Machining method of 170 supercharger ZB axial bearing

By employing a machining method involving multiple precision turnings and positioning clamping, the problem of dimensional deviations in ZB bearings after precision turning was solved, achieving high-precision machining and stability of the bearings and ensuring dimensional accuracy and parallelism.

CN118926844AActive Publication Date: 2024-11-12CHONGQING JIANGJIN SHIPBUILDING IND

Patent Information

Application Number
CN202411194822.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-29
Publication Date
2024-11-12
Estimated Expiration
2044-08-29

AI Technical Summary

Technical Problem

In the existing technology, the ZB axial bearing of the 170 turbocharger has a problem of dimensional deviation when the tooling pressure plate is removed and measured again after the final precision machining process. In particular, since the dimensional boundary is two planes, the deviation is unstable after measuring multiple points.

Method used

The process employs multiple precision turning and positioning clamping steps, including rough turning, two and a half precision turnings, milling of inclined grooves, center line marking by a fitter, positioning using internal holes, drilling and milling of oil wedges using a five-axis machining equipment, to ensure that the parallelism of the clamping surfaces is within 0.004. Precision machining is then performed using a three-jaw chuck and a five-axis machine.

Benefits of technology

This effectively solved the deformation problem caused by the clamping surface, ensuring the dimensional stability and parallelism of the ZB bearing after machining, reducing the occurrence of dimensional deviations, and improving machining accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118926844A_ABST
    Figure CN118926844A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of supercharger manufacturing, in particular to a machining method of a 170 supercharger ZB axial bearing, which comprises the following steps: marking a center line of a workpiece by a bench worker, aligning according to the center line, and then milling an oil groove and drilling; the ZB axial bearing workpiece is positioned through the machined inner hole, groove milling and drilling are conducted again, and milling burrs are removed; three jaws are used for clamping the large outer circle of the ZB axial bearing workpiece, then first-time finish turning machining is conducted on the workpiece, and finish turning machining is conducted on the two end faces subjected to semi-finish turning machining; second-time finish turning is conducted, the two end faces subjected to first-time finish turning are clamped, and after alignment, the large-appearance outline of the part is obtained through finish turning; alignment of the workpiece is conducted, and then third-time finish turning is conducted; after the chute milling and the drilling are completed, a finish turning process is added, and the mutual parallelism of two surfaces of a positioning and clamping surface required by a finish turning tool is required to be within 0.004 mm, so that the problem of deformation of the positioning and clamping surface caused by the chute milling and the drilling is effectively solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of supercharger manufacturing, and in particular to a processing method for a 170 supercharger ZB axial bearing. Background Art

[0002] The 170 supercharger is an internal support, sliding bearing, radial flow supercharger. The ZB axial bearing part is an important part of this type of supercharger. It has many important characteristics. It plays the role of supporting the turbine shaft rotor assembly, protecting the rotating support part, and transmitting the load in the supercharger. At the same time, it also plays a vital role in the operation stability of the whole system. The ZB axial bearing is located between the compressor impeller and the bearing shell. The parts that have a matching relationship with it include: compressor shell, sealing sleeve (important part), support bearing (important part), and bearing shell (important part). The ZB axial bearing passes through the turbine shaft and matches the outer circle of the sealing sleeve. The pin hole on the body and the pin hole on the bearing shell are connected and fixed by locating pins. Its inner hole is assembled with the outer circle of the support bearing, and the end face of the ZB axial bearing is flush with the end face of the bearing shell. The processing route of the ZB axial bearing is rough turning to remove more excess of the bar material, milling the inclined groove, turning the outer positioning surface, drilling, milling the groove, fine turning the outer shape, fine turning the groove and bottom, drilling, and milling the oil wedge. Chemical composition analysis of the ZB axial bearing material CuZn40Al2: The copper content is 57%-60%, copper has good plasticity, and its deformation resistance is better than aluminum but much less than steel and iron; the aluminum content is 2.5%-3.5%, aluminum can improve the strength and hardness of copper alloys, and corrosion resistance; the nickel content is 2%-3%, which has good plasticity; it also contains less than 0.5% iron, less than 0.1% lead, and less than 0.9% impurities, and the rest is zinc, which has good plasticity. In summary, the ZB axial bearing material has good plasticity, and its hardness is relatively high among copper alloys, but much lower than steel materials.

[0003] The large end face is positioned tightly and the small end face is pressed tightly. Because the large and small end faces are poorly parallel to each other, and in order to find the correct runout, the small end face is pressed tightly, causing the small end face to deform. In this way, when finishing, the small end face is used as the starting point for machining. Axial dimension (processed according to the intermediate tolerance). Measured in the clamped state on the machine tool Dimensions, inspection passed.

[0004] However, in the above-mentioned prior art, during the final finishing process, after the tooling pressure plate is removed, the size will be out of tolerance when measured again. In addition, since the dimension boundary is two planes, after measuring multiple points, the size will be unstable. Summary of the invention

[0005] The purpose of the present invention is to provide a processing method for the ZB axial bearing of a 170 supercharger, which solves the problem in the prior art that during the final finishing process, after the tooling pressure plate is removed, the size will be out of tolerance when measured again, and because the size boundary is two planes, there is still an unstable out-of-tolerance situation after measuring multiple points.

[0006] To achieve the above object, the present invention provides a method for processing a 170 supercharger ZB axial bearing, comprising the following steps:

[0007] Rough turning is performed on the ZB axial bearing workpiece to remove most of the excess;

[0008] Perform two semi-finishing turning operations on the ZB axial bearing workpiece to produce two end faces;

[0009] Milling of bevel grooves on ZB axial bearing workpieces;

[0010] The fitter marks the center line of the workpiece, aligns it according to the center line, and then mills the oil groove and drills the hole;

[0011] Use the processed inner hole to position the ZB axial bearing workpiece, and then perform milling and drilling again, and then remove the milling burrs;

[0012] Use three jaws to clamp the large outer circle of the ZB axial bearing workpiece, then perform the first finish turning of the workpiece, and perform finish turning on the two end faces of the semi-finish turning;

[0013] Carry out the second finishing process, clamp the two end faces of the first finishing process, align them, and finish the outline of the large shape of the part;

[0014] Align the workpiece and then perform the third finishing process;

[0015] Use five-axis machining equipment to perform drilling and oil wedge milling, then remove burrs and clean the workpiece;

[0016] Carry out surface crack inspection on the workpiece, remove the workpiece from the fixture, remove the clamping force, inspect the size, and check if it passes the inspection.

[0017] Among them, in the rough turning of ZB axial bearing workpiece:

[0018] First, clamp the outer circle, and use the general turning CA6140 drilling machine to remove most of the excess, with the spindle speed of 400r / min and the feed of 2mm;

[0019] Then, a general lathe CA6140 is used to drill through holes, turn large outer circles and step holes, and then cut off. The spindle speed is 400r / min and the feed is 2mm.

[0020] Among them, the ZB axial bearing workpiece is processed in two semi-finishing processes:

[0021] First, the CNC lathe QTN200 equipment is used to turn the inner holes and end faces. The inner holes with higher tolerance requirements and the end faces with higher shape and position requirements are left with a margin. The inner holes have a margin of 0.5mm, and the end faces have a margin of 0.2mm. The speed is 800r / min, the feed rate is 0.1-0.2mm, and a 55° turning tool is used for processing;

[0022] Then, the CNC lathe QTN200 equipment is used to process the two end faces and the inner hole. The inner hole is processed in place, and a margin of 0.2mm is left on the two end faces. The speed is 800r / min, the feed rate is 0.1~0.2mm, and a 55° turning tool is used for processing.

[0023] Among them, in the process of milling the inclined groove of the ZB axial bearing workpiece:

[0024] The five-axis machining center C42U is used to mill the bevel grooves and process three 45° bevel notches. The speed is 1000r / min and the cutting depth is 5mm. A Φ10 end mill is used to remove the excess, and then a Φ6 ball head milling cutter is used to mill out the root R3 shape.

[0025] Among them, the fitter marks the center line of the workpiece, aligns it according to the center line, and then performs the steps of milling the oil groove and drilling the hole:

[0026] The fitter uses a marking tool to draw the center line of the workpiece for subsequent alignment; the five-axis machining center C42U is used to mill the notch, drill and ream the hole system, and mill the oil groove to the requirements of the drawing (mill the oil grooves of the shapes shown in the dimensions R2, R3, R1, 1.5, R0.4, 1.5, 6°, and R1.5 according to the drawing), the milling depth is 3mm, the speed is 1000r / min, the Φ4.1 and Φ4.8 drill bits are used to machine the bottom hole, and the reamer 5H7 is used to ream the Φ5 hole for subsequent positioning;

[0027] Use a bench drill, model Z3032, to drill a radial Φ2.4 hole with a cutting depth of 2mm, and a Φ2.85 hole with a cutting depth of 2mm;

[0028] Remove the burrs at the intersection of the Φ4 hole and the Φ2.4 hole, then clean the parts to remove oil and impurities, and finally use the 170Q-05 steel ball pressing tool to press the Φ3 steel ball into the Φ2.85 hole.

[0029] Among them, in the steps of positioning the ZB axial bearing workpiece using the processed inner hole, milling and drilling again, and then removing the milling burrs:

[0030] Use the Φ5 hole reamed out in the above process for positioning, use the milling tool model 170X-08 slotting tool, and use a Φ6 end mill to machine a slot with a width of 6mm and a depth of 7.7mm, with a feed rate of 3mm and a speed of 600r / min, and then remove the milling burrs.

[0031] Among them, in the steps of using three jaws to clamp the large outer circle of the ZB axial bearing workpiece, and then performing the first finishing machining of the workpiece, the two end faces of the semi-finishing machining are finished by finishing machining:

[0032] The lathe model QTN200 was used to machine the two end faces with a size of 6.3mm in the semi-finishing process to 0.05mm, ensuring that the parallelism between the two machined surfaces was 0.004. The tool used was a 55° finishing blade and the spindle speed was 800r / min.

[0033] Among them, in the second finishing process, the two end faces of the first finishing process are clamped, and the contour of the large shape of the part is finished after alignment:

[0034] The model of the numerical turning equipment used is QTN200, and the workpiece turning tool is 170C-15. The two end faces processed in the first fine turning process are clamped, and the contour of the large shape of the workpiece is fine turned after alignment. A 55° turning tool is used, and the spindle speed is 800r / min.

[0035] Among them, in the steps of aligning the workpiece and then performing the third finishing process:

[0036] The model of the numerical turning equipment used is QTN200, and the workpiece turning tool is 170C-16. After aligning the end face runout of the tooling, place the workpiece and press the end face pressure plate. When the outer circle runout of the workpiece is aligned, press the outer pressure plate tightly, remove the end face pressure plate, and perform fine turning as required to turn each end face to the required size.

[0037] Among them, in the steps of using five-axis machining equipment to perform drilling and milling oil wedge processing, then removing burrs and cleaning the workpiece:

[0038] The five-axis machining equipment used is C42U, and the Φ5 hole is expanded to Φ6, the cutting depth is 2mm, the speed is 1000r / min, and the oil wedge is milled by the milling cutter, and the speed is 1200r / min;

[0039] Perform chamfer R1 and clean the parts.

[0040] The invention discloses a processing method for a 170 supercharger ZB axial bearing, which comprises the following steps: performing rough turning on a ZB axial bearing workpiece to remove most of the excess; performing two semi-finishing turning processes on the ZB axial bearing workpiece to process two end faces; performing milling of an inclined groove on the ZB axial bearing workpiece; a fitter marks the center line of the workpiece, aligns the workpiece according to the center line, and then performs milling of an oil groove and drilling of a hole; positioning the ZB axial bearing workpiece by using the processed inner hole, and performing milling of a groove and drilling of a hole again, and then removing milling burrs; using three jaws to clamp the large outer circle of the ZB axial bearing workpiece, and then performing the first fine turning of the workpiece to machine the two end faces processed by the semi-fine turning process. Perform fine turning; perform a second fine turning process, clamp the two end faces of the first fine turning process, and fine turn the outline of the large shape of the part after alignment; align the workpiece, and then perform a third fine turning process; use five-axis processing equipment to perform drilling and oil wedge milling, then remove burrs and clean the workpiece; perform surface crack inspection on the workpiece, remove the workpiece from the tooling, cancel the clamping force, inspect the size, and if the inspection is qualified, add a fine turning process after milling the bevel groove and drilling. The positioning and clamping surfaces required by the fine turning tool require that the parallelism of the two surfaces is within 0.004, which effectively solves the deformation problem of the positioning and clamping surfaces caused by milling the bevel groove and drilling. BRIEF DESCRIPTION OF THE DRAWINGS

[0041] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art are briefly introduced below.

[0042] Figure 1 It is a flow chart of the steps of the processing method of the 170 supercharger ZB axial bearing of the present invention.

[0043] Figure 2 It is a schematic diagram of the structure of 170C-15 of the present invention.

[0044] Figure 3 It is a schematic diagram of the structure of 170C-16 of the present invention.

[0045] 1-ZB axial bearing workpiece, 2-170C-15, 3-170C-16, 4-quick release washer, 5-tooling pressure plate. DETAILED DESCRIPTION

[0046] Embodiments of the present invention are described in detail below. Examples of the embodiments are shown in the accompanying drawings. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present invention, but should not be construed as limiting the present invention.

[0047] See also Figures 1 to 3 The present invention provides a method for processing a 170 supercharger ZB axial bearing, comprising the following steps:

[0048] S1: Rough turning the ZB axial bearing workpiece 1 to remove most of the excess;

[0049] S2: Perform two semi-finishing turning operations on the ZB axial bearing workpiece 1 to produce two end faces;

[0050] S3: milling the bevel groove of the ZB axial bearing workpiece 1;

[0051] S4: The fitter marks the center line of the workpiece, aligns it according to the center line, and then mills the oil groove and drills the hole;

[0052] S5: Positioning the ZB axial bearing workpiece 1 using the processed inner hole, and performing milling and drilling again, and then removing the milling burrs;

[0053] S6: Use three jaws to clamp the large outer circle of the ZB axial bearing workpiece 1, and then perform the first finishing machining of the workpiece, and perform finishing machining on the two end faces of the semi-finishing machining;

[0054] S7: Perform the second finishing process, clamp the two end faces of the first finishing process, align them, and finish the outline of the large shape of the part;

[0055] S8: Align the workpiece and then perform the third finishing process;

[0056] S9: Use five-axis machining equipment to perform drilling and oil wedge milling, then remove burrs and clean the workpiece;

[0057] S10: Check the surface cracks of the workpiece, remove the workpiece from the fixture, remove the clamping force, check the size, and check if it is qualified.

[0058] When using a processing method of a 170 supercharger ZB axial bearing of this embodiment, the ZB axial bearing workpiece 1 is rough-turned to remove most of the excess;

[0059] Perform two semi-finishing turning operations on the ZB axial bearing workpiece 1 to produce two end faces;

[0060] Milling the bevel groove of the ZB axial bearing workpiece 1;

[0061] The fitter marks the center line of the workpiece, aligns it according to the center line, and then mills the oil groove and drills the hole; uses the processed inner hole to position the ZB axial bearing workpiece 1, and then mills the groove and drills the hole again, and then removes the milling burrs; uses three jaws to clamp the large outer circle of the ZB axial bearing workpiece 1, and then performs the first fine turning of the workpiece, and performs fine turning on the two end faces of the semi-fine turning; performs the second fine turning, clamps the two end faces of the first fine turning, and fine turns the outline of the large shape of the part after alignment; aligns the workpiece, and then performs the third fine turning; uses five-axis processing equipment to drill and mill the oil wedge, and then removes the burrs and cleans the workpiece; performs surface crack inspection on the workpiece, removes the workpiece from the tooling, removes the clamping force, inspects the size, and passes the inspection;

[0062] After the milling of the bevel groove and the drilling of the hole are completed, a finishing process is added. The positioning and clamping surfaces required by the finishing tool are required to be parallel to each other within 0.004, which effectively solves the deformation problem of the positioning and clamping surfaces caused by the milling of the bevel groove and the drilling of the hole; in the second finishing process, the positioning surface and the clamping surface are parallel to each other within 0.004, and the clamping force is evenly distributed on the contact surface, so that after the finishing is completed, the quick release washer 4 is removed, and the rebound of the clamping surface has little effect on the large and small end faces, ensuring that the large and small end faces are better parallel to each other. In the third finishing process, because the large and small end faces are better parallel to each other, the clamping force is evenly distributed on the small end face and the large end face, and the force is evenly applied to each surface, so that the rebound of the clamping surface has little effect on the large and small end faces, and the size is improved. The influence is small. After aligning the small end face and the outer circle, fine turning is performed according to the attached figure. After processing, the parts are removed from the tooling, the clamping force is removed, and the dimensions are inspected. Passed the inspection.

[0063] What is disclosed above is only one or more preferred embodiments of the present application, and cannot be used to limit the scope of rights of the present application. Ordinary technicians in this field can understand that all or part of the processes of implementing the above embodiments and equivalent changes made according to the claims of the present application are still within the scope covered by the present application.

Claims

1. A processing method for the ZB axial bearing of a 170 supercharger. It is characterized in that The steps include: Rough turning is performed on the ZB axial bearing workpiece to remove most of the excess; Perform two semi-finishing turning operations on the ZB axial bearing workpiece to produce two end faces; Milling of bevel grooves on ZB axial bearing workpieces; The fitter marks the center line of the workpiece, aligns it according to the center line, and then mills the oil groove and drills the hole; Use the processed inner hole to position the ZB axial bearing workpiece, and then perform milling and drilling again, and then remove the milling burrs; Use three jaws to clamp the large outer circle of the ZB axial bearing workpiece, then perform the first finish turning of the workpiece, and perform finish turning on the two end faces of the semi-finish turning; Carry out the second finishing process, clamp the two end faces of the first finishing process, align them, and finish the outline of the large shape of the part; Align the workpiece and then perform the third finishing process; Use five-axis machining equipment to perform drilling and oil wedge milling, then remove burrs and clean the workpiece; Carry out surface crack inspection on the workpiece, remove the workpiece from the fixture, remove the clamping force, inspect the size, and check if it passes the inspection.

2. The processing method of the 170 supercharger ZB axial bearing as claimed in claim 1, It is characterized in that During rough turning of ZB axial bearing workpieces: First, clamp the outer circle, and use the general turning CA6140 drilling machine to remove most of the excess, with the spindle speed of 400r / min and the feed of 2mm; Then, a general lathe CA6140 is used to drill through holes, turn large outer circles and step holes, and then cut off. The spindle speed is 400r / min and the feed is 2mm.

3. The processing method of the 170 supercharger ZB axial bearing as claimed in claim 2, It is characterized in that In the two-pass semi-finishing turning of the ZB axial bearing workpiece: First, the CNC lathe QTN200 equipment is used to turn the inner holes and end faces. The inner holes with higher tolerance requirements and the end faces with higher shape and position requirements are left with a margin. The inner holes have a margin of 0.5mm, and the end faces have a margin of 0.2mm. The speed is 800r / min, the feed rate is 0.1-0.2mm, and a 55° turning tool is used for processing; Then, the CNC lathe QTN200 equipment is used to process the two end faces and the inner hole. The inner hole is processed in place, and a margin of 0.2mm is left on the two end faces. The speed is 800r / min, the feed rate is 0.1~0.2mm, and a 55° turning tool is used for processing.

4. The processing method of the 170 supercharger ZB axial bearing as claimed in claim 3, It is characterized in that In the process of milling the bevel groove of the ZB axial bearing workpiece: The five-axis machining center C42U is used to mill the bevel grooves and process three 45° bevel notches. The speed is 1000r / min and the cutting depth is 5mm. A Φ10 end mill is used to remove the excess, and then a Φ6 ball head milling cutter is used to mill out the root R3 shape.

5. The processing method of the 170 supercharger ZB axial bearing as claimed in claim 4, It is characterized in that When the fitter marks the center line of the workpiece, aligns it according to the center line, and then performs the steps of milling the oil groove and drilling the hole: The fitter uses a marking tool to draw the center line of the workpiece for subsequent alignment; the five-axis machining center C42U is used to mill the notch, drill and ream the hole system, and mill the oil groove to the requirements of the drawing (mill the oil grooves of the shapes shown in the dimensions R2, R3, R1, 1.5, R0.4, 1.5, 6°, and R1.5 according to the drawing), the milling depth is 3mm, the speed is 1000r / min, the Φ4.1 and Φ4.8 drill bits are used to machine the bottom hole, and the reamer 5H7 is used to ream the Φ5 hole for subsequent positioning; Use a bench drill, model Z3032, to drill a radial Φ2.4 hole with a cutting depth of 2mm, and a Φ2.85 hole with a cutting depth of 2mm; Remove the burrs at the intersection of the Φ4 hole and the Φ2.4 hole, then clean the parts to remove oil and impurities, and finally use the 170Q-05 steel ball pressing tool to press the Φ3 steel ball into the Φ2.85 hole.

6. The processing method of the 170 supercharger ZB axial bearing as claimed in claim 5, It is characterized in that In the steps of positioning the ZB axial bearing workpiece using the processed inner hole, milling and drilling again, and then removing the milling burrs: Use the Φ5 hole reamed out in the above process for positioning, use the milling tool model 170X-08 slotting tool, and use a Φ6 end mill to machine a slot with a width of 6mm and a depth of 7.7mm, with a feed rate of 3mm and a speed of 600r / min, and then remove the milling burrs.

7. The processing method of the 170 supercharger ZB axial bearing as claimed in claim 6, It is characterized in that In the steps of using three jaws to clamp the large outer circle of the ZB axial bearing workpiece, and then performing the first finishing machining of the workpiece, the two end faces of the semi-finishing machining are finished: The lathe model QTN200 was used to machine the two end faces with a size of 6.3mm in the semi-finishing process to 0.05mm, ensuring that the parallelism between the two machined surfaces was 0.

004. The tool used was a 55° finishing blade and the spindle speed was 800r / min.

8. The processing method of the 170 supercharger ZB axial bearing as claimed in claim 7, It is characterized in that In the second finishing process, the two end faces of the first finishing process are clamped, and the contour of the large shape of the part is finished after alignment: The model of the numerical turning equipment used is QTN200, and the workpiece turning tool is 170C-15. The two end faces processed in the first fine turning process are clamped, and the contour of the large shape of the workpiece is fine turned after alignment. A 55° turning tool is used, and the spindle speed is 800r / min.

9. The processing method of the 170 supercharger ZB axial bearing as claimed in claim 8, It is characterized in that During the alignment of the workpiece and the third finishing process: The model of the numerical turning equipment used is QTN200, and the workpiece turning tool is 170C-16. After the end face runout of the tooling is aligned, the workpiece is placed and the end face pressure plate is pressed. When the outer circle runout of the workpiece is aligned, the outer pressure plate is pressed tightly, and the end face pressure plate is removed. Finish turning is performed as required, and each end face is turned to the required size [the two end faces after the first finish turning are turned from a size of 6.2mm (6.3-2×0.05) to a size of 5.9mm. The turning allowances of the two end faces are consistent, the end face size is 4.1mm, the end face size is 3.9mm, and the inner hole is Φ60].

10. The processing method of the 170 supercharger ZB axial bearing according to claim 9, It is characterized in that In the steps of using five-axis machining equipment to perform drilling and milling oil wedge processing, then remove burrs and clean the workpiece: The five-axis machining equipment used is C42U, and the Φ5 hole is expanded to Φ6, the cutting depth is 2mm, the speed is 1000r / min, and the oil wedge is milled by the milling cutter, and the speed is 1200r / min; Perform chamfer R1 and clean the parts.

Citation Information

Patent Citations

  • Double-channel diamond roller grinding machining method

    CN108857274A

  • Machining process for triple driving cylindrical gear

    CN109175924A

  • Method of manufacturing bearing raceway and bearing

    JP2003232370A

  • Wheel bearing device and its manufacturing method

    JP2019123268A

  • Method and apparatus for superfinishing tapered roller bearing

    US20020152616A1

Cited By

  • Machining method for annular thrust bearing of supercharger

    CN119820262A

  • Machining method for multi-stage air seal skewed slot of large pressure end sealing cover