Processing method

By coating E-beam photoresist of different materials on the wafer and describing E-beam, forming grooves of different widths for metal evaporation, the high production costs caused by the integration of multiple processes in the prior art are solved and The problem of low sheet efficiency achieves an efficient and accurate process method.

CN118919409APending Publication Date: 2024-11-08FUJIAN FULIAN INTEGRATED CIRCUIT CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410981571.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The existing 0.5um and 0.15um gate process technologies require two process integration, resulting in high production costs, many process steps, low chip efficiency, and increased wafer surface cleaning and photoresist removal times, increasing process risks.

Method used

Using a process method, first coat the E-beam photoresist A and E-beam photoresist B of different materials on the wafer, and form two grooves of different widths through E-beam description and development, and perform metal evaporation once. Plating forms a metal structure and removes excess metal and photoresist to simplify the process.

Benefits of technology

The E-beam operation time is reduced, and two different line widths are completed in one process, saving production costs, improving sheet efficiency and accuracy, and reducing wafer surface cleaning and process layers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919409A_ABST
    Figure CN118919409A_ABST
Patent Text Reader

Abstract

The invention provides a processing method, which comprises the following steps of: 1, coating a layer of E-beam photoresist A on the upper surface of a wafer, and then coating a layer of E-beam photoresist B which is made of a material different from that of the E-beam photoresist A; 2, writing two spaced grooves, namely a first top groove and a second top groove, on an E-beam photoresist B through E-beam tracing and developing; 3, depicting and developing by adopting E-beam, forming a first line width groove at the bottom of the first top groove, and forming a second line width groove at the bottom of the second top groove; 4, performing metal evaporation to form a metal structure I and a metal structure II; and 5, removing redundant metal and light resistance. According to the method, the manufacturing procedures of two different line widths can be completed only through one procedure, only one-time evaporation is needed, the procedure is simple and compact, the production cost is saved, and efficiency and precision are high.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of process technology, and in particular to a process method. Background Art

[0002] The existing 0.5um gate process and 0.15um gate process are integrated into two processes. The general operation of the 0.5um line width gate process is to alkaline wash the surface of the wafer to remove the surface oxide, then apply I-line photoresist, and after I-line exposure and development, form a 0.5um line width, then evaporate metal to form metal structure A, and finally remove excess metal and I-line photoresist. The general operation of the 0.15um line width gate process is to alkaline wash the surface to remove the surface oxide, apply E-beam photoresist, use E-beam description and development, form a 0.15um line width after development, then evaporate metal to form metal structure B, and finally remove excess metal and photoresist. The I-line method has high efficiency, but lower precision than the E-beam method; the E-beam method is the opposite, with high precision and low efficiency.

[0003] There are three problems with the above-mentioned method: (1) The 0.5um process and the 0.15um process are integrated into two processes, which require two vapor depositions, wasting precious metals and increasing production costs; (2) The wafer surface needs to be cleaned twice and the photoresist removed twice in the 0.15um and 0.5um processes, increasing process risks; (3) The two-process integration has many process steps, which is not conducive to wafer production efficiency. Summary of the invention

[0004] The present invention proposes a process method, which solves the defects that the existing process of different line width devices needs to adopt two processes, has many process steps and high labor cost.

[0005] The technical solution of the present invention is achieved in this way:

[0006] A manufacturing method comprises the following steps:

[0007] Step 1: Coat a layer of E-beam photoresist A on the upper surface of the wafer, and then coat a layer of E-beam photoresist B with a material different from that of E-beam photoresist A;

[0008] Step 2: Write and develop on the E-beam photoresist B by E-beam. The E-beam uses high energy to write two spaced grooves on the E-beam photoresist B, namely the first top groove and the second top groove. The inner bottom surfaces of the first top groove and the second top groove are the E-beam photoresist A.

[0009] Step 3: Using E-beam to describe and develop the E-beam photoresist A on the inner bottom surfaces of the first top groove and the second top groove, forming a first line width groove at the bottom of the first top groove, and forming a second line width groove at the bottom of the second top groove, the inner bottoms of the first line width groove and the second line width groove are wafers, and the width of the first line width groove is smaller than that of the second line width groove;

[0010] Step 4, performing metal evaporation to form a metal structure I in the first top groove and the first line width groove, and also forming a metal structure II in the second top groove and the second line width groove;

[0011] Step 5: remove the excess metal outside the metal structure I and the metal structure II, and then remove the remaining E-beam photoresist A and E-beam photoresist B.

[0012] Furthermore, the width of the first line width groove is 0.15 um, and the width of the second line width groove is 0.5 um.

[0013] Furthermore, the width of the first top groove is greater than that of the first line width groove, and the width of the second top groove is greater than or equal to that of the second line width groove.

[0014] Furthermore, the width of the first top groove is 3-5 times that of the first line width groove, and the width of the second top groove is 1-2 times that of the second line width groove.

[0015] Further, the E-beam photoresist A is PMMA, and the E-beam photoresist B is MMA; or, the E-beam photoresist A is MMA, and the E-beam photoresist B is PMMA.

[0016] Furthermore, the thickness of the E-beam photoresist A is less than 3000 Å.

[0017] Furthermore, the thickness of the E-beam photoresist B is 9000-11000A.

[0018] Furthermore, the metal evaporation includes sequentially evaporating a Pt metal layer, a Ti metal layer, a Pt metal layer and an Au metal layer.

[0019] Furthermore, the metal structure I is a gate, and the metal structure II is a gate.

[0020] Furthermore, before coating the wafer with E-beam photoresist in step 1, the surface of the wafer is alkaline washed to remove surface oxides.

[0021] Beneficial effects of the present invention:

[0022] 1. The first top groove and the second top groove can be written with high E-beam energy without requiring high precision, which greatly reduces the time of E-beam operation and improves the efficiency of wafer production.

[0023] 2. The method of the present invention can complete the process of two different line widths in just one step, and only requires one evaporation deposition. The process is simple and compact, saving production costs, high efficiency and high precision.

[0024] 3. Reduce the cleaning of the wafer surface by one pre-cleaning step and reduce one process layer, thus improving the tape-out efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0026] Figure 1 The present invention is a process diagram of a process method. DETAILED DESCRIPTION

[0027] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0028] Reference Figure 1 , a process method, comprising the following steps:

[0029] Step 1: Coat a layer of E-beam photoresist A on the upper surface of the wafer, and then coat a layer of E-beam photoresist B with a material different from that of E-beam photoresist A;

[0030] Step 2: Write and develop on the E-beam photoresist B by E-beam. The E-beam uses high energy to write two spaced grooves on the E-beam photoresist B, namely the first top groove and the second top groove. The inner bottom surfaces of the first top groove and the second top groove are the E-beam photoresist A.

[0031] Step 3: Using E-beam to describe and develop the E-beam photoresist A on the inner bottom surfaces of the first top groove and the second top groove, forming a first line width groove at the bottom of the first top groove, and forming a second line width groove at the bottom of the second top groove, the inner bottoms of the first line width groove and the second line width groove are wafers, and the width of the first line width groove is smaller than that of the second line width groove;

[0032] Step 4, performing metal evaporation to form a metal structure I in the first top groove and the first line width groove, and also forming a metal structure II in the second top groove and the second line width groove;

[0033] Step 5: remove the excess metal outside the metal structure I and the metal structure II, and then remove the remaining E-beam photoresist A and E-beam photoresist B.

[0034] As a further implementation, the width of the first line width groove is 0.15um, and the width of the second line width groove is 0.5um. Of course, the patent solution is not limited to the combination of 0.15um and 0.5um line widths, and other line widths are also possible.

[0035] As a further embodiment, the width of the first top groove is greater than the first line width groove, and the width of the second top groove is greater than or equal to the second line width groove. Specifically, the width of the first top groove may be 3-5 times that of the first line width groove, and the width of the second top groove may be 1-2 times that of the second line width groove.

[0036] As a further implementation, the E-beam photoresist A is PMMA, and the E-beam photoresist B is MMA; or, the E-beam photoresist A is MMA, and the E-beam photoresist B is PMMA.

[0037] As a further embodiment, the thickness of the E-beam photoresist A is less than 3000A. Specifically, it can be 3000A, 2900A, 2800A, 2700A, 2600A, 2500A, 2300A, 2000A or 1500A. The thickness of the E-beam photoresist B is 9000-11000A. Specifically, it can be 9000A, 10000A or 11000A.

[0038] As a further embodiment, the metal evaporation includes sequentially evaporating a Pt metal layer, a Ti metal layer, a Pt metal layer and an Au metal layer. As required, metal layers of different materials and different numbers of layers can be selected for evaporation, and are not limited to the scheme of evaporating a Pt metal layer, a Ti metal layer, a Pt metal layer and an Au metal layer.

[0039] As a further embodiment, the metal structure I is a gate, and the metal structure II is a gate. The metal structure I and the metal structure II are not limited to being gates, but may also be other types.

[0040] As a further implementation method, before coating the wafer with E-beam photoresist in step 1, the surface of the wafer is alkaline washed to remove surface oxides.

[0041] The first top groove and the second top groove of the present invention can be opened with high E-beam energy without requiring high precision, which greatly reduces the time of E-beam operation and improves the efficiency of wafer taping. The method of the present invention can complete two processes with different line widths in one process, and only requires one evaporation. The process is simple and compact, saves production costs, and has high efficiency and precision. It reduces the cleaning of the wafer surface by one pre-cleaner and reduces one process layer, which improves the efficiency of wafer taping.

[0042] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. A process method, Features: The following steps are involved: Step 1: Coat a layer of E-beam photoresist A on the upper surface of the wafer, and then coat a layer of E-beam photoresist B with a material different from that of E-beam photoresist A; Step 2: Write and develop on the E-beam photoresist B by E-beam. The E-beam uses high energy to write two spaced grooves on the E-beam photoresist B, namely the first top groove and the second top groove. The inner bottom surfaces of the first top groove and the second top groove are the E-beam photoresist A. Step 3: Using E-beam to describe and develop the E-beam photoresist A on the inner bottom surfaces of the first top groove and the second top groove, forming a first line width groove at the bottom of the first top groove, and forming a second line width groove at the bottom of the second top groove, the inner bottoms of the first line width groove and the second line width groove are wafers, and the width of the first line width groove is smaller than that of the second line width groove; Step 4, performing metal evaporation to form a metal structure I in the first top groove and the first line width groove, and also forming a metal structure II in the second top groove and the second line width groove; Step 5: remove the excess metal outside the metal structure I and the metal structure II, and then remove the remaining E-beam photoresist A and E-beam photoresist B.

2. The process as claimed in claim 1, Features: The width of the first line width groove is 0.15 um, and the width of the second line width groove is 0.5 um.

3. The process as claimed in claim 1, Features: The width of the first top groove is greater than that of the first line width groove, and the width of the second top groove is greater than or equal to that of the second line width groove.

4. The process as claimed in claim 3, Features: The width of the first top groove is 3-5 times that of the first line width groove, and the width of the second top groove is 1-2 times that of the second line width groove.

5. The process as claimed in claim 1, Features: The E-beam photoresist A is PMMA, and the E-beam photoresist B is MMA; or, the E-beam photoresist A is MMA, and the E-beam photoresist B is PMMA.

6. The process as claimed in claim 1, Features: The thickness of the E-beam photoresist A is less than 3000 Å.

7. The process as claimed in claim 1, Features: The thickness of the E-beam photoresist B is 9000-11000 Å.

8. The process as claimed in claim 1, Features: The metal evaporation includes sequentially evaporating a Pt metal layer, a Ti metal layer, a Pt metal layer and an Au metal layer.

9. The process as claimed in claim 1, Features: The metal structure I is a gate, and the metal structure II is a gate.

10. The process according to any one of claims 1 to 9, Features: Before coating the wafer with E-beam photoresist in step 1, the surface of the wafer is alkaline washed to remove surface oxides.