Fe monatomic composite catalytic membrane as well as preparation method and application thereof

Through the preparation and application of Fe single-atom composite catalytic membrane, the problem of low removal efficiency of new antibiotic pollutants in the prior art is solved, and efficient removal of antibiotic pollutants, especially BPA and COD, significantly improving the efficiency of wastewater treatment .

CN118925802AInactive Publication Date: 2024-11-12SHANGHAI ACADEMY OF ENVIRONMENTAL SCIENCES

Patent Information

Application Number
CN202410979320.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-11-12
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The prior art is difficult to efficiently remove pollution from new antibiotic pollutants entering water from livestock and poultry manure, especially sulfonamide and tetracycline antibiotics. The removal rate of conventional sewage treatment processes is insufficient and targeted control technology is lacking.

Method used

The preparation method of Fe single atom composite catalytic film is adopted, and the composite film is prepared by the combination of Fe-Co double single atom catalyst with polyacrylonitrile and PVDF, and the composite film is prepared by electrospinning technology, and catalytic with high activity and selectivity is formed by annealing treatment. Membrane, used to remove antibiotic contaminants.

Benefits of technology

It has achieved efficient removal of antibiotic pollutants, especially the removal rate of BPA reaches 98%, and the COD removal rate reaches 86%, which has significantly improved the efficiency of wastewater treatment and reduced water pollution.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118925802A_ABST
    Figure CN118925802A_ABST
Patent Text Reader

Abstract

The invention discloses a Fe monatomic composite catalytic membrane as well as a preparation method and application thereof, and the preparation process comprises the following steps: preparing a PAN (polyaniline)-Fe-Co / NC (nitrocellulose) membrane by adopting a Fe-Co double monatomic catalyst and adopting an electrostatic spinning technology, then annealing, and then coating the surface with a PVDF (polyvinylidene fluoride) membrane by adopting the electrostatic spinning technology to form the monatomic composite catalytic membrane. When the monatomic composite catalytic membrane is applied to sewage treatment, antibiotic pollutants in livestock breeding wastewater can be effectively degraded, and the monatomic composite catalytic membrane is of great significance to environmental protection.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of agricultural environmental engineering and organic wastewater treatment, and more specifically to an Fe single-atom composite catalytic membrane and a preparation method and application thereof. Background Art

[0002] In recent years, with the continuous increase in drug use and the innovation and progress of compound trace detection technology, more and more human and veterinary drugs have been detected in the environment, especially in water bodies. After long-term enrichment, high-concentration drug residues will cause serious toxic stress to organisms, and then have an adverse effect on the health of the ecosystem. Among them, antibiotics, as a new type of pollutants controlled by international conventions, have attracted much attention at home and abroad. my country is not only a major producer of antibiotics, but also ranks first in the world in annual consumption. It is mainly used in economically developed areas. Among them, the antibiotics used for livestock and poultry disease control are mainly sulfonamides (Sulfonamide), tetracyclines (Tetracyclines) and other types of drugs. In 2021, the national use of veterinary antibacterial drugs was equivalent to about 32,500 tons in pure amount. Most of these antibiotics cannot be completely absorbed by animals. Antibiotics excreted from the body of animals in the form of parent or metabolites account for about 40% to 90% of the amount of drugs, and will enter the surface or groundwater bodies through farmland consumption, surface runoff and infiltration, etc., causing harm to the water ecology.

[0003] Antibiotics have large molecular weight, are difficult to degrade, and have biological toxicity. At present, the removal rate of antibiotics by conventional anaerobic treatment processes for pig farm wastewater is less than 30%. Due to the lack of antibiotic control technical specifications and emission standards for the return of manure to farmland, there are few reports on the application of related control technologies in China. The application of related antibiotic management technologies is mostly seen in industrial fields such as sewage treatment plants and pharmaceutical factories.

[0004] Advanced oxidation technology generates reactive oxygen species (ROS) with strong oxidative properties, such as hydroxyl radicals ( · OH), sulfate radical (SO4 ·- ), singlet oxygen ( 1 O2), etc., can attack antibiotics in organic wastewater. Among them, single-atom catalysts achieve ultra-high catalytic activity by utilizing the minimum size effect of metals to obtain maximum atomic utilization and fully expose catalytic active centers. In recent years, they have been gradually applied to the field of environmental water restoration and have broad practical application prospects in the removal of antibiotics from livestock and poultry wastewater.

[0005] In the context of attaching great importance to the control of new pollutants, how to selectively remove new antibiotic pollutants based on conventional processes for resource utilization of manure and sewage has become a new scientific proposition in the field of green breeding and circular agricultural development. Summary of the invention

[0006] In view of this, in order to achieve the above-mentioned purpose, the present invention provides a method for preparing a Fe single-atom composite catalytic film and its application in antibiotic-contaminated wastewater, specifically adopting the following technical scheme:

[0007] First, the present invention provides a method for preparing a Fe single-atom composite catalytic film, comprising the following steps:

[0008] (1) The Fe-Co double single atom catalyst was added to DMF and fully dispersed by ultrasonication, and then polyacrylonitrile was added, heated and stirred to obtain a spinning solution, and then the PAN@Fe-Co / NC membrane was prepared by electrospinning technology;

[0009] (2) annealing the film obtained in step (1);

[0010] (3) adding PVDF to a mixed solution of DMAc and acetone and stirring to obtain a mixed solution, and then applying the mixed solution to the surface of the membrane after annealing in step (2) by using an electrospinning technique to form a composite catalytic membrane.

[0011] Preferably, in step (1), the mass ratio of the Fe-Co double single atom catalyst to polyacrylonitrile is 1:3, and the mass volume ratio of the Fe-Co double single atom catalyst to DMF is 0.5 mg / mL.

[0012] Preferably, the heating and stirring in step (1) is performed at a temperature of 50° C. and for 6 hours.

[0013] Preferably, the electrospinning technical parameters in step (1) are: voltage 25 kV, boost rate 1 mL / h, and distance from needle tip to receiver 15 cm.

[0014] Preferably, the annealing treatment in step (2) is: heating to 900° C. at a heating rate of 5° C. / min and maintaining for 3 hours, followed by natural cooling to room temperature.

[0015] Preferably, in the mixed solution of DMAc and acetone in step (3), the volume ratio of DMAc:acetone=8:2, and the amount of PVDF added is 10% of the mass of the mixed solution.

[0016] Preferably, the stirring time in step (3) is 12 h.

[0017] Preferably, the electrospinning technical parameters in step (3) are: voltage 16 kV, boost rate 0.5 mL / h, and distance from needle tip to receiver 15 cm.

[0018] In addition, the present invention also provides an Fe single-atom composite catalytic film prepared by the method described in the above technical solution.

[0019] And the Fe single-atom composite catalytic film prepared by the method described in the above technical scheme or the use of the Fe single-atom composite catalytic film in degrading new pollutants in wastewater.

[0020] The new pollutants are antibiotics used in animal husbandry, specifically sulfonamides, tetracyclines, etc.

[0021] It can be seen from the above technical solutions that, compared with the prior art, the present invention discloses a Fe single-atom composite catalytic film and a preparation method and application thereof, which have the following beneficial effects:

[0022] This patent proposes a revolutionary Fe single-atom composite catalytic membrane technology, which shows unprecedented high efficiency in treating organic matter BPA. Specifically, this catalytic membrane can remove up to 98% of BPA in just 30 minutes, showing the ability to remove harmful pollutants extremely quickly. In addition, it has also achieved remarkable results in the removal of chemical oxygen demand (COD), with a removal rate of up to 86%, effectively reducing the degree of pollution in wastewater. The design of the Fe single-atom composite catalytic membrane makes full use of the high activity and high selectivity of single-atom catalysts, and achieves efficient degradation of BPA by carefully regulating its structure and composition. At the same time, its unique membrane structure ensures the efficient progress of the catalytic reaction and further improves the treatment efficiency. The successful application of this technology not only provides strong technical support for solving water pollution problems, but also promotes technological progress in the field of environmental governance. By using this catalytic membrane, BPA and COD in wastewater can be effectively removed in a relatively short time, significantly improving the efficiency and effect of wastewater treatment, which is of great significance for protecting water resources and improving environmental quality. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the provided drawings without paying creative work.

[0024] Figure 1 is a schematic diagram of a membrane filter;

[0025] Figure 2 Schematic diagram of the preparation process of Fe single atom composite catalytic film;

[0026] Figure 3 This is the SEM image of the Fe single atom composite catalytic film;

[0027] Figure 4 It is the BPA concentration-time variation graph;

[0028] Figure 5 It is the actual wastewater membrane flux and conductivity-time variation spectrum;

[0029] Figure 6 It is the actual wastewater COD removal spectrum. DETAILED DESCRIPTION

[0030] The technical solution of the present invention will be clearly and completely described below in conjunction with the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0031] (1) 5 mg of Fe-Co double single atom catalyst was added to 10 mL of DMF and dispersed by ultrasonication for 2 h. Then, 15 mg of polyacrylonitrile (PAN) was added and stirred at 50 °C for 6 h. Then, PAN@Fe-Co / NC membrane was prepared by electrospinning technology. The operating parameters were adjusted as follows: voltage 25 kV, boost rate 1 mL / h, and distance from needle tip to receiver 15 cm.

[0032] (2) annealing the film obtained in step (1) to obtain a PAN@Fe-Co / NC double monoatomic film; the annealing is carried out in a tubular annealing furnace, wherein the temperature in the furnace is raised to 900° C. at a heating rate of 5° C. / min, maintained for 3 h, and then naturally cooled to room temperature;

[0033] (3) 10% PVDF was added to a solution of DMAc and acetone (volume ratio 8:2) and stirred for 12 h to obtain a mixed solution; the mixed solution was coated on the annealed PAN@Fe-Co / NC double single atom film in step (2) by electrospinning technology to form a single atom composite catalytic film, and the operating parameters were adjusted as follows: voltage 16 kV, boost rate 0.5 mL / h, and distance from needle tip to receiver 15 cm.

[0034] like Figure 2 As shown in Figure 2, after two stages of electrospinning, a PAN@FeCo / NC@PVDF membrane with a black hydrophilic layer (PAN@FeCo / CN0) and a white hydrophobic layer (PVDF) was generated. The cross-sectional morphology showed that the continuous overlap of nanofibers resulted in interconnected pores throughout the membrane thickness; Figure 3 As described above, the two layers show a three-dimensional open framework, although their fiber morphologies are different. The fibers in the PVDF layer are relatively rough due to the presence of beads, which can increase the roughness and thus enhance the hydrophobicity.

[0035] The purpose of this experiment is to evaluate the desalination performance of different membranes using a laboratory-scale membrane distillation (MD) system.2 The membrane (6 cm long and 3 cm wide) was firmly sandwiched between two chambers, which were used to store the feed liquid (wastewater) and the permeate (pure water). In order to ensure the uniform flow and circulation of the liquid during the experiment, the feed liquid and the permeate were circulated through a peristaltic pump system, and the flow rate was controlled at 0.5 L / min. Figure 1 As shown, the prepared single-atom composite catalytic membrane was fixed in a membrane filter, and the circulation pump was turned on for 10 min (0.5 L / h) and added to the wastewater to be treated containing BPA (20 mg / L), and circulated for 10 min to establish adsorption-desorption equilibrium;

[0036] PMS solution (0.2 g / L) was added to the wastewater to be treated to induce a Fenton-like reaction to remove BPA in the wastewater. The experimental results showed that as the reaction time progressed, 98% of BPA was completely degraded ( Figure 4 ), BPA in water can be completely degraded after 30 minutes of reaction; Figure 5 It shows that as the reaction time progresses, the membrane flux always maintains a high level (15kg / m 2 h). Figure 6 The data results show that the PVDF membrane (commercial membrane) has a COD removal rate of about 1% for raw water and a COD removal rate of about 75% for pure water; while the composite catalytic membrane has a COD removal rate of about 50% for raw water and a COD removal rate of about 86% for pure water.

[0037] In this specification, each embodiment is described in a progressive manner, and each embodiment focuses on the differences from other embodiments, and the same and similar parts between the embodiments can be referred to each other. The above description of the disclosed embodiments enables professionals and technicians in this field to implement or use the present invention. Various modifications to these embodiments will be obvious to professionals and technicians in this field, and the general principles defined herein can be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to these embodiments shown in this article, but will comply with the widest range consistent with the principles and novel features disclosed herein.

Claims

1. A method for preparing a Fe single-atom composite catalytic film, characterized in that: The following steps are involved: (1) The Fe-Co double single atom catalyst was added to DMF and fully dispersed by ultrasonication, and then polyacrylonitrile was added, heated and stirred to obtain a spinning solution, and then the PAN@Fe-Co / NC membrane was prepared by electrospinning technology; (2) annealing the film obtained in step (1); (3) adding PVDF to a mixed solution of DMAc and acetone and stirring to obtain a mixed solution, and then applying the mixed solution to the surface of the membrane after annealing in step (2) by using an electrospinning technique to form a composite catalytic membrane.

2. The method for preparing a Fe single atom composite catalytic film according to claim 1, characterized in that: In step (1), the mass ratio of the Fe-Co double single atom catalyst to polyacrylonitrile is 1:3, and the mass volume ratio of the Fe-Co double single atom catalyst to DMF is 0.5 mg / mL.

3. The method for preparing a Fe single atom composite catalytic film according to claim 1, characterized in that: The heating and stirring temperature in step (1) is 50° C. and the time is 6 h.

4. The method for preparing a Fe single atom composite catalytic film according to claim 1, characterized in that: The electrospinning technical parameters in step (1) are: voltage 25 kV, boost rate 1 mL / h, and distance from needle tip to receiver 15 cm.

5. The method for preparing a Fe single atom composite catalytic film according to claim 1, characterized in that: The annealing treatment in step (2) is as follows: heating to 900°C at a rate of 5°C / min and maintaining for 3 hours, followed by natural cooling to room temperature.

6. The method for preparing a Fe single atom composite catalytic film according to claim 1, characterized in that: In step (3), the volume ratio of DMAc and acetone in the mixed solution is DMAc:acetone=8:2, and the amount of PVDF added is 10% of the mass of the mixed solution.

7. The method for preparing a Fe single atom composite catalytic film according to claim 1, characterized in that: The stirring time in step (3) is 12 h.

8. The method for preparing a Fe single atom composite catalytic film according to claim 1, characterized in that: The electrospinning technical parameters in step (3) are: voltage 16 kV, boost rate 0.5 mL / h, and distance from needle tip to receiver 15 cm.

9. An Fe single atom composite catalytic film prepared by the method according to any one of claims 1 to 8.

10. Use of the Fe single-atom composite catalytic film prepared by the method according to any one of claims 1 to 8 or the Fe single-atom composite catalytic film according to claim 9 in degrading wastewater pollutants.

Citation Information

Patent Citations

  • Double-layer distillation membrane with monatomic catalysis function as well as preparation method and application of double-layer distillation membrane

    CN117323840A

Cited By

  • In-situ self-cleaning cathode monatomic iron-carbon-based electroactive membrane and preparation method and application thereof

    CN121317973A

  • In-situ self-cleaning cathode monatomic iron-carbon-based electroactive film, and preparation method and application thereof

    CN121317973B