Packaging structure and packaging method for improving chemical resistance of release layer

By preparing a passivation layer on the release layer to isolate the outside world, the problem of insufficient resistance to the release layer is solved, the integrity of the rewiring layer and the completion of the package are ensured, and the resistance to the release layer and the package are improved. stability.

CN118919497APending Publication Date: 2024-11-08HUATIAN TECHNOLOGY (KUNSHAN) ELECTRONICS CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202411018245.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-29
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

In the prior art, insufficient resistance to the release layer leads to corrosion or dissolving in the rewiring preparation process, resulting in defects in the rewiring layer and inability to complete the package.

Method used

By preparing a passivation layer on the release layer, completely isolating the release layer from the outside world and avoiding contact with chemical reagents, thereby improving the resistance of the release layer, and precise control is carried out in the rewiring layer construction and debonding process to ensure release layer integrity.

Benefits of technology

The resistance of the release layer is significantly improved, the integrity of the rewiring layer and the completion of the package are ensured, and the defect problem caused by insufficient resistance of the release layer is solved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919497A_ABST
    Figure CN118919497A_ABST
Patent Text Reader

Abstract

The invention discloses a packaging structure and a packaging method for improving chemical resistance of a release layer. The packaging method comprises the following steps: preparing the release layer on a temporary slide; the release layer at the edge of the temporary slide glass is removed, a release layer blank area is reserved, and the release layer blank area is in a wafer invalid area range; a passivation layer is prepared on the release layer, the passivation layer covers the release layer and the blank area of the release layer, and the release layer is isolated from air; constructing a rewiring layer on the passivation layer; placing the integrated circuit crystal grains on the rewiring layer and carrying out plastic packaging to form a recombined wafer; carrying out ring cutting on the recombined wafer, and cutting off a packaging body at the edge of the temporary slide glass; and stripping the temporary slide. The passivation layer covers the release layer and the blank area of the release layer, so that the release layer is isolated from the outside, the possibility that the release layer is in contact with a chemical reagent is avoided, the chemical resistance of the release layer is remarkably improved, the completion of the packaging body is effectively ensured, and the defect that the redistribution layer is incomplete due to insufficient chemical resistance of the release layer is overcome.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of semiconductor chip packaging, and in particular relates to a packaging structure and a packaging method for improving the chemical resistance of a release layer. Background Art

[0002] After the semiconductor chip is mounted on the redistribution layer and plastic-sealed to form a reconstructed wafer, it is usually necessary to remove the temporary carrier through the release layer through a debonding process. The chemical reagents in the redistribution layer preparation process, such as developer, plating solution, degumming solution, etching solution, etc., will corrode the release layer to varying degrees, which requires the chemical resistance of the release layer to be high enough to complete the subsequent processes. Due to the insufficient chemical resistance of the release layer, the release layer will be corroded or dissolved in chemical reagents during the redistribution preparation process, resulting in major defects in the redistribution, such as the inability to carry out the redistribution process or the peeling of the redistribution layer, and ultimately the inability to complete the formation of the package. Summary of the invention

[0003] In order to solve the technical problems existing in the prior art, an object of the present invention is to provide a packaging structure and a packaging method for improving the chemical resistance of a release layer.

[0004] In order to achieve the above purpose and the above technical effect, the technical solution adopted by the present invention is:

[0005] A packaging method for improving the chemical resistance of a release layer comprises the following steps:

[0006] Step 1: preparing a release layer on a temporary carrier;

[0007] Step 2: removing the release layer at the edge of the temporary carrier, leaving a release layer blank area at the edge of the temporary carrier, wherein no release layer remains in the release layer blank area, and the release layer blank area is within the invalid area of ​​the wafer;

[0008] Step 3: preparing a passivation layer on the release layer, wherein the passivation layer covers the release layer and the blank area of ​​the release layer, and the release layer is completely isolated from the air;

[0009] Step 4: construct a redistribution layer on the passivation layer;

[0010] Step 5: placing the integrated circuit die on the redistribution layer and performing plastic sealing to form a reconstructed wafer;

[0011] Step 6: Circular cut the reconstructed wafer, remove the package at the edge of the temporary carrier, and leave a blank area at the edge of the temporary carrier;

[0012] Step 7: Peel off the temporary carrier.

[0013] Furthermore, in step one, the thickness of the release layer is not less than 0.3 μm.

[0014] Furthermore, in step 2, the release layer at the edge of the temporary carrier is removed by a cleaning process.

[0015] Furthermore, in step 2, the width of the blank area of ​​the release layer is smaller than the invalid area of ​​the wafer, and the accuracy is controlled within 10% of the edge washing width.

[0016] Furthermore, in step 4, the thickness of the release layer is less than the thickness of the redistribution layer, and the TTV is less than 5% of the thickness of the release layer.

[0017] Furthermore, in step five, the integrated circuit grains include integrated circuit grain I, integrated circuit grain II, and integrated circuit grain III. The integrated circuit grain I, integrated circuit grain II, and integrated circuit grain III are respectively placed on the redistribution layer through a connecting structure, and the gaps in the connecting structure are completely filled with bottom filling materials, and the entire integrated circuit grain is covered with a packaging glue material to form a reconstructed wafer.

[0018] Furthermore, in step six, the circular cutting width is not less than the edge washing width of the release layer.

[0019] Furthermore, in step seven, a debonding process is performed to separate the release layer and the temporary carrier. The debonding process includes thermal decomposition, laser irradiation, mechanical debonding, chemical dissolution, etc., which is determined by the material type of the release layer.

[0020] The present invention also discloses a packaging structure prepared by the packaging method for improving the chemical resistance of the release layer as described above.

[0021] Furthermore, the packaging structure includes a release layer, a passivation layer, a redistribution layer and an integrated circuit grain, the release layer is arranged below the passivation layer, the redistribution layer is arranged above the passivation layer, the integrated circuit grain is placed on the redistribution layer through a connecting structure, the gap in the connecting structure is filled with a bottom filling material, and the integrated circuit grain is wrapped in a packaging glue material.

[0022] Compared with the prior art, the present invention has the following beneficial effects:

[0023] The present invention discloses a packaging structure and a packaging method for improving the chemical resistance of a release layer. The release layer and a blank area of ​​the release layer are covered with a passivation layer, so that the release layer is isolated from the outside world, thereby avoiding the possibility of the release layer contacting with chemical reagents, avoiding the release layer from being corroded or dissolved, etc., significantly improving the chemical resistance of the release layer, effectively ensuring the integrity of the redistribution layer, effectively ensuring the completion of the package, and solving the problem of incomplete redistribution layer caused by insufficient chemical resistance of the release layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1It is a structural schematic diagram of step 1 of the present invention;

[0025] Figure 2 It is a structural schematic diagram of step 2 of the present invention;

[0026] Figure 3 It is a structural schematic diagram of step three of the present invention;

[0027] Figure 4 It is a structural schematic diagram of step 4 of the present invention;

[0028] Figure 5 It is a structural schematic diagram of step five of the present invention;

[0029] Figure 6 It is a structural schematic diagram of step six of the present invention;

[0030] Figure 7 It is a structural schematic diagram of step seven of the present invention. DETAILED DESCRIPTION

[0031] The present invention is described in detail below so that the advantages and features of the present invention can be more easily understood by those skilled in the art, thereby making a clearer and more definite definition of the protection scope of the present invention.

[0032] A brief summary of one or more aspects is given below to provide a basic understanding of these aspects. This summary is not an exhaustive overview of all conceived aspects, and is neither intended to identify the key or critical elements of all aspects nor to define the scope of any or all aspects. Its only purpose is to give some concepts of one or more aspects in a simplified form as a prelude to a more detailed description that will be given later.

[0033] like Figure 1-7 As shown, the present invention discloses a packaging method for improving the chemical resistance of a release layer, comprising the following steps:

[0034] Step 1: If Figure 1 As shown, the release layer 200 is prepared by spin coating a temporary bonding adhesive on the temporary carrier 100. According to the requirements of the debonding process, the thickness of the release layer 200 is different, and is generally required to be ≥0.3μm;

[0035] Step 2: If Figure 2 As shown, the release layer 200 at the edge of the temporary carrier 100 is removed through the edge cleaning process; a release layer blank area 300 is left at the edge of the temporary carrier 100, and the release layer blank area 300 is within the invalid area of ​​the wafer; through the control of the edge cleaning process, there is no release layer residue in the release layer blank area 300, the width is less than the invalid area of ​​the wafer, and the accuracy is controlled within 10% of the edge cleaning width; the edge cleaning equipment includes an edge cleaning machine, a single-wafer cleaning machine, a developing machine, a wet etching machine, a spin coater, etc.;

[0036] Step 3: If Figure 3 As shown, after the edge washing process is completed, a passivation layer 400 is spin-coated on the release layer 200, and the material is epoxy resin, acrylate, polyimide, polyisobutylene, phenolic resin, etc.; the passivation layer 400 covers the release layer 200 and the blank area 300 of the release layer, and the release layer 200 is completely isolated from the air. If there are abnormal phenomena such as bubbles and gaps in the passivation layer 400 in the blank area 300 of the release layer, these abnormalities can be eliminated through coating or vacuum baking and other process methods. If the blank area 300 of the release layer is not completely covered by the passivation layer 400, it can be solved by coating, changing the glue dripping method such as mosquito coil shape, etc., and then adjusting the film forming rotation speed of the passivation layer 400 so that the blank area 300 of the release layer is completely covered by the passivation layer 400; according to the requirements of wafer warping and rewiring, the thickness of the release layer 200 is less than the thickness of the rewiring layer, and the total thickness change TTV is less than 5% of the thickness of the release layer;

[0037] Step 4: If Figure 4 As shown, a redistribution layer is constructed on the passivation layer 400, and the redistribution layer includes a redistribution RDL 500, a dielectric layer 600 and a metal layer UBM 700, wherein the redistribution RDL 500 is wrapped in the dielectric layer 600, and the metal layer UBM 700 is electrically connected to the redistribution RDL 500;

[0038] Step 5: If Figure 5As shown, after the redistribution layer is constructed, the integrated circuit grain I 901, the integrated circuit grain II 902a, and the integrated circuit grain III 902b are respectively placed on the redistribution layer through the connection structure 800, and the integrated circuit grain I 901, the integrated circuit grain II 902a, and the integrated circuit grain III 902b are respectively connected to the redistribution layer through the connection structure 800, and the gap of the connection structure 800 is completely filled with the bottom filling material 1000 (polymer, epoxy resin and or other types of insulating materials), and then the entire integrated circuit grain is wrapped with the packaging glue material 1100 (polymer, epoxy resin and or other types of insulating materials) to form a reconstructed wafer. If there are bubbles or voids in the bottom filling material area, the abnormal phenomenon can be eliminated by filling process, vacuum pressure curing, pre-activation, etc.; it should be noted that the integrated circuit grain I 901 is a logic chip / analog chip / RF chip / MEMS, etc., the integrated circuit grain II 902a and the integrated circuit grain III 902b are HBM, and the number and type of integrated circuit grains can be flexibly selected according to actual needs; the connection structure 800 can adopt bumps, solder balls, micro bumps, UBM structures, etc., and can include one or more materials, such as gold (Au), copper (Cu), silver (Ag), nickel (Ni), tin (Sn), lead (Pb) materials, etc.; when the integrated circuit grain is placed on the redistribution layer, the connection structure 800 is prone to abnormal phenomena such as bridging. By improving the FC (Flip chip) process, reducing the offset, or increasing the connection strength after FC, it is avoided that the connection structure 800 is seriously offset before reflow;

[0039] Step 6: If Figure 6 As shown, after the reconstructed wafer is formed, the wafer is subjected to a ring cutting process to remove the package body at the edge of the temporary carrier 100, leaving a blank area 1200 at the edge of the temporary carrier; if burrs appear at the edge of the ring cutting area or the ring cutting is not clean, the abnormal phenomenon can be removed by means of laser or a cutter wheel; according to the requirements of the debonding process, the ring cutting width is ≥ the edge washing width of the release layer, and the thickness of the blank area at the edge of the temporary carrier is ≤ the thickness of the temporary carrier without ring cutting; the ring cutting equipment is a plasma cutting machine, a laser cutting machine, a cutter wheel cutting machine, a water jet cutting machine, a flame cutting machine, a blade cutting machine and other related cutting machines; after the ring cutting, if the debonding cannot be peeled off smoothly and there is adhesion, the side wall adhesion caused by the molding offset can be solved by increasing the ring cutting width;

[0040] Step 7: If Figure 7 As shown, after the reconstructed wafer is ring-cut, a debonding process is performed to separate the release layer 200 from the temporary carrier 100. If the temporary carrier 100 is difficult to peel off or damaged, such abnormal phenomena can be eliminated through a debonding process or a ring-cutting process. The debonding process includes laser, mechanical, chemical, thermal sliding debonding, etc., which is determined by the type of release layer material.

[0041] The present invention also discloses a packaging structure for improving the chemical resistance of a release layer, which is prepared by using a packaging method for improving the chemical resistance of a release layer as described above. The packaging structure includes a release layer 200, a passivation layer 400, a redistribution layer, and integrated circuit grains, wherein the release layer 200 is arranged below the passivation layer 400, and the redistribution layer is arranged above the passivation layer 400. The integrated circuit grains include three types: integrated circuit grain I 901, integrated circuit grain II 902a, and integrated circuit grain III 902b. The integrated circuit grain I 901, the integrated circuit grain II 902a, and the integrated circuit grain III 902b are respectively arranged on the redistribution layer through a connecting structure 800, and the gap of the connecting structure 800 is completely filled with a bottom filling material 1000, and the integrated circuit grains are completely covered with a packaging glue material 1100.

[0042] Example 1

[0043] like Figure 1-7 As shown, a packaging method for improving the chemical resistance of a release layer comprises the following steps:

[0044] Step 1: If Figure 1 As shown, the release layer 200 is prepared by spin coating a temporary bonding adhesive on the temporary carrier 100. According to the requirements of the debonding process, the thickness of the release layer 200 is different, and is generally required to be ≥0.3μm;

[0045] Step 2: If Figure 2 As shown, the release layer 200 at the edge of the temporary carrier 100 is removed by the edge washing process; a release layer blank area 300 is left at the edge of the temporary carrier 100, and the release layer blank area 300 is within the invalid area of ​​the wafer; through the control of the edge washing process, there is no release layer residue in the release layer blank area 300, the width is less than the invalid area of ​​the wafer, and the accuracy is controlled within 10% of the edge washing width; the edge washing equipment is an edge washing machine;

[0046] Step 3: If Figure 3 As shown, after the edge washing process is completed, a passivation layer 400 made of epoxy resin is spin-coated on the release layer 200; the passivation layer 400 covers the release layer 200 and the blank area 300 of the release layer, and the release layer 200 is completely isolated from the air. If there are abnormal phenomena such as bubbles and gaps in the passivation layer 400 in the blank area 300 of the release layer, these abnormalities can be eliminated through coating or vacuum baking and other process methods. If the blank area 300 of the release layer is not completely covered by the passivation layer 400, it can be solved by coating, changing the glue dripping method such as mosquito coil shape, and then adjusting the film forming rotation speed of the passivation layer 400 so that the blank area 300 of the release layer is completely covered by the passivation layer 400; according to the requirements of wafer warping and rewiring, the thickness of the release layer 200 is less than the thickness of the rewiring layer, and the total thickness change TTV is less than 5% of the thickness of the release layer;

[0047] Step 4: If Figure 4 As shown, a redistribution layer is constructed on the passivation layer 400, and the redistribution layer includes a redistribution RDL 500, a dielectric layer 600 and a metal layer UBM 700, wherein the redistribution RDL 500 is wrapped in the dielectric layer 600, and the metal layer UBM 700 is electrically connected to the redistribution RDL 500;

[0048] Step 5: If Figure 5 As shown, after the redistribution layer is constructed, the integrated circuit grain I 901, the integrated circuit grain II 902a, and the integrated circuit grain III 902b are respectively placed on the redistribution layer through the connection structure 800, and the integrated circuit grain I 901, the integrated circuit grain II 902a, and the integrated circuit grain III 902b are respectively connected to the redistribution layer through the connection structure 800, and the gap of the connection structure 800 is completely filled with the bottom filling material 1000 (epoxy resin), and then the entire integrated circuit grain is wrapped with the packaging glue material 1100 (epoxy resin) to form a reconstructed wafer. If there are bubbles or gaps in the bottom filling material area, the abnormal phenomenon can be eliminated by filling process, vacuum pressure curing, pre-activation and other methods; it should be noted that the integrated circuit grain I 901 is a logic chip, the integrated circuit grain II 902a and the integrated circuit grain III 902b are HBM, and the number and type of integrated circuit grains can be flexibly selected according to actual needs; the connection structure 800 can use gold bumps; when the integrated circuit grain is placed on the redistribution layer, the connection structure 800 is prone to abnormal phenomena such as bridging. By improving the FC (Flipchip) process, reducing the offset, or increasing the connection strength after FC, it is avoided that the connection structure 800 is seriously offset before reflow;

[0049] Step 6: If Figure 6 As shown, after the reconstructed wafer is formed, the wafer is subjected to a ring cutting process to remove the package body at the edge of the temporary carrier 100, leaving a blank area 1200 at the edge of the temporary carrier; if burrs appear at the edge of the ring cutting area or the ring cutting is not clean, the abnormal phenomenon can be removed by means of laser or a cutter wheel; according to the requirements of the debonding process, the ring cutting width is ≥ the edge washing width of the release layer, and the thickness of the blank area at the edge of the temporary carrier is ≤ the thickness of the temporary carrier without ring cutting; the ring cutting equipment is a plasma cutting machine. After the ring cutting, if the debonding cannot be peeled off smoothly and there is adhesion, the side wall adhesion caused by the molding offset can be solved by increasing the ring cutting width;

[0050] Step 7: If Figure 7As shown, after the reconstructed wafer is ring-cut, a debonding process is performed to separate the release layer 200 from the temporary carrier 100. If the temporary carrier 100 is difficult to peel off or damaged, the debonding process or ring-cut process can be used to eliminate such abnormal phenomena. The debonding process is a laser method, which is determined by the type of release layer material.

[0051] A packaging structure for improving the chemical resistance of a release layer is prepared by using a packaging method for improving the chemical resistance of a release layer as described above. The packaging structure includes a release layer 200, a passivation layer 400, a redistribution layer, and integrated circuit grains, wherein the release layer 200 is arranged below the passivation layer 400, and the redistribution layer is arranged above the passivation layer 400. The integrated circuit grains include three types: integrated circuit grain I 901, integrated circuit grain II 902a, and integrated circuit grain III 902b. The integrated circuit grain I 901, the integrated circuit grain II 902a, and the integrated circuit grain III 902b are respectively arranged on the redistribution layer through a connection structure 800, and the gap of the connection structure 800 is completely filled with a bottom filling material 1000, and the integrated circuit grains are completely covered with a packaging glue material 1100.

[0052] Parts or structures not specifically described in the present invention may adopt existing technologies or existing products and will not be described in detail here.

[0053] The above descriptions are merely embodiments of the present invention and are not intended to limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made using the contents of the present invention specification, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.

Claims

1. A packaging method for improving the chemical resistance of a release layer, characterized in that: The following steps are involved: Step 1: preparing a release layer on a temporary carrier; Step 2: removing the release layer at the edge of the temporary carrier, leaving a release layer blank area at the edge of the temporary carrier, wherein no release layer remains in the release layer blank area, and the release layer blank area is within the invalid area of ​​the wafer; Step 3: preparing a passivation layer on the release layer, wherein the passivation layer covers the release layer and the blank area of ​​the release layer, and the release layer is completely isolated from the air; Step 4: construct a redistribution layer on the passivation layer; Step 5: placing the integrated circuit die on the redistribution layer and performing plastic sealing to form a reconstructed wafer; Step 6: Circular cut the reconstructed wafer, remove the package at the edge of the temporary carrier, and leave a blank area at the edge of the temporary carrier; Step 7: Peel off the temporary carrier.

2. The packaging method for improving the chemical resistance of a release layer according to claim 1, characterized in that: In step 1, the thickness of the release layer is not less than 0.3 μm.

3. The packaging method for improving the chemical resistance of a release layer according to claim 1, characterized in that: In step 2, the release layer at the edge of the temporary carrier is removed by an edge washing process.

4. The packaging method for improving the chemical resistance of a release layer according to claim 1, characterized in that: In step 2, the width of the blank area of ​​the release layer is smaller than the invalid area of ​​the wafer, and the accuracy is controlled within 10% of the edge washing width.

5. The packaging method for improving the chemical resistance of a release layer according to claim 1, characterized in that: In step 4, the thickness of the release layer is less than the thickness of the redistribution layer, and the TTV is less than 5% of the thickness of the release layer.

6. The packaging method for improving the chemical resistance of a release layer according to claim 1, characterized in that: In step five, the integrated circuit grains include integrated circuit grain I, integrated circuit grain II, and integrated circuit grain III. The integrated circuit grain I, integrated circuit grain II, and integrated circuit grain III are respectively placed on the redistribution layer through a connecting structure, and the gaps in the connecting structure are completely filled with bottom filling materials. The entire integrated circuit grain is covered with a packaging glue material to form a reconstructed wafer.

7. The packaging method for improving the chemical resistance of a release layer according to claim 1, characterized in that: In step six, the circular cutting width is not less than the edge washing width of the release layer.

8. The packaging method for improving the chemical resistance of a release layer according to claim 1, characterized in that: In step seven, a debonding process is performed to separate the release layer and the temporary carrier. The debonding process includes thermal decomposition, laser irradiation, and chemical dissolution, which is determined by the material type of the release layer. 9 . A packaging structure prepared by a packaging method for improving the chemical resistance of a release layer according to any one of claims 1 to 8 .

10. The packaging structure for improving the chemical resistance of the release layer according to claim 9, characterized in that: It includes a release layer, a passivation layer, a redistribution layer and an integrated circuit grain, wherein the release layer is arranged below the passivation layer, the redistribution layer is arranged above the passivation layer, the integrated circuit grain is placed on the redistribution layer through a connection structure, the gaps in the connection structure are filled with a bottom filling material, and the integrated circuit grain is wrapped in a packaging glue material.

Citation Information

Patent Citations

  • Chip packaging structure and chip packaging method

    CN117457618A

  • Carrier and method for manufacturing semiconductor device

    JP2021044447A

  • Method of manufacturing semiconductor package

    TW201503267A