T-shaped through hole structure and manufacturing method thereof

By using a single-sided etching process on the silicon substrate to form a T-shaped through-hole structure, the problem of difficult to prepare high-deep aspect ratio and easy copper column fall off on thicker substrates in the prior art is solved, and process simplification is achieved and the stability of copper columns.

CN118943081APending Publication Date: 2024-11-12SHANGHAI IND U TECH RES INST
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411259989.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-10
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The existing through-silicon process is difficult to prepare a high-deep and aspect ratio through-pore structure on thicker substrates, and the copper columns are prone to fall off, resulting in complex and unstable processes.

Method used

Using a single-sided etching process, a T-shaped through-hole structure is formed on the substrate using a layer of mask, a trench is etched through the Bosch process, and a barrier layer is formed on the bottom and side walls of the trench. The portion is removed by ICP etching. The barrier layer forms a T-shaped through-hole structure with a depth-to-width ratio of (10-30): 1. The side wall barrier layer is retained to protect the side walls, and the isolation layer and seed layer are subsequently grown for electroplating.

Benefits of technology

The same technical effect of the double-sided etching process is achieved in the single-sided etching process, simplifying the process flow, improving the stability of the copper column, and avoiding the risk of shedding.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118943081A_ABST
    Figure CN118943081A_ABST
Patent Text Reader

Abstract

The invention discloses a T-shaped through hole structure and a manufacturing method thereof, and the method comprises the steps: 1, carrying out the etching of a first surface of a substrate to form a groove, and enabling the bottom of the groove to stop in the substrate; step 2, forming a barrier layer on the bottom and the side wall surface of the groove; step 3, etching to remove a part of the barrier layer at the bottom of the groove so as to expose a part of the bottom of the groove; and 4, performing secondary etching along the exposed part of the bottom of the groove until the second surface of the substrate, and removing the rest of the barrier layer to form a T-shaped through hole structure. Through the mode, the same technical effect of using two layers of masks in a double-sided etching process is achieved by using one layer of mask in a single-sided etching process, and the process flow is optimized.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor manufacturing, and in particular to a T-shaped through-hole structure and a manufacturing method thereof. Background Art

[0002] Currently, through silicon via technology is widely used in the advanced packaging of integrated circuits (ICs) and micro electro mechanical systems (MEMS). For example, MEMS and its driving circuit can be stacked and packaged together through through silicon via interconnection, which has the characteristics of high transmission bandwidth and low transmission delay.

[0003] Conventional through silicon via fabrication processes, such as Figure 1 As shown, deep holes are directly etched on the substrate, and then a seed layer is deposited in the deep hole and electroplating is performed to achieve metal filling. However, the silicon vias prepared on thicker substrates often require a very high aspect ratio, which makes the silicon via etching, subsequent seed layer growth and copper electroplating processes very difficult. In addition, the vertical copper pillars made by the conventional silicon via process are prone to fall off during subsequent use, causing device failure. Therefore, the prior art often uses double-sided etching to reduce the difficulty of etching and ensure the stability of the copper pillars, such as Figure 2 As shown in the figure, a large hole is etched on one side of the substrate and a small hole is etched on the other side to form a T-shaped silicon via structure, which reduces the risk of copper pillars falling off during use. However, double-sided etching requires an etching process on both sides of the substrate respectively, requiring two layers of masks. Compared with single-sided etching, it increases the etching steps and the process flow is complicated. Summary of the invention

[0004] In order to solve the above technical problems, the present invention provides a T-type through-hole structure and a manufacturing method thereof, which achieves the same technical effect of a double-sided etching process using two layers of masks by adopting a single-sided etching process and using one layer of mask, thereby optimizing the process flow.

[0005] A technical solution adopted by the present invention is to provide a method for manufacturing a T-shaped through-hole structure, comprising:

[0006] Step 1: Etching a groove on the first surface of the substrate, wherein the bottom of the groove stops in the substrate.

[0007] Step 2: forming a barrier layer on the bottom and sidewall surfaces of the trench.

[0008] Step three: etching and removing a portion of the barrier layer at the bottom of the trench to expose a portion of the bottom of the trench.

[0009] Step 4: Perform secondary etching along the exposed portion of the bottom of the trench until reaching the second surface of the substrate, remove the remaining barrier layer, and form a T-shaped through-hole structure.

[0010] The aspect ratio of the T-shaped through hole structure is (10-30):1, and the depth of the groove is 40%-60% of the thickness of the substrate. The groove is used to form the larger opening structure of the T-shaped through hole structure. The remaining thickness of the substrate is used to form the smaller opening structure of the T-shaped through hole structure.

[0011] In the step three, the portion of the barrier layer removed by etching is located in the middle of the bottom of the trench, and portions of the barrier layer shared with the sidewalls are left on both sides of the bottom of the trench.

[0012] In step 3, the portion of the barrier layer removed by etching is located in the middle of the bottom of the trench, and portions of the barrier layer shared with the sidewalls are left on both sides of the bottom of the trench. Retaining the barrier layer on the sidewalls of the trench can protect the sidewalls from being damaged during secondary etching.

[0013] In the step three, the ICP etching process is used to etch away part of the barrier layer at the bottom of the groove, and the etching gas used is mainly fluoride gas; the etching power is 400-1000W, and the pressure is 6-10mTorr. Specifically, the etching gas is mainly fluoride gas such as CF4 and C4F8. The etching effect is to remove the bottom barrier layer, and the lateral etching amount needs to be controlled to retain the side wall barrier layer.

[0014] The substrate is a silicon wafer, and the etching of the substrate in step 1 and step 4 adopts the Bosch process; the material of the barrier layer is silicon oxide or silicon nitride. Using the Bosch process, etching can be performed only along the longitudinal direction, which is conducive to forming a through-hole structure with a higher aspect ratio.

[0015] When the material of the barrier layer is silicon oxide, the barrier layer is grown by a thermal oxidation process or a chemical vapor deposition process; when the material of the barrier layer is silicon nitride, the barrier layer is grown by a chemical vapor deposition process.

[0016] The manufacturing method of a T-shaped through hole structure of the present invention further includes step five: growing an isolation layer and a seed layer in the T-shaped through hole structure and electroplating. Further, the isolation layer material is one of titanium, tantalum, titanium nitride or tantalum nitride, and is formed by sputtering.

[0017] In the step 4, the method for removing the remaining barrier layer is to use HF solution to remove it.

[0018] The present invention also provides a T-shaped through hole structure, and the special silicon through hole structure is prepared by using a manufacturing method of a T-shaped through hole structure described in any one of the above technical solutions. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0020] Figure 1 It is a schematic diagram of a vertical through silicon via structure formed by a conventional process;

[0021] Figure 2 It is a schematic diagram of the T-shaped through silicon via structure formed by the double-sided process;

[0022] Figure 3 It is a flow chart of a method for manufacturing a T-shaped through-hole structure of the present invention;

[0023] Figure 4 is a schematic diagram of the structure after processing in step 1 of Example 1 of the present invention;

[0024] Figure 5 is a schematic diagram of the structure after processing in step 2 in Example 1 of the present invention;

[0025] Figure 6 It is a schematic diagram of the structure after processing in step 3 and step 4 in Example 1 of the present invention;

[0026] Figure 7 It is a schematic diagram of the structure after processing in step five in Example 1 of the present invention.

[0027] 1. Substrate; 2. Copper pillar; 3. Groove; 4. Barrier layer; 5. T-type through-hole structure. DETAILED DESCRIPTION

[0028] In order to make the purpose, technical scheme and advantages of the present invention clearer, the specific embodiments of the present invention are described in detail below in conjunction with the accompanying drawings. Examples of these preferred embodiments are illustrated in the accompanying drawings. The embodiments of the present invention shown in the accompanying drawings and described according to the accompanying drawings are merely exemplary, and the present invention is not limited to these embodiments.

[0029] It should also be noted that, in order to avoid obscuring the present invention due to unnecessary details, only structures and / or processing steps closely related to the solutions according to the present invention are shown in the accompanying drawings, while other details that are not closely related to the present invention are omitted.

[0030] Example 1

[0031] See also Figures 3 to 7 , an embodiment of the present invention includes: a method for manufacturing a T-shaped through-hole structure, comprising:

[0032] Step 1: A groove 3 is formed by etching on the first surface of the substrate 1 , and the bottom of the groove 3 stops inside the substrate 1 .

[0033] In this embodiment, the substrate 1 is a silicon wafer. A groove 3 having a thickness of 40% to 60% of the substrate thickness is etched on the substrate 1 by Bosch process. Figure 4 , the groove 3 is used to form the larger opening structure of the T-shaped through hole structure 5. The remaining thickness of the substrate 1 is used to form the smaller opening structure of the T-shaped through hole structure 5. The aspect ratio of the T-shaped through hole structure is (10-30): 1, and the aspect ratio is the ratio of the thickness of the substrate to the width of the groove 3. In this embodiment, the depth of the groove 3 is 40%-60% of the thickness of the substrate 1.

[0034] The Bocsh process achieves etching and sidewall passivation by alternately switching etching gas and passivation gas, with one cycle of etching and passivation switching every 5 to 10 seconds. After a short period of isotropic etching, the silicon surface that has just been etched is passivated. Due to the physical sputtering bombardment of ions in the depth direction, the passivation film can be retained, so that lateral etching will not occur in the next cycle of etching. Using the Bocsh process, etching can be performed only in the vertical direction, which is conducive to the formation of a silicon-through-hole structure with a higher aspect ratio.

[0035] Step 2: forming a barrier layer 4 on the bottom and sidewall surface of the trench 3, see Figure 5 .

[0036] The barrier layer 4 is used to protect the side wall of the groove 3 from being damaged during the secondary etching process. At the same time, the thickness of the barrier layer 4 determines the size of the smaller opening of the T-shaped through-hole structure 5, and its thickness is determined according to the device requirements. In this embodiment, the thickness of the barrier layer 4 is 2um to 5um. In this embodiment, the barrier layer 4 is silicon oxide, which is grown by a thermal oxidation process. In another embodiment, the silicon oxide barrier layer 4 can also be grown by a chemical vapor deposition process. In other embodiments, the barrier layer 4 can also be silicon nitride, which is grown by a chemical vapor deposition process.

[0037] Step three: etching and removing a portion of the barrier layer 4 at the bottom of the trench 3 to expose a portion of the bottom of the trench 3 .

[0038] In the step three, the part of the barrier layer 4 removed by the ICP etching process is located in the middle of the bottom of the groove 3, and part of the barrier layer 4 shared with the side wall is left on both sides of the bottom of the groove 3. Retaining the barrier layer 4 on the side wall of the groove 3 can protect the side wall from being damaged during the secondary etching. Specifically, the etching gas used is mainly fluoride gas; the etching power is 400~1000W, and the pressure is 6-10mTorr. Specifically, the etching gas is mainly fluoride gas such as CF4 and C4F8.

[0039] Step 4: Perform secondary etching along the exposed portion of the bottom of the trench 3 until the second surface of the substrate 1, remove the remaining barrier layer 4, and form a T-shaped through-hole structure 5, see Figure 6 .

[0040] Through the Bosch process, the exposed portion of the bottom of the trench 3 is etched again until the second surface of the substrate 1, forming a T-shaped through-hole structure 5. At this time, a T-shaped silicon through-hole structure 5 with a large opening on one side and a small opening on the other side is initially formed. The barrier layer 4 on the surface of the substrate 1 and the sidewall of the trench 3 is removed using an HF solution to prepare for the subsequent metal filling process.

[0041] Step 5: growing an isolation layer and a seed layer in the T-shaped through hole structure 5 and performing electroplating, see Figure 7 .

[0042] Specifically, an isolation layer and a seed layer (not shown in the figure) are sputtered in the T-shaped through hole structure 5. In this embodiment, the isolation layer material is titanium, and the seed layer material is copper. Then, the T-shaped through hole structure 5 is electroplated with copper metal to obtain a "T"-shaped copper column with a large opening on one side and a small opening on the other side. Compared with the vertical copper column in the prior art, the "T"-shaped copper column is not easy to fall off during use. In other embodiments, the isolation layer can also be any one of tantalum, titanium nitride or tantalum nitride.

[0043] The manufacturing method of a T-shaped through hole structure of the present invention adopts a single-sided etching process using one layer of mask to achieve the same technical effect as a double-sided etching process using two layers of masks, thereby optimizing the process flow.

[0044] The present invention also provides a T-shaped through hole structure, and the special silicon through hole structure is prepared by using a manufacturing method of a T-shaped through hole structure described in any one of the above technical solutions.

[0045] In addition, it should be noted that in this specification, "includes", "comprising" or any other variant thereof is intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also includes other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, an element defined by the sentence "comprising a ..." does not exclude the existence of other identical elements in the process, method, article or device including the element.

[0046] It should be understood that although this specification is described according to implementation methods, not every implementation method contains only one independent technical solution. This narrative method of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment can also be appropriately combined to form other implementation methods that can be understood by those skilled in the art.

Claims

1. A method for manufacturing a T-shaped through-hole structure, characterized in that: include: Step 1: etching a groove on the first surface of the substrate, wherein the bottom of the groove stops in the substrate; Step 2: forming a barrier layer on the bottom and sidewall surface of the trench; Step 3: etching and removing a portion of the barrier layer at the bottom of the trench to expose a portion of the bottom of the trench; Step 4: Perform secondary etching along the exposed portion of the bottom of the trench until reaching the second surface of the substrate, remove the remaining barrier layer, and form a T-shaped through-hole structure.

2. The method for manufacturing a T-shaped through hole structure according to claim 1, characterized in that: The aspect ratio of the T-shaped through hole structure is (10-30):1, and the depth of the groove is 40%-60% of the thickness of the substrate.

3. The method for manufacturing a T-shaped through hole structure according to claim 1, characterized in that: In the step three, the portion of the barrier layer removed by etching is located in the middle of the bottom of the trench, and portions of the barrier layer shared with the sidewalls are left on both sides of the bottom of the trench.

4. The method for manufacturing a T-shaped through hole structure according to claim 1, characterized in that: The substrate is a silicon wafer, and the etching of the substrate in step 1 and step 4 adopts a Bosch process; the material of the barrier layer is silicon oxide or silicon nitride.

5. The method for manufacturing a T-shaped through hole structure according to claim 4, characterized in that: When the material of the barrier layer is silicon oxide, the barrier layer is grown by a thermal oxidation process or a chemical vapor deposition process; when the material of the barrier layer is silicon nitride, the barrier layer is grown by a chemical vapor deposition process.

6. The method for manufacturing a T-shaped through hole structure according to claim 1, characterized in that: In the step three, the ICP etching process is used to etch away part of the barrier layer at the bottom of the groove, and the etching gas used is mainly fluoride gas; the etching power is 400-1000W, and the pressure is 6-10mTorr.

7. The method for manufacturing a T-shaped through hole structure according to claim 1, characterized in that: The method also includes step five: growing an isolation layer and a seed layer in the T-shaped through-hole structure and performing electroplating.

8. The method for manufacturing a T-shaped through hole structure according to claim 7, characterized in that: The isolation layer material is one of titanium, tantalum, titanium nitride or tantalum nitride, and is formed by sputtering.

9. The method for manufacturing a T-shaped through hole structure according to claim 1, characterized in that: In the step 4, the method for removing the remaining barrier layer is to use HF solution to remove it.

10. A T-shaped through hole structure, characterized in that: The T-shaped through hole structure is prepared by the manufacturing method of any one of claims 1 to 9.