Method for synthesizing 2, 2 '-dinitrobibenzyl

By using paraffin oil and strong alkali-supported solid catalysts in the synthesis of 2,2'-dinitrobenzyl, combined with activated carbon or NaY molecular sieve, the equipment corrosion, low purity and high cost in traditional synthesis methods are solved. A highly efficient and low-pollution synthesis process is achieved, and the selectivity and conversion rate of products are improved.

CN118908838APending Publication Date: 2024-11-08GUANGXI JINYUAN BIOCHEMICAL IND CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410994268.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-24
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The traditional synthesis method of 2,2’-dinitrobenzyl is problematic of equipment corrosion, low product purity, large solvent usage, high cost and low yield, making it difficult to achieve environmentally friendly low pollution and high efficiency synthesis.

Method used

Using paraffin oil as solvent, using a strong alkali-supported solid catalyst with alkali metal or alkaline earth metal carbonate, acetate or hydroxide as active components, combined with activated carbon or NaY molecular sieve as support, control the reaction temperature and molar ratio, achieve efficient synthesis of 2,2'-dinitrobenzyl.

Benefits of technology

It improves the selectivity and conversion rate of products, reduces costs, and can reuse the catalyst, reduces pollution and equipment corrosion, and achieves an efficient and low-pollution synthesis process.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a method for synthesizing 2, 4-difluorobenzene. According to the method, o-nitrotoluene is taken as a raw material, paraffin oil is taken as a solvent, ethyl formate and an alkaline supported solid are taken as a catalyst, and the catalyst is a supported catalyst which takes carbonate, acetate or hydroxide of alkali metal or alkaline earth metal as an active component and takes activated carbon or a NaY molecular sieve as a carrier. When the catalyst is used for synthesizing 2, 2 '-dinitrobibenzyl under given test conditions, good raw material conversion rate and target product selectivity can be obtained, the conversion rate of o-nitrotoluene can reach 92%, and the selectivity of 2, 2'-dinitrobibenzyl reaches up to 98%. The invention provides a novel synthesis method, the catalyst can be recycled, the emission of pollutants is reduced, the method is suitable for industrial production, and the total yield can reach 90% or above.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for synthesizing 2,2'-dinitrobibenzyl in organic chemical industry, and specifically provides an environmentally friendly, low-pollution and high-efficiency method for synthesizing 2,2'-dinitrobibenzyl. Background Art

[0002] The conventional synthesis methods of 2,2'-dinitrobibenzyl are as follows: (i) o-nitrotoluene and o-nitrobenzaldehyde are mixed with ionic liquid and potassium hydroxide to generate 1,2-di(2-nitrophenyl)ethanol, which is then brominated with phosphorus tribromide to generate 1,2-di(2-nitrophenyl)ethyl bromide, and finally debrominated with sodium borohydride to obtain the target product. This method is highly corrosive to the production equipment due to the bromination reaction, and the product contains bromine; (ii) o-nitrotoluene is used as a raw material, petroleum ether is used as a solvent, ethyl formate and sodium methoxide are used to prepare the target product. This method has low product purity, large amount of three wastes, poor reaction control and easy material impact. This method is also the current mainstream method, but the total yield is only 73-75%, which is relatively low; (iii) o-nitrobenzyl chloride is used as a raw material, noble metals are used as catalysts, and the target product is prepared in the presence of a large amount of solvent and under the condition of light. This method uses a large amount of solvent, high cost, and is not conducive to market competition. Summary of the invention

[0003] The purpose of the present invention is to provide an environmentally friendly, low-pollution, and efficient method for synthesizing 2,2'-dinitrobibenzyl. Specifically, it is a method for synthesizing 2,2'-dinitrobibenzyl using o-nitrotoluene as a raw material, paraffin oil as a solvent, ethyl formate, and a strongly alkaline supported solid catalyst. The catalyst is a supported catalyst using an alkali metal or alkaline earth metal carbonate, acetate, or hydroxide as an active component and activated carbon or NaY molecular sieve as a carrier. The catalyst is insoluble in solvents such as water, paraffin oil, and xylene. The catalyst can be repeatedly used several times without losing its activity. The purpose of the present invention is achieved according to the following scheme:

[0004] A method for synthesizing 2,2'-dinitrobibenzyl is characterized in that the raw material used is o-nitrotoluene, the solvent used is paraffin oil, the catalyst used is ethyl formate and a strongly alkaline supported solid catalyst, the strongly alkaline solid catalyst uses carbonate, acetate or hydroxide of an alkali metal or alkaline earth metal as an active component, uses activated carbon or NaY molecular sieve as a carrier, the loading amount of the active component in the supported solid catalyst is 10% to 50% of the catalyst mass, the synthesis reaction temperature is 40 to 80°C, and the molar ratio of o-nitrotoluene to ethyl formate is 1 to 2:1.

[0005] The supported solid catalyst used has potassium carbonate as an active component.

[0006] The strongly alkaline supported solid catalyst is prepared by the following method: Prepare a solution of carbonate, acetate or hydroxide of alkali metal or alkaline earth metal with the same volume as the carrier, add activated carbon or NaY molecular sieve with a certain particle size of 20-80 mesh into it while stirring, stir evenly, put it into a vacuum dryer, immerse it for 16-24 hours, take it out and dry it at 150°C for 8-10 hours.

[0007] The loading amount of the carbonate, acetate or hydroxide of the alkali metal or alkaline earth metal active component of the supported solid catalyst is 30% of the catalyst mass.

[0008] The synthesis reaction is carried out in a rapidly stirred reactor with a stirring speed of more than 130 revolutions per minute and a reaction temperature of 40 to 80°C.

[0009] The molar ratio of the raw materials o-nitrotoluene and ethyl formate is 1-2:1.

[0010] The amount of the supported solid catalyst added is 35% of the mass of the raw material o-nitrotoluene, wherein the molar ratio of the raw materials o-nitrotoluene to ethyl formate is 1.4:1.

[0011] The catalyst is continuously applied and replaced in 50-100 batches.

[0012] The synthesis reaction temperature is 80°C or less.

[0013] The catalyst is insoluble in water, paraffin oil and xylene solvent.

[0014] Compared with the prior art, the present invention has the advantages of low toxicity of raw materials, simple and easy preparation of catalysts, high selectivity and conversion rate, and convenient post-processing of products. Strong alkaline solid catalysts can be reused, which greatly reduces costs. The conversion rate of o-nitrotoluene can reach 92%, and the selectivity of 2,2'-dinitrobibenzyl can reach 98%. DETAILED DESCRIPTION

[0015] The supported catalyst for synthesizing 2,2'-dinitrobibenzyl in the following examples was prepared as follows: Prepare a solution of alkali metal or alkaline earth metal carbonate, acetate or hydroxide with the same volume as the carrier, add activated carbon or NaY molecular sieve of a certain particle size (20-80 mesh) into it while stirring, stir evenly, put it into a vacuum dryer and soak it for 16-24 hours, then take it out and dry it at 150°C for 8-10 hours for use.

[0016] Example 1 To a stirred four-necked flask, 500 ml of paraffin oil was added, and at the same time, 150 g of a catalyst of 30% activated carbon-supported potassium carbonate was added. The catalyst was put into a bag and fixed on a stirring shaft. 585 g of a mixture of o-nitrotoluene and ethyl formate (mixing molar ratio of 1.4:1) was added dropwise. The addition lasted for 3 hours. The catalyst activity was evaluated under different temperature conditions. The reaction conditions were as follows: reaction temperature 40°C, raw material molar ratio (o-nitrotoluene: ethyl formate = 1.4:1), o-nitrotoluene conversion rate 80%, 2,2'-dinitrobibenzyl selectivity 96%.

[0017] Example 2 To a stirred four-necked flask, 500 ml of paraffin oil was added, and at the same time, 150 g of a catalyst of 5% activated carbon-supported potassium carbonate was added. The catalyst was put into a bag and fixed on a stirring shaft. 585 g of a mixture of o-nitrotoluene and ethyl formate (mixing molar ratio of 1.4:1) was added dropwise. The addition was completed over 6 hours. The catalyst activity was evaluated under different temperature conditions. The reaction conditions were as follows: reaction temperature 60°C, raw material molar ratio (o-nitrotoluene: ethyl formate = 1.4:1), o-nitrotoluene conversion rate 65%, 2,2'-dinitrobibenzyl selectivity 98%.

[0018] Example 3 To a stirred four-necked flask, 500 ml of paraffin oil was added, and at the same time, 150 g of a catalyst of 20% activated carbon-supported potassium carbonate was added. The catalyst was put into a bag and fixed on a stirring shaft. 585 g of a mixture of o-nitrotoluene and ethyl formate (mixing molar ratio of 1.4:1) was added dropwise. The addition lasted for 3 hours. The catalyst activity was evaluated under different temperature conditions. The reaction conditions were as follows: reaction temperature 60°C, raw material molar ratio (o-nitrotoluene: ethyl formate = 1.4:1), o-nitrotoluene conversion rate 75%, 2,2'-dinitrobibenzyl selectivity 97%.

[0019] Example 4 To a stirred four-necked flask, 500 ml of paraffin oil was added, and at the same time, 150 g of a catalyst of 50% activated carbon-supported potassium carbonate was added. The catalyst was put into a bag and fixed on a stirring shaft. 585 g of a mixture of o-nitrotoluene and ethyl formate (mixing molar ratio of 1.4:1) was added dropwise. The addition lasted for 3 hours. The catalyst activity was evaluated under different temperature conditions. The reaction conditions were as follows: reaction temperature 60°C, raw material molar ratio (o-nitrotoluene: ethyl formate = 1.4:1), o-nitrotoluene conversion rate 95%, 2,2'-dinitrobibenzyl selectivity 90%.

[0020] Example 5 To a stirred four-necked flask, 500 ml of paraffin oil was added, and at the same time, 150 g of a catalyst of 30% activated carbon-supported potassium carbonate was added. The catalyst was put into a bag and fixed on a stirring shaft. 585 g of a mixture of o-nitrotoluene and ethyl formate (mixed molar ratio of 1.4:1) was added dropwise. The addition was completed after 3 hours. The catalyst activity was evaluated under different temperature conditions. The reaction conditions were as follows: reaction temperature 60°C, raw material molar ratio (o-nitrotoluene: ethyl formate = 1.4:1), o-nitrotoluene conversion rate 92%, 2,2'-dinitrobibenzyl selectivity 98%.

[0021] Example 6 To a stirred four-necked flask, 500 ml of paraffin oil was added, and at the same time, 150 g of a catalyst of 30% activated carbon-supported potassium carbonate was added. The catalyst was put into a bag and fixed on a stirring shaft. 585 g of a mixture of o-nitrotoluene and ethyl formate (mixed molar ratio was 1.4:1) was added dropwise. The addition lasted for 3 hours. The catalyst activity was evaluated under different temperature conditions. The reaction conditions were as follows: reaction temperature 80°C, raw material molar ratio (o-nitrotoluene: ethyl formate = 1.4:1), o-nitrotoluene conversion rate 96%, and 2,2'-dinitrobibenzyl selectivity 80%.

[0022] Example 7 To a stirred four-necked flask, 500 ml of paraffin oil was added, and at the same time, 150 g of a catalyst of 30% activated carbon-supported potassium carbonate was added. The catalyst was put into a bag and fixed on a stirring shaft. 585 g of a mixture of o-nitrotoluene and ethyl formate (mixed molar ratio was 1.4:1) was added dropwise. The addition lasted for 3 hours. The catalyst activity was evaluated under different temperature conditions. The reaction conditions were as follows: reaction temperature 80°C, raw material molar ratio (o-nitrotoluene: ethyl formate = 1.4:1), o-nitrotoluene conversion rate 96%, and 2,2'-dinitrobibenzyl selectivity 80%.

Claims

1. A method for synthesizing 2,2'-dinitrobibenzyl, Features The raw material used is o-nitrotoluene, the solvent used is paraffin oil, the catalyst used is ethyl formate and a strongly alkaline supported solid catalyst, the strongly alkaline solid catalyst uses carbonate, acetate or hydroxide of an alkali metal or alkaline earth metal as an active component and uses activated carbon or NaY molecular sieve as a carrier, the loading amount of the active component in the supported solid catalyst used is 10% to 50% of the catalyst mass, the synthesis reaction temperature is 40 to 80°C, and the molar ratio of o-nitrotoluene to ethyl formate is 1 to 2:

1.

2. A method for synthesizing 2,2'-dinitrobibenzyl as claimed in claim 1, Features The supported solid catalyst used has potassium carbonate as an active component.

3. A method for synthesizing 2,2'-dinitrobibenzyl as claimed in claim 1, Features The strongly alkaline supported solid catalyst is prepared by the following method: Prepare a solution of carbonate, acetate or hydroxide of alkali metal or alkaline earth metal with the same volume as the carrier, add activated carbon or NaY molecular sieve with a certain particle size of 20-80 mesh into it while stirring, stir evenly, put it into a vacuum dryer, immerse it for 16-24 hours, take it out and dry it at 150°C for 8-10 hours.

4. A method for synthesizing 2,2'-dinitrobibenzyl as claimed in claim 1, Features The loading amount of the carbonate, acetate or hydroxide of the alkali metal or alkaline earth metal active component of the supported solid catalyst is 30% of the catalyst mass.

5. A method for synthesizing 2,2'-dinitrobibenzyl as claimed in claim 1, Features The synthesis reaction is carried out in a rapidly stirred reactor with a stirring speed of more than 130 revolutions per minute and a reaction temperature of 40 to 80°C.

6. A method for synthesizing 2,2'-dinitrobibenzyl as claimed in claim 1, Features The molar ratio of the raw materials o-nitrotoluene and ethyl formate is 1-2:

1.

7. A method for synthesizing 2,2'-dinitrobibenzyl as claimed in claim 1, Features The amount of the supported solid catalyst added is 35% of the mass of the raw material o-nitrotoluene, wherein the molar ratio of the raw materials o-nitrotoluene to ethyl formate is 1.4:

1.

8. A method for synthesizing 2,2'-dinitrobibenzyl as claimed in claim 1, Features The catalyst is continuously applied and replaced in 50-100 batches.

9. A method for synthesizing 2,2'-dinitrobibenzyl as claimed in claim 1, Features The synthesis reaction temperature is 80°C or less.

10. A method for synthesizing 2,2'-dinitrobibenzyl as claimed in claim 1, Features The catalyst is insoluble in water, paraffin oil and xylene solvent.