Energy storage cell and preparation method thereof
By dispensing and specific arrangement on the film layer of the lithium-ion battery energy storage battery cell, and combining the winding process to form an adhesive layer, the problems of bending and diaphragm folding during the winding process are solved, and the problem of the battery cell is improved. The adhesion and yield of the battery cell reduce the preparation cost.
Patent Information
- Application Number
- CN202411396823.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-08
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2044-10-08
AI Technical Summary
Existing lithium-ion battery energy storage batteries are prone to bending, wrinkling and diaphragm folding problems during winding, resulting in safety risks and high preparation costs.
By dispensing the film layer, multiple groups of glue dots arranged in a specific direction are formed, and the density is reduced along the edges is reduced, and the glue dots are molten in the winding process to form a adhesive layer to fix the positive electrode sheet , diaphragm and negative electrode sheet to reduce glue usage and reduce cost.
It effectively avoids interface problems caused by diaphragm folds, improves the adhesion and yield of the battery cell, reduces the preparation cost, and enhances the mechanical performance and safety of the battery cell.
Smart Images

Figure CN118919876A_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present application relate to the field of energy storage, and in particular to an energy storage battery cell and a method for preparing the same. Background Art
[0002] In recent years, lithium-ion batteries have attracted great attention due to their excellent characteristics such as high energy density, high output voltage, low self-discharge rate, long service life, no memory effect and environmental friendliness. They have developed by leaps and bounds, their market share has continued to expand, and they have occupied a dominant position.
[0003] The development focus of the preparation process of lithium-ion batteries is on the cycle stability, preparation cost and yield of the battery cells. At present, there are mainly two ways to improve the energy density of the battery cells, one is the stacking type and the other is the winding type. Among them, the winding method is the most common way to improve the energy density. In the cross-section of the wound battery cell, the wound battery cell contains two parts, one is the flat extension area, and the other is the curved bending area. The core is made of multiple layers of thin film materials. Tension will be generated during winding. If the tension is not large enough, it will cause problems such as bending, wrinkling and even fracture. These defects increase the safety risk of the battery, especially in the bending area corresponding to the curvature, where the diaphragm is more prone to wrinkling. One of the current improvement measures is to release the stress of the diaphragm before preparing the lithium battery. This method is costly and will pollute the environment. The second current improvement measure is to change the structure of the crystalline and amorphous regions of the diaphragm to enhance the diaphragm's anti-wrinkle ability, but this may introduce other side effects, such as causing excessive self-discharge of the lithium battery, or the high modulus diaphragm may cause the lithium battery cell to be more susceptible to "S" shape deformation during recycling.
[0004] Therefore, there is an urgent need for a method for preparing an energy storage cell that can fix the separator, the positive electrode sheet, and the negative electrode sheet to each other, so as to improve the yield of the energy storage cell and reduce the preparation cost. Summary of the invention
[0005] The embodiments of the present application provide an energy storage battery cell and a method for preparing the same, which are at least beneficial to improving the yield of the energy storage battery cell and reducing the preparation cost.
[0006] According to some embodiments of the present application, on the one hand, an embodiment of the present application provides a method for preparing an energy storage battery cell, comprising: providing a film layer, wherein the film layer is one of a positive electrode sheet, a separator or a negative electrode sheet, and the film layer has a first edge and a second edge arranged opposite to each other along a first direction; performing a glue dispensing treatment on the film layer so that the surface of the film layer has a plurality of glue dot groups arranged along the first direction; the distribution density of the glue dot groups decreases along the direction from the second edge to the first edge; forming the positive electrode sheet, the separator or the other two of the negative electrode sheet; performing a winding treatment on the positive electrode sheet, the negative electrode sheet and the separator, and performing the winding treatment from the second edge toward the first edge; wherein the separator is located between the positive electrode sheet and the negative electrode sheet, and the winding treatment is at least used to make the glue points of the glue dot group present a molten state and form an adhesive layer to fix the positive electrode sheet to the separator and / or to fix the separator to the negative electrode sheet.
[0007] In some embodiments, the film layer also has two third edges arranged opposite to each other along the second direction, and both ends of each of the third edges are respectively connected to the first edge and the second edge; during the process of performing glue dispensing treatment on the film layer, from the center of the film layer in the second direction toward the third edge, in the same glue point group, the distribution density within the glue point group increases.
[0008] In some embodiments, along the second direction and pointing to the third edge, the spacing between adjacent glue dots in the same glue dot group decreases; and / or, along the second direction and pointing to the third edge, the size of the glue dots in the same glue dot group increases.
[0009] In some embodiments, the glue dot group includes: a first glue dot group near the first edge and a second glue dot group near the second edge, the size of the first glue dot in the first glue dot group is smaller than the size of the second glue dot in the second glue dot group; and / or, the first spacing between adjacent first glue dots in the first glue dot group is larger than the second spacing between adjacent second glue dots in the second glue dot group.
[0010] In some embodiments, the ratio of the first spacing to the second spacing is 1.03-1.3.
[0011] In some embodiments, the ratio of the total area of the orthographic projections of the plurality of glue dot groups on the film layer to the surface area of the film layer is 10% to 14%.
[0012] In some embodiments, the process steps of the winding treatment include: hot winding treatment and cold pressing treatment, the hot winding treatment is used to make the glue points of the glue point group molten and form an adhesive layer to fix the positive electrode sheet to the diaphragm and / or to fix the diaphragm to the negative electrode sheet; the cold pressing treatment is used to bond the positive electrode sheet, the negative electrode sheet and the diaphragm together.
[0013] In some embodiments, before the positive electrode sheet, the negative electrode sheet and the separator are wound, the film layer is heated, and the heating treatment is at least used to melt the glue points of the glue point group and pre-fix the positive electrode sheet and the separator and / or pre-fix the negative electrode sheet and the separator.
[0014] In some embodiments, while the positive electrode sheet, the negative electrode sheet and the separator are being wound, the process also includes: heating the film layer, wherein the heating process is at least used to melt the glue points of the glue point group and form an adhesive layer.
[0015] According to some embodiments of the present application, on the other hand, the embodiments of the present application further provide an energy storage battery cell, including: a positive electrode sheet, a negative electrode sheet and a separator, the separator is located between the positive electrode sheet and the negative electrode sheet; an adhesive layer is provided between the positive electrode sheet and the separator or between the negative electrode sheet and the separator, the positive electrode sheet and the separator are fixed to each other through the adhesive layer and / or the negative electrode sheet and the separator are fixed to each other through the adhesive layer; an adhesive group, the adhesive group includes a plurality of the adhesive layers; along the winding direction from the inner circle to the outer circle, the distribution density of the adhesive group decreases.
[0016] The technical solution provided by the embodiment of the present application has at least the following advantages: In the technical solution provided in the embodiment of the present application, glue is dispensed on one of the positive electrode sheet, the diaphragm or the negative electrode sheet, and the glue point group is arranged in a specific manner to alleviate or offset the stress problem caused by the bending area of the core, thereby avoiding the problem of wrinkles at the interface between the positive electrode sheet and the diaphragm and the interface between the diaphragm and the negative electrode sheet caused by the wrinkles of the diaphragm, so as to improve the interface effect. Based on this uneven arrangement, the distribution density of the glue point group decreases as it approaches the first edge, that is, the distribution density is smaller at the position closer to the outer circle of the core, which can ensure that the adhesion of the glue points between the inner circle diaphragm and the positive electrode sheet and between the diaphragm and the negative electrode sheet is greater, and then used to resist the stress caused by the bending arc, so that the positive electrode sheet and the diaphragm, the diaphragm and the negative electrode sheet are more closely attached, and the problem of easy wrinkles in the inner circle of the core at the full interface is improved, and the amount of glue used can be reduced, reducing the preparation cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] One or more embodiments are exemplarily illustrated by the figures in the corresponding drawings. These exemplified descriptions do not constitute a limitation on the embodiments. Unless otherwise specified, the figures in the drawings do not constitute a scale limitation. In order to more clearly illustrate the embodiments of the present application or the technical solutions in the traditional technology, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0018] Figure 1 A flow chart of a method for preparing an energy storage cell provided in one embodiment of the present application; Figure 2 A preparation flow chart of a method for preparing an energy storage cell provided in one embodiment of the present application, wherein the film layer is a positive electrode sheet or a negative electrode sheet; Figure 3 A preparation flow chart of a membrane layer as a diaphragm in a method for preparing an energy storage battery cell provided in one embodiment of the present application; Figure 4 A top view of a film layer corresponding to the step of providing a film layer in the method for preparing an energy storage battery cell provided in one embodiment of the present application; Figure 5 A first top view of a film layer corresponding to a step of performing glue dispensing in a method for preparing an energy storage battery cell provided in an embodiment of the present application; Figure 6 A second top view of a film layer corresponding to the step of performing glue dispensing in the method for preparing an energy storage battery cell provided in one embodiment of the present application; Figure 7 A third top view of a film layer corresponding to the step of performing glue dispensing in the method for preparing an energy storage battery cell provided in one embodiment of the present application; Figure 8 A cross-sectional view of an energy storage cell corresponding to a winding step in a method for preparing an energy storage cell provided in an embodiment of the present application. DETAILED DESCRIPTION
[0019] As can be seen from the background technology, the yield of current energy storage cells is poor and the preparation cost is high.
[0020] Analysis found that one of the reasons why the current energy storage cells have a poor yield and high preparation cost is that the main function of conventional diaphragms is to separate the cathode (negative electrode represented by the negative electrode sheet) and anode (positive electrode represented by the positive electrode sheet) materials of the battery to prevent the two electrodes of different polarities from contacting and short-circuiting. In addition, during the electrochemical reaction, it can maintain the necessary electrolyte and form a channel for the movement of ions.
[0021] In order to achieve the fixation between the diaphragm and the positive electrode sheet, and between the diaphragm and the negative electrode sheet, a glue coating layer is generally provided on the base film where the diaphragm is located to form a glue-coated diaphragm. The glue coating layer is sticky and adheres to the surface of the electrode sheet (positive electrode sheet or negative electrode sheet) after hot pressing, increasing the shrinkage resistance and flatness, making the electrode sheet and the diaphragm fit closely, shortening the lithium ion transmission path, and reducing the interface impedance between the electrode sheets. After hot pressing, the glue coating layer of the glue-coated diaphragm solidifies after cooling, which improves the mechanical properties of the winding core composed of the positive electrode sheet, diaphragm and negative electrode sheet, and facilitates assembly.
[0022] However, the use of glue-coated diaphragms also brings other problems. The diaphragm is completely attached to the surface of the electrode. On the one hand, the surface of the glue-coated diaphragm is completely attached to the surface of the electrode, which increases the amount of glue layer and increases the cost of the diaphragm. On the other hand, due to the different curvatures of the bending areas of the inner and outer rings of the winding core, the stress of the inner ring is greater, resulting in a greater possibility of delamination, which makes the diaphragm of the inner ring prone to wrinkles.
[0023] The present application provides a method for preparing an energy storage battery cell, forming multiple glue point groups and non-uniformly distributed glue points on a film layer, thereby reducing the preparation cost of glue and improving the problem of easy wrinkling of the inner circle.
[0024] In the description of the embodiments of the present application, the technical terms "first", "second", etc. are only used to distinguish different objects, and cannot be understood as indicating or implying relative importance or implicitly indicating the number, specific order or primary and secondary relationship of the indicated technical features. In the description of the embodiments of the present application, the meaning of "multiple" is more than two, unless otherwise clearly and specifically defined.
[0025] Reference to "embodiments" herein means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present application. The appearance of the phrase in various locations in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described herein may be combined with other embodiments.
[0026] In the description of the embodiments of the present application, the term "and / or" is only a description of the association relationship of associated objects, indicating that three relationships may exist. For example, A and / or B can represent: A exists, A and B exist at the same time, and B exists. In addition, the character " / " in this article generally indicates that the associated objects before and after are in an "or" relationship.
[0027] In the description of the embodiments of the present application, the term "multiple" refers to more than two (including two). Similarly, "multiple groups" refers to more than two groups (including two groups), and "multiple pieces" refers to more than two pieces (including two pieces).
[0028] In the description of the embodiments of the present application, the technical terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential", etc. indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, which are only for the convenience of describing the embodiments of the present application and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the embodiments of the present application.
[0029] In the description of the embodiments of the present application, unless otherwise clearly specified and limited, technical terms such as "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, and it can be the internal connection of two elements or the interaction relationship between two elements. For those of ordinary skill in the art, the specific meanings of the above terms in the embodiments of the present application can be understood according to the specific circumstances.
[0030] In the accompanying drawings corresponding to the embodiments of the present application, the thickness and area of the layer are magnified for better understanding and ease of description. When describing a component (such as a layer, film, region or substrate) on another component or on the surface of another component, the component may be "directly" located on the surface of the other component, or a third component may be present between the two components. On the contrary, when describing a component on the surface of another component or when another component is formed or provided on the surface of a component, it means that there is no third component between the two components. In addition, when describing a component as "substantially" formed on another component, it means that the component is not formed on the entire surface (or front surface) of the other component, nor is it formed on a partial edge of the entire surface.
[0031] In the description of the embodiments of the present application, when a component "includes" another component, unless otherwise specified, other components are not excluded, and other components may be further included. In addition, when a component such as a layer, film, region, or plate is referred to as "on / located on" another component, it can be "directly on" the other component (i.e., located on the surface of the other component with no other components between them), or another component may exist in between. In addition, when a component such as a layer, film, region, or plate is "directly located on" another component, or when a component such as a layer, film, region, or plate is located on the surface of another component, it means that no other components are located in between.
[0032] The terms used in the description of the various embodiments described herein are only used to describe specific embodiments and are not intended to be limiting. As used in the description of the various embodiments described and in the appended claims, "the part" is also intended to include plural forms unless the context clearly indicates otherwise. Among them, components include layers, films, regions, or panels. Thereby improving the yield of the battery cell.
[0033] Figure 1 A flow chart of a method for preparing an energy storage cell provided in one embodiment of the present application.
[0034] According to some embodiments of the present application, the present application provides a method for preparing an energy storage battery cell. Figure 1 The preparation method includes: providing a film layer, the film layer is one of a positive electrode sheet, a separator or a negative electrode sheet; performing a dispensing process on the film layer to form the other two of the positive electrode sheet, the separator or the negative electrode sheet; and performing a winding process on the positive electrode sheet, the negative electrode sheet and the separator.
[0035] The film layer has a first edge and a second edge arranged relatively along a first direction; the film layer is subjected to a glue dot treatment so that the surface of the film layer has a plurality of glue dot groups arranged along the first direction; the distribution density of the glue dot groups decreases along the direction from the second edge to the first edge; during the winding process, the winding process is performed from the second edge toward the first edge; the diaphragm is located between the positive electrode sheet and the negative electrode sheet, and the winding process is at least used to make the glue dots of the glue dot group molten and form an adhesive layer so as to fix the positive electrode sheet to the diaphragm and / or the diaphragm to the negative electrode sheet.
[0036] The preparation method of the energy storage battery provided by the present application performs glue dispensing on one of the positive electrode sheet, the diaphragm or the negative electrode sheet, and arranges the glue point group in a specific manner to alleviate or offset the stress problem caused by the bending area of the core, thereby avoiding the problem of wrinkles at the interface between the positive electrode sheet and the diaphragm and the interface between the diaphragm and the negative electrode sheet caused by the subsequent wrinkles of the diaphragm, so as to improve the interface effect. Based on this uneven arrangement method, that is, the distribution density of the glue point group is smaller as it approaches the first edge, that is, the distribution density is smaller at the position closer to the outer circle of the core, which can ensure that the adhesion of the glue points between the inner circle diaphragm and the positive electrode sheet and between the diaphragm and the negative electrode sheet is greater, and then used to resist the stress caused by the bending curvature, so that the positive electrode sheet and the diaphragm, the diaphragm and the negative electrode sheet are more closely attached, and the problem of easy wrinkles in the inner circle of the core at the full charge interface is improved, and the amount of glue used can be reduced, reducing the preparation cost.
[0037] According to the appearance classification, the prepared energy storage cells can be divided into square cells, round cells or soft-pack cells. According to the capacity classification, the energy storage cells can be divided into 50Ah, 100Ah, 150Ah, 200Ah, 280Ah, 306Ah, 314Ah, 500+Ah, 800+Ah and 1000+Ah and other models. According to the chemical composition and working principle of the cell, the energy storage cell can be a lithium-ion battery, a lead-acid battery, a sodium-ion battery or a nickel-metal hydride battery. The embodiment of the present application takes the preparation method of a lithium-ion battery as an example. Those skilled in the art can replace the lithium ions in the positive electrode sheet, the negative electrode sheet and the electrolyte with corresponding metal ions according to actual needs. For example, in sodium ion batteries, the lithium transition metal oxide of the subsequent positive electrode active material is replaced by any of the corresponding layered metal oxides (such as NaFeO2), polyanion compounds (NaFePO4) and Prussian blue compound systems (such as NaMnFe(CN)6-zH2O), and the electrolyte is replaced by any of the organic liquid electrolyte, solid composite electrolyte or solid electrolyte.
[0038] The following will describe the various embodiments of the present application in detail with reference to the accompanying drawings. However, it will be appreciated by those skilled in the art that in the various embodiments of the present application, many technical details are provided in order to enable the reader to better understand the present application. However, even without these technical details and various changes and modifications based on the following embodiments, the technical solution claimed in the present application can be implemented.
[0039] In some embodiments, the positive electrode sheet and the negative electrode sheet serve as the positive electrode and negative electrode of the energy storage cell, respectively. The positive electrode is the electrode plate where oxidation reaction occurs in the energy storage cell, and the negative electrode is the electrode plate where reduction reaction occurs in the energy storage cell. The positive electrode and the negative electrode are separated and connected together by an electrolyte, and the positive electrode and the negative electrode serve as the electrochemical reaction areas of the energy storage cell.
[0040] The positive electrode sheet includes a positive electrode current collector and a positive electrode active material layer, and the positive electrode active material layer is located on the positive electrode current collector. A portion of the positive electrode current collector is cut into the shape of a tab and serves as a positive electrode tab.
[0041] The positive electrode current collector can be aluminum foil, which is cheaper than copper foil. A dense oxide film is formed on the surface of the aluminum foil, and the oxide film is very thin, which can improve the corrosion resistance of the aluminum foil, and electrons can achieve conductivity through the tunnel effect.
[0042] In some embodiments, the positive electrode current collector may also be a composite current collector, which includes three stacked layers, the middle layer is an organic material, and the upper and lower layers are copper-plated layers and aluminum-plated layers. The organic material is PET (polyethylene terephthalate), PP (polypropylene), PI (polyimide), etc.
[0043] In some embodiments, the positive electrode current collector may also be a carbon-based current collector, that is, a conductive carbon layer is provided on the aluminum foil, and the conductive carbon layer may serve as a protective layer to effectively protect the current collector to prevent corrosion of the metal current collector, thereby increasing the life of the current collector; secondly, the conductive carbon layer itself has a low resistivity, so as not to generate excessive electrical losses.
[0044] It should be noted that the carbon-based current collector may be in the form of both the upper and lower surfaces of the aluminum foil being coated with a conductive carbon layer, or may be in the form of a portion of the surface of the aluminum foil being covered with a conductive carbon layer.
[0045] The positive electrode tab is a metal conductor that leads the positive electrode of the energy storage cell out of the battery cell. The positive electrode tab is the contact point between the positive electrode sheet and the external contact component when the battery cell is charged and discharged. The external contact component can be a pole.
[0046] The negative electrode sheet includes a negative electrode current collector and a negative electrode active material layer, and the negative electrode active material layer is located on the negative electrode current collector, and a portion of the negative electrode current collector is cut into a shape of a tab and serves as a negative electrode tab.
[0047] In some embodiments, the negative electrode current collector may be copper foil, which has low electrical conductivity and can have high electron transmission capacity, and copper foil has weak lithium insertion capacity and captures fewer lithium ions, thereby effectively reducing the loss of lithium ions. In other embodiments, the negative electrode current collector may also be a foam copper current collector, a copper mesh current collector, and a three-dimensional nano copper array current collector.
[0048] In some embodiments, the negative electrode active material layer may be composed of a negative electrode active material, a conductive agent, and a binder. The negative electrode active material may be carbon material and non-carbon material: carbon-based materials include graphite materials (natural graphite, artificial graphite, and mesophase carbon spheres) and other carbon-based materials (hard carbon, soft carbon, and graphene); non-carbon-based materials may be subdivided into titanium-based materials, silicon-based materials, tin-based materials, nitrides, and metallic lithium, etc.
[0049] The conductive agent is similar to that of the positive electrode active material layer, and the adhesive for the negative electrode is similar to that for the positive electrode, mainly including oil-based PVDF (polyvinylidene fluoride), water-based CMC (carboxymethyl cellulose), PVA (polyvinyl alcohol), sodium alginate, etc., which will not be repeated here.
[0050] The negative electrode tab is a metal conductor that leads the negative electrode of the energy storage cell out of the battery cell. The negative electrode tab is the contact point between the negative electrode sheet and the external contact component when the battery cell is charged and discharged. The external contact component can be a pole.
[0051] The separator is used to prevent short circuit problems caused by physical contact between the positive electrode and the negative electrode, while allowing ions to conduct through the electrolyte and hindering the transmission of electrons, so that ions and electrons form a circuit during the charging and discharging process of the battery.
[0052] The diaphragm can be any one of a microporous membrane, a modified microporous membrane, a non-woven membrane and a composite membrane. A microporous membrane is a membrane with a pore size in the micrometer range, mainly including polyolefin microporous membranes and other polymer microporous membranes. A modified microporous membrane is a diaphragm obtained by modifying a microporous membrane. Common modification methods include surface treatment, chemical grafting, surface coating, etc. Non-woven membranes have a small fiber diameter and generally exhibit a higher porosity than other types of membranes. Composite membranes are prepared by coating or filling inorganic materials in microporous membranes or non-woven membranes, and have higher thermal stability and electrolyte wettability than other types of membranes.
[0053] Figure 2 A preparation flow chart of a method for preparing an energy storage cell provided in one embodiment of the present application, wherein the film layer is a positive electrode sheet or a negative electrode sheet; Figure 3 A preparation flow chart of a membrane layer as a diaphragm in a method for preparing an energy storage cell provided in one embodiment of the present application.
[0054] refer to Figure 2 , the film layer is a positive electrode sheet or a negative electrode sheet, and before the glue dispensing process is performed, it also includes: die-cutting the positive electrode sheet or the negative electrode sheet to form a pole ear adjacent to the first edge. In this way, the glue dispensing process on the positive electrode sheet / negative electrode sheet can avoid the situation where large areas of wrinkles appear around the glue-coated area due to the soft texture of the diaphragm, and even the problem of "dead wrinkles" formed during the subsequent cold pressing process. In other words, the glue dispensing process on the positive electrode sheet / negative electrode sheet can effectively avoid the wrinkle problem caused by the glue dispensing process of the diaphragm, thereby avoiding the subsequent wrinkle problem at the interface between the positive electrode sheet and the diaphragm and the interface between the diaphragm and the negative electrode sheet caused by the wrinkles of the diaphragm, so as to improve the interface effect. The pole ear can be the positive pole ear of the positive electrode sheet or the negative pole ear of the negative electrode sheet.
[0055] In some embodiments, after the conventional positive electrode sheet and the negative electrode sheet are coated with the active material layer, they are cut into corresponding positive electrode sheets / negative electrode sheets, and then the formed positive electrode sheet and the negative electrode sheet are subjected to a die-cutting process based on certain die-cutting parameters. The die-cutting process includes the steps of die-cutting loading, unwinding and conveying, tab die-cutting, and winding and unloading. The preparation method provided in the embodiment disclosed in the present application performs a dispensing process after the tab die-cutting, that is, the first edge and the second edge are distinguished based on the position of the tab, and then the inner circle and the outer circle are distinguished during the subsequent winding process, which is more convenient and quick compared with other distinguishing processes and distinguishing methods. In addition, improvements based on the original process will not have a significant impact on the original equipment and steps, thereby reducing the preparation cost.
[0056] refer to Figure 3The film layer is a diaphragm, and the process steps of performing glue dispensing treatment, forming positive electrode sheets and negative electrode sheets and performing winding treatment include: providing a diaphragm, a positive electrode sheet, and a negative electrode sheet; sequentially loading the diaphragm, the positive electrode sheet, and the negative electrode sheet; performing glue dispensing treatment on the diaphragm; and performing winding treatment on the positive electrode sheet, the negative electrode sheet, and the diaphragm.
[0057] In some embodiments, after the conventional positive electrode sheet and the negative electrode sheet are coated with the active material layer, they are cut into corresponding positive electrode sheets / negative electrode sheets, and then the formed positive electrode sheet and negative electrode sheet are subjected to a die-cutting process based on certain die-cutting parameters, and finally a winding process is performed. The die-cutting process includes the steps of die-cutting loading, unwinding and conveying, tab die-cutting, and winding and unwinding. The winding process includes the steps of winding loading, unwinding and conveying, winding processing, and unloading. The preparation method provided in the embodiment disclosed in the present application performs a dispensing process on the diaphragm after unwinding and conveying. That is to say, the diaphragm, the positive electrode sheet, and the negative electrode sheet are aligned at this time. In this way, the first edge and the second edge can be distinguished based on the position of the tab, and then the inner circle and the outer circle during the subsequent winding process can be distinguished. Compared with other distinguishing processes and distinguishing methods, it is more convenient and quick.
[0058] The distribution arrangement in the glue dispensing process provided in the embodiment of the present application will be described below in conjunction with the relevant drawings.
[0059] Figure 4 A top view of a film layer corresponding to a film layer provided in a method for preparing an energy storage battery cell provided in an embodiment of the present application; Figure 5 A first top view of a film layer corresponding to the glue dispensing process in the method for preparing an energy storage battery cell provided in one embodiment of the present application; Figure 6 A second top view of a film layer corresponding to the glue dispensing process in the method for preparing an energy storage battery cell provided in one embodiment of the present application; Figure 7 A third top view of a film layer corresponding to the glue dispensing process in the method for preparing an energy storage cell provided in one embodiment of the present application.
[0060] refer to Figure 4 The preparation method includes: providing a film layer 10, the film layer 10 is one of a positive electrode sheet, a separator or a negative electrode sheet, and the film layer 10 has a first edge 101 and a second edge 102 arranged opposite to each other along a first direction X.
[0061] In some embodiments, if the film layer 10 is a positive electrode sheet or a negative electrode sheet, the end near the first edge 101 has a tab, that is, the positive electrode sheet / negative electrode sheet after the die-cutting step, and the first edge 101 and the second edge 102 are distinguished by the position of the tab.
[0062] refer to Figure 5 or Figure 6The preparation method includes: performing glue dot treatment on the film layer 10 so that the surface of the film layer 10 has multiple groups of glue dots arranged along the first direction X; the distribution density of the glue dots in the glue dot group decreases along the direction from the second edge 102 to the first edge 101. The glue dot group is composed of multiple glue dots arranged at intervals along the second direction.
[0063] In some embodiments, the size of the glue dot is d0, and d0 is between 0.1 mm and 0.5 mm. The size of the glue dot can be any one of any ranges of 0.1 mm to 0.2 mm, 0.2 mm to 0.3 mm, 0.3 mm to 0.4 mm, or 0.4 mm to 0.5 mm. The size of the glue dot can be 0.1 mm, 0.18 mm, 0.23 mm, 0.38 mm, 0.46 mm, or 0.5 mm. The size range of the glue dot can make the distribution density of the glue dot group easier to plan, thereby reducing the difficulty of preparing the glue dot. The size range of the glue dot can also avoid the area of the glue dot being large, and the stress caused by subsequent curing will have an adverse effect on the film layer, thereby improving the yield of the energy storage battery.
[0064] In some embodiments, the distance between two adjacent glue dots is L0, and L0 is between 1d0 and 2d0. L0 can be any range of 1d0 to 1.2d0, 1.2d0 to 1.5d0, 1.5d0 to 1.8d0, or 1.8d0 to 2d0. L0 can be 1d0, 1.3d0, 1.6d0, or 1.9d0.
[0065] In some embodiments, the spacing between two adjacent groups of glue dots is S0, and S0 is between 1.2d0 and 2.5d0. S0 can be any range of 1.2d0 to 1.5d0, 1.5d0 to 1.8d0, 1.8d0 to 2.1d0, or 2.1d0 to 2.5d0. S0 can be 1.3d0, 1.6d0, 1.9d0, 2.3d0, or 2.5d0.
[0066] In some embodiments, the total area of the orthographic projection of the glue dots in the plurality of glue dot groups on the film layer 10 accounts for 10% to 14% of the surface area of the film layer 10. The total area of the orthographic projection of the glue dot group on the film layer 10 accounts for 10%, 11%, 12%, 13% or 14% of the surface area of the film layer 10. In this way, the total area of the orthographic projection of the glue dot group on the film layer 10 accounts for the surface area of the film layer 10. It can be understood as the area where the glue dots are formed in a front film layer. If the total area of the glue dots and the surface area of the film layer are within the above range, the content of the glue dots is more appropriate, thereby achieving mutual bonding between the positive electrode sheet and the diaphragm and mutual bonding between the negative electrode sheet and the diaphragm, and avoiding the separation of the two; secondly, the content of glue is also more appropriate, thereby reducing the preparation cost of the glue and avoiding the problem of overflowing glue.
[0067] In some embodiments, the middle position of the film layer along the first direction is taken as the boundary, the area from the boundary to the first edge is the sparse area, and the area from the boundary to the second edge is the dense area. For the dense area, the size of the glue dots is D1, D1 is between 1d0 and 1.2d0, the spacing between two adjacent glue dot groups is S1, S1 is 0.9S0, the spacing between two adjacent glue dots is C1, C1 is 0.9L0, and the total area of the glue dots accounts for 12% to 16% of the film layer area. For the sparse area, the size of the glue dots is D2, D2 is between 0.8d0 and 1d0, the spacing between two adjacent glue dot groups is S2, S2 is 1.1S0, the spacing between two adjacent glue dots is C2, C2 is 1.3L0, and the total area of the glue dots accounts for 7% to 11% of the film layer area.
[0068] It should be noted that the spacing refers to the straight-line distance between the center of a glue dot and the center of another glue dot, and the size of a glue dot refers to any value between the minimum distance and the maximum distance of the glue dot.
[0069] In some embodiments, the glue points of each glue point group are sequentially formed by interpolation, which may be a linear interpolation model or a Lagrangian interpolation model.
[0070] In some embodiments, reference Figure 5 , the first glue point group 120 near the first edge 101 and the second glue point group 130 near the second edge 102, the first spacing L1 of adjacent first glue points 121 in the first glue point group 120 is greater than the second spacing L2 of adjacent second glue points 131 in the second glue point group 130. The difference in spacing between glue point groups at different positions also makes the distribution density of glue points different within a unit area, that is, the distribution density of the first glue points 121 in the first glue point group 120 near the first edge 101 is less than the distribution density of the second glue points 131 in the second glue point group 130 near the second edge 102, that is, the distribution density of glue points near the inner circle is larger, so that it has great adhesion to avoid and resist the stress caused by the winding process, so that the inner circle separator and the positive electrode sheet / the separator and the negative electrode sheet will not be delaminated, thereby avoiding separator wrinkles.
[0071] In addition, if the spacing is larger, the area where the outer circle is located can be used as a channel for gas discharge, that is, when the gas released by the outer circle's diaphragm, positive electrode plate and negative electrode plate due to the electrolyte can be discharged through the channel formed by the two glue points, it can avoid the problem of bubbles formed by the gas and causing wrinkles in the diaphragm.
[0072] In some embodiments, the ratio of the first spacing L1 to the second spacing L2 is 1.03-1.3. The ratio of the first spacing to the second spacing may be 1.03, 1.1, 1.2 or 2. Thus, the spacing ratio of the glue dots of the inner and outer circles is within this range, and the relevant parameters of the glue dispensing process are controlled to reduce the preparation cost while ensuring a good fit between the diaphragm and the positive electrode sheet, so as to improve the corresponding problems.
[0073] In some embodiments, reference Figure 6 , the glue point group includes: a first glue point group 120 near the first edge 101 and a second glue point group 130 near the second edge 102, and the size d1 of the first glue point 121 in the first glue point group 120 is smaller than the size d2 of the second glue point 131 in the second glue point group 130. In this way, the distribution density of the first glue point group 120 near the first edge 101 is smaller than the distribution density of the second glue point group 130 near the second edge 102, that is, the distribution density of the glue points near the inner circle is larger, so that it has a great adhesive force to avoid and resist the stress caused by the winding process, so that the inner circle of the separator and the positive electrode sheet or the separator and the negative electrode sheet will not be delaminated, thereby avoiding the separator wrinkles.
[0074] in, Figure 5 The size of each glue dot shown can be the same, that is, they are all the original size d. In some embodiments, the sizes of the glue dots can also be different, but it is necessary to satisfy that the distribution density of the glue dot group near the first edge 101 is less than the distribution density of the glue dot group near the second edge 102. For example, the size of the first glue dot 121 is smaller than the size of the second glue dot 131. Similarly, Figure 6 The spacing between each adjacent glue point shown can be the same, that is, the original spacing L. In some embodiments, the spacing between adjacent glue points can also be different, but it is necessary to satisfy that the distribution density of the glue point group near the first edge 101 is less than the distribution density of the glue point group near the second edge 102. For example, the glue point spacing of the glue points in the first glue point group 120 is greater than the glue point spacing of the second glue point group 130.
[0075] It should be noted that Figure 5~Figure 7 The shape of the glue dots is circular as an example, but this does not constitute a limitation on the shape and size of the glue dots. Those skilled in the art can design the shape and size of the glue dots as needed to ensure that the distribution density near the first edge 101 is less than the distribution density near the second edge 102.
[0076] In some embodiments, the film layer 10 further has two third edges 103 arranged opposite to each other along the second direction Y, and the two ends of each third edge 103 are respectively connected to the first edge 101 and the second edge 102; during the process of dispensing glue on the film layer 10, the distribution density of the glue points in the glue point group close to the third edge 103 is the largest in the direction from the center of the film layer in the second direction to the third edge. The high density of glue points on both sides ensures that the edge separator and the positive / negative electrode sheet are more closely attached, improves the misalignment damage between the friction layers on the side during the subsequent core transportation process, and the impact of the airflow and electrolyte on the core during the liquid injection formation process, and improves the problem of brown spots on the bottom of the core head at the full filling interface; it can also reduce the amount of glue used and reduce the preparation cost.
[0077] In some embodiments, along the second direction Y and pointing to the third edge 103, the spacing between adjacent glue dots decreases; and / or, referring to Figure 7 , along the second direction and in the direction pointing to the third edge 103, the size of the glue dots increases, for example, the size d21 of the glue dots close to the third edge is larger than the size d20 of the glue dots away from the third edge. The decreasing spacing of the glue dots and the increasing size of the glue dots can make the distribution density increase along the second direction and in the direction toward the third edge 103, so that the content of glue near the edge is larger, and the edge of the diaphragm can be more closely attached to the electrode.
[0078] It should be noted that Figure 7 Only the second glue dots in the second glue dot group 130 are shown to have an increasing size trend along the second direction and pointing to the third edge 103, but the first glue dots in the first glue dot group 120 and the groups of glue dots in the first glue dot group 120 and the second glue dot group 130 may also show this trend, and the embodiments of the present application do not limit this description.
[0079] In some embodiments, before the positive electrode sheet, the negative electrode sheet and the separator are wound, the film layer 10 is heated, and the heating treatment is at least used to make the glue points of the glue point group present a molten state and pre-fix the positive electrode sheet and the separator and / or pre-fix the negative electrode sheet and the separator. In this way, the glue points on the film layer will be activated and become sticky after heating. When fixing, the battery cell formed subsequently is preheated and pressed, and the glue after preheating and pressing is activated and becomes sticky, thereby bonding and fixing the positive electrode sheet / negative electrode sheet and the separator.
[0080] In some embodiments, while the positive electrode sheet, the negative electrode sheet and the separator are being wound, the film layer 10 is also heated, and the heating process is at least used to melt the glue points of the glue point group and form an adhesive layer. Heating while winding, that is, hot winding, can activate the viscosity of the glue points on the film layer, so that the subsequent cold pressing process and the core forming effect are better, and the interface between the separator and the positive electrode sheet is more closely attached.
[0081] refer to Figure 8 The preparation method includes: winding a positive electrode sheet 1, a negative electrode sheet 2 and a separator 3. During the winding process, the winding process is performed from the second edge 102 toward the first edge 101; wherein the separator is located between the positive electrode sheet and the negative electrode sheet, and the winding process is at least used for the glue points of the glue point group to be in a molten state and form an adhesive layer, so that the positive electrode sheet is fixed to the separator or the separator is fixed to the negative electrode sheet.
[0082] In some embodiments, the winding process is to wind the separator 3, the positive electrode sheet 1, and the negative electrode sheet 2 into a single winding core by a winding machine. The order is to use the negative electrode sheet 2 to wrap the positive electrode sheet 1, and then separate the positive electrode sheet 1 and the negative electrode sheet 2 by the separator 3.
[0083] In some embodiments, a small winding tension will affect the internal resistance and shell penetration rate; excessive tension can easily cause short circuit or fragmentation risks. Therefore, the winding tension is generally between 0.08Mpa and 0.15Mpa for positive tension, 0.08Mpa and 0.15Mpa for negative tension, 0.08Mpa and 0.15Mpa for upper diaphragm, and 0.08Mpa and 0.15Mpa for lower diaphragm. The width of the negative electrode sheet 2, the width of the positive electrode sheet 1, and the width of the diaphragm 3 are not the same. For example, the width of the negative electrode sheet is 59.5mm, the width of the positive electrode sheet is 58mm, and the width of the diaphragm is 61mm. The three are aligned in the center to improve the alignment of the electrode sheets and avoid the risk of short circuit. The electrode sheet alignment refers to the relative positions of the positive electrode sheet 1, the negative electrode sheet 2, and the diaphragm 3.
[0084] In some embodiments, the process steps of the winding treatment include: hot winding treatment and cold pressing treatment. The hot winding treatment is used to make the glue points of the glue point group molten and form an adhesive layer to fix the positive electrode sheet to the diaphragm and / or the diaphragm to the negative electrode sheet; the cold pressing treatment is used to bond the positive electrode sheet, the negative electrode sheet and the diaphragm together.
[0085] It should be noted that in order to explain and distinguish the diaphragm, the positive electrode sheet and the negative electrode sheet, Figure 8 The dotted line indicates the separator, the thinner solid line indicates the negative electrode, and the thicker solid line indicates the positive electrode, but this does not represent the thickness relationship between the separator, the positive electrode, and the negative electrode. Figure 8 There are gaps between the middle diaphragm 3, the positive electrode sheet 1 and the negative electrode sheet 2. This is to clearly indicate the winding correspondence between the diaphragm 3, the positive electrode sheet 1 and the negative electrode sheet 2, but it does not mean that there must be a gap between the diaphragm 3 and the positive electrode sheet 1 or between the diaphragm 3 and the negative electrode sheet 2. In other words, the diaphragm 3 and the positive electrode sheet 1 can be in contact with each other, or the diaphragm 3 and the negative electrode sheet 2 can be in contact with each other.
[0086] The method for preparing the energy storage battery cell also includes: placing the whole body formed by winding the positive electrode sheet 1, the negative electrode sheet 2 and the separator 3 in a cavity formed by the shell, and the cavity is also filled with electrolyte.
[0087] The electrolyte is a carrier that conducts electrons between the positive and negative electrodes in the battery. In some embodiments, the electrolyte can be an electrolyte, which consists of three parts: a solvent, a lithium salt, and an additive. The solvent is used to dissolve the lithium salt, and the solvent may include cyclic carbonates (PC, EC); chain carbonates (DEC, DMC, EMC); carboxylates (MF, MA, EA, MA, MP, etc.). The lithium salt may be LiPF6, LiClO4, LiBF4, LiAsF6, etc. The additive may be a film-forming additive, a conductive additive, a flame retardant additive, an overcharge protection additive, an additive for controlling the content of H2O and HF in the electrolyte, an additive for improving low temperature performance, and a multifunctional additive. One or more.
[0088] The preparation method includes: welding the pole ear, welding the pole ear to the adapter, connecting the other end of the adapter to the pole, and engaging the top rod with the shell. The adapter is located in the chamber, and the pole passes through the top cover.
[0089] Among them, the adapter plate includes at least a first adapter plate and a second adapter plate, the pole includes a positive pole pole and a negative pole pole, the first adapter plate is electrically connected to the pole ear of the positive pole plate and the positive pole pole respectively, and the second adapter plate is electrically connected to the negative pole ear of the negative pole plate and the negative pole pole respectively.
[0090] The preparation method of the energy storage battery provided in the present application performs glue dispensing on one of the positive electrode sheet 1, the diaphragm 3 or the negative electrode sheet 2, and arranges the glue point group in a specific manner to alleviate and offset the stress problem caused by the bending area of the core, thereby avoiding the problem of wrinkles at the interface between the positive electrode sheet and the diaphragm and the interface between the diaphragm and the negative electrode sheet caused by the subsequent wrinkles of the diaphragm, so as to improve the interface effect. Based on this uneven arrangement, that is, the distribution density of the glue point group is smaller as it approaches the first edge 101, that is, the distribution density is smaller at the position closer to the outer circle of the core, which can ensure that the adhesion of the glue points between the inner circle diaphragm and the positive electrode sheet and between the diaphragm and the negative electrode sheet is greater, and then used to resist the stress caused by the bending curvature, so that the positive electrode sheet and the diaphragm, the diaphragm and the negative electrode sheet are more closely attached, and the problem of easy wrinkles in the inner circle of the core at the full charge interface is improved, and the amount of glue used can be reduced, reducing the preparation cost.
[0091] Accordingly, according to some embodiments of the present application, the embodiments of the present application further provide an energy storage cell, which can be prepared using the preparation method provided in the above embodiments, and the technical features that are the same as or corresponding to the above embodiments will not be described in detail here.
[0092] refer to Figure 8and Figure 7 The energy storage cell includes: a positive electrode sheet 1, a negative electrode sheet 2 and a separator 3, wherein the separator 3 is located between the positive electrode sheet 1 and the negative electrode sheet 2; an adhesive layer 140 is provided between the positive electrode sheet 1 and the separator 3 or between the negative electrode sheet 2 and the separator 3, wherein the positive electrode sheet 1 and the separator 3 are fixed to each other through the adhesive layer 140 and / or the negative electrode sheet 2 and the separator 3 are fixed to each other through the adhesive layer 140; an adhesive group, wherein the adhesive group includes a plurality of adhesive layers 140; and along the winding direction from the inner circle to the outer circle, the distribution density of the adhesive group decreases.
[0093] The inner circle refers to the inner circle of the winding core structure formed, corresponding to Figure 6 The outer ring refers to the outer ring of the formed core structure, corresponding to Figure 6 The first edge in .
[0094] The energy storage cell provided in the embodiment of the present application has an unevenly distributed glue, and the positive electrode sheet or negative electrode sheet corresponding to the outer ring and the diaphragm are not completely adhered, so that there is a microscopic channel between the positive electrode sheet / negative electrode sheet or between the positive electrode sheet and the positive electrode sheet, and the electrolyte can flow directly to the adhered area in the middle of the electrode sheet, so that not only the edge penetrates into the middle area through capillary action, which reduces the difficulty of cell infiltration, thereby improving the yield of the energy storage cell. Moreover, this channel can also be used as a gas holding area, so that the gas generated by the charging and discharging of the battery cell stays in the gas holding area, which can reduce the impact of the gas on the diaphragm and prevent the diaphragm from separating from the electrode sheet. The gas holding area can also be used as a buffer zone to facilitate gas seepage, especially when the battery cell is not working, the gas continues to seep out from the gas holding area to achieve the emptying of the gas holding area, so that after the gas is generated by the charging and discharging of the battery cell, the gas will gather in the gas holding area again.
[0095] Those skilled in the art will appreciate that the above-mentioned embodiments are specific examples for implementing the present application, and in practical applications, various changes may be made to the embodiments in form and detail without departing from the spirit and scope of the present application. Any person skilled in the art may make various changes and modifications without departing from the spirit and scope of the present application, and therefore the scope of protection of the present application shall be subject to the scope defined in the claims.
Claims
1. A method for preparing an energy storage battery cell, characterized in that: include: Providing a film layer, wherein the film layer is one of a positive electrode sheet, a separator or a negative electrode sheet, and the film layer has a first edge and a second edge that are arranged opposite to each other along a first direction; Performing glue dispensing treatment on the film layer, so that the surface of the film layer has a plurality of glue dot groups arranged along a first direction; along the direction from the second edge to the first edge, the distribution density of the glue dot groups decreases; forming the positive electrode sheet, the separator or the other two of the negative electrode sheet; The positive electrode sheet, the negative electrode sheet and the separator are subjected to a winding process, and the winding process is performed from the second edge toward the first edge; wherein the separator is located between the positive electrode sheet and the negative electrode sheet, and the winding process is at least used to make the glue points of the glue point group present a molten state and form an adhesive layer to fix the positive electrode sheet to the separator and / or to fix the separator to the negative electrode sheet.
2. The method for preparing the energy storage battery cell according to claim 1, characterized in that: The film layer also has two third edges arranged opposite to each other along the second direction, and the two ends of each third edge are respectively connected to the first edge and the second edge; in the process of glue dispensing treatment on the film layer, the distribution density of the glue points in the same glue point group increases from the center of the film layer in the second direction toward the third edge.
3. The method for preparing the energy storage battery cell according to claim 2, characterized in that: Along the second direction and pointing to the third edge, the spacing between adjacent glue dots in the same glue dot group decreases; and / or, along the second direction and pointing to the third edge, the size of the glue dots in the same glue dot group increases.
4. The method for preparing the energy storage battery cell according to claim 1, characterized in that: The glue dot group includes: a first glue dot group close to the first edge and a second glue dot group close to the second edge, the size of the first glue dot in the first glue dot group is smaller than the size of the second glue dot in the second glue dot group; and / or, the first spacing between adjacent first glue dots in the first glue dot group is larger than the second spacing between adjacent second glue dots in the second glue dot group.
5. The method for preparing the energy storage battery cell according to claim 4, characterized in that: The ratio of the first spacing to the second spacing is 1.03-1.
3.
6. The method for preparing the energy storage battery cell according to claim 1, characterized in that: The ratio of the total area of the orthographic projections of the plurality of glue dot groups on the film layer to the surface area of the film layer is 10% to 14%.
7. The method for preparing the energy storage battery cell according to claim 1, characterized in that: The process steps of the winding treatment include: hot winding treatment and cold pressing treatment. The hot winding treatment is used to make the glue points of the glue point group present a molten state and form the adhesive layer to fix the positive electrode sheet to the diaphragm and / or to fix the diaphragm to the negative electrode sheet; the cold pressing treatment is used to make the positive electrode sheet, the negative electrode sheet and the diaphragm fit each other.
8. The method for preparing the energy storage battery cell according to claim 1, characterized in that: Before winding the positive electrode sheet, the negative electrode sheet and the separator, the film layer is subjected to a heating treatment, wherein the heating treatment is at least used to melt the glue points of the glue point group and pre-fix the positive electrode sheet and the separator and / or pre-fix the negative electrode sheet and the separator.
9. The method for preparing the energy storage battery cell according to claim 1, characterized in that: While the positive electrode sheet, the negative electrode sheet and the separator are being wound, the method further includes: heating the film layer, wherein the heating treatment is at least used to melt the glue points of the glue point group and form the adhesive layer.
10. An energy storage battery cell, characterized in that: include: A positive electrode sheet, a negative electrode sheet and a separator, wherein the separator is located between the positive electrode sheet and the negative electrode sheet; an adhesive layer is provided between the positive electrode sheet and the separator or between the negative electrode sheet and the separator, and the positive electrode sheet and the separator are fixed by the adhesive layer and / or the negative electrode sheet and the separator are fixed by the adhesive layer; The viscose group includes a plurality of viscose layers; along the winding direction from the inner circle to the outer circle, the distribution density of the viscose group decreases.
Citation Information
Patent Citations
Reel member, winding method for adhesive film, and unwinding method for adhesive film
CN104203789A
Polymer coating diaphragm and lithium ion battery
CN111092192A
Battery pole group for improving winding stress and battery using same
CN111934025A
Diaphragm, pole piece, winding type battery cell, battery and electric device
CN115842215A
Diaphragm and preparation method thereof, electrode assembly, battery monomer, battery and electric device
CN115939672A
Cited By
Battery cell, separator and preparation method therefor, battery, and electric device
WO2026174710A1