Waterborne polyurethane paint and preparation method thereof

By using the technology of using magnesium-aluminum alloy core to coat polyvinyl chloride polymer film particles in water-based polyurethane paint, the problem of complex construction and poor anti-slip effect of self-leveling floor paint is solved, and simple construction and anti-slip effect are achieved. Significant and wear-resistant coating.

CN118909475AActive Publication Date: 2024-11-08WUXI YINGBO CHEM CO LTD

Patent Information

Application Number
CN202411007271.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-11-08
Estimated Expiration
2044-07-25

AI Technical Summary

Technical Problem

The existing anti-slip process of self-leveling floor paint has problems such as cumbersome construction process, poor anti-slip effect, easy material falls off and high cost.

Method used

Water-based polyurethane paint is used, which contains polyvinyl chloride polymer envelope particles coated with magnesium-aluminum alloy core. The particles are prepared by high-speed rotary granulation method and fluidized bed coating process, and are uniformly suspended in the coating to form a uniformly distributed convex. Points to improve anti-slip performance.

Benefits of technology

It achieves an anti-slip effect with simple construction process, significant anti-slip effect, wear and pressure resistance of materials, not easy to fall off, and low cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118909475A_ABST
    Figure CN118909475A_ABST
Patent Text Reader

Abstract

The invention discloses a waterborne polyurethane paint, which comprises 62-72 parts of polyurethane resin; 14 to 18 parts of dimethylaminoethyl methacrylate; 15 to 32 parts of metal core organic polymer coated particles; 13 to 32 parts of deionized water; 10-30 parts of a density control agent; 20-50 parts of a filler; 1 to 1.5 parts of a leveling agent; 0.5 to 0.7 part of a defoaming agent; 2-4 parts of a diluent; 0.8 to 1.4 parts of a dispersant; 16-22 parts of a curing agent; in addition to the surface anti-skid and anti-wear properties, the metal core organic polymer coating particles are uniformly dispersed and suspended in the self-leveling emulsion before the self-leveling paint is cured, so that after the self-leveling paint is cured, the metal core organic polymer coating particles are uniformly dispersed and suspended in the self-leveling emulsion before the self-leveling paint is cured; a large number of metal core organic polymer coated particles are uniformly embedded in the cured self-leveling coating in a three-dimensional space, so that the cured self-leveling coating has a remarkable structural supporting capability, and the compression resistance and deformation resistance of the coating are effectively improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of polyurethane coatings. Background Art

[0002] The anti-slip processes of existing self-leveling floor paints during the construction phase generally include the following:

[0003] 1. Surface roughening, the surface roughening process of the paint, including base treatment, primer application, roller coating of flat coating, and use of special roughening rollers or tools for roughening before the flat coating is dry; it includes a variety of construction processes, the process is cumbersome, and the construction requirements are high. The paint surface forms a delicate texture effect and has a certain anti-slip ability. When there is water accumulation, the anti-slip ability is reduced. The delicate raised texture of the paint surface itself is part of the paint. Its texture is not supported by a hard core and its strength is weak.

[0004] 2. The coating surface spreading method, on the basis of ordinary self-leveling, when the coating has not yet dried, evenly spread sand, gravel and anti-skid particles on the surface. After solidification, there are raised particles on the surface and you need to grasp the timing of sand spreading. Too early will cause the sand to sink too much in the paint surface, resulting in the failure to form surface protrusions. Too late will cause the paint surface to solidify, the sand cannot bond with the paint, and a large number of anti-skid bumps will form on the paint surface. It has strong anti-slip ability, but due to the high hardness of the sand and the sharp surface, it is easy to scratch the soles of the feet; at the same time, the sand on the paint surface is easy to fall off; and the spreading is not uniform.

[0005] 3. The closed layer method is to apply a closed coating film on the basis of the "surface spreading method". The process is more complicated than the "surface spreading method" of the paint, and the second coating construction process is added, and the cost is further increased. It improves the problem of the "surface spreading method" that the sand is hard and sharp, which is easy to scratch the soles of the feet, but it will easily cause the surface protrusions to be covered by the second coating construction process, thereby losing the anti-slip ability.

[0006] It can be seen that the above three common processes have certain disadvantages in construction technology and paint effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0007] Attached Figure 1 Schematic diagram of a part of the paint surface. Summary of the invention

[0008] Purpose of the invention: In order to overcome the deficiencies in the prior art, the present invention provides a water-based polyurethane paint and a preparation method thereof. The paint produced by the present invention has the characteristics of simple construction process and easy operation, and the discrete and evenly distributed convex points on the paint surface have an anti-slip effect on pedestrians.

[0009] Technical solution: To achieve the above-mentioned purpose, the water-based polyurethane paint of the present invention comprises 62-72 parts of polyurethane resin; 14-18 parts of dimethylaminoethyl methacrylate; 15-32 parts of metal core organic polymer coated particles; 13-32 parts of deionized water; 10-30 parts of density control agent; 20-50 parts of filler; 1-1.5 parts of leveling agent; 0.5-0.7 parts of defoaming agent; 2-4 parts of diluent; 0.8-1.4 parts of dispersant; and 16-22 parts of curing agent.

[0010] Furthermore, the metal core organic polymer coated particles are particles with a magnesium-aluminum alloy core coated with a layer of polymer coating.

[0011] Furthermore, the particle size range of the metal core organic polymer coated particles is 1.8 mm to 2.6 mm.

[0012] Furthermore, the polymer coating material of the metal core organic polymer coating particles is polyvinyl chloride.

[0013] Furthermore, the preparation method of the metal core organic polymer coated particles is:

[0014] S1-1, a metal granulator using a high-speed rotary granulation method, which uses a high-speed rotating rotor to cut, crush, squeeze and rub the magnesium-aluminum alloy material to gradually form uniform spherical or elliptical particles; the particle size of the final magnesium-aluminum alloy particles is controlled by adjusting the rotor speed, blade spacing and feed speed;

[0015] S1-2, the formed particles are sent into the screening system, the particles with qualified particle size are separated, and discharged through the discharge port, collected for standby use, and the unqualified particles will continue to remain in the equipment for re-crushing, and finally the magnesium-aluminum alloy particles with uniform particle size are obtained; the particle size range of the magnesium-aluminum alloy particles finally discharged from the discharge port is 1.7mm to 1.9mm;

[0016] S1-3, using a fluidized bed coating machine to uniformly coat the molten polyvinyl chloride on the outer surface of the magnesium-aluminum alloy particles obtained in S1-2 to obtain metal core organic polymer coated particles;

[0017] S1-4, selecting metal core organic polymer coated particles with qualified density.

[0018] Furthermore, the operation process of S1-4 is: prepare a solution with a density of Pa and b solution with a density of Pb, Pa>Pb; put the metal core organic polymer coated particles obtained in S1-3 into a solution, stir and let stand, then put all the floating metal core organic polymer coated particles in a solution into b solution, stir and let stand, all the metal core organic polymer coated particles sunk in b solution are metal core organic polymer coated particles with qualified density, and the density range of the metal core organic polymer coated particles with qualified density is Pb~Pa.

[0019] Furthermore, in the coating process of the fluidized bed coating machine in S1-3, the supply mass of polyvinyl chloride is assumed to be ma, the supply mass of the magnesium-aluminum alloy particles is assumed to be mb, the density of the polyvinyl chloride after cooling and solidification is P1, and the density of the magnesium-aluminum alloy particles is P2; the following quantitative relationship must be followed: assume Pc = (Pb + Pa) / 2, Pc = (ma + mb) / (ma / P1 + mb / P2), Pb = (Pc-0.02Pc), Pa = (Pc + 0.02Pc).

[0020] Further, S2-1, the weighed polyurethane resin, deionized water, dimethylaminoethyl methacrylate, diluent and dispersant are mixed, and stirred at 850 r / min to 1100 r / min for 60 min to 90 min;

[0021] S2-2, adding the weighed curing agent, leveling agent, defoaming agent and filler to the mixture obtained in S2-1, stirring at 1000 r / min to 1200 r / min for 60 min to 90 min;

[0022] S2-3, assume that the density of the emulsion is Px, and measure the density of the emulsion Px obtained at the end of S2-2 by a density meter. In the initial state, Px < Pc, and then gradually add a density control agent to the emulsion obtained in S2-2 according to a gradient, and stir at 800r / min to 900r / min in stages to gradually increase the density of the emulsion Px until Px = Pc;

[0023] S2-4, weigh the metal core organic polymer coated particles obtained at the end of S1-4, add them to the emulsion at the end of S2-3, and stir at 800r / min~900r / min for 15min~30min to make the metal core organic polymer coated particles evenly suspended in the emulsion at the end of S2-3; thereby preparing a polyurethane self-leveling anti-skid water coating with discrete suspended particles.

[0024] Beneficial effects: The coating produced by the present invention has the characteristics of simple construction process and easy operation, and the convex points on the paint surface are discretely and evenly distributed to prevent pedestrians from slipping; since each metal core organic polymer coated particle is an aluminum-magnesium core particle coated with a layer of polyvinyl chloride shell, the polyvinyl chloride shell not only has an anti-slip effect, but also the texture of the polyvinyl chloride shell is softer than stone or sand, harder than general resin particles, and its convex points are rounded, so as not to scratch the soles of pedestrians; at the same time, the polyvinyl chloride shell has a role in strengthening the corrosion resistance of the wrapped aluminum-magnesium alloy, and the polyvinyl chloride shell outside the metal core organic polymer coated particle is The olefin shell has a strong affinity with polyurethane and is not easy to fall off; the magnesium-aluminum alloy core of the metal core organic polymer coated particles effectively ensures the pressure resistance and wear resistance of the paint surface bumps; at the same time, in addition to having surface anti-slip and wear resistance, since the metal core organic polymer coated particles of the self-leveling paint are evenly dispersed and suspended in the self-leveling emulsion before curing before curing, after the self-leveling paint is cured, a large number of metal core organic polymer coated particles are evenly embedded in the cured self-leveling paint in three-dimensional space, which has a significant structural support capacity for the cured self-leveling itself, and effectively improves the coating's pressure resistance and deformation resistance. DETAILED DESCRIPTION

[0025] The present invention will be further described below in conjunction with the accompanying drawings.

[0026] A water-based polyurethane paint comprises 62-72 parts of polyurethane resin, 14-18 parts of dimethylaminoethyl methacrylate, 15-32 parts of metal core organic polymer coated particles, 13-32 parts of deionized water, 10-30 parts of density control agent, 20-50 parts of filler, 1-1.5 parts of leveling agent, 0.5-0.7 parts of defoaming agent, 2-4 parts of diluent, 0.8-1.4 parts of dispersant and 16-22 parts of curing agent.

[0027] In the embodiment, the density control agent described above is barite powder (BaSO4); the filler is one or more of wollastonite, titanium dioxide, alumina, and polytetrafluoroethylene wax; the leveling agent is polyether polyester modified organic siloxane; the defoaming agent is a polyether type defoaming agent; the diluent is phenyl glycidyl ether; the curing agent is toluene diisocyanate; and the dispersant is sodium polycarboxylate.

[0028] The metal core organic polymer coated particles are particles with a magnesium aluminum alloy core coated with a layer of polymer coating; the particle size range of the metal core organic polymer coated particles is 1.8mm to 2.6mm; the polymer coating material of the metal core organic polymer coated particles is polyvinyl chloride.

[0029] Preparation method of metal core organic polymer coated particles:

[0030] S1-1, a metal granulator using a high-speed rotary granulation method, which uses a high-speed rotating rotor to cut, crush, squeeze and rub the magnesium-aluminum alloy material to gradually form uniform spherical or elliptical particles; the particle size of the final magnesium-aluminum alloy particles is controlled by adjusting the rotor speed, blade spacing and feed speed;

[0031] S1-2, the formed particles are sent into the screening system, the particles with qualified particle size are separated, and discharged through the discharge port, collected for standby use, and the unqualified particles will continue to remain in the equipment for re-crushing, and finally the magnesium-aluminum alloy particles with uniform particle size are obtained; the particle size range of the magnesium-aluminum alloy particles finally discharged from the discharge port is 1.7mm to 1.9mm;

[0032] S1-3, using a fluidized bed coating machine to uniformly coat the molten polyvinyl chloride on the outer surface of the magnesium-aluminum alloy particles obtained in S1-2 to obtain metal core organic polymer coated particles;

[0033] S1-4, sorting out metal core organic polymer coated particles with qualified density by density sorting method.

[0034] Preset Pc = 1.65g / cm 3 , Pc is the target density of the metal core organic polymer coated particles (under ideal conditions); in the coating process of the fluidized bed coating machine in S1-3, the supply mass of polyvinyl chloride is ma, the supply mass of magnesium-aluminum alloy particles is mb, the density of polyvinyl chloride is P1, and the density of polyvinyl chloride in this case is 1.4 g / cm 3 The particle density of magnesium-aluminum alloy is P2, and the density of magnesium-aluminum alloy is usually 1.3-1.9 g / cm 3 In this case, a relatively high-density magnesium-aluminum alloy is used, and the specific density of the aluminum alloy particles is 1.75g / cm 3 ; It is necessary to follow Pc=(ma+mb) / (ma / P1+mb / P2), so that in an ideal state, the density of all metal core organic polymer coated particles obtained by the coating process of the fluidized bed coating machine is exactly Pc. Since the coating process of the fluidized bed coating machine has certain process errors, the density of the metal core organic polymer coated particles actually obtained is different, and fluctuates up and down on the basis of Pc. The density range of metal core organic polymer coated particles with qualified density is Pb~Pa; Set Pc=(Pb+Pa) / 2, Pb=(Pc-0.02Pc), Pa=(Pc+0.02Pc); According to the set value of Pc, the values ​​of Pa and Pb are obtained in combination with the above quantitative relationship;

[0035] The operation process of the density sorting method in S1-4 is as follows: prepare and mix a solution with a density of Pa and b solution with a density of Pb; put the metal core organic polymer coated particles obtained in S1-3 into a solution, stir and let it stand, then put all the floating metal core organic polymer coated particles in a solution into b solution, stir and let it stand, all the metal core organic polymer coated particles sunk in b solution are metal core organic polymer coated particles with qualified density, and the density range of the metal core organic polymer coated particles with qualified density is Pb~Pa. From the above mathematical relationship, it can be seen that all the metal core organic polymer coated particles with qualified density obtained after S1-4 are within Pc=1.65g / cm 3 The fluctuation range is no more than 2% of the Pc value, which provides a basis for the subsequent suspension effect.

[0036] S2-1, mix the weighed polyurethane resin, deionized water, dimethylaminoethyl methacrylate, diluent and dispersant, and stir at 850 r / min to 1100 r / min for 60 min to 90 min.

[0037] S2-2, add the weighed curing agent, leveling agent, defoaming agent and filler to the mixture obtained in S2-1, and stir at 1000 r / min to 1200 r / min for 60 min to 90 min.

[0038] S2-3, let the density of the emulsion be Px, and measure the density of the emulsion Px obtained at the end of S2-2 by a densitometer. The actual value of Px measured in the initial state is 1.45 g / cm 3 , Px<Pc, then gradually add density control agent (barite powder) to the emulsion obtained in S2-2 according to the gradient, and stir at 800r / min~900r / min in stages to gradually increase the density of the emulsion Px until Px=Pc=1.65g / cm 3 .

[0039] S2-4, weigh the metal core organic polymer coated particles obtained at the end of S1-4 and add them to the density at the end of S2-3, which is exactly Pc = 1.65 g / cm 3 The emulsion was stirred at 800r / min~900r / min for 15min~30min. Since all the qualified density metal core organic polymer coated particles obtained by S1-4 were within Pc=1.65g / cm 3 Since the emulsion at the end of S2-3 has a certain viscosity, the metal core organic polymer coated particles will be evenly suspended in the emulsion at the end of S2-3; thus, a polyurethane self-leveling anti-skid water-based paint with discrete suspended particles is obtained and finally filled.

[0040] An embodiment of the above polyurethane self-leveling anti-skid water-based coating is shown in the following table by weight:

[0041] Components Weight Polyurethane resin 66 Dimethylaminoethyl methacrylate 16 Metal core organic polymer coated particles 20 Deionized water 22 Density control agent (barite powder) 16 Leveling agent (polyether polyester modified organosiloxane) 1 Defoamer (polyether defoamer) 0.6 Diluent (phenyl glycidyl ether) 3 Dispersant (sodium polycarboxylate) 1 Curing agent (toluene diisocyanate) 18 Filler 1 (wollastonite) 10 Filler 2 (alumina) 12 Filler 3 (PTFE wax) 12

[0042] Usage method and technical effect of polyurethane self-leveling anti-skid water-based coating:

[0043] Before self-leveling, the canned polyurethane self-leveling anti-skid water-based paint with discrete suspended particles should be properly shaken or stirred, and then self-leveled on the ground to form a paint surface. During the curing process, due to water evaporation and other reasons, the paint surface will automatically shrink inward during the curing process, so that some of the metal core organic polymer coating particles in the paint that are discrete and evenly distributed will be evenly distributed on the surface of the self-leveling paint in the form of convex points. Figure 1 As shown in the figure, the discrete and evenly distributed convex points on the cured paint surface have an anti-slip effect on pedestrians, especially when there is water on the paint surface, it can effectively prevent pedestrians from falling; because each metal core organic polymer coating particle is an aluminum-magnesium core particle covered with a layer of polyvinyl chloride shell, the polyvinyl chloride shell not only has an anti-slip effect, but also the texture of the polyvinyl chloride shell is softer than stone or sand, harder than ordinary resin particles, and its convex points are rounded, so they will not scratch the soles of pedestrians; at the same time, the polyvinyl chloride shell has a role in strengthening the corrosion protection of the wrapped aluminum-magnesium alloy, and the polyvinyl chloride shell outside the metal core organic polymer coating particle The ethylene shell has a strong affinity with polyurethane and is not easy to fall off; the magnesium-aluminum alloy core of the metal core organic polymer coated particles effectively ensures the pressure resistance and wear resistance of the paint surface bumps; at the same time, in addition to having surface anti-slip and wear resistance, since the metal core organic polymer coated particles of the self-leveling paint are evenly dispersed and suspended in the self-leveling emulsion before curing, after the self-leveling paint is cured, a large number of metal core organic polymer coated particles are evenly embedded in the cured self-leveling paint in three-dimensional space, which has a significant structural support capacity for the cured self-leveling itself, and effectively improves the coating's pressure resistance and deformation resistance.

[0044] The comparison of the anti-slip process with the existing self-leveling floor paint is as follows:

[0045]

[0046]

[0047]

[0048] It can be seen from the above table that this solution has significant advantages over the existing anti-slip construction technology in terms of both the difficulty of construction and the final paint effect.

[0049] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.

Claims

1. A water-based polyurethane paint, Features: The invention comprises 62-72 parts of polyurethane resin, 14-18 parts of dimethylaminoethyl methacrylate, 15-32 parts of metal core organic polymer coated particles, 13-32 parts of deionized water, 10-30 parts of density control agent, 20-50 parts of filler, 1-1.5 parts of leveling agent, 0.5-0.7 parts of defoaming agent, 2-4 parts of diluent, 0.8-1.4 parts of dispersant and 16-22 parts of curing agent.

2. A waterborne polyurethane paint according to claim 1, Features: The metal core organic polymer coated particles are particles with a magnesium-aluminum alloy core coated with a layer of polymer coating.

3. A waterborne polyurethane paint according to claim 2, Features: The particle size range of the metal core organic polymer coated particles is 1.8 mm to 2.6 mm.

4. A water-based polyurethane paint according to claim 3, Features: The polymer coating material of the metal core organic polymer coated particles is polyvinyl chloride.

5. A method for preparing a waterborne polyurethane paint according to claim 4, Features: The preparation method of the metal core organic polymer coated particles: S1-1, a metal granulator using a high-speed rotary granulation method, which uses a high-speed rotating rotor to cut, crush, squeeze and rub the magnesium-aluminum alloy material to gradually form uniform spherical or elliptical particles; the particle size of the final magnesium-aluminum alloy particles is controlled by adjusting the rotor speed, blade spacing and feed speed; S1-2, the formed particles are sent into the screening system, the particles with qualified particle size are separated, and discharged through the discharge port, collected for standby use, and the unqualified particles will continue to remain in the equipment for re-crushing, and finally the magnesium-aluminum alloy particles with uniform particle size are obtained; the particle size range of the magnesium-aluminum alloy particles finally discharged from the discharge port is 1.7mm to 1.9mm; S1-3, using a fluidized bed coating machine to uniformly coat the molten polyvinyl chloride on the outer surface of the magnesium-aluminum alloy particles obtained in S1-2 to obtain metal core organic polymer coated particles; S1-4, selecting metal core organic polymer coated particles with qualified density.

6. A method for preparing a waterborne polyurethane paint according to claim 4, Features: The operation process of S1-4 is as follows: prepare a solution with a density of Pa and b solution with a density of Pb, Pa>Pb; put the metal core organic polymer coated particles obtained in S1-3 into a solution, stir and let stand, then put all the floating metal core organic polymer coated particles in a solution into b solution, stir and let stand, all the metal core organic polymer coated particles sunk in b solution are metal core organic polymer coated particles with qualified density, and the density range of the metal core organic polymer coated particles with qualified density is Pb~Pa.

7. A method for preparing a waterborne polyurethane paint according to claim 6, Features: In the coating process of the fluidized bed coating machine in S1-3, let the supply mass of polyvinyl chloride be ma, the supply mass of magnesium-aluminum alloy particles be mb, the density of polyvinyl chloride after cooling and solidification be P1, and the density of magnesium-aluminum alloy particles be P2; the following quantitative relationship must be followed: let Pc = (Pb + Pa) / 2, Pc = (ma + mb) / (ma / P1 + mb / P2), Pb = (Pc-0.02Pc), Pa = (Pc + 0.02Pc).

8. A method for preparing a waterborne polyurethane paint according to claim 7, Features: S2-1, mixing the weighed polyurethane resin, deionized water, dimethylaminoethyl methacrylate, diluent and dispersant, and stirring at 850 r / min to 1100 r / min for 60 min to 90 min; S2-2, adding the weighed curing agent, leveling agent, defoaming agent and filler to the mixture obtained in S2-1, stirring at 1000 r / min to 1200 r / min for 60 min to 90 min; S2-3, assume that the density of the emulsion is Px, and measure the density of the emulsion Px obtained at the end of S2-2 by a density meter. In the initial state, Px < Pc, and then gradually add a density control agent to the emulsion obtained in S2-2 according to a gradient, and stir at 800r / min to 900r / min in stages to gradually increase the density of the emulsion Px until Px = Pc; S2-4, weigh the metal core organic polymer coated particles obtained at the end of S1-4, add them to the emulsion at the end of S2-3, and stir at 800r / min~900r / min for 15min~30min to make the metal core organic polymer coated particles evenly suspended in the emulsion at the end of S2-3; thereby preparing a polyurethane self-leveling anti-skid water coating with discrete suspended particles.

Citation Information

Patent Citations

  • High-hardness two-component waterborne polyurethane floor paint and preparing method thereof

    CN105820738A

  • Preparation method of heat-conducting flame-retardant soft polyvinyl chloride

    CN107793671A

  • Aqueous dispersion, production method therefor, and image formation method

    CN107849349A

  • Graphene water-based super-wear-resisting floor paint and preparation method thereof

    CN108059860A

  • Liquid metal microparticles with core-shell structures and preparation method and application thereof

    CN109570515A

Cited By

  • Anti-crack polyurethane paint coating and process thereof

    CN119264713A