Testing device for mechanical response of prestressed resin anchor cable in erosion environment
By designing a test device including concrete mound seat, anchor cable, PVC pipe and annular stainless steel mesh, the problem of difficult testing of prestressed resin anchor cables in the erosion environment and the changes in the concrete compressive stress of concrete are achieved, and the anchoring is achieved Effective evaluation of cable mechanics properties and concrete compressive stress improves the safety of tunnel engineering.
Patent Information
- Application Number
- CN202411224505.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-03
- Publication Date
- 2024-11-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In an erosion environment, the anchoring force of the prestressed resin anchor cable is easily affected by corrosion, resulting in anchoring force loss. It is difficult for the prior art to effectively test its mechanical response and changes in the compressive stress of concrete, which affects the safety of tunnel engineering.
A test device including concrete mound seats, anchor cables, PVC pipes and annular stainless steel mesh was designed to simulate corrosive solutions, electrochemical corrosion and dry-wet-dry alternating environments to test the mechanics of prestressed resin anchor cables under different erosion conditions. Response and concrete compressive stress diffusion.
The device can effectively test the mechanical properties of prestressed resin anchor cables and the compressive stress of concrete under different erosion environments, provide testing capabilities for anchor cable spacing and prestress changes, and improve the safety and engineering reliability of tunnel projects .
Smart Images

Figure CN118913909A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of anchor cable mechanics testing, and in particular to a test device for mechanical response of a prestressed resin anchor cable in a corrosive environment. Background Art
[0002] With the construction and development of the tunnel industry, it is now difficult to effectively control the large deformations in some soft rock tunnels using the traditional forced protection mode by increasing the strength and thickness of the lining. Therefore, experts have proposed an active support technology based on prestressed anchor cables, and implemented it in actual projects, achieving significant deformation control effects.
[0003] In soft rock large deformation tunnels with complex geological conditions, the anchoring force that prestressed resin anchor cables can exert is easily affected by environmental factors, especially in corrosive solutions and some corrosive gases. Prestressed resin anchor cables will be corroded and their anchoring force may be partially lost, and even electrochemical corrosion or dry-wet alternating corrosion may occur in the environment, which is likely to have a great impact on the prestressed resin anchor cables.
[0004] As a permanent support structure in tunnel engineering, it is necessary to clarify the force changes of prestressed resin anchor cables in actual engineering. In order to ensure the safety of the project and clarify the force changes of prestressed resin anchor cables in erosive environments, it is urgent to propose a test device suitable for testing the mechanical response of prestressed resin anchor cables in erosive environments. Summary of the invention
[0005] The technical problem to be solved by the present invention is to overcome the deficiencies in the prior art, and the purpose is to provide a test device for the mechanical response of prestressed resin anchor cables under corrosive environments, which can complete the mechanical response test of prestressed resin anchor cables under different corrosive environments such as corrosive solutions, corrosive gases, electrochemical corrosion, and dry-wet alternation, and can test the changes in the prestress of resin anchor cables and the changes in the compressive stress of concrete under various corrosive environments. It can also test the characteristics of the group anchor effect under different anchor cable spacings and the size of the compressive stress diffusion zone of the anchored concrete under the group anchor effect.
[0006] The present invention is achieved through the following technical solutions:
[0007] A test device for the mechanical response of a prestressed resin anchor cable under a corrosive environment comprises a concrete pier, a power supply and a plurality of anchor cables, wherein a groove is provided on the top of the concrete pier, a rear end reserved anchor hole is provided on the inner wall of the groove, a resin anchor is provided in the rear end reserved anchor hole, a PVC pipe is also provided in the groove, the anchor cable passes through the PVC pipe from the side of the concrete pier and is inserted into the rear end reserved anchor hole and is bonded and anchored with the resin anchor; an annular stainless steel mesh is also provided in the PVC pipe, and the annular stainless steel mesh is sleeved on the anchor cable, the annular stainless steel mesh is connected to the negative electrode of the power supply through a wire, and the positive electrode of the power supply is connected to the anchor cable exposed in the groove through a wire, so as to form a corrosion primary cell.
[0008] An earth pressure box is also embedded in the concrete pier;
[0009] Two pads and an anchor are sleeved on the anchor cable in a direction away from the concrete pier seat, and an anchor cable dynamometer is arranged between the two pads.
[0010] Further, the PVC pipe includes a transverse pipe, a short pipe, a T-shaped three-way pipe and a longitudinal pipe, the short pipe is connected to the side wall of the longitudinal pipe, and the T-shaped three-way pipe connects the longitudinal pipe with the transverse pipe through the short pipe;
[0011] The transverse pipe and the T-shaped three-way pipe are both sleeved on the anchor cable.
[0012] Further, one end of the transverse tube is sealed with epoxy resin AB glue and is in contact with the rear end reserved anchor hole in the groove;
[0013] The other end of the transverse tube is installed with an annular PVC pipe cover and sealed with epoxy resin AB glue, and there is a gap of 0.01m between the transverse tube and the inner wall of the groove.
[0014] Furthermore, the longitudinal tube is made of transparent material, and the upper and lower ends of the longitudinal tube are sealed with PVC tube covers, and the PCV tube cover at the upper end of the longitudinal tube is provided with a reserved hole for the wire to pass through.
[0015] Furthermore, each of the longitudinal tubes is connected to three transverse tubes, and the transverse tubes are arranged in sequence from top to bottom, and different erosion environments are respectively arranged in each transverse tube;
[0016] The corrosive environment includes corrosive solution immersion corrosion, corrosive solution electrochemical corrosion, corrosive gas corrosion and dry-wet alternation.
[0017] Furthermore, the side surface of the concrete pier is provided with front end reserved anchor holes, the number of which is the same as the number of anchor cables, and the anchor cables are inserted into the rear end reserved anchor holes of the concrete pier through the front end reserved anchor holes;
[0018] The earth pressure box is fixedly buried around the front reserved anchor hole when the concrete pier is poured;
[0019] The earth pressure box is evenly pre-buried at the four corners of the pad where the compressive stress of the pad acts, and the earth pressure box is located in the middle of the compressive stress action area of the concrete pier pad in the longitudinal direction. It is used to test the diffusion of compressive stress on the concrete pier during the prestressing tensioning stage of the anchor cable and the prestressing loss stage.
[0020] Furthermore, the power supply can be used only as a current and voltage measuring meter to test the voltage and current that may be generated by the anchor cable being immersed in corrosion environments of different corrosive solutions, and to reflect and compare the degree of corrosion;
[0021] The power source can also apply a specific voltage or current to generate electrochemical corrosion, and test the change of prestress of the anchor cable under the erosion environment of electrochemical corrosion.
[0022] Compared with the prior art, the present invention has the following advantages and beneficial effects:
[0023] 1. The present invention can change the spacing and number of the reserved anchor holes of the concrete pier as well as the anchoring length and free end length of the resin anchor cable according to the needs, tension different prestressed anchor cables, and complete the mechanical response test of the prestressed resin anchor cable under the erosion environment under different conditions;
[0024] 2. The present invention can also compare and test the characteristics of the group anchor effect under different anchor cable spacing. The PVC pipe can effectively contain corrosive solutions and gases and reduce the amount used, ensuring that the corrosive environment only acts on the anchor cable. The longitudinal PVC pipe uses transparent materials, which can be used to observe the corrosive solution and the internal situation of the reaction solution. The upper and lower ends of the pipe are sealed with PVC pipe covers, and the PVC pipe covers at both ends can be opened, which is convenient for changing different corrosive environments.
[0025] 3. The present invention can test the difference in mechanical properties of prestressed resin anchor cables under different erosion environments. The anchor cable dynamometer can test the change in stress of each resin anchor cable during the tensioning process. The earth pressure cell can be used to test the diffusion of compressive stress on concrete during the prestressing tensioning stage and the prestressing loss stage of the resin anchor cable, and can reflect the change in compressive stress on concrete under the action of the erosion environment.
[0026] 4. The power supply of the present invention which can adjust and measure current or voltage can be used only for measurement, to test the voltage and current that may be generated by immersion corrosion of the resin anchor cable in a corrosive solution erosion environment, to reflect its corrosion degree, and can subsequently apply a specific voltage / current to generate electrochemical corrosion, to test the prestress change and prestress loss of the resin anchor cable. The annular stainless steel mesh uses materials of uniform specifications, which can control variables, and compare the voltage and current generated by electrochemical corrosion of the resin anchor cable in different corrosive solution erosion environments to reflect its corrosion degree. The hollow section of the resin anchor cable loses electrons as the anode of the corrosion galvanic cell, and its surface corrosion can be observed, which intuitively reflects its corrosion degree. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] The drawings described herein are used to provide a further understanding of the embodiments of the present invention, constitute a part of this application, and do not constitute a limitation of the embodiments of the present invention. In the drawings:
[0028] Figure 1 This is a schematic diagram of the internal structure of the concrete pier of the present invention;
[0029] Figure 2 It is a schematic diagram of the structure of the present invention;
[0030] Figure 3 For the present invention Figure 2 Schematic diagram of the AA section structure;
[0031] Figure 4 For the present invention Figure 2 Schematic diagram of the structure of the middle BB section;
[0032] Figure 5 This is a schematic diagram of the structure of the PVC pipe of the present invention;
[0033] Figure 6 It is a schematic diagram of the local structure of the anchor cable of the present invention;
[0034] Figure 7 This is a partial structural schematic diagram of the annular stainless steel mesh of the present invention;
[0035] Figure 8 It is a schematic diagram of the structure of the two ends of the longitudinal tube of the present invention;
[0036] Fig. 9 For the present invention Figure 8 Schematic diagram of the structure after enlarging part C in the middle.
[0037] Marks and corresponding parts names in the attached drawings:
[0038] 1. Concrete pier; 2. Anchor cable; 3. Resin anchor; 4. PVC pipe; 5. Power supply; 6. Annular stainless steel mesh; 7. Earth pressure box; 8. Pad; 9. Anchor cable dynamometer; 10. Anchor; 11. Horizontal pipe; 12. Longitudinal pipe; 13. Short pipe; 14. T-type three-way pipe; 15. Upper cover; 16. First airbag component; 17. Limit block; 18. Lower cover; 19. Movable rod; 20. Second airbag component; 21. Connecting pipe; 22. Hose; 23. First fixed plate; 24. First elastic component; 25. Unlocking rod; 26. Block. DETAILED DESCRIPTION
[0039] In order to make the objectives, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with embodiments and drawings. The exemplary embodiments of the present invention and their description are only used to explain the present invention and are not intended to limit the present invention.
[0040] Example 1
[0041] like Figures 1 to 7 As shown, the present invention includes a concrete pier 1, an anchor cable 2, a resin anchor 3, a PVC pipe 4, an adjustable power supply 5 for measuring A / U, an annular stainless steel mesh 6, an earth pressure box 7, a pad 8, an anchor cable dynamometer 9, and an anchor 10, wherein the PVC pipe 4 specifically includes a transverse pipe 11, a longitudinal pipe 12, a short pipe 13, and a T-shaped three-way pipe 14.
[0042] The concrete pier 1 is a large volume of concrete with a hollowed-out groove and reserved anchor holes in the middle. The size is designed to be 1.05m*0.8m*0.8m, the bottom thickness of the hollowed-out section is 0.1m, the anchoring section at the rear end of the pier is 0.45m long and a 0.4m long anchor hole section is reserved. The hollowed-out part in the middle of the pier is the free section of the anchor cable and the section with erosion environment action is 0.5m long. The section with compressive stress action of the front pad of the pier is 0.1m long and a through anchor hole is reserved. The reserved anchor hole has a diameter of 28mm and is cast with C30 concrete. The spacing and number of the reserved anchor holes of the concrete pier 1 and the anchor length of the anchor cable 2 can be changed according to demand, and the number and position of the anchor cable dynamometer 9 and the soil pressure box 7 can be changed accordingly. Different prestressed anchor cables 2 are tensioned to complete the mechanical response test of prestressed resin anchor cables under erosion environment under different conditions, and the group anchor effect characteristics under different anchor cable spacing can be compared and tested.
[0043] When pouring the concrete pier 1, a total of 16 earth pressure boxes 7 are evenly buried. The model used is YT-ZX0320, with a range of 2Mpa, a resolution of 0.001Mpa, a diameter of 120mm, a thickness of 2.5mm, corrosion resistance, and an applicable temperature of -20℃-80℃. Its lateral position is evenly buried at the four corners where the pad compressive stress acts, and its longitudinal position is in the middle of the compressive stress action area of the pad at the front end of the concrete pier 1. It can be used to test the diffusion of compressive stress on concrete during the prestressing tensioning stage of the anchor cable 2 and the prestressing loss stage. It can reflect the changes in the compressive stress of concrete under the action of the corrosive environment, and can realize the test of the size of the compressive stress diffusion area of the anchored concrete under the group anchor effect. At the same time, it can test the characteristics of the distribution of the compressed area of the anchored concrete under different tensioning sequences of the anchor cable 2.
[0044] The anchor cable 2 is inserted into the anchor hole reserved at the front end of the concrete pier seat 1, passes through the preset transverse tube 11 in the middle of the pier seat, and then enters the anchor hole reserved at the rear end of the pier seat. It is bonded and anchored after being mixed and cured with the resin anchor agent roll placed in advance through an external turner. The designed number is 9, the designed diameter is 21.8 mm, and they are evenly arranged on the concrete pier seat 1. The central anchor cable 2 is arranged in the center of the concrete pier seat 1. The layout spacing of the anchor cable 2 is 0.2m, the designed length of the anchoring section is 0.4m, the designed length of the free section is 0.6m, and the total designed length is 1.45m. It can realize the tensioning of multiple prestressed anchor cables 2 at one time, which is used for comparative testing of results under different working conditions, including but not limited to different tensioning forces, tensioning speeds, solution erosion environments and rates, etc.
[0045] The resin anchor 3 uses model MSZ2340, which is a medium-speed resin anchor with a diameter of 23mm and a length of 40cm. After the concrete pier 1 is poured, the resin anchor 3 is placed using an anchor roll, and is filled into the reserved anchor hole at the rear end of the concrete pier through the stirring and curing of the anchor cable 2. After the anchor cable 2 and the placed resin anchor 3 are stirred and cured by an external converter, the bonding and anchoring of the rear end of the anchor cable and the concrete pier can be achieved, which is convenient for the subsequent tensioning of the anchor cable prestress.
[0046] The PVC pipe 4 includes 9 transverse pipes 11, 3 longitudinal pipes 12, 9 short pipes 13 and 18 T-shaped three-way pipes 14. Except for the T-shaped three-way pipe 14, a PVC wire threading pipe of model De40 is used, with an outer diameter of 40 mm and a thickness of 2 mm. The transverse pipe 11 is designed to be 0.49 m long, which is slightly shorter than the middle hollow section of the concrete pier 1. The rear end of the transverse pipe 11 is in contact with the concrete pier 1, and there is a 0.01 m hollow part of the anchor cable at the front end, which can be connected with a wire as a corrosion primary battery anode. After the wire connection is completed, the rear end of the transverse pipe 11 is sealed with epoxy resin AB glue, and the front end is equipped with an annular PVC pipe cover, and then sealed with epoxy resin AB glue, which can ensure that corrosive solutions and gases will not leak in the pipe and will not be affected by the external environment. It can effectively accommodate corrosive solutions and gases and reduce the amount used, ensuring that the corrosive environment only acts on the anchor cable 2 without affecting the concrete.
[0047] The longitudinal tube 12 is designed to have a length of 0.8m. After the anchor cable is prestressed, the annular stainless steel mesh 6 connecting wire is placed in the reserved opening of the transverse tube 11. The longitudinal tube 12 is connected to the transverse tube 11 using a short tube 13 and a T-shaped three-way tube 14. The upper opening is used for power supply wires and solution circulation. The longitudinal tube 12 uses transparent materials and can be used to observe the height of the corrosive solution, the degree of solution turbidity, whether the liquid level is stable, the internal conditions of the reaction solution, whether the anchor cable 2 is completely immersed, and whether leakage occurs. The upper and lower ends of the longitudinal tube 12 are sealed with PVC pipe caps to ensure that the corrosive solution and gas will not leak in the tube and will not be affected by the external environment. The upper PVC pipe cap needs to reserve an aperture for the wire to pass through. The PVC pipe caps at both ends can be fully opened to change the erosion environment. The upper opening can be used to add solution and discharge gas, and the lower opening can be used to add gas and discharge solution.
[0048] The T-shaped three-way pipe 14 has an inner diameter of 40 mm and a thickness of 2 mm. It is used to connect the pipelines. Each longitudinal PVC pipe is connected to three transverse ones. Three different corrosion environments can be set through the longitudinal pipe 12. The differences in the mechanical properties of the prestressed resin anchor cables under different corrosion environments can be compared, including but not limited to corrosive solution immersion corrosion, corrosive solution electrochemical corrosion, corrosive gas corrosion, and dry-wet alternation.
[0049] After the rear end of the anchor cable 2 is bonded and anchored, two pads 8 are set for each anchor cable on the outside of the front end of the concrete pier 1, which can disperse the stress area of the anchor, improve the shear strength of the anchor, and ensure the firmness and stability of the anchor. The anchor cable dynamometer 9 is arranged between the two pads 8 at the front end of each anchor cable 2, and a 500T type 3-cable anchor cable dynamometer with a range of 0-500KN is used. The stress changes of each anchor cable 2 during the tensioning process and the magnitude of the stress of the anchor cable 2 after the prestressing is completed can be intuitively tested, and the prestress loss characteristics under the erosion environment can be tested. The influence of the post-tensioning anchor cable on the stress of the pre-tensioning anchor cable 2 can be tested by different tensioning sequences of the anchor cable 2. The anchor cable 2 pulling test can also be carried out later to test the changes in the ultimate anchoring force of the anchor cable 2 to evaluate the influence of the resin anchoring performance on the erosion environment.
[0050] The anchor 10 uses a model of KM22 and is installed on the front end pad 8. After the anchor cable 2 is tensioned and prestressed, it locks the anchor cable 2 with a rebound tendency and cooperates with the pad 8 to generate compressive stress acting on the front end of the concrete pier 1.
[0051] The annular stainless steel mesh 6 is connected to the external power source 5 through a wire and buried in the transverse tube 11 through an opening position. The material of uniform specification is selected and can pass through the PVC tube 4 with an inner diameter of 36mm. The annular stainless steel mesh 6 obtains electrons in the corrosive chemical solution as the cathode of the corrosion galvanic cell. Its flexible mesh structure can half wrap the anchor cable to cause uniform electrochemical corrosion. The use of uniform specifications can control variables, test the voltage and current generated by the electrochemical corrosion of the anchor cable 2 under the erosion environment of different corrosive solutions, and reflect its corrosion degree. The hollow section anchor cable 2 loses electrons as the anode of the corrosion galvanic cell, and its surface corrosion can be directly observed to reflect its corrosion degree.
[0052] The power supply 5 that can adjust and measure A / U has a negative electrode connected to the wire of the annular stainless steel mesh 6, and a positive electrode connected to the exposed anchor cable 2 in the hollowed-out part of the concrete pier 1 through a wire, forming a corrosion galvanic cell. The power supply 5 can be used only as a current and voltage measuring meter to test the voltage and current that may be generated by the resin anchor cable 2 being immersed and corroded in the erosion environment of different corrosive solutions, react and compare its corrosion degree, and can also subsequently apply a specific voltage / current to generate electrochemical corrosion, and test the change of prestress of the anchor cable 2 in the erosion environment of electrochemical corrosion.
[0053] The present invention can change the spacing and number of the reserved anchor holes of the concrete pier 1 and the anchoring length and free end length of the resin anchor cable according to needs, tension different prestressed anchor cables 2, complete the mechanical response test of the prestressed resin anchor cable 2 under the erosion environment under different conditions, and can also compare and test the group anchor effect characteristics under different anchor cable 2 spacings. The PVC pipe 4 can effectively accommodate corrosive solutions and gases and reduce the amount used, ensuring that the corrosive environment only acts on the anchor cable. The longitudinal pipe 12 uses transparent materials and can be used to observe the corrosive solution and the internal situation of the reaction solution. The upper and lower ends of the pipe are sealed with PVC pipe covers, and the PVC pipe covers at both ends can be opened, which is convenient for changing different erosion environments, including but not limited to corrosive solution immersion corrosion, corrosive solution electrochemical corrosion, corrosive gas corrosion and dry-wet alternation, etc., and the differences in the mechanical properties of the prestressed resin anchor cable 2 under different erosion environments can be tested. The anchor cable dynamometer 9 can test each tree The stress changes of the resin anchor cable during the tensioning process, the earth pressure box 7 can be used to test the diffusion of compressive stress on the concrete during the prestressing tensioning stage and the prestressing loss stage of the resin anchor cable 2, and can reflect the changes in the compressive stress of the concrete under the action of the corrosive environment. The power supply 5 that can adjust and measure A / U can be used only for measurement, and can test the voltage and current that may be generated by the immersion corrosion of the resin anchor cable 2 in the corrosive solution corrosion environment to reflect its corrosion degree. It can also subsequently apply a specific voltage / current to generate electrochemical corrosion to test the prestress change and prestress loss of the resin anchor cable 2. The annular stainless steel mesh 6 uses materials of uniform specifications to control variables, and compare the voltage and current generated by the electrochemical corrosion of the resin anchor cable 2 in the erosion environment of different corrosive solutions to reflect its corrosion degree. The hollow section of the resin anchor cable loses electrons as the anode of the corrosion primary battery, and its surface corrosion can be observed, which intuitively reflects its corrosion degree.
[0054] Example 2
[0055] like Figure 8 , 9 As shown, on the basis of Example 1, the upper end of the longitudinal tube 12 is provided with an upper cover body 15 with a convex structure, and the outer diameter of the raised portion of the upper cover body 15 is consistent with the inner diameter of the upper end of the longitudinal tube 12. When in use, the raised portion of the upper cover body 15 is inserted into the longitudinal tube 12, thereby achieving sealing of the upper end portion of the longitudinal tube 12.
[0056] The lower end of the longitudinal tube 12 is also provided with a lower cover body 18 with a convex structure. The outer diameter of the raised part of the lower cover body 18 is consistent with the inner diameter of the lower end of the longitudinal tube 12. When in use, the raised part of the lower cover body 18 is first inserted into the lower end of the longitudinal tube 12, and then the corrosive solution is filled into the longitudinal tube 12. Finally, the upper cover body 15 is installed at the upper end of the longitudinal tube 12 to conduct a test on the mechanical response of the prestressed resin anchor cable under a corrosive environment.
[0057] A first airbag component 16 is provided at the end of the raised portion of the lower cover body 18, a blind hole is provided on the side wall of the raised portion of the lower cover body 18, a second airbag component 20 and a limit block 17 are provided in the blind hole, and the telescopic end of the second airbag component 20 is connected to the limit block 17; a limit groove is provided on the inner wall of the longitudinal tube 12, and the limit groove is close to the lower end of the longitudinal tube 12; a through hole is also provided at the bottom of the lower cover body 18, and the through hole passes through the top of the raised portion of the lower cover body 18; a connecting tube 21 is also provided in the through hole, one end of the connecting tube 21 extends into the first airbag component 16 and communicates with the interior of the first airbag component 16, and a first fixing plate 23 and a second are also provided in the other end of the connecting tube 21 Fixed disk, the outer diameters of the first fixed disk 23 and the second fixed disk are consistent with the inner diameter of the connecting tube 21, and the first fixed disk 23 and the second fixed disk are arranged along the axial direction of the connecting tube 21, and a first elastic member 24 is provided on the end face of the first fixed disk 23 facing the second fixed disk, and a blocking block 26 is provided on the first elastic member 24; a first exhaust hole is also provided on the first fixed disk 23, and a second exhaust hole is provided on the second fixed disk, and the first elastic member 24 is used to push the blocking block 26 to block the second exhaust hole; a hose 22 is also provided on the side wall of the connecting tube 21, one end of the hose 22 is connected to the connecting tube 21, and the other end is connected to the second airbag member 20.
[0058] In order to prevent the corrosive solution loaded into the longitudinal tube 12 from leaking, a lower cover 18 needs to be provided at the bottom of the longitudinal tube 12. The lower cover 18 in the prior art is connected to the bottom of the longitudinal tube 12 by a plug-in or threaded method. The threaded connection is not conducive to repeated use. When the lower cover 18 is repeatedly connected to the longitudinal tube 12, it is easy to cause thread wear. In actual application, the plug-in method is adopted. Since a certain volume of corrosive solution is contained in the longitudinal tube 12, the corrosive solution exerts a certain pressure on the lower cover 18, causing the lower cover 18 to fall off from the bottom of the longitudinal tube 12, resulting in the leakage of the corrosive solution. In order to prevent the above situation from happening, a first airbag member 16 is provided on the top of the raised portion of the lower cover 18 in this embodiment. The first airbag member 16 is made of corrosion-resistant rubber material and is filled with a certain amount of gas. When in use, the first airbag member 16 in an expanded state is first inserted into the lower portion of the longitudinal body 12. The first airbag 16 is pressed and deformed by the corrosive solution, and the gas inside it is squeezed into the connecting tube 21. Since the lower end of the connecting tube 21 is in a blocked state under the joint action of the first elastic member 24 and the blocking block 26, the gas entering the connecting tube 21 can only enter the unexpanded second airbag 20 through the hose 22, forcing the second airbag 20 to gradually expand. During the expansion process, the second airbag 20 pushes the limit block 17 to move toward the limit groove of the inner wall of the longitudinal tube 12, and finally the limit block 17 is inserted into the limit groove. Under the joint action of the limit groove and the limit block 17, the lower cover 18 can be limited, so that the lower cover 18 is stably fixed at the lower end of the longitudinal tube 12 and is not easy to fall off from the bottom of the longitudinal tube 12.
[0059] When the raised portion of the lower cover 18 is completely inserted into the lower end of the longitudinal tube 12 , the horizontal height of the limiting block 17 is greater than the horizontal height of the limiting groove.
[0060] In actual application, assuming that the raised portion of the lower cover 18 is fully inserted into the lower end of the longitudinal tube 12, the limit block 17 is flush with the limit groove. As the corrosive solution is poured into the longitudinal tube 12, the corrosive solution exerts instantaneous pressure on the first airbag component 16, which causes the first airbag component 16 and the lower cover 18 to be displaced downward as a whole, thereby causing the limit block 17 to move instantly to the bottom of the limit groove, and finally making it impossible for the second airbag component 20 to push the limit block 17 to be stuck in the limit groove, causing the lower cover 18 to fall off from the lower end of the longitudinal tube 12. Therefore, in order to prevent the above situation from occurring, the limit block 17 is set when the raised portion of the lower cover 18 is fully inserted into the longitudinal tube 12. The positioning block 17 is located above the limiting groove, so that when a corrosive solution is poured into the longitudinal tube 12, the instantaneous impact of the corrosive solution on the first airbag component 16 causes the lower cover 18 to move downward as a whole, and the first airbag component 16 is squeezed during the downward movement to transfer the internal gas to the second airbag component 20, so that the second airbag component 20 gradually expands and pushes the positioning block 17 to be in close contact with the inner wall of the longitudinal tube 12, and the friction resistance between the positioning block 17 and the inner wall of the longitudinal tube 12 can reduce the sliding speed of the lower cover 18; and when the positioning block 17 on the lower cover 18 slides down to be flush with the limiting groove, the positioning block 17 will be inserted into the limiting groove to fix the lower cover 18 in the lower end of the longitudinal tube 12.
[0061] A movable rod 19 is also provided at the bottom of the lower cover body 18, and the movable rod 19 is located in the through hole at the bottom of the lower cover body 18. The outer diameter of the movable rod 19 is smaller than the inner diameter of the through hole. An unlocking rod 25 is provided at the end of the movable rod 19 located in the through hole, and the outer diameter of the unlocking rod 25 is smaller than the inner diameter of the second exhaust hole of the second fixed plate; an assembly groove is also provided on the inner wall of the through hole of the lower cover body 18, and a second elastic member is provided in the assembly groove. The second elastic member is sleeved on the movable rod 19, and the second elastic member is connected to the outer wall of the movable rod 19.
[0062] After the test is completed, when the lower cover 18 needs to be removed from the longitudinal tube 12, the movable rod 19 is pushed upward to force the unlocking rod 25 on the movable rod 19 to be inserted into the second exhaust hole of the second fixed plate, and the blocking block 26 originally in the second exhaust hole is pushed upward to move and compress the first elastic member 24. At this time, under the action of the connecting tube 21, the first airbag member 16 and the second airbag member 20 are both connected to the outside world. A third elastic member is provided in the first airbag member 16, and a fourth elastic member is provided in the second airbag member 20. When the first airbag member 16 is in a compressed state, the third elastic member is in a compressed state. When the second airbag member 20 is in an expanded state, the fourth elastic member is in a stretched state. Therefore, when the first airbag member 16 is in a compressed state, the third elastic member is in a compressed state. When the second airbag member 20 is in an expanded state, the fourth elastic member is in a stretched state. 6 and the second airbag component 20 are connected to the outside world, under the action of the third elastic member, the first airbag component 16 will slowly recover its deformation, and the first airbag component 16 will generate negative pressure inside during the process of recovering its deformation, so that the outside air is sucked into the first airbag component 16, so that the first airbag component 16 recovers its deformation again for subsequent continued use; and when the second airbag component 20 is connected to the outside air, under the action of the fourth elastic member, the second airbag component 20, which was originally in an expanded state, is pulled to gradually shrink and recover to its initial state, and the second airbag component 20 will discharge the internal gas to the outside during the process of recovering its deformation, and at the same time pull the limit block 17 out of the limit groove, remove the constraint of the limit block 17 on the lower cover body 18, so that the lower cover body 18 can be quickly removed from the longitudinal tube 12.
[0063] The specific implementation methods described above further illustrate the objectives, technical solutions and beneficial effects of the present invention in detail. It should be understood that the above description is only a specific implementation method of the present invention and is not intended to limit the scope of protection of the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the scope of protection of the present invention.
Claims
1. A test device for the mechanical response of prestressed resin anchor cables under corrosive environments, characterized in that: The invention comprises a concrete pier (1), a power source (5) and a plurality of anchor cables (2); the top of the concrete pier (1) is provided with a groove, the inner wall of the groove is provided with a rear end reserved anchor hole, the rear end reserved anchor hole is provided with a resin anchoring agent (3), the groove is also provided with a PVC pipe (4), the anchor cable (2) passes through the PVC pipe (4) from the side of the concrete pier (1), is inserted into the rear end reserved anchor hole, and is bonded and anchored with the resin anchoring agent (3); An annular stainless steel net (6) is also provided in the PVC pipe (4), and the annular stainless steel net (6) is sleeved on the anchor cable (2), the annular stainless steel net (6) is connected to the negative electrode of the power source (5) through a wire, and the positive electrode of the power source (5) is connected to the anchor cable (2) exposed in the groove through a wire, so as to form a corrosion galvanic cell; An earth pressure box (7) is also pre-buried in the concrete pier (1); Two pads (8) and an anchor (10) are sleeved on the anchor cable (2) in a direction away from the concrete pier (1), and an anchor cable dynamometer (9) is provided between the two pads (8).
2. The test device for mechanical response of prestressed resin anchor cables under corrosive environment according to claim 1, characterized in that: The PVC pipe (4) comprises a transverse pipe (11), a short pipe (13), a T-shaped three-way pipe (14) and a longitudinal pipe (12); the short pipe (13) is connected to the side wall of the longitudinal pipe (12); the T-shaped three-way pipe (14) connects the longitudinal pipe (12) with the transverse pipe (11) through the short pipe (13); The transverse tube (11) and the T-shaped three-way tube (14) are both sleeved on the anchor cable (2).
3. The test device for mechanical response of prestressed resin anchor cables under corrosive environment according to claim 2, characterized in that: One end of the transverse tube (11) is sealed with epoxy resin AB glue and is in contact with the anchor hole reserved at the rear end in the groove; The other end of the transverse tube (11) is installed with an annular PVC tube cover and sealed with epoxy resin AB glue, and a gap of 0.01m is formed between the transverse tube (11) and the inner wall of the groove.
4. The test device for mechanical response of prestressed resin anchor cables under corrosive environment according to claim 2, characterized in that: The longitudinal tube (12) is made of transparent material, and the upper and lower ends of the longitudinal tube (12) are sealed with PVC tube covers, and the PCV tube cover at the upper end of the longitudinal tube (12) is provided with a reserved hole for the wire to pass through.
5. The test device for mechanical response of prestressed resin anchor cables under corrosive environment according to claim 2, characterized in that: Each of the longitudinal tubes (12) is connected to three transverse tubes (11), the transverse tubes (11) are sequentially distributed from top to bottom, and different erosion environments are respectively arranged in each transverse tube (11); The corrosive environment includes corrosive solution immersion corrosion, corrosive solution electrochemical corrosion, corrosive gas corrosion and dry-wet alternation.
6. The test device for mechanical response of prestressed resin anchor cables under corrosive environment according to claim 1, characterized in that: The side surface of the concrete pier (1) is provided with front end reserved anchor holes, the number of which is the same as the number of anchor cables (2), and the anchor cables (2) are inserted into the rear end reserved anchor holes of the concrete pier (1) through the front end reserved anchor holes; The earth pressure box (7) is fixedly buried around the front reserved anchor hole when the concrete pier (1) is poured; The earth pressure box (7) is evenly pre-buried at the four corners where the compressive stress of the pad (8) acts, and the earth pressure box (7) is located in the middle of the compressive stress action area of the pad (8) of the concrete pier (1) in the longitudinal direction, and is used to test the diffusion of the compressive stress on the concrete pier (1) during the prestressing tensioning stage of the anchor cable (2) and the prestress loss stage.
7. The test device for mechanical response of prestressed resin anchor cables under corrosive environment according to claim 1, characterized in that: The power source (5) can be used only as a current and voltage measuring meter to test the voltage and current that may be generated by the anchor cable (2) being immersed in corrosion environments of different corrosive solutions, and to reflect and compare the degree of corrosion; The power source (5) can also apply a specific voltage or current to generate electrochemical corrosion, and test the change in prestress of the anchor cable (2) under the erosion environment of electrochemical corrosion.
Citation Information
Patent Citations
Anchorage bedding slope model test system and method for simulating corrosive environment
CN106525707A
Corrosion simulation device and method for prestressed tensioning anchor device
CN110501280A
Pipeline steel stress corrosion test system
CN110954424A
Supporting equipment for roadway
CN114526106A
Anchor cable corrosion testing device and testing method under complex geological conditions
CN115656019A
Cited By
Fabricated adjustable inhaul cable anchoring device and mounting method
CN119779847A