Composite material anti-dazzling plate for expressway

The anti-glare board with phenolic resin composite and reinforced fibers is solved, and the problem of poor durability of existing anti-glare board materials is achieved, high-strength, weather resistance and anti-glare effects are achieved, extending service life and reducing costs.

CN118909393APending Publication Date: 2024-11-08TIANJIN YONGBANG NEW MATERIALS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411188502.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-27
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The anti-glare board materials in the existing highway central partition facilities are heavy, fragile and poor durability, especially in high temperature wind and rain environments, which leads to poor anti-glare effect and increases the risk of traffic accidents.

Method used

Anti-glare boards are prepared using phenolic resin composite materials. By adding carbon fiber, glass fiber and curing agent, a highly rigid and corrosion-resistant board is formed, and ventilation through holes and reinforced cylinders are installed on the board to enhance wind resistance. Stainless steel connecting seat improves installation stability.

Benefits of technology

It provides high-strength, weather-resistant, fire-resistant, wind-proof and lightweight anti-glare boards, which can be used for a long time in high temperature and high cold environments, extend service life, reduce traffic accident risks, and reduce raw material costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118909393A_ABST
    Figure CN118909393A_ABST
Patent Text Reader

Abstract

The invention provides a composite material anti-dazzling plate for a highway, and relates to the field of highway capital construction equipment. The composite material anti-dazzling plate for the expressway comprises an anti-dazzling plate main body, and the preparation material of the anti-dazzling plate main body is a phenolic resin composite material. The phenolic resin composite material of the anti-dazzling plate main body is prepared from the following raw materials: phenolic resin, benzene dilute 36D, stearic acid, calcium powder, a carbon fiber reinforced raw material, a glass fiber reinforced raw material, magnesium oxide, a color paste additive and a curing agent. The phenolic aldehyde-based composite material is adopted as the plate material of the anti-dazzling plate, the anti-dazzling plate has good strength and toughness, the wood fiber has good toughness, it can be guaranteed that the anti-dazzling plate is not prone to being broken off when impacted by high-strength external force, meanwhile, due to the fact that phenolic resin forms a cross-linked network structure after being cured, the anti-dazzling plate has extremely high rigidity, and the anti-dazzling plate is not prone to being broken off. And it can be guaranteed that under the strong wind load, the swing amplitude of the anti-glare panel is not large, and the fatigue resistance is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of highway infrastructure equipment, in particular to a composite anti-glare plate for expressways. Background Art

[0002] When vehicles passing each other on the road at night, the strong light of their headlights will cause dazzle to the driver, causing the quality of visual information obtained by the driver to be significantly reduced, which is a potential factor inducing traffic accidents. The installation of anti-glare facilities can prevent dazzle from the headlights of oncoming vehicles, improve nighttime driving conditions, increase the driver's sight distance, eliminate the driver's nervousness when driving at night, reduce the traffic accident rate, and ensure driving safety. The existing central separation facilities of expressways are generally anti-glare plates and anti-glare nets. The anti-glare nets are mesh structures with poor anti-glare effects. The existing anti-glare plates are generally metal plates or plastic plates. Metal plates are relatively heavy and inconvenient to transport and install, while plastic plates have a relatively fragile structure and will accelerate aging in high temperature, windy and rainy extreme cold environments, resulting in a decrease in lifespan. Therefore, the present invention proposes an anti-glare plate of a phenolic resin composite material, thereby effectively solving the above-mentioned troubles and problems. Summary of the invention

[0003] 1. Technical issues to be resolved

[0004] In view of the deficiencies in the prior art, the present invention provides a composite anti-glare board for a highway, which can adopt phenolic-based composite materials as the board material of the anti-glare board. Since phenolic resin has excellent properties such as high bonding strength, water resistance, high temperature resistance, acid and alkali corrosion resistance, etc., the anti-glare board of the present invention has the characteristics of fire prevention, windproof, lightweight, high strength, corrosion resistance, and durability. It has good strength and toughness, and the wood fiber has good toughness, which can ensure that the anti-glare board will not be easily broken when subjected to high-intensity external force impact. At the same time, since the phenolic resin forms a cross-linked network structure after curing, it has extremely strong rigidity, which can ensure that the anti-glare board does not swing much under strong wind loads, thereby improving fatigue resistance.

[0005] (II) Technical solution

[0006] To achieve the above purpose, the present invention is implemented by the following technical scheme: a highway composite anti-glare board, comprising an anti-glare board body, the preparation material of the anti-glare board body is a phenolic resin composite material, the raw materials for making the phenolic resin composite material of the anti-glare board body are phenolic resin, styrene 36D, stearic zinc acid, calcium powder, carbon fiber reinforced raw material, glass fiber reinforced raw material, magnesium oxide, color paste additive and curing agent, wherein the weight ratio of phenolic resin is 80%, the weight ratio of carbon fiber reinforced raw material is 5%, the weight ratio of glass fiber reinforced raw material is 7%, the ratio of curing agent is 10% of the phenolic resin raw material, the phenolic resin is a thermosetting phenolic resin, and the preparation process of the phenolic resin composite material is:

[0007] S1: Mix phenolic resin and styrene 36D, and stir the mixed raw materials for 40 minutes to 60 minutes;

[0008] S2: After stirring, zinc stearate is added to the raw materials, and then calcium powder and curing agent are added, and stirred again for 40 minutes;

[0009] S3: adding the color paste additive and magnesium oxide to the stirred mixture, and then placing the mixture in a high-speed stirrer and stirring at a speed of 1000 rpm for more than one minute;

[0010] S4: After high-speed stirring is completed, the stirred mixed material is added to the glass fiber reinforced raw material and the carbon fiber reinforced raw material for mixing, and after the mixing is completed, the raw materials are pressed into a plate shape of an anti-glare board;

[0011] S5: Place the pressed sheet in a constant temperature box above 35 degrees Celsius for 24 hours;

[0012] S6: taking the formed sheet out of the constant temperature box after being placed for 24 hours, placing it in a hydraulic press, and baking it at a high temperature of 160 degrees Celsius for more than 3 hours;

[0013] S7: The baked formed sheet is taken out of the oven, put into a constant temperature box at 35 degrees Celsius and left to stand for 24 hours before being taken out;

[0014] S8: grinding and cutting the surface and periphery of the phenolic resin composite material plate, and after the treatment, the anti-glare plate of the phenolic resin composite material plate is manufactured;

[0015] Through the above technical scheme, the preparation material of the anti-glare plate is phenolic resin, which is prepared into a phenolic resin composite material by adding a curing agent, calcium powder and reinforcing raw materials. In the process of preparing the phenolic resin composite anti-glare plate of the present invention, carbon fiber, glass fiber and a curing agent are added, so that the unique chemical structure of the phenolic resin composite material gives it good physical and chemical properties, and it has high adhesion, heat resistance, ablation resistance, flame retardancy, acid resistance and electrical insulation, and is very suitable for use in outdoor devices.

[0016] Preferably, the anti-glare panel body is in the shape of a meandering S-shaped plate with thickness, five reinforcement cylinders are evenly distributed on the plate surface of the anti-glare panel body, the thickness of the five reinforcement cylinders is greater than the thickness of the anti-glare panel body, and a plurality of ventilation holes are provided on the anti-glare panel body;

[0017] Through the above technical scheme, the anti-glare panel is set as an S-shaped panel, which increases the wind resistance of the panel, and five cylindrical reinforcement bodies are provided on the panel to further enhance the wind resistance of the panel. A plurality of slender ventilation holes are provided on the anti-glare panel, so that when the panel faces strong winds, the force can be unloaded through the ventilation holes, allowing strong winds to pass through the ventilation holes, thereby reducing the wind resistance of the panel, and making the panel have better resistance when facing super strong winds, thereby extending the service life of the anti-glare panel.

[0018] Preferably, a connecting seat is fixedly provided at the bottom of the anti-glare plate body, the connecting seat is integrally cast with the anti-glare plate body, and four fixing screw holes are fixedly opened on the connecting seat;

[0019] Through the above technical solution, the bottom of the anti-glare plate has a thickened one-piece cast connection seat, the connection seat is a quadrangular pyramid, and a fixing screw hole is opened on the connection seat. The anti-glare plate is fixed to the mounting seat through the fixing screw hole.

[0020] Preferably, a mounting seat is provided at the bottom of the anti-glare plate body, and the anti-glare plate body is fixedly connected to the mounting seat by installing four fixing bolts in four fixing screw holes of the connecting seat.

[0021] Preferably, the mounting seat is fixed with two mounting screw holes, and the mounting seat is fixed to the roadbed guardrail of the highway by installing bolts on the two mounting screw holes, and the mounting seat is made of stainless steel;

[0022] Through the above technical solution, by providing a mounting seat at the bottom of the support seat, it can be well connected to the guardrail of the highway, and the mounting seat is made of stainless steel, which enhances the strength and durability of the mounting seat.

[0023] Preferably, the thickness of the anti-glare plate body is 3MM-5MM, the length is 900MM-1200MM, the width is 300MM-500MM, and the color of the anti-glare plate body is green;

[0024] Through the above technical solution, the anti-glare plate is set to green, which is in line with the relaxation of human visual nerves and has a good visual protection function for drivers traveling at high speeds. The thickness is 5MM but is set to S shape, which can enhance the overall thickness of the plate.

[0025] Working principle: The highway composite material anti-glare board is prepared by mixing phenolic resin as raw material, adding styrene 36D, stearic zinc acid, calcium powder, carbon fiber reinforcement raw material, glass fiber reinforcement raw material, magnesium oxide, color paste additive and curing agent, and mixing to prepare a phenolic resin composite material. The preparation process is as follows:

[0026] S1: Mix phenolic resin and styrene 36D, and stir the mixed raw materials for 40 minutes to 60 minutes;

[0027] S2: After stirring, zinc stearate is added to the raw materials, and then calcium powder and curing agent are added, and stirred again for 40 minutes;

[0028] S3: adding the color paste additive and magnesium oxide to the stirred mixture, and then placing the mixture in a high-speed stirrer and stirring at a speed of 1000 rpm for more than one minute;

[0029] S4: After high-speed stirring is completed, the stirred mixed material is added to the glass fiber reinforced raw material and the carbon fiber reinforced raw material for mixing, and after the mixing is completed, the raw materials are pressed into a plate shape of an anti-glare board;

[0030] S5: Place the pressed sheet in a constant temperature box above 35 degrees Celsius for 24 hours;

[0031] S6: taking the formed sheet out of the constant temperature box after being placed for 24 hours, placing it in a hydraulic press, and baking it at a high temperature of 160 degrees Celsius for more than 3 hours;

[0032] S7: The baked formed sheet is taken out of the oven, put into a constant temperature box at 35 degrees Celsius and left to stand for 24 hours before being taken out;

[0033] S8: grinding and cutting the surface and periphery of the phenolic resin composite material plate. After the treatment, the anti-glare plate of the phenolic resin composite material plate is manufactured.

[0034] After the phenolic resin composite material anti-glare sheet is manufactured, the mounting base is first installed on the guardrail of the highway. After it is fixed with bolts, the anti-glare sheet is inserted into the fixing groove of the supporting base, and then the anti-glare sheet is tightly fixed in the supporting base with fixing bolts.

[0035] (III) Beneficial effects

[0036] The present invention provides a composite anti-glare plate for a highway, which has the following beneficial effects:

[0037] 1. The present invention provides a composite anti-glare board for a highway. A phenolic-based composite material is used as the board material of the anti-glare board. Since phenolic resin has excellent properties such as high bonding strength, water resistance, high temperature resistance, acid and alkali corrosion resistance, etc., the anti-glare board of the present invention has the characteristics of fire prevention, windproof, lightweight, high strength, corrosion resistance, and durability. It has good strength and toughness. The wood fiber has good toughness, which can ensure that the anti-glare board will not break easily when subjected to high-intensity external force impact. At the same time, since the phenolic resin forms a cross-linked network structure after curing, it has extremely strong rigidity, which can ensure that the anti-glare board does not swing much under strong wind loads, thereby improving fatigue resistance.

[0038] 2. The present invention provides a composite anti-glare board for highways, which can meet the strict use requirements of high temperature, high cold, high humidity and other conditions for highways. The performance indicators such as mechanical strength, weather resistance and aging resistance can meet the requirements of "Technical Conditions for Highway Anti-glare Facilities" and "Anti-glare Boards". The phenolic resin anti-glare board has the advantages of excellent performance, low raw material cost and recyclable raw materials and waste. It has broad market prospects. At the same time, compared with plastic anti-glare boards and fiberglass anti-glare boards, the service life of the anti-glare board made of phenolic resin composite materials can be up to more than 5 years. Therefore, the average use cost of the phenolic resin wood composite anti-glare board is lower, and the economic benefits are significant.

[0039] 3. The present invention provides a composite anti-glare plate for highways, which is equipped with a mounting seat. An integrally cast connecting seat is provided at the bottom of the anti-glare plate. The connecting seat and the mounting seat are fixed to fix the anti-glare plate. The mounting seat is made of high-strength stainless steel. The mounting seat is installed on the guardrail of the highway to make the anti-glare plate more secure. BRIEF DESCRIPTION OF THE DRAWINGS

[0040] Figure 1 It is a front view of a composite anti-glare plate for a highway according to the present invention;

[0041] Figure 2 A side view of a composite anti-glare plate for a highway according to the present invention;

[0042] Figure 3 A plan view of a composite anti-glare plate for a highway according to the present invention;

[0043] Figure 4 The present invention is a process diagram for preparing a composite anti-glare plate for a highway.

[0044] Among them, 1. Anti-glare panel main body; 2. Reinforced cylinder; 3. Connecting seat; 4. Mounting seat; 5. Mounting screw hole; 6. Fixing screw hole; 7. Ventilation hole. DETAILED DESCRIPTION

[0045] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. In the description of this application, it should be noted that the terms used here are only for describing specific implementations, and are not intended to limit the exemplary implementations according to the present application. For ease of description, the sizes of the various parts shown in the drawings are not drawn according to the actual proportional relationship. The techniques, methods and devices known to ordinary technicians in the relevant fields may not be discussed in detail, but where appropriate, the techniques, methods and devices should be regarded as part of the authorization specification. In all examples shown and discussed here, any specific value should be interpreted as merely exemplary, not as a limitation. Therefore, other examples of the exemplary embodiments may have different values. It should be noted that similar reference numerals and letters represent similar items in the following drawings, so once an item is defined in one drawing, it does not need to be further discussed in subsequent drawings.

[0046] Embodiment 1:

[0047] like Figure 1-4 As shown, an embodiment of the present invention provides a highway composite material anti-glare board, a highway composite material anti-glare board, comprising an anti-glare board body 1, the preparation material of the anti-glare board body (1) is a phenolic resin composite material, the raw materials for making the phenolic resin composite material of the anti-glare board body 1 are phenolic resin, styrene 36D, stearic zinc acid, calcium powder, carbon fiber reinforcement raw material, glass fiber reinforcement raw material, magnesium oxide, color paste additive and curing agent, wherein the weight ratio of phenolic resin is 80%, the weight ratio of carbon fiber reinforcement raw material is 5%, the weight ratio of glass fiber reinforcement raw material is 7%, the ratio of curing agent is 10% of the phenolic resin raw material, the phenolic resin is a thermosetting phenolic resin, and the preparation process of the phenolic resin composite material is as follows:

[0048] S1: Mix phenolic resin and styrene 36D, and stir the mixed raw materials for 40 minutes to 60 minutes;

[0049] S2: After stirring, zinc stearate is added to the raw materials, and then calcium powder and curing agent are added, and stirred again for 40 minutes;

[0050] S3: adding the color paste additive and magnesium oxide to the stirred mixture, and then placing the mixture in a high-speed stirrer and stirring at a speed of 1000 rpm for more than one minute;

[0051] S4: After high-speed stirring is completed, the stirred mixed material is added to the glass fiber reinforced raw material and the carbon fiber reinforced raw material for mixing, and after the mixing is completed, the raw materials are pressed into a plate shape of an anti-glare board;

[0052] S5: Place the pressed sheet in a constant temperature box above 35 degrees Celsius for 24 hours;

[0053] S6: taking the formed sheet out of the constant temperature box after being placed for 24 hours, placing it in a hydraulic press, and baking it at a high temperature of 160 degrees Celsius for more than 3 hours;

[0054] S7: The baked formed sheet is taken out of the oven, put into a constant temperature box at 35 degrees Celsius and left to stand for 24 hours before being taken out;

[0055] S8: grinding and cutting the surface and periphery of the phenolic resin composite material plate. After the treatment, the anti-glare plate of the phenolic resin composite material plate is manufactured.

[0056] The shape of the anti-glare plate body 1 is a meandering S-shaped plate with thickness. Five reinforcing cylinders 2 are evenly distributed on the plate surface of the anti-glare plate body 1. The thickness of the five reinforcing cylinders 2 is greater than the thickness of the anti-glare plate body 1. A connecting seat 3 is fixedly provided at the bottom of the anti-glare plate body 1. The connecting seat 3 is integrally cast with the anti-glare plate body 1. Four fixing screw holes 6 are fixedly provided on the connecting seat 3. A mounting seat 4 is provided at the bottom of the anti-glare plate body 1. The anti-glare plate body 1 is fixedly connected to the mounting seat 4 by installing four fixing bolts in the four fixing screw holes 6 of the connecting seat 3. Two fixing screw holes 6 are fixedly provided on the mounting seat 4. The mounting base 4 is fixed on the roadbed guardrail of the highway by installing bolts on the two mounting screw holes 5. The mounting base 4 is made of stainless steel. The thickness of the anti-glare board body 1 is 3MM-5MM, the length is 900MM-1200MM, and the width is 300MM-500MM. The color of the anti-glare board body 1 is green. The preparation material of the anti-glare board is phenolic resin, which is prepared into a phenolic resin composite material by adding a curing agent, calcium powder and reinforcing raw materials. In the process of preparing the phenolic resin composite anti-glare board of the present invention, carbon fiber, glass fiber and a curing agent are added. The unique chemical structure of the phenolic resin composite material gives it good physical and chemical properties, with high adhesion, heat resistance, ablation resistance, flame retardancy, acid resistance and electrical insulation, and is very suitable for outdoor installations. The anti-glare panel is set as an S-shaped panel, which increases the wind resistance of the panel, and five cylindrical reinforcements are set on the panel to further enhance the wind resistance of the panel. A number of slender ventilation holes are opened on the anti-glare panel, so that when the panel faces strong winds, the force can be unloaded through the ventilation holes, allowing strong winds to pass through the ventilation holes, reducing the wind resistance of the panel, so that the panel can have a better performance when facing super strong winds. Good resistance, thereby extending the service life of the anti-glare plate. The bottom of the anti-glare plate has a thickened one-piece cast connecting seat. The connecting seat is a quadrangular pyramid. There are fixing screw holes on the connecting seat. The anti-glare plate is fixed to the mounting seat through the fixing screw holes. By arranging a mounting seat at the bottom of the support seat, it can be well connected to the guardrail of the highway, and the mounting seat is made of stainless steel to enhance the strength and durability of the mounting seat. The anti-glare plate is set to green, which is in line with the relaxation of human visual nerves and has good visual protection function for high-speed drivers. The thickness is 5MM but is set to S-type, which can enhance the overall thickness of the plate.

[0057] Embodiment 2:

[0058] like Figure 1-4 As shown, an embodiment of the present invention provides a composite anti-glare plate for a highway. After preparation, the anti-glare plate needs to be quality inspected and compared with anti-glare plates of other materials and the same size, and the test data is recorded.

[0059] First, the appearance quality inspection is carried out. The length is inspected. The inspection steps are as follows: make a plane projection of the sample, use a steel tape measure with a graduation value of 1mm, measure 3 values ​​at the maximum length position of the sample projection, and take the arithmetic mean as the measurement result. The width is inspected. The inspection steps are as follows: make a plane projection of the sample, use a steel ruler with a graduation value of 1mm, measure 3 measurement values ​​at the upper, middle and lower parts of the sample projection respectively, and take the arithmetic mean as the measurement result. The thickness of the plate is inspected. For samples with uniform plate thickness, use a micrometer with a graduation value of 0.02mm to measure 3 measurement values ​​in the middle and edge parts of the plate respectively, and take the arithmetic mean as the measurement result. It meets the standard.

[0060] The wind load resistance quality test of the anti-glare board is carried out. The bottom of the anti-glare board is fixed on the test platform, the middle of the board is clamped with a standard clamp, and the midpoint of the standard clamp is used as the mechanical traction point. The rigid connecting medium is used to firmly connect it to the traction system of the mechanical testing machine through the fixed pulley. The traction point should be in the same line with the lower edge of the fixed pulley, and the traction direction should be perpendicular to the board surface. When the connecting medium is completely relaxed, the board is pulled at a speed of 100mm / min until the board surface breaks or the maximum load is reached. The test is stopped. The maximum traction load is the wind load resistance of the sample. A total of 3 groups of tests are carried out in this way, and the arithmetic mean of the 3 test results is the test result.

[0061] The anti-deformation test of the anti-glare board is carried out. The test equipment is set with the same wind load. The anti-glare board is fixed on the test platform and well connected with the test machine. The projection S from the upper end of the board to the plane of the operating table is marked, and the test machine is started. The traction is carried out at a speed of 15mm / min. When the traction load reaches the wind load of the corresponding specification, the traction is stopped, and the applied load is removed to allow the anti-glare board to recover freely and elastically. After 5 minutes, the projection from the upper end of the board to the plane of the operating table is made, marked as S2, and the anti-deformation amount R of the anti-glare board can be expressed by the formula: R = (S1-S2) / H

[0062] R Deformation resistance, in millimeters per meter (mm / m)

[0063] S1 end projection displacement, in millimeters (mm)

[0064] S2 Initial projection displacement, in millimeters (mm).

[0065] The anti-glare panel is tested for impact resistance. The sample is placed under standard environmental conditions for 24 hours before the test. The sample should be placed flat on a hard surface or test bench. A 1kg steel ball is dropped freely from a height of 1m above the panel surface to impact the sample. It is ensured that the steel ball contacts the sample only once during the impact process. The impact point of each sample should be selected from the top, middle and bottom three parts for impact test, and the test results should be observed.

[0066] The anti-glare panel is subjected to an environmental adaptability test. The anti-glare panel is placed in an environmental simulation box with a high temperature upper limit of not less than 100°C, a low temperature lower limit of not higher than -40°C, a temperature fluctuation range of not more than ±1°C, a relative humidity of not less than 95%, and a relative humidity fluctuation range of not more than ±2.5% for 144 hours. The total irradiation energy is greater than 3.5×10000kJ / m 2 The artificial accelerated aging test was carried out to observe the aging phenomena such as discoloration, cracking, and powdering of the anti-glare panel.

[0067] After various performance tests, the comparison results are shown in the following table:

[0068] Table 1 Performance comparison of anti-glare panels made of various materials

[0069]

[0070] The comprehensive results show that the phenolic resin composite anti-glare panel can meet the strict use requirements of high temperature, high cold and high humidity on highways. The performance indicators such as mechanical strength, weather resistance and aging resistance can meet the requirements of "Technical Conditions for Highway Anti-glare Facilities" and "Anti-glare Panels". It has the characteristics of fireproof, windproof, lightweight, high strength, corrosion resistance and durability. It also has the advantages of excellent performance, low raw material cost and renewable raw materials and waste. It has broad market prospects.

[0071] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A composite anti-glare plate for a highway, comprising an anti-glare plate body (1), characterized in that: The preparation material of the anti-glare plate body (1) is a phenolic resin composite material. The raw materials for making the phenolic resin composite material of the anti-glare plate body (1) are phenolic resin, styrene 36D, stearic zinc acid, calcium powder, carbon fiber reinforcement raw material, glass fiber reinforcement raw material, magnesium oxide, color paste additive and curing agent. The weight ratio of the phenolic resin is 80%, the weight ratio of the carbon fiber reinforcement raw material is 5%, the weight ratio of the glass fiber reinforcement raw material is 7%, the ratio of the curing agent is 10% of the phenolic resin raw material, and the phenolic resin is a thermosetting phenolic resin. The preparation process of the phenolic resin composite material is as follows: S1: Mix phenolic resin and styrene 36D, and stir the mixed raw materials for 40 minutes to 60 minutes; S2: After stirring, zinc stearate is added to the raw materials, and then calcium powder and curing agent are added, and stirred again for 40 minutes; S3: adding the color paste additive and magnesium oxide to the stirred mixture, and then placing the mixture in a high-speed stirrer and stirring at a speed of 1000 rpm for more than one minute; S4: After high-speed stirring is completed, the stirred mixed material is added to the glass fiber reinforced raw material and the carbon fiber reinforced raw material for mixing, and after the mixing is completed, the raw materials are pressed into a plate shape of an anti-glare board; S5: Place the pressed sheet in a constant temperature box above 35 degrees Celsius for 24 hours; S6: taking the formed sheet out of the constant temperature box after being placed for 24 hours, placing it in a hydraulic press, and baking it at a high temperature of 160 degrees Celsius for more than 3 hours; S7: The baked formed sheet is taken out of the oven, put into a constant temperature box at 35 degrees Celsius and left to stand for 24 hours before being taken out; S8: grinding and cutting the surface and periphery of the phenolic resin composite material plate. After the treatment, the anti-glare plate of the phenolic resin composite material plate is manufactured.

2. The composite anti-glare plate for highway according to claim 1, characterized in that: The anti-glare panel body (1) is in the shape of a meandering S-shaped plate with thickness. Five reinforcing cylinders (2) are evenly distributed on the panel surface of the anti-glare panel body (1). The thickness of the five reinforcing cylinders (2) is greater than the thickness of the anti-glare panel body (1). The anti-glare panel body (1) is provided with a plurality of ventilation holes (7).

3. The composite anti-glare plate for highway according to claim 1, characterized in that: A connecting seat (3) is fixedly provided at the bottom of the anti-glare plate body (1); the connecting seat (3) and the anti-glare plate body (1) are integrally cast; and four fixing screw holes (6) are fixedly provided on the connecting seat (3).

4. The composite anti-glare plate for highway according to claim 1, characterized in that: A mounting seat (4) is provided at the bottom of the anti-glare panel body (1), and the anti-glare panel body (1) is fixedly connected to the mounting seat (4) by installing four fixing bolts in four fixing screw holes (6) of the connecting seat (3).

5. The composite anti-glare plate for highway according to claim 4, characterized in that: The mounting seat (4) is fixedly provided with two mounting screw holes (5), and the mounting seat (4) is fixed to the roadbed guardrail of the expressway by installing bolts on the two mounting screw holes (5). The mounting seat (4) is made of stainless steel.

6. The composite anti-glare plate for highway according to claim 1, characterized in that: The anti-glare plate main body (1) has a thickness of 3MM-5MM, a length of 900MM-1200MM, a width of 300MM-500MM, and a color of green.