Oil rail type forge piece embracing cutting die and design method thereof

By designing a blade with partial hollowing and overall scaling during the cutting process of stainless steel oil rail forgings, combined with virtual parts and 3D modeling, the problem of woven and flashing during the cutting process is solved, and the cutting accuracy is improved. Mold closure accuracy simplifies the design process and improves production efficiency.

CN118950910APending Publication Date: 2024-11-15JIANGSU LONGCHENG PREC FORGING CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411305557.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-19
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The prior art is prone to problems such as woven yarn, excessive residual flew or crushing during the cutting process of stainless steel oil rail forgings, resulting in incomplete cleaning and mold wear, and lack of specific methods for designing edge cutting die and edge cutting punch. .

Method used

An oil rail forging die is designed, including a cutting edge die and a cutting edge die. The edge design is used for partial hollowing and overall scaling, and the difference is calculated in combination with virtual part design and 3D modeling to ensure the closing of the mold. Accuracy and stability of press blocks optimize the mold structure through interference analysis.

Benefits of technology

It effectively solves problems such as overcutting, edge-cutting and large residual flashing, improves edge-cutting accuracy and quality, reduces mold wear, simplifies the design process, and improves production efficiency and operation convenience.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118950910A_ABST
    Figure CN118950910A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of embracing cutting dies, and discloses an oil rail type forge piece embracing cutting die and a design method thereof.The oil rail type forge piece embracing cutting die comprises an edge cutting female die and an edge cutting male die, and one side of the edge cutting female die is connected with a material pressing block; a forge piece body located on the lower sides of the trimming female die and the pressing block is placed on the top of the trimming male die. A cutting edge is arranged on one side of the trimming female die, a local hollowed-out scheme is adopted through the design of the cutting edge, overall scaling and local fine adjustment are combined, the problems of over-cutting, trimming galling, large residual flash and the like are effectively solved, the trimming precision and quality are improved, the design of the trimming male die and the pressing block fully considers the structural characteristics of a forge piece body, and the design of the forge piece is reasonable. According to the method, the difference design is carried out through the virtual part, crushing damage to the forge piece body in the trimming process is avoided, the trimming female die and the trimming male die are the same in height, the outer contour size is accurately controlled, the closing precision of the die is ensured, and abrasion and deformation of the die in the using process are reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of cutting dies, and in particular to an oil rail forging cutting die and a design method thereof. Background Art

[0002] As an important engine component, stainless steel oil rails not only require high dimensional accuracy, but also have high requirements for their appearance. When trimming the oil rail forgings, there must be no overcutting, rough trimming, excessive residual flash, or crushing. Stainless steel oil rail forgings have a large deformation resistance and require a large trimming force. In addition, stainless steel is very sticky, and the material is easy to stick to the cutting edge of the trimming die during trimming, resulting in roughening of the forgings during trimming. When the oil rail trimming is rough or the residual flash is too large, the pickling liquid will enter the gap between the residual flash and the forging during pickling, resulting in a failure to clean the cleaning process, causing the flash to rust.

[0003] In the Chinese patent with the authorization announcement number CN209647338U, a trimming die frame for an integral forged stainless steel oil rail is disclosed, and an integral forged stainless steel oil rail trimming die frame is provided, which mainly includes an upper die frame body and a lower die frame body, and solves the problems of crushing and trimming burrs caused by the misalignment of forgings during the trimming process; in the Chinese patent with the authorization announcement number CN212551342U, a trimming correction composite die for manufacturing integral stainless steel oil rail forgings is disclosed, and a trimming correction composite die for stainless steel oil rail forgings is provided, including an upper die assembly and a lower die assembly. The lower die assembly adds a lower die seat core, a floating plate and a lower elastic element, which can effectively ensure the dimensional accuracy of the stainless steel oil rail, such as straightness and position; the Chinese patent with the authorization announcement number CN216656022U discloses a high-pressure oil rail trimming and shaping composite die, and provides a high-pressure oil rail trimming and shaping composite die, including a trimming upper die, a base, a punching die, a trimming lower die, a discharge spring, a discharge plate and a nitrogen spring and other components. The trimming and shaping are carried out simultaneously, which solves the problem of springback after straightening.

[0004] The above patent has the following defects: the above die frame or mold solves the accuracy of forging placement during trimming and the accuracy of relative movement of the mold during trimming, so as to avoid trimming burrs and crushing. No specific method is given for how to design the trimming die cutting edge, trimming punch and pressure block. If the trimming die cutting edge and the trimming punch are not designed properly, no matter how accurate the die frame is, or only by adjusting the positions of the various components of the trimming die frame, it is impossible to solve the problems of trimming burrs, large residual flash or crushing. For this reason, a cutting die for oil rail forgings and a design method thereof are proposed. Summary of the invention

[0005] The object of the present invention is to provide a cutting die for oil rail forgings and a design method thereof to solve the problems raised in the above-mentioned background technology.

[0006] To achieve the above object, the present invention provides the following technical solutions: a cutting die for oil rail forgings, comprising a trimming die and a trimming punch, wherein a pressure block is connected to one side of the trimming die;

[0007] A forging body located at the bottom of the trimming die and the pressure block is placed on the top of the trimming punch;

[0008] A cutting edge is arranged on one side of the trimming die.

[0009] Preferably, the trimming die has the same height as the trimming punch, and the outer contour of the trimming punch is 1-1.5 mm smaller than the edge of the trimming die on one side.

[0010] Preferably, the clearance between the pressing block and the cutting edge is 0.25-0.3 mm, and the height of the pressing block is 8-12 mm higher than that of the trimming die.

[0011] The present invention also provides a design method for a cutting die for a fuel rail forging, comprising the following steps:

[0012] S1. Design of trimming die;

[0013] S2, virtual parts design;

[0014] S3, trimming punch design;

[0015] S4, press block design;

[0016] S5, interference analysis;

[0017] S6. Design is completed.

[0018] Preferably, in S1, the trimming die design includes overall scaling, local fine-tuning and cutting edge design to control the size of the residual flash;

[0019] When designing the cutting edge, the thermal expansion coefficient is selected to be 1.018-1.020.

[0020] Preferably, the cutting edge design is through-through from top to bottom, and the back side is not hollowed out. For the parts prone to roughening, a partial hollowing design is performed.

[0021] Preferably, in S2, the virtual component design follows the principle of pressing down necessary parts and avoiding easily deformed parts.

[0022] Preferably, in S3, the trimming punch design is obtained by using 3D modeling and virtual part subtraction.

[0023] Preferably, in S4, the design of the pressing block is also obtained by using 3D modeling and virtual part subtraction to control the gap between the pressing block and the trimming die and to round the mouth.

[0024] Preferably, in S5, the interference analysis uses 3D modeling software to analyze whether there is interference between the trimming punch, the pressure block and the forging body, and optimizes the interference location.

[0025] Compared with the prior art, the present invention adopts the above technical solution and has the following technical effects:

[0026] 1. The cutting edge design adopts a local hollowing scheme, combined with overall scaling and local fine-tuning, which effectively solves the problems of over-cutting, edge roughening, and large residual flash, and improves the accuracy and quality of edge cutting. The design of the edge cutting punch and the pressure block fully considers the structural characteristics of the forging body, and the difference design is carried out through virtual parts to avoid crushing of the forging body during the edge cutting process.

[0027] Second, by making the height of the trimming die and the trimming punch the same and the outer contour dimensions precisely controlled, the closing accuracy of the mold is ensured and the wear and deformation of the mold during use is reduced. The gap between the pressure block and the trimming die is reasonably designed, which not only ensures the stability of the pressure block during the trimming process, but also avoids the problem of the pressure block getting stuck in the trimming die.

[0028] 3. The cutting mold designed by using this method has good consistency, and the ideal mold can be obtained without repeated testing, which shortens the mold development cycle and improves production efficiency. The mold has a reasonable structure and is easy to operate, which reduces the operating difficulty and labor intensity. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0030] Figure 1 It is a schematic diagram of the structure of the cutting die of the present invention;

[0031] Figure 2 is a flow chart of the design method of the present invention;

[0032] Figure 3 It is a schematic diagram of the structure of the cutting edge of the present invention;

[0033] Figure 4 It is a structural schematic diagram of a first cutting edge hollowing avoidance solution of the present invention;

[0034] Figure 5 For the present invention Figure 4 A schematic diagram of the structure of the middle cutting edge;

[0035] Figure 6 It is a structural schematic diagram of the second cutting edge hollowing avoidance solution of the present invention;

[0036] Figure 7 For the present invention Figure 6 A schematic diagram of the structure of the middle cutting edge;

[0037] Figure 8 It is a schematic diagram of the avoidance position structure of the first virtual part and the forging body of the present invention;

[0038] Fig. 9 It is a schematic diagram of the avoidance position structure of the second virtual part and the forging body of the present invention;

[0039] Fig.10 It is a schematic diagram of the main structure of the oil rail forging of the present invention;

[0040] Fig.11 It is a schematic diagram of the top view of the main body of the oil rail forging of the present invention.

[0041] Explanation of the reference numerals: 1. trimming die; 2. trimming punch; 3. pressing block; 4. forging body; 5. cutting edge. DETAILED DESCRIPTION

[0042] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0043] It should be noted that the structures, proportions, sizes, etc. illustrated in the drawings of this specification are only used to match the contents disclosed in the specification for people familiar with this technology to understand and read, and are not used to limit the conditions under which this application can be implemented. Therefore, they have no substantive technical significance. Any structural modification, change in proportional relationship or adjustment of size should still fall within the scope of the technical content disclosed in this application without affecting the effects and purposes that can be achieved by this application.

[0044] Example

[0045] See also Figure 1-11The present invention provides a technical solution: a cutting die for oil rail forgings, comprising a trimming die 1 and a trimming punch 2, wherein a pressure block 3 is connected to one side of the trimming die 1; a forging body 4 located below the trimming die 1 and the pressure block 3 is placed on the top of the trimming punch 2; and a cutting edge 5 is provided on one side of the trimming die 1.

[0046] The trimming die 1 has the same height as the trimming punch 2. The outer contour of the trimming punch 2 is 1.2 mm smaller than the cutting edge 5 of the trimming die 1. The gap between the pressure block 3 and the cutting edge 5 is 0.27 mm. The height of the pressure block 3 is 10 mm higher than that of the trimming die 1.

[0047] The present invention also provides a design method for a cutting die for a fuel rail forging, comprising the following steps:

[0048] S1, design of trimming die 1;

[0049] The design of the trimming die 1 includes overall scaling, local fine-tuning and cutting edge 5 design to control the size of the residual flash;

[0050] The residual flash of the main body 4 of the oil rail forging made of stainless steel is generally 0.4-0.6mm. If the residual flash is too small, it is easy to cause burrs or overcutting during trimming; if the residual flash is too large, a gap will be formed between the flash and the forging. The main body 4 of the oil rail forging is hot-cut, and the design of the trimming edge 5 adopts the method of overall scaling plus local fine-tuning, that is, the thermal expansion coefficient is generally selected as 1.018-1.020, and local fine-tuning is performed on the parts that are prone to burrs and the parts with larger flash. For stainless steel oil rail forgings, due to their large shrinkage coefficient, the residual flash is most likely to be too large on the left and right end faces of the oil rail forging;

[0051] Therefore, the cutting edges 5 at both ends should be appropriately reduced to make the residual flash 0.25-0.35mm. For the oil rail forging body 4 with flash on the branches, the inner side of the leftmost and rightmost branches are prone to burrs, and the cutting edge 5 should be enlarged by 0.1-0.2mm, and the outer cutting edge 5 can be appropriately reduced by 0.1-0.2mm. For the oil rail with a large head, the cutting edge 5 at the transition between the large head and the main oil pipe should also be enlarged by 0.1-0.2mm.

[0052] When designing the trimming die 1, the thermal expansion coefficient is selected to be 1.018-1.020, the cutting edge 5 is designed to be through-through from top to bottom, and the back is not hollowed out. For the parts prone to burring, a partial hollowing design is performed.

[0053] There are two hollowing avoidance schemes: Scheme 1: The height H1 of the cutting edge 5 is 1 to 2 mm, the transition slope angle α is 5°, and the distance D1 between the avoidance straight edge and the cutting edge 5 is 1 to 1.5 mm. Figure 4 shown.

[0054] Solution 2: The height H2 of the cutting edge 5 is 1-2mm, and the distance D2 between the avoidance straight edge and the cutting edge 5 is 1-1.5mm. In order to increase the strength of the cutting edge 5, the cutting edge 5 and the avoidance straight edge are transitioned with a large arc chamfer Ra. The radius is generally selected from R4 to R6mm. Figure 5 As shown;

[0055] When designing the trimming punch 2 and the pressure block 3, if the forging body 4 is used directly for difference calculation, a large number of crushing injuries will occur after trimming. Since the shape of the oil rail forging body 4 is relatively complex, the crushing position is often difficult to adjust. Therefore, a virtual part is added to the design. When designing the trimming punch 2 and the pressure block 3, the virtual part is used for difference calculation. No adjustment is required after the difference calculation, and no crushing injuries will occur during trimming.

[0056] S2, virtual parts design;

[0057] The design of virtual parts follows the principle of pressing necessary parts and avoiding parts that are easy to deform. In order to prevent the oil rail forging body 4 from being deformed and crushed during trimming, the design principle of the trimming punch 2 and the pressing block 3 is to press the parts that should be pressed, such as the main oil pipe, each branch and both ends, and avoid the parts that should be avoided, such as the transition between the reducer and reducer and the main oil pipe and each fillet. Therefore, the above principles should also be followed when designing virtual parts;

[0058] When designing virtual parts, the transition between the reducer and the main oil pipe needs to be avoided, such as Figure 6 As shown, the length of the big end of the virtual part L1 should be 1 to 2 mm longer than the length of the big end of the forging L2, and the length of the small end of the virtual part L3 should be 1 to 1.5 mm shorter than the length of the small end of the forging L4;

[0059] When designing the virtual part, small bosses such as the coding platform on the main oil pipe need to be avoided. The small boss shape of the virtual part should be 1 to 1.5 mm larger than the small boss shape of the forging body 4 on one side. The highest surface of the small boss of the virtual part can be 0 to 0.15 mm higher than the highest surface of the small boss of the forging body 4.

[0060] When designing virtual parts, in addition to pressing down the branches, appropriate avoidance should be done. The avoidance plan is as follows: Figure 7 As shown, the virtual part profile is similar to an ellipse, consisting of two parallel line segments and two semicircles. The semicircle diameter of the virtual part is equal to the cylinder diameter of the forging body 4. For the branches farther from the center, the length b of the parallel line segments is 0.8-1.5 mm, and for the branches closer to the center, the length b of the parallel line segments is 0.5-0.7 mm.

[0061] When designing virtual parts, all fillets need to be avoided, that is, the fillets of virtual parts should be 1 to 5 mm larger than the fillets of corresponding parts of the forging body 4. When designing virtual parts, except for the above parts that need to be avoided, the sizes of other parts should be consistent with the sizes of the forgings.

[0062] S3, design of trimming punch 2;

[0063] The design of trimming punch 2 is obtained by using 3D modeling and virtual part subtraction;

[0064] The height of the trimming punch 2 is equal to that of the trimming die 1, and the outer contour is 1 to 1.5 mm smaller than the contour of the cutting edge 5 of the trimming die 1. If the gap is too small, the flash after cutting will easily get stuck on the trimming punch 2, making it inconvenient to take out; if the gap is too large, the trimming punch 2 cannot support the oil rail forging body 4 well, and deformation will occur during trimming. After the shape of the trimming punch 2 is determined, the 3D modeling forging body 4 and the virtual part are used for subtraction to obtain the trimming punch 1. After subtraction, the mouth of the trimming punch 2 is a sharp angle. To avoid crushing the forging body 4, the chamfer size of its mouth is R1 to R2 mm.

[0065] S4, design of press block 3;

[0066] The design of the pressing block 3 is also obtained by using 3D modeling and virtual part difference calculation to control the gap between it and the trimming die 1 and the rounded corners of the mouth;

[0067] To prevent the pressing block 3 from shaking in the trimming die 1, the gap between the pressing block 3 and the cutting edge 5 of the trimming die 1 in the four directions of front, back, left, and right is 0.25-0.3mm per side. If the gap is too small, the pressing block 3 is easy to get stuck in the trimming die 1 during trimming; if the gap is too large, the position of the pressing block 3 in the trimming die 1 is unstable, which will damage the forging body 4. The four directions of the pressing block 3 are controlled, and the gaps in the remaining parts should be increased to 0.8-1mm. If the gap is too small, the pressing block 3 is also easy to get stuck in the trimming die 1 during trimming; if the gap is too large, the pressing block 3 cannot press the oil rail forging body 4 well, and deformation will occur during trimming. After the shape of the pressing block 3 is determined, the 3D modeling forging body 4 is used to perform a difference with the virtual part to obtain the pressing block 3. After the difference is calculated, the chamfer size of the mouth of the pressure block 3 is R1-R2mm, and the height of the pressure block 3 should be 8-12mm higher than the trimming die 1, that is, during trimming, the pressure block 3 first presses the forging body 4, and then the trimming die 1 performs trimming.

[0068] S5, interference analysis;

[0069] Interference analysis uses 3D modeling software to analyze whether there is interference between the trimming punch 2, the pressure block 3 and the hot forging body 4, and optimize the interference position;

[0070] The purpose of interference analysis is to determine from a theoretical perspective whether the forging body 4 is crushed during trimming. Use 3D modeling software to analyze whether there is interference between the trimming punch 2, the pressure block 3 and the hot forging body 4. If there is interference, it means that crushing will occur during trimming, and the interference part should be optimized. If there is no interference, theoretically no crushing will occur during trimming, but it should also be checked whether the above-mentioned avoidance parts are avoided.

[0071] S6. Design is completed.

[0072] Examples of implementation methods:

[0073] A fuel rail forging body 4, such as Figure 8 As shown, it includes a main oil pipe, four branches, a big head, a small head and a coding platform M. The coding platform M is a square with a size of 10×10mm. These structural characteristics put forward specific requirements for the design of the cutting die. The design method of the cutting die includes the design of the trimming die 1, the design of the virtual part, the design of the trimming die 2, the design of the pressing block 3, and the interference analysis.

[0074] Design of trimming die 1. First, the trimming edge 5 is designed, the residual flash is designed to be 0.5 mm, the thermal expansion coefficient is selected to be 1.019, and local fine-tuning is performed on the parts prone to burring and the parts with larger flash;

[0075] As attached Figure 8 As shown, the cutting edge 5 at the two end faces A and B is reduced to a residual flash of 0.3 mm, the cutting edge 5 at the inner side of the branches Z1 and Z4, namely at E and F, is enlarged by 0.15 mm, and the cutting edge 5 at the transition between the big head and the main oil pipe C1 and C2 is enlarged by 0.15 mm;

[0076] The cutting edge 5 of the trimming die 1 is partially hollowed out, and the inner sides of the branches Z1 and Z4, that is, the cutting edges at E and F are hollowed out. Figure 5 In the second scheme shown, the height H2 of the cutting edge 5 is designed to be 1 mm, the distance D2 between the avoidance straight edge and the cutting edge 5 is designed to be 1 mm, and the transition radius between the cutting edge 5 and the avoidance straight edge is R4 mm;

[0077] In the design of virtual parts, the transition between the big and small heads and the main oil pipe needs to be avoided. The length of the big head L1 of the virtual part is 2mm longer than the length of the big head L2 of the forging, and the length of the small head L3 of the virtual part is 1mm shorter than the length of the small head L4 of the forging. The virtual part coding platform is designed to be 11×11mm;

[0078] The design of virtual branches Z1~Z4 adopts the following Figure 7 In the scheme shown, the virtual part has an ellipse-like outline, consisting of two parallel line segments and two semicircles. The semicircle diameter of the virtual part is equal to the cylindrical diameter of the forged part, and the length b of the parallel line segments of the branches Z1 and Z4 is 1 mm; the length b of the parallel line segments of the branches Z2 and Z3 is 0.6 mm.

[0079] All fillets of virtual parts need to be avoided, that is, the fillets of virtual parts are 1 to 5 mm larger than the fillets of corresponding parts of forgings.

[0080] Except for the parts that need to be avoided, the sizes of other parts are consistent with the size of the forging body 4. After the above steps, a virtual part can be obtained;

[0081] The trimming punch 2 is designed. The outer contour of the trimming punch 2 is 1.2mm smaller than the contour of the trimming edge 5 on one side. Its height is equal to that of the trimming die 1. Then, the trimming punch 2 can be obtained by subtracting the 3D modeled forging body 4 from the virtual part. After subtracting, the chamfer of the mouth of the trimming punch 2 is R1mm;

[0082] The design of the pressure block 3 is that the clearance between the pressure block 3 and the cutting edge 5 of the trimming die 1 in the four directions of front, back, left, and right is 0.3mm on one side, and the clearance in other parts is 1mm. After the shape of the pressure block 3 is determined, the pressure block 3 can be obtained by subtracting the forging body 4 and the virtual part using 3D modeling. After subtracting, the chamfer R1mm is set at the mouth of the pressure block 3, and the height of the pressure block 3 is 10mm higher than that of the trimming die 1, that is, when trimming, the pressure block 3 first presses the forging body 4, and then the trimming die 1 performs trimming;

[0083] Interference analysis uses 3D modeling software to analyze whether there is interference between the trimming punch 2, the pressure block 3 and the hot forging body 4, and at the same time, focus on checking whether the above-mentioned avoidance areas are avoided.

[0084] After the above steps, a set of cutting dies for the oil rail forging main body 4 can be obtained, including a trimming die 1, a trimming punch 2 and a pressing block 3.

[0085] In summary, the cutting edge 5 is designed with a local hollowing solution, combined with overall scaling and local fine-tuning, which effectively solves the problems of overcutting, edge roughening, and large residual flash, and improves the accuracy and quality of edge cutting. The design of the edge cutting punch 2 and the pressure block 3 fully considers the structural characteristics of the forging body 4, and the difference design is performed through virtual parts to avoid crushing of the forging body 4 during the edge cutting process.

[0086] The trimming die 1 and the trimming punch 2 have the same height, and the outer contour dimensions are precisely controlled, which ensures the closing accuracy of the mold and reduces the wear and deformation of the mold during use. The gap between the pressure block 3 and the trimming die 1 is reasonably designed, which not only ensures the stability of the pressure block 3 during the trimming process, but also avoids the problem of the pressure block 3 getting stuck in the trimming die 1.

[0087] The cutting mold designed using this method has good consistency, and the ideal mold can be obtained without repeated testing, which shortens the mold development cycle and improves production efficiency. In addition, the mold has a reasonable structure and is easy to operate, which reduces the operating difficulty and labor intensity.

[0088] It will be appreciated by those skilled in the art that the features described in the various embodiments and / or claims of the present invention may be combined and / or combined in various ways, even if such combinations and / or combinations are not explicitly described in the present invention. In particular, the features described in the various embodiments and / or claims of the present invention may be combined and / or combined in various ways without departing from the spirit and teachings of the present invention. All of these combinations and / or combinations fall within the scope of the present invention.

Claims

1. A cutting die for oil rail forgings, comprising a cutting die (1) and a cutting punch (2), characterized in that: A material pressing block (3) is connected to one side of the trimming die (1); A forging body (4) located below the trimming die (1) and the pressure block (3) is placed on the top of the trimming punch (2); A cutting edge (5) is provided on one side of the trimming die (1).

2. The oil rail forging cutting die according to claim 1, characterized in that: The trimming die (1) and the trimming punch (2) have the same height, and the outer contour of the trimming punch (2) is 1-1.5 mm smaller than the edge (5) of the trimming die (1) on one side.

3. The oil rail forging cutting die according to claim 2, characterized in that: The gap between the pressing block (3) and the cutting edge (5) is 0.25-0.3 mm, and the height of the pressing block (3) is 8-12 mm higher than that of the trimming die (1).

4. A method for designing a cutting die for a fuel rail forging according to any one of claims 1 to 3, characterized in that: The following steps are involved: S1. Design of trimming die (1); S2, virtual parts design; S3, design of trimming punch (2); S4, design of the press block (3); S5, interference analysis; S6. Design is completed.

5. The design method of a cutting die for a fuel rail forging according to claim 2 is characterized in that: In S1, the trimming die (1) design includes overall scaling, local fine-tuning and cutting edge (5) design to control the size of the residual flash; When designing the cutting edge (5), the thermal expansion coefficient is selected to be 1.018-1.

020.

6. The design method of a cutting die for a fuel rail forging according to claim 2 is characterized in that: The cutting edge (5) is designed to be through-through from top to bottom, and the back side is not hollowed out. Partial hollowing is performed on the part that is prone to roughening.

7. The design method of a cutting die for a fuel rail forging according to claim 2 is characterized in that: In S2, the virtual component design follows the principle of pressing down necessary parts and avoiding parts that are prone to deformation.

8. The design method of a cutting die for a fuel rail forging according to claim 2 is characterized in that: In S3, the trimming punch (2) is designed using 3D modeling and virtual part subtraction.

9. The design method of a cutting die for a fuel rail forging according to claim 2 is characterized in that: In S4, the design of the pressing block (3) is also obtained by using 3D modeling and virtual part subtraction to control the gap between it and the trimming die and the rounded corners of the mouth.

10. The design method of a cutting die for a fuel rail forging according to claim 2, characterized in that: In S5, the interference analysis uses 3D modeling software to analyze whether there is interference between the trimming punch (2), the pressure block (3) and the forging body (4), and optimizes the interference position.

Citation Information

Patent Citations

  • Integral stainless steel oil rail forging and a manufacturing process thereof

    CN111590004A

  • Forging and trimming die remanufacturing method

    CN111940662A

  • Trimming and shaping composite die for high-pressure oil rail

    CN114082838A

  • Crankshaft forge piece trimming die and design method

    CN116060506A

  • High-precision trimming die for full-streamline near-net forming of front axle forgings

    CN116197335A