Semiconductor device and manufacturing method thereof
By adopting a separate gate structure and self-alignment process in semiconductor devices, the problems of channel resistance and parasitic capacitance are solved, and lower impedance and higher reliability are achieved.
Patent Information
- Application Number
- CN202310507717.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-08
- Publication Date
- 2024-11-08
AI Technical Summary
In high-power applications with high voltage and high current, the channel resistance (RON) is large, and the parasitic capacitance and size inconsistency caused by alignment errors affect the performance of the device.
Using a separate gate structure, multiple doped regions and gates are formed through a self-alignment process, ensuring that the size of doped regions and channel regions is within the design range, reducing parasitic capacitance, and dielectric through dielectric layers and gates The design of the layer reduces the electric field strength and parasitic capacitance.
It effectively reduces the channel resistance of the semiconductor device, improves the switching rate, reduces power loss, and improves the reliability and dimensional accuracy of the device.
Smart Images

Figure CN118919412A_ABST
Abstract
Description
Technical Field
[0001] Some embodiments of the present disclosure relate to semiconductor devices and methods of manufacturing the same. Background Art
[0002] In recent years, due to environmental issues such as zero carbon emissions and electric vehicles replacing fuel vehicles, the international community has begun to develop related research. Power semiconductor devices made of silicon carbide have gradually replaced silicon-based power semiconductor devices and are developing towards high-power applications with high voltage and high current. Among them, the vertical double-diffused metal-oxide-semiconductor field-effect transistor (VDMOSFET) using planar silicon carbide has played the main role of power transistors in related applications from 600V to 3000V. Among them, channel resistance is still the main source of resistance contribution in the entire VDMOSFET structure. In order to reduce the on-resistance (R ON ), shortening the channel length of the device and maintaining the same channel length is an effective way to reduce R ON One of the methods. Summary of the invention
[0003] Some embodiments of the present disclosure provide a method for forming a semiconductor device, including forming an epitaxial layer on a substrate, forming a hard mask layer on the epitaxial layer, the hard mask layer having a first portion and a second portion, and a gap between the first portion and the second portion, performing an oxidation process to form an oxide layer on the surface of the hard mask layer, forming a source region in the epitaxial layer through the gap in the hard mask layer, removing the first portion of the hard mask layer and the oxide layer, using the second portion of the hard mask layer as an ion implantation mask to form a well in the epitaxial layer, forming a sacrificial dielectric layer on the source region and the well, removing the second portion of the hard mask layer, using the sacrificial dielectric layer as an ion implantation mask to form a junction field effect transistor region in the epitaxial layer, forming a dielectric layer on the junction field effect transistor region, removing the sacrificial dielectric layer, and forming a gate structure on one side of the dielectric layer.
[0004] In some embodiments, the well includes a channel region, the channel region of the well is adjacent to the source region, and the thickness of the oxide layer is the same as the width of the channel region of the well.
[0005] In some embodiments, forming a gate structure on one side of the dielectric layer includes forming a gate dielectric material layer on the source region and the well, forming a gate material layer on the gate dielectric material layer and the dielectric layer, removing a horizontal portion of the gate material layer, leaving a vertical portion of the gate material layer to form a gate on the channel region of the well, and patterning the gate dielectric material layer using the gate as a mask to form a gate dielectric layer.
[0006] In some embodiments, when the sacrificial dielectric layer is formed, the sacrificial dielectric layer contacts the second portion of the hard mask layer.
[0007] In some embodiments, when the dielectric layer is formed, the dielectric layer contacts the sacrificial dielectric layer.
[0008] Some embodiments of the present disclosure provide a semiconductor device, including an epitaxial layer, a dielectric layer, and a gate. The epitaxial layer includes a well, a base region, a source region, and a junction field effect transistor region. The well includes a channel region, the base region is in the well, the source region is in the well and adjacent to the base region, wherein the channel region of the well is adjacent to the source region, and the junction field effect transistor region is adjacent to the well. The dielectric layer is on the junction field effect transistor region. The gate is adjacent to the dielectric layer and covers the channel region of the well, and the boundary of the gate is substantially aligned with the boundary between the junction field effect transistor region and the well.
[0009] In some embodiments, a vertical projection of the gate on the epitaxial layer does not overlap with the JFET region.
[0010] In some embodiments, the width of the gate becomes wider as it gets closer to the epitaxial layer.
[0011] In some embodiments, the thickness of the dielectric layer may be between 0.8 and 1 μm.
[0012] In some embodiments, the semiconductor device further includes a gate dielectric layer, wherein a thickness of the gate dielectric layer is smaller than a thickness of the dielectric layer between the gate and the well.
[0013] Some embodiments of the present disclosure are related to a semiconductor device with a split gate structure. In some embodiments of the present disclosure, multiple doped regions and gates of the semiconductor device are formed by a self-alignment process, thereby reducing parasitic capacitance generated on the semiconductor device due to alignment errors and ensuring that the sizes of the doped regions and the channel region are within a designed range. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figures 1 to 15 A cross-sectional view is shown of a process for manufacturing a semiconductor device in some embodiments of the present disclosure. DETAILED DESCRIPTION
[0015] Some embodiments of the present disclosure are related to a semiconductor device with a split gate structure. In some embodiments of the present disclosure, multiple doped regions and gates of the semiconductor device are formed by a self-alignment process, thereby reducing parasitic capacitance generated on the semiconductor device due to alignment errors and ensuring that the sizes of the doped regions and the channel region are within a designed range.
[0016] Figures 1 to 15 FIG. 1 is a cross-sectional view showing a process of manufacturing a semiconductor device 100 in some embodiments of the present disclosure. Figure 1 , forming an epitaxial layer 110 on the substrate 105. The substrate 105 and the epitaxial layer 110 are any suitable substrates. In some embodiments, the substrate 105 may be made of, for example, but not limited to, silicon carbide. The substrate 105 may be doped with a dopant of a first semiconductor type and be of the first semiconductor type. For example, the substrate 105 may be an N-type heavily doped substrate, such as a heavily doped region including N-type dopants such as phosphorus, arsenic, and nitrogen. In some embodiments, the epitaxial layer 110 may be made of, for example, but not limited to, silicon carbide. The epitaxial layer 110 may be doped with a dopant of a first semiconductor type and be of the first semiconductor type. For example, the epitaxial layer 110 may be an N-type lightly doped region, such as a lightly doped region including N-type dopants such as phosphorus, arsenic, and nitrogen.
[0017] refer to Figure 2 , a plurality of base regions 112 are formed in the epitaxial layer 110. Specifically, a hard mask layer 120 may be first formed on the epitaxial layer 110. The hard mask layer 120 may expose a portion of the epitaxial layer 110. Next, an ion implantation process IMP1 is performed using the hard mask layer 120 as an ion implantation mask to form base regions 112 in the epitaxial layer 110. In the ion implantation process IMP1, dopants having a second semiconductor type may be implanted into the epitaxial layer 110 to form a base region 112 of a second semiconductor type in the epitaxial layer 110, and the second semiconductor type is different from the first semiconductor type. For example, the base region 112 may be a heavily doped P-type region, such as a heavily doped region containing P-type dopants such as boron, aluminum, and gallium. Other regions of the epitaxial layer 110 that are not implanted with ions by the ion implantation process IMP1 are drift regions 111. After the base region 112 is formed, refer to Figure 3 , remove the hard mask layer 120. In some embodiments, the hard mask layer 120 can be removed by a suitable method, such as etching.
[0018] refer to Figure 4 , a hard mask layer 130 is formed on the epitaxial layer 110, the hard mask layer 130 having a first portion 132 on the base region 112 and a second portion 134 not on the base region 112, with a gap G between the first portion 132 and the second portion 134. The hard mask layer 130 can be defined using a conventional photolithography process. The gap G can expose a portion of the base region 112 and also expose a portion of the epitaxial layer 110 not occupied by the base region 112. In some embodiments, the hard mask layer 130 can be made of polysilicon.
[0019] refer to Figure 5, an oxidation process is performed to form an oxide layer 136 on the surface of the hard mask layer 130. A portion of the oxide layer 136 can be obtained by oxidizing and sacrificing a portion of the hard mask layer 130. In some embodiments, the oxidation process is a selective oxidation process, so that the oxide layer 136 has a higher oxidation rate on the surface of the hard mask layer 130. On the contrary, the oxide layer 136 has a lower oxidation rate on the surface of the epitaxial layer 110, so that in some embodiments, the oxide layer 136 forms a relatively thin oxide layer on the surface of the epitaxial layer 110. In some embodiments, in order to prevent the oxidation process from also oxidizing the epitaxial layer 110, a thin protective layer can be formed on the epitaxial layer 110 before forming the hard mask layer 130 to protect the epitaxial layer 110. In some embodiments, the oxide layer 136 has a uniform thickness W1. In some embodiments, the sidewalls of the oxide layer 136 can be substantially aligned with the boundaries of the base region 112, such as Figure 5 In some embodiments, the thickness W1 of the oxide layer 136 is between 0.5 μm and 1 μm. The thickness W1 of the oxide layer 136 can be used to determine the channel width of the semiconductor device 100 .
[0020] refer to Figure 6 , a plurality of source regions 114 are formed in the epitaxial layer 110 through the gaps G of the hard mask layer 130, and each source region 114 is adjacent to the base region 112. That is, the source region 114 is defined by the gaps G of the hard mask layer 130. The hard mask layer 130 and the oxide layer 136 may be used as ion implantation masks to perform an ion implantation process IMP2 to form the source region 114 in the epitaxial layer 110. In the ion implantation process IMP2, dopants having a first semiconductor type may be implanted into the epitaxial layer 110 to form a source region 114 of the first semiconductor type in the epitaxial layer 110. For example, the source region 114 may be an N-type heavily doped region, such as a heavily doped region containing N-type dopants such as phosphorus, arsenic, and nitrogen. The gaps G of the hard mask layer 130 may simultaneously define both sides of the source region 114, so that the source region 114 is adjacent to and contacts the base region 112.
[0021] refer to Figure 7, remove the first portion 132 of the hard mask layer 130 and the oxide layer 136. Then, use the second portion 134 of the hard mask layer 130 as an ion implantation mask to form a plurality of wells 116 in the epitaxial layer 110. Specifically, since there is an etching selectivity between the oxide layer 136 and the hard mask layer 130, the oxide layer 136 on the hard mask layer 130 can be removed first. Then, use a photomask to remove the first portion 132 of the hard mask layer 130. In this way, the base region 112 and the source region 114 are completely exposed, and a portion of the epitaxial layer 110 not occupied by the base region 112 and the source region 114 is also exposed. Then, the second portion 134 of the hard mask layer 130 can be used as an ion implantation mask to perform an ion implantation process IMP3 to form a well 116 in the epitaxial layer 110. In the ion implantation process IMP3, dopants of the second semiconductor type may be implanted into the epitaxial layer 110 to form a well 116 of the second semiconductor type in the epitaxial layer 110. For example, the well 116 may be a P-type lightly to medium doped region, such as a lightly to medium doped region containing P-type dopants such as boron, aluminum, and gallium.
[0022] The bottom of the well 116 is lower than the bottom of the base region 112 and the source region 114, so that the base region 112 and the source region 114 can be located in the well 116. The well 116 includes a channel region 116C, the channel region 116C of the well 116 is adjacent to the source region 114, and the oxide layer 136 (see Figure 6 ) is substantially the same as the width W2 of the channel region 116C of the well 116. Since the oxide layer 136 has a uniform thickness W1, it is also possible to ensure that the width W2 of the channel region 116C of the well 116 on both sides of the second portion 134 of the hard mask layer 130 is consistent. In this way, the channel region 116C of the well 116 having the same width W2 can be defined through a self-alignment process.
[0023] refer to Figure 8 , a sacrificial dielectric layer 140 is formed on the base region 112, the source region 114, and the well 116. Specifically, a sacrificial dielectric material layer can be formed on the base region 112, the source region 114, the well 116, and the second portion 134 of the hard mask layer 130. Then, the sacrificial dielectric material layer is planarized until the surface of the second portion 134 of the hard mask layer 130 is exposed, and the sacrificial dielectric layer 140 is formed on the base region 112, the source region 114, and the well 116. The sacrificial dielectric layer 140 contacts the second portion 134 of the hard mask layer 130, so the sacrificial dielectric layer 140 can be used to define a self-aligned junction field-effect transistor (JFET) region in subsequent processes. The sacrificial dielectric layer 140 can be made of a material different from the second portion 134 of the hard mask layer 130. For example, the sacrificial dielectric layer 140 can be made of nitride.
[0024] refer to Fig. 9 , remove the second portion 134 of the hard mask layer 130, and use the sacrificial dielectric layer 140 as an ion implantation mask to form a junction field-effect transistor (JFET) region 118 in the epitaxial layer 110. Specifically, since the second portion 134 of the hard mask layer 130 and the sacrificial dielectric layer 140 are made of different materials, the second portion 134 of the hard mask layer 130 can be removed by utilizing the selectivity of the etching process to different materials. Next, an ion implantation process IMP4 is performed using the sacrificial dielectric layer 140 as an ion implantation mask to form a JFET region 118 in the epitaxial layer 110. The JFET region 118 can be formed between the two wells 116. In the ion implantation process IMP4, a dopant having a first semiconductor type can be implanted into the epitaxial layer 110 to form a first semiconductor type in the epitaxial layer 110 to form a JFET region 118 in the epitaxial layer 110. For example, the JFET region 118 formed in the epitaxial layer 110 may be an N-type medium or lightly doped region, such as a medium or lightly doped region containing N-type dopants such as phosphorus, arsenic, and nitrogen. In this way, the JFET region 118 may be formed in the middle of the well 116. The position of the JFET region 118 may be determined by the gap between the sacrificial dielectric layers 140 (i.e., Figure 8 The JFET region 118 is defined by the second portion 134 of the hard mask layer 130, so no additional mask is needed to define the position of the JFET region 118, which would cause the problem of positional displacement of the JFET region 118. The JFET region 118 will not overlap with the channel region 116C of the well 116 to reduce device characteristics. It should be noted that the formation order of the base region 112, the source region 114, the well 116, and the JFET region 118 is only an example and is not limited to the one disclosed in the present case.
[0025] refer to Fig.10 , an annealing process AN is performed on the epitaxial layer 110. The annealing process AN can be used to activate the ions implanted into the epitaxial layer 110 and repair the damage caused by the ion implantation process. In some embodiments, the operating temperature of the annealing process AN can be between 1600 degrees Celsius and 1700 degrees Celsius.
[0026] refer to Fig.11, a dielectric layer 150 is formed on the JFET region 118. Specifically, a dielectric material layer may be formed on the JFET region 118 and the sacrificial dielectric layer 140. Next, the dielectric material layer is planarized until the surface of the sacrificial dielectric layer 140 is exposed, and the dielectric layer 150 is formed on the JFET region 118. The dielectric layer 150 contacts the sacrificial dielectric layer 140, so that the gates subsequently formed on both sides of the dielectric layer 150 can be self-aligned with the channel region 116C. The dielectric layer 150 may be made of a material having an etching selectivity ratio with the sacrificial dielectric layer 140. For example, the dielectric layer 150 may be made of oxide (SiO2) or nitride (SiN). In some embodiments, the thickness W3 of the dielectric layer 150 may be between 0.8 and 1 μm. When the thickness of the dielectric layer 150 exceeds the disclosed range, it will cause problems in the subsequent photolithography and etching processes, but when the thickness of the dielectric layer 150 is less than the disclosed range, there is a risk of excessive electric field leading to reduced reliability and premature breakdown. The dielectric layer 150 with a thickness of W3 can be used to reduce the intensity of the induced electric field, thereby reducing the risk of dielectric layer 150 breakdown.
[0027] refer to Figure 12 to Figure 14 , remove the sacrificial dielectric layer 140 and form the gate structure GS of the transistor on both sides of the dielectric layer 150. Specifically, refer to Fig.12 , the sacrificial dielectric layer 140 is removed and a gate dielectric material layer 155 is formed on the base region 112, the source region 114, and the well 116. In some embodiments, a thermal oxidation process may be performed to form the gate dielectric material layer 155 on the base region 112, the source region 114, and the well 116. The gate dielectric material layer 155 may be in contact with the dielectric layer 150, and the thickness of the gate dielectric material layer 155 is less than the thickness of the dielectric layer 150. Since the dielectric layer 150 is made of a material having an etching selectivity ratio with the sacrificial dielectric layer 140, the selectivity of the etching process to different materials may be utilized to remove the sacrificial dielectric layer 140.
[0028] Next, refer to Fig.13 , a gate material layer 162 is formed on the gate dielectric material layer 155 and the dielectric layer 150. The process of forming the gate material layer 162 is a conformal deposition process, so the gate material layer 162 can be conformally formed on the gate dielectric material layer 155 and the dielectric layer 150. That is, the gate material layer 162 has a uniform thickness.
[0029] refer to Fig.14, remove the horizontal portion of the gate material layer 162, leaving the vertical portion of the gate material layer 162 to form the gate 160 on the channel region 116C of the well 116, and then pattern the gate dielectric material layer 155 using the gate 160 as a mask to form a gate dielectric layer 157. The gate 160 can be formed on both sides of the dielectric layer 150, and the gate dielectric layer 157 is formed between the gate 160 and the well 116. The gate dielectric layer 157 and the gate 160 can be collectively referred to as a gate structure GS. The horizontal portion of the gate material layer 162 can be removed using a dry etching process. Since the gate material layer 162 has a uniform thickness, the width of the gate 160 can also be ensured to be consistent. The width of the gate 160 can be adjusted by adjusting the thickness of the gate material layer 162, so that the gate 160 can completely cover the channel region 116C of the well 116 to avoid resistance increase. In addition, the gate 160 can be self-aligned with the boundary between the channel region 116C of the well 116 and the JFET region 118, and avoid the gate 160 contacting or crossing the JFET region 118 to generate parasitic capacitance, so as to avoid the parasitic capacitance affecting the high-frequency switching characteristics and increasing power consumption. This can also reduce the channel resistance effect of the semiconductor device 100. In some embodiments, the gate 160 can be made of a low-impedance material such as polysilicon or metal. Since the gate 160 is Fig.10 The gate 160 is formed after the annealing process AN, so the high temperature of the annealing process AN will not have a negative impact on the gate 160, for example, the high temperature of the annealing process AN will not melt the gate 160. Since the gate 160 is formed by etching the gate material layer 162 conformally on the dielectric layer 150, the gate 160 is a structure that is narrow at the top and wide at the bottom. That is, the width of the gate 160 is wider when it is closer to the epitaxial layer 110. In addition, the gate 160 has both a vertical sidewall and a curved sidewall, and the vertical sidewall of the gate 160 contacts the dielectric layer 150.
[0030] refer to Fig.15, a source contact 170 is formed on the base region 112 and the source region 114, and a drain electrode 180 is formed under the substrate 105. Thus, the semiconductor device 100 is formed. The semiconductor device 100 may include a substrate 105, an epitaxial layer 110, a dielectric layer 150 and a gate 160. The epitaxial layer 110 is on the substrate 105, and the epitaxial layer 110 includes a drift region 111, a well 116, a base region 112, a source region 114 and a JFET region 118. The well 116 includes a channel region 116C. The base region 112 is in the well 116. The source region 114 is in the well 116 and is adjacent to the base region 112, wherein the channel region 116C of the well 116 is adjacent to the source region 114. The JFET region 118 is adjacent to the well 116. That is, the channel region 116C of the well 116 is located between the JFET region 118 and the source region 114, and the JFET region 118 is between two different wells 116. The drift region 111 is below the well 116 and the JFET region 118. The substrate 105, the drift region 111, the source region 114, and the JFET region 118 may be of a first semiconductor type, the base region 112 and the well 116 may be of a second semiconductor type, and the first semiconductor type is different from the second semiconductor type. The ion doping concentration of the source region 114 is greater than that of the JFET region 118, and the ion doping concentration of the JFET region 118 is greater than that of the drift region 111. The ion doping concentration of the base region 112 is greater than that of the well 116. In some embodiments, the ion doping concentration of the source region 114 is 1.0E19 / cm 3 To 5.0E20 / cm 3 The ion doping concentration of the JFET region 118 and the drift region 111 is 1.0E15 / cm 3 To 5.0E17 / cm 3 The ion doping concentration of the base region 112 is 1.0E19 / cm 3 To 5.0E20 / cm 3 , and the ion doping concentration of well 116 is 1.0E16 / cm 3 To 1.0E18 / cm 3 .
[0031] The dielectric layer 150 is on the JFET region 118. The dielectric layer 150 can be used to reduce the electric field strength induced therein, thereby reducing the risk of breakdown of the dielectric layer 150. The gate 160 is adjacent to the dielectric layer 150 and covers the channel region 116C of the well 116, and the boundary of the gate 160 is substantially aligned with the boundary between the JFET region 118 and the well 116. The gate 160 directly contacts the channel region 116C. The gate 160 is a separated gate, that is, the gate 160 is formed on both sides of the dielectric layer 150, rather than formed on top of the dielectric layer 150. The separated gate can reduce the stress damage of the high voltage to the dielectric layer 150 and improve the reliability performance. In addition, the vertical projection of the gate 160 on the epitaxial layer 110 does not overlap with the junction field effect transistor region 118, so the gate 160 can reduce parasitic capacitance and increase the switching rate, thereby reducing the power loss caused by switching. In addition, the thickness W3 ( Fig.11 ) can be very thick to reduce the electric field strength induced by the dielectric layer 150 and thus reduce the risk of breakdown of the dielectric layer 150. The semiconductor device 100 further includes a gate dielectric layer 157 between the gate 160 and the well 116, the thickness of the gate dielectric layer 157 is less than the thickness of the dielectric layer 150, and the gate dielectric layer 157 contacts the dielectric layer 150. The semiconductor device 100 further includes a source contact 170 on the base region 112 and the source region 114 and a drain electrode 180 under the epitaxial layer 110.
[0032] In summary, the channel region, source region, JFET region and gate of the semiconductor device of some embodiments of the present disclosure can be formed by a self-aligned method, so a single mask (ie Figure 4 The ion implantation process and gate formation of the channel region, source region, JFET region are completed by using a mask for defining the hard mask layer. This can avoid the problem of deviation or size inconsistency of the channel region, source region, JFET region and gate caused by the alignment error of the mask. In addition, the parasitic capacitance in the semiconductor device can be reduced and the semiconductor device can have a lower impedance.
[0033] The above descriptions are only some embodiments of the present disclosure, not all embodiments. Any equivalent changes made to the technical solution of the present disclosure by ordinary technicians in this field after reading the specification of the present disclosure are covered by the claims of the present disclosure.
[0034]
Explanation of symbols
[0035] 100: Semiconductor devices
[0036] 105: Substrate
[0037] 110: Epitaxial layer
[0038] 111: Drift Zone
[0039] 112: Base region
[0040] 114: Source region
[0041] 116: Trap
[0042] 116C: Channel area
[0043] 118: Junction Field Effect Transistor Region / JFET Region
[0044] 120: Hard mask layer
[0045] 130: Hard mask layer
[0046] 132: Part 1
[0047] 134: Part 2
[0048] 136: Oxide layer
[0049] 140: Sacrificial dielectric layer
[0050] 150: Dielectric layer
[0051] 155: Gate dielectric material layer
[0052] 157: Gate dielectric layer
[0053] 160: Gate
[0054] 162: Gate material layer
[0055] 170: Source contact
[0056] 180: Drain electrode
[0057] AN: Annealing process
[0058] G: Gap
[0059] GS: Gate Structure
[0060] IMP1: Ion Implantation Process
[0061] IMP2: Ion Implantation Process
[0062] IMP3: Ion Implantation Process
[0063] IMP4: Ion Implantation Process
[0064] W1: Thickness
[0065] W2: Width
[0066] W3: Thickness.
Claims
1. A method for forming a semiconductor device, characterized in that: Include: forming an epitaxial layer on a substrate; forming a hard mask layer on the epitaxial layer, wherein the hard mask layer has a first portion and a second portion, and a gap is formed between the first portion and the second portion; performing an oxidation process to form an oxide layer on a surface of the hard mask layer; forming a source region in the epitaxial layer through the gap of the hard mask layer; removing the first portion of the hard mask layer and the oxide layer; using the second portion of the hard mask layer as an ion implantation mask to form a well in the epitaxial layer; forming a sacrificial dielectric layer on the source region and the well; removing the second portion of the hard mask layer; Using the sacrificial dielectric layer as an ion implantation mask to form a junction field effect transistor region in the epitaxial layer; forming a dielectric layer on the junction field effect transistor region; removing the sacrificial dielectric layer; and A gate structure is formed on one side of the dielectric layer.
2. The method according to claim 1, characterized in that: The well includes a channel region, the channel region of the well is adjacent to the source region, and the thickness of the oxide layer is the same as the width of the channel region of the well.
3. The method according to claim 2, characterized in that Forming the gate structure on the side of the dielectric layer comprises: forming a gate dielectric material layer on the source region and the well; forming a gate material layer on the gate dielectric material layer and the dielectric layer; Removing a horizontal portion of the gate material layer, leaving a vertical portion of the gate material layer to form the gate on the channel region of the well; as well as The gate dielectric material layer is patterned using the gate as a mask to form the gate dielectric layer.
4. The method according to claim 1, characterized in that: When the sacrificial dielectric layer is formed, the sacrificial dielectric layer contacts the second portion of the hard mask layer.
5. The method according to claim 1 or 4, characterized in that: When the dielectric layer is formed, the dielectric layer contacts the sacrificial dielectric layer.
6. A semiconductor device, characterized in that: Include: An epitaxial layer, the epitaxial layer comprising: a well, the well comprising a channel region; a base region in the well; a source region in the well and adjacent to the base region, wherein the channel region of the well is adjacent to the source region; and a junction field effect transistor region adjacent to the well; a dielectric layer on the JFET region; as well as A gate is adjacent to the dielectric layer and covers the channel region of the well, wherein a boundary of the gate is substantially aligned with a boundary between the junction field effect transistor region and the well.
7. The semiconductor device according to claim 6, wherein: The width of the gate is wider as it is closer to the epitaxial layer.
8. The semiconductor device according to claim 6 or 7, characterized in that: The vertical projection of the gate on the epitaxial layer does not overlap with the junction field effect transistor region.
9. The semiconductor device according to claim 6 or 7, characterized in that: The thickness of the dielectric layer is between 0.8 and 1 μm.
10. The semiconductor device according to claim 6 or 7, characterized in that: A gate dielectric layer is also included. The gate dielectric layer is between the gate and the well, and the thickness of the gate dielectric layer is less than the thickness of the dielectric layer.