Asymmetric copper thickness laminated PCB structure and preparation method thereof
Through asymmetric copper thick stack structure and specialized manufacturing processes, the problem that symmetric copper thick stack cannot meet the needs of high conduction and complex circuits is solved, achieving higher electrical performance and thermal stability, and reducing production costs.
Patent Information
- Application Number
- CN202411245535.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-05
- Publication Date
- 2024-11-08
AI Technical Summary
The existing symmetrical copper thick stacked structure cannot meet the needs of higher conduction capabilities and complex circuit layouts, and there is room for improvement in cost and production efficiency.
Asymmetric copper thick laminated structure is adopted, by alternately bonding the semi-cured sheet and the copper laminate, a thick copper layer and a thin copper layer are arranged, the thick copper layer is a wireless path layer and a power layer, the thin copper layer is a circuit layer, and the copper stack is The number is more than the semi-cured sheet, and the thick copper layer is located in the outermost layer and is manufactured by electroless copper plating, electroplating, film patching, exposure, film stripping and etching processes.
It realizes flexible adjustment of copper thickness value and stacking relationship, improves electrical performance and thermal stability, adapts to complex circuit layout, improves integration and reliability, and reduces production costs.
Smart Images

Figure CN118921840A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of printed circuit boards, and in particular to an asymmetric copper thick laminated PCB structure and a preparation method thereof. Background Art
[0002] As the requirements for printed circuit boards in communications and other equipment continue to increase, the network speed and data volume will increase, forcing the number of layers and conduction capacity of printed circuit boards to continue to increase. Figure 1 A symmetrical copper thickness stack is presented, which includes eight copper stacks L1, L2, L3, L4, L5, L6, L7, and L8 arranged in sequence. The thickness of each copper stack can be 16um, of which L1, L3, L5, L7, and L8 are line layers, and L2, L4, and L6 are power layers. This symmetrical copper thickness stack cannot fully meet the design requirements of higher conductivity because each layer of copper is equal in thickness and relatively thin. Therefore, the research and development direction points to a more flexible asymmetric copper thickness stack.
[0003] The Chinese utility model patent with the announcement number "CN215581874U" discloses "an asymmetric blind buried via board". The asymmetric blind buried via board is designed with 1 ounce thick copper, yin and yang thick copper (i.e., 0.5 ounce thick copper), daughter board and mother board structure, and the total copper thickness reaches 20 ounces. The heat resistance of high-power electronic products is greatly improved, the product stability is good, and the high heat dissipation and high heat resistance requirements of high-power and high-current products are met.
[0004] For the design of asymmetric copper thickness stacking, the main goal is to achieve the circuit layout of specific functions, while optimizing costs, improving production efficiency and ensuring product reliability. Therefore, there are more detailed and in-depth designs of asymmetric copper thickness stacking that need to be developed. Summary of the invention
[0005] This application is made in view of the above-mentioned state of the prior art. In a first aspect, the purpose of this application is to provide an asymmetric copper thick laminated PCB structure.
[0006] The technical solution adopted by the present application to solve its technical problems includes: an asymmetric copper thick laminate PCB structure, including: a prepreg; a copper laminate, a plurality of the copper laminates and a plurality of the prepregs are alternately laminated with each other; wherein the copper laminate is divided into a thick copper layer and a thin copper layer according to different thicknesses, and the copper thickness value of the thick copper layer is greater than the copper thickness value of the thin copper layer; the copper laminate is divided into a circuit layer and a non-circuit layer according to whether there is a circuit, the thick copper layer is the non-circuit layer and the power supply layer, and the thin copper layer is the circuit layer; the number of the copper laminates is one more than the number of the prepregs, and the outermost layer in the copper laminate is the thin copper layer; the number of the thick copper layer is one, the copper thickness value of each thin copper layer is equal, and the difference in the number of the thin copper layers on both sides of the thick copper layer is one.
[0007] As a further improvement of the present application, the number of the copper laminates is an even number, and the number of the prepreg sheets is an odd number.
[0008] As a further improvement of the present application, the number of the copper stacks is six, and the number of the prepregs is five.
[0009] As a further improvement of the present application, the copper thickness of a single thick copper layer is greater than twice the copper thickness of a single thin copper layer.
[0010] As a further improvement of the present application, the copper thickness of each copper laminate ranges from 12 um to 70 um.
[0011] As a further improvement of the present application, the copper thickness of the thick copper layer ranges from 35um to 39um, and the copper thickness of the thin copper layer ranges from 14um to 18um.
[0012] As a further improvement of the present application, the copper thickness of the thick copper layer is 37um, and the line width of the thick copper layer is 60um; the copper thickness of the thin copper layer is 16um, and the line width of the thin copper layer is 30um.
[0013] As a further improvement of the present application, the cross-sectional profiles of the copper wires of the thick copper layer and the thin copper layer are both isosceles trapezoids.
[0014] As a further improvement of the present application, when observed from a perspective perpendicular to the plane where the copper stack is located, the copper stack is at least partially provided with the thick copper layer, and the thick copper layer is correspondingly arranged with SMT patch components; within a unit area, the wiring density of the thick copper layer is greater than the wiring density of the thin copper layer.
[0015] As a further improvement of the present application, the thickness of each of the prepregs is equal.
[0016] In the second aspect, a method for preparing an asymmetric copper thick laminated PCB is provided. It is used to manufacture the asymmetric copper thick laminated PCB structure of the present application, including: step S1, chemical copper plating: depositing chemical copper on the surface of the outermost copper laminate; step S2, electroplating: coating a layer of electroplating on the surface of the chemical copper by electroplating; step S3, film pasting: pasting a photosensitive dry film on the side of the electroplating layer away from the copper laminate; step S4, light exposure: placing the photosensitive dry film under ultraviolet irradiation, and the photosensitive dry film forms a circuit pattern; step S5, film stripping: stripping the photosensitive dry film in step S3; step S6, etching: partially etching the chemical copper, the electroplating layer, and the copper laminate, and the remaining chemical copper, the electroplating layer, and the copper laminate form a circuit matching the circuit pattern; wherein the copper laminate is thickened in step S2.
[0017] The beneficial effects of the asymmetric copper thick laminated PCB structure of the present application include: the copper laminates are thick and thin, forming an asymmetric design, so that the copper thickness values of different copper laminates and the mutual lamination relationship of the thick copper layer and the thin copper layer in the copper laminate can be flexibly adjusted according to the actual needs of the circuit to achieve the best electrical performance and thermal stability. Compared with the symmetrical design, the asymmetric copper thick laminated PCB structure of the present application can better adapt to the layout of complex circuits, has good heat resistance and stability, can meet the high heat dissipation and high heat resistance requirements of high-power and high-current products, and improves the integration and reliability of the circuit board. Compared with the existing asymmetric design, the asymmetric copper thick laminated PCB structure of the present application has a thick copper layer that is bonded to the semi-cured sheet located in the middle layer, and the thick copper layer is a non-circuit layer and a power layer, which can give full play to its high conduction and high heat dissipation capabilities. The specific principle of improving heat dissipation performance is that increasing the thickness of the copper laminate can improve its heat dissipation performance, because the thicker copper layer can better conduct heat, which helps to quickly dissipate the heat generated during the operation of the circuit. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] In order to more clearly illustrate the technical solutions in the embodiments, the drawings of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0019] Figure 1 is a schematic diagram of an implementation of a symmetrical copper thick stacked PCB structure;
[0020] Figure 2 is a schematic diagram of an embodiment of an asymmetric copper thick laminated PCB structure of the present application;
[0021] Figure 3 is a process flow chart of an implementation of an asymmetric copper thick laminated PCB structure of the present application;
[0022] Figure 4 It is a wiring comparison diagram of an implementation of the asymmetric copper thick stacked PCB structure of the present application and a related symmetric copper design;
[0023] Figure 5 This is a power consumption comparison chart of L4 of an implementation of the asymmetric copper thick laminated PCB structure of the present application and a related symmetric copper design.
[0024] Description of Reference Numerals
[0025] 1-Copper laminate; 2-Prepreg. DETAILED DESCRIPTION
[0026] The exemplary embodiments of the present application are described below with reference to the accompanying drawings. It should be understood that these specific descriptions are only used to teach those skilled in the art how to implement the present application, and are not intended to exhaust all possible methods of the present application, nor to limit the scope of the present application.
[0027] See also Figure 2 , an embodiment of the present application provides an asymmetric copper thick laminate PCB structure. The PCB structure includes a plurality of semi-cured sheets 2 and copper laminates 1 that are alternately laminated to each other. Among them, the copper laminate 1 is divided into a thick copper layer and a thin copper layer according to different thicknesses, and the copper thickness of the thick copper layer is greater than the copper thickness of the thin copper layer; the copper laminate 1 is divided into a circuit layer and a non-circuit layer according to whether there is a circuit, the thick copper layer is a non-circuit layer and a power layer, and the thin copper layer is a circuit layer; the number of copper laminates 1 is one more than the number of semi-cured sheets 2, and the thin copper layer located at the outermost layer of the entire PCB structure in the copper laminate 1; the number of thick copper layers is one, and the copper thickness of each thin copper layer is equal. The number of thin copper layers on both sides of the thick copper layer is different, and the value of the number of relatively more thin copper layers on one side of the thick copper layer minus the number of relatively less thin copper layers on the one side of the thick copper layer is one.
[0028] The non-circuit layer is mainly the power layer. The thickening of the power layer will increase the corresponding current carrying capacity. The advantages of thickening copper are as follows: first, it can carry large current; second, it can reduce thermal strain; and third, it can improve heat dissipation performance. Since the PCB board has high requirements for carrying large currents, choosing a thicker copper design can better realize the circuit function and improve the circuit's current carrying capacity and stability. There will be no signal interference between different layers of thick copper layers and thin copper layers.
[0029] In one embodiment, the number of copper laminates 1 is an even number, and the number of prepregs 2 is an odd number. For example, the number of copper laminates 1 may be six, and the number of prepregs 2 may be five.
[0030] Figure 2 The number of layers of the copper laminate 1 and the prepreg 2 is only an example. According to actual production requirements, the total number of layers of the copper laminate 1 can also be twelve layers, ten layers, eight layers, etc. The advantages of reducing the total number of layers of the copper laminate 1 include: first, it can carry large current; second, it can reduce thermal strain; third, the heat dissipation performance is improved; fourth, the production cost is reduced.
[0031] In order to ensure the accurate alignment and pressing between the different layers of copper laminate 1 and prepreg 2. First, alignment is required. Since the different copper thicknesses lead to different deformations of the PCB board, the thick copper layer and the thin copper layer have different alignment methods. Second, pressing, the copper thickness of the thick copper layer increases, and the amount of resin that needs to be filled increases to deal with the risk of resin voids.
[0032] In one embodiment, the copper thickness of the thick copper layer ranges from 30 um to 70 um.
[0033] In one embodiment, the copper thickness of the thick copper layer is greater than twice the copper thickness of the single thin copper layer. The copper thickness of each copper stack 1 may range from 12 um to 70 um.
[0034] In one embodiment, the copper thickness of the thick copper layer ranges from 35um to 39um, and the copper thickness of the thin copper layer ranges from 14um to 18um. Figure 4 As shown, the copper thickness of the thick copper layer can be 37um, and the line width of the thick copper layer is 60um; the copper thickness of the thin copper layer can be 16um, and the line width of the thin copper layer is 30um. The line width values of the thick copper layer and the thin copper layer are used as examples. The technical connotation embodied is that the number of power layers is reduced and merged into one layer, and the corresponding copper thickness of this layer is increased, so that the total number of layers of the copper stack 1 can be reduced, and then part of the power layer or the ground layer (also called: ground layer, GND layer) in the line layer can be reduced to increase the line density.
[0035] like Figure 4 , Figure 5 As shown in FIG. 1 , in one embodiment, the cross-sectional profiles of the copper wires of the thick copper layer and the thin copper layer can both be isosceles trapezoids. Figure 5 As shown in the figure, if the line widths of the thick copper layer and the thin copper layer are equal, the line density of the thick copper layer and the thin copper layer in the PCB board is the same, but the cross-sectional area of the thick copper layer must be larger than that of the thin copper layer. Figure 4 As shown in the figure, if the line width of the thick copper layer is smaller than that of the thin copper layer, the line density of the thick copper layer in the PCB must be greater than that of the thin copper layer in the PCB. Moreover, when the line width of the thick copper layer is not much different from that of the thin copper layer, the thick copper layer can take into account both the advantages of large cross-sectional area and high line density in the PCB.
[0036] like Figure 2 As shown, one embodiment of the asymmetric copper thick laminate PCB structure of the present application may include six copper laminates 1, namely L1, L2, L3, L4, L5, and L6 arranged in sequence, wherein L1, L2, L3, L5, and L6 are thin copper layers and circuit layers, and the copper thickness is 16um, and L4 is a thick copper layer and a power layer. In an example, the copper thickness of L4 can range from 30um to 70um.
[0037] like Figure 4As shown in the comparison chart, the copper thickness value of L4 in the comparative example (usually) is 16um, but in this embodiment, the copper thickness value of L4 is changed to 37um. When L3 and L5 are unchanged, the density of L4 with a copper thickness value of 37um can be significantly higher. Specifically, in a non-limiting example, in a symmetrical copper stacking wiring design, the line width of the L3 copper layer and the L5 copper layer is 60um and the copper thickness value is 16um, while the line width of the L4 copper layer is 100um and the copper thickness value is 16um. In the asymmetrical copper stacking wiring design, the line width of the L3 copper layer and the L5 copper layer is 30um and the copper thickness value is 16um, while the line width of the L4 copper layer is 60um and the copper thickness value is 37um. By comparison Figure 4 The distribution of single-layer line width can be reduced because the copper thickness increases, so the wiring density can be increased.
[0038] To illustrate the power consumption advantage of thick copper layers, Figure 5 As shown in the comparison diagram, the upper base length of the trapezoid of the power layer cross section is B, and the lower base length is C, wherein the height of the symmetrical copper design of the comparative example is A, and the height of the asymmetrical copper design of the embodiment is A+a.
[0039] According to the DC resistance formula Where R is the resistance, ρ is the resistivity, L is the wire length, and S is the wire cross-sectional area. The actual resistance of the symmetrical copper design for the comparison is The actual resistance of the asymmetric copper design of the embodiment
[0040] According to the power consumption formula W = I 2 Rt, where W is the heat generated by power consumption, I is the current, R is the resistance, and t is the time. The actual resistance of the asymmetric copper design of the embodiment
[0041] Finally, the power consumption ratio is This indicates that power consumption is directly related to copper thickness, and the power consumption of the embodiment is small.
[0042] In order to further illustrate the relationship between different copper thicknesses and power consumption in thick copper layers, five different copper thickness values are taken as shown in the following table. Among them, the variables such as copper resistivity, line length, top line width, bottom line width, current, and time are controlled, and the five copper thickness values are different, and then the copper cross-sectional area, resistance, and power consumption are different. The final results are also shown in the following table:
[0043]
[0044] like Figure 5As shown, after adopting the asymmetric copper thick layer PCB structure of the present application, the thick copper layer resistance is set to be smaller than the thin copper layer resistance, and the power consumption is lower under the same current time. Similarly, the lower the power consumption, the better the heat dissipation.
[0045] In one embodiment, when observed from a perspective perpendicular to the plane where the copper laminate 1 is located, a thick copper layer is at least partially provided in the copper laminate 1, and SMT (surface assembly technology) patch components are arranged correspondingly in the thick copper layer (that is, when projected in a direction perpendicular to the plane where the copper laminate 1 is located, the SMT patch components will intersect with the thick copper layer). Within a unit area, the wiring density of the thick copper layer is greater than that of the thin copper layer. The thick copper layer has better conductivity and heat dissipation performance, which is just right for nearby assembly of SMT patch components. The wiring line density increases, and the thick copper layer is a non-circuit layer and a power layer, which can give full play to its high conductivity and high heat dissipation capabilities.
[0046] In one embodiment, if Figure 2 As shown, the thickness of each prepreg 2 is equal. In this way, each prepreg 2 has a unified specification, which is convenient for manufacturing.
[0047] The asymmetric copper thickness laminated PCB structure of the present application mainly involves etching, lamination, electroplating, drilling and other processes in its own manufacturing process. These processes require fine control of parameters to ensure that the copper thickness of different layers and the laminated structure meet the design requirements. For example, in the etching process, it is necessary to select appropriate etching liquid and etching parameters and processes according to the complexity and precision requirements of the circuit pattern; in the lamination process, it is necessary to control parameters such as pressure, temperature and time to ensure close bonding between different layers; in the electroplating process, it is necessary to control parameters such as current, speed and temperature to achieve the goal of asymmetric copper thickness.
[0048] Figure 3The manufacturing process of the asymmetric copper thick laminated PCB structure shown is carried out in sequence according to the steps of starting, chemical copper plating, electroplating, film pasting, exposure, film stripping, and etching. Among them, the thickening of the thick copper layer of the asymmetric copper thick laminated PCB structure is carried out in the above-mentioned electroplating step. The starting step in the asymmetric copper thick laminated PCB preparation method of the present application refers to the preparation of the raw materials required for the manufacture of the PCB structure; chemical copper plating refers to the deposition of a chemical copper layer on the surface of a non-conductive substrate by chemical reaction, that is, a chemical copper layer is deposited on the surface of the outermost copper laminate 1; the electroplating step refers to covering the surface of the chemical copper layer with a layer of electroplated copper layer by electroplating, and the copper laminate 1 is thickened in the electroplating step; the film pasting step refers to accurately pasting the photosensitive dry film to the surface of the electroplated copper layer, and pasting the photosensitive dry film on the side of the electroplated layer facing away from the copper laminate 1; the exposure step is the exposure step, which is to paste the PCB with the photosensitive dry film. The board is exposed to ultraviolet light to cause the photosensitive material on the photosensitive dry film to undergo a chemical reaction, thereby forming the desired circuit pattern; the stripping step is to remove the unnecessary part of the photosensitive dry film on the PCB board after the photosensitive dry film is exposed and developed. The purpose of stripping is to expose the copper layer part that needs to be etched for subsequent etching process; the etching step is to remove the unnecessary part of the copper layer on the PCB board, so as to use the remaining copper layer to form the desired circuit pattern and line, and partially etch the chemical copper, electroplating layer, and copper laminate 1. The remaining part of the chemical copper, electroplating layer, and copper laminate 1 form a line matching the circuit pattern.
[0049] The asymmetric copper thickness stacked PCB structure needs to ensure accurate alignment and pressing between different layers in its own manufacturing process, which requires precise equipment and process control. At the same time, due to the complexity of asymmetric design, it is also necessary to consider optimizing circuit layout, reducing production costs and improving production efficiency. While ensuring the copper thickness value, the power line layer must be completed to meet the design specifications and the impedance must also meet the requirements.
[0050] The asymmetric copper thick laminated PCB structure can adopt either MSAP process (i.e., modified semi-additive process) or Tenting process (i.e., dry film hole covering process) for the pattern formation process in its own manufacturing process. Among them, MSAP is the abbreviation of Modified Semi-Additive Process. The Tenting process is a method of making circuit shielding in the form of tents. A more precise term refers to the production method of using dry film to make a protective cover above the through hole of the circuit board to prevent the etching solution from corroding the copper in the hole.
[0051] The overall beneficial effects of the asymmetric copper thick laminated PCB structure of the present application include:
[0052] First, the signal transmission quality is improved. Through asymmetric design, the thickness of the inner copper laminate 1 and the impedance control capability of signal transmission can be more effectively controlled, which is crucial to improving the transmission quality of high-speed digital signals and radio frequency (RF) signals. Accurate impedance control helps reduce signal loss and distortion, ensuring reliable data transmission on the PCB board.
[0053] Secondly, it enhances heat dissipation. Asymmetric copper design usually includes thicker copper layers in key areas, which can significantly improve the heat dissipation performance of the PCB. When using high-power surface mount technology (SMT) patch components, this design can significantly reduce the temperature inside the PCB, thereby improving the stability and reliability of the system.
[0054] Thirdly, the wiring density and flexibility are improved. The asymmetric design allows for increased wiring density and flexibility in the structure of the PCB board, and can easily create a structure with smaller spacing between the power layer and the signal layer. This means that more wiring space can be achieved through PCB board design or flip design, further meeting the wiring needs of complex electronic products.
[0055] Finally, optimize cost-effectiveness. Although the asymmetric copper design may increase certain manufacturing costs, the thick copper layer increases the copper thickness and the electroplating time, the number of electroplating times increases, and the different copper thicknesses on both sides result in different amounts of etched copper. The cost of the thick copper layer increases by 20%, but Figure 2 compared to Figure 1 After the total number of layers is reduced by two, the total cost is reduced by 19%. Considering the performance improvement and reliability enhancement it brings, this design can bring higher cost-effectiveness.
[0056] The above embodiments are only for illustrating the technical concept and features of the present application, and their purpose is to enable people familiar with this technology to understand the content of the present application and implement it. They cannot be used to limit the scope of protection of the present application. All equivalent changes or modifications made according to the spirit of the present application should be included in the scope of protection of the present application.
Claims
1. An asymmetric copper thick laminated PCB structure, characterized in that: include: Prepreg (2); Copper laminate (1), a plurality of the copper laminate (1) and a plurality of the prepreg sheets (2) are alternately laminated to each other; The copper laminate (1) is divided into a thick copper layer and a thin copper layer according to thickness, and the copper thickness of the thick copper layer is greater than the copper thickness of the thin copper layer; the copper laminate (1) is divided into a circuit layer and a non-circuit layer according to whether there is a circuit, the thick copper layer is the non-circuit layer and the power supply layer, and the thin copper layer is the circuit layer; the number of the copper laminate (1) is one more than the number of the prepreg (2), and the outermost layer in the copper laminate (1) is the thin copper layer; the number of the thick copper layer is one, the copper thickness of each thin copper layer is equal, and the difference in the number of the thin copper layers on both sides of the thick copper layer is one.
2. The asymmetric copper thick laminated PCB structure according to claim 1, characterized in that: The number of the copper laminates (1) is an even number, and the number of the prepreg sheets (2) is an odd number.
3. The asymmetric copper thick laminated PCB structure according to claim 1, characterized in that: The number of the copper laminates (1) is six, and the number of the prepreg sheets (2) is five.
4. The asymmetric copper thick laminated PCB structure according to claim 1, characterized in that: The copper thickness of a single thick copper layer is greater than twice the copper thickness of a single thin copper layer.
5. The asymmetric copper thick laminated PCB structure according to claim 1, characterized in that: The copper thickness of the copper laminate (1) ranges from 12 um to 70 um.
6. The asymmetric copper thick laminated PCB structure according to claim 1, characterized in that: The copper thickness of the thick copper layer ranges from 35um to 39um, and the copper thickness of the thin copper layer ranges from 14um to 18um.
7. The asymmetric copper thick laminated PCB structure according to claim 6, characterized in that: The copper thickness of the thick copper layer is 37um, and the line width of the thick copper layer is 60um; the copper thickness of the thin copper layer is 16um, and the line width of the thin copper layer is 30um.
8. The asymmetric copper thick laminated PCB structure according to claim 1, characterized in that: The cross-sectional profiles of the copper wires of the thick copper layer and the thin copper layer are both isosceles trapezoids.
9. The asymmetric copper thick laminated PCB structure according to claim 1, characterized in that: When observed from a perspective perpendicular to the plane where the copper laminate (1) is located, the copper laminate (1) is at least partially provided with the thick copper layer, and SMT patch components are arranged corresponding to the thick copper layer; within a unit area, the wiring density of the thick copper layer is greater than the wiring density of the thin copper layer.
10. The asymmetric copper thick laminated PCB structure according to claim 1, characterized in that: The thickness of each prepreg sheet (2) is equal.
11. A method for preparing an asymmetric copper thick laminated PCB, used for manufacturing the asymmetric copper thick laminated PCB structure according to any one of claims 1 to 10, characterized in that: include: Step S1, chemical copper plating: depositing chemical copper on the surface of the outermost copper laminate (1); Step S2, electroplating: coating the surface of the chemical copper with an electroplating layer by electroplating; Step S3, film pasting: pasting a photosensitive dry film on the side of the electroplated layer facing away from the copper laminate (1); Step S4, exposure to light: placing the photosensitive dry film under ultraviolet light, so that the photosensitive dry film forms a circuit pattern; Step S5, film stripping: stripping the photosensitive dry film in step S3; Step S6, etching: partially etching the chemical copper, the electroplating layer, and the copper laminate (1), and the remaining portions of the chemical copper, the electroplating layer, and the copper laminate (1) form a circuit matching the circuit pattern; Wherein, the copper laminate (1) is thickened in the step S2.