Preparation method of electronic grade sulfuric acid

By recovering low-concentration sulfuric acid and liquid sulfur oxidation and catalyzed oxidation, high-purity electronic-grade sulfuric acid is produced, which solves the problems of complex sulfuric acid solution treatment process and waste of resources, and achieves efficient and environmentally friendly sulfuric acid recycling and utilization.

CN118929583AInactive Publication Date: 2024-11-12CHINA PETROLEUM & CHEMICAL CORP +1
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202310521065.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-10
Publication Date
2024-11-12
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

In the prior art, the sulfuric acid solution treatment process in the semiconductor and integrated circuit industries is complex and cannot be efficiently utilized, resulting in waste of sulfuric acid resources and environmental pollution.

Method used

Concentration and redox reaction with liquid sulfuric acid by recovered low-concentration sulfur to produce sulfur dioxide-containing gas, and oxidize it into sulfur trioxide in the presence of a catalyst, and then liquefied, evaporated and filtered, and finally reacted with ultrapure water to produce high purity Electronic grade sulfuric acid.

Benefits of technology

It reduces energy consumption, improves the purity and utilization efficiency of sulfuric acid, meets the standards of G5 electronic grade sulfuric acid, and realizes high-quality and efficient recycling of sulfuric acid.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004220863280000121
    Figure BDA0004220863280000121
  • Figure BDA0004220863280000131
    Figure BDA0004220863280000131
  • Figure BDA0004220863280000141
    Figure BDA0004220863280000141
Patent Text Reader

Abstract

The invention relates to the field of electronic chemicals, and discloses an electronic grade sulfuric acid preparation method, which comprises: concentrating recovered low-concentration sulfuric acid, carrying out an oxidation reduction reaction on the obtained concentrated sulfuric acid liquid and liquid sulfur, and carrying out purification treatment on the obtained sulfur dioxide-containing gas to obtain purified sulfur dioxide. And oxidizing the purified sulfur dioxide to obtain the sulfur trioxide-containing gas. And liquefying, evaporating, demisting and filtering the sulfur trioxide-containing gas to obtain the high-purity sulfur trioxide gas. And mixing the high-purity sulfur trioxide gas with ultrapure water for reaction to obtain the electronic-grade sulfuric acid. The invention provides a process method for regenerating electronic-grade sulfuric acid by taking recycled low-concentration sulfuric acid as a raw material, so that the pollution of the sulfuric acid is avoided, and the sulfuric acid is efficiently utilized with high quality.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of electronic chemicals, and in particular to a method for preparing electronic-grade sulfuric acid. Background Art

[0002] Electronic grade sulfuric acid is an ultra-clean, high-purity reagent among semiconductor wet electronic chemicals. The purity of the main components is greater than 99.99wt%, and the number of impurity ions and particles must strictly meet the requirements. It is an indispensable key basic chemical reagent in the development of microelectronics technology and is widely used in the cleaning and etching of silicon wafers in the assembly and processing of semiconductors and integrated circuits.

[0003] At present, the production processes of electronic-grade sulfuric acid mainly include distillation and gas absorption. Distillation is a distillation method that uses reflux to separate liquid mixtures with high purity. It includes four parts: chemical pretreatment system, continuous distillation system, ultra-clean multi-stage filtration system and ultra-clean canning system. The gas absorption method is to directly absorb the purified sulfur trioxide with ultra-pure water or ultra-pure sulfuric acid. The purification of sulfur trioxide is the key to product compliance. The electronic-grade sulfuric acid produced in this way is widely used for etching and cleaning in the microelectronics industry such as semiconductors and integrated circuits, so a large amount of sulfuric acid solution needs to be recycled. With the increasingly stringent national environmental protection policies and the pursuit of maximizing corporate benefits, the topic of sulfuric acid recycling has received more and more attention. The main purpose of recycling sulfuric acid is to remove impurities in the recycled low-concentration sulfuric acid and to increase the concentration of sulfuric acid. The main processes include concentrating the recycled low-concentration sulfuric acid, chemical oxidation, high-temperature cracking, extraction, crystallization, and producing fertilizers. Generally, different treatment processes are adopted according to the amount and concentration of the recycled low-concentration sulfuric acid, the impurity composition and content, and the use of the treated sulfuric acid. Sometimes several processes need to be used in combination. Therefore, effectively recovering sulfuric acid solution is an important issue to be solved at present. Summary of the invention

[0004] The purpose of the present invention is to overcome the problems in the prior art that a large amount of sulfuric acid solution generated by etching and cleaning in microelectronic industries such as semiconductors and integrated circuits has a complicated treatment process and cannot be efficiently utilized, and to provide a method for preparing electronic-grade sulfuric acid. The method uses recycled low-concentration sulfuric acid as a raw material to regenerate electronic-grade sulfuric acid, which can avoid sulfuric acid pollution and enable sulfuric acid to be used in a high-quality and efficient manner.

[0005] In order to achieve the above object, the present invention provides a method for preparing electronic grade sulfuric acid, the preparation method comprising the following steps:

[0006] Step S1: concentrating the recovered low-concentration sulfuric acid to obtain concentrated sulfuric acid liquid, then mixing the concentrated sulfuric acid liquid with liquid sulfur for oxidation-reduction reaction to obtain sulfur dioxide-containing gas, and then purifying the sulfur dioxide-containing gas to obtain purified sulfur dioxide;

[0007] Step S2: in the presence of a catalyst, mixing the purified sulfur dioxide and an oxidant to react to obtain a sulfur trioxide-containing gas;

[0008] Step S3: liquefying, evaporating, demisting and filtering the sulfur trioxide-containing gas to obtain high-purity sulfur trioxide gas;

[0009] Step S4: mixing the high-purity sulfur trioxide gas with ultrapure water to react to obtain the electronic grade sulfuric acid.

[0010] Through the above technical solution, the beneficial effects of the present invention are:

[0011] Electronic-grade sulfuric acid is widely used for etching and cleaning in the semiconductor, integrated circuit and other microelectronic industries, and a large amount of sulfuric acid solution is generated and urgently needs to be recovered. The present invention concentrates the recovered low-concentration sulfuric acid and reacts it with liquid sulfur to generate sulfur dioxide-containing gas. Compared with obtaining sulfur dioxide through cracking reaction, obtaining sulfur dioxide through chemical reaction greatly reduces the reaction temperature, thereby reducing energy consumption; the present invention purifies the sulfur dioxide-containing gas and oxidizes it into sulfur trioxide-containing gas. The sulfur trioxide-containing gas can obtain high-purity sulfur trioxide gas through liquefaction, evaporation, demisting and filtration, so that high-purity electronic-grade sulfuric acid can be obtained after being absorbed by ultrapure water, which can be used again for etching and cleaning in semiconductor, integrated circuit and other microelectronic industries.

[0012] In a preferred embodiment of the present invention, by selecting appropriate redox reaction temperatures of concentrated sulfuric acid liquid and liquid sulfur, purification treatment temperature of sulfur dioxide-containing gas, oxidation conditions of purified sulfur dioxide, liquefaction temperature of sulfur trioxide-containing gas and evaporation temperature of sulfur trioxide-containing liquid, electronic-grade sulfuric acid with a concentration of 96-97wt% that meets the standard of G5 electronic-grade sulfuric acid is obtained. DETAILED DESCRIPTION

[0013] The endpoints and any values ​​of the ranges disclosed in this article are not limited to the precise ranges or values, and these ranges or values ​​should be understood to include values ​​close to these ranges or values. For numerical ranges, the endpoint values ​​of each range, the endpoint values ​​of each range and the individual point values, and the individual point values ​​can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed in this article.

[0014] The present invention provides a method for preparing electronic grade sulfuric acid, the preparation method comprising the following steps:

[0015] Step S1: concentrating the recovered low-concentration sulfuric acid to obtain concentrated sulfuric acid liquid, then mixing the concentrated sulfuric acid liquid with liquid sulfur for oxidation-reduction reaction to obtain sulfur dioxide-containing gas, and then purifying the sulfur dioxide-containing gas to obtain purified sulfur dioxide;

[0016] Step S2: in the presence of a catalyst, mixing the purified sulfur dioxide and an oxidant to react to obtain a sulfur trioxide-containing gas;

[0017] Step S3: liquefying, evaporating, demisting and filtering the sulfur trioxide-containing gas to obtain high-purity sulfur trioxide gas;

[0018] Step S4: mixing the high-purity sulfur trioxide gas with ultrapure water to react to obtain the electronic grade sulfuric acid.

[0019] Electronic-grade sulfuric acid is widely used for etching and cleaning in the semiconductor, integrated circuit and other microelectronic industries, and a large amount of sulfuric acid solution is generated and urgently needs to be recovered. The present invention concentrates the recovered low-concentration sulfuric acid and reacts it with liquid sulfur to generate sulfur dioxide-containing gas, obtains sulfur dioxide through chemical reaction, greatly reduces the reaction temperature, and thus reduces energy consumption; the present invention purifies the sulfur dioxide-containing gas and oxidizes it into sulfur trioxide-containing gas, and the sulfur trioxide-containing gas can obtain high-purity sulfur trioxide gas through liquefaction, evaporation, demisting and filtration, so that high-purity electronic-grade sulfuric acid can be obtained after being absorbed by ultrapure water, and can be used again for etching and cleaning in semiconductor, integrated circuit and other microelectronic industries.

[0020] According to the present invention, preferably, in step S1, the recovered low-concentration sulfuric acid is concentrated under vacuum conditions, and the concentration of the concentrated sulfuric acid liquid is 85-95wt%. Concentrating the recovered low-concentration sulfuric acid to this concentration range can make the concentrated sulfuric acid liquid oxidizable and can undergo redox reaction with liquid sulfur.

[0021] According to the present invention, preferably, in step S1, the temperature of the oxidation-reduction reaction is 120-180°C and the time is 3-5 hours. When the temperature and time of the oxidation-reduction reaction meet this range, the reaction of the concentrated sulfuric acid solution and the liquid sulfur can be as complete as possible.

[0022] Furthermore, the temperature of the redox reaction is 130-150°C.

[0023] According to the present invention, in step S1, the purification method comprises: cooling the sulfur dioxide-containing gas obtained after the oxidation-reduction reaction. Since sulfur dioxide, water molecules and sulfuric acid molecules have different boiling points, sulfur dioxide and water molecules can be separated from sulfuric acid molecules by cooling, thereby removing water molecules and sulfuric acid to obtain purified sulfur dioxide. Preferably, the temperature of the purification treatment is below 50°C, preferably 20-30°C.

[0024] According to the present invention, preferably, in step S2, the molar ratio of the purified sulfur dioxide, the oxidant and the catalyst is 1:(1.05-1.2):(0.009-0.013).

[0025] According to the present invention, preferably, in step S2, the catalyst is selected from at least one of vanadium pentoxide, titanium dioxide and silicon aluminum oxide.

[0026] According to the present invention, preferably, the oxidant is selected from at least one of hydrogen peroxide, ozone and potassium persulfate.

[0027] According to the present invention, preferably, the reaction described in step S2 is a three-stage reaction, the temperature of the first stage reaction is 350-400°C, the time is 2-3h; the temperature of the second stage reaction is 400-470°C, the time is 3-4h; the temperature of the third stage reaction is 400-460°C, the time is 2-3h. Purified sulfur dioxide and oxidant are subjected to three-stage reaction under these conditions, which can make the reaction more complete.

[0028] Furthermore, the temperature of the first stage reaction is 375-385° C., the temperature of the second stage reaction is 445-455° C., and the temperature of the third stage reaction is 435-445° C. According to these conditions, the three-stage reaction is carried out, and the above catalyst and oxidant are used, the purified sulfur dioxide can be basically oxidized into sulfur trioxide, and the conversion rate of sulfur dioxide reaches more than 99%.

[0029] According to a specific embodiment of the present invention, in step S3, the sulfur trioxide-containing gas is liquefied to obtain a sulfur trioxide-containing liquid and impurities after liquefaction; wherein, the liquefaction is condensed and liquefied by using a cooler, and after condensation and liquefaction, on the one hand, the sulfur dioxide that has not reacted completely in step S2 can be removed, and on the other hand, the impurities in the condensate can be discharged during the condensation process of the cooler, and the sulfur dioxide that has not reacted completely and the impurities in the condensate are the impurities after liquefaction. Then, the sulfur trioxide-containing liquid is evaporated to obtain evaporated sulfur trioxide, and then the evaporated sulfur trioxide is defogged by a demister, and the water, sulfuric acid, sulfate and sulfur dioxide contained in the evaporated sulfur trioxide are captured by the demister, thereby removing the water, sulfuric acid, sulfate and sulfur dioxide contained in the evaporated sulfur trioxide to obtain defogged sulfur trioxide. After filtration, the high-purity sulfur trioxide gas is obtained.

[0030] According to the present invention, preferably, in step S3, the liquefaction temperature is 20-40° C. Liquefying the sulfur trioxide-containing gas at this temperature can fully liquefy the sulfur trioxide and separate it from other impurity gases.

[0031] Furthermore, the liquefaction temperature is 25-35°C.

[0032] According to the present invention, preferably, in step S3, the evaporation temperature is 60-90° C. Evaporating the sulfur trioxide-containing liquid at this temperature can fully gasify the sulfur trioxide-containing liquid so that the liquid can enter the demister for purification.

[0033] Furthermore, the evaporation temperature is 70-80°C.

[0034] According to the present invention, preferably, the preparation method further comprises: returning the water, sulfuric acid, sulfates and sulfur dioxide removed after the demisting, i.e. the water, sulfuric acid, sulfates and sulfur dioxide captured by the demister, to the sulfuric acid recovery system to be mixed with the raw sulfuric acid for concentration, and repeating steps S1-S4.

[0035] According to the present invention, preferably, in step S3, a precision filter is used to filter the defogged sulfur trioxide carrying metal ions to obtain high-purity sulfur trioxide gas; the precision filter includes at least three filter columns.

[0036] According to the present invention, preferably, the pore sizes of the first filter column, the second filter column and the third filter column of the precision filter are 0.1-0.3 μm, 0.01-0.03 μm and 0.001-0.003 μm respectively. When the pore sizes of the three filter columns meet this range, the solid particles in the sulfur trioxide after demisting can be removed as much as possible.

[0037] According to the present invention, preferably, the first-stage filter column, the second-stage filter column and the third-stage filter column are made of at least one polymer selected from tetrafluoroethylene-perfluoroalkoxy vinyl ether copolymer, polyvinylidene fluoride and chlorinated polyvinyl chloride. The three-stage filter column made of the above polymers is resistant to acid corrosion and has good cleanliness.

[0038] According to the present invention, preferably, the weight average molecular weight of the polymer is 1 million to 1.5 million g / mol. When the weight average molecular weight of the polymer meets this range, the prepared three-stage filtration column can have sufficient strength and corrosion resistance.

[0039] According to a specific embodiment of the present invention, in step S4, the high-purity sulfur trioxide gas and ultrapure water are introduced into an absorption tower, and the high-purity sulfur trioxide gas is absorbed by the ultrapure water to obtain the electronic-grade sulfuric acid. The ultrapure water can reach a purity of 99.9999wt% under filtration in an ultrapure water system. The ultrapure water and the high-purity sulfur trioxide gas are made to form a countercurrent in the absorption tower system, which can accelerate the absorption process, so that the absorption rate of the high-purity sulfur trioxide gas can reach more than 99.99%, thereby obtaining electronic-grade sulfuric acid with a concentration of 93-98wt%. Under preferred conditions, electronic-grade sulfuric acid with a concentration of 96-97wt% can be obtained.

[0040] The present invention will be described in detail below through examples. The reagents used in the following examples, unless otherwise specified, are all conventional biochemical reagents; the raw materials, instruments and equipment used, etc., can all be purchased from the market or can be obtained by existing methods; the reagent dosage, unless otherwise specified, is the reagent dosage in conventional experimental operations; the experimental method, unless otherwise specified, is a conventional method. In the following examples, the sulfuric acid concentration of the recovered low-concentration sulfuric acid solution is 30%-75wt%.

[0041] In various embodiments of the present invention, the testing method of each evaluation item is as follows:

[0042] (1) Metal impurity analysis: Electronic grade sulfuric acid was diluted 10 times and metal ions (such as Na + , K + , Ca 2+ 、Ti 4+ , Li + , Fe 3+ etc.) content was tested.

[0043] (2) Non-metallic impurity analysis: Ion chromatography (IC) was used to analyze the non-metallic ions (such as Cl - 、NO3 - PO4 3- NH4 + The content of etc. was tested and analyzed.

[0044] (3) Particle analysis: Use a liquid particle counter to characterize the particle impurities in electronic grade sulfuric acid solution.

[0045] (4) Sulfuric acid content analysis: According to GB / T534-2014, the sulfuric acid content was tested using a potentiometric titrator.

[0046] (5) Conversion rate of SO2 after purification in step S2: (the amount of sulfur dioxide after purification - the amount of sulfur dioxide gas in the sulfur trioxide-containing gas) / the amount of sulfur dioxide after purification × 100%.

[0047] The following example is used to illustrate the preparation of electronic grade sulfuric acid.

[0048] Example 1

[0049] (1) The recovered low-concentration sulfuric acid with a concentration of 38.47 wt% is heated and concentrated under vacuum conditions, and the sulfuric acid concentration in the obtained concentrated sulfuric acid liquid can reach 87.4 wt%; at 130° C., the concentrated sulfuric acid liquid and liquid sulfur undergo an oxidation-reduction reaction for 3 hours to produce sulfur dioxide-containing gas and water, and at this time the temperature is reduced to 30° C. to obtain purified sulfur dioxide.

[0050] (2) The catalyst is vanadium pentoxide, the oxidant is hydrogen peroxide, the purified sulfur dioxide, the oxidant and the catalyst are mixed in a molar ratio of 1:1.05:0.009, and the purified sulfur dioxide is oxidized through a three-stage reaction to obtain a sulfur trioxide-containing gas;

[0051] The temperature of the first stage reaction is 380°C and the time is 2h; the temperature of the second stage reaction is 450°C and the time is 3h; the temperature of the third stage reaction is 440°C and the time is 2h.

[0052] (3) Condensing the obtained sulfur trioxide-containing gas at 25° C. to remove the sulfur dioxide that has not reacted completely in step (2), and discharging impurities in the condensate during the condensation process in the cooler to obtain a sulfur trioxide-containing liquid.

[0053] (4) In an evaporator at 70° C., the sulfur trioxide-containing liquid is vaporized to obtain evaporated sulfur trioxide.

[0054] (5) After evaporation, sulfur trioxide enters the demister to obtain defogged sulfur trioxide, in which water, sulfuric acid, sulfate and sulfur dioxide are captured by the demister and returned to the sulfuric acid system to be mixed with the raw sulfuric acid for concentration.

[0055] (6) filtering the metal ions carried by the demisted sulfur trioxide through a precision filter to obtain high-purity sulfur trioxide gas;

[0056] Among them, the precision filter includes three-stage filter columns, all of which are made of polyvinylidene fluoride with a weight-average molecular weight of 1 million g / mol; the pore sizes of the first-stage filter column, the second-stage filter column and the third-stage filter column are 0.1μm, 0.01μm and 0.001μm respectively.

[0057] (7) High-purity sulfur trioxide gas is introduced into an absorption tower to form a countercurrent with ultrapure water with a purity of 99.9999 wt % to carry out an absorption process, thereby producing electronic grade sulfuric acid with a concentration of 96.1 wt %.

[0058] Example 2

[0059] (1) The recovered low-concentration sulfuric acid with a concentration of 46.33 wt% is heated and concentrated under vacuum conditions, and the sulfuric acid concentration in the obtained concentrated sulfuric acid liquid can reach 89.2 wt%; at 140° C., the concentrated sulfuric acid liquid and liquid sulfur undergo an oxidation-reduction reaction for 4 hours to produce sulfur dioxide-containing gas and water, and at this time the temperature is reduced to 25° C. to obtain purified sulfur dioxide.

[0060] (2) The catalyst is vanadium pentoxide, the oxidant is ozone, the purified sulfur dioxide, the oxidant and the catalyst are mixed in a molar ratio of 1:1.1:0.01, and the purified sulfur dioxide is oxidized through a three-stage reaction to obtain a sulfur trioxide-containing gas;

[0061] The temperature and time of the three-stage reaction are the same as those in Example 1.

[0062] (3) Condensing the obtained sulfur trioxide-containing gas at 30° C. to remove the sulfur dioxide that has not reacted completely in step (2), and discharging impurities in the condensate during the condensation process in the cooler to obtain a sulfur trioxide-containing liquid.

[0063] (4) In an evaporator at 75° C., the sulfur trioxide-containing liquid is vaporized to obtain evaporated sulfur trioxide.

[0064] (5)-(6) Same as Example 1.

[0065] (7) High-purity sulfur trioxide gas is introduced into an absorption tower to form a countercurrent with ultrapure water with a purity of 99.9999 wt % to carry out an absorption process, thereby producing electronic grade sulfuric acid with a concentration of 96.3 wt %.

[0066] Example 3

[0067] (1) The recovered low-concentration sulfuric acid with a concentration of 52.37 wt% is heated and concentrated under vacuum conditions, and the sulfuric acid concentration in the obtained concentrated sulfuric acid liquid can reach 91.3 wt%; at 150° C., the concentrated sulfuric acid liquid and liquid sulfur undergo an oxidation-reduction reaction for 5 hours to produce sulfur dioxide-containing gas and water, and at this time the temperature is reduced to 20° C. to obtain purified sulfur dioxide.

[0068] (2) Same as Example 1;

[0069] The temperature and time of the three-stage reaction are the same as those in Example 1.

[0070] (3) Condensing the obtained sulfur trioxide-containing gas at 35° C. to remove the sulfur dioxide that has not reacted completely in step (2), and discharging impurities in the condensate during the condensation process in the cooler to obtain a sulfur trioxide-containing liquid.

[0071] (4) In an evaporator at 80°C, the sulfur trioxide-containing liquid is vaporized to obtain evaporated sulfur trioxide.

[0072] (5)-(6) Same as Example 1.

[0073] (7) High-purity sulfur trioxide gas is introduced into an absorption tower to form a countercurrent with ultrapure water with a purity of 99.9999 wt % to carry out an absorption process, thereby producing electronic grade sulfuric acid with a concentration of 96.4 wt %.

[0074] Example 4

[0075] (1) The recovered low-concentration sulfuric acid with a concentration of 67.06 wt% is heated and concentrated under vacuum conditions, and the sulfuric acid concentration in the obtained concentrated sulfuric acid liquid can reach 92.6 wt%; at 120° C., the concentrated sulfuric acid liquid and liquid sulfur undergo an oxidation-reduction reaction for 5 hours to produce sulfur dioxide-containing gas and water, and at this time the temperature is reduced to 50° C. to obtain purified sulfur dioxide.

[0076] (2) The catalyst is silicon aluminum oxide, the oxidant is potassium persulfate, the purified sulfur dioxide, the oxidant and the catalyst are mixed in a molar ratio of 1:1.12:0.011, and the purified sulfur dioxide is oxidized through a three-stage reaction to obtain a sulfur trioxide-containing gas;

[0077] The temperature and time of the three-stage reaction are the same as those in Example 1.

[0078] (3) Condensing the obtained sulfur trioxide-containing gas at 20° C. to remove the sulfur dioxide that has not reacted completely in step (2), and discharging impurities in the condensate during the condensation process in the cooler to obtain a sulfur trioxide-containing liquid.

[0079] (4) In an evaporator at 60° C., the sulfur trioxide-containing liquid is vaporized to obtain evaporated sulfur trioxide.

[0080] (5)-(6) Same as Example 1.

[0081] (7) High-purity sulfur trioxide gas is introduced into an absorption tower to form a countercurrent with ultrapure water with a purity of 99.9999 wt % to carry out an absorption process, thereby producing electronic grade sulfuric acid with a concentration of 96.7 wt %.

[0082] Example 5

[0083] (1) The recovered low-concentration sulfuric acid with a concentration of 59.38 wt% is heated and concentrated under vacuum conditions, and the sulfuric acid concentration in the obtained concentrated sulfuric acid liquid can reach 91.5 wt%; at 180° C., the concentrated sulfuric acid liquid and liquid sulfur undergo an oxidation-reduction reaction for 4 hours to produce sulfur dioxide-containing gas and water, and at this time the temperature is reduced to 40° C. to obtain purified sulfur dioxide.

[0084] (2) The catalyst is titanium dioxide and the oxidant is ozone. The purified sulfur dioxide, the oxidant and the catalyst are mixed in a molar ratio of 1:1.15:0.012, and the purified sulfur dioxide is oxidized through a three-stage reaction to obtain a sulfur trioxide-containing gas;

[0085] The temperature and time of the three-stage reaction are the same as those in Example 1.

[0086] (3) condensing the obtained sulfur trioxide-containing gas at 40° C. to remove the sulfur dioxide that has not reacted completely in step (2), and discharging impurities in the condensate during the condensation process in the cooler to obtain a sulfur trioxide-containing liquid.

[0087] (4) In an evaporator at 90° C., the sulfur trioxide-containing liquid is vaporized to obtain evaporated sulfur trioxide.

[0088] (5)-(6) Same as Example 1.

[0089] (7) High-purity sulfur trioxide gas is introduced into an absorption tower to form a countercurrent with ultrapure water with a purity of 99.9999 wt % to carry out an absorption process, thereby producing electronic grade sulfuric acid with a concentration of 96.9 wt %.

[0090] Example 6

[0091] Electronic grade sulfuric acid was prepared according to the method of Example 1, except that in step (1), the oxidation-reduction reaction was carried out at 200° C. Electronic grade sulfuric acid with a concentration of 95.4 wt % was obtained.

[0092] Example 7

[0093] Electronic grade sulfuric acid was prepared according to the method of Example 1, except that in step (1), after the oxidation-reduction reaction, the temperature was lowered to 55° C. Electronic grade sulfuric acid with a concentration of 94.6 wt % was obtained.

[0094] Example 8

[0095] Electronic grade sulfuric acid was prepared according to the method of Example 1, except that the oxidation conditions of the purified sulfur dioxide were different. Specifically, in step (2), the temperature of the first stage reaction was 450°C and the time was 1 hour; the temperature of the second stage reaction was 380°C and the time was 2 hours; the temperature of the third stage reaction was 440°C and the time was 1 hour. Electronic grade sulfuric acid with a concentration of 93.2 wt% was obtained.

[0096] Example 9

[0097] Electronic grade sulfuric acid was prepared according to the method of Example 1, except that in step (3), the obtained sulfur trioxide-containing gas was condensed at 15° C. Electronic grade sulfuric acid with a concentration of 97.3 wt % was obtained.

[0098] Example 10

[0099] Electronic grade sulfuric acid was prepared according to the method of Example 1, except that in step (4), evaporation was carried out in an evaporator at 100° C. Electronic grade sulfuric acid with a concentration of 93.6 wt % was obtained.

[0100] Comparative Example 1

[0101] Electronic grade sulfuric acid was prepared according to the method of Example 1, except that the sulfur dioxide-containing gas was prepared by a method of sulfuric acid concentration and cracking. Specifically, in step (1), natural gas was used as fuel, and sulfuric acid in the concentrated sulfuric acid liquid was reduced to sulfur dioxide in a cracking furnace at a temperature of 1000° C.-1200° C., and the reaction time was 3-5 hours, wherein the amount of natural gas used was 60-80 kg based on the mass of the concentrated sulfuric acid liquid being 1 ton. Electronic grade sulfuric acid with a concentration of 93.2 wt% was prepared.

[0102] Test Case

[0103] The results of the metal impurity content, non-metallic impurity content, particulate impurity content, sulfuric acid concentration in concentrated sulfuric acid solution, conversion rate of purified sulfur dioxide, absorption rate of high-purity sulfur trioxide gas and concentration of electronic grade sulfuric acid prepared in each embodiment and comparative example are shown in Table 1. The symbols Li to Bi in the table all represent ions.

[0104] Table 1

[0105]

[0106]

[0107]

[0108] Table 1 (Continued Table 1)

[0109]

[0110]

[0111]

[0112] Table 1 (Continued Table 2)

[0113]

[0114]

[0115] It can be seen from the results in Table 1 that the method for preparing electronic-grade sulfuric acid provided by the present invention can effectively utilize the recovered low-concentration sulfuric acid, so that the sulfur element can be recycled. The electronic-grade sulfuric acid prepared in Examples 1-5 meets the quality requirements of electronic-grade sulfuric acid with a G5 concentration of 96%-97wt% in the SEMI standard. Among them, Examples 1-3 show more prominent advantages in comprehensive effects. Comparative Example 1 uses a cracking method to reduce sulfuric acid in concentrated sulfuric acid solution to sulfur dioxide, and the cracking temperature is 1000℃-1200℃. On the one hand, the reaction temperature is greatly increased, thereby increasing energy consumption. On the other hand, the conversion rate of sulfur dioxide after purification decreases, and the impurity content and particle number of the obtained electronic-grade sulfuric acid are significantly increased, and the concentration of the electronic-grade sulfuric acid does not meet 96-97wt%, so it does not meet the standard of G5 electronic-grade sulfuric acid.

[0116] In addition, compared with Example 1, Example 6 increases the redox reaction temperature of concentrated sulfuric acid liquid and liquid sulfur, Example 7 increases the purification temperature when purifying sulfur dioxide-containing gas, Example 8 changes the oxidation conditions of purified sulfur dioxide, Example 9 reduces the liquefaction temperature of sulfur trioxide-containing gas, and Example 10 increases the evaporation temperature of sulfur trioxide-containing liquid. Although the impurity content and particle number of the electronic-grade sulfuric acid prepared in Examples 6-10 and the conversion rate of purified sulfur dioxide meet the requirements of impurity content, particle number and conversion rate of purified sulfur dioxide of G5-grade electronic-grade sulfuric acid, the concentration of the electronic-grade sulfuric acid does not meet 96-97wt%, and therefore does not meet the quality requirements of G5-grade electronic-grade sulfuric acid.

[0117] The preferred embodiments of the present invention are described in detail above, but the present invention is not limited thereto. Within the technical concept of the present invention, the technical solution of the present invention can be subjected to a variety of simple modifications, including the combination of various technical features in any other suitable manner, and these simple modifications and combinations should also be regarded as the contents disclosed by the present invention and belong to the protection scope of the present invention.

Claims

1. A method for preparing electronic grade sulfuric acid, characterized in that: The preparation method comprises the following steps: Step S1: concentrating the recovered low-concentration sulfuric acid to obtain concentrated sulfuric acid liquid, then mixing the concentrated sulfuric acid liquid with liquid sulfur for oxidation-reduction reaction to obtain sulfur dioxide-containing gas, and then purifying the sulfur dioxide-containing gas to obtain purified sulfur dioxide; Step S2: in the presence of a catalyst, mixing the purified sulfur dioxide and an oxidant to react to obtain a sulfur trioxide-containing gas; Step S3: liquefying, evaporating, demisting and filtering the sulfur trioxide-containing gas to obtain high-purity sulfur trioxide gas; Step S4: mixing the high-purity sulfur trioxide gas with ultrapure water to react to obtain the electronic grade sulfuric acid.

2. The preparation method according to claim 1, characterized in that: In step S1, the concentration of the concentrated sulfuric acid solution is 85-95wt%.

3. The preparation method according to claim 1 or 2, characterized in that: In step S1, the temperature of the redox reaction is 120-180°C, preferably 130-150°C, and the time is 3-5h.

4. The preparation method according to any one of claims 1 to 3, characterized in that: In step S1, the temperature of the purification treatment is below 50°C, preferably 20-30°C.

5. The preparation method according to any one of claims 1 to 4, characterized in that: In step S2, the catalyst is selected from at least one of vanadium pentoxide, titanium dioxide and silicon aluminum oxide; Preferably, the oxidant is selected from at least one of hydrogen peroxide, ozone and potassium persulfate.

6. The preparation method according to any one of claims 1 to 5, characterized in that: The reaction described in step S2 is a three-stage reaction, the temperature of the first stage reaction is 350-400°C, and the time is 2-3h; the temperature of the second stage reaction is 400-470°C, and the time is 3-4h; the temperature of the third stage reaction is 400-460°C, and the time is 2-3h.

7. The preparation method according to any one of claims 1 to 6, characterized in that: In step S3, the liquefaction temperature is 20-40°C, preferably 25-35°C.

8. The preparation method according to any one of claims 1 to 7, characterized in that: In step S3, the evaporation temperature is 60-90°C, preferably 70-80°C.

9. The preparation method according to any one of claims 1 to 8, characterized in that: The preparation method further comprises: mixing the water, sulfuric acid, sulfate and sulfur dioxide removed after the demisting with the recovered low-concentration sulfuric acid, and then repeating steps S1-S4.

10. The preparation method according to any one of claims 1 to 9, characterized in that: In step S3, the filtration is performed using a precision filter, wherein the precision filter comprises at least three-stage filter columns; Preferably, the pore sizes of the first-stage filter column, the second-stage filter column and the third-stage filter column of the precision filter are 0.1-0.3 μm, 0.01-0.03 μm and 0.001-0.003 μm respectively; Preferably, the first-stage filter column, the second-stage filter column and the third-stage filter column are made of at least one polymer selected from tetrafluoroethylene-perfluoroalkoxy vinyl ether copolymer, polyvinylidene fluoride and chlorinated polyvinyl chloride; Preferably, the weight average molecular weight of the polymer is 1 million to 1.5 million g / mol.

Citation Information

Patent Citations

  • Method and device for preparing sulfuric acid

    CN101698470A

  • Environment-friendly production process for producing sulfuric acid by using waste sulfuric acid by virtue of sulfur reduction

    CN104291277A

  • Waste sulfuric acid treatment method

    CN105502308A

  • Electronic-grade sulfuric acid production device

    CN217418195U