Processing method for preventing electrochemical migration of Hall switch circuit board
Through laser cutting and fiberglass mat semi-cured sheet lamination technology, the electrochemical migration problem of Hall switch circuit boards is solved, material utilization and production efficiency are improved, and cost is reduced.
Patent Information
- Application Number
- CN202410951360.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2024-11-08
AI Technical Summary
Hall switch circuit boards are prone to electrochemical migration problems during use, resulting in low material utilization and high cost, and it is difficult for the existing technology to effectively solve this problem.
Using laser cutting technology to form a cutting groove between the holes of Hall switch parts, and laminated with a glass fiber mat semi-cured sheet to break the glass fiber bundle in the insulating layer to avoid electrochemical migration. Combined with ultrasonic scanning microscope detection, ensure that the resin is filled without filling The hole is followed by CNC drilling and subsequent processes.
It effectively improves the electrochemical migration resistance of Hall switch circuit board, restores material utilization of more than 85%, reduces material application costs, and improves production efficiency.
Smart Images

Figure CN118921891A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to circuit board processing technology, and in particular to a processing method for preventing electrochemical migration of a Hall switch circuit board. Background Art
[0002] Voltage sensors are used in motor variable speed drives, industrial power supplies, AC / DC converters, computer uninterruptible power supply systems, automotive applications, renewable energy and other fields. They use closed-loop Hall effect technology and have an application range of 100-4000V for DC and AC pulse voltages. Such devices have circuit boards with Hall switch components, and their wave soldered switch components contain Hall ICs, which have built-in Hall elements. When current flows into this Hall element, the magnetic field, i.e., the magnet, is brought close to this IC at a right angle to the current flow direction. The main charged particles of the current will be affected by the Lorentz force. According to the Lorentz force, when the current and the magnetic field are at right angles, a voltage, i.e., the Hall voltage, is also called the Hall effect. After the Hall IC detects this generated voltage, it detects the presence of the magnetic field, i.e., the magnet. The output voltage gradually increases in proportion to the magnetic flux density. The Hall voltage will continue to be applied to the switch welding parts, forming a bias voltage on the pins of different networks, causing CAF, i.e., electrochemical migration, to occur in the PTH holes of different pins on the circuit board. Summary of the invention
[0003] In order to overcome the above-mentioned defects, the present application provides a processing method for preventing electrochemical migration of a Hall switch circuit board, which can effectively improve the CAF resistance of the circuit board equipped with Hall switch components, improve the utilization rate of the substrate material, and reduce the application cost of the material.
[0004] The technical solution adopted by this application to solve its technical problems is:
[0005] A processing method for preventing electrochemical migration of a Hall switch circuit board comprises the following steps:
[0006] Cutting: Cutting out the substrate of preset size, the substrate includes an insulating layer and a copper foil layer pressed onto the insulating layer;
[0007] Inner layer: the inner layer circuit is made on the substrate to obtain the core board;
[0008] Laser cutting: Positioning the inner target point, using a carbon dioxide laser to form a cutting groove between two adjacent holes of the preset Hall switch parts, and the cutting groove breaks the glass fiber bundle in the insulating layer;
[0009] Lamination: The substrate is layered with a glass fiber mat prepreg to obtain a multilayer board, wherein the cutting groove is filled with resin in the glass fiber mat prepreg. The glass fiber mat is made by a non-woven process, and the glass fibers in the glass fiber mat are irregularly arranged and cannot form channels, which can effectively avoid the problem of electrochemical migration;
[0010] SAT test: Use ultrasonic scanning microscope to test the cutting groove to ensure that the cutting groove is filled with resin;
[0011] Drilling: CNC drilling of multilayer boards to process all via holes, Hall switch part holes and positioning holes;
[0012] Post-process: electroplating → dry film → etching → AOI → solder mask → text → molding → electrical testing → inspection → OSP → packaging to get the finished circuit board.
[0013] Optionally, in the laser cutting step, the working conditions of the carbon dioxide laser are: laser size: 8 mil pulse width, energy: 5-6 mj, laser: 4 shots.
[0014] Optionally, in the laser cutting step, the size of the cutting groove is: length*width is 0.8±0.1mm*0.15±0.05mm. When the thickness of the core board is ≤0.2mm, single-sided ablation is adopted. When the thickness of the core board is 0.2-0.5mm, double-sided ablation is adopted.
[0015] Optionally, in the pressing step, the pressing press program parameters are: a 5±0.5mm high temperature resistant buffer pad is placed between the carrier plate and the steel plate, the upper pressure point is 80±5°C, the maximum pressure is 300±20PSI, the maximum material temperature is 180±20°C, and when the material temperature is 150°C, it is maintained for 83±5min, the temperature rise time is 40±5min, and the heating rate is 1.5±0.2°C / min.
[0016] Optionally, in the lamination step, the glass fiber mat prepreg has a glue content of ≥55wt%, and the glass fiber mat prepreg is purchased from Nan Ya Company with a brand name of NPG-150BM.
[0017] The beneficial effects of the present application are as follows: after the inner layer graphics processing is completed, the processing method adopts laser cutting to form cutting grooves for the positions of the holes of the Hall switch parts, thereby disconnecting the glass fiber warp and weft lines in the insulating layer, and using glass fiber mat semi-cured sheet materials during lamination, thereby avoiding the CAF risk of glass fiber bundles; the present processing method can overcome the CAF quality problem and restore the layout utilization rate to more than 85%, the utilization rate can be increased by about 30%, and the comprehensive cost can be reduced by more than 18%. The present application can effectively improve the CAF resistance of circuit boards equipped with Hall switch components, and improve the utilization rate of substrate materials, reduce the application cost of materials, and improve the production efficiency of circuit boards. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 This is a simplified diagram of the circuit board after drilling in this application. DETAILED DESCRIPTION
[0019] The following will be combined with the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0020] A processing method for preventing electrochemical migration of a Hall switch circuit board comprises the following steps:
[0021] Cutting: cutting out a substrate of a preset size, the substrate comprising an insulating layer and a copper foil layer laminated to the insulating layer; the insulating layer is composed of epoxy resin and glass fiber cloth, and the glass fiber cloth comprises glass fiber bundles;
[0022] Inner layer: the inner layer circuit is made on the substrate to obtain the core board;
[0023] Laser cutting: With the inner target point positioned, a carbon dioxide laser is used to form a cutting groove between two adjacent holes of the preset Hall switch parts, and the cutting groove breaks the glass fiber bundle in the insulating layer; with the inner target point positioned, the positioning accuracy can be controlled within ±0.05mm, and the laser cutting process is simple, which can efficiently cut off the glass fiber bundle in the core board, avoiding the wick caused by the cutting of glass fiber cloth in the subsequent drilling process, which further derives the CAF failure problem;
[0024] Lamination: The substrate is layered with a glass fiber mat prepreg to obtain a multilayer board, wherein the cutting groove is filled with resin in the glass fiber mat prepreg. The glass fiber mat is made by a non-woven process, and the glass fibers in the glass fiber mat are irregularly arranged and cannot form a channel, which can effectively avoid the problem of electrochemical migration. The glass fiber mat prepreg includes glass fiber and epoxy resin. The epoxy resin is filled in the cutting groove to effectively maintain the disconnected state of the glass fiber bundle in the insulating layer.
[0025] SAT test: Use ultrasonic scanning microscope to test the cutting groove to ensure that the cutting groove is filled with resin. SAT is: Scanning Acoustic Tomography. Use SAT to confirm the effect of cutting groove resin filling and ensure that there is no hollow cutting groove.
[0026] Drilling: CNC drilling is performed on the multilayer board to process all the via holes, Hall switch component holes and positioning holes; after drilling, the Hall switch component holes need to be sliced and analyzed to check the glass fiber disconnection quality and glue filling quality between the Hall component holes of different networks;
[0027] Post-process: electroplating → dry film → etching → AOI → solder mask → text → molding → electrical testing → inspection → OSP → packaging, and the finished circuit board is obtained. The post-process is a conventional process. Figure 1 The circuit board after drilling is shown. The circuit board is a 4-layer board. The substrate is a FR-4 copper-clad substrate. The insulating layer uses a conventional FR-4 prepreg. Two adjacent Hall switch part holes are shown in the figure. A laser cutting groove is formed between the two Hall switch part holes, and laminated using a glass fiber mat prepreg.
[0028] In this processing method, a laser cutting groove is used in the insulating layer to cut off the glass fiber bundles in the insulating layer, so as to avoid the wick phenomenon caused by cutting the glass fiber cloth in the subsequent drilling process, which further derives the electrochemical migration, i.e., CAF failure problem; the wick phenomenon is simply that after the glass fiber bundle is cut by the drill bit, it will be directly exposed on the hole wall. In the subsequent electroplating process, copper will be plated on the hole wall. During the copper plating process, because the glass fiber bundle is broken up, copper will penetrate into it, further forming a phenomenon similar to a wick.
[0029] After the inner layer graphics processing is completed, this processing method uses laser cutting to form a cutting groove for the position of the Hall switch part hole, thereby disconnecting the glass fiber warp and weft in the insulating layer, and using glass fiber mat semi-cured sheet materials during lamination, thereby avoiding the CAF risk of glass fiber bundles; this processing method can overcome the CAF quality problem and restore the layout utilization rate to more than 85%, the utilization rate can be increased by about 30%, and the comprehensive cost can be reduced by more than 18%. This application can effectively improve the CAF resistance of circuit boards equipped with Hall switch components, improve the utilization rate of substrate materials, reduce the application cost of materials, and improve the production efficiency of circuit boards.
[0030] In the laser cutting step, the working conditions of the carbon dioxide laser are: laser size: 8mil pulse width, energy: 5-6mj, laser: 4 shots.
[0031] In the laser cutting step, the size of the cutting groove is: length*width is 0.8±0.1mm*0.15±0.05mm. When the thickness of the core board is ≤0.2mm, a single-sided ablation method is used. When the thickness of the core board is 0.2-0.5mm, a double-sided ablation method is used. The maximum thickness of the core board processed by laser cannot exceed 0.5mm to ensure that the glass fiber bundle can be broken.
[0032] In the pressing step, the pressing press program parameters are: a 5±0.5mm high temperature resistant cushion is placed between the carrier and the steel plate, the upper pressure point is 80±5°C, the maximum pressure is 300±20PSI, the maximum material temperature is 180±20°C, and the material temperature is maintained at 150°C for 83±5min, the temperature rise time is 40±5min, and the temperature rise rate is 1.5±0.2°C / min. In a possible implementation, a 5mm high temperature resistant cushion is placed between the carrier and the steel plate, the upper pressure point is 80°C, the maximum pressure is 300PSI, the maximum material temperature is 180°C, the material temperature is maintained at 150°C for 83min, the temperature rise time is 40min, and the temperature rise rate is 1.5°C / min.
[0033] In the lamination step, the glass fiber mat semi-cured sheet has a glue content of ≥55wt%. The glass fiber mat semi-cured sheet is purchased from Nan Ya Company with a brand name of NPG-150BM.
[0034] Nan Ya Company is Nan Ya Electronic Materials (Kunshan) Co., Ltd. The glass fiber mat semi-cured sheet is a newly developed product of Nan Ya Company. The glass fiber mat is made by non-woven technology. The glass fiber fibers in the glass fiber mat are irregularly arranged and cannot form channels, which can effectively avoid the problem of electrochemical migration.
[0035] Example 1: Figure 1 As shown, a processing method for preventing electrochemical migration of a Hall switch circuit board comprises the following steps:
[0036] Step 1: Cutting: Cutting out a substrate of a preset size, the substrate comprising an insulating layer and a copper layer pressed onto the insulating layer;
[0037] Step 2: Inner layer: Complete the production of inner layer circuits on the substrate to obtain the core board;
[0038] Step 3: Laser cutting: Position the inner target point and use a carbon dioxide laser to form a cutting groove between two preset adjacent Hall switch part holes. The width and length of the cutting groove are 0.15mm*0.8mm. The cutting groove breaks the glass fiber bundle in the insulating layer. The conditions of the carbon dioxide laser are: laser size: 8mil pulse width, energy: 5-6mj, laser: 4 shots;
[0039] Step 4: Lamination: Use glass fiber mat prepreg to add layers to the substrate to obtain a multilayer board, wherein the lamination conditions are: a 5mm high temperature resistant cushion is placed between the carrier and the steel plate, the upper pressure point is 80°C, the maximum pressure is 300PSI, the maximum material temperature is 180°C, the material temperature is maintained at 150°C for 85min, the temperature rise time is 40min, and the heating rate is 1.5°C / min;
[0040] Step 5: SAT test: Use an ultrasonic microscope to test the cutting groove to ensure that the cutting groove is filled with resin;
[0041] Step 6: Drilling: CNC drilling is performed on the multilayer board to process all the via holes, Hall switch component holes and positioning holes; after drilling, the Hall switch component holes need to be sliced and analyzed to check the glass fiber disconnection quality and glue filling quality between the Hall component holes of different networks;
[0042] Step 7: Post-processing: The multilayer board after drilling will go through the following processes in sequence: electroplating → dry film → etching → AOI → solder mask → text → molding → electrical testing → inspection → OSP → packaging to obtain the finished circuit board.
[0043] It should be noted that, for those skilled in the art, several modifications and improvements can be made without departing from the concept of the present application, and these modifications and improvements are all within the scope of protection of the present application. Therefore, the scope of protection of the patent of the present application shall be subject to the attached claims.
Claims
1. A processing method for preventing electrochemical migration of a Hall switch circuit board, characterized in that: The steps include: Cutting: Cutting out the substrate of preset size, the substrate includes an insulating layer and a copper foil layer pressed onto the insulating layer; Inner layer: the inner layer circuit is made on the substrate to obtain the core board; Laser cutting: Positioning the inner target point, using a carbon dioxide laser to form a cutting groove between two adjacent holes of the preset Hall switch parts, and the cutting groove breaks the glass fiber bundle in the insulating layer; Lamination: The substrate is layered with a glass fiber mat prepreg to obtain a multilayer board, wherein the cutting groove is filled with resin in the glass fiber mat prepreg. The glass fiber mat is made by a non-woven process, and the glass fibers in the glass fiber mat are irregularly arranged and cannot form channels, which can effectively avoid the problem of electrochemical migration; SAT test: Use ultrasonic scanning microscope to test the cutting groove to ensure that the cutting groove is filled with resin; Drilling: CNC drilling of multilayer boards to process all via holes, Hall switch part holes and positioning holes; Post-process: electroplating → dry film → etching → AOI → solder mask → text → molding → electrical testing → inspection → OSP → packaging to get the finished circuit board.
2. The processing method for preventing electrochemical migration of a Hall switch circuit board according to claim 1, characterized in that: In the laser cutting step, the working conditions of the carbon dioxide laser are: laser size: 8mil pulse width, energy: 5-6mj, laser: 4 shots.
3. The processing method for preventing electrochemical migration of a Hall switch circuit board according to claim 1, characterized in that: In the laser cutting step, the size of the cutting groove is: length*width is 0.8±0.1mm*0.15±0.05mm. When the thickness of the core board is ≤0.2mm, single-sided ablation is adopted. When the thickness of the core board is 0.2-0.5mm, double-sided ablation is adopted.
4. The processing method for preventing electrochemical migration of a Hall switch circuit board according to claim 1, characterized in that: In the pressing step, the pressing press program parameters are: a 5±0.5mm high temperature resistant buffer pad is placed between the carrier plate and the steel plate, the upper pressure point is 80±5°C, the maximum pressure is 300±20PSI, the maximum material temperature is 180±20°C, and when the material temperature is 150°C, it is maintained for 83±5min, the temperature rise time is 40±5min, and the heating rate is 1.5±0.2°C / min.
5. The processing method for preventing electrochemical migration of a Hall switch circuit board according to claim 1, characterized in that: In the lamination step, the glass fiber mat semi-cured sheet has a glue content of ≥55wt%. The glass fiber mat semi-cured sheet is purchased from Nan Ya Company with a brand name of NPG-150BM.