and after confirming that the extended drying time is the target time, the step of performing the drying operation on the extracted first test block with the target wind speed and the target time is returned to until it is confirmed that the measured drying rate is within the preset target drying rate range;

[0046] If the measured drying rate is greater than the upper limit of the drying rate, then the time period corresponding to the extracted target time is confirmed based on the extracted target time, if the time period corresponding to the extracted target time is the first drying time, the shortened drying time is obtained, and the corrected second drying time is obtained based on the shortened drying time and the second drying time. After confirming that the corrected second drying time is the target time, the process returns to the step of performing the drying operation on the extracted first test block using the target wind speed and the target time, otherwise, the drying sample is confirmed to be an invalid sample;

[0047] If the measured drying rate is within the target drying rate interval, it is confirmed that the measured drying rate is within the preset target drying rate interval.

[0048] Optionally, after confirming that the dried sample is effectively dried based on the surface image, the method further comprises:

[0049] A grayscale operation is performed on the surface image to obtain a grayscale image, a grayscale image matrix is ​​obtained using a pre-constructed image coordinate system and the grayscale image, the grayscale image matrix is ​​divided based on a preset window size to obtain a grayscale block matrix, block matrices are extracted from the grayscale block matrix in sequence, and the following operations are performed on the extracted block matrices:

[0050] Based on the extracted block matrix, a maximum grayscale value and a minimum grayscale value in the extracted block matrix are obtained, and a grayscale difference value is calculated based on the maximum grayscale value and the minimum grayscale value;

[0051] Compare the grayscale difference with the preset defect threshold;

[0052] If the grayscale difference is greater than the defect threshold, confirm that the area corresponding to the block matrix corresponding to the grayscale difference in the grayscale image is a defect area, otherwise, confirm that the area corresponding to the block matrix corresponding to the grayscale difference in the grayscale image is a regular area;

[0053] Summarize the defective areas to obtain a defective area set, and determine whether the defective area set is an empty set. If the defective area set is an empty set, confirm that the dried sample is effectively dried; otherwise, confirm that the dried sample is an invalid sample.

[0054] Optionally, the using a pre-built coating unit to obtain a product to be coated, and obtaining a coating trajectory according to the product to be coated, includes:

[0055] Acquire a product set based on the coating unit, and extract a product set to be modeled from the product set in sequence, wherein the product set includes multiple product sets to be modeled, each of the multiple product sets to be modeled is of a different type, and the product set to be modeled includes multiple products, and the multiple products are of the same type;

[0056] Extracting products to be coated from a set of products to be modeled, and introducing the products to be coated into a coating unit;

[0057] Acquire volume data of the product to be coated based on the product set to be modeled, wherein the volume data includes product height, product width and product length of the product to be coated;

[0058] The moving trajectory and moving step length of the laser emitter are obtained according to the volume data and the pre-built laser emitter, the moving trajectory is divided into a plurality of unit detection points by using the moving step length, unit detection points are sequentially extracted from the plurality of unit detection points, and the following operations are performed on the extracted unit detection points:

[0059] A plurality of laser emission angle pairs are acquired based on a unit detection point, wherein each of the plurality of laser emission angle pairs is different, and the laser emission angle pairs include: a horizontal emission angle and a vertical emission angle, and the laser emission angle pairs are sequentially extracted from the plurality of laser emission angle pairs, and the following operations are performed on the extracted laser emission angle pairs:

[0060] Using the laser transmitter located at the extracted unit detection point and the extracted laser emission angle to emit a pulse laser to the product to be coated, the laser emission time is obtained, the laser transmitter receives the emitted pulse laser, the laser reception time is obtained, the laser flight distance is calculated based on the laser emission time and the laser reception time, and the three-dimensional point data corresponding to the extracted unit detection point is obtained based on the laser flight distance and the pre-constructed coordinate point calculation formula;

[0061] Aggregate multiple 3D point data corresponding to multiple unit detection points to obtain a 3D point data set;

[0062] A coating model corresponding to the product to be coated is spliced ​​out based on the three-dimensional point data set, and a coating trajectory is obtained based on the coating model.

[0063] Optionally, the step of obtaining three-dimensional point data corresponding to the extracted unit detection point based on the laser flight distance and a pre-constructed coordinate point calculation formula includes:

[0064] Obtain the coordinate point calculation formula, and calculate the model horizontal coordinate, model vertical coordinate, and model vertical coordinate corresponding to the extracted unit detection point based on the coordinate point formula. The unit detection point of the pulsed laser emitted by the laser transmitter is the origin of the pre-constructed spatial coordinate system. The coordinate point calculation formula is as follows:

[0065]

[0066] Wherein, x represents the model horizontal coordinate in the spatial coordinate system, y represents the model vertical coordinate in the spatial coordinate system, and xoy represents the plane parallel to the ground in the spatial coordinate system, z represents the model vertical coordinate perpendicular to the ground in the spatial coordinate system, s represents the laser flight distance, β represents the vertical emission angle in the laser emission angle pair, and the vertical emission angle is the angle between the pulse laser and the direction perpendicular to the ground, α represents the horizontal emission angle in the laser emission angle pair, and the horizontal emission angle is the angle between the pulse laser and the plane parallel to the ground;

[0067] Based on the model horizontal coordinate, the model vertical coordinate and the model vertical coordinate, the three-dimensional point coordinate corresponding to the extracted unit detection point is obtained, wherein the three-dimensional point coordinate is: (x, y, z);

[0068] The geodetic detection coordinates of the extracted unit detection points are obtained using a pre-constructed geodetic coordinate system, and three-dimensional point data are obtained based on the three-dimensional point coordinates, wherein the three-dimensional point data includes: a geodetic coordinate system, geodetic detection coordinates, a spatial coordinate system and three-dimensional point coordinates.

[0069] To achieve the above object, the present invention also provides a rust-resistant paint preparation and application system based on a stable rust layer, comprising:

[0070] A first mixed material acquisition module is used to obtain a water-based paint solution, wherein the solute in the water-based paint solution is water-based paint, the solution is pure water, and the ratio between the mass of the water-based paint and the mass of the pure water is 2:3;

[0071] Obtaining a solution mass based on a water-based paint solution, obtaining an iron oxide mass based on the solution mass, obtaining iron oxide corresponding to the iron oxide mass based on the iron oxide mass, introducing the iron oxide and the water-based paint solution into a pre-constructed stirring unit to obtain a material to be stirred, and performing a stirring operation on the material to be stirred using a pre-constructed stirring method and a stirring unit to obtain a first mixed material, wherein the iron oxide mass is numerically equal to the solution mass;

[0072] A second mixed material module is used to obtain an acetic acid solution, obtain a copper sulfate solution based on a preset copper sulfate mass, and introduce the copper sulfate solution and the acetic acid solution into a stirring unit to obtain a second mixed material, wherein the acetic acid solution includes acetic acid and pure water, the copper sulfate solution includes copper sulfate and pure water, and the mass ratio of the acetic acid mass, the copper sulfate mass and the pure water is 3:5:42;

[0073] A coating module, configured to obtain a plurality of first test blocks based on a first mixed material, wherein a pre-constructed test area in the first test block is uniformly coated with the first mixed material of a preset thickness, and construct a first drying scheme using a pre-constructed drying unit and the plurality of first test blocks;

[0074] Using a pre-built coating unit to obtain a product to be coated, obtaining a coating trajectory according to the product to be coated, and performing a coating operation on the object to be coated according to the coating trajectory and the first mixed material to obtain a coated product;

[0075] Performing a drying operation on the coated product using a drying unit and a first drying scheme to obtain a dried product;

[0076] The spraying module is used to perform a spraying operation on the dried product using a pre-built spraying unit and a second mixed material to obtain a sprayed product, and to complete the preparation and application of a rust paint for stabilizing the rust layer based on the sprayed product.

[0077] In order to solve the above problem, the present invention further provides an electronic device, the electronic device comprising:

[0078] a memory storing at least one instruction; and

[0079] The processor executes the instructions stored in the memory to implement the above-mentioned method for preparing and applying rust paint based on a stable rust layer.

[0080] In order to solve the above problems, the present invention also provides a computer-readable storage medium, in which at least one instruction is stored. The at least one instruction is executed by a processor in an electronic device to implement the above-mentioned method for preparing and applying rust paint based on a stable rust layer.

[0081] The present invention is to solve the problem described in the background technology. The present invention obtains a water-based paint solution, obtains a solution mass based on the water-based paint solution, obtains an iron oxide mass according to the solution mass, obtains an iron oxide corresponding to the iron oxide mass based on the iron oxide mass, introduces the iron oxide and the water-based paint solution into a pre-constructed stirring unit, obtains a material to be stirred, uses a pre-constructed stirring method and a stirring unit to perform a stirring operation on the material to be stirred, obtains a first mixed material, obtains an acetic acid solution, obtains a copper sulfate solution based on a preset copper sulfate mass, and introduces the copper sulfate solution and the acetic acid solution into the stirring unit to obtain a second mixed material. Therefore, the embodiment of the present invention can use the stirring unit to predict the stirring time and stirring speed required for the material to be stirred when performing the stirring operation, thereby constructing a stirring method to perform a stirring operation on the material to be stirred. Based on the first mixed material, multiple first test blocks are obtained, and a first drying scheme is constructed using a pre-constructed drying unit and multiple first test blocks. In the embodiment of the present invention, a reasonable first drying scheme is formulated to avoid excessive drying temperature and excessive drying rate, which may cause pinhole-shaped defects on the surface, and avoid incomplete drying. A product to be coated is obtained by using a pre-constructed coating unit, a coating trajectory is obtained according to the product to be coated, a coating operation is performed on the object to be coated according to the coating trajectory and the first mixed material to obtain a coated product, a drying operation is performed on the coated product by using a drying unit and a first drying scheme to obtain a dried product, a spraying operation is performed on the dried product by using a pre-constructed spraying unit and a second mixed material to obtain a sprayed product, and the preparation and application of rust paint with a stable rust layer is completed based on the sprayed product. The embodiment of the present invention constructs a model of the product to be coated, and can be directly implemented by a computer in a variety of tests, so that the application of the first mixed material and the second mixed material can be completed for the same type of product through the same steps, and further, mass production can be achieved. Therefore, the present invention provides a method for preparing rust paint and enables the rust paint to be effectively and automatically applied through a variety of detection methods. BRIEF DESCRIPTION OF THE DRAWINGS

[0082] Figure 1 A schematic flow chart of a method for preparing and applying a rust paint based on a stable rust layer provided by an embodiment of the present invention;

[0083] Figure 2 A functional module diagram of a rust paint preparation and application system based on a stable rust layer provided by an embodiment of the present invention;

[0084] Figure 3 A schematic structural diagram of an electronic device for implementing the method for preparing and applying rust paint based on a stable rust layer provided in one embodiment of the present invention.

[0085] The realization of the purpose, functional features and advantages of the present invention will be further explained in conjunction with embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION

[0086] It should be understood that the specific embodiments described herein are only used to explain the present invention, and are not used to limit the present invention.

[0087] The embodiment of the present application provides a method for preparing and applying a rust paint based on a stable rust layer. The execution subject of the method for preparing and applying a rust paint based on a stable rust layer includes but is not limited to at least one of the electronic devices such as a server and a terminal that can be configured to execute the method provided in the embodiment of the present application. In other words, the method for preparing and applying a rust paint based on a stable rust layer can be executed by software or hardware installed on a terminal device or a server device, and the software can be a blockchain platform. The server includes but is not limited to: a single server, a server cluster, a cloud server or a cloud server cluster, etc.

[0088] Reference Figure 1 FIG. 1 is a flow chart of a method for preparing and applying a rust paint based on a stable rust layer according to an embodiment of the present invention. In this embodiment, the method for preparing and applying a rust paint based on a stable rust layer includes:

[0089] S1. Obtain a water-based paint solution, obtain a solution mass based on the water-based paint solution, obtain an iron oxide mass based on the solution mass, obtain iron oxide corresponding to the iron oxide mass based on the iron oxide mass, introduce the iron oxide and the water-based paint solution into a pre-constructed stirring unit to obtain a material to be stirred, and perform a stirring operation on the material to be stirred using a pre-constructed stirring method and a stirring unit to obtain a first mixed material.

[0090] Furthermore, the solute in the water-based paint solution is water-based paint, the solution is pure water, and the ratio between the mass of the water-based paint and the mass of the pure water is 2:3;

[0091] Specifically, the mass of the iron oxide is numerically equal to the mass of the solution.

[0092] It is understandable that the embodiment of the present invention does not limit the composition of the water-based paint, and the water-based paint in the embodiment of the present invention is a water-based paint that can be purchased. The water-based paint solution is a solution including water-based paint and pure water. The embodiment of the present invention limits the mass ratio between water-based paint and pure water, but the pure water here does not include the water content of the water-based paint itself. The solution mass is the mass of the water-based paint solution, and the iron oxide mass is the mass of the iron oxide. For example, if there are 2kg of water-based paint and 3kg of pure water, 5kg of iron oxide is obtained, and 2kg of water-based paint, 3kg of pure water and 5kg of iron oxide are introduced into the stirring unit to obtain the material to be stirred. In the embodiment of the present invention, water-based paint is used as a supporting carrier in order to protect the product that needs to be coated with the first mixed material.

[0093] It should be noted that the material to be stirred is the material that has not been stirred after the iron oxide and the water-based paint solution are introduced into the stirring unit. The stirring unit is a unit for stirring the material in the stirring unit. Optionally, the stirring unit is provided with a stirrer, and the stirrer can perform a stirring operation on the material introduced into the stirring unit. The first mixed material is the material obtained after the material to be stirred is fully stirred by the stirrer.

[0094] Furthermore, the first mixed material is obtained by performing a stirring operation on the material to be stirred using the pre-constructed stirring method and stirring unit, including:

[0095] Acquire a stirring sample set based on the material to be stirred, wherein the stirring sample set includes a plurality of unit sample sets, the unit sample set includes a plurality of unit samples, the ratio of the mass of the material to be stirred to the mass of the tracer corresponding to the unit samples in all the unit sample sets is the same, and the mass of the unit samples in the same unit sample set is the same, while the mass of the unit samples in different unit sample sets is different;

[0096] Extract unit sample sets from the stirred sample set in sequence, and perform the following operations on the extracted unit sample sets:

[0097] Based on the stirring unit, a stirring speed sequence and a stirring time sequence are obtained, wherein the stirring speed sequence is a sequence in which the stirring speeds are arranged from small to large, and the stirring time sequence is a sequence in which the stirring time is arranged from short to long;

[0098] Based on the extracted unit sample set, the stirring speed sequence and the stirring time sequence, multiple stirring schemes are constructed, wherein the stirring scheme includes: unit sample, stirring speed and stirring time, stirring schemes are sequentially extracted from the multiple stirring schemes, and the following operations are performed on the extracted stirring schemes:

[0099] Extracting unit sample, stirring speed and stirring time based on the extracted stirring scheme;

[0100] The extracted unit sample is introduced into the stirring unit, and a pre-built stirrer in the stirring unit is started based on the stirring time and the stirring speed, and the stirrer performs a stirring operation on the unit sample to obtain a sample to be tested;

[0101] Calculating the tracer volume error of the tracer in the test sample based on the test sample and a pre-constructed volume fraction calculation formula, comparing the tracer volume error with a preset tracer error threshold, and confirming that the tracer volume error is less than or equal to the tracer error threshold, confirming that the extracted stirring scheme is a valid stirring scheme;

[0102] Aggregate multiple effective mixing schemes to obtain a unit effective mixing scheme set;

[0103] A plurality of effective stirring scheme sets corresponding to the stirring sample set are summarized to obtain a stirring data set, a stirring model is constructed based on the stirring data set, an optimal stirring scheme is obtained using the stirring model, and a stirring operation is performed on the material to be stirred using the optimal stirring scheme and the stirring unit to obtain a first mixed material.

[0104] It can be understood that the unit sample is a sample used to construct a stirring model, and the unit sample includes a material to be stirred and a tracer, and the ratio between the iron oxide and the water-based paint solution in the unit sample is 2:3. Exemplarily, the material to be stirred in the embodiment of the present invention is a mixed material of 2kg of water-based paint, 3kg of pure water and 5kg of iron oxide, then the unit sample is: 200g of water-based paint, 300g of pure water, 500g of iron oxide and ag of tracer, that is, in the embodiment of the present invention, multiple mixed materials with the same composition as the material to be stirred are constructed, and tracers are added to the multiple mixed materials, thereby constituting a unit sample, and if the tracer in the unit sample does not affect the stirring effect.

[0105] It should be noted that, according to the stirring sample set, the embodiment of the present invention uses unit samples of different masses to construct a stirring model under different stirring times and stirring speeds, so that the stirring time and stirring speed required for the material to be stirred when performing the stirring operation can be predicted.

[0106] For example, take a plurality of unit samples with a total weight of 100g, a plurality of unit samples with a total weight of 200g, and a plurality of unit samples with a total weight of 300g, respectively, the stirring speed sequence is a (rad / min), b (rad / min), and c (rad / min), and the stirring time sequence is 100s, 150s, and 200s, then the stirring schemes that can be formed are: stirring 100g unit sample at a stirring speed of a (rad / min) for 100s, stirring 100g unit sample at a stirring speed of a (rad / min) for 150s, stirring 100g unit sample at a stirring speed of a (rad / min) for 200s, ..., stirring 100g unit sample at a stirring speed of c (rad / min) for 200s, ..., stirring 300g unit sample at a stirring speed of c (rad / min) for 200s, and so on, no more examples are given here. And so on, no more details are given here. Therefore, after determining that the extracted stirring scheme is an effective stirring scheme, a stirring model can be obtained according to a plurality of unit effective stirring scheme sets.

[0107] Furthermore, the effective stirring scheme is a scheme that can fully stir the unit sample. The optimal stirring scheme is a scheme that is obtained according to the stirring model and is suitable for stirring the material to be stirred. The characteristics of the optimal stirring scheme are: short stirring time, lowest stirring speed, and the tracer volume error is less than or equal to the tracer error threshold.

[0108] It should be noted that the reason why the effective stirring scheme cannot be directly used to perform stirring operations on the material to be stirred is that the embodiment of the present invention takes proportionally smaller samples when constructing the unit sample. Therefore, the effective stirring scheme cannot be directly applied to the material to be stirred, but the optimal stirring scheme suitable for the material to be stirred can be predicted from the stirring model.

[0109] It is understandable that after the mass of the material to be stirred is input into the stirring model, an optimal stirring scheme that can fully stir the material to be stirred can be obtained.

[0110] Furthermore, the tracer volume error of the tracer in the test sample is calculated based on the test sample and the pre-constructed volume fraction calculation formula, the tracer volume error is compared with a preset tracer error threshold, and after confirming that the tracer volume error is less than or equal to the tracer error threshold, the extracted stirring scheme is confirmed to be a valid stirring scheme, including:

[0111] Obtaining an initial sample volume and an initial tracer volume based on the extracted unit sample;

[0112] The volume of the sample to be tested and the stirring tracer volume are obtained based on the sample to be tested, and the tracer volume error of the extracted stirring scheme is calculated based on the initial sample volume, the initial tracer volume, the volume of the sample to be tested, the stirring tracer volume and the volume fraction calculation formula, wherein the volume fraction calculation formula is:

[0113]

[0114] Where ΔV represents the tracer volume error of the extracted stirring scheme, V1 represents the initial tracer volume, and V a1 represents the initial sample volume, V2 represents the stirring tracer volume, V a2 Indicates the volume of the sample to be tested, |*| indicates taking the absolute value;

[0115] comparing the tracer volume error with a tracer error threshold;

[0116] If the tracer volume error is greater than the tracer error threshold, the extracted stirring scheme is confirmed to be an invalid scheme, and the extracted stirring scheme is discarded;

[0117] If the tracer volume error is less than or equal to the tracer error threshold, the extracted stirring scheme is confirmed to be a valid scheme, and the extracted stirring scheme is confirmed to be a valid stirring scheme.

[0118] It can be understood that the initial sample volume is the volume of the unit sample, the initial tracer volume is the volume occupied by the hypothetical tracer in the unit sample, the test sample volume is the volume of the test sample used to detect whether the stirring is balanced, and the stirring tracer volume is the volume occupied by the tracer in the test sample.

[0119] It should be noted that the sample to be tested is a sample that needs to detect the tracer volume error after stirring. The volume and mass of the sample to be tested are smaller than the unit sample, that is, a local unit sample is randomly extracted from the unit sample to detect whether the stirring is sufficient, and whether the stirring is sufficient is determined by the tracer error threshold. The tracer error threshold is the tracer volume error corresponding to the sample to be tested when it is considered that the sample to be tested is sufficiently stirred. The tracer volume error is the error between the volume fraction of the tracer in the sample to be tested and the volume fraction of the tracer in the unit sample.

[0120] Specifically, the tracer volume error is the difference between the ratio of the initial sample volume and the initial tracer volume and the ratio of the volume of the sample to be tested and the stirring tracer volume. The tracer volume error represents the error between the volume ratio of the tracer in the sample to be tested and the volume ratio of the tracer in the unit sample after stirring by the extracted stirring scheme. When the tracer volume error is too large, it means that only a small amount of tracer can be detected in the sample to be tested, indicating that the extracted stirring scheme cannot fully stir the extracted unit sample, and therefore, the extracted stirring scheme needs to be eliminated. When the tracer volume error is less than or equal to the tracer error threshold, it means that the extracted stirring scheme can fully stir the unit sample.

[0121] It is understandable that the embodiment of the present invention constructs a stirring model and thus extracts the optimal solution. This is because during the stirring process, too short a stirring time and too slow a stirring speed will lead to uneven stirring, while too fast a stirring speed and too long a stirring time will cause over-shear of the material. At the same time, it will also cause the material to be stirred to generate unnecessary heat due to stirring, waste energy, and affect the performance of the material to be stirred. Furthermore, because the embodiment of the present invention requires that the iron oxide be evenly coated on the product, if the material to be stirred is not sufficiently stirred, it will directly affect the application effect. Therefore, it is necessary to construct a stirring model.

[0122] S2, obtaining an acetic acid solution, obtaining a copper sulfate solution based on a preset copper sulfate mass, and introducing the copper sulfate solution and the acetic acid solution into a stirring unit to obtain a second mixed material.

[0123] Furthermore, the acetic acid solution includes acetic acid and pure water, the copper sulfate solution includes copper sulfate and pure water, and the mass ratio of the acetic acid, the copper sulfate and the pure water is 3:5:42.

[0124] It is understandable that in the process of preparing the second mixed material, the second mixed material is also introduced into the stirring unit for stirring, but the stirring scheme in the process of preparing the second mixed material is different from the stirring scheme for preparing the first mixed material, and the second stirring model corresponding to the stirring scheme corresponding to the second mixed material is consistent with the construction method of the stirring model described above, so it will not be repeated here.

[0125] S3. Acquire a plurality of first test blocks based on the first mixed material, wherein a pre-constructed test area in the first test block is uniformly coated with the first mixed material of a preset thickness, and construct a first drying scheme using a pre-constructed drying unit and the plurality of first test blocks.

[0126] It is understandable that the first test block is a test block for testing the drying scheme, the first mixed material is evenly coated on the test area, and then the weight before and after drying is measured, and the drying rate is calculated and measured based on the weight difference.

[0127] It should be noted that when the drying temperature and drying rate are too high, pinhole-shaped defects will appear on the surface of the first test block coated with the first mixed material. When the drying temperature and drying rate are too low, the drying is too slow, which may also lead to incomplete drying and affect production efficiency. Therefore, a reasonable drying plan needs to be formulated.

[0128] Furthermore, the use of the pre-built drying unit and the plurality of first test blocks to build the first drying scheme includes:

[0129] Extracting first test blocks from the multiple first test blocks in sequence, and performing the following operations on each of the extracted first test blocks:

[0130] Obtaining the test block mass and the coated test block mass of the extracted first test block, wherein the test block mass is the mass of the test area when it is not coated with the first mixed material, and the coated test block mass is the mass of the test area when it is uniformly coated with the first mixed material of a preset thickness, and calculating the undried material mass according to the test block mass and the coated test block mass, wherein the undried material mass is the difference between the coated test block mass and the test block mass;

[0131] Importing the extracted first test block into a drying unit, and acquiring a drying time based on the drying unit, wherein the drying time includes a first drying time and a second drying time;

[0132] The target time is extracted based on the drying time, and the following operations are performed on the extracted target time:

[0133] Determine a target wind speed according to the extracted target time, and perform a drying operation on the extracted first test block using the target wind speed and the target time to obtain a dried sample;

[0134] The mass of the dried block is obtained based on the dried sample, the drying rate is calculated based on the mass of the dried block, and after confirming that the measured drying rate is within a preset target drying rate range, a surface image of the dried sample is obtained using a pre-constructed image unit, and after confirming that the dried sample is effectively dried based on the surface image, an initial drying scheme corresponding to the extracted first test block is obtained;

[0135] A plurality of initial drying schemes are aggregated to obtain an initial drying scheme set, and a first drying scheme is constructed based on the initial drying scheme set.

[0136] Further, the method of obtaining the mass of the dried block based on the drying sample and calculating and measuring the drying rate according to the mass of the dried block includes:

[0137] The drying rate is calculated based on the mass of the coated test block and the mass of the dried block, wherein the calculation formula of the drying rate is as follows:

[0138]

[0139] Among them, ΔC represents the measured drying rate, C0 represents the mass of the coated test block, C1 represents the mass of the dried block, and C δ Indicates the mass of undried material.

[0140] It can be understood that the drying time in the embodiment of the present invention includes a first drying time and a second drying time, that is, two drying times are used to perform a drying operation on the extracted first test block, and the drying temperature and drying rate in the first drying time are both lower than the corresponding drying rate and drying temperature in the second drying time. This is because pinhole defects are prone to occur when the first test block is directly dried using high temperature and high wind speed. Pinhole defects are defects caused by the rupture and evaporation of water vapor under sudden high temperature. Therefore, the embodiment of the present invention controls the drying of plastic to ensure the surface quality of the product.

[0141] Furthermore, the target time is the first drying time or the second drying time extracted from the drying time. Regardless of whether it is the first drying time or the second drying time, the steps required to perform the drying operation are the same. The target wind speed is the wind speed for drying the first test block at the target time. The greater the wind speed, the faster the drying. The drying sample is the first test block after drying. The mass of the dried block is the total mass of the dried sample. The target drying rate interval is a preset measured drying rate that can ensure that no pinhole defects appear on the surface of the dried sample. However, if the drying time can be saved as much as possible, the energy consumption and economic cost of the embodiment of the present invention during the implementation process will be reduced. Therefore, in the embodiment of the present invention, relying solely on the target drying rate interval can only preliminarily ensure that no surface pinhole defects appear, so it is also necessary to detect the surface of the dried sample.

[0142] It is understandable that the surface image is an image collected by an image unit, and the image unit is a unit that collects the surface image by machine vision and identifies whether there are defects in the surface image. The initial drying scheme is a scheme corresponding to the drying time corresponding to the initial drying scheme.

[0143] Exemplarily, after drying at a wind speed of 5 m / s at 65°C for 10 minutes, and then drying at a wind speed of 10 m / s at 85°C for 5 minutes, after the image unit confirms that the dried sample is effectively dried, the initial drying plan is to dry at a wind speed of 5 m / s at 65°C for 10 minutes, and then dry at a wind speed of 10 m / s at 85°C for 5 minutes.

[0144] Further, after confirming that the measured drying rate is within a preset target drying rate range, the method further comprises:

[0145] Obtaining a lower limit and an upper limit of a drying rate based on a target drying rate interval, and determining whether the measured drying rate is within the target drying rate interval;

[0146] If the measured drying rate is less than the target drying rate lower limit, the extended drying time is obtained, and after confirming that the extended drying time is the target time, the step of performing the drying operation on the extracted first test block with the target wind speed and the target time is returned to until it is confirmed that the measured drying rate is within the preset target drying rate range;

[0147] If the measured drying rate is greater than the upper limit of the drying rate, then the time period corresponding to the extracted target time is confirmed based on the extracted target time, if the time period corresponding to the extracted target time is the first drying time, the shortened drying time is obtained, and the corrected second drying time is obtained based on the shortened drying time and the second drying time. After confirming that the corrected second drying time is the target time, the process returns to the step of performing the drying operation on the extracted first test block using the target wind speed and the target time, otherwise, the drying sample is confirmed to be an invalid sample;

[0148] If the measured drying rate is within the target drying rate interval, it is confirmed that the measured drying rate is within the preset target drying rate interval.

[0149] It is understandable that the lower limit of the drying rate and the upper limit of the drying rate are the maximum measured drying rate and the minimum measured drying rate in the target drying rate interval, respectively. The extended drying time is the time obtained by extending the extracted target time. In the embodiment of the present invention, different target drying rate intervals are set for the measured drying rate after the first drying time and the measured drying rate after the second drying time. Among them, the target drying rate interval corresponding to the second drying time is the drying rate interval that the experimenter hopes to achieve in the end. The shortened drying time is the time after the target time is shortened, and the corrected second drying time is the second drying time modified according to the shortened drying time. The invalid sample is a sample whose final measured drying rate exceeds the upper limit of the drying rate of the second drying time, indicating that the moisture retained in the drying sample cannot meet the use requirements, so the drying scheme corresponding to the invalid sample should be eliminated.

[0150] Exemplarily, within the first drying time, the drying rate of the dried sample is too large, exceeding the upper limit of the drying rate corresponding to the first drying time, indicating that the dried sample is dried too much in the first drying time, and it is necessary to reduce the drying time in the second drying time to ensure that after the first drying time and the second drying time, an ideal drying rate can be obtained. Within the first drying time, if the measured drying rate of the dried sample is too small, if the drying operation is performed according to the original drying scheme of the second drying time, the dried sample will not be able to meet the standard in the end, and then, the coating effect in the embodiment of the present invention is affected. Therefore, it is necessary to correct the second drying time to obtain a corrected second drying time. If the measured drying rate of the dried sample is small within the second drying time, the extended drying time can be obtained, that is, the dried sample is dried again using the drying unit. If the measured drying rate of the dried sample within the second drying time is too large, it means that the water retained in the dried sample cannot meet the use requirements.

[0151] It is understandable that, according to the above steps, multiple first test blocks need to be tested continuously, so that a series of initial drying schemes that can effectively dry the extracted first test blocks can be obtained. The first drying scheme is a better drying scheme for finally drying the first mixed material. Optionally, the first drying scheme is an initial drying scheme with the shortest time and no surface defects.

[0152] Further, after confirming that the dried sample is effectively dried based on the surface image, the method further comprises:

[0153] A grayscale operation is performed on the surface image to obtain a grayscale image, a grayscale image matrix is ​​obtained using a pre-constructed image coordinate system and the grayscale image, the grayscale image matrix is ​​divided based on a preset window size to obtain a grayscale block matrix, block matrices are extracted from the grayscale block matrix in sequence, and the following operations are performed on the extracted block matrices:

[0154] Based on the extracted block matrix, a maximum grayscale value and a minimum grayscale value in the extracted block matrix are obtained, and a grayscale difference value is calculated based on the maximum grayscale value and the minimum grayscale value;

[0155] Compare the grayscale difference with the preset defect threshold;

[0156] If the grayscale difference is greater than the defect threshold, confirm that the area corresponding to the block matrix corresponding to the grayscale difference in the grayscale image is a defect area, otherwise, confirm that the area corresponding to the block matrix corresponding to the grayscale difference in the grayscale image is a regular area;

[0157] Summarize the defective areas to obtain a defective area set, and determine whether the defective area set is an empty set. If the defective area set is an empty set, confirm that the dried sample is effectively dried; otherwise, confirm that the dried sample is an invalid sample.

[0158] It is understandable that the grayscale operation is a prior art and will not be described in detail here. The grayscale image matrix is ​​a matrix constructed using the grayscale values ​​corresponding to all pixels in the grayscale image, that is, the grayscale values ​​of the pixels in the grayscale image can be represented by the elements in the grayscale image matrix, and the element positions in the grayscale image matrix correspond one-to-one to the pixel coordinates in the grayscale image, and the elements in the grayscale image matrix correspond one-to-one to the grayscale values ​​corresponding to the pixel coordinates. The window size is the window for dividing the grayscale image matrix. For example, the window size is 2×2, and the grayscale image matrix is ​​4×4, then the grayscale image matrix can be divided into a 2×2 grayscale block matrix, and each element in the grayscale block matrix is ​​a 2×2 matrix. For example: the grayscale image matrix is ​​shown below:

[0159]

[0160] Among them, l represents the grayscale image matrix, l 11 ,…,l 44 Represents the elements in the grayscale mean matrix.

[0161]

[0162] Where M represents the grayscale block matrix, and

[0163] It is understandable that the maximum grayscale value and the minimum grayscale value are the values ​​with the largest grayscale value and the smallest grayscale value in the block matrix, and the grayscale difference is the difference between the maximum grayscale value and the minimum grayscale value. The defect threshold is the maximum grayscale value and the minimum grayscale value corresponding to the grayscale difference that are not the maximum value of the defect. In the embodiment of the present invention, the first mixed material is evenly coated. If surface defects appear during the drying process, in the surface image after grayscale processing, the grayscale value corresponding to the defective part will be different from the grayscale value corresponding to the part without the defect, and the difference between the two is very obvious. Therefore, the embodiment of the present invention adopts this method to detect defects. When a defective area appears in the surface image, it means that the corresponding initial drying scheme will cause defects on the surface of the first test block. Therefore, the initial drying scheme should be eliminated.

[0164] It should be noted that the defective area is an area where the grayscale difference is too large and can be determined as a defect in the surface image. The regular area is an area where the grayscale difference is less than or equal to the defect threshold and it can be considered that the corresponding area in the grayscale surface image does not have a defect.

[0165] S4. Obtain a product to be coated using a pre-built coating unit, obtain a coating trajectory according to the product to be coated, and perform a coating operation on the object to be coated according to the coating trajectory and the first mixed material to obtain a coated product.

[0166] It is understandable that the product to be coated is a product that needs to be coated with the first mixed material in the embodiment of the present invention, and is also a product that the embodiment of the present invention is intended to use rust paint. The embodiment of the present invention does not limit the product to be coated, but the first mixed material and the second mixed material in the embodiment of the present invention will not damage the product to be coated. The coating trajectory is the running trajectory of the coating unit coating the first mixed material on the product to be coated. The coated product is the product after the first mixed material is coated on the surface of the product to be coated. In the embodiment of the present invention, the combined application of the first mixed material and the second mixed material is called the application of rust paint.

[0167] Furthermore, the method of using the pre-built coating unit to obtain the product to be coated, and obtaining the coating trajectory according to the product to be coated, includes:

[0168] Acquire a product set based on the coating unit, and extract a product set to be modeled from the product set in sequence, wherein the product set includes multiple product sets to be modeled, each of the multiple product sets to be modeled is of a different type, and the product set to be modeled includes multiple products, and the multiple products are of the same type;

[0169] Extracting products to be coated from a set of products to be modeled, and introducing the products to be coated into a coating unit;

[0170] Acquire volume data of the product to be coated based on the product set to be modeled, wherein the volume data includes product height, product width and product length of the product to be coated;

[0171] The moving trajectory and moving step length of the laser emitter are obtained according to the volume data and the pre-built laser emitter, the moving trajectory is divided into a plurality of unit detection points by using the moving step length, unit detection points are sequentially extracted from the plurality of unit detection points, and the following operations are performed on the extracted unit detection points:

[0172] A plurality of laser emission angle pairs are acquired based on a unit detection point, wherein each of the plurality of laser emission angle pairs is different, and the laser emission angle pairs include: a horizontal emission angle and a vertical emission angle, and the laser emission angle pairs are sequentially extracted from the plurality of laser emission angle pairs, and the following operations are performed on the extracted laser emission angle pairs:

[0173] Using the laser transmitter located at the extracted unit detection point and the extracted laser emission angle to emit a pulse laser to the product to be coated, the laser emission time is obtained, the laser transmitter receives the emitted pulse laser, the laser reception time is obtained, the laser flight distance is calculated based on the laser emission time and the laser reception time, and the three-dimensional point data corresponding to the extracted unit detection point is obtained based on the laser flight distance and the pre-constructed coordinate point calculation formula;

[0174] Aggregate multiple 3D point data corresponding to multiple unit detection points to obtain a 3D point data set;

[0175] A coating model corresponding to the product to be coated is spliced ​​out based on the three-dimensional point data set, and a coating trajectory is obtained based on the coating model.

[0176] It is understandable that the product set is a collection of various and multiple products that need to be coated. The product to be modeled is a collection of multiple products of the same product type. The coating unit is a unit that coats the product to be coated. The moving trajectory is the trajectory that the laser emitter needs to move divided according to the volume data, and the moving step length is the step length of the laser emitter's one movement. The unit detection point is the point where the laser emitter emits the laser. The embodiment of the present invention emits laser according to the laser emission angle pair at the unit detection point, and each laser emission angle pair emits the laser once, and receives the laser after emission, so that the three-dimensional point coordinates of the product to be coated that receives the laser can be calculated. The laser flight distance is the distance between the product to be coated and the laser emitter detected after the laser is emitted. In the step of splicing the three-dimensional point data set to obtain the model to be coated corresponding to the product to be coated, the splicing method is a prior art and will not be repeated here.

[0177] Furthermore, the method of obtaining the three-dimensional point data corresponding to the extracted unit detection point based on the laser flight distance and the pre-constructed coordinate point calculation formula includes:

[0178] Obtain the coordinate point calculation formula, and calculate the model horizontal coordinate, model vertical coordinate, and model vertical coordinate corresponding to the extracted unit detection point based on the coordinate point formula. The unit detection point of the pulsed laser emitted by the laser transmitter is the origin of the pre-constructed spatial coordinate system. The coordinate point calculation formula is as follows:

[0179]

[0180] Wherein, x represents the model horizontal coordinate in the spatial coordinate system, y represents the model vertical coordinate in the spatial coordinate system, and xoy represents the plane parallel to the ground in the spatial coordinate system, z represents the model vertical coordinate perpendicular to the ground in the spatial coordinate system, s represents the laser flight distance, β represents the vertical emission angle in the laser emission angle pair, and the vertical emission angle is the angle between the pulse laser and the direction perpendicular to the ground, α represents the horizontal emission angle in the laser emission angle pair, and the horizontal emission angle is the angle between the pulse laser and the plane parallel to the ground;

[0181] Based on the model horizontal coordinate, the model vertical coordinate and the model vertical coordinate, the three-dimensional point coordinate corresponding to the extracted unit detection point is obtained, wherein the three-dimensional point coordinate is: (x, y, z);

[0182] The geodetic detection coordinates of the extracted unit detection points are obtained using a pre-constructed geodetic coordinate system, and three-dimensional point data are obtained based on the three-dimensional point coordinates, wherein the three-dimensional point data includes: a geodetic coordinate system, geodetic detection coordinates, a spatial coordinate system and three-dimensional point coordinates.

[0183] It is understandable that the model horizontal coordinate, model vertical coordinate and model vertical coordinate are the horizontal coordinate, vertical coordinate and vertical coordinate of the point where the product to be coated receives the laser in the space coordinate system constructed with the laser emitter as the origin. In the embodiment of the present invention, the corresponding space coordinate system will be transformed every time the laser emitter moves according to the step length. On this basis, the embodiment of the present invention introduces the earth coordinate system as the static coordinate system, so the model to be coated can be constructed through the three-dimensional point data, and the coating trajectory can be obtained according to the model to be coated.

[0184] S5. Perform a drying operation on the coated product using a drying unit and the first drying scheme to obtain a dried product.

[0185] It can be understood that the dried product is a product obtained by performing a drying operation on the coated product using the first drying scheme.

[0186] S6. Use the pre-constructed spraying unit and the second mixed material to perform a spraying operation on the dried product to obtain a sprayed product, and complete the preparation and application of rust paint for stabilizing the rust layer based on the sprayed product.

[0187] It is understandable that the product corresponding to the coating model in the embodiment of the present invention is the same product as the product to be sprayed, so after the coating model is imported into the spray unit, the spray trajectory is obtained according to the coating model. For example, the product to be coated is a plane, and the coating trajectory is 3mm away from the product to be coated, along a straight line, and the first mixed material is used to evenly coat the product to be coated. Since what needs to be sprayed in the spray unit is a liquid, and the viscosity of the first mixed material in the coating unit is greater than that of the second mixed material, in the spray unit, the spray trajectory that can be obtained according to the coating model is also a straight line.

[0188] It should be noted that, in the embodiment of the present invention, when the spraying unit is used to perform the spraying operation on the dried product, the principle of small amounts and multiple times is referred to.

[0189] Furthermore, in the embodiment of the present invention, a model of the product to be coated is constructed, and various tests can be directly implemented by a computer, so that the application of the first mixed material and the second mixed material can be completed through the same steps for the same type of products, and further, mass production can be achieved.

[0190] The present invention is to solve the problem described in the background technology. The present invention obtains a water-based paint solution, obtains a solution mass based on the water-based paint solution, obtains an iron oxide mass according to the solution mass, obtains an iron oxide corresponding to the iron oxide mass based on the iron oxide mass, introduces the iron oxide and the water-based paint solution into a pre-constructed stirring unit, obtains a material to be stirred, uses a pre-constructed stirring method and a stirring unit to perform a stirring operation on the material to be stirred, obtains a first mixed material, obtains an acetic acid solution, obtains a copper sulfate solution based on a preset copper sulfate mass, and introduces the copper sulfate solution and the acetic acid solution into the stirring unit to obtain a second mixed material. Therefore, the embodiment of the present invention can use the stirring unit to predict the stirring time and stirring speed required for the material to be stirred when performing the stirring operation, thereby constructing a stirring method to perform a stirring operation on the material to be stirred. Based on the first mixed material, multiple first test blocks are obtained, and a first drying scheme is constructed using a pre-constructed drying unit and multiple first test blocks. In the embodiment of the present invention, a reasonable first drying scheme is formulated to avoid excessive drying temperature and excessive drying rate, which may cause pinhole-shaped defects on the surface, and avoid incomplete drying. A product to be coated is obtained by using a pre-constructed coating unit, a coating trajectory is obtained according to the product to be coated, a coating operation is performed on the object to be coated according to the coating trajectory and the first mixed material to obtain a coated product, a drying operation is performed on the coated product by using a drying unit and a first drying scheme to obtain a dried product, a spraying operation is performed on the dried product by using a pre-constructed spraying unit and a second mixed material to obtain a sprayed product, and the preparation and application of rust paint with a stable rust layer is completed based on the sprayed product. The embodiment of the present invention constructs a model of the product to be coated, and can be directly implemented by a computer in a variety of tests, so that the application of the first mixed material and the second mixed material can be completed for the same type of product through the same steps, and further, mass production can be achieved. Therefore, the present invention provides a method for preparing rust paint and enables the rust paint to be effectively and automatically applied through a variety of detection methods.

[0191] like Figure 2 As shown, it is a functional module diagram of a rust paint preparation and application system based on a stable rust layer provided by an embodiment of the present invention.

[0192] The rust paint preparation and application system 100 based on the stable rust layer of the present invention can be installed in an electronic device. According to the functions to be implemented, the rust paint preparation and application system 100 based on the stable rust layer can include a first mixed material acquisition module 101, a second mixed material module 102, a coating module 103 and a spraying module 104. The module of the present invention can also be called a unit, which refers to a series of computer program segments that can be executed by an electronic device processor and can complete fixed functions, which are stored in the memory of the electronic device.

[0193] The first mixed material acquisition module 101 is used to obtain a water-based paint solution, wherein the solute in the water-based paint solution is water-based paint, the solution is pure water, and the ratio between the mass of the water-based paint and the mass of the pure water is 2:3;

[0194] Obtaining a solution mass based on a water-based paint solution, obtaining an iron oxide mass based on the solution mass, obtaining iron oxide corresponding to the iron oxide mass based on the iron oxide mass, introducing the iron oxide and the water-based paint solution into a pre-constructed stirring unit to obtain a material to be stirred, and performing a stirring operation on the material to be stirred using a pre-constructed stirring method and a stirring unit to obtain a first mixed material, wherein the iron oxide mass is numerically equal to the solution mass;

[0195] The second mixed material module 102 is used to obtain an acetic acid solution, obtain a copper sulfate solution based on a preset copper sulfate mass, and introduce the copper sulfate solution and the acetic acid solution into a stirring unit to obtain a second mixed material, wherein the acetic acid solution includes acetic acid and pure water, the copper sulfate solution includes copper sulfate and pure water, and the mass ratio of the acetic acid mass, the copper sulfate mass and the pure water is 3:5:42;

[0196] The coating module 103 is used to obtain a plurality of first test blocks based on the first mixed material, wherein the pre-constructed test area in the first test block is uniformly coated with the first mixed material of a preset thickness, and a first drying scheme is constructed using the pre-constructed drying unit and the plurality of first test blocks;

[0197] Using a pre-built coating unit to obtain a product to be coated, obtaining a coating trajectory according to the product to be coated, and performing a coating operation on the object to be coated according to the coating trajectory and the first mixed material to obtain a coated product;

[0198] Performing a drying operation on the coated product using a drying unit and a first drying scheme to obtain a dried product;

[0199] The spraying module 104 is used to perform a spraying operation on the dried product using a pre-constructed spraying unit and a second mixed material to obtain a sprayed product, and to complete the preparation and application of a rust paint with a stable rust layer based on the sprayed product.

[0200] In detail, each module in the rust paint preparation and application system 100 based on the stable rust layer in the embodiment of the present invention is used in the same manner as described above. Figure 1 The technical means for preparing the rust paint based on the stable rust layer and the application method are the same and can produce the same technical effects, so they will not be repeated here.

[0201] like Figure 3 , which is a schematic diagram of the structure of an electronic device for implementing a method for preparing and applying rust paint based on a stable rust layer provided by an embodiment of the present invention.

[0202] The electronic device 1 may include a processor 10, a memory 11 and a bus 12, and may also include a computer program stored in the memory 11 and executable on the processor 10, such as a rust paint preparation and application method program based on a stable rust layer.

[0203] Wherein, the memory 11 includes at least one type of readable storage medium, and the readable storage medium includes flash memory, mobile hard disk, multimedia card, card-type memory (for example: SD or DX memory, etc.), magnetic memory, disk, optical disk, etc. In some embodiments, the memory 11 can be an internal storage unit of the electronic device 1, such as a mobile hard disk of the electronic device 1. In other embodiments, the memory 11 can also be an external storage device of the electronic device 1, such as a plug-in mobile hard disk, a smart memory card (Smart Media Card, SMC), a secure digital (SecureDigital, SD) card, a flash card (Flash Card), etc. equipped on the electronic device 1. Further, the memory 11 also includes an internal storage unit of the electronic device 1 and an external storage device. The memory 11 can not only be used to store application software and various types of data installed in the electronic device 1, such as the code of the rust paint preparation and application method program based on the stable rust layer, but also can be used to temporarily store data that has been output or is to be output.

[0204] The processor 10 may be composed of an integrated circuit in some embodiments, for example, a single packaged integrated circuit, or a plurality of packaged integrated circuits with the same or different functions, including one or more central processing units (CPUs), microprocessors, digital processing chips, graphics processors, and combinations of various control chips, etc. The processor 10 is the control core (Control Unit) of the electronic device, and uses various interfaces and lines to connect various components of the entire electronic device, and executes or executes programs or modules stored in the memory 11 (for example, a rust paint preparation and application method program based on a stable rust layer, etc.), and calls data stored in the memory 11 to execute various functions of the electronic device 1 and process data.

[0205] The bus 12 may be a peripheral component interconnect (PCI) bus or an extended industry standard architecture (EISA) bus, etc. The bus 12 may be divided into an address bus, a data bus, a control bus, etc. The bus 12 is configured to realize connection and communication between the memory 11 and at least one processor 10, etc.

[0206] Figure 3 Only an electronic device with components is shown, and those skilled in the art will understand that Figure 3 The structure shown does not constitute a limitation on the electronic device 1, and may include fewer or more components than shown in the figure, or combine certain components, or arrange the components differently.

[0207] For example, although not shown, the electronic device 1 may also include a power source (such as a battery) for supplying power to each component. Preferably, the power source may be logically connected to the at least one processor 10 through a power management device, so that the power management device can realize functions such as charging management, discharging management, and power consumption management. The power source may also include any components such as one or more DC or AC power sources, recharging devices, power failure detection circuits, power converters or inverters, power status indicators, etc. The electronic device 1 may also include a variety of sensors, Bluetooth modules, Wi-Fi modules, etc., which will not be repeated here.

[0208] Furthermore, the electronic device 1 may also include a network interface. Optionally, the network interface may include a wired interface and / or a wireless interface (such as a WI-FI interface, a Bluetooth interface, etc.), which is generally used to establish a communication connection between the electronic device 1 and other electronic devices.

[0209] Optionally, the electronic device 1 may further include a user interface, which may be a display, an input unit (such as a keyboard), or a standard wired interface or a wireless interface. Optionally, in some embodiments, the display may be an LED display, a liquid crystal display, a touch-sensitive liquid crystal display, and an OLED (Organic Light-Emitting Diode) touch device. The display may also be appropriately referred to as a display screen or a display unit, which is used to display information processed in the electronic device 1 and to display a visual user interface.

[0210] It should be understood that the embodiment is for illustration only and the scope of the patent application is not limited to this structure.

[0211] The rust paint preparation and application method program based on the stable rust layer stored in the memory 11 of the electronic device 1 is a combination of multiple instructions. When running in the processor 10, it can achieve:

[0212] Obtaining a water-based paint solution, wherein the solute in the water-based paint solution is water-based paint, the solution is pure water, and the ratio between the mass of the water-based paint and the mass of the pure water is 2:3;

[0213] Obtaining a solution mass based on a water-based paint solution, obtaining an iron oxide mass based on the solution mass, obtaining iron oxide corresponding to the iron oxide mass based on the iron oxide mass, introducing the iron oxide and the water-based paint solution into a pre-constructed stirring unit to obtain a material to be stirred, and performing a stirring operation on the material to be stirred using a pre-constructed stirring method and a stirring unit to obtain a first mixed material, wherein the iron oxide mass is numerically equal to the solution mass;

[0214] Obtaining an acetic acid solution, obtaining a copper sulfate solution based on a preset copper sulfate mass, and introducing the copper sulfate solution and the acetic acid solution into a stirring unit to obtain a second mixed material, wherein the acetic acid solution includes acetic acid and pure water, the copper sulfate solution includes copper sulfate and pure water, and the mass ratio of the mass of acetic acid, the mass of copper sulfate, and the mass of pure water is 3:5:42;

[0215] Acquire a plurality of first test blocks based on the first mixed material, wherein a pre-constructed test area in the first test block is uniformly coated with the first mixed material of a preset thickness, and construct a first drying scheme using a pre-constructed drying unit and the plurality of first test blocks;

[0216] Using a pre-built coating unit to obtain a product to be coated, obtaining a coating trajectory according to the product to be coated, and performing a coating operation on the object to be coated according to the coating trajectory and the first mixed material to obtain a coated product;

[0217] Performing a drying operation on the coated product using a drying unit and a first drying scheme to obtain a dried product;

[0218] The dried product is sprayed using a pre-built spray unit and a second mixed material to obtain a sprayed product, and the rust paint for stabilizing the rust layer is prepared and applied based on the sprayed product.

[0219] Specifically, the specific implementation method of the processor 10 for the above instructions can refer to Figures 1 to 3 The description of the relevant steps in the corresponding embodiments will not be repeated here.

[0220] Furthermore, if the module / unit integrated in the electronic device 1 is implemented in the form of a software functional unit and sold or used as an independent product, it can be stored in a computer-readable storage medium. The computer-readable storage medium can be volatile or non-volatile. For example, the computer-readable medium can include: any entity or device capable of carrying the computer program code, a recording medium, a USB flash drive, a mobile hard disk, a magnetic disk, an optical disk, a computer memory, and a read-only memory (ROM).

[0221] The present invention further provides a computer-readable storage medium, wherein the computer-readable storage medium stores a computer program, and when the computer program is executed by a processor of an electronic device, the computer program can implement:

[0222] Obtaining a water-based paint solution, wherein the solute in the water-based paint solution is water-based paint, the solution is pure water, and the ratio between the mass of the water-based paint and the mass of the pure water is 2:3;

[0223] Obtaining a solution mass based on a water-based paint solution, obtaining an iron oxide mass based on the solution mass, obtaining iron oxide corresponding to the iron oxide mass based on the iron oxide mass, introducing the iron oxide and the water-based paint solution into a pre-constructed stirring unit to obtain a material to be stirred, and performing a stirring operation on the material to be stirred using a pre-constructed stirring method and a stirring unit to obtain a first mixed material, wherein the iron oxide mass is numerically equal to the solution mass;

[0224] Obtaining an acetic acid solution, obtaining a copper sulfate solution based on a preset copper sulfate mass, and introducing the copper sulfate solution and the acetic acid solution into a stirring unit to obtain a second mixed material, wherein the acetic acid solution includes acetic acid and pure water, the copper sulfate solution includes copper sulfate and pure water, and the mass ratio of the mass of acetic acid, the mass of copper sulfate, and the mass of pure water is 3:5:42;

[0225] Acquire a plurality of first test blocks based on the first mixed material, wherein a pre-constructed test area in the first test block is uniformly coated with the first mixed material of a preset thickness, and construct a first drying scheme using a pre-constructed drying unit and the plurality of first test blocks;

[0226] Using a pre-built coating unit to obtain a product to be coated, obtaining a coating trajectory according to the product to be coated, and performing a coating operation on the object to be coated according to the coating trajectory and the first mixed material to obtain a coated product;

[0227] Performing a drying operation on the coated product using a drying unit and a first drying scheme to obtain a dried product;

[0228] The dried product is sprayed using a pre-built spray unit and a second mixed material to obtain a sprayed product, and the rust paint for stabilizing the rust layer is prepared and applied based on the sprayed product.

[0229] In the several embodiments provided by the present invention, it should be understood that the disclosed devices, systems and methods can be implemented in other ways. For example, the system embodiments described above are only illustrative, and actual implementation may have other division methods.

[0230] The modules described as separate components may or may not be physically separated, and the components shown as modules may or may not be physical units, that is, they may be located in one place or distributed on multiple network units. Some or all of the modules may be selected according to actual needs to achieve the purpose of the solution of this embodiment.

[0231] In addition, each functional module in each embodiment of the present invention may be integrated into one processing unit, each unit may exist physically separately, or two or more units may be integrated into one unit. The above-mentioned integrated unit may be implemented in the form of hardware or in the form of hardware plus software functional modules.

[0232] It is obvious to those skilled in the art that the present invention is not limited to the details of the above exemplary embodiments, and that the present invention can be implemented in other specific forms without departing from the spirit or essential characteristics of the present invention.

[0233] In addition, it is clear that the word "comprising" does not exclude other units or steps, and the singular does not exclude the plural. Multiple units or devices stated in the system claim can also be implemented by one unit or device through software or hardware. The second and other words are used to indicate names, but not to indicate any particular order.

[0234] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the spirit and scope of the technical solution of the present invention.

Claims

1. A method for preparing and applying rust-resistant paint based on a stable rust layer, It is characterized in that The method comprises: Obtaining a water-based paint solution, wherein the solute in the water-based paint solution is water-based paint, the solution is pure water, and the ratio between the mass of the water-based paint and the mass of the pure water is 2:3; Obtaining a solution mass based on a water-based paint solution, obtaining an iron oxide mass based on the solution mass, obtaining iron oxide corresponding to the iron oxide mass based on the iron oxide mass, introducing the iron oxide and the water-based paint solution into a pre-constructed stirring unit to obtain a material to be stirred, and performing a stirring operation on the material to be stirred using a pre-constructed stirring method and a stirring unit to obtain a first mixed material, wherein the iron oxide mass is numerically equal to the solution mass; Obtaining an acetic acid solution, obtaining a copper sulfate solution based on a preset copper sulfate mass, and introducing the copper sulfate solution and the acetic acid solution into a stirring unit to obtain a second mixed material, wherein the acetic acid solution includes acetic acid and pure water, the copper sulfate solution includes copper sulfate and pure water, and the mass ratio of the mass of acetic acid, the mass of copper sulfate, and the mass of pure water is 3:5:42; Acquire a plurality of first test blocks based on the first mixed material, wherein a pre-constructed test area in the first test block is uniformly coated with the first mixed material of a preset thickness, and construct a first drying scheme using a pre-constructed drying unit and the plurality of first test blocks; Using a pre-built coating unit to obtain a product to be coated, obtaining a coating trajectory according to the product to be coated, and performing a coating operation on the object to be coated according to the coating trajectory and the first mixed material to obtain a coated product; Performing a drying operation on the coated product using a drying unit and a first drying scheme to obtain a dried product; The dried product is sprayed using a pre-built spray unit and a second mixed material to obtain a sprayed product, and the rust paint for stabilizing the rust layer is prepared and applied based on the sprayed product.

2. The method for preparing and applying the rust paint based on the stable rust layer according to claim 1, It is characterized in that The method of using the pre-built stirring method and stirring unit to perform a stirring operation on the material to be stirred to obtain a first mixed material includes: Acquire a stirring sample set based on the material to be stirred, wherein the stirring sample set includes a plurality of unit sample sets, the unit sample set includes a plurality of unit samples, the ratio of the mass of the material to be stirred to the mass of the tracer corresponding to the unit samples in all the unit sample sets is the same, and the mass of the unit samples in the same unit sample set is the same, while the mass of the unit samples in different unit sample sets is different; Extract unit sample sets from the stirred sample set in sequence, and perform the following operations on the extracted unit sample sets: Based on the stirring unit, a stirring speed sequence and a stirring time sequence are obtained, wherein the stirring speed sequence is a sequence in which the stirring speeds are arranged from small to large, and the stirring time sequence is a sequence in which the stirring time is arranged from short to long; Based on the extracted unit sample set, the stirring speed sequence and the stirring time sequence, multiple stirring schemes are constructed, wherein the stirring scheme includes: unit sample, stirring speed and stirring time, stirring schemes are sequentially extracted from the multiple stirring schemes, and the following operations are performed on the extracted stirring schemes: Extracting unit sample, stirring speed and stirring time based on the extracted stirring scheme; The extracted unit sample is introduced into the stirring unit, and a pre-built stirrer in the stirring unit is started based on the stirring time and the stirring speed, and the stirrer performs a stirring operation on the unit sample to obtain a sample to be tested; Calculating the tracer volume error of the tracer in the test sample based on the test sample and a pre-constructed volume fraction calculation formula, comparing the tracer volume error with a preset tracer error threshold, and confirming that the tracer volume error is less than or equal to the tracer error threshold, confirming that the extracted stirring scheme is a valid stirring scheme; Aggregate multiple effective mixing schemes to obtain a unit effective mixing scheme set; A plurality of effective stirring scheme sets corresponding to the stirring sample set are summarized to obtain a stirring data set, a stirring model is constructed based on the stirring data set, an optimal stirring scheme is obtained using the stirring model, and a stirring operation is performed on the material to be stirred using the optimal stirring scheme and the stirring unit to obtain a first mixed material.

3. The method for preparing and applying the rust paint based on the stable rust layer as claimed in claim 2, It is characterized in that The method comprises: calculating the tracer volume error of the tracer in the test sample based on the test sample and the pre-constructed volume fraction calculation formula, comparing the tracer volume error with a preset tracer error threshold, and confirming that the tracer volume error is less than or equal to the tracer error threshold, and confirming that the extracted stirring scheme is a valid stirring scheme, including: Obtaining an initial sample volume and an initial tracer volume based on the extracted unit sample; The volume of the sample to be tested and the stirring tracer volume are obtained based on the sample to be tested, and the tracer volume error of the extracted stirring scheme is calculated based on the initial sample volume, the initial tracer volume, the volume of the sample to be tested, the stirring tracer volume and the volume fraction calculation formula, wherein the volume fraction calculation formula is: Where ΔV represents the tracer volume error of the extracted stirring scheme, V 1 represents the initial tracer volume, V a1 represents the initial sample volume, V 2 represents the stirring tracer volume, V a2 Indicates the volume of the sample to be tested, |*| indicates taking the absolute value; comparing the tracer volume error with a tracer error threshold; If the tracer volume error is greater than the tracer error threshold, the extracted stirring scheme is confirmed to be an invalid scheme, and the extracted stirring scheme is discarded; If the tracer volume error is less than or equal to the tracer error threshold, the extracted stirring scheme is confirmed to be a valid scheme, and the extracted stirring scheme is confirmed to be a valid stirring scheme.

4. The method for preparing and applying the rust-resistant paint based on the stable rust layer according to claim 1, It is characterized in that The method of constructing a first drying scheme using a pre-constructed drying unit and a plurality of first test blocks includes: Extracting first test blocks from the multiple first test blocks in sequence, and performing the following operations on each of the extracted first test blocks: Obtaining the test block mass and the coated test block mass of the extracted first test block, wherein the test block mass is the mass of the test area when it is not coated with the first mixed material, and the coated test block mass is the mass of the test area when it is uniformly coated with the first mixed material of a preset thickness, and calculating the undried material mass according to the test block mass and the coated test block mass, wherein the undried material mass is the difference between the coated test block mass and the test block mass; Importing the extracted first test block into a drying unit, and acquiring a drying time based on the drying unit, wherein the drying time includes a first drying time and a second drying time; The target time is extracted based on the drying time, and the following operations are performed on the extracted target time: Determine a target wind speed according to the extracted target time, and perform a drying operation on the extracted first test block using the target wind speed and the target time to obtain a dried sample; The mass of the dried block is obtained based on the dried sample, the drying rate is calculated based on the mass of the dried block, and after confirming that the measured drying rate is within a preset target drying rate range, a surface image of the dried sample is obtained using a pre-constructed image unit, and after confirming that the dried sample is effectively dried based on the surface image, an initial drying scheme corresponding to the extracted first test block is obtained; A plurality of initial drying schemes are aggregated to obtain an initial drying scheme set, and a first drying scheme is constructed based on the initial drying scheme set.

5. The method for preparing and applying the rust paint based on the stable rust layer as claimed in claim 4, It is characterized in that The method of obtaining the mass of the dried block based on the dried sample and calculating the drying rate according to the mass of the dried block includes: The drying rate is calculated based on the mass of the coated test block and the mass of the dried block, wherein the calculation formula of the drying rate is as follows: Where ΔC represents the measured drying rate, C 0 Indicates the mass of the coated test block, C 1 Indicates the mass of dried blocks, C δ Indicates the mass of undried material.

6. The method for preparing and applying the rust paint based on the stable rust layer as claimed in claim 5, It is characterized in that After confirming that the measured drying rate is within a preset target drying rate range, the method includes: Obtaining a lower limit and an upper limit of a drying rate based on a target drying rate interval, and determining whether the measured drying rate is within the target drying rate interval; If the measured drying rate is less than the target drying rate lower limit, the extended drying time is obtained, and after confirming that the extended drying time is the target time, the step of performing the drying operation on the extracted first test block with the target wind speed and the target time is returned to until it is confirmed that the measured drying rate is within the preset target drying rate range; If the measured drying rate is greater than the upper limit of the drying rate, then the time period corresponding to the extracted target time is confirmed based on the extracted target time, if the time period corresponding to the extracted target time is the first drying time, the shortened drying time is obtained, and the corrected second drying time is obtained based on the shortened drying time and the second drying time. After confirming that the corrected second drying time is the target time, the process returns to the step of performing the drying operation on the extracted first test block using the target wind speed and the target time, otherwise, the drying sample is confirmed to be an invalid sample; If the measured drying rate is within the target drying rate interval, it is confirmed that the measured drying rate is within the preset target drying rate interval.

7. The method for preparing and applying the rust paint based on the stable rust layer as claimed in claim 4, It is characterized in that After confirming that the dried sample is effectively dried based on the surface image, the method includes: A grayscale operation is performed on the surface image to obtain a grayscale image, a grayscale image matrix is ​​obtained using a pre-constructed image coordinate system and the grayscale image, the grayscale image matrix is ​​divided based on a preset window size to obtain a grayscale block matrix, block matrices are extracted from the grayscale block matrix in sequence, and the following operations are performed on the extracted block matrices: Based on the extracted block matrix, a maximum grayscale value and a minimum grayscale value in the extracted block matrix are obtained, and a grayscale difference value is calculated based on the maximum grayscale value and the minimum grayscale value; Compare the grayscale difference with the preset defect threshold; If the grayscale difference is greater than the defect threshold, confirm that the area corresponding to the block matrix corresponding to the grayscale difference in the grayscale image is a defect area, otherwise, confirm that the area corresponding to the block matrix corresponding to the grayscale difference in the grayscale image is a regular area; Summarize the defective areas to obtain a defective area set, and determine whether the defective area set is an empty set. If the defective area set is an empty set, confirm that the dried sample is effectively dried; otherwise, confirm that the dried sample is an invalid sample.

8. The method for preparing and applying the rust paint based on the stable rust layer according to claim 1, It is characterized in that The method of obtaining the product to be coated by using the pre-built coating unit and obtaining the coating trajectory according to the product to be coated includes: Acquire a product set based on the coating unit, and extract a product set to be modeled from the product set in sequence, wherein the product set includes multiple product sets to be modeled, each of the multiple product sets to be modeled is of a different type, and the product set to be modeled includes multiple products, and the multiple products are of the same type; Extracting products to be coated from the set of products to be modeled, and introducing the products to be coated into a coating unit; Acquire volume data of the product to be coated based on the product set to be modeled, wherein the volume data includes product height, product width and product length of the product to be coated; The moving trajectory and moving step length of the laser emitter are obtained according to the volume data and the pre-built laser emitter, the moving trajectory is divided into a plurality of unit detection points by using the moving step length, unit detection points are sequentially extracted from the plurality of unit detection points, and the following operations are performed on the extracted unit detection points: A plurality of laser emission angle pairs are acquired based on a unit detection point, wherein each of the plurality of laser emission angle pairs is different, and the laser emission angle pairs include: a horizontal emission angle and a vertical emission angle, and the laser emission angle pairs are sequentially extracted from the plurality of laser emission angle pairs, and the following operations are performed on the extracted laser emission angle pairs: Using the laser transmitter located at the extracted unit detection point and the extracted laser emission angle to emit a pulse laser to the product to be coated, the laser emission time is obtained, the laser transmitter receives the emitted pulse laser, the laser reception time is obtained, the laser flight distance is calculated based on the laser emission time and the laser reception time, and the three-dimensional point data corresponding to the extracted unit detection point is obtained based on the laser flight distance and the pre-constructed coordinate point calculation formula; Aggregate multiple 3D point data corresponding to multiple unit detection points to obtain a 3D point data set; A coating model corresponding to the product to be coated is spliced ​​out based on the three-dimensional point data set, and a coating trajectory is obtained based on the coating model.

9. The method for preparing and applying the rust paint based on the stable rust layer as claimed in claim 8, It is characterized in that The method of obtaining the three-dimensional point data corresponding to the extracted unit detection point based on the laser flight distance and the pre-constructed coordinate point calculation formula includes: Obtain the coordinate point calculation formula, and calculate the model horizontal coordinate, model vertical coordinate, and model vertical coordinate corresponding to the extracted unit detection point based on the coordinate point formula. The unit detection point of the pulsed laser emitted by the laser transmitter is the origin of the pre-constructed spatial coordinate system. The coordinate point calculation formula is as follows: Wherein, x represents the model horizontal coordinate in the spatial coordinate system, y represents the model vertical coordinate in the spatial coordinate system, and xoy represents the plane parallel to the ground in the spatial coordinate system, z represents the model vertical coordinate perpendicular to the ground in the spatial coordinate system, s represents the laser flight distance, β represents the vertical emission angle in the laser emission angle pair, and the vertical emission angle is the angle between the pulse laser and the direction perpendicular to the ground, α represents the horizontal emission angle in the laser emission angle pair, and the horizontal emission angle is the angle between the pulse laser and the plane parallel to the ground; Based on the model horizontal coordinate, the model vertical coordinate and the model vertical coordinate, the three-dimensional point coordinate corresponding to the extracted unit detection point is obtained, wherein the three-dimensional point coordinate is: (x, y, z); The geodetic detection coordinates of the extracted unit detection points are obtained using a pre-constructed geodetic coordinate system, and three-dimensional point data are obtained based on the three-dimensional point coordinates, wherein the three-dimensional point data includes: a geodetic coordinate system, geodetic detection coordinates, a spatial coordinate system and three-dimensional point coordinates.

10. A rust paint preparation and application system based on a stable rust layer, It is characterized in that The system comprises: A first mixed material acquisition module is used to obtain a water-based paint solution, wherein the solute in the water-based paint solution is water-based paint, the solution is pure water, and the ratio between the mass of the water-based paint and the mass of the pure water is 2:3; Obtaining a solution mass based on a water-based paint solution, obtaining an iron oxide mass based on the solution mass, obtaining iron oxide corresponding to the iron oxide mass based on the iron oxide mass, introducing the iron oxide and the water-based paint solution into a pre-constructed stirring unit to obtain a material to be stirred, and performing a stirring operation on the material to be stirred using a pre-constructed stirring method and a stirring unit to obtain a first mixed material, wherein the iron oxide mass is numerically equal to the solution mass; A second mixed material module is used to obtain an acetic acid solution, obtain a copper sulfate solution based on a preset copper sulfate mass, and introduce the copper sulfate solution and the acetic acid solution into a stirring unit to obtain a second mixed material, wherein the acetic acid solution includes acetic acid and pure water, the copper sulfate solution includes copper sulfate and pure water, and the mass ratio of the acetic acid mass, the copper sulfate mass and the pure water is 3:5:42; A coating module, configured to obtain a plurality of first test blocks based on a first mixed material, wherein a pre-constructed test area in the first test block is uniformly coated with the first mixed material of a preset thickness, and construct a first drying scheme using a pre-constructed drying unit and the plurality of first test blocks; Using a pre-built coating unit to obtain a product to be coated, obtaining a coating trajectory according to the product to be coated, and performing a coating operation on the object to be coated according to the coating trajectory and the first mixed material to obtain a coated product; Performing a drying operation on the coated product using a drying unit and a first drying scheme to obtain a dried product; The spraying module is used to perform a spraying operation on the dried product using a pre-built spraying unit and a second mixed material to obtain a sprayed product, and to complete the preparation and application of a rust paint for stabilizing the rust layer based on the sprayed product.

Citation Information

Patent Citations

  • Method for measuring homogeneous degree of fodder

    CN102928368A

  • Treating fluid for accelerating stabilization of weathering-resistant steel rust layers

    CN108754474A

  • Rust-imitating paint and preparation method thereof and rust-imitating method

    CN110804346A

  • Automatic detection method and system for flaws of quick-dry fabric

    CN111709915A

  • Weathering resistant steel surface rust layer stabilizing treatment agent and use method

    CN115354314A

Cited By

  • A method for preparing a metal oxide texture on a substrate surface

    CN122828925A