Vibration electroplating device and vibration electroplating system

By setting screen holes and material separation channels in the vibration disk, the problem of small flow of the plating solution in the vibration electroplating device is solved, the deposition speed of the anode metal ions and the plating quality are improved, and a more efficient plating process and better Product quality.

CN118910700APending Publication Date: 2024-11-08佘世尧
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411265485.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-10
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The plating solution flow in existing vibrating electroplating devices is small, resulting in slow deposition of anode metal ions and is prone to oxidation during the deposition process, resulting in poor plating quality.

Method used

By setting screen holes on the bottom plate and side wall of the vibration disk and setting a material part to form a channel in the vibration disk, the flow of the electroplating solution is increased, the deposition rate and deposition amount of anode metal ions on the product surface are increased, and the risk of oxidation is reduced. Ensure uniformity and integrity of the coating.

Benefits of technology

It improves the quality of the plating and the weldability performance of the products after electroplating, increases the number of single-selectroplating products, reduces the risk of oxidation, and improves the uniformity and integrity of the plating.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118910700A_ABST
    Figure CN118910700A_ABST
Patent Text Reader

Abstract

The invention provides a vibration electroplating device and a vibration electroplating system. The device comprises a rotating shaft, a vibration disc and a plurality of groups of cathode columns, the rotating shaft is connected with a vibration source; the side wall of the vibration disc is arranged on the bottom plate in a surrounding mode to form a containing cavity, and the rotating shaft extends into the containing cavity and is connected with the bottom plate. Screen holes are formed in a bottom plate and / or the side wall of the vibration disc. The bottom plate comprises a low-position area, a transition area and a high-position area which are sequentially arranged in the spiral direction of the vibration source. A material distributing piece of the vibration disc is arranged in the containing cavity and located above the low-position area, and the two ends of an arc-shaped bridge surface of the material distributing piece communicate with the high-position area and the transition area correspondingly; the cathode column extends into the containing cavity and is exposed out of the bottom plate. The flow amount of the electroplating liquid can be increased, the risk of an oxidation phenomenon in the deposition process is reduced, the exchangeability of a product and an electroplating medium in the vibration disc is improved, and the quality of a plating layer and the product is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of vibration electroplating, and in particular to a vibration electroplating device and a vibration electroplating system. Background Art

[0002] In the production process of ceramic components such as MLCC (chip multilayer ceramic capacitors), it is necessary to electroplate certain areas on their surfaces to form corresponding coatings. At present, the industry generally adopts a vibration plating process for electroplating, that is, the product is placed on a vibration plate, and then the vibration plate is immersed in a plating solution. The vibration source drives the vibration plate to vibrate, so that the plating solution flows on the surface of the product and deposits the anode metal ions on the surface of the product, thereby forming a coating. However, in existing vibration plating devices, the vibration plate is provided with fewer sieve holes, and even some manufacturers' vibration plates are not provided with sieve holes but only exchange electrolyte through the opening at the upper end. This results in fewer plating solution flow channels inside and outside the vibration plate, a small flow rate of the plating solution, a slow deposition rate of the anode metal ions on the surface of the product, and an insufficient deposition amount. In particular, oxidation is prone to occur during the deposition process, resulting in poor coating quality and reduced product solderability, which seriously threatens product quality. Summary of the invention

[0003] In view of this, the present application provides a vibration electroplating device and a vibration electroplating system, which can improve the problem of small flow rate of electroplating solution in existing vibration electroplating devices, and the resulting slow deposition of anode metal ions and easy oxidation during the deposition process, resulting in poor coating quality.

[0004] The present application provides a vibration electroplating device, comprising:

[0005] A rotating shaft, one end of which is used to connect to a vibration source;

[0006] A vibration plate, comprising a bottom plate, a side wall and a material dividing piece provided with an arc-shaped bridge surface; the side wall is arranged on the bottom plate to form a receiving cavity, and the other end of the rotating shaft extends into the receiving cavity and is connected to the bottom plate; the bottom plate and / or the side wall are provided with sieve holes; the bottom plate comprises a low-position area, a transition area and a high-position area arranged in sequence along the spiral direction of the vibration source; the material dividing piece is arranged in the receiving cavity and is located above the low-position area, and the two ends of the arc-shaped bridge surface are respectively connected to the high-position area and the transition area to form a channel passing through the bottom of the material dividing piece and connecting the high-position area and the transition area;

[0007] A plurality of cathode columns extend into the receiving cavity and are exposed to the bottom plate.

[0008] Optionally, at least one of the following is met:

[0009] The diameter of the sieve hole provided on the side wall is larger than the diameter of the sieve hole provided on the bottom plate;

[0010] The sieve holes provided on the side wall are arranged on the side wall in a spiral shape along the spiral direction;

[0011] The sieve holes arranged on the side wall are evenly arranged in an array on the side wall.

[0012] Optionally, the material dividing piece is provided with an inner baffle plate, which is located on the side of the arc-shaped bridge deck close to the rotating shaft, and is arranged opposite to the rotating shaft at one end facing the transition zone to form a gap; the vibration electroplating device also includes a first block, which blocks the gap.

[0013] Optionally, along a direction perpendicular to the bottom plate, a side of the first stopper facing away from the rotation axis has the same curvature as that of the inner baffle.

[0014] Optionally, on the radius of the vibration plate where the entrance of the channel is located, the width of the entrance of the channel is d1, the length from the side wall to the channel is d2, and d1 <d2。

[0015] Optionally, the material dividing member is provided with an inner baffle plate, which is located on a side of the arc-shaped bridge deck close to the rotating shaft, and one end of the inner baffle plate facing the transition zone is connected to the rotating shaft.

[0016] Optionally, the material dividing member is provided with an outer baffle plate, which is located on the side of the curved bridge deck close to the side wall; the vibration electroplating device also includes a second stopper, which is provided at the connection between the outer baffle plate and the side wall but does not block the channel.

[0017] Optionally, the second stopper is flush with the top of the outer baffle, or the top surface of the second stopper is an inclined surface, and the height of the inclined surface gradually decreases along the side wall toward the rotation axis.

[0018] Optionally, one end of the arc-shaped bridge deck connected to the transition zone is suspended relative to the transition zone; and / or one end of the high-position zone connected to the channel is suspended relative to the low-position zone.

[0019] Optionally, the end of the arc-shaped bridge deck connected to the transition zone has a suspended height relative to the transition zone of H1, and 2 cm

[0020] The present application also provides a vibration electroplating system, comprising a vibration source, an anode and any one of the vibration electroplating devices described above, wherein the vibration source is connected to the rotating shaft, and the anode can extend to the plating liquid in the receiving chamber and form a closed-loop circuit with the cathode column through the plating liquid. ​

[0021] As described above, the present application provides sieve holes on the bottom plate and / or side walls of the vibration plate to increase the flow channels of the plating solution inside and outside the vibration plate, thereby increasing the flow rate of the plating solution, thereby increasing the deposition rate and deposition amount of the anode metal ions on the product surface, reducing the risk of oxidation during the deposition process, and thus helping to improve the quality of the coating and the product after electroplating.

[0022] In addition, a channel is formed by the material dividing piece arranged in the vibration plate. When the product runs through the material dividing piece, the product in the inner circle of the vibration plate and the product in the outer circle of the vibration plate are evenly exchanged. The coating of the product plated by vibration is uniform and the coating at the end of the product is complete, thereby further improving the quality of the coating and the product after electroplating.

[0023] In addition, by setting a first block to seal the gap between the inner baffle plate of the material dividing piece and the rotating shaft, or setting the inner baffle plate of the material dividing piece to be connected to the rotating shaft, a dead angle between the inner baffle plate of the material dividing piece and the rotating shaft can be avoided, thereby avoiding the product from being trapped in the dead angle and affecting the electroplating quality. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 A structural top view of a vibration electroplating device provided in an embodiment of the present application;

[0025] Figures 2 to 4 The structural side views of three different viewing angles of a vibration electroplating device provided in an embodiment of the present application;

[0026] Figure 5 A top view of the structure of another vibration electroplating device provided in an embodiment of the present application.

[0027] A first direction x, a second direction y and a third direction z

[0028] Vibration plating device 1

[0029] Rotating shaft 11

[0030] Flange ring 111

[0031] Vibration plate 12

[0032] Screen hole 120 Bottom plate 121 Side wall 122 Material dividing piece 123

[0033] Inner baffle 124 Outer baffle 125 First baffle 126 Second baffle 127

[0034] Support block 128

[0035] Low area 12a transition area 12b high area 12c curved bridge deck 12d channel 12e

[0036] Multiple cathode columns 13

[0037] The first group of cathode columns 131 The second group of cathode columns 132 The third group of cathode columns 133 DETAILED DESCRIPTION

[0038] In order to solve the above problems existing in the prior art, the present application provides a vibration electroplating device and a vibration electroplating system. The two protection themes are based on the same concept, and the principles of solving the problems are basically the same or similar. The implementation methods of each protection theme can refer to each other, and the repeated parts will not be repeated.

[0039] In order to make the purpose, technical solutions and advantages of the present application clearer, the technical solutions of the present application will be clearly described below in conjunction with specific embodiments and corresponding drawings. Obviously, the embodiments described below are only part of the embodiments of the present application, not all of the embodiments. In the absence of conflict, the following embodiments and their technical features can be combined with each other and also belong to the technical solutions of the present application.

[0040] In the description of the embodiments of the present application, terms such as "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", and "counterclockwise" indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the technical solutions of the corresponding embodiments, rather than indicating or implying that a device or element must have a specific orientation, be constructed and operated in a specific orientation, and should not be understood as a limitation on the present application.

[0041] Please also read Figures 1 to 4 As shown, a vibration electroplating device 1 provided in an embodiment of the present application includes a rotating shaft 11 , a vibration plate 12 and a plurality of cathode columns 13 .

[0042] The rotating shaft 11 is a columnar or long strip-shaped structural member extending along the second direction y, and the shape of the cross section (i.e., the xz cross section) is not limited to the circle shown in the figure, and can also be a polygon such as an ellipse or a trapezoid. The rotating shaft 11 includes two opposite ends along the second direction y, one end (i.e., the upper end shown in the figure) is used to connect to the vibration source, and the other end (i.e., the lower end shown in the figure) extends toward the vibration plate 12. In actual scenarios, flange rings 111 can be provided at both ends of the rotating shaft 11, respectively, and connected to the vibration source and the vibration plate 12 respectively through corresponding flange rings 111. The connection method based on the flange ring 111 can improve the stability and sealing of the connection, and also facilitate the subsequent replacement and maintenance of the connected structural members.

[0043] The second direction y can be regarded as the height direction of the rotating shaft 11 and the vibration electroplating device 1, the length direction of the rotating shaft 11 and the vibration electroplating device 1 is the first direction x, the width direction of the rotating shaft 11 and the vibration electroplating device 1 is the third direction z, and the first direction x, the second direction y and the third direction z are perpendicular to each other and can be regarded as two coordinate axes of the three-dimensional rectangular coordinate system. For the rotating shaft 11 and the vibration plate 12 with circular cross sections, the first direction x and the third direction z can be regarded as the radial direction of the two. It should be understood that the so-called verticality in the whole application does not require that the angle between the two must be 90°, but allows a deviation of ±10°, that is, the angle between the two perpendicular directions is 80° to 100°; similarly, the so-called parallelism does not require that the angle between the two must be 0° or 180°, but allows a deviation of ±10°, that is, the angle between the two parallel directions is 0° to 10° or 170° to 190°.

[0044] The vibration plate 12 includes a bottom plate 121 , a side wall 122 and a material dividing member 123 .

[0045] The side wall 122 is arranged on the bottom plate 121 to form a receiving cavity, and the vibration plate 12 can also be called a vibration basket. The lower end of the rotating shaft 11 extends from the opening at the upper end of the vibration plate 12 into the receiving cavity and is connected to the bottom plate 121, so that the bottom plate 121 can be driven to drive the vibration plate 12 to vibrate.

[0046] For the scenario where the cross-section of the vibration plate 12 is circular, the side wall 122 and the bottom plate 121 cooperate to form a structural member with an upper opening and a lower end through the bottom plate 121 as a bearing plate. The bottom plate 121 includes a low-position area 12a, a transition area 12b and a high-position area 12c arranged in sequence along the spiral direction of the vibration source (which can be regarded as the rotation direction of the rotating shaft 11 in the electroplating process), and along the second direction y, the heights of these three areas gradually increase, thereby forming a spiral surface spiraling upward in the vibration plate 12, which surrounds the rotating shaft 11 and gradually extends upward in a spiral. Optionally, the low-position area 12a, the transition area 12b and the high-position area 12c each occupy 1 / 3 of the bottom of the vibration plate (specifically, the positive projection of the bottom plate 121 along the second direction y). The material dividing piece 123 is arranged in the receiving cavity and is provided with an arc-shaped bridge surface 12d. Specifically, the material dividing piece 123 is located above the low-position area 12a, and the two ends of the arc-shaped bridge deck 12d are respectively connected to the high-position area 12c and the transition area 12b to form a channel 12e that passes through the bottom of the material dividing piece 123 and connects the high-position area 12c and the transition area 12b.

[0047] In one example, one end of the arc-shaped bridge deck 12d connecting the transition zone 12b is suspended relative to the transition zone 12b, and the suspended setting allows the arc-shaped bridge deck 12d to be vertically discharged downward, so that the product is not easily blocked here when the vibration plate 12 vibrates; and / or, one end of the high-position zone 12c connecting the channel 12e is suspended relative to the low-position zone 12a, and the suspended setting allows the product passing through the high-position zone 12c to be vertically discharged and enter the channel 12e, thereby avoiding the product being blocked here.

[0048] The bottom plate 121 and the side wall 122 are respectively provided with sieve holes 120. It should be understood that in other examples, the present application may only provide sieve holes 120 on the bottom plate 121, while the side wall 122 is not provided with sieve holes 120, or only provide sieve holes 120 on the side wall 122, while the bottom plate 121 is not provided with sieve holes 120. The sieve holes 120 are through holes that can allow the electroplating solution and the anode metal ions in the electroplating solution to pass through. For example, the sieve holes 120 may include: a water leakage hole opened on the bottom plate 121 and the side wall 122 to allow the electroplating solution to leak, and a filter screen covering the water leakage hole, which can at least allow the anode metal ions in the electroplating solution to pass through.

[0049] It should be understood that the mesh holes 120 provided on the bottom plate 121 can only allow the electroplating solution and the anode metal ions in the electroplating solution to pass through, and do not allow the product to leak out. The main function of the mesh holes 120 here is to increase the effective electroplating efficiency and enhance the conductivity. The mesh holes 120 provided on the side wall 122 can be adaptively set according to actual needs to allow the product to leak out, on the basis of satisfying the main function. When the product is allowed to leak out, the mesh holes 120 are only through holes and no filter covering the through holes is provided.

[0050] Multiple groups of cathode columns 13 are arranged in the receiving cavity, including an embodiment in which the cathode columns 13 are at least extended into the receiving cavity. Along the spiral direction, the height of each group of cathode columns 13 gradually increases, and the end of each group of cathode columns 13 extends to be exposed to the spiral surface, so that the products at the positions of each group of cathode columns 13 vibrated to the spiral surface can contact with the corresponding cathode columns 13 and be conductively connected.

[0051] In one implementation scenario, the cathode column 13 is connected to the base plate 121 of the vibration disk 12 by threaded locking. For example, a thread is provided at the lower end of the cathode column 13, and a threaded hole is provided at the base plate 121 of the vibration disk 12. The lower end of the cathode column 13 is inserted into the threaded hole and connected by threaded locking; further, the lower end of the cathode column 13 extends out of the base plate 121 to extend outside the vibration disk 12, and is powered.

[0052] exist Figures 1 to 4In the scene, the same group of cathode columns 13 are arranged along the radial direction of the vibration plate 12. The number of cathode columns 13 in each group can be determined according to the adaptability of the actual scene. The figure shows that each group contains 3 cathode columns 13, which is only an exemplary display. The more cathode columns 13 in each group, the stronger the conductivity and the better the electroplating effect. Observe along the line of sight perpendicular to the bottom plate 121, the angle between any two adjacent groups of cathode columns 13 is equal, and the uniform distribution of cathode columns 13 is conducive to better conductive connection of the product to the cathode.

[0053] In order to adapt to the inclined setting of the spiral surface, the heights of the cathode columns 13 in the same group can be different. For example, the cathode columns 13 closer to the rotating shaft 11 have smaller heights. Of course, the heights of the cathode columns 13 in the same group can also be the same. Figures 1 to 4 As shown, the maximum height of the first group of cathode columns 131 is lower than the minimum height of the second group of cathode columns 132, and the maximum height of the second group of cathode columns 132 is lower than the minimum height of the third group of cathode columns 133. Therefore, the first group of cathode columns 131 can also be called low-position cathode columns 131, the second group of cathode columns 132 can be called middle-position cathode columns 132, and the third group of cathode columns 133 can be called high-position cathode columns 133. The angle α between the spiral surface of each group of cathode columns 13 and the rotating shaft 11 can be adaptively designed. For example, the angle α corresponding to the low-position cathode column 131 is 92°, the angle α corresponding to the middle-position cathode column 132 is 90°, and the angle α corresponding to the high-position cathode column 133 is 88°. The uniform reduction of the angle α is conducive to the uniform thickness of the coating formed by the deposition of the anode metal ions, and the product is not easy to accumulate.

[0054] Optionally, the angle between the spiral surface and the rotating shaft 11 remains unchanged along the spiral direction, that is, the inclination angle of the spiral surface remains unchanged from bottom to top. Alternatively, the angle between the spiral surface and the rotating shaft 11 gradually decreases along the spiral direction, that is, the inclination angle of the spiral surface toward the rotating shaft 11 gradually decreases from bottom to top, so that the number of products carried on the spiral surface gradually decreases from bottom to top, and the width of the movable path of the product becomes smaller as it goes up, which is conducive to delaying the movement of the product, and the product is not easy to accumulate to produce phenomena such as sticking, black end and unplated, rough end, etc. The anode metal ions can be better deposited on the surface of the product to form a more uniform coating thickness.

[0055] The present application does not limit the structure, material, and relative positional relationship between the anode and any of the above-mentioned structural elements of the vibration electroplating device 1. For example, the anode and the cathode column 13 can be connected to the same power source as the vibration source. During the electroplating process, the anode extends into the plating solution in the receiving cavity of the vibration plate 12, and forms a closed loop circuit with the cathode column 13 through the plating solution.

[0056] The working principle and process of the vibration electroplating device 1 are exemplified as follows:

[0057] First, place the product to be electroplated into the receiving cavity of the vibration plate 12, and immerse the vibration plate 12 loaded with the product into a device containing a plating solution. The product includes but is not limited to coupling components such as MLCC. In the scenario where the product to be electroplated is a smaller coupling component such as MLCC, optionally, a plating medium, such as conductive particles such as steel balls, can be placed in the receiving cavity of the cathode column 13. The plating medium is mixed with the product to ensure a good electrical connection between the product and the cathode column 13. The plating medium is used to increase the conductivity and stirring of the product. Because MLCC products are particularly small (millimeter level), it is difficult for each product to contact the cathode column 13. Therefore, after the plating medium is added, the plating medium contacts the cathode column 13 to form a large cathode. As long as the product contacts the plating medium, it can be electroplated and the current can be dispersed to many products, thereby improving the efficiency and quality of the plating. It should be understood that the electroplating medium can also include zirconium balls (i.e. spherical particles made of ZrO2), aluminum balls (i.e. spherical particles made of Al2O3), etc. The particle size is generally 5-10cm, which is relatively large compared to MLCC products, steel balls and other conductive particles. The main purpose is to stir and break up the sticky products. Even if the product size is small, it is not easy to stick to the film.

[0058] Then, start the vibration source, which drives the rotating shaft 11 to vibrate, so as to drive the vibration plate 12 to vibrate; the spiral surface formed by the material dividing piece 123 can make the product and the plating solution move along the spiral surface when the vibration plate 12 vibrates, that is, rotate relative to the rotating shaft 11, so as to increase the flow rate of the plating solution; in addition, the sieve hole 120 increases the flow channel of the plating solution inside and outside the vibration plate 12, so as to increase the flow rate of the plating solution, and also reduce the resistance encountered by the product during the movement, so that the product is not easy to accumulate. Therefore, the present application can increase the deposition rate and deposition amount of the anode metal ions on the surface of the product, the thickness of the formed coating is more uniform, and the risk of oxidation during the deposition process is reduced, which is conducive to improving the quality of the coating and the product after electroplating. For example, according to the research and experimental results, the coating quality is improved, so that the weldability is improved, and the welding yield can be increased from 90% of the prior art to 99.9% and above. In addition, since the flow rate of the plating solution is increased, the number of products that can be plated in a single time by the vibration plating device 1 of the present application can be increased from 3,500,000 in the prior art to 4,500,000.

[0059] For the sake of distinction, the present application may refer to the sieve hole 120 provided on the side wall 122 as the first sieve hole 120, and the sieve hole 120 provided on the bottom plate 121 as the second sieve hole 120. Optionally, the diameter of the first sieve hole 120 is greater than the diameter of the second sieve hole 120. During the vibration plating process, the flow of the plating solution in the direction passing through the first sieve hole 120 is large, while the flow in the direction passing through the second sieve hole 120 (i.e., the second direction y) is small. Therefore, by setting the diameter of the first sieve hole 120 to be larger, the internal and external exchange requirements of the plating solution when the product rotates along the spiral surface can be met.

[0060] The shapes of the sieve holes 120 on the side wall 122 and the bottom plate 121 and the arrangement of the sieve holes 120 are not limited in this application. For example, the first sieve holes 120 can be arranged in a spiral shape on the side wall 122 along the spiral direction, so that the first sieve holes 120 are located in the direction of the centrifugal force generated by the rotation of the electroplating liquid along the spiral direction, and the resistance to the exchange of the electroplating liquid inside and outside is small, which is conducive to the exchange of the electroplating liquid inside and outside the vibration plate 12. For another example, Figures 1 to 5 In the scenario, the first sieve holes 120 are evenly arranged in an array on the side wall 122, that is, forming columns along the second direction y and forming rows along the radial direction.

[0061] In the working principle and process of the aforementioned vibration electroplating device 1, the product in the outer ring area (the area near the side wall 122, also called the "outer ring area of ​​the vibration plate") runs through the arc bridge surface 12d of the material dividing member 123 to the transition area 12b, thereby entering the inner ring area (the area near the rotating shaft 11, also called the "inner ring area of ​​the vibration plate"), combined with Figure 1 and Figure 5 As shown by the thick arrow, the product in the inner circle area passes through the high-level area 12c to reach the entrance of the channel 12e. The entrance is suspended so that the product can be fed vertically downward without blocking, and then enters the low-level area 12a and the channel 12e, and then reaches the transition area 12b through the channel 12e and the outlet of the channel 12e, and then enters the outer circle area again, and the cycle is executed in sequence. Every time the product runs a cycle in the vibration plate 12, the products in the outer circle area and the inner circle area are exchanged once. Here, through the channel 12e, the products in the outer circle area and the inner circle area are evenly exchanged, the coating of the product plated by vibration is uniform and the coating of the product end is complete, which can further improve the quality of the coating and the electroplated product. In the electroplating process, the purpose of the curved bridge deck 12d is to improve the exchangeability of products and electroplating media. The curved bridge deck 12d transports the products in the outer circle area of ​​the vibration plate 12 to the inner circle area of ​​the vibration plate 12 through the curved bridge deck 12d. At the same time, the lower channel of the curved bridge deck 12d transports the products in the inner circle area of ​​the vibration plate 12 to the outer circle area of ​​the vibration plate 12 through the lower channel of the curved bridge deck, thereby implementing the internal and external exchange of product positions, making the overall electroplating film thickness, crystallization, etc. of the product more uniform.

[0062] In one example, when observing along the line of sight from top to bottom, on the same radius of the vibrating disk 12 (i.e., the radius where the entrance of the channel 12e is located), the width of the entrance of the channel 12e is smaller than the width of the outer ring area (i.e., the length between the side wall 122 and the entrance of the channel 12e). In other words, on the radius of the vibrating disk where the entrance of the channel 12e (the straight line formed by the orthographic projection) is located, the width of the entrance of the channel 12e is d1, and the length from the side wall 122 to the channel 12e (the straight line formed by the orthographic projection) is d2, and d1 < d2, which is equivalent to the outer ring diameter being larger than the inner ring diameter. Since the rotational speed of the outer ring is faster than that of the inner ring, the smaller inner ring diameter can reduce the occurrence of material blockage in the inner ring area and improve the exchangeability of the products and the electroplating medium in the vibrating disk 12, thereby ensuring that the exchangeability of the products in the inner and outer ring areas is within the expected range. In this regard, in an actual scenario, the width d2 of the outer ring area can be 60 mm, and the width d1 of the entrance of the channel 12e can be 38 mm.

[0063] Please continue to refer to Figure 1 , the material distribution member 123 can be provided with an inner baffle 124 and an outer baffle 125 that are oppositely arranged (for example, parallel). The inner baffle 124 is located on the side of the arc-shaped bridge surface 12d close to the rotating shaft 11. The outer baffle 125 is located on the side of the arc-shaped bridge surface 12d close to the side wall 122. One end of the inner baffle 124 facing the transition area 12b is oppositely arranged (i.e., not in contact) with the rotating shaft 11 to form a notch.

[0064] Adaptively, the vibration electroplating device 1 can further include a first stopper 126, and the first stopper 126 blocks the notch. By providing the first stopper 126 to block the notch between the inner baffle 124 of the material distribution member 123 and the rotating shaft 11, it is possible to avoid the formation of dead corners between the inner baffle 124 of the material distribution member 123 and the rotating shaft 11, thereby preventing products from staying in this dead corner and affecting the electroplating quality. In addition, one end of the inner baffle 124 facing the transition area 12b is oppositely arranged with the rotating shaft 11 to form a notch. For the injection-molded material distribution member 123, when installing the material distribution member 123, for example, it is not necessary to accurately position the material distribution member 123, which makes the installation of the material distribution member 123 convenient; in addition, if the inner baffle 124 is directly bent and connected (for example, welded) to the rotating shaft 11, not only is it easy to have problems with insecure welding, and it is prone to cracking under the influence of vibration after welding, but also the welding cannot be made flat, and it is difficult to achieve the accuracy required for use.

[0065] In one example, along the direction perpendicular to the bottom plate 121 (i.e., along the second direction y), the side of the first stopper 126 facing away from the rotating shaft 11 has the same curvature as the inner baffle 124, that is, the side and the inner baffle 124 form a smoothly transitioning arc surface, which is conducive to the products being transported in a spiral direction.

[0066] In another example, if Figure 5 As shown, the end of the inner baffle 124 facing the transition zone 12b is connected to the rotating shaft 11, that is, the gap is not formed between the inner baffle 124 and the rotating shaft 11. At this time, the vibration electroplating device 1 does not need to be provided with the first stopper 126, and can also avoid the dead angle between the inner baffle 124 of the material dividing member 123 and the rotating shaft 11, thereby preventing the product from being trapped in the dead angle and affecting the electroplating quality. In order to ensure a firm connection between the inner baffle 124 and the rotating shaft 11, a relatively firm welding process can be used, or the Figure 5 The structure shown is suitable for electroplating scenarios with less vibration.

[0067] Please continue reading Figure 1 , the outer baffle 125 and the side wall 122 form a natural arc transition, and the products in the outer ring area have better fluidity here and are not easy to pile up. The vibration electroplating device 1 can also include a second block 127, which is arranged at the connection between the outer baffle 125 and the side wall 122, but does not block the channel 12e. For example, the second block 127 also extends to the bottom of the arc bridge deck 12d (as shown by the dotted line) to limit the left side of the channel 12e to a straight retaining wall. The second block 127 can avoid a dead angle between the outer baffle 125 and the side wall 122 of the material dividing member 123, thereby preventing the product from being trapped in the dead angle and affecting the electroplating quality.

[0068] In one example, the second stopper 127 is flush with the top of the outer baffle 125. Alternatively, the top surface of the second stopper 127 is an inclined surface, the height of which gradually decreases along the side wall 122 toward the rotation axis 11, that is, the inclined surface is an inwardly inclined surface, and even if the product is thrown onto the inclined surface by centrifugal force during the vibration plating process, it will slide onto the arc-shaped bridge surface 12d due to gravity.

[0069] A support block 128 (i.e. Figure 1 The support block is arranged below the material dividing member 123 and close to the inner circle area, for example, close to the first stopper 126. In one example, the support block 128 can be an extension of the first stopper 126, which is equivalent to extending the blocking position of the first stopper 126.

[0070] The support block 128 supports and ensures the strength of the material dividing member 123 without affecting the uniform exchange of the product between the outer ring area and the inner ring area. Figure 1As shown, the first stopper 126 and the support block 128 form a straight retaining wall toward the outer ring area. The products running in the channel 12e are forced to run toward the outer ring area due to the obstruction of the straight retaining wall. Here, the support block 128 has a guiding function, which can transfer all products toward the outer ring area without allowing some products to move around the rotating shaft 11. In one example, the support block 128 can divide the proportion of the inner ring area and the outer ring area equally, so that the number of products performing the inner and outer ring exchange is more balanced, which is conducive to improving the electroplating quality.

[0071] It should be understood that the specific position, shape and other parameters of the support block 128 can be determined according to the adaptability of the requirements. For example, the side of the support block 128 adjacent to the channel 12e (which can be called "the outer side of the support block") can be an arc with the same curvature as the outer baffle 125; for another example, the end of the support block 128 facing the transition zone 12b and the end of the arc bridge deck 12d connecting the transition zone 12b are flush with each other, so as to ensure that the material dividing piece 123 is suspended at the end facing the transition zone 12b to achieve vertical material feeding to avoid material blockage.

[0072] In the vibration plating device 1 provided in the embodiment of the present application, the size of each structural component can be determined according to the adaptability required in the actual scene, and the present application does not limit it.

[0073] For example, the height (i.e., the length along the second direction y) of the rotating shaft 11 (including the flange ring 111 set on the top) is 450 mm; the diameter of the flange ring 111 is 125 mm and the thickness is 8 mm; the diameter of the rotating shaft 11 is 90 mm, and the diameter of the vibration plate 12 can be between 290 mm and 300 mm; the area of ​​the spiral surface where the low-position cathode column 131 is located is the starting position of the spiral surface, and when observed along the line of sight in the second direction y, the area of ​​the spiral surface where the low-position cathode column 131 is located can also be the end position of the spiral surface. In the same group of cathode columns 13, the distance between the centers of any two adjacent cathode columns 13 is 30 mm.

[0074] For another example, in a scenario where one end of the arc-shaped bridge deck 12d connecting the transition zone 12b is suspended relative to the transition zone 12b (i.e., the outlet of the material dividing piece 123 is suspended), its suspension height (relative to the height at the lowest point of the bottom plate 121) should ensure smooth product flow in the channel below the arc-shaped bridge deck 12d (i.e., the cathode head adhesion and film adhesion rates are within the expected range) while avoiding excessive suspension height that may cause product falling and damage. The suspension height is H1.

[0075] Input amount (product + electroplating medium <![CDATA[Suspended height H1 (cm)]]> Product Operation Porcelain loss Cathode head adhesive Sorting sticking rate 1000cc 1.5 Slow operation 400ppm 5 / 9 0.10% 1000cc 2.0 Slightly slower operation 150ppm 2 / 9 0.10% 1000cc 2.5 Smooth operation 110ppm 1 / 9 0.10% 1000cc 2.8 Smooth operation 100ppm 1 / 9 0.10% 1000cc 3.0 Smooth operation 100ppm 1 / 9 0.10% 1000cc 3.5 Smooth operation 160ppm 1 / 9 0.10% 1000cc 4.0 Smooth operation 320ppm 1 / 9 0.10%

[0076] Example 1

[0077] In Example 1, the suspension height at the entrance of Channel 12e is H2. To ensure that the product will not be damaged due to excessive dropping height and to have a certain height conducive to product dispersion to prevent poor chip sticking, in this Example 1, the value of H2 is selected as 0.5 cm; and the values of the suspension height H1 are 1.5 cm, 2.0 cm, 2.5 cm, 2.8 cm, 3 cm, 3.5 cm, and 4.0 cm respectively. The input amounts of MLCC products and electroplating medium are 1000 cc. According to the verification results shown in the above table, when the suspension height H1 is 2.0 cm and below (taking 1.5 cm as an example), the products in the channel under the arc-shaped bridge deck 12d are piled up and squeezed, resulting in slow product operation, increased porcelain damage, and more serious sticking of the cathode head; when the suspension height H1 is 3.5 cm and above (taking 4.0 cm as an example), the product operation is smooth, but the porcelain damage increases, and as the suspension height increases, the porcelain damage becomes serious; when the suspension height H1 satisfies 2 cm < H1 ≤ 3.5 cm, the product operation is smooth, and the porcelain damage and cathode head sticking are less than those at other values of the suspension height H1. Considering comprehensively, it is more reasonable that the suspension height H1 satisfies 2 cm < H1 ≤ 3.5 cm, and the preferred suspension height H1 is 2.8 cm.

[0078] <![CDATA[Drop height H2 (cm)]]> Product Operation Porcelain loss Cathode head adhesive Sorting sticking rate 0.0 Smooth operation 95ppm 1 / 9 0.20% 0.2 Smooth operation 95ppm 1 / 9 0.12% 0.5 Smooth operation 95ppm 1 / 9 0.10% 1.0 Smooth operation 100ppm 1 / 9 0.10% 1.2 Smooth operation 180ppm 1 / 9 0.10%

[0079] Example 2

[0080] In Example 2, the input amounts of MLCC products and electroplating medium are 1000 cc. The suspension height H1 is taken as 2.8 cm and verified under the conditions of this example. The values of the suspension height H2 are 0.0 cm, 0.2 cm, 0.5 cm, 1.0 cm, and 1.2 cm respectively. According to the verification results shown in the above table, when the suspension height H2 is 0.0 cm and 0.2 cm, the product operation is smooth, but the chip sticking rate has an increasing trend and the product dispersion effect is poor. When the suspension height H2 is 0.5 cm and 1.0 cm, the product operation is smooth, and at the same time, the porcelain damage, cathode head sticking, and chip sticking rate are relatively good. When the suspension height H2 is 1.2 cm, the product operation is smooth, but the porcelain damage has an increasing trend. Considering comprehensively, the suspension height H2 satisfies 0 < H2 ≤ 1 cm, and the preferred value is equal to 0.5 cm, so as to ensure that the product will not be damaged due to excessive dropping height and to have a certain height conducive to product dispersion to prevent poor chip sticking. In addition, the width of the material separating part 123 (including the width of the outlet) is 55.5 mm; the heights of the inner baffle 124 and the outer baffle 125 are both 30 mm.

[0081] The embodiment of the present application also provides a vibration electroplating system, including a vibration source, an anode, and a vibration electroplating device 1 of any of the above embodiments, so as to have the beneficial effects that can be produced by the corresponding embodiment. The vibration source is connected to the rotating shaft 11, and during the electroplating process, the anode can extend into the plating solution in the receiving cavity of the vibration plate 12, and form a closed loop circuit with the cathode column 13 through the plating solution.

[0082] It should be understood that the vibration plating system provided in the embodiment of the present application is a complete vibration plating system, and also has the structure of a known vibration plating system. Here, only the components involving the rotating shaft 11, the vibration plate 12 and the multiple groups of cathode columns 13 in the vibration plating system are described, and other components are not described in detail.

[0083] The above descriptions are only some embodiments of the present application, and are not intended to limit the patent scope of the present application. For ordinary technicians in this field, all equivalent structural changes made using the contents of this specification and drawings are also included in the patent protection scope of the present application.

[0084] Although the terms "first, second", etc. are used herein to describe various information, such information should not be limited to these terms. These terms are only used to distinguish information of the same type from each other. In addition, the singular forms "one", "an", and "the" are intended to include plural forms as well. The terms "or" and "and / or" are interpreted as inclusive, or mean any one or any combination. Only when the combination of elements, functions, steps, or operations is inherently mutually exclusive in some way, an exception to this definition will occur.

Claims

1. A vibration electroplating device, characterized in that: include: A rotating shaft, one end of which is used to connect to a vibration source; A vibration plate, comprising a bottom plate, side walls and a dividing piece provided with a curved bridge deck; The side wall is arranged on the bottom plate to form a receiving cavity, and the other end of the rotating shaft extends into the receiving cavity and is connected to the bottom plate; the bottom plate and / or the side wall are provided with sieve holes; the bottom plate includes a low-position area, a transition area and a high-position area arranged in sequence along the spiral direction of the vibration source; the material dividing piece is arranged in the receiving cavity and is located above the low-position area, and the two ends of the arc-shaped bridge deck are respectively connected to the high-position area and the transition area to form a channel passing through the bottom of the material dividing piece and connecting the high-position area and the transition area; A plurality of cathode columns extend into the receiving cavity and are exposed to the bottom plate.

2. The vibration plating device according to claim 1, characterized in that: Satisfy at least one of the following: The diameter of the sieve hole provided on the side wall is larger than the diameter of the sieve hole provided on the bottom plate; The sieve holes provided on the side wall are arranged on the side wall in a spiral shape along the spiral direction; The sieve holes arranged on the side wall are evenly arranged in an array on the side wall.

3. The vibration plating device according to claim 1, characterized in that: The material dividing member is provided with an inner baffle plate, which is located on a side of the arc-shaped bridge deck close to the rotating shaft, and is arranged opposite to the rotating shaft at one end facing the transition zone to form a notch; The vibration electroplating device also includes a first stopper, which blocks the gap.

4. The vibration plating device according to claim 3, characterized in that: Along a direction perpendicular to the bottom plate, a side of the first stopper facing away from the rotation axis has the same curvature as that of the inner stopper.

5. The vibration plating device according to claim 1, characterized in that: On the radius of the vibration plate where the entrance of the channel is located, the width of the entrance of the channel is d1, the length from the side wall to the channel is d2, and d1 <d2。 6. The vibration plating device according to any one of claims 3 to 5, characterized in that: The material dividing member is provided with an outer baffle plate, which is located on a side of the arc-shaped bridge deck close to the side wall; The vibration electroplating device also includes a second stopper, which is arranged at the connection between the outer baffle plate and the side wall but does not block the channel.

7. The vibration plating device according to claim 6, characterized in that: The second stopper is flush with the top of the outer baffle, or the top surface of the second stopper is an inclined surface, and the height of the inclined surface gradually decreases along the side wall toward the rotation axis.

8. The vibration plating device according to claim 1, characterized in that: One end of the arc-shaped bridge deck connected to the transition zone is suspended relative to the transition zone; and / or one end of the high-level zone connected to the channel is suspended relative to the low-level zone.

9. The vibration plating device according to claim 8, characterized in that: The end of the arc-shaped bridge deck connected to the transition zone has a suspended height H1 relative to the transition zone, and 2 cm <H1≤3.5cm; And / or, the end of the high position area connected to the channel has a suspension height H2 relative to the low position area, and 0 <H2≤1cm。 10. A vibration electroplating system, characterized in that: It comprises a vibration source, an anode and the vibration electroplating device according to any one of claims 1 to 9, wherein the vibration source is connected to the rotating shaft, and the anode can extend to the plating liquid in the receiving chamber and form a closed loop circuit with the cathode column through the plating liquid.

Citation Information

Cited By

  • Alloy powder electric vibration plating device and method

    CN121321177A