Oil seal material and preparation method thereof

By modifying the formulation and preparation method of components such as molybdenum disulfide and carbon black, the problem of insufficient friction resistance of fluoroelastomer is solved, the wear resistance and thermal conductivity of the oil sealing material are improved, and the use needs at high speeds are met.

CN118931071APending Publication Date: 2024-11-12QINGDAO HILYWILL ADVANCED MATERIALS TECH
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202410886981.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-03
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

Due to insufficient friction resistance in seals, fluoroelastomer is prone to wear and seal failure, which makes it difficult to meet the requirements of use at high speeds.

Method used

The low-friction oil sealing material formula with modified molybdenum disulfide and carbon black is used to improve the friction and thermal conductivity of the rubber and enhance its wear resistance through the preparation method of modified molybdenum disulfide and specific kneading steps.

Benefits of technology

It significantly improves the wear resistance and thermal conductivity of the oil sealing material, reduces the friction coefficient, and extends the service life of the seal.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The low-friction oil seal material comprises the following components in parts by weight: 90-110 parts of fluororubber; 25 to 35 parts of carbon black N990; 5.0 to 10.0 parts of molybdenum disulfide; 0.1 to 1.5 parts of palm wax; 5.0 to 10.0 parts of magnesium oxide; 1.0 to 6.0 parts of calcium hydroxide; 1.0 to 2.0 parts of bisphenol AF; and preferably, the molybdenum disulfide is subjected to modification treatment. The low-friction sealing material is wide in application range and is used for rubber products with relatively high requirements on wear resistance and heat resistance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of rubber compounds, in particular to rubber products with high requirements on wear resistance and heat resistance. Background Art

[0002] Fluororubber is widely used in seals, especially in oil seal products. There are many types of fluororubber, mainly divided into four categories: vinylidene fluoride fluororubber, nitroso fluororubber, perfluoroether fluororubber and fluorinated phosphazene fluororubber. Fluororubber has excellent high temperature resistance, oil resistance and corrosion resistance because it has fluorine atoms connected to the carbon atoms of the main chain or side chain of the molecular polymer. However, compared with other elastomer rubbers, fluororubber has slightly worse processing performance and is not easy to form.

[0003] Fluororubber has insufficient friction resistance and is prone to wear during use. After long-term use, the seal is prone to failure. As people's requirements for automotive technology and comfort are getting higher and higher, the requirements for the performance of oil seal products are also gradually increasing. Ordinary fluororubber oil seals are not conducive to use at high speeds due to their large friction coefficient.

[0004] CN106317712A discloses a fluororubber for an engine oil seal, wherein every 100 parts of fluororubber raw rubber contains 0.5-1.5 parts by mass of modified graphene, wherein the modified graphene is a composite nanoparticle formed by calcining graphite oxide after surface modification with polyacrylamide and co-precipitation with aluminum hydroxide. After the modification, the friction coefficient of the fluororubber material is greatly reduced and the thermal conductivity is greatly improved.

[0005] CN112592550A discloses a fluororubber material for oil seal and a preparation method thereof. The fluororubber has a low friction coefficient and a high thermal conductivity coefficient. The fluororubber material uses 2462 type fluororubber as a base material and improves the performance of the fluororubber material by adding multi-component anti-friction and thermal conductive materials and composite organic polymers. Summary of the invention

[0006] The object of the present invention is to provide a low-friction rubber material, the wear resistance of the oil seal made of the material is greatly improved.

[0007] One aspect of the present invention discloses a low-friction oil seal material, which comprises the following components in parts by weight: 90-110 fluororubber; 25-35 carbon black N990; 5.0-10.0 molybdenum disulfide; 0.1-1.5 palm wax; 5.0-10.0 magnesium oxide; 1.0-6.0 calcium hydroxide; 1.0-2.0 bisphenol AF; and 0.1-0.8 benzyltriphenylphosphonium chloride (BPP).

[0008] Preferably, the low-friction oil seal material comprises the following components in parts by weight: 95-105 fluororubber; 30-35 carbon black N990; 7.0-8.0 molybdenum disulfide; 0.5-1.0 palm wax; 7.0-8.0 magnesium oxide; 3.0-4.0 calcium hydroxide; 1.5-1.7 bisphenol AF; and 0.3-0.6 benzyl triphenylphosphine chloride (BPP).

[0009] Preferably, the molybdenum disulfide of the present invention is subjected to a modification treatment, and the modification treatment is carried out by using a solution blending method to undergo in-situ polymerization by a 3-caprolactam ring-opening reaction to obtain a functionalized modified molybdenum disulfide, and then surface modification is performed using siloxane to obtain a modified molybdenum disulfide with improved mechanical properties and better dispersibility.

[0010] The preparation method of the modified molybdenum disulfide comprises the following steps: a) acid washing the molybdenum disulfide and then heating and drying; b) mixing molybdenum disulfide and 3-caprolactam in proportion, adding an initiator and reacting at 120-200° C.; c) washing and drying the reaction product obtained in step b), adding siloxane and water, and filtering and drying after ultrasonic stirring to obtain modified molybdenum disulfide.

[0011] In the pickling in step a), one of sulfuric acid, hydrochloric acid and nitric acid with a molar concentration of less than 1M is used; in the modification reaction in step b), the initiator used is one of zinc persulfate and benzoyl peroxide; in step b), the mass ratio of molybdenum disulfide, 3-caprolactam and initiator is 100-120:50-70:1-5.

[0012] In step d), the mass ratio of the reaction product obtained in step c) to siloxane and water is 100-120:30-50:60-100; and the ultrasonic treatment time is 1-10 min.

[0013] The present invention provides a method for preparing a low-friction oil seal material, comprising the following steps in sequence: S1. First, put the fluororubber into the internal mixer and mix for 60-90 seconds, then put in carbon black N990, palm wax, magnesium oxide and calcium hydroxide, and continue mixing for 180-240 seconds until there is no white powder on the surface; S2, adding molybdenum disulfide to the mixed materials in step S1, and then mixing for 90-120S until the color is uniform; S3, discharge the mixed materials in step S2 to an open mixing mill, thinly slice them, and leave them for 16 hours; S4, putting the mixture obtained in step S3 into the internal mixer again, adding bisphenol AF and benzyl triphenylphosphonium chloride (BPP) thereto, and mixing for 180-240 seconds; S5, discharge the mixed materials in step S4 to an open mixing mill, and sheet them after thinning.

[0014] Preferably, the mixing in steps S1, S2 and S4 is carried out at a rotation speed of 20-50 rpm.

[0015] Preferably, the number of thin pass treatments in S3 and S5 is 5-10 times, more preferably 6-8 times.

[0016] In the above scheme, fluororubber has excellent heat resistance, carbon black N990 plays a role of reinforcement and filling, bisphenol AF and benzyltriphenylphosphine chloride (BPP) can adjust the degree of vulcanization, and molybdenum disulfide provides good wear resistance for the rubber material.

[0017] Molybdenum disulfide is an inorganic filler with a two-dimensional layered structure, which has good solid lubrication properties. When mixed with fluororubber, molybdenum disulfide still maintains mechanical anisotropy and sliding surface, making the surface of the product made of the mixed rubber have a self-lubricating effect, thereby improving wear resistance.

[0018] Compared with the prior art, the present invention has the following significant features and positive effects: the present invention applies modified molybdenum disulfide to the rubber field, thereby improving the wear resistance of rubber products.

[0019] Scope of application of this project: Used for rubber products with high requirements for wear resistance and heat resistance. DETAILED DESCRIPTION

[0020] Embodiment 1: Low friction oil seal materials are composed of the following materials by mass: Fluororubber 100 Carbon Black N990 25 Molybdenum disulfide 5 Palm wax 0.3 Magnesium oxide 5 Calcium hydroxide 3 Bisphenol AF 1.3 Benzyltriphenylphosphonium chloride (BPP) 0.3 This embodiment provides a method for preparing the rubber material, comprising the following steps: S1. First, put the fluororubber into the internal mixer and mix it at a speed of 30rpm for 60-90s. Then, add carbon black N990, palm wax, magnesium oxide and calcium hydroxide, and continue mixing at the same speed for 180-240s until there is no white powder on the surface. S2, adding molybdenum disulfide to the mixed materials in step S1, and then mixing at a speed of 30 rpm for 90-120 seconds until the color is uniform; S3, discharge the mixed materials in step S2 to the open mixing mill, thinly pass through 6 times, and then put the sheets down and park for 16 hours; S4, putting the mixture obtained in step S3 into the internal mixer again, adding bisphenol AF and benzyl triphenylphosphine chloride (BPP) thereto, and mixing for 180-240 seconds at a rotation speed of 25 rpm; S5. The mixed materials in step S4 are discharged to an open mixing mill and thinly passed through 7 times before being unrolled.

[0021] Embodiment 2: The preparation method and steps are consistent with those in Example 1, except that: Low friction oil seal materials are composed of the following materials by mass: Fluororubber 100 Carbon Black N990 25 Molybdenum disulfide 10 Palm wax 0.3 Magnesium oxide 5 Calcium hydroxide 3 Bisphenol AF 1.3 Benzyltriphenylphosphonium chloride (BPP) 0.3 Embodiment 3: The preparation method and steps are consistent with those in Example 1, except that: Low friction oil seal materials are composed of the following materials by mass: Fluororubber 100 Carbon Black N990 25 Molybdenum disulfide 10 Palm wax 0.3 Magnesium oxide 5 Calcium hydroxide 3 Bisphenol AF 1.4 Benzyltriphenyl 0.3 Embodiment 4: The preparation method and steps are consistent with those in Example 1, except that: Low friction oil seal materials are composed of the following materials by mass: Fluororubber 100 Carbon Black N990 25 Modified Molybdenum Disulfide 10 Palm wax 0.3 Magnesium oxide 5 Calcium hydroxide 3 Bisphenol AF 1.3 Benzyltriphenylphosphonium chloride (BPP) 0.4.

[0022] The preparation method of the modified molybdenum disulfide comprises the following steps: a) washing the molybdenum disulfide with hydrochloric acid having a concentration of 0.5M for 0.5h, and then drying it at 110°C for 20min; b) mixing molybdenum disulfide, 3-caprolactam and zinc persulfate at a mass ratio of 100:50:5, adding an initiator and reacting at 150°C; c) adding the reaction product obtained in step b), siloxane and water at a mass ratio of 100:30:80, subjecting the mixture to ultrasonic stirring for 10min, filtering and drying at 90°C for 30min to obtain modified molybdenum disulfide.

[0023] Embodiment 5: The preparation method and steps are consistent with those in Example 1, except that: Low friction oil seal materials are composed of the following materials by mass: Fluororubber 100 Carbon Black N990 25 Modified Molybdenum Disulfide 10 Palm wax 0.3 Magnesium oxide 5 Calcium hydroxide 3 Bisphenol AF 1.4 Benzyltriphenylphosphonium chloride (BPP) 0.4.

[0024] The preparation method of the modified molybdenum disulfide comprises the following steps: a) washing the molybdenum disulfide with 1M nitric acid for 0.3h, and then drying it at 100°C for 20min; b) mixing molybdenum disulfide, 3-caprolactam and zinc persulfate in a mass ratio of 100:60:5, adding an initiator and reacting at 150°C; c) adding the reaction product obtained in step b), siloxane and water in a mass ratio of 100:40:100, ultrasonically stirring for 10min, filtering and drying at 90°C for 20min to obtain modified molybdenum disulfide.

[0025] Comparative Example 1: The preparation method is the same as that of Example 1, except that the composition of the oil seal material is as follows: Fluororubber 100 Carbon Black N990 30 Palm wax 0.3 Magnesium oxide 5 Calcium hydroxide 3 Bisphenol AF 1.4 Benzyltriphenylphosphonium chloride (BPP) 0.4 Comparative Example 2: The preparation method is the same as that of Example 1, except that the composition of the oil seal material is as follows: Fluororubber 100 Carbon Black N990 25 Molybdenum disulfide 5 Palm wax 0.3 Magnesium oxide 5 Calcium hydroxide 3 Bisphenol AF 1.1 Benzyltriphenylphosphonium chloride (BPP) 0.2 Test items unit Example 1 Example 2 Example 3 Example 4 Example 5 Comparative Example 1 Comparative Example 2 hardness Shao A 70 72 72 73 73 71 69 Tensile Strength Mpa 13.16 14.05 14.37 14.12 14.75 13.41 11.73 Elongation at break % 265 256 245 238 233 276 297 Akron Wear cm3 0.58 0.49 0.46 0.41 0.37 0.72 0.68 The experimental data obtained according to the above 7 implementation schemes are listed in a table, as shown in the following table: According to the comparison of the above 7 implementation schemes, it can be seen that the overall performance of the product obtained in Example 5 is the best. By increasing the content of molybdenum disulfide, the number of sliding surfaces in the rubber will increase, the friction coefficient will decrease, and the wear resistance will be improved; by increasing the content of bisphenol AF and benzyl triphenylphosphine chloride (BPP), the number of crosslinking points will increase, the stability will be better, the elasticity of the rubber will increase, and the wear resistance will also be improved.

[0026] Obviously, the above embodiments of the present invention are merely examples for clearly explaining the present invention, and are not intended to limit the implementation methods of the present invention. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is impossible to list all implementation methods here. Any obvious changes or modifications derived from the technical solution of the present invention are still within the scope of protection of the present invention.

Claims

1. A low friction oil seal material, characterized in that: The composition includes the following components in parts by weight: fluororubber 90-110; carbon black N990 25-35; molybdenum disulfide 5.0-10.0; palm wax 0.1-1.5; magnesium oxide 5.0-10.0; calcium hydroxide 1.0-6.0; bisphenol AF 1.0-2.0; benzyl triphenyl phosphine chloride (BPP) 0.1-0.

8.

2. The oil seal material according to claim 1, characterized in that The composition includes the following components in parts by weight: fluororubber 95-105; carbon black N990 30-35; molybdenum disulfide 7.0-8.0; palm wax 0.5-1.0; magnesium oxide 7.0-8.0; calcium hydroxide 3.0-4.0; bisphenol AF 1.5-1.7; benzyltriphenylphosphonium chloride (BPP) 0.3-0.

6.

3. The oil seal material according to claim 1, characterized in that Molybdenum disulfide is subjected to a modification treatment, wherein the modification treatment comprises the following steps: a) Molybdenum disulfide is acid-washed and then heated and dried; b) Molybdenum disulfide and 3-caprolactam are mixed in proportion, an initiator is added and the mixture is reacted at 120-200° C.; c) the reaction product obtained in step b) is washed with water and dried, siloxane and water are added, and the mixture is filtered and dried after ultrasonic stirring to obtain modified molybdenum disulfide.

4. The oil seal material according to claim 3, characterized in that In the pickling in step a), one of sulfuric acid, hydrochloric acid and nitric acid with a molar concentration of less than 1M is used; in the modification reaction in step b), the initiator used is one of zinc persulfate and benzoyl peroxide; in step b), the mass ratio of molybdenum disulfide, 3-caprolactam and initiator is 100-120:50-70:1-5.

5. The oil seal material according to claim 1, characterized in that In step d), the mass ratio of the reaction product obtained in step c) to siloxane and water is 100-120:30-50:60-100; and the ultrasonic treatment time is 1-10 min.

6. A method for preparing the low friction oil seal material as claimed in claim 1, characterized in that: The following steps are involved: S1. First, put the fluororubber into the internal mixer and mix for 60-90 seconds, then put in carbon black N990, palm wax, magnesium oxide and calcium hydroxide, and continue mixing for 180-240 seconds until there is no white powder on the surface; S2, adding molybdenum disulfide to the mixed materials in step S1, and then mixing for 90-120S until the color is uniform; S3, discharge the mixed materials in step S2 to an open mixing mill, thinly slice them, and leave them for 16 hours; S4, putting the mixture obtained in step S3 into the internal mixer again, adding bisphenol AF and benzyl triphenylphosphonium chloride (BPP) thereto, and mixing for 180-240 seconds; S5, discharge the mixed materials in step S4 to an open mixing mill, and sheet them after thinning.

7. The method according to claim 6, characterized in that The mixing in steps S1, S2 and S4 is carried out at a rotation speed of 20-50 rpm.

8. The method according to claim 6, characterized in that The number of thin pass treatments in S3 and S5 is 5-10 times, more preferably 6-8 times.

Citation Information

Patent Citations

  • Engine-oil-seal fluoride rubber and preparation method thereof

    CN106317712A

  • Fluororubber material for oil seal and preparation method thereof

    CN112592550A