Method for producing 2-hydroxy-3-naphthoic acid by gas-solid phase method
By adding a resin adsorption step to the gas-solid phase production process of 2-hydroxy-3-naphtholic acid, and using macroporous adsorption resin to remove 2-naphthol impurities, the problems of unstable product purity and raw material waste were solved, achieving high-purity and low-cost production results.
Patent Information
- Application Number
- CN202410296988.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-15
- Publication Date
- 2024-11-12
AI Technical Summary
The existing gas-solid phase process for producing 2-hydroxy-3-naphtholic acid results in unstable product purity, the presence of 2-naphthol impurities, which affects high-end applications, and also leads to raw material waste and high production costs.
A resin adsorption step is added between the pressure filtration and acid precipitation processes. Macroporous adsorption resins such as HP-20 or SIP-1200 are used to remove 2-naphthol from the filtrate through resin adsorption, and the eluent is recovered and recycled.
It improves the purity and resource utilization of 2-hydroxy-3-naphthoic acid, reduces production costs and wastewater discharge, and produces products with suitable particle size, easy separation, and strong process stability.
Smart Images

Figure CN118930423A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of organic synthesis and relates to a method for producing 2-hydroxy-3-naphthoic acid by a gas-solid phase method. Background Art
[0002] 2-Hydroxy-3-naphthoic acid, also known as 2,3-acid, is made from 2-naphthol by carboxylation. It is mainly used as an important intermediate for dyes, organic pigments and medicines, and has a wide range of uses. 2-Hydroxy-3-naphthoic acid is not only a raw material for organic pigments and ice dyeing phenol, but also has the function of stabilizing vitamin B2 in medicine. In the synthetic fiber industry, 2-hydroxy-3-naphthoic acid can be condensed with formaldehyde to obtain di-2-hydroxy-3-naphthoic acid, which is an important raw material for the preparation of polyester fibers and polyamide fibers. In recent years, 2-hydroxy-3-naphthoic acid has also been widely used in paints, waterproofing agents, photosensitive materials and other fields.
[0003] In industry, 2-hydroxy-3-naphthoic acid is produced by the Kolbe-Schmidt reaction, that is, 2-naphthol sodium salt undergoes electrophilic substitution with carbon dioxide to generate 2,3-acid disodium salt, and then the 2-hydroxy-3-naphthoic acid product is obtained by neutralization and acid precipitation. At present, the synthesis process is mainly divided into solid phase method and solvent method. Although the two methods have their own advantages, the 2-hydroxy-3-naphthoic acid products produced generally have common problems: the quality of 2-hydroxy-3-naphthoic acid products is unstable, the color is dark, the particles are small, and the content is low, which affects its export competitiveness.
[0004] At present, the gas-solid phase method is mainly used to prepare 2-hydroxy-3-naphthoic acid in industrial production. The specific process is: first, 2-naphthol and liquid alkali react to generate 2-naphthol sodium salt, then carboxylate with carbon dioxide, and remove the by-products generated by the reaction and the 2-naphthol that is not fully reacted through resin residue separation, neutralization, and filter pressing. Finally, the 2-hydroxy-3-naphthoic acid product is obtained through acid precipitation, centrifugation, drying and other processes. Since 2-naphthol has a certain solubility in water, a certain amount of 2-naphthol will exist in the mother liquor after neutralization, cooling and filter pressing. In the acid precipitation process, as the acid value increases during the process, the solubility of 2-naphthol decreases and is precipitated. Therefore, 2-naphthol impurities are inevitably contained in 2-hydroxy-3-naphthoic acid, which affects the purity of the produced 2-hydroxy-3-naphthoic acid and limits the application of 2-hydroxy-3-naphthoic acid in high-end industries. In conventional production processes, reducing the content of beta-naphthol mainly relies on reducing the solubility of beta-naphthol by lowering the temperature of the neutralizing solution, thereby improving the purity of the produced 2-hydroxy-3-naphthoic acid, which not only improves efficiency but also causes waste of raw materials, and the power consumption of production is also high, which is not conducive to the control of product cost. Therefore, it is urgent to develop a new process to improve the purity of 2-hydroxy-3-naphthoic acid.
[0005] Chinese invention patent CN110283065A discloses a 2-hydroxy-3-naphthoic acid production process, which improves the purity of 2-hydroxy-3-naphthoic acid finished product by enhancing the carboxylation reaction rate of ethyl naphthol sodium salt. However, this production process needs to be provided with annular groove plates of several carboxylation reaction grooves in a dehydration autoclave, and the operation is complicated, and the production cost is relatively improved. Chinese invention patent CN1026232C discloses a preparation method of 2-hydroxy-3-naphthoic acid with a content of 99%, and the method improves product purity by adsorbing the 2-naphthol that cannot be separated by post-treatment with activated carbon decolorization, although the method has a single production equipment and less loss of refined products, the 2-naphthol adsorbed with activated carbon decolorization and activated carbon do not realize effective recycling, causing waste of raw materials. Summary of the invention
[0006] In order to overcome the technical problems of the prior art, the object of the present invention is to provide a method for producing 2-hydroxy-3-naphthoic acid by a gas-solid phase process, which can improve the purity of the 2-hydroxy-3-naphthoic acid product while reducing raw material waste and production power consumption, thereby reducing production costs.
[0007] To achieve the above purpose, the technical solution adopted by the present invention is as follows:
[0008] The present invention provides a method for producing 2-hydroxy-3-naphthoic acid by a gas-solid phase process, comprising the following steps:
[0009] (1) Salt-forming reaction: 2-naphthol reacts with a base to form 2-naphthol salt;
[0010] (2) carboxylation reaction: the 2-naphthol salt described in step (1) is subjected to a carboxylation reaction with carbon dioxide to obtain a mixture;
[0011] (3) separating resin residues: separating the resin residues in the mixture described in step (2) to obtain a carboxylated product;
[0012] (4) neutralization reaction: the carboxylation product described in step (3) is subjected to a neutralization reaction with an acid to obtain a reaction solution;
[0013] (5) cooling and filtering: the reaction solution in step (4) is cooled to precipitate 2-naphthol, which is filtered to obtain a filtrate;
[0014] (6) resin adsorption: subjecting the filtrate described in step (5) to resin adsorption to obtain a clear solution after adsorption;
[0015] (7) Acid precipitation reaction: adding acid to the supernatant after adsorption described in step (6) to carry out acid precipitation reaction, and after centrifugation and drying, 2-hydroxy-3-naphthoic acid is obtained;
[0016] In the resin adsorption in step (6), the adsorption temperature is 40-45°C.
[0017] Furthermore, the pH of the reaction solution in step (4) is 4.5-5.8.
[0018] Furthermore, the cooling in step (5) reduces the temperature of the reaction solution to 40-45°C.
[0019] Furthermore, in the resin adsorption of step (6), the concentration of 2-naphthol in the filtrate is 0.005-0.02wt%, the pH of the filtrate is 4.5-5.8, the volume ratio of the filtrate to the resin is 15-20:1, and the adsorption rate of the filtrate is 3-4 resin volumes per hour.
[0020] Furthermore, in the resin adsorption of step (6), the adsorption rate of the filtrate is 3 times the resin volume per hour, and the adsorption temperature is 42°C.
[0021] Furthermore, in the resin adsorption in step (6), the resin is a macroporous adsorption resin; the model of the macroporous adsorption resin is any one of the HP series and the SIP series.
[0022] Furthermore, the macroporous adsorption resin model is any one of HP-20 and SIP-1200.
[0023] Furthermore, step (6) further comprises the following steps:
[0024] (6-1) washing the resin column with water, and then washing the resin column with an alkaline solution, so that the resin loses its adsorption effect on 2-naphthol, and the alkaline solution reacts with 2-naphthol to generate 2-naphthol salt to form a decomposition solution;
[0025] (6-2) The analytical solution described in step (6-1) is added back into the resin residue separation described in step (3).
[0026] Furthermore, in step (6-1), the volume ratio of water to resin is 0.5-1:1, and the temperature of the water is 70-95°C.
[0027] Furthermore, the concentration of the alkaline solution in step (6-1) is 4-4.5 wt%.
[0028] Furthermore, the temperature of the alkaline solution in step (6-1) is 70-95° C., and the volume ratio of the alkaline solution to the resin is 1-1.5:1.
[0029] Furthermore, the reaction time of the alkaline solution and the resin is 30-60 minutes; the alkaline solution enters the resin column from top to bottom.
[0030] Furthermore, the base described in step (6-1) is at least one of sodium hydroxide, potassium hydroxide, aqueous ammonia, sodium ethoxide, sodium methoxide, potassium ethoxide, and potassium methoxide.
[0031] Furthermore, the alkali is sodium hydroxide.
[0032] Furthermore, the acid in step (7) is at least one of sulfuric acid, hydrochloric acid and nitric acid.
[0033] The particle size of 2-hydroxy-3-naphthoic acid product is an important indicator to measure its quality. On the one hand, the appropriate particle size is conducive to expanding the market and increasing competitiveness; on the other hand, if the product particles are small and light in weight, they are prone to loss during the drying process, affecting the yield.
[0034] Compared with the prior art, the present invention has the following beneficial effects:
[0035] The present invention adds a resin adsorption process between the filter pressing and the acid precipitation process, removes the 2-naphthol remaining in the filtrate after the filter pressing by using the macroporous adsorption resin, and improves the purity of 2-hydroxy-3-naphthoic acid.
[0036] The present invention recovers the analytical solution generated after the adsorption saturated resin is analyzed, thereby realizing the recycling of 2-naphthol and improving the resource utilization rate.
[0037] The invention reduces the water consumption in the neutralization section, reduces the wastewater discharge, has a simple process, is easy to operate, has high product purity, and the prepared 2-hydroxy-naphthoic acid product has an appropriate particle size, is easy to separate, is not prone to material leakage, has strong process stability, and has high reliability. BRIEF DESCRIPTION OF THE DRAWINGS
[0038] Figure 1 The present invention is a flow chart of the method for producing 2-hydroxy-3-naphthoic acid by the gas-solid phase method. DETAILED DESCRIPTION
[0039] The following non-limiting examples can enable those skilled in the art to more fully understand the present invention, but do not limit the present invention in any way. The following content is merely an exemplary description of the scope of the present invention, and those skilled in the art can make various changes and modifications to the present invention based on the disclosed content, which should also fall within the scope of the present invention.
[0040] When the embodiments give numerical ranges, it should be understood that, unless otherwise specified in the present invention, both endpoints of each numerical range and any numerical value between the two endpoints can be selected. Unless otherwise defined, all technical and scientific terms used in the present invention have the same meanings as those generally understood by those of ordinary skill in the art to which the present invention belongs.
[0041] The present invention is further described below by way of specific examples. Unless otherwise specified, the various chemical reagents or raw materials used in the examples of the present invention are obtained through conventional commercial channels.
[0042] HP-20 macroporous resin was purchased from Mitsubishi Chemical Corporation.
[0043] SIP-1200 macroporous resin was purchased from Rebo (Shanghai) Biochemical Technology Co., Ltd.
[0044] Example 1
[0045] A method for producing 2-hydroxy-3-naphthoic acid by a gas-solid phase process comprises the following steps:
[0046] (1) Salt-forming reaction: 1450 kg of 2-naphthol and 550 L of 50 wt% sodium hydroxide solution were placed in a salt-forming kettle, stirred and heated to 135° C., and reacted for 50 min to obtain 2-naphthol salt;
[0047] (2) Carboxylation reaction: the 2-naphthol salt generated in step (1) is pressed into an autoclave, the autoclave is heated, the pressure is controlled to be 0.2 MPa, and dehydration is performed; when the temperature rises to 240° C., the autoclave is depressurized, evacuated, and reduced-pressure drying is started for 30 min. When the temperature drops to 230° C., the vacuum is stopped, and carbon dioxide is introduced step by step, and the 2-naphthol generated by the reaction is recovered by distillation. After the reaction is completed, the pressure is released, and 2.5 m 3 Dilute with water to obtain a mixture solution;
[0048] The step (2) of introducing carbon dioxide in steps and simultaneously distilling and recovering the 2-naphthol generated by the reaction is specifically as follows: the first step of carboxylation: introducing carbon dioxide into the autoclave, keeping the carbon dioxide pressure in the autoclave at 0.4-0.7Mpa, and reacting for 15 minutes; the first step of distillation: exhausting the carbon dioxide pressure, distilling under reduced pressure, and recovering the 2-naphthol; the second step of carboxylation: introducing carbon dioxide into the autoclave, keeping the carbon dioxide pressure in the autoclave at 0.4-0.7Mpa, and reacting for 50 minutes; the second step of distillation: exhausting the carbon dioxide pressure, distilling under reduced pressure, and recovering the 2-naphthol; the third step of carboxylation: introducing carbon dioxide into the autoclave, keeping the carbon dioxide pressure in the autoclave at 0.4-0.7Mpa, and reacting for 20 minutes; the third step of distillation: exhausting the carbon dioxide pressure, distilling under reduced pressure, and recovering the 2-naphthol;
[0049] (3) Resin residue separation: Add 10m3 of 3 water, pumping the mixture solution obtained in step (2) into a resin separation barrel, standing for stratification, separating about 100 kg of the generated resin residue, taking the supernatant, and obtaining a carboxylation product solution;
[0050] (4) Neutralization reaction: the carboxylation product solution obtained in step (3) was heated to 55° C., and then a sulfuric acid solution (35 wt %) was slowly added, the temperature was controlled at 55° C., and a neutralization reaction was performed until the pH value reached 5.5 to obtain a reaction solution;
[0051] (5) Cooling and filtering: cooling the reaction solution obtained in step (4) to 42° C. to precipitate 2-naphthol, filtering the solution to obtain a filtrate and a filter cake, distilling the filter cake to recover the 2-naphthol, wherein the pressure of the filtering is ≤0.2 MPa;
[0052] (6) Resin adsorption: The filtrate obtained in step (5) is subjected to resin adsorption until saturation, thereby obtaining a clear solution after adsorption;
[0053] In the resin adsorption of step (6), the concentration of 2-naphthol in the filtrate is 0.013wt%, the pH of the filtrate is 5.5, the volume ratio of the filtrate to the resin is 16.5:1, and the resin filling volume is 10m 3 , the adsorption rate of the filtrate is 3 times the resin filling volume per hour, and the adsorption temperature is 42°C;
[0054] Step (6) further includes the following steps:
[0055] (6-1): When the resin adsorption reaches saturation, add 0.5 times the volume of resin into the macroporous adsorption resin from top to bottom along the resin column, and push the liquid in the resin column to the post-filtration liquid tank, which can reduce material loss and reduce the amount of alkali at the same time;
[0056] (6-2): Add 1 times the volume of the resin into the macroporous adsorption resin. Add alkali from top to bottom along the resin column. After the sodium hydroxide is added, the resin column is allowed to stand for 40 minutes. When the feed liquid becomes turbid, start collecting the analytical solution. At the same time, take samples to detect the alkali concentration and COD, and observe the color of the analytical solution. When the color of the analytical solution becomes transparent, stop collecting the analytical solution, and return the analytical solution to step (3) for continued use in resin residue separation;
[0057] (6-3): Add 0.5 times the volume of 85°C water into the macroporous adsorption resin from top to bottom along the resin column to push out the low-concentration analytical solution in the resin column. The solution contains a certain alkali concentration and can be used for further preparation of alkali.
[0058] The macroporous adsorption resin used in step (6) is HP-20 macroporous adsorption resin;
[0059] (7) Acid precipitation reaction: The supernatant after adsorption described in step (6) is heated to 98° C., and then sulfuric acid (35 wt %) is added to adjust the pH to 2, and an acid precipitation reaction is carried out. After reacting for 25 min, the mixture is centrifuged and dried to obtain 2-hydroxy-3-naphthoic acid.
[0060] The purity of 2-hydroxy-3-naphthoic acid was 99.61%.
[0061] Reducing the water consumption in the neutralization stage by 10% per pot can reduce the amount of wastewater per ton of product by 9%.
[0062] The particle size of the 2-hydroxy-3-naphthoic acid product was measured to be 497 μm, and the centrifugal filtration was good.
[0063] Example 2
[0064] A method for producing 2-hydroxy-3-naphthoic acid by a gas-solid phase process comprises the following steps:
[0065] (1) Salt-forming reaction: 1450 kg of 2-naphthol and 550 L of 50 wt% sodium hydroxide solution were placed in a salt-forming kettle, stirred and heated to 135° C., and reacted for 50 min to obtain 2-naphthol salt;
[0066] (2) Carboxylation reaction: the 2-naphthol salt generated in step (1) is pressed into an autoclave, the autoclave is heated, the pressure is controlled to be 0.2 MPa, and dehydration is performed; when the temperature rises to 240° C., the autoclave is depressurized, evacuated, and reduced-pressure drying is started for 30 min. When the temperature drops to 230° C., the vacuum is stopped, and carbon dioxide is introduced step by step, and the 2-naphthol generated by the reaction is recovered by distillation. After the reaction is completed, the pressure is released, and 2.5 m 3 Dilute with water to obtain a mixture solution;
[0067] The step (2) of introducing carbon dioxide in steps and simultaneously distilling and recovering the 2-naphthol generated by the reaction is specifically as follows: the first step of carboxylation: introducing carbon dioxide into the autoclave, keeping the carbon dioxide pressure in the autoclave at 0.4-0.7Mpa, and reacting for 15 minutes; the first step of distillation: exhausting the carbon dioxide pressure, distilling under reduced pressure, and recovering the 2-naphthol; the second step of carboxylation: introducing carbon dioxide into the autoclave, keeping the carbon dioxide pressure in the autoclave at 0.4-0.7Mpa, and reacting for 50 minutes; the second step of distillation: exhausting the carbon dioxide pressure, distilling under reduced pressure, and recovering the 2-naphthol; the third step of carboxylation: introducing carbon dioxide into the autoclave, keeping the carbon dioxide pressure in the autoclave at 0.4-0.7Mpa, and reacting for 20 minutes; the third step of distillation: exhausting the carbon dioxide pressure, distilling under reduced pressure, and recovering the 2-naphthol;
[0068] (3) Resin residue separation: Add 10m3 of 3 water, pumping the mixture solution obtained in step (2) into a resin separation barrel, standing for stratification, separating about 100 kg of the generated resin residue, taking the supernatant, and obtaining a carboxylation product solution;
[0069] (4) Neutralization reaction: the carboxylation product solution obtained in step (3) was heated to 55° C., and then a sulfuric acid solution (35 wt %) was slowly added, the temperature was controlled at 55° C., and a neutralization reaction was performed until the pH value was 5.3 to obtain a reaction solution;
[0070] (5) Cooling and filtering: cooling the reaction solution obtained in step (4) to 44° C. to precipitate 2-naphthol, filtering the solution to obtain a filtrate and a filter cake, distilling the filter cake to recover the 2-naphthol, wherein the pressure of the filtering is ≤0.2 MPa;
[0071] (6) Resin adsorption: The filtrate obtained in step (5) is subjected to resin adsorption until saturation, thereby obtaining a clear solution after adsorption;
[0072] In the resin adsorption of step (6), the concentration of 2-naphthol in the filtrate is 0.015wt%, the pH is 5.3, the volume ratio of the filtrate to the resin is 15:1, and the resin filling volume is 10m 3 , the adsorption rate of the filtrate is 3 times the volume of resin per hour, and the adsorption temperature is 44°C;
[0073] Step (6) further includes the following steps:
[0074] (6-1): When the resin adsorption reaches saturation, add 0.5 times the volume of resin into the macroporous adsorption resin from top to bottom along the resin column, and push the liquid in the resin column to the post-filtration liquid tank, which can reduce material loss and reduce the amount of alkali used;
[0075] (6-2): Add 1 times the volume of the resin into the macroporous adsorption resin. Add alkali from top to bottom along the resin column. After the sodium hydroxide is added, the resin column is allowed to stand for 40 minutes. When the feed liquid becomes turbid, start collecting the analytical solution. At the same time, take samples to detect the alkali concentration and COD, and observe the color of the analytical solution. When the color of the analytical solution becomes transparent, stop collecting the analytical solution, and return the analytical solution to step (3) for continued use in resin residue separation;
[0076] (6-3): Add 0.5 times the volume of 85°C water into the macroporous adsorption resin from top to bottom along the resin column to push out the low-concentration analytical solution in the resin column. The solution contains a certain alkali concentration and can be used for further preparation of alkali.
[0077] The macroporous adsorption resin used in step (6) is HP-20 macroporous adsorption resin;
[0078] (7) Acid precipitation reaction: The supernatant after adsorption described in step (6) is heated to 98° C., and then sulfuric acid (35 wt %) is added to adjust the pH to 2, and an acid precipitation reaction is carried out. After reacting for 25 min, the mixture is centrifuged and dried to obtain 2-hydroxy-3-naphthoic acid.
[0079] The purity of 2-hydroxy-3-naphthoic acid was 99.58%.
[0080] Reducing the water consumption in the neutralization stage by 10% per pot can reduce the amount of wastewater per ton of product by 9%.
[0081] The particle size of the 2-hydroxy-3-naphthoic acid product was measured to be 478 μm, and the centrifugal filtration was good.
[0082] Example 3
[0083] A method for producing 2-hydroxy-3-naphthoic acid by a gas-solid phase process comprises the following steps:
[0084] (1) Salt-forming reaction: 1450 kg of 2-naphthol and 550 L of 50 wt% sodium hydroxide solution were placed in a salt-forming kettle, stirred and heated to 135° C., and reacted for 50 min to obtain 2-naphthol salt;
[0085] (2) Carboxylation reaction: the 2-naphthol salt generated in step (1) is pressed into an autoclave, the autoclave is heated, the pressure is controlled to be 0.2 MPa, and dehydration is performed; when the temperature rises to 240° C., the autoclave is depressurized, evacuated, and reduced-pressure drying is started for 30 min. When the temperature drops to 230° C., the vacuum is stopped, and carbon dioxide is introduced step by step, and the 2-naphthol generated by the reaction is recovered by distillation. After the reaction is completed, the pressure is released, and 2.5 m 3 Dilute with water to obtain a mixture solution;
[0086] The step (2) of introducing carbon dioxide in steps and simultaneously distilling and recovering the 2-naphthol generated by the reaction is specifically as follows: the first step of carboxylation: introducing carbon dioxide into the autoclave, keeping the carbon dioxide pressure in the autoclave at 0.4-0.7Mpa, and reacting for 15 minutes; the first step of distillation: exhausting the carbon dioxide pressure, distilling under reduced pressure, and recovering the 2-naphthol; the second step of carboxylation: introducing carbon dioxide into the autoclave, keeping the carbon dioxide pressure in the autoclave at 0.4-0.7Mpa, and reacting for 50 minutes; the second step of distillation: exhausting the carbon dioxide pressure, distilling under reduced pressure, and recovering the 2-naphthol; the third step of carboxylation: introducing carbon dioxide into the autoclave, keeping the carbon dioxide pressure in the autoclave at 0.4-0.7Mpa, and reacting for 20 minutes; the third step of distillation: exhausting the carbon dioxide pressure, distilling under reduced pressure, and recovering the 2-naphthol;
[0087] (3) Resin residue separation: Add 10m3 of 3 water, pumping the mixture solution obtained in step (2) into a resin separation barrel, standing for stratification, separating about 100 kg of the generated resin residue, taking the supernatant, and obtaining a carboxylation product solution;
[0088] (4) Neutralization reaction: the carboxylation product solution obtained in step (3) was heated to 55° C., and then a sulfuric acid solution (35 wt %) was slowly added, the temperature was controlled at 55° C., and a neutralization reaction was performed until the pH value reached 4.5 to obtain a reaction solution;
[0089] (5) Cooling and filtering: cooling the reaction solution obtained in step (4) to 42° C. to precipitate 2-naphthol, filtering the solution to obtain a filtrate and a filter cake, distilling the filter cake to recover the 2-naphthol, wherein the pressure of the filtering is ≤0.2 MPa;
[0090] (6) Resin adsorption: The filtrate obtained in step (5) is subjected to resin adsorption until saturation, thereby obtaining a clear solution after adsorption;
[0091] In the resin adsorption of step (6), the concentration of 2-naphthol in the filtrate is 0.012wt%, the pH is 4.5, the volume ratio of the filtrate to the resin is 18.5:1, and the resin filling volume is 10m 3 , the adsorption rate of the filtrate is 3 times the volume of resin per hour, and the adsorption temperature is 45°C;
[0092] Step (6) further includes the following steps:
[0093] (6-1): When the resin adsorption reaches saturation, add 0.5 times the volume of resin into the macroporous adsorption resin from top to bottom along the resin column, and push the liquid in the resin column to the post-filtration liquid tank, which can reduce material loss and reduce the amount of alkali used at the same time;
[0094] (6-2): Add 1 times the volume of the resin into the macroporous adsorption resin. Add alkali from top to bottom along the resin column. After the sodium hydroxide is added, the resin column is allowed to stand for 60 minutes. When the feed liquid becomes turbid, start collecting the analytical solution. At the same time, take samples to detect the alkali concentration and COD, and observe the color of the analytical solution. When the color of the analytical solution becomes transparent, stop collecting the analytical solution, and return the analytical solution to step (3) for continued use in resin residue separation;
[0095] (6-3): Add 0.5 times the volume of the resin into the macroporous adsorption resin from top to bottom along the resin column to push out the low-concentration analytical solution in the resin column. The solution contains a certain alkali concentration and can be used for further preparation of alkali.
[0096] The macroporous adsorption resin used in step (6) is HP-20 macroporous adsorption resin;
[0097] (7) Acid precipitation reaction: The supernatant after adsorption described in step (6) is heated to 98° C., and then sulfuric acid (35 wt %) is added to adjust the pH to 2, and an acid precipitation reaction is carried out. After reacting for 25 min, the mixture is centrifuged and dried to obtain 2-hydroxy-3-naphthoic acid.
[0098] The purity of 2-hydroxy-3-naphthoic acid was 99.55%.
[0099] Reducing the water consumption in the neutralization stage by 10% per pot can reduce the amount of wastewater per ton of product by 9%.
[0100] The particle size of the 2-hydroxy-3-naphthoic acid product was measured to be 484 μm, and the centrifugal filtration was good.
[0101] Example 4
[0102] A method for producing 2-hydroxy-3-naphthoic acid by a gas-solid phase process comprises the following steps:
[0103] (1) Salt-forming reaction: 1450 kg of 2-naphthol and 550 L of 50 wt% sodium hydroxide solution were placed in a salt-forming kettle, stirred and heated to 135° C., and reacted for 50 min to obtain 2-naphthol salt;
[0104] (2) Carboxylation reaction: the 2-naphthol salt generated in step (1) is pressed into an autoclave, the autoclave is heated, the pressure is controlled to be 0.2 MPa, and dehydration is performed; when the temperature rises to 240° C., the autoclave is depressurized, evacuated, and reduced-pressure drying is started for 30 min. When the temperature drops to 230° C., the vacuum is stopped, and carbon dioxide is introduced step by step, and the 2-naphthol generated by the reaction is recovered by distillation. After the reaction is completed, the pressure is released, and 2.5 m 3 Dilute with water to obtain a mixture solution;
[0105] The step (2) of introducing carbon dioxide in steps and simultaneously distilling and recovering the 2-naphthol generated by the reaction is specifically as follows: the first step of carboxylation: introducing carbon dioxide into the autoclave, keeping the carbon dioxide pressure in the autoclave at 0.4-0.7Mpa, and reacting for 15 minutes; the first step of distillation: exhausting the carbon dioxide pressure, distilling under reduced pressure, and recovering the 2-naphthol; the second step of carboxylation: introducing carbon dioxide into the autoclave, keeping the carbon dioxide pressure in the autoclave at 0.4-0.7Mpa, and reacting for 50 minutes; the second step of distillation: exhausting the carbon dioxide pressure, distilling under reduced pressure, and recovering the 2-naphthol; the third step of carboxylation: introducing carbon dioxide into the autoclave, keeping the carbon dioxide pressure in the autoclave at 0.4-0.7Mpa, and reacting for 20 minutes; the third step of distillation: exhausting the carbon dioxide pressure, distilling under reduced pressure, and recovering the 2-naphthol;
[0106] (3) Resin residue separation: Add 10m3 of 3 water, pumping the mixture solution obtained in step (2) into a resin separation barrel, standing for stratification, separating about 100 kg of the generated resin residue, taking the supernatant, and obtaining a carboxylation product solution;
[0107] (4) Neutralization reaction: the carboxylation product solution obtained in step (3) was heated to 55° C., and then a sulfuric acid solution (35 wt %) was slowly added, the temperature was controlled at 55° C., and a neutralization reaction was performed until the pH value reached 4.8 to obtain a reaction solution;
[0108] (5) Cooling and filtering: cooling the reaction solution obtained in step (4) to 42° C. to precipitate 2-naphthol, filtering the solution to obtain a filtrate and a filter cake, distilling the filter cake to recover the 2-naphthol, wherein the pressure of the filtering is ≤0.2 MPa;
[0109] (6) Resin adsorption: The filtrate obtained in step (5) is subjected to resin adsorption until saturation, thereby obtaining a clear solution after adsorption;
[0110] In the resin adsorption of step (6), the concentration of 2-naphthol in the filtrate is 0.011wt%, the pH is 4.8, the volume ratio of the filtrate to the resin is 20:1, and the resin filling volume is 10m 3 , the adsorption rate of the filtrate is 3 times the volume of resin per hour, and the adsorption temperature is 41°C;
[0111] Step (6) further includes the following steps:
[0112] (6-1): When the resin adsorption reaches saturation, add 90°C water (1 times the volume of the resin) into the macroporous adsorption resin from top to bottom along the resin column, and push the liquid in the resin column to the post-filtration liquid tank, which can reduce material loss and also reduce the amount of alkali used;
[0113] (6-2): Add 1.5 times the volume of the resin into the macroporous adsorption resin. Add alkali from top to bottom along the resin column. After adding sodium hydroxide, let the resin column stand for 30 minutes. When the feed liquid becomes turbid, start collecting the analytical solution. At the same time, take samples to detect the alkali concentration and COD, and observe the color of the analytical solution. When the color of the analytical solution becomes transparent, stop collecting the analytical solution, and return the analytical solution to step (3) for continued use in resin residue separation;
[0114] (6-3): Add 0.5 times the volume of 90°C water into the macroporous adsorption resin from top to bottom along the resin column to push out the low-concentration analytical solution in the resin column. The solution contains a certain alkali concentration and can be used for further preparation of alkali.
[0115] The macroporous adsorption resin used in step (6) is HP-20 macroporous adsorption resin;
[0116] (7) Acid precipitation reaction: The supernatant after adsorption described in step (6) is heated to 98° C., and then sulfuric acid (35 wt %) is added to adjust the pH to 2, and an acid precipitation reaction is carried out. After reacting for 25 min, the mixture is centrifuged and dried to obtain 2-hydroxy-3-naphthoic acid.
[0117] The purity of 2-hydroxy-3-naphthoic acid was 99.62%.
[0118] Reducing the water consumption in the neutralization stage by 10% per pot can reduce the amount of wastewater per ton of product by 9%.
[0119] The particle size of the 2-hydroxy-3-naphthoic acid product was measured to be 469 μm, and the centrifugal filtration was good.
[0120] Example 5
[0121] A method for producing 2-hydroxy-3-naphthoic acid by a gas-solid phase process comprises the following steps:
[0122] (1) Salt-forming reaction: 1450 kg of 2-naphthol and 550 L of 50 wt% sodium hydroxide solution were placed in a salt-forming kettle, stirred and heated to 135° C., and reacted for 50 min to obtain 2-naphthol salt;
[0123] (2) Carboxylation reaction: the 2-naphthol salt generated in step (1) is pressed into an autoclave, the autoclave is heated, the pressure is controlled to be 0.2 MPa, and dehydration is performed; when the temperature rises to 240° C., the autoclave is depressurized, evacuated, and reduced-pressure drying is started for 30 min. When the temperature drops to 230° C., the vacuum is stopped, and carbon dioxide is introduced step by step, and the 2-naphthol generated by the reaction is recovered by distillation. After the reaction is completed, the pressure is released, and 2.5 m 3 Dilute with water to obtain a mixture solution;
[0124] The step (2) of introducing carbon dioxide in steps and simultaneously distilling and recovering the 2-naphthol generated by the reaction is specifically as follows: the first step of carboxylation: introducing carbon dioxide into the autoclave, keeping the carbon dioxide pressure in the autoclave at 0.4-0.7Mpa, and reacting for 15 minutes; the first step of distillation: exhausting the carbon dioxide pressure, distilling under reduced pressure, and recovering the 2-naphthol; the second step of carboxylation: introducing carbon dioxide into the autoclave, keeping the carbon dioxide pressure in the autoclave at 0.4-0.7Mpa, and reacting for 50 minutes; the second step of distillation: exhausting the carbon dioxide pressure, distilling under reduced pressure, and recovering the 2-naphthol; the third step of carboxylation: introducing carbon dioxide into the autoclave, keeping the carbon dioxide pressure in the autoclave at 0.4-0.7Mpa, and reacting for 20 minutes; the third step of distillation: exhausting the carbon dioxide pressure, distilling under reduced pressure, and recovering the 2-naphthol;
[0125] (3) Resin residue separation: Add 10m3 of 3 water, pumping the mixture solution obtained in step (2) into a resin separation barrel, standing for stratification, separating about 100 kg of the generated resin residue, taking the supernatant, and obtaining a carboxylation product solution;
[0126] (4) Neutralization reaction: the carboxylation product solution obtained in step (3) was heated to 55° C., and then a sulfuric acid solution (35 wt %) was slowly added, the temperature was controlled at 55° C., and a neutralization reaction was performed until the pH value was 5.8 to obtain a reaction solution;
[0127] (5) Cooling and filtering: cooling the reaction solution obtained in step (4) to 42° C. to precipitate 2-naphthol, filtering the solution to obtain a filtrate and a filter cake, distilling the filter cake to recover the 2-naphthol, wherein the pressure of the filtering is ≤0.2 MPa;
[0128] (6) Resin adsorption: The filtrate obtained in step (5) is subjected to resin adsorption until saturation, thereby obtaining a clear solution after adsorption;
[0129] In the resin adsorption of step (6), the concentration of 2-naphthol in the filtrate is 0.015wt%, the pH is 5.8, the volume ratio of the filtrate to the resin is 15:1, and the resin filling volume is 10m 3 , the adsorption rate of the filtrate is 3 times the volume of resin per hour, and the adsorption temperature is 44°C;
[0130] Step (6) further includes the following steps:
[0131] (6-1): When the resin adsorption reaches saturation, add 0.5 times the volume of the resin into the macroporous adsorption resin from top to bottom along the resin column, and push the liquid in the resin column to the post-filtration liquid tank, which can reduce material loss and reduce the amount of alkali used at the same time;
[0132] (6-2): Add 1 times the volume of the resin into the macroporous adsorption resin. Sodium hydroxide solution (4 wt%) at 95°C is added from top to bottom along the resin column. After the sodium hydroxide is added, the resin column is allowed to stand for 40 minutes. When the feed liquid becomes turbid, the analytical solution is collected. At the same time, samples are taken to detect the alkali concentration and COD. The color of the analytical solution is observed. When the color of the analytical solution becomes transparent, the analytical solution is stopped from being collected. The analytical solution is returned to step (3) for continued use in the separation of resin residues.
[0133] (6-3): Add 0.5 times the volume of the resin into the macroporous adsorption resin from top to bottom along the resin column to push out the low-concentration analytical solution in the resin column. The solution contains a certain alkali concentration and can be used for further preparation of alkali.
[0134] The macroporous adsorption resin used in step (6) is a SIP-1200 macroporous adsorption resin;
[0135] (7) Acid precipitation reaction: The supernatant after adsorption described in step (6) is heated to 98° C., and then sulfuric acid (35 wt %) is added to adjust the pH to 2, and an acid precipitation reaction is carried out. After reacting for 25 min, the mixture is centrifuged and dried to obtain 2-hydroxy-3-naphthoic acid.
[0136] The purity of 2-hydroxy-3-naphthoic acid was 99.53%.
[0137] Reducing the water consumption in the neutralization stage by 10% per pot can reduce the amount of wastewater per ton of product by 9%.
[0138] The particle size of the 2-hydroxy-3-naphthoic acid product was measured to be 438 μm, and the centrifugal filtration was good.
[0139] Comparative Example 1
[0140] The difference between this comparative example and Example 1 is that the macroporous adsorption resin used in step (6) is replaced by LX-300C resin instead of HP-20.
[0141] The purity of 2-hydroxy-3-naphthoic acid was 98.53%.
[0142] The particle size of the 2-hydroxy-3-naphthoic acid product was measured to be 235 μm. It was difficult to dehydrate by centrifugation, the product had a high water content, and the drying cost was high.
[0143] Comparative Example 2
[0144] The difference between this comparative example and Example 1 is that in the resin adsorption in step (6), the concentration of 2-naphthol in the filtrate is changed to 0.03 wt %.
[0145] The purity of 2-hydroxy-3-naphthoic acid was 98.49%.
[0146] Comparative Example 3
[0147] The difference between this comparative example and Example 1 is that in the resin adsorption in step (6), the pH of the filtrate is changed to 6.1.
[0148] The purity of 2-hydroxy-3-naphthoic acid was 98.48%.
[0149] Comparative Example 4
[0150] The difference between this comparative example and Example 1 is that the cooling temperature in step (5) is 48° C., and in the resin adsorption in step (6), the adsorption temperature of the filtrate is changed to 48° C.
[0151] The purity of 2-hydroxy-3-naphthoic acid was 98.45%.
[0152] Finally, it should be noted that the above content is only used to illustrate the technical solution of the present invention, rather than to limit the scope of protection of the present invention. Simple modifications or equivalent substitutions of the technical solution of the present invention by ordinary technicians in this field do not deviate from the essence and scope of the technical solution of the present invention.
Claims
1. A method for producing 2-hydroxy-3-naphthoic acid by a gas-solid phase process, characterized in that: The following steps are involved: (1) Salt-forming reaction: 2-naphthol reacts with a base to form 2-naphthol salt; (2) carboxylation reaction: the 2-naphthol salt described in step (1) is subjected to a carboxylation reaction with carbon dioxide to obtain a mixture; (3) separating resin residues: separating the resin residues in the mixture described in step (2) to obtain a carboxylated product; (4) neutralization reaction: the carboxylation product described in step (3) is subjected to a neutralization reaction with an acid to obtain a reaction solution; (5) cooling and filtering: the reaction solution in step (4) is cooled to precipitate 2-naphthol, which is filtered to obtain a filtrate; (6) resin adsorption: subjecting the filtrate described in step (5) to resin adsorption to obtain a clear solution after adsorption; (7) Acid precipitation reaction: adding acid to the supernatant after adsorption described in step (6) to carry out acid precipitation reaction, and after centrifugation and drying, 2-hydroxy-3-naphthoic acid is obtained; In the resin adsorption described in step (6), the adsorption temperature is 40-45°C.
2. The method according to claim 1, characterized in that The pH value of the reaction solution in step (4) is 4.5-5.8; the cooling in step (5) reduces the temperature of the reaction solution to 40-45°C.
3. The method according to claim 1, characterized in that In the resin adsorption of step (6), the concentration of 2-naphthol in the filtrate is 0.005-0.02wt%, and the pH of the filtrate is 4.5-5.
8.
4. The method according to claim 1, characterized in that: In the resin adsorption of step (6), the volume ratio of the filtrate to the resin is 15-20:1, and the adsorption rate of the filtrate is 3-4 times the volume of the resin per hour.
5. The method according to claim 1, characterized in that In the resin adsorption in step (6), the resin is a macroporous adsorption resin, and the model of the macroporous adsorption resin is any one of the HP series and the SIP series.
6. The method according to claim 5, characterized in that The model of the macroporous adsorption resin is selected from any one of HP-20 and SIP-1200.
7. The method according to claim 1, characterized in that Step (6) further includes the following steps: (6-1) washing the resin column with water and then with an alkaline solution to make the resin lose its adsorption effect on 2-naphthol and form a analytical solution; (6-2) The analytical solution obtained in step (6-1) is added back into the resin residue separation described in step (3).
8. The method according to claim 7, characterized in that In step (6-1), the volume ratio of water to resin is 0.5-1:1, and the temperature of the water is 70-95°C.
9. The method according to claim 7, characterized in that: The concentration of the alkaline solution described in step (6-1) is 4-4.5wt%; the temperature of the alkaline solution is 70-95°C, and the volume ratio of the alkaline solution to the resin is 1-1.5:1; the reaction time of the alkaline solution and the resin in step (6-1) is 30-60min; the alkaline solution enters the resin column from top to bottom.
10. The method according to claim 7, characterized in that The base described in step (6-1) is at least one of sodium hydroxide, potassium hydroxide, aqueous ammonia, sodium ethoxide, sodium methoxide, potassium ethoxide and potassium methoxide.
Citation Information
Patent Citations
Method for preparation of 2-hydroxy-3-naphthalenformic acid with content of 99 percentage
CN1026232C
Technology for producing 2-hydroxy-3-naphthoic acid
CN110283065A