Preprocessing device for cutting titanium foil material by femtosecond laser

By introducing cleaning components and transmission wheels into the pre-processing treatment device for femtosecond laser cutting of titanium foil material, the problems of low cutting efficiency and high labor intensity in the prior art are solved, and more efficient cleaning and automation are achieved Movement improves cutting efficiency and practicality of the device.

CN118905473APending Publication Date: 2024-11-08SHAANXI AEROSPACE INTELLIGENT MANUFACTURING NEW MATERIALS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411235588.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The prior art lacks cleaning treatment and automated movement when cutting titanium foil materials using CNC laser cutting machines, resulting in low cutting efficiency and high labor intensity.

Method used

A pre-processing device for femtosecond laser cutting titanium foil material is designed, including a cleaning assembly and a transmission wheel. The cleaning assembly is used to clean the titanium foil roll, the transmission wheel is used to drive the movement of the titanium foil roll, and the auxiliary assembly is provided. Used to separate the cut materials.

Benefits of technology

The cleanliness and cutting efficiency of the titanium foil coil are improved, labor intensity is reduced, and the practicality of the device is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118905473A_ABST
    Figure CN118905473A_ABST
Patent Text Reader

Abstract

The invention discloses a preprocessing device for cutting a titanium foil material through femtosecond laser, and relates to the technical field of metal material cutting, the preprocessing device comprises a shell, a placing shell installed at the top of the shell and a laser cutting assembly arranged in the shell, a titanium foil coiled material is arranged in the placing shell, and a cleaning assembly is arranged at one end in the shell; the cleaning assembly is used for cleaning the titanium foil coiled material, the titanium foil coiled material penetrates through the interior of the cleaning assembly and extends to the position of the laser cutting assembly, and the laser cutting assembly is used for cutting the titanium foil coiled material. According to the titanium foil coiled material cutting device, the cleaning assembly is arranged, when the titanium foil coiled material is cut, the titanium foil coiled material penetrates through the interior of the cleaning assembly through the transmission wheel and extends to the position of the laser cutting assembly, the cleaning assembly cleans the surface of the titanium foil coiled material, and the cutting effect of the titanium foil coiled material is further improved; therefore, the titanium foil coiled material cutting efficiency is improved, and the labor intensity of people for moving the titanium foil coiled material is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of metal material cutting, and in particular to a pre-processing device for cutting titanium foil material with a femtosecond laser. Background Art

[0002] Titanium foil is a titanium plate, strip, coil or sheet with a thickness of 0.1mm or less. Another indicator for evaluating the thickness of titanium foil is the weight per unit area, such as g / m or oz / fi, etc. The larger the value, the greater the thickness. The width of titanium foil is cut according to the user's requirements. However, the wider the width during manufacturing, the higher the productivity. The length of the roller body determines the maximum width of the rolled foil. The wider, thinner and harder the rolled piece is, the more difficult it is to roll. The maximum width of rolled titanium foil is about 600mm. Titanium and alloy foils are mainly used in electronics, aerospace, instrumentation and other departments.

[0003] According to Chinese patent announcement number: CN112548364, a CNC laser cutting machine is disclosed, including a workbench, a laser cutting device, a CNC control panel, and an automatic normal line laser testing device. A CNC control panel is provided on one side of the workbench, a laser cutting device is provided on the workbench, and the automatic normal line laser testing device is located on one side of the laser cutting device. The CNC control panel is electrically connected to the laser cutting device, and the CNC control panel is electrically connected to the automatic normal line laser testing device. The CNC laser cutting machine is provided with a laser cutting device, which greatly improves the efficiency of laser cutting processing, makes the cutting processing more accurate, has a simple structure, and is reasonably designed. However, when using the above device to laser cut titanium foil materials, it is not possible to clean the titanium foil coil, and then the titanium foil coil needs to be cleaned manually or by other mechanisms before laser cutting, which affects the cutting efficiency of the titanium foil coil, and the metal sheet needs to be manually placed during cutting, which increases people's labor intensity.

[0004] Therefore, when the above device is used, the titanium foil coil cannot be cleaned, and the metal sheet needs to be placed manually, which affects the cutting efficiency of the titanium foil coil and increases the labor intensity of people. Summary of the invention

[0005] In order to achieve the above object, the present invention is achieved through the following technical solutions:

[0006] A pre-processing device for femtosecond laser cutting of titanium foil materials comprises an outer shell, a placing shell installed on the top of the outer shell, and a laser cutting component arranged inside the outer shell, wherein a titanium foil coil is arranged inside the placing shell, a cleaning component is arranged at one end inside the outer shell, the cleaning component is used to clean the titanium foil coil, the titanium foil coil passes through the inside of the cleaning component and extends to the position of the laser cutting component, the laser cutting component is used to cut the titanium foil coil, transmission wheels are rotatably installed at the inner bottom of the placing shell and at the upper and lower ends of one end of the inner shell near the cleaning component, the titanium foil coil is transmission-connected to a plurality of transmission wheels, the transmission wheels are used to drive the titanium foil coil to move, and an auxiliary component is arranged at the bottom of the outer shell, the auxiliary component is used to separate the cut titanium foil coil.

[0007] More preferably, the cleaning component comprises:

[0008] There are two first cleaning rods, which are symmetrically rotatably mounted on the upper part of one end of the inner part of the shell.

[0009] There are two second cleaning rods, which are symmetrically rotatably mounted at one end of the inner portion of the housing near the bottom of the first cleaning rod. A first cleaning rod and a second cleaning rod are connected by a belt.

[0010] There are two injection blocks, which are symmetrically rotated and installed at one end of the inner part of the shell near the upper part of the second cleaning rod. The two injection blocks inject cleaning liquid into the second cleaning rod.

[0011] There are two spray pipes, which are symmetrically rotated and installed at the middle position of one end of the inner part of the shell. The spray pipes are used to spray cleaning liquid on the surface of the titanium foil coil.

[0012] There are two third cleaning rods, which are symmetrically rotatably installed at one end of the inner part of the shell near the lower part of the spray pipe. The two third cleaning rods are used to remove liquid from the surface of the titanium foil coil. A second cleaning rod and a third cleaning rod are connected by a belt.

[0013] There are two jet pipes, which are symmetrically rotated and installed at the bottom of one end of the inner part of the shell. The two jet pipes are used to remove liquid from the surface of the titanium foil coil.

[0014] The transmission gear is rotatably mounted on the bottom of the transmission wheel at the upper end of the cleaning component, close to one end inside the shell, and the transmission gear is transmission-connected to the transmission wheel. The transmission gear is connected to the first cleaning rod by a belt.

[0015] More preferably, the titanium foil coil passes through two first cleaning rods, two second cleaning rods, two spray pipes, two third cleaning rods and two air jet pipes from top to bottom.

[0016] More preferably, the two first cleaning rods, the two second cleaning rods and the two third cleaning rods are all connected by belts.

[0017] Further preferably, a liquid storage tank is installed at the other side of the shell near the injection block and the spray pipe, and an air storage tank is fixedly connected to the other side of the shell near the two air injection pipes.

[0018] More preferably, the auxiliary components include:

[0019] The mounting base is fixedly connected to the bottom end of the shell.

[0020] The first discharge port is opened on one side of the shell, and the first discharge port is used to discharge the waste of the cut titanium foil coil.

[0021] There are two clamping blocks, which are symmetrically installed on both sides of the mounting seat along the length direction, and the two clamping blocks are used to clamp on both sides of the titanium foil coil.

[0022] The second discharge port is opened on one side of the mounting seat, and the second discharge port is used to discharge the cut titanium foil coil.

[0023] Further preferably, a protective door is hingedly installed on the placement shell, and the protective door is opened to place the titanium foil coil in the placement shell.

[0024] Compared with the prior art, the present invention has the following advantages: through the setting of a cleaning component, when the titanium foil coil is cut, the titanium foil coil passes through the interior of the cleaning component through the transmission wheel and extends to the position of the laser cutting component, the cleaning component cleans the surface of the titanium foil coil, improves the cleanliness of the titanium foil coil, and further improves the cutting effect of the titanium foil coil; through the setting of the transmission wheel, the titanium foil coil can be continuously driven to move when the titanium foil coil is cut, thereby improving the cutting efficiency of the titanium foil coil and reducing the labor intensity of people moving the titanium foil coil; and when cutting, the auxiliary component is used to separate the cut titanium foil coil, thereby improving the practicality of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 It is a structural schematic diagram of this embodiment;

[0026] Figure 2 Schematic diagram of the internal structure of the outer shell and the placement shell of this embodiment;

[0027] Figure 3 This is a schematic diagram of the cleaning component structure of this embodiment;

[0028] Figure 4 for Figure 3 The enlarged schematic diagram at A in the middle;

[0029] Figure 5 Schematic diagram of the auxiliary component structure of this embodiment.

[0030] Figure numerals: 1. outer shell; 2. placement shell; 3. protective door; 4. laser cutting assembly; 5. titanium foil coil; 6. cleaning assembly; 61. first cleaning rod; 62. second cleaning rod; 63. injection block; 64. spray pipe; 65. third cleaning rod; 66. jet pipe; 67. transmission gear; 7. transmission wheel; 8. auxiliary assembly; 81. mounting seat; 82. first discharge port; 83. clamping block; 84. second discharge port; 9. liquid storage tank; 10. air storage tank. DETAILED DESCRIPTION

[0031] A CNC laser cutting machine disclosed in the prior art includes a workbench, a laser cutting device, a CNC control panel, and an automatic normal line laser testing device. A CNC control panel is provided on one side of the workbench, a laser cutting device is provided on the workbench, and the automatic normal line laser testing device is located on one side of the laser cutting device. The CNC control panel is electrically connected to the laser cutting device, and the CNC control panel is electrically connected to the automatic normal line laser testing device. The CNC laser cutting machine is provided with a laser cutting device, which greatly improves the efficiency of the laser cutting process, makes the cutting process more accurate, has a simple structure, and is reasonably designed. However, when the above device is used to laser cut titanium foil materials, the titanium foil coil is not cleaned, and the titanium foil coil needs to be cleaned manually or by other mechanisms before laser cutting, which affects the cutting efficiency of the titanium foil coil, and the metal sheet needs to be placed manually during cutting, which increases the labor intensity of people.

[0032] Therefore, when the above device is used, the titanium foil coil cannot be cleaned, and the metal sheet needs to be placed manually, which affects the cutting efficiency of the titanium foil coil and increases the labor intensity of people.

[0033] In response to the above technical problems, this application has made the following designs and ideas: In order to solve the problems existing in the prior art, it is envisaged that a certain cleaning mechanism and transmission mechanism can have better effects of cleaning metal sheets and continuously moving metal sheets than the prior art, thereby achieving the purpose of improving cutting efficiency and continuously cutting metal.

[0034] The following is combined with Figures 1 to 5 The present invention is further described in detail.

[0035] A femtosecond laser cutting titanium foil material pre-processing device, such as Figure 1As shown, it includes a shell 1 and a placement shell 2 installed on the top of the shell 1 and a laser cutting component 4 arranged inside the shell 1. Specifically, the laser cutting component 4 is a prior art and is not limited in this application. A titanium foil coil 5 is arranged inside the placement shell 2. A cleaning component 6 is arranged at one end of the shell 1. Specifically, a cleaning chamber is arranged at one end of the shell 1. The cleaning component 6 is arranged in the cleaning chamber. The cleaning component 6 is used to clean the titanium foil coil 5. The titanium foil coil 5 passes through the cleaning component 6 and extends to the position of the laser cutting component 4. The laser cutting component 4 is used to To cut the titanium foil coil 5, transmission wheels 7 are rotatably installed at the inner bottom of the placement shell 2 and at the upper and lower ends of the cleaning component 6 at one end of the inner side of the outer shell 1. Specifically, a transmission wheel 7 is rotatably installed at the inner bottom of the placement shell 2, and transmission wheels 7 are rotatably installed at the upper and lower ends of the cleaning chamber. The three transmission wheels 7 are all driving wheels with an external power source. The titanium foil coil 5 is transmission-connected to multiple transmission wheels 7, and the transmission wheels 7 are used to drive the titanium foil coil 5 to move. An auxiliary component 8 is provided at the bottom of the outer shell 1, and the auxiliary component 8 is used to separate the cut titanium foil coil 5.

[0036] By setting up a cleaning component 6, when the titanium foil coil 5 is cut, the titanium foil coil 5 passes through the interior of the cleaning component 6 through the transmission wheel 7 and extends to the position of the laser cutting component 4. The cleaning component 6 cleans the surface of the titanium foil coil 5 to improve the cleanliness of the titanium foil coil 5 and further improve the cutting effect of the titanium foil coil 5. By setting up the transmission wheel 7, the titanium foil coil 5 can be continuously driven to move when the titanium foil coil 5 is cut, thereby improving the cutting efficiency of the titanium foil coil 5 and reducing the labor intensity of people moving the titanium foil coil 5. When cutting, the auxiliary component 8 is used to separate the cut titanium foil coil 5, thereby improving the practicality of the device.

[0037] Specifically, Figure 2 , Figure 3 and Figure 4 As shown, the cleaning assembly 6 includes:

[0038] There are two first cleaning rods 61 , which are symmetrically rotatably mounted on the upper part of one end of the inner part of the housing 1 . Furthermore, cleaning cloths are wound around the two first cleaning rods 61 .

[0039] There are two second cleaning rods 62 , which are symmetrically rotatably installed at one end of the inner side of the housing 1 near the bottom of the first cleaning rod 61 . A first cleaning rod 61 and a second cleaning rod 62 are connected by a belt. Furthermore, cleaning cloths are wrapped around the two second cleaning rods 62 .

[0040] There are two injection blocks 63 , which are symmetrically rotatably mounted at one end of the inner portion of the housing 1 near the upper portion of the second cleaning rod 62 . The two injection blocks 63 inject cleaning liquid into the second cleaning rod 62 . Specifically, the cleaning liquid is compatible with the titanium foil coil 5 .

[0041] There are two spray pipes 64 , which are symmetrically mounted at the middle position of one end of the housing 1 . The spray pipes 64 are used to spray cleaning liquid onto the surface of the titanium foil coil 5 . Specifically, the spray from the spray pipes 64 is in the shape of atomization.

[0042] There are two third cleaning rods 65, which are symmetrically rotatably installed at one end of the inner part of the shell 1 near the lower position of the spray pipe 64. The two third cleaning rods 65 are used to remove liquid from the surface of the titanium foil coil 5. A second cleaning rod 62 and a third cleaning rod 65 are connected by a belt. Furthermore, cleaning cloths are wrapped around the two third cleaning rods 65.

[0043] There are two jet pipes 66, which are symmetrically mounted at the bottom of one end of the housing 1. The two jet pipes 66 are used to remove liquid from the surface of the titanium foil coil 5. Furthermore, the temperature of the gas ejected from the jet pipe 66 is hot gas.

[0044] The transmission gear 67 is rotatably mounted at the bottom of the transmission wheel 7 at the upper end of the cleaning component 6 near one end of the inner portion of the housing 1 , and the transmission gear 67 is transmission-connected to the transmission wheel 7 , and the transmission gear 67 is belt-connected to the first cleaning rod 61 .

[0045] Furthermore, before cutting the titanium foil coil 5, the two first cleaning rods 61 pre-treat the two surfaces of the titanium foil coil 5, and then the liquid injection block 63 soaks the second cleaning rod 62, and the two second cleaning rods 62 re-treat the two surfaces of the titanium foil coil 5. Further, the spray pipe 64 rinses the two surfaces of the titanium foil coil 5 with clean water, and the two third cleaning rods 65 absorb the clean water remaining on the two surfaces of the titanium foil coil 5. Finally, the two air jet pipes 66 dry the clean water remaining on the two surfaces of the titanium foil coil 5, thereby improving the cleanliness of the titanium foil coil 5 before laser cutting of the titanium foil coil 5, and further improving the cutting effect of the titanium foil coil 5.

[0046] Specifically, Figure 3 As shown, the titanium foil coil 5 passes through two first cleaning rods 61, two second cleaning rods 62, two spray pipes 64, two third cleaning rods 65 and two air jet pipes 66 from top to bottom, and further, before laser cutting the titanium foil coil 5, the cleanliness of the titanium foil coil 5 is improved, and the cutting effect of the titanium foil coil 5 is further improved.

[0047] Specifically, Figure 3 As shown, the two first cleaning rods 61 , the two second cleaning rods 62 , and the two third cleaning rods 65 are all connected by belts, and further, the cleanliness of the titanium foil coil 5 is improved before cutting the titanium foil coil 5 .

[0048] Specifically, Figure 2 and Figure 3 As shown, a liquid storage tank 9 is installed at the other side of the shell 1 near the injection block 63 and the spray pipe 64, and an air storage tank 10 is fixedly connected to the other side of the shell 1 near the two air injection pipes 66.

[0049] Furthermore, the liquid storage tank 9 stores the liquid compatible with the titanium foil coil 5 inside the liquid injection block 63 and the clean water sprayed on the surface of the titanium foil coil 5 by the spray pipe 64 .

[0050] Specifically, Figure 5 As shown, the auxiliary component 8 includes:

[0051] The mounting base 81 is fixedly connected to the bottom end of the housing 1 .

[0052] The first discharge port 82 is opened at one side of the housing 1 , and is used to discharge waste of the cut titanium foil coil 5 .

[0053] There are two clamping blocks 83 , which are symmetrically installed on both sides of the mounting seat 81 along the length direction, and the two clamping blocks 83 are used to clamp on both sides of the titanium foil coil 5 .

[0054] The second discharge port 84 is provided at one side of the mounting seat 81 , and is used to discharge the cut titanium foil coil 5 .

[0055] Furthermore, after laser cutting of the titanium foil coil 5 is completed, the waste of the cut titanium foil coil 5 is discharged from the first discharge port 82, and the cut titanium foil workpiece is discharged from the second discharge port 84, thereby facilitating the separation of the processed titanium foil and further improving the practicability of the device.

[0056] Specifically, Figure 1 As shown, a protection door 3 is hingedly installed on the placement shell 2, and the protection door 3 is opened to place the titanium foil coil 5 in the placement shell 2.

[0057] How it works

[0058] When in use, the titanium foil coil 5 to be cut is placed in the placement shell 2, and the titanium foil coil 5 is sequentially passed through the two first cleaning rods 61, the two second cleaning rods 62, the two spray pipes 64, the two third cleaning rods 65 and the two air jet pipes 66 and extended to the position of the laser cutting assembly 4. At this time, the two first cleaning rods 61 pre-treat the two surfaces of the titanium foil coil 5, and then the injection block 63 soaks the second cleaning rod 62, and the two second cleaning rods 62 re-treat the two surfaces of the titanium foil coil 5. Further, the spray pipe 64 rinses the two surfaces of the titanium foil coil 5 with clean water, the two third cleaning rods 65 absorb the clean water remaining on the two surfaces of the titanium foil coil 5, and the two air jet pipes 66 finally dry the clean water remaining on the two surfaces of the titanium foil coil 5. At this time, the cleaned titanium foil coil 5 moves to the position of the laser cutting component 4, the laser cutting component 4 cuts the titanium foil coil 5, and the cut workpiece falls at the position of the second discharge port 84, and the cut titanium foil coil 5 waste is discharged from the first discharge port 82.

[0059] This specific embodiment is merely an explanation of the invention and is not a limitation of the invention. After reading this specification, those skilled in the art may make non-creative modifications to this embodiment as needed. However, as long as they are within the scope of protection of the invention, they are protected by patent law.

Claims

1. A femtosecond laser cutting titanium foil material pre-processing device, comprising a housing (1), a placement shell (2) installed on the top of the housing (1), and a laser cutting component (4) arranged inside the housing (1), characterized in that: A titanium foil coil (5) is arranged inside the placement shell (2), and a cleaning component (6) is arranged at one end inside the outer shell (1). The cleaning component (6) is used to clean the titanium foil coil (5). The titanium foil coil (5) passes through the interior of the cleaning component (6) and extends to the position of the laser cutting component (4). The laser cutting component (4) is used to cut the titanium foil coil (5). Transmission wheels (7) are rotatably installed at the inner bottom of the placement shell (2) and at the upper and lower ends of the cleaning component (6) at one end inside the outer shell (1). The titanium foil coil (5) is transmission-connected to a plurality of transmission wheels (7). The transmission wheels (7) are used to drive the titanium foil coil (5) to move. An auxiliary component (8) is arranged at the bottom of the outer shell (1). The auxiliary component (8) is used to separate the titanium foil coil (5) after cutting.

2. The femtosecond laser cutting titanium foil material pre-processing device according to claim 1 is characterized in that: The cleaning component (6) comprises: Two first cleaning rods (61) are symmetrically mounted on the upper part of one end of the housing (1); Two second cleaning rods (62) are symmetrically mounted at one end of the housing (1) near the bottom of the first cleaning rod (61), and one of the first cleaning rods (61) and one of the second cleaning rods (62) are connected by a belt; There are two injection blocks (63) which are symmetrically mounted at one end of the interior of the housing (1) near the upper portion of the second cleaning rod (62). The two injection blocks (63) inject cleaning liquid into the second cleaning rod (62); Two spray pipes (64) are symmetrically mounted at a middle position of one end of the inner portion of the housing (1), and the spray pipes (64) are used to spray cleaning liquid onto the surface of the titanium foil coil (5); There are two third cleaning rods (65), which are symmetrically mounted at one end of the inner part of the housing (1) near the lower part of the spray pipe (64). The two third cleaning rods (65) are used to remove liquid from the surface of the titanium foil coil (5). One of the second cleaning rods (62) and one of the third cleaning rods (65) are connected by a belt. There are two jet pipes (66) which are symmetrically mounted at the bottom of one end of the inner part of the housing (1). The two jet pipes (66) are used to remove liquid from the surface of the titanium foil coil (5); A transmission gear (67) is rotatably mounted at one end of the inner portion of the housing (1) and located at the bottom of the transmission wheel (7) at the upper end of the cleaning assembly (6), and the transmission gear (67) is transmission-connected to the transmission wheel (7). The transmission gear (67) is connected to the first cleaning rod (61) by a belt.

3. The pre-processing device for femtosecond laser cutting titanium foil material according to claim 2, characterized in that: The titanium foil coil (5) passes through, from top to bottom, the two first cleaning rods (61), the two second cleaning rods (62), the two spray pipes (64), the two third cleaning rods (65) and the two air jet pipes (66).

4. The femtosecond laser cutting titanium foil material pre-processing device according to claim 3 is characterized in that: The two first cleaning rods (61), the two second cleaning rods (62) and the two third cleaning rods (65) are all connected by belts.

5. The pre-processing device for femtosecond laser cutting titanium foil material according to claim 2, characterized in that: A liquid storage tank (9) is installed at a position close to the liquid injection block (63) and the spray pipe (64) on the other side of the shell (1), and an air storage tank (10) is fixedly connected at a position close to the two air injection pipes (66) on the other side of the shell (1).

6. The femtosecond laser cutting titanium foil material pre-processing device according to claim 1, characterized in that: The auxiliary component (8) comprises: A mounting seat (81) fixedly connected to the bottom end of the housing (1); A first discharge port (82) is provided on one side of the housing (1), and the first discharge port (82) is used to discharge waste of the titanium foil coil (5) after cutting; Two clamping blocks (83) are symmetrically mounted on both sides of the mounting seat (81) along the length direction, and the two clamping blocks (83) are used to clamp on both sides of the titanium foil coil (5); A second discharge port (84) is provided on one side of the mounting seat (81), and the second discharge port (84) is used to discharge the titanium foil coil (5) that has been cut.

7. The pre-processing device for femtosecond laser cutting titanium foil material according to claim 1, characterized in that: A protective door (3) is hingedly mounted on the placement shell (2), and the protective door (3) is opened to place the titanium foil coil (5) in the placement shell (2).