Production method of anti-ultraviolet nanometer self-cleaning automobile glass

By adding polypropylene, nylon and ultraviolet shielding agent to the production of automobile glass, the ultraviolet-resistant nano-self-cleaning glass is solved, and the driver's comfort and skin protection effect in summer is improved.

CN118930018AInactive Publication Date: 2024-11-12TAIWAN GLASS YUEDA AUTO GLASS CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202410879740.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-02
Publication Date
2024-11-12
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing automotive glass lacks an effective anti-UV method, which causes drivers to easily experience sun spots, premature aging and skin damage when driving in summer.

Method used

During the glass production process, the ratio of polypropylene to nylon is 1 to 2, and the ratio of ultraviolet shielding agent and glass coating agent is 1 to 1, and the ultraviolet resistant nano-self-cleaning glass is formed by high-temperature heating and hot pressing treatment.

Benefits of technology

Effectively reduce ultraviolet rays to the skin, improve drivers' comfort in hot summers, and reduce the impact of ultraviolet rays on drivers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118930018A_ABST
    Figure CN118930018A_ABST
Patent Text Reader

Abstract

The invention discloses a production method of anti-ultraviolet nano self-cleaning automobile glass, which mainly selects a plurality of inorganic minerals such as quartz sand, borax, boric acid, barite, barium carbonate, limestone, feldspar, sodium carbonate and the like as main raw materials, and additionally adds a small amount of auxiliary raw materials including soda, mirabilite, dolomite and the like, and after the selection of the processing raw materials is completed, the raw materials are added into the glass to prepare the anti-ultraviolet nano self-cleaning automobile glass. The method comprises the following steps: selecting raw materials, cleaning the selected raw materials to remove silt, stains and dust on the surfaces of the raw materials, after the selected raw materials are cleaned, removing defective raw materials in the raw materials, removing the raw materials with the radius smaller than 2cm, and only reserving the raw materials with the radius larger than or equal to 3cm. Damage of ultraviolet rays to the skin is reduced, the influence of the ultraviolet rays on a driver is reduced, the driving comfort of the driver in hot summer is improved, and use is convenient.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of glass production, in particular to a method for producing anti-ultraviolet nano self-cleaning automobile glass. Background Art

[0002] Automotive glass is an indispensable accessory of automobile body, and it mainly plays a protective role. There are three main types of automotive glass: laminated glass, tempered glass and regional tempered glass, which can withstand strong impact. Automotive glass is divided into four types according to its location: front windshield, side windows, rear windshield and sunroof. The state stipulates that the front windshield must be laminated glass. The front windshield of some low-cost agricultural vehicles is still tempered glass or regional tempered glass, the side windows are tempered glass, and the rear windshield is generally tempered glass with electric heating wire. Data shows that the global automotive glass industry is divided by consumer market themes. Europe, North America, Japan, China and South Korea account for 34%, 26%, 19%, 9% and 5% respectively, and together account for 93% of the global automotive glass market. Divided by companies, the global automotive glass market is highly monopolized. Japan's Asahi Glass Company is the world's largest glass manufacturer, occupying almost 25% of the automotive glass market. Moreover, glass industry giants Saint-Gobain and Nippon Sheet Glass also occupy a huge share of the automotive glass market. The world's three largest automotive glass manufacturers, Nippon Sheet Glass, Asahi Glass and Saint-Gobain, together with their joint ventures around the world, account for about 60% of the global OEM market.

[0003] The development of modern car appearance is closely related to the development of glass technology. As early as more than 40 years ago, the front windshield of the car has adopted a single-piece curved windshield and gradually abandoned the flat windshield. Today's car windshields are generally made into a large curved surface with a certain curvature on the top, bottom, left and right. This kind of curved glass is a product with very high technical requirements in terms of processing and assembly, because it involves many issues such as car model, strength, heat insulation, assembly, etc. Car windshield, laminated glass, refers to a transparent adhesive plastic film attached between two or three layers of glass to strengthen the strength of the plastic. The combination of toughness and hardness of glass increases the glass's resistance to shattering. Tempered glass refers to ordinary glass that has been quenched to form a certain internal stress in the internal structure, thereby strengthening the strength of the glass. When it is broken by impact, the glass will split into small fragments with blunt edges, which is less likely to cause harm to the occupants. Regional tempered glass is a new type of tempered glass. It has been specially treated so that when it is broken by impact, the cracks in the glass can still maintain a certain clarity, ensuring that the driver's field of vision is not affected. At present, automobile windshields are mainly made of laminated tempered glass and laminated regional tempered glass, which can withstand strong impact.

[0004] However, the existing management methods and systems have the following deficiencies: Most existing car windows lack effective UV protection. When drivers drive in the hot summer, sunlight shines through the car windows onto the driver's body, which can easily cause sun spots on the skin, loss of elasticity, premature aging, sensitivity, and wrinkles. More importantly, skin damage causes unbearable stinging and itching, weakening the skin's own disease resistance and immunity, and forming skin diseases.

[0005] Therefore, we propose a method for producing ultraviolet-resistant nano self-cleaning automobile glass to solve the problems mentioned above. Summary of the Invention

[0006] The object of the present invention is to provide a method for producing UV-resistant nano self-cleaning automotive glass, by adding polypropylene and nylon in a ratio of 1 to 2 during the production process, and then adding an ultraviolet shielding agent and a glass coating agent in a ratio of 1 to 1, so as to solve the problems raised by the above-mentioned background technology.

[0007] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a method for producing UV-resistant nano self-cleaning automotive glass, comprising the following steps: when selecting and processing raw materials, mainly selecting a variety of inorganic minerals such as quartz sand, borax, boric acid, barite, barium carbonate, limestone, feldspar, soda ash, etc. as the main raw materials, and adding a small amount of auxiliary raw materials, including soda and Glauber's salt, dolomite, etc.; after the selection of the processing raw materials is completed, the selected raw materials need to be cleaned to remove mud, stains, and dust on the surface of the raw materials; after the selected raw materials are cleaned, the defective raw materials need to be removed from the raw materials, and the raw materials with a radius less than 2 cm are removed, and only the raw materials with a radius greater than or equal to 3 cm are retained.

[0008] Preferably, after the removal of defective raw materials is completed, the raw materials need to be pre-processed, and the raw materials are placed in a dryer to dry the wet raw materials. The power of the dryer is greater than or equal to 3500W. After the pre-processing of the raw materials is completed, the raw materials need to be crushed. The raw materials are added to a crusher with a motor power greater than 3000W for crushing. After the block raw materials are crushed, an electromagnetic suction cup is used to remove the iron in the raw materials.

[0009] Preferably, after the iron-containing raw materials are deironed, the raw materials need to be mixed and prepared. 30 kilograms of raw materials are selected, and polypropylene and nylon are added to the raw materials. The ratio of polypropylene to nylon is 1 to 2. Then the raw materials are fully stirred and mixed in a high-speed blender. After stirring for 30 minutes, the high-speed blender is turned off, and then ultraviolet shielding agent and glass coating agent are added. The ratio of ultraviolet shielding agent to glass coating agent is 1 to 1. Then continue to turn on the high-speed blender and continue stirring for 10 minutes before taking out the raw materials.

[0010] Preferably, after the mixture is prepared, the mixture is placed in a tank kiln or a crucible kiln for high-temperature heating. The temperature in the tank kiln or the crucible kiln cannot be lower than 1580 degrees. The mixture is heated to form a uniform, bubble-free liquid glass.

[0011] Preferably, after the mixed glass raw materials are heated in a tank furnace or a crucible furnace, the liquid glass is sent into a tin bath filled with nitrogen and hydrogen protective gas, floated on the surface of the tin liquid, and the glass liquid is naturally spread and thinned. The glass liquid is then cooled for 3 hours, and the glass is taken out and the glass surface is polished. It is then transferred to an annealing furnace to form raw glass. The raw glass must first be cut into blanks. Cutting oil is used to control the pressure and depth during cutting. After the blank glass is edged, cleaned, and dried, a layer of silicon dioxide will be sprinkled on the surface to prevent sticking during bending. Next, a special person will check whether the glass has impurities or cracks.

[0012] Preferably, after the quenching of the formed glass is completed, the glass needs to be bent, and the glass is placed in a tempering furnace or a hot bending furnace, heated at a furnace temperature exceeding 700°C, and annealed and cooled. Specifically, during production, the corresponding mold is placed in a bending trolley, and the upper and lower pieces are placed. The operator puts the pre-treated qualified semi-finished glass onto the mold, and the bending trolley is raised to the upper layer of the bending furnace by the lifting and conveying device, and passes through the preheating section and the bending section in turn. In the preheating section, the glass is heated from room temperature to slightly below the glass softening temperature Tf, Tf is generally between 570-600°C. In the bending section, the glass temperature is higher than the softening temperature, and the glass has basically softened and is in a relatively plastic state. The effect of gravity causes the glass to gradually sag and fit with the four sides of the mold to form a spherical surface, thereby achieving the curvature and spherical surface requirements of the final product.

[0013] Preferably, after the quenched glass is bent, a laminating machine is needed to insert PVB film into the glass. First, the PVB film is evenly heated and stretched into a fan shape at the same time. Then, the PVB film is allowed to cool for 1 hour. At this time, the PVB film is bent. Then, the glass that needs to be inserted with the PVB film is placed on the laminating machine, the upper piece is sucked up with a vacuum suction cup, the PVB film is placed, and then it is punched through the laminating machine.

[0014] Preferably, after the PVB film is placed in the laminating machine, the glass needs to be placed in an autoclave for heating and pressurization. The autoclave is first preheated. When the glass enters the autoclave, it is first heated to 75°C, then pressurized to 0.5Mpa, and then the heating is started and raised together. In order to increase the pressure and temperature at the same time, the temperature change is adjusted according to the temperature of the air in the autoclave. When the autoclave is full of laminated glass, the temperature inside can be higher than the glass temperature. When the temperature inside the laminated glass is consistent with the highest value in the heating stage, the heating process is completed. After heating for 3 to 4 hours, the glass is taken out and cooled for 1 hour to complete the manufacturing.

[0015] Preferably, the laminating machine in step 7 is a double-glass laminating machine with equipment dimensions of L7000mm*W3980mm*H3000mm and a rated power of 4kW.

[0016] Preferably, the autoclave in step 8 is a KCFD series autoclave made of 304 stainless steel.

[0017] Compared with the prior art, the present invention has the following beneficial effects: In the production process of the present invention, main raw materials such as quartz sand, borax, boric acid, barite, barium carbonate, limestone, feldspar, and soda ash are selected, and then the raw materials are cleaned, and raw materials with a radius of less than 2 cm are removed. The raw materials are then placed in a dryer for drying, and then the raw materials are added to a grinder with a motor power greater than 3000W for crushing, and an electromagnetic chuck is used to remove iron in the raw materials. Polypropylene and nylon are then added to the raw materials, and the ratio of polypropylene to nylon is 1 to 2. The raw materials are then fully stirred and mixed in a high-speed stirrer, and the high-speed stirrer is turned off after stirring for 30 minutes. Then add the UV shielding agent and glass coating agent, the ratio of UV shielding agent to glass coating agent is 1:1, continue to turn on the high-speed mixer and continue stirring for 10 minutes, then take out the raw materials, and then put the mixed materials into the pool kiln or crucible kiln for high-temperature heating. The temperature in the pool kiln or crucible kiln cannot be lower than 1580 degrees. Heat the mixed materials to form a uniform, bubble-free liquid glass, and send the liquid glass into a tin tank filled with nitrogen and hydrogen protective gas, float on the surface of the tin liquid, and naturally spread and thin the glass liquid. Then cool the glass liquid for 3 hours, take out the glass, polish the glass surface, and then send it to the annealing The glass is placed in a tempering furnace or a hot bending furnace, heated at a temperature exceeding 700°C, and annealed and cooled. The bending trolley is raised to the upper layer of the bending furnace by a lifting and conveying device, and passes through the preheating section and the bending section in sequence. In the preheating section, the glass is heated from room temperature to slightly below the softening temperature Tf of the glass, which is generally between 570-600°C. In the bending section, the glass temperature is higher than the softening temperature, and the glass has basically softened and is in a relatively plastic state. The effect of gravity causes the glass to gradually sag and fit around the mold to form a spherical surface. Finally, when the glass is placed in the autoclave, it is first heated to 75°C. Then, the pressure is increased to 0.5 MPa, and then the heating is started, and the pressure and temperature are increased together. In order to increase the pressure and temperature at the same time, the temperature change is adjusted according to the temperature of the air in the autoclave. When the autoclave is full of laminated glass, the temperature inside can be higher than the temperature of the glass. When the temperature inside the laminated glass is consistent with the highest value in the heating stage, the heating process is completed. After heating for 3 to 4 hours, the glass is taken out and cooled for 1 hour to complete the manufacturing. The automotive glass produced by the present invention is convenient for reducing the damage of ultraviolet rays to the skin, reduces the impact of ultraviolet rays on the driver, increases the comfort of the driver when driving in the hot summer, and is convenient for use. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 This is a diagram of the production steps in a method for producing ultraviolet-resistant nano self-cleaning automotive glass according to the present invention; Figure 2 This is a diagram of the mixing steps in the method for producing ultraviolet-resistant nano self-cleaning automotive glass of the present invention. DETAILED DESCRIPTION

[0019] The following will clearly and completely describe the technical solutions in the embodiments of the present invention in conjunction with the accompanying drawings. Obviously, the implementation regulations described are only part of the embodiments of the present invention, not all of the embodiments. All other embodiments obtained by ordinary technicians in this field based on the embodiments of the present invention without making any creative efforts shall fall within the scope of protection of the present invention.

[0020] See also Figure 1-2 As shown, the present invention provides a technical solution: when selecting raw materials for processing, a variety of inorganic minerals such as quartz sand, borax, boric acid, barite, barium carbonate, limestone, feldspar, soda ash, etc. are mainly selected as main raw materials, and a small amount of auxiliary raw materials, including soda, sodium sulfate, dolomite, etc., are added. After the selection of the processing raw materials is completed, the selected raw materials need to be cleaned to remove mud, stains, and dust on the surface of the raw materials. After the selected raw materials are cleaned, the defective raw materials need to be removed from the raw materials, and the raw materials with a radius less than 2 cm are removed, and only the raw materials with a radius greater than or equal to 3 cm are retained.

[0021] according to Figure 1-2 As shown, after the removal of defective raw materials is completed, the raw materials need to be pre-processed and placed in a dryer to dry the wet raw materials. The power of the dryer is greater than or equal to 3500W. After the pre-processing of the raw materials is completed, the raw materials need to be crushed and placed in a crusher with a motor power greater than 3000W for crushing. After the block raw materials are crushed, an electromagnetic suction cup is used to remove the iron in the raw materials.

[0022] according to Figure 1-2 As shown, after the iron-containing raw materials are deironed, the raw materials need to be mixed and prepared. 30 kilograms of raw materials are selected, and polypropylene and nylon are added to the raw materials. The ratio of polypropylene to nylon is 1 to 2. Then the raw materials are fully stirred and mixed in a high-speed blender. After stirring for 30 minutes, the high-speed blender is turned off, and then ultraviolet shielding agent and glass coating agent are added. The ratio of ultraviolet shielding agent to glass coating agent is 1 to 1. Then continue to turn on the high-speed blender and continue stirring for 10 minutes before taking out the raw materials.

[0023] according to Figure 1-2As shown, after the mixture is prepared, the mixture is placed in a tank kiln or a crucible kiln for high-temperature heating. The temperature in the tank kiln or the crucible kiln cannot be lower than 1580 degrees. The mixture is heated to form a uniform, bubble-free liquid glass.

[0024] according to Figure 1-2 As shown, after the mixed glass raw materials are heated in a tank furnace or a crucible furnace, the liquid glass is sent into a tin bath filled with nitrogen and hydrogen protective gas, floated on the surface of the tin liquid, and the glass liquid is naturally spread and thinned. The glass liquid is then cooled for 3 hours, and the glass is taken out and polished. It is then transferred to an annealing furnace to form raw glass. The raw glass must first be cut into blanks. Cutting oil is used to control the pressure and depth during cutting. After the blank glass is edged, cleaned, and dried, a layer of silicon dioxide will be sprinkled on the surface to prevent sticking during bending. Next, a special person will check whether the glass has impurities or cracks.

[0025] according to Figure 1-2 As shown, after the quenching of the formed glass is completed, the glass needs to be bent. The glass is placed in a tempering furnace or a hot bending furnace, heated at a furnace temperature of more than 700°C, and annealed and cooled. Specifically, during production, the corresponding mold is placed in a bending trolley, and the upper and lower pieces are placed. The operator puts the pre-treated qualified semi-finished glass onto the mold, and the bending trolley is raised to the upper layer of the bending furnace by the lifting and conveying device, and passes through the preheating section and the bending section in turn. In the preheating section, the glass is heated from room temperature to slightly below the glass softening temperature Tf, which is generally between 570-600°C. In the bending section, the glass temperature is higher than the softening temperature, and the glass has basically softened and is in a relatively plastic state. The action of gravity causes the glass to gradually sag and fit around the mold to form a spherical surface, thereby achieving the curvature and spherical surface requirements of the final product.

[0026] according to Figure 1-2 As shown, after the quenched glass is bent, a laminating machine is needed to insert PVB film into the glass. First, the PVB film is evenly heated and stretched into a fan shape. Then, the PVB film is cooled for 1 hour. At this time, the PVB film is bent. Then, the glass to be inserted with the PVB film is placed on the laminating machine, and the upper piece is sucked up with a vacuum suction cup. The PVB film is placed and then punched through the laminating machine.

[0027] according to Figure 1-2As shown, after the PVB film is placed in the laminating machine, the glass needs to be placed in an autoclave for heating and pressurization. The autoclave is first preheated. When the glass enters the autoclave, it is first heated to 75°C, then pressurized to 0.5Mpa, and then the heating is started and raised together. In order to increase the pressure and temperature at the same time, the temperature change is adjusted according to the temperature of the air in the autoclave. When the autoclave is full of laminated glass, the temperature inside can be higher than the glass temperature. When the temperature inside the laminated glass is consistent with the highest value in the heating stage, the heating process is completed. After heating for 3 to 4 hours, the glass is taken out and cooled for 1 hour to complete the manufacturing.

[0028] according to Figure 1-2 As shown, the laminating machine in step 7 is a double-glass laminating machine with equipment dimensions of L7000mm*W3980mm*H3000mm and a rated power of 4kW.

[0029] according to Figure 1-2 As shown, the autoclave in step 8 adopts a KCFD series high-pressure reactor, which is made of 304 stainless steel.

[0030] The effect achieved by the entire mechanism is as follows: quartz sand, borax, boric acid, barite, barium carbonate, limestone, feldspar, soda ash and other main raw materials are selected, and then the raw materials are cleaned, and the raw materials with a radius of less than 2 cm are removed. The raw materials are then placed in a dryer for drying, and then the raw materials are added to a grinder with a motor power greater than 3000W for crushing. At the same time, an electromagnetic suction cup is used to remove the iron in the raw materials. Polypropylene and nylon are then added to the raw materials. The ratio of polypropylene to nylon is 1 to 2. The raw materials are then fully stirred and mixed in a high-speed blender. After stirring for 30 minutes, the high-speed blender is turned off. , then add UV shielding agent and glass coating agent, the ratio of UV shielding agent to glass coating agent is 1 to 1, continue to turn on the high-speed mixer and continue stirring for 10 minutes, then take out the raw materials, and then put the mixture into the pool kiln or crucible kiln for high-temperature heating. The temperature in the pool kiln or crucible kiln cannot be lower than 1580 degrees. Heat the mixture to form a uniform, bubble-free liquid glass, and send the liquid glass into a tin tank filled with nitrogen and hydrogen protective gas, float on the surface of the tin liquid, spread and thin the glass liquid naturally, and then cool the glass liquid for 3 hours. After that, take out the glass and polish the glass surface, and then send it to the retreat The furnace forms the original glass. The glass is placed in a tempering furnace or a hot bending furnace, heated at a temperature exceeding 700°C, and annealed and cooled. The bending trolley is raised to the upper layer of the bending furnace by a lifting and conveying device, and passes through the preheating section and the bending section in sequence. In the preheating section, the glass is heated from room temperature to slightly below the glass softening temperature Tf, which is generally between 570-600°C. In the bending section, the glass temperature is higher than the softening temperature, and the glass has basically softened and is in a relatively plastic state. The effect of gravity causes the glass to gradually sag and fit around the mold to form a spherical surface. Finally, when the glass is placed in the autoclave, it is first heated to 75°C , then pressurize to 0.5Mpa, then start heating, and rise together. In order to increase the pressure and temperature at the same time, the temperature change is adjusted according to the temperature of the air in the autoclave. When the autoclave is full of laminated glass, the temperature inside can be higher than the glass temperature. When the temperature inside the laminated glass is consistent with the highest value in the heating stage, the heating program is completed. After heating for 3 to 4 hours, the glass is taken out and cooled for 1 hour to complete the manufacturing. The car glass produced by the present invention is convenient for reducing the damage of ultraviolet rays to the skin, reducing the impact of ultraviolet rays on the driver, increasing the driver's driving comfort in hot summer, and convenient for use.

[0031] Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments, or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the scope of protection of the present invention.

Claims

1. A method for producing anti-ultraviolet nano self-cleaning automobile glass, comprising the following steps: S1. When selecting raw materials for processing, various inorganic minerals such as quartz sand, borax, boric acid, barite, barium carbonate, limestone, feldspar, soda ash, etc. are mainly selected as the main raw materials, and a small amount of auxiliary raw materials, including soda, sodium sulfate, dolomite, etc., are added. After the selection of the raw materials for processing is completed, the selected raw materials need to be cleaned to remove the sand, stains, and dust on the surface of the raw materials. After the selected raw materials are cleaned, the defective raw materials need to be removed from the raw materials, and the raw materials with a radius less than 2 cm are removed, and only the raw materials with a radius greater than or equal to 3 cm are retained; S2. After the removal of defective raw materials is completed, the raw materials need to be pre-processed. The raw materials are placed in a dryer to dry the wet raw materials. The power of the dryer is greater than or equal to 3500W. After the pre-processing of the raw materials is completed, the raw materials need to be crushed. The raw materials are added to a crusher with a motor power greater than 3000W for crushing. After the block raw materials are crushed, an electromagnetic chuck is used to remove the iron in the raw materials; S3. After the iron-containing raw material is deironed, the raw material needs to be mixed and prepared. 30 catties of raw material is selected, polypropylene and nylon are added to the raw material, and the ratio of polypropylene to nylon is 1:

2. Then, the raw material is fully stirred and mixed by a high-speed mixer. After stirring for 30 minutes, the high-speed mixer is turned off, and then ultraviolet shielding agent and glass coating agent are added. The ratio of ultraviolet shielding agent to glass coating agent is 1:

1. Then, the high-speed mixer is turned on and stirred for 10 minutes to take out the raw material. S4. After the mixed material is prepared, the mixed material is placed in a tank kiln or a crucible kiln for high-temperature heating. The temperature in the tank kiln or the crucible kiln cannot be lower than 1580 degrees. The mixed material is heated to form a uniform, bubble-free liquid glass. S5. After the mixed glass raw materials are heated in a tank furnace or a crucible furnace, the liquid glass is sent into a tin bath filled with nitrogen and hydrogen protective gas, floated on the surface of the tin liquid, and the glass liquid is naturally flattened and thinned. The glass liquid is then cooled for 3 hours, and the glass is taken out and the surface of the glass is polished. Then, it is sent to an annealing furnace to form raw glass. The raw glass must be cut into blanks first. Cutting oil is used to control the pressure and depth during cutting. After the blank glass is edged, cleaned, and dried, a layer of silicon dioxide will be sprinkled on the surface to prevent sticking during bending. Then, a special person will check whether the glass has impurities or cracks. S6. After the quenching of the formed glass is completed, the glass needs to be bent. The glass is placed in a tempering furnace or a hot bending furnace, heated at a furnace temperature of more than 700°C, and annealed and cooled. Specifically, during production, the corresponding mold is placed in a bending trolley. On the upper and lower pieces, the operator puts the pre-treated qualified semi-finished glass on the mold, and the bending trolley is raised to the upper layer of the bending furnace through the lifting and conveying device. It passes through the preheating section and the bending section in turn. In the preheating section, the glass is heated from room temperature to slightly lower than the glass softening temperature Tf, which is generally between 570 and 600°C. In the bending section, the glass temperature is higher than the softening temperature, and the glass has basically softened and is in a relatively plastic state. The gravity causes the glass to gradually sag and fit around the mold to form a spherical surface, so as to meet the curvature and spherical surface requirements of the final product. S7. After the quenched glass is bent, a laminating machine is used to place a PVB film in the glass. First, the PVB film is evenly heated and stretched into a fan shape. Then, the PVB film is cooled for 1 hour. At this time, the PVB film is bent. Then, the glass to be placed with the PVB film is placed on the laminating machine. The upper glass is sucked up with a vacuum suction cup, and the PVB film is placed. Then, the laminating machine is used for stamping. S8. After the PVB film is placed in the laminating machine, the glass needs to be placed in an autoclave for heating and pressurization. The autoclave is first preheated. When the glass enters the autoclave, it is first heated to 75°C, then pressurized to 0.5Mpa, and then the heating is started and they rise together. In order to increase the pressure and temperature at the same time, the temperature change is adjusted according to the temperature of the air in the autoclave. When the autoclave is full of laminated glass, the temperature inside can be higher than the glass temperature. When the temperature inside the laminated glass is consistent with the highest value in the heating stage, the heating program is completed. After heating for 3 to 4 hours, take out the glass and cool it for 1 hour to complete the manufacturing.

2. The method for producing anti-ultraviolet nano self-cleaning automobile glass according to claim 1, characterized in that: The laminating machine in step 7 is a double-glass laminating machine, and its equipment size is L7000mm*W3980mm*H3000mm and its rated power is 4kW.

3. The method for producing anti-ultraviolet nano self-cleaning automobile glass according to claim 1, characterized in that: The autoclave in step 8 is a KCFD series autoclave made of 304 stainless steel.

Citation Information

Patent Citations

  • Production method of sodium flat protective glass

    CN103449706A

  • Automotive glass processing process