Preparation method of cosmetic pigment powder and application of cosmetic pigment powder
By forming an inorganic intermediate layer and an amino acid surfactant double coating on the surface of cosmetic pigment powder, the problems of pigment powder dispersion and photoactivity in silicone-free systems are solved, improving the slip and skin-adhesive properties and avoiding the defects of traditional silicone oil.
Patent Information
- Application Number
- CN202411065124.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-05
- Publication Date
- 2024-11-19
AI Technical Summary
Existing silicone-free cosmetic pigment powders suffer from problems such as poor dispersion, low color rendering, and easy darkening. Furthermore, traditional silicone oils may cause skin problems and environmental pollution.
The double-layer coating technology first forms an inorganic intermediate layer on the surface of the raw material powder, and then forms an amino acid surfactant coating layer on the outer layer. By adjusting the pH value and stirring, a stable coating layer is formed, which improves dispersibility and skin affinity.
It significantly improves the dispersibility, smoothness, and skin adhesion of cosmetic pigment powders in silicone-free systems, while reducing photoactivity and avoiding the skin and environmental problems associated with traditional silicone oils.
Smart Images

Figure CN118975945A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of cosmetic base makeup, and more specifically, to a method for preparing cosmetic pigment powder and an application of the cosmetic pigment powder. Background Art
[0002] As a common cosmetic ingredient, silicone oil can improve the skin feel of cosmetics and increase their spreadability. However, silicone oil is suspected of clogging skin pores, leading to skin problems such as acne and blackheads. Silicone oil is also not easily biodegradable in the environment, which means that some silicone oil will remain in the environment, which is not environmentally friendly.
[0003] In the current cosmetics market, more and more brands use environmental protection and sustainability as differentiated selling points, and silicone-free cosmetics are increasingly popular. However, most of the current cosmetic pigment powders in silicone-free systems have problems such as difficulty in dispersion, low color rendering, and easy dullness. These problems limit the further improvement of the performance of silicone-free cosmetics. Therefore, it is urgent to develop a preparation method for environmentally friendly cosmetic pigment powders that are easy to disperse in silicone-free systems.
[0004] In the prior art, CN115449235B provides a modified titanium dioxide and a preparation method thereof. By coating titanium dioxide with bismuth oxychloride and silicone resin, the partial photoactivity of titanium dioxide can be reduced, and at the same time, the fluidity between particles can be enhanced, so that the particles have a smooth and glossy feel and have an anti-dullness effect.
[0005] In view of the above-mentioned related technologies, the inventors found that although the coating of bismuth oxychloride and silicone resin can reduce the photoactivity of titanium dioxide and enhance the fluidity of particles to a certain extent, this method has some shortcomings. First, bismuth oxychloride, as a semiconductor material, has its own photoactivity problem, and coating it on titanium dioxide may affect the stability and safety of the product; secondly, silicone resin is incompatible with the formula of the silicone-free system, which may cause the product to have a poor skin feel, such as dryness, and is not suitable for the silicone-free system. Summary of the invention
[0006] In order to reduce the photosensitivity of cosmetic pigment powder while improving the dispersibility, slippery feel and skin adhesion of the cosmetic pigment powder, the present application provides a method for preparing cosmetic pigment powder and an application of cosmetic pigment powder.
[0007] In a first aspect, the present application provides a method for preparing cosmetic pigment powder, using the following technical solution: A method for preparing cosmetic pigment powder comprises the following steps: S1: dispersing the raw material powder in water and performing surface treatment to obtain an active pigment powder solution; S2: adding the intermediate layer raw material into water to prepare an intermediate layer salt solution, adding the active pigment powder solution of step S1, mixing and stirring to obtain a mixture A; S3: adjusting the pH of the mixture A to 4-6 using dilute hydrochloric acid, stirring and mixing, and uniformly depositing to obtain a mixture B, and forming an inorganic intermediate layer on the surface of the raw material powder; S4: adding an amino acid surfactant into water to prepare an amino acid surfactant solution, adding the mixture B, stirring and mixing to obtain a mixture C, and forming a secondary coating layer outside the inorganic intermediate layer; S5: Filter and wash the mixture C with deionized water for 3-5 times to obtain a double-layer coated cosmetic powder filter cake; S6: drying the double-layer coated cosmetic powder filter cake obtained in step S5 at 105-120° C. for 2-4 hours, crushing it and sieving it.
[0008] By adopting the above technical solution, the surface treatment can improve the surface roughness and reactivity of the raw material powder, which is conducive to the uniform adhesion of the subsequent double-layer coating.
[0009] The pH is adjusted with dilute hydrochloric acid, so that the intermediate layer raw materials can form a stable inorganic intermediate layer on the surface of the raw material powder. This inorganic intermediate layer can physically block part of the light, reduce the raw material powder's response to light, and thus effectively reduce its photoactivity. The inorganic intermediate layer further increases the surface roughness of the raw material powder, provides more active sites, significantly improves the dispersibility of the raw material powder in the cosmetic formula, and improves the spreadability and skin-fitting performance of the cosmetics.
[0010] A secondary coating layer formed by an amino acid surfactant is formed outside the inorganic intermediate layer. This coating layer can improve the dispersibility and skin-affinity of the raw material powder. In addition, the amino acid surfactant contains carboxyl groups, which can chemically bond with the hydroxyl groups on the raw material powder or the inorganic intermediate layer. This chemical bonding helps to stabilize the coating layer and can change the electronic structure and energy level distribution on the surface of the raw material powder, thereby affecting its light absorption and emission characteristics, and further reducing the photosensitivity of the raw material powder.
[0011] Amino acid surfactants are not only green, natural, skin-friendly, mild, and biodegradable, but also have good compatibility with silicon-free systems and excellent dispersibility in carbon chain oils, especially polar carbon chain oils. In addition, due to the presence of the intermediate layer, the photoactivity of the raw material powder is reduced, and the rich and uniform hydroxyl groups on the surface of the raw material powder also make secondary coating easier.
[0012] The setting of the double coating layer significantly reduces the photostability of the raw material powder, and can improve the dispersibility, slipperiness and skin-friendliness of the raw material powder in the silicon-free system.
[0013] Optionally, the specific steps of the surface treatment in step S1 are: dispersing the raw material powder in water, adjusting the pH to acid or alkaline soaking for 50-70 minutes, adjusting the pH to 2-3 during acid soaking, and adjusting the pH to 11-12 during alkaline soaking.
[0014] By adopting the above technical scheme, the surface roughness of the raw material powder can be significantly increased through surface treatment with acid or alkali bubbles, the surface active sites can be increased, and at the same time, it helps to adjust the surface charge of the raw material powder, so that the raw material powder is away from the isoelectric point and can be dispersed more evenly in the wet system, thereby improving its reaction activity and stability in subsequent steps.
[0015] Optionally, the specific steps of the surface treatment in step S1 are: dispersing the raw material powder in water, adding any one of polyethylene glycol or polyvinyl pyrrolidone in an amount of 1-5% of the added amount of the raw material powder, and stirring for 50-70 minutes.
[0016] By adopting the above technical solution, polyethylene glycol or polyvinyl pyrrolidone is added to graft polymers on the surface of the raw material powder to increase steric hindrance, which can increase the hydroxyl group and dispersibility on the surface of the raw material powder, and help the coating uniformity of the subsequent double-layer coating. Then, inorganic oxides or inorganic hydroxides are directionally deposited on the surface of the raw material powder through metal coordination or hydrogen bonding, so that the surface of the raw material powder is uniformly grafted with amino acid surfactants.
[0017] Optionally, the raw material for the intermediate layer is any one of tetraethyl orthosilicate, sodium metasilicate and sodium metaaluminate, and the mass of the raw material for the intermediate layer is 1-10% of the mass of the raw material powder.
[0018] By adopting the above technical scheme, ethyl orthosilicate, sodium metasilicate and sodium metaaluminate are used as intermediate layer raw materials to form a uniform inorganic layer on the surface of the raw material powder, which not only improves the stability and dispersibility of the raw material powder, but also improves its compatibility with cosmetic formulas.
[0019] Optionally, the amino acid surfactant is any one or more combinations of sodium lauroyl glutamate, sodium cocoyl glutamate, sodium myristoyl glutamate, sodium palmitoyl glycinate, and sodium stearoyl glutamate, and the mass of the amino acid surfactant is 1-10% of the mass of the raw material powder.
[0020] By adopting the above technical solutions, these surfactants not only provide excellent slip and softness, but also enhance the market competitiveness and consumer acceptance of the products due to their biodegradability and environmental friendliness.
[0021] Optionally, the raw material powder is one or more combinations of powders selected from titanium dioxide, zinc oxide, iron oxide yellow, iron oxide red, iron oxide black, iron oxide brown, chromium oxide green, hydrated chromium oxide green, ultramarine, manganese violet, lake, mica, sericite, mercerized sericite, synthetic fluorphlogopite, bismuth oxychloride, boron nitride, talc, calcium carbonate, barium sulfate, hydroxyapatite, silica, hydrated silica, kaolin, etc.
[0022] Optionally, the dilute hydrochloric acid in step S3 is concentrated hydrochloric acid and water in a volume ratio of 1:2.
[0023] Optionally, in step S4, an amino acid surfactant is added to water to prepare an amino acid surfactant solution, and the water temperature is 40-70°C.
[0024] In a second aspect, the present application provides a method for preparing a cosmetic pigment powder, and the prepared cosmetic pigment powder is used for preparing silicone-free system cosmetics.
[0025] Optionally, the silicone-free system cosmetics are selected from any one of liquid foundation, foundation cream, natural cream, concealer, sunscreen, face cream, and isolation cream.
[0026] Optionally, the liquid foundation comprises 12-13% by mass of the cosmetic pigment powder.
[0027] In summary, this application has the following beneficial effects: 1. Since the present application double-coats the cosmetic pigment powder by providing an inorganic intermediate layer and an amino acid surfactant, the photoactivity of the cosmetic pigment powder is reduced while improving the dispersibility, slipperiness and skin adhesion of the cosmetic pigment powder in a silicon-free system.
[0028] 2. The preparation method of the present application can be applied to the preparation of a variety of other different silicone-free system cosmetics, so that the prepared silicone-free system cosmetics have the characteristic of significant anti-dullness effect.
[0029] 3. The method of the present application can significantly improve the application performance of cosmetic pigment powder in silicone-free cosmetics, while avoiding the skin problems and environmental impacts that may be caused by traditional silicone oil. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 From left to right ad are photos of titanium dioxide (R5) double-coated with aluminum hydroxide and myristoyl glutamate, red iron oxide (R6), yellow iron oxide (R7), and black iron oxide (R8) dispersed in caprylic / capric triglyceride after standing for 5 hours.
[0031] Figure 2In the figure, ad represents titanium dioxide (R5), red iron oxide (R6), yellow iron oxide (R7), and black iron oxide (R8) coated with aluminum hydroxide and myristoyl glutamate, respectively.
[0032] Figure 3 This is a scatter diagram of Application Example 1 under a 10× microscope.
[0033] Figure 4 This is the color difference curve of the test formula of Application Example 1. DETAILED DESCRIPTION
[0034] The following examples further illustrate the present application in detail.
[0035] raw material Unless otherwise specified, the raw materials used in the preparation examples, embodiments and comparative examples in this application are all commercially available cosmetic raw material products, specifically: Titanium dioxide, yellow iron oxide, red iron oxide, and black iron oxide are all cosmetic grade powders; Polyvinylpyrrolidone, selected from Qingdao Tuohai Iodine Products Co., Ltd., 9003-39-8; Sodium metasilicate and sodium metaaluminate are both premium grade, with a content of 99%; Sodium lauroyl glutamate, selected from Shanghai Yuanye Biotechnology Co., Ltd., S29791; Sodium stearoyl glutamate, selected from Shanghai Yuanye Biotechnology Co., Ltd., S29792; Sodium myristoyl glutamate, selected from Shanghai Yuanye Biotechnology Co., Ltd., Y47111; Sodium cocoyl glutamate, selected from Sichuan Weikeqi Biotechnology Co., Ltd., WKQ-0012811; Sanshanyujing, selected from Shanghai Yuanye Biotechnology Co., Ltd., S62850; VP / hexadecene copolymer, selected from Ashland, USA, V-216; Disteardimethylammonium hectorite, selected from ZHPU, HOPE 138V; Coconut oil alcohol-caprylate / caprate, selected from Guangzhou Bolu Chemical Co., Ltd., 12452; Sorbitan isostearate, selected from Croda, Span 120; Caprylic / capric triglyceride selected from CRODAMOL, GTCC. Example
[0036] Example 1 A method for preparing cosmetic pigment powder comprises the following steps: S1: Disperse 100 g of titanium dioxide in 500 mL of water, adjust the pH to 2, and stir for 60 min for surface treatment to obtain an active pigment powder solution; S2: 5 g of sodium metasilicate was added to 10 mL of water and stirred to dissolve to prepare an intermediate layer salt solution, and the active pigment powder solution of step S1 was added, and the mixture was stirred for 30 min to obtain a mixture A; S3: Using dilute hydrochloric acid (concentrated hydrochloric acid and water in a volume ratio of 1:2) to adjust the pH of the mixture A to 4, stirring and mixing, and uniformly depositing to obtain a mixture B, forming an inorganic intermediate layer coated with silicon dioxide on the surface of the titanium dioxide; S4: 10 g of sodium lauroyl glutamate was added to 20 mL of water, dissolved in a 60°C water bath to prepare an amino acid surfactant solution, added to mixture B, and stirred for 30 min to obtain mixture C, forming a secondary coating layer outside the inorganic intermediate layer; S5: The mixture C is filtered and washed with deionized water for 4 times to obtain a double-layer coated titanium dioxide filter cake; S6: drying the double-layer coated titanium dioxide filter cake obtained in step S5 in an oven at 120° C. for 2 h, sieving after air flow crushing, and obtaining titanium dioxide double-coated with silicon dioxide and lauroyl glutamate, which is marked as R1.
[0037] Example 2 A method for preparing cosmetic pigment powder comprises the following steps: S1: Disperse 100g of yellow iron oxide in 500mL of water, adjust the pH to 3, and stir for 50min for surface treatment to obtain an active pigment powder solution; S2: Add 1 g of sodium metasilicate into 10 mL of water and stir to dissolve to prepare an intermediate layer salt solution, add the active pigment powder solution of step S1, mix and stir for 30 minutes to obtain a mixture A; S3: Using dilute hydrochloric acid (concentrated hydrochloric acid and water in a volume ratio of 1:2) to adjust the pH of the mixture A to 4, stirring and mixing, and uniformly depositing to obtain a mixture B, forming a silicon dioxide-coated inorganic intermediate layer on the surface of the yellow iron oxide; S4: 3 g of sodium stearoyl glutamate was added to 20 mL of water, dissolved in a 40°C water bath to prepare an amino acid surfactant solution, added to mixture B, and stirred for 30 min to obtain mixture C, forming a secondary coating layer outside the inorganic intermediate layer; S5: The mixture C is filtered and washed with deionized water for 5 times to obtain a double-layer coated iron oxide yellow filter cake; S6: The double-layer coated yellow iron oxide filter cake obtained in step S5 is dried in an oven at 110° C. for 4 h, sieved after air flow crushing, and the yellow iron oxide double-coated with silicon dioxide and stearoyl glutamic acid is obtained, which is marked as R2.
[0038] Example 3 A method for preparing cosmetic pigment powder comprises the following steps: S1: Disperse 100 g of red iron oxide in 500 mL of water, adjust the pH to 11, and stir for 60 min for surface treatment to obtain an active pigment powder solution; S2: 3 g of sodium metasilicate was added to 10 mL of water and stirred to dissolve to prepare an intermediate layer salt solution, and the active pigment powder solution of step S1 was added, and the mixture was stirred for 30 minutes to obtain a mixture A; S3: Using dilute hydrochloric acid (concentrated hydrochloric acid and water in a volume ratio of 1:2) to adjust the pH of the mixture A to 5, stirring and mixing, and uniformly depositing to obtain a mixture B, forming a silicon dioxide-coated inorganic intermediate layer on the surface of the red iron oxide; S4: 5 g of sodium myristoyl glutamate was added to 20 mL of water, dissolved in a 60°C water bath to prepare an amino acid surfactant solution, added to mixture B, and stirred for 30 min to obtain mixture C, forming a secondary coating layer outside the inorganic intermediate layer; S5: The mixture C is filtered and washed with deionized water for three times to obtain a double-layer coated iron oxide red filter cake; S6: The double-layer coated red iron oxide filter cake obtained in step S5 is dried in an oven at 105° C. for 3 h, sieved after air flow crushing, and the red iron oxide double-coated with silicon dioxide and myristoyl glutamate is obtained, which is marked as R3.
[0039] Example 4 A method for preparing cosmetic pigment powder comprises the following steps: S1: Disperse 100 g of black iron oxide in 500 mL of water, adjust the pH to 12, and stir for 70 min for surface treatment to obtain an active pigment powder solution; S2: adding 10 g of sodium metasilicate to 10 mL of water and stirring to dissolve to prepare an intermediate layer salt solution, adding the active pigment powder solution of step S1, mixing and stirring for 30 minutes to obtain a mixture A; S3: Using dilute hydrochloric acid (concentrated hydrochloric acid and water in a volume ratio of 1:2) to adjust the pH of the mixture A to 6, stirring and mixing, and uniformly depositing to obtain a mixture B, forming an inorganic intermediate layer coated with silicon dioxide on the surface of the black iron oxide; S4: 1 g of sodium cocoyl glutamate was added to 20 mL of water, dissolved in a 70°C water bath to prepare an amino acid surfactant solution, added to mixture B, and stirred for 30 min to obtain mixture C, forming a secondary coating layer outside the inorganic intermediate layer; S5: The mixture C is filtered and washed with deionized water for three times to obtain a double-layer coated iron oxide black filter cake; S6: The double-layer coated black iron oxide filter cake obtained in step S5 is dried in an oven at 105° C. for 3 h, sieved after air flow crushing, and iron oxide black double-coated with silicon dioxide and cocoyl glutamate is obtained, and marked as R4.
[0040] Example 5 A method for preparing cosmetic pigment powder comprises the following steps: S1: 100 g of titanium dioxide was dispersed in 500 mL of water, and 2 g of polyethylene glycol was added, and stirred for 60 min for surface treatment to obtain an active pigment powder solution; S2: 5 g of sodium aluminate was added to 10 mL of water and stirred to dissolve to prepare an intermediate layer salt solution, and the active pigment powder solution of step S1 was added, and the mixture was stirred for 30 minutes to obtain a mixture A; S3: Using dilute hydrochloric acid (concentrated hydrochloric acid and water in a volume ratio of 1:2) to adjust the pH of the mixture A to 4, stirring and mixing, and uniformly depositing to obtain a mixture B, forming an inorganic intermediate layer coated with aluminum hydroxide on the surface of the titanium dioxide; S4: 10 g of sodium myristoyl glutamate was added to 20 mL of water, dissolved in a 60°C water bath to prepare an amino acid surfactant solution, added to mixture B, and stirred for 30 min to obtain mixture C, forming a secondary coating layer outside the inorganic intermediate layer; S5: The mixture C is filtered and washed with deionized water for 4 times to obtain a double-layer coated titanium dioxide filter cake; S6: The double-layer coated titanium dioxide filter cake obtained in step S5 is dried in an oven at 120° C. for 2 h, sieved after air flow crushing, and titanium dioxide double-coated with aluminum hydroxide and myristoyl glutamate is obtained, which is marked as R5.
[0041] Example 6 A method for preparing cosmetic pigment powder comprises the following steps: S1: Disperse 100g of yellow iron oxide in 500mL of water, add 1g of polyethylene glycol, and stir for 50min for surface treatment to obtain an active pigment powder solution; S2: Add 1 g of sodium aluminate to 10 mL of water and stir to dissolve to prepare an intermediate layer salt solution, add the active pigment powder solution of step S1, mix and stir for 30 minutes to obtain a mixture A; S3: Using dilute hydrochloric acid (concentrated hydrochloric acid and water in a volume ratio of 1:2) to adjust the pH of the mixture A to 4, stirring and mixing, and uniformly depositing to obtain a mixture B, forming an inorganic intermediate layer coated with aluminum hydroxide on the surface of the yellow iron oxide; S4: 3 g of sodium myristoyl glutamate was added to 20 mL of water, dissolved in a 40°C water bath to prepare an amino acid surfactant solution, added to mixture B, and stirred for 30 min to obtain mixture C, forming a secondary coating layer outside the inorganic intermediate layer; S5: The mixture C is filtered and washed with deionized water for 5 times to obtain a double-layer coated iron oxide yellow filter cake; S6: The double-layer coated yellow iron oxide filter cake obtained in step S5 is dried in an oven at 110° C. for 4 h, sieved after air flow crushing, and the yellow iron oxide double-coated with aluminum hydroxide and myristoyl glutamate is obtained, which is marked as R6.
[0042] Example 7 A method for preparing cosmetic pigment powder comprises the following steps: S1: Disperse 100 g of red iron oxide in 500 mL of water, add 2 g of polyethylene glycol, and stir for 60 min for surface treatment to obtain an active pigment powder solution; S2: 3 g of sodium aluminate was added to 10 mL of water and stirred to dissolve to prepare an intermediate layer salt solution, and the active pigment powder solution of step S1 was added, and the mixture was stirred for 30 minutes to obtain a mixture A; S3: Using dilute hydrochloric acid (concentrated hydrochloric acid and water in a volume ratio of 1:2), adjusting the pH of the mixture A to 5, stirring and mixing, and uniformly depositing to obtain a mixture B, forming an inorganic intermediate layer coated with aluminum hydroxide on the surface of the red iron oxide; S4: 5 g of sodium myristoyl glutamate was added to 20 mL of water, dissolved in a 60°C water bath to prepare an amino acid surfactant solution, added to mixture B, and stirred for 30 min to obtain mixture C, forming a secondary coating layer outside the inorganic intermediate layer; S5: The mixture C is filtered and washed with deionized water for three times to obtain a double-layer coated iron oxide red filter cake; S6: The double-layer coated red iron oxide filter cake obtained in step S5 is dried in an oven at 105° C. for 3 h, sieved after air flow crushing, and red iron oxide double-coated with aluminum hydroxide and myristoyl glutamate is obtained, which is marked as R7.
[0043] Example 8 A method for preparing cosmetic pigment powder comprises the following steps: S1: Disperse 100 g of black iron oxide in 500 mL of water, add 5 g of polyvinyl pyrrolidone, and stir for 70 min for surface treatment to obtain an active pigment powder solution; S2: 10 g of sodium aluminate was added to 10 mL of water and stirred to dissolve to prepare an intermediate layer salt solution, and the active pigment powder solution of step S1 was added, and the mixture was stirred for 30 minutes to obtain a mixture A; S3: Using dilute hydrochloric acid (concentrated hydrochloric acid and water in a volume ratio of 1:2) to adjust the pH of the mixture A to 6, stirring and mixing, and uniformly depositing to obtain a mixture B, forming an inorganic intermediate layer coated with aluminum hydroxide on the surface of the black iron oxide; S4: 1 g of sodium myristoyl glutamate was added to 20 mL of water, dissolved in a 70°C water bath to prepare an amino acid surfactant solution, added to mixture B, and stirred for 30 min to obtain mixture C, forming a secondary coating layer outside the inorganic intermediate layer; S5: The mixture C is filtered and washed with deionized water for three times to obtain a double-layer coated iron oxide black filter cake; S6: The double-layer coated black iron oxide filter cake obtained in step S5 is dried in an oven at 105° C. for 3 h, sieved after air flow crushing, and the black iron oxide double-coated with aluminum hydroxide and myristoyl glutamate is obtained, which is marked as R8.
[0044] Comparative Example Comparative Example 1 A method for preparing a cosmetic pigment powder, which differs from Example 1 in that the raw material powder is not coated with an inorganic intermediate layer, specifically comprising the following steps: S1: Disperse 100 g of titanium dioxide in 500 mL of water, adjust the pH to 2, and stir for 60 min for surface treatment to obtain an active pigment powder solution; S2: 10 g of sodium lauroyl glutamate was added to 20 mL of water, dissolved in a 60° C. water bath to prepare an amino acid surfactant solution, and the active pigment powder solution obtained in step S1 was added, stirred for 30 min to obtain a blend, and a lauroyl glutamate coating layer was formed on the surface of titanium dioxide; S3: The blend was filtered and washed with deionized water for 4 times to obtain a lauroyl glutamate-coated titanium dioxide filter cake; S4: drying the lauroyl glutamate-coated titanium dioxide filter cake obtained in step S5 in an oven at 120° C. for 2 h, sieving after air flow crushing, and obtaining lauroyl glutamate-coated titanium dioxide, which is marked as D1.
[0045] Comparative Example 2 A method for preparing a cosmetic pigment powder, which differs from Example 3 in that the raw material powder is not secondary coated with an amino acid surfactant, and specifically comprises the following steps: S1: Disperse 100 g of red iron oxide in 500 mL of water, adjust the pH to 11, and stir for 60 min for surface treatment to obtain an active pigment powder solution; S2: 3 g of sodium metasilicate was added to 10 mL of water and stirred to dissolve to prepare an intermediate layer salt solution, and the active pigment powder solution of step S1 was added, and the mixture was stirred for 30 minutes to obtain a mixture A; S3: Using dilute hydrochloric acid (concentrated hydrochloric acid and water in a volume ratio of 1:2) to adjust the pH of the mixture A to 5, stirring and mixing, and uniformly depositing to obtain a mixture B, forming a silicon dioxide-coated inorganic intermediate layer on the surface of the red iron oxide; S4: The mixture B is filtered and washed with deionized water for 4 times to obtain a filter cake of iron oxide red coated with silica; S5: The silica-coated titanium dioxide filter cake obtained in step S5 is dried in an oven at 120° C. for 2 h, pulverized by air flow, and then sieved to obtain silica-coated iron oxide red, which is marked as D2.
[0046] Comparative Example 3 A method for preparing a cosmetic pigment powder, which differs from Example 1 in that the raw material powder is not surface treated, and step S1 is specifically: dispersing 100 g of titanium dioxide in 500 mL of water, stirring evenly to obtain an active pigment powder solution, and the other steps are the same as Example 1, and the finally obtained cosmetic pigment powder is marked as D3.
[0047] Comparative Example 4 A method for preparing a cosmetic pigment powder, which differs from Example 7 in that the raw material powder is not surface treated, and step S1 is specifically: dispersing 100 g of red iron oxide in 500 mL of water, stirring evenly to obtain an active pigment powder solution, and the other steps are the same as Example 1, and the finally obtained cosmetic pigment powder is marked as D4.
[0048] Application Examples The present application discloses a method for preparing a cosmetic pigment powder, which can be used to prepare a silicone-free system formula, such as liquid foundation, foundation cream, bare face cream, concealer, sunscreen, face cream, and isolation cream. Here, the method is described as being used to prepare a silicone-free system liquid foundation formula.
[0049] Application Example 1 A silicone-free liquid foundation, wherein the raw materials and the mass percentages of the raw materials are shown in Table 1, wherein the cosmetic pigment powder A and the cosmetic pigment powder B are R5 and R7 obtained in Example 5 and Example 7, respectively.
[0050] The method for preparing the above-mentioned silicone-free liquid foundation comprises the following steps: S1: Mix phase A and heat to 80°C with stirring; S2: Mix phase B and homogenize at 5000 rpm for 15 min; S3: Slowly add phase A to phase B under stirring and continue homogenizing for 15 minutes; S4: Stir and cool to 35°C.
[0051] Application Example 2 A silicone-free liquid foundation, which differs from Application Example 1 in that the cosmetic pigment powder A and the cosmetic pigment powder B in the raw materials are R5 and R8 obtained in Example 5 and Example 8 respectively, the mass percentage of the cosmetic pigment powder A is 2.5%, and the mass percentage of the cosmetic pigment powder B is 10.5%, and the other steps are the same as those in Application Example 1.
[0052] Application Example 3 A silicone-free liquid foundation, which differs from Application Example 1 in that the cosmetic pigment powder A and the cosmetic pigment powder B in the raw materials are R5 and R6 obtained in Example 5 and Example 6 respectively, the mass percentage of the cosmetic pigment powder A is 1%, and the mass percentage of the cosmetic pigment powder B is 11%, and the other steps are the same as in Application Example 1.
[0053] Application Example 4 A silicone-free liquid foundation, which differs from Application Example 1 in that the cosmetic pigment powder A and the cosmetic pigment powder B in the raw materials are R1 and R2 obtained in Example 1 and Example 2, respectively, and the other steps are the same as those in Application Example 1.
[0054] Application Example 5 A silicone-free liquid foundation, which differs from Application Example 1 in that the cosmetic pigment powder A and the cosmetic pigment powder B in the raw materials are R1 and R3 obtained in Example 1 and Example 3 respectively, and the other steps are the same as those in Application Example 1.
[0055] Application Example 6 A silicone-free liquid foundation, which differs from Application Example 1 in that the cosmetic pigment powder A and the cosmetic pigment powder B in the raw materials are R1 and R4 obtained in Example 1 and Example 4 respectively, and the other steps are the same as those in Application Example 1.
[0056] Application Example 7 A silicone-free liquid foundation, which differs from Application Example 1 in that the cosmetic pigment powder A and the cosmetic pigment powder B in the raw materials are D1 and D2 obtained in Comparative Examples 1 and 2, respectively, and the other steps are the same as those in Application Example 1.
[0057] Application Example 8 A silicone-free liquid foundation, which differs from Application Example 1 in that the cosmetic pigment powder A and the cosmetic pigment powder B in the raw materials are D3 and D4 obtained in Comparative Examples 3 and 4 respectively, and the other steps are the same as those in Application Example 1.
[0058] Performance testing Test Example 1 Skin Feel Test The skin feel test of the silicone-free liquid foundation of Examples 1-8 was conducted by a consumer blind test. Ten consumers were randomly selected for blind testing, and the four indicators of slipperiness, skin adhesion, anti-dullness and softness were scored respectively. The minimum score interval was 0.5 points, and the full score was 10 points. The higher the score, the better the performance. The arithmetic mean of the scores of the ten consumers was taken as the final data and recorded in Table 2 to analyze the various properties of the silicone-free liquid foundation prepared by the method for preparing the cosmetic pigment powder suitable for the silicone-free system of the present application.
[0059] Table 2 According to the results of the above test data, it can be seen that when the method for preparing a cosmetic pigment powder of the present application is used to prepare a silicone-free cosmetic formula, the slippery feeling, skin-fitting performance, anti-dulling and softness of the silicone-free system formula are better than the commercially available anti-dulling liquid foundation products. Therefore, the cosmetic pigment powder obtained by the method for preparing a cosmetic pigment powder of the present application has improved slippery feeling and skin-fitting performance, and can effectively improve the slippery feeling, skin-fitting performance, anti-dulling and softness of cosmetics when used to prepare silicone-free system cosmetics.
[0060] Compared with Application Examples 1-6, the cosmetic pigment powder used in Application Example 7 is only coated with an inorganic intermediate layer or an amino acid surfactant during the preparation process. From the results of skin feel testing, it can be seen that the slippery feel, skin adhesion, anti-dullness and softness of the single-layer coated cosmetic pigment powder are significantly poorer.
[0061] Compared with Application Examples 1-6, the cosmetic pigment powder used in Application Example 8 was not surface treated during the preparation process. From the results of skin feel testing, it can be seen that the cosmetic pigment powder without surface treatment has significantly poorer slip, skin adhesion, anti-dullness and softness when used to prepare silicone-free cosmetics. This shows that surface treatment can improve the surface roughness and reactivity of the raw powder, which helps to uniformly adhere to the subsequent double-layer coating layer, thereby improving the various performances of the cosmetics.
[0062] Test Example 2 Dispersion Test Weigh 0.05 g of titanium dioxide, yellow iron oxide, red iron oxide and black iron oxide (R5-R8) double-coated with aluminum hydroxide and myristoyl glutamate prepared in Examples 5-8 as test samples, add 10 g of caprylic / capric triglyceride respectively, shake up and down manually 50 times, and take real-life pictures after standing overnight (such as Figure 1 shown) and microscope images (as Figure 2 shown).
[0063] according to Figure 1 and Figure 2 It can be seen from the test results that the cosmetic pigment powder of the present application has good dispersibility in silicone-free system cosmetics.
[0064] Test Example 3 Anti-dullness application formula test The formula test for anti-dullness application was carried out on the silicone-free foundation liquid prepared in Example 1. The specific method is as follows: Take 0.25g of the silicone-free foundation liquid prepared in Application Example 1 and apply it on a 5×5cm 2 The color difference value was then tested with a colorimeter on the PMMA plate. The color difference value was then tested every 0.5-1h for a total of 8h. The color difference value data obtained is shown in the figure. Figure 4 As shown, a microscope picture of the sample formula is taken to observe the dispersion of the sample formula, such as Figure 3 shown.
[0065] The color difference value is automatically calculated by the colorimeter software using the DEcmc color difference system. It is generally believed that when DEcmc>0.8, the color difference is observable to the naked eye.
[0066] according to Figure 3 From the microscope dispersion diagram of the liquid foundation of Application Example 1, it can be seen that the cosmetic pigment powder prepared by the method for preparing cosmetic pigment powder suitable for a silicone-free system of the present application has good dispersibility when used in preparing silicone-free system cosmetics.
[0067] according to Figure 4 The test results of the anti-dulling application formula of the liquid foundation in Application Example 1 show that DEcmc>0.8 was detected 6 hours after the color difference test corresponding to the formula in Application Example 1, indicating that the preparation method of the cosmetic pigment powder suitable for a silicone-free system of the present application has a good anti-dulling effect when applied to the preparation of silicone-free system cosmetics.
[0068] This specific embodiment is merely an explanation of the present application and is not a limitation of the present application. After reading this specification, those skilled in the art may make modifications to the present embodiment without any creative contribution as needed, but such modifications are protected by the patent law as long as they are within the scope of the claims of the present application.
Claims
1. A method for preparing cosmetic pigment powder, characterized in that: The following steps are involved: S1: dispersing the raw material powder in water and performing surface treatment to obtain an active pigment powder solution; S2: adding the intermediate layer raw material into water to prepare an intermediate layer salt solution, adding the active pigment powder solution of step S1, mixing and stirring to obtain a mixture A; S3: adjusting the pH of the mixture A to 4-6 using dilute hydrochloric acid, stirring and mixing, and uniformly depositing to obtain a mixture B, and forming an inorganic intermediate layer on the surface of the raw material powder; S4: adding an amino acid surfactant into water to prepare an amino acid surfactant solution, adding the mixture B, stirring and mixing to obtain a mixture C, and forming a secondary coating layer outside the inorganic intermediate layer; S5: Filter and wash the mixture C with deionized water for 3-5 times to obtain a double-layer coated cosmetic powder filter cake; S6: drying the double-layer coated cosmetic powder filter cake obtained in step S5 at 105-120° C. for 2-4 hours, crushing it and sieving it.
2. The method for preparing the cosmetic pigment powder according to claim 1, characterized in that: The specific steps of the surface treatment in step S1 are: dispersing the raw material powder in water, adjusting the pH and performing acid or alkaline soaking for 50-70 minutes, wherein the pH is adjusted to 2-3 during acid soaking and the pH is adjusted to 11-12 during alkaline soaking.
3. The method for preparing cosmetic pigment powder according to claim 1, characterized in that: The specific steps of the surface treatment in step S1 are: dispersing the raw material powder in water, adding 1-5% of the mass of polyethylene glycol or polyvinyl pyrrolidone added to the raw material powder, and stirring for 50-70 minutes.
4. The method for preparing the cosmetic pigment powder according to claim 1, characterized in that: The intermediate layer raw material is any one of tetraethyl orthosilicate, sodium metasilicate and sodium metaaluminate, and the mass of the intermediate layer raw material is 1-10% of the mass of the raw material powder.
5. The method for preparing the cosmetic pigment powder according to claim 1, characterized in that: The amino acid surfactant is any one or more combinations of sodium lauroyl glutamate, sodium cocoyl glutamate, sodium myristoyl glutamate, sodium palmitoyl glycinate, and sodium stearoyl glutamate, and the mass of the amino acid surfactant is 1-10% of the mass of the raw material powder.
6. The method for preparing the cosmetic pigment powder according to claim 1, characterized in that: The raw material powder is one or more combinations of powders selected from titanium dioxide, zinc oxide, iron oxide yellow, iron oxide red, iron oxide black, iron oxide brown, chromium oxide green, hydrated chromium oxide green, ultramarine, manganese violet, lake, mica, sericite, mercerized sericite, synthetic fluorphlogopite, bismuth oxychloride, boron nitride, talc, calcium carbonate, barium sulfate, hydroxyapatite, silica, hydrated silica, kaolin and the like.
7. The cosmetic pigment powder prepared by the method for preparing cosmetic pigment powder according to any one of claims 1 to 6, characterized in that: Used in the preparation of silicone-free cosmetics.
8. The use according to claim 7, characterized in that: The silicone-free cosmetics are selected from any one of liquid foundation, foundation cream, natural cream, concealer, sunscreen, face cream, and isolation cream.
9. The use according to claim 8, characterized in that: The foundation liquid comprises 12-13% by mass of the cosmetic pigment powder.
Citation Information
Patent Citations
Modified titanium dioxide and preparation method thereof
CN115449235B
Cited By
Composite cosmetic powder with water resistance and skin fitness and preparation method
CN119488440A