Slow cooling forming device for zinc alloy liquid

By introducing slow cooling and automated demolding components into the zinc alloy molding device, the strength problems caused by rapid cooling and low manual demolding efficiency during the zinc alloy molding process are solved, and safe cooling and efficient demolding are achieved.

CN118976885APending Publication Date: 2024-11-19山西启运金属制品有限公司
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411077580.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-06
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

The existing zinc alloy molding devices are prone to cracking in the rapid cooling process, and the mold release process requires manual operation and low efficiency.

Method used

A zinc alloy liquid slow cooling molding device is designed, using hydraulic rod to drive the upper mold and molding cavity to cooperate. The cooling component uses activated carbon adsorption layer, refrigerator and heat dissipation device to achieve slow cooling, and the release component uses electric telescopic rod. and spring mechanism automatic mold release.

Benefits of technology

Effectively prevent zinc alloy from cracking due to rapid cooling, ensure the strength of the finished product, and reduce manual operation time through automated mold release components and improve production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118976885A_ABST
    Figure CN118976885A_ABST
Patent Text Reader

Abstract

The invention discloses a zinc alloy liquid slow cooling forming device, and relates to the technical field of zinc alloy liquid cooling forming, the zinc alloy liquid slow cooling forming device comprises a base, the top of the base is provided with a lower die, the top of the lower die is provided with a forming cavity, the top of the base is provided with a mounting rack, and the inner top of the mounting rack is provided with a hydraulic rod; a liquid inlet pipe is arranged on the right side wall of the upper mold in a penetrating and communicating mode, a forming block matched with the forming cavity is arranged at the bottom of the upper mold, a cooling assembly is arranged on the rear side wall of the mounting frame, a cavity is formed in the lower mold, and a demolding assembly is arranged in the cavity. Zinc alloy is prevented from adhering to the inner wall of the forming cavity, and zinc alloy cracking or influence on the use strength caused by rapid cooling is avoided; and under the action of the demolding assembly, the cooled zinc alloy can be rapidly demolded, and manual demolding is not needed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of zinc alloy liquid cooling and forming, in particular to a zinc alloy liquid slow cooling and forming device. Background Art

[0002] Zinc alloy is an alloy composed of zinc and other elements. Commonly added alloying elements include aluminum, copper, magnesium, cadmium, lead, titanium, etc. Zinc alloy has a low melting point, good fluidity, easy to weld, braze and plastic processing, corrosion resistance in the atmosphere, and waste materials are easy to recycle and remelt, but the creep strength is low and it is easy to cause dimensional changes due to natural aging. Zinc alloy can be divided into two categories according to the processing technology: deformation zinc alloy and casting zinc alloy. Casting zinc alloy has good fluidity and corrosion resistance, and is suitable for die-casting instruments, automobile parts shells, etc. The zinc alloy liquid is injected into the mold for molding. In order to improve the efficiency of cooling and cooling, the current mold mostly uses cooling water for spraying and cooling. However, at this time, the molded zinc alloy is in a high temperature state. Rapid cooling will cause the molded zinc alloy to crack or affect its use strength, which may be counterproductive; and the existing molding device is not convenient for demolding the zinc alloy after molding, and manual demolding is required, which is slow. Therefore, we propose a zinc alloy liquid slow cooling molding device. Summary of the invention

[0003] The object of the present invention is to provide a zinc alloy liquid slow cooling molding device to solve the problems raised in the above background technology.

[0004] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a zinc alloy liquid slow cooling molding device, comprising a base, a lower mold is arranged on the top of the base, a molding cavity is opened on the top of the lower mold, a mounting frame is arranged on the top of the base, a hydraulic rod is arranged on the top of the mounting frame, an upper mold is arranged on one end of the hydraulic rod, a liquid inlet pipe is arranged through the right side wall of the upper mold, a molding block matching the molding cavity is arranged at the bottom of the upper mold, a cooling assembly is arranged on the rear side wall of the mounting frame, the cooling assembly comprises a cooling box arranged on the rear side wall of the mounting frame, an activated carbon adsorption layer is arranged on the inner wall of the cooling box, a liquid adding pipe is arranged through the top of the cooling box, and a cooling A refrigerator is provided at the bottom of the cooling box, a heat dissipation device is penetrated and connected through the left side wall of the cooling box, a water pump is provided on the right side wall of the cooling box, a water inlet pipe is provided at one end of the water pump, a water pump is provided on the left side wall of the cooling box, a return pipe is provided at one end of the water pump, a first cooling cavity and a second cooling cavity are provided inside the lower mold, one end of the water inlet pipe is connected to the inside of the first cooling cavity, one end of the water pump is connected to the inside of the second cooling cavity, a plurality of cooling channels are provided inside the lower mold, both ends of the cooling channels are respectively connected to the inside of the first cooling cavity and the second cooling cavity, a cavity is provided inside the lower mold, and a demolding component is provided in the cavity.

[0005] The top of the two sliding panels is hinged on the top of the two sliding panels, and one end of the two sliding panels is hinged on the top of the two sliding panels, and the other end of the two sliding panels is hinged on the bottom of the two sliding panels.

[0006] Furthermore, the left and right side walls in the cavity are both provided with limiting grooves, and the left and right side walls of the sliding plate and the top plate are both provided with limiting blocks matching the limiting grooves.

[0007] Furthermore, a guide groove is provided at the bottom of the cavity, and a guide block matching the guide groove is provided at the bottom of the sliding block.

[0008] Furthermore, a placement groove is provided at the bottom of the molding cavity, and the stripping plate matches the placement groove.

[0009] Furthermore, the extrusion block and the movable block are both arranged in an isosceles trapezoidal shape.

[0010] Furthermore, the first cooling cavity and the second cooling cavity are both arranged in a rectangular ring shape, and the first cooling cavity and the second cooling cavity are both arranged outside the molding cavity.

[0011] Furthermore, a plurality of groups of cooling channels are arranged in a rectangular ring shape in the lower mold.

[0012] Compared with the prior art, the beneficial effects of the present invention are as follows: the present invention can slowly cool the formed zinc alloy under the action of the cooling component, prevent the zinc alloy from adhering to the inner wall of the forming cavity, and avoid rapid cooling to cause the zinc alloy to crack or affect its use strength; the cooled zinc alloy can be quickly demolded under the action of the demolding component, and manual demolding is not required. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 1 It is a schematic diagram of the structure of the present invention;

[0014] Figure 2 It is a rear view of the structure of the present invention;

[0015] Figure 3This is a rear view of the internal structure of the cooling box of the present invention;

[0016] Figure 4 This is a schematic diagram of the structure of the first cooling cavity, the cooling channel and the second cooling cavity of the present invention;

[0017] Figure 5 A top view of the internal structure of the first cooling chamber of the present invention;

[0018] Figure 6 Schematic diagram of the internal structure of the cavity of the present invention.

[0019] In the figure: 1, base; 2, lower mold; 3, molding cavity; 4, cooling assembly; 40, water inlet pipe; 41, cooling box; 42, water pump; 43, reflux pipe; 44, water pump; 45, heat dissipation device; 46, refrigerator; 47, activated carbon adsorption layer; 48, first cooling cavity; 49, cooling channel; 400, second cooling cavity; 5, mounting frame; 6, molding block; 7, liquid inlet pipe; 8, upper mold; 9, hydraulic rod; 10, cavity; 11, demoulding assembly; 110, demoulding plate; 11111, placement groove; 11112, movable rod; 113, top plate; 114, sliding plate; 115, connecting rod; 116, sliding rod; 117, slider; 11118, spring; 11119, slide groove; 1100, movable block; 1101, extrusion block; 1102, sliding block; 1103, electric telescopic rod. DETAILED DESCRIPTION

[0020] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0021] Embodiment 1:

[0022] See also Figure 1-6The present invention provides a technical solution: a zinc alloy liquid slow cooling molding device, comprising a base 1, a lower mold 2 is arranged on the top of the base 1, a molding cavity 3 is opened on the top of the lower mold 2, a mounting frame 5 is arranged on the top of the base 1, a hydraulic rod 9 is arranged on the top of the mounting frame 5, an upper mold 8 is arranged at one end of the hydraulic rod 9, a liquid inlet pipe 7 is penetrated and connected to the right side wall of the upper mold 8, a molding block 6 matching the molding cavity 3 is arranged at the bottom of the upper mold 8, a cooling component 4 is arranged on the rear side wall of the mounting frame 5, the cooling component 4 includes a cooling box 41 arranged on the rear side wall of the mounting frame 5, an activated carbon adsorption layer 47 is arranged on the inner wall of the cooling box 41, a liquid adding pipe is penetrated on the top of the cooling box 41, a refrigerator 46 is arranged on the bottom of the cooling box 41, a heat dissipation device 45 is penetrated and connected to the left side wall of the cooling box 41, a water pump 44 is arranged on the right side wall of the cooling box 41, and the water pump 4 4 is provided with a water inlet pipe 40 at one end, a water pump 42 is provided on the left wall of the cooling box 41, a return pipe 43 is provided at one end of the water pump 42, a first cooling cavity 48 and a second cooling cavity 400 are provided inside the lower mold 2, the first cooling cavity 48 and the second cooling cavity 400 are both arranged in a rectangular ring shape, the first cooling cavity 48 and the second cooling cavity 400 are both arranged outside the molding cavity 3, one end of the water inlet pipe 40 is connected with the inside of the first cooling cavity 48, one end of the water pump 42 is connected with the inside of the second cooling cavity 400, a plurality of cooling channels 49 are provided inside the lower mold 2, both ends of the cooling channels 49 are respectively connected with the inside of the first cooling cavity 48 and the second cooling cavity 400, the plurality of cooling channels 49 are arranged in a rectangular ring shape inside the lower mold 2, a cavity 10 is provided inside the lower mold 2, and a demoulding component 11 is provided in the cavity 10.

[0023] See also Figure 6The demoulding assembly 11 includes a top plate 113 and a sliding plate 114 which are slidably connected in the cavity 10. The left and right side walls of the cavity 10 are provided with limiting grooves. The left and right side walls of the sliding plate 114 and the top plate 113 are provided with limiting blocks matching the limiting grooves. Under the action of the limiting blocks and the limiting grooves, the sliding plate 114 and the top plate 113 move up and down more stably. A movable rod 112 is provided on the top of the top plate 113. One end of the movable rod 112 passes through the top of the cavity 10 and is connected to the stripping plate 110 provided in the molding cavity 3. A placement groove 111 is provided at the bottom of the molding cavity 3. The stripping plate 110 matches the placement groove 111. Under the action of the placement plate 111, the stripping plate 110 can be folded The sliding plate 114 is provided with a sliding groove 119 at the top, and a sliding rod 116 is provided in the sliding groove 119. The two ends of the sliding rod 116 are respectively connected to the left and right side walls in the sliding groove 119. The outer wall of the sliding rod 116 is sleeved with two groups of sliders 117. The outer wall of the sliding rod 116 is sleeved with two groups of springs 118. One end of the two groups of springs 118 is respectively connected to the side walls away from the two groups of sliders 117. The other ends of the two groups of springs 118 are respectively connected to the left and right side walls in the sliding groove 119. The tops of the two groups of sliders 117 are hinged with connecting rods 115. One end of the two groups of connecting rods 115 is hinged to the bottom of the top plate 113. The bottom of the sliding plate 114 is provided with a movable block 1100. The bottom of the cavity 10 is slidably connected with a sliding block 1100. The movable block 1102 has a guide groove at the bottom of the cavity 10, and a guide block matching the guide groove is provided at the bottom of the sliding block 1102. Under the action of the guide groove and the guide block, the sliding block 1102 moves left and right more stably. The top of the sliding block 1102 is provided with an extrusion block 1101, and the right side wall of the cavity 10 is provided with an electric telescopic rod 1103, one end of the electric telescopic rod 1103 is connected to the right side wall of the sliding block 1102, and the extrusion block 1101 and the movable block 1100 are both arranged in an isosceles trapezoidal shape. The electric telescopic rod 1103 drives the sliding block 1102 to move left and right, and the sliding block 1102 drives the extrusion block 1101 to move left and right. The inclined surface of the extrusion block 1101 can move the movable block 11 00 is extruded, the movable block 1100 drives the sliding plate 114 to move upward, the sliding plate 114 extrudes the connecting rod 115, the connecting rod 115 drives the slider 117 to squeeze the spring 118 on the outer wall of the sliding rod 116, the connecting rod 115 drives the top plate 113 to move upward, the top plate 113 drives the movable rod 112 to move upward, the movable rod 112 drives the stripping plate 110 to move upward to eject the formed zinc alloy, and completes the demoulding of the zinc alloy. After the demoulding is completed, the spring 118 can drive the connecting rod 115 to reset, the connecting rod 115 drives the top plate 113 and the stripping plate 110 to move downward, and the stripping plate 110 is stored in the placement groove 111.

[0024] Working principle: the hydraulic rod 9 drives the upper mold 8 to move downward, and the upper mold 8 drives the forming block 6 to cooperate with the forming cavity 3, and then the zinc alloy liquid enters the forming cavity 3 from the liquid inlet pipe 7. With the cooperation of the forming block 6, the zinc alloy can be formed. When the formed zinc alloy needs to be cooled, the coolant in the cooling box 41 can be cooled by the refrigerator 46, and the heat generated by the cooling can be dissipated by the heat dissipation device 45. The water pump 44 transports the coolant to the first cooling cavity 48 through the water inlet pipe 40, and then the coolant slowly enters the second cooling cavity 400 along the cooling channel 49, so that the formed zinc alloy can be cooled and formed. Under the action of the water pump 42, the coolant in the second cooling cavity 400 can be pumped into the cooling box 41 through the reflux pipe 43, and the coolant can be adsorbed and purified under the action of the activated carbon adsorption layer 47. Under the action of the refrigerator 46, the coolant can be cooled to achieve recycling. The hydraulic rod 9 drives the upper mold 8 to move upward, and the molding block 6 can be separated from the molding cavity 3. Then the electric telescopic rod 1103 drives the sliding block 1102 to move left and right. The sliding block 1102 drives the extrusion block 1101 to move left and right. The inclined surface of the extrusion block 1101 can squeeze the inclined surface of the movable block 1100. The movable block 1100 drives the sliding plate 114 to move upward. The sliding plate 114 squeezes the connecting rod 115. The connecting rod 115 drives the slider 117 to move on the sliding rod 116. The outer wall squeezes the spring 118, the connecting rod 115 drives the top plate 113 to move upward, the top plate 113 drives the movable rod 112 to move upward, the movable rod 112 drives the stripping plate 110 to move upward to eject the formed zinc alloy, and completes the demolding of the zinc alloy. After the demolding is completed, the spring 118 can drive the connecting rod 115 to reset under the action of the elastic force of the spring 118, and the connecting rod 115 drives the top plate 113 and the stripping plate 110 to move downward, and the stripping plate 110 is stored in the placement groove 111.

[0025] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A zinc alloy liquid slow cooling molding device, comprising a base (1), a lower mold (2) is provided on the top of the base (1), a molding cavity (3) is opened on the top of the lower mold (2), a mounting frame (5) is provided on the top of the base (1), a hydraulic rod (9) is provided on the top of the mounting frame (5), an upper mold (8) is provided at one end of the hydraulic rod (9), a liquid inlet pipe (7) is provided through and connected to the right side wall of the upper mold (8), and a molding block (6) matching the molding cavity (3) is provided at the bottom of the upper mold (8), characterized in that: The rear side wall of the mounting frame (5) is provided with a cooling assembly (4), and the cooling assembly (4) includes a cooling box (41) provided on the rear side wall of the mounting frame (5), an activated carbon adsorption layer (47) is provided on the inner wall of the cooling box (41), a liquid adding pipe is provided through the top of the cooling box (41), a refrigerator (46) is provided at the bottom of the cooling box (41), a heat dissipation device (45) is provided through the left side wall of the cooling box (41), a water pump (44) is provided on the right side wall of the cooling box (41), a water inlet pipe (40) is provided at one end of the water pump (44), a water pump (42) is provided on the left side wall of the cooling box (41), and the water pump ( A return pipe (43) is provided at one end of the lower mold (42), a first cooling cavity (48) and a second cooling cavity (400) are provided inside the lower mold (2), one end of the water inlet pipe (40) is connected to the inside of the first cooling cavity (48), one end of the water pump (42) is connected to the inside of the second cooling cavity (400), a plurality of cooling channels (49) are provided inside the lower mold (2), two ends of the cooling channels (49) are respectively connected to the inside of the first cooling cavity (48) and the second cooling cavity (400), a cavity (10) is provided inside the lower mold (2), and a demoulding component (11) is provided in the cavity (10).

2. The zinc alloy liquid slow cooling forming device according to claim 1, characterized in that: The demoulding assembly (11) comprises a top plate (113) and a sliding plate (114) which are slidably connected in the cavity (10); a movable rod (112) is provided on the top of the top plate (113); one end of the movable rod (112) passes through the top of the cavity (10) and is connected to a demoulding plate (110) provided in the molding cavity (3); a sliding groove (119) is provided on the top of the sliding plate (114); a sliding rod (116) is provided in the sliding groove (119); two ends of the sliding rod (116) are respectively connected to the left and right side walls in the sliding groove (119); two groups of sliding blocks (117) are sleeved on the outer wall of the sliding rod (116); two groups of springs (118) are sleeved on the outer wall of the sliding rod (116); the two groups of springs (118) ) one end is respectively connected to the side wall away from the two groups of sliders (117), the other ends of the two groups of springs (118) are respectively connected to the left and right side walls in the slide groove (119), the tops of the two groups of sliders (117) are hinged with connecting rods (115), one end of the two groups of connecting rods (115) are hinged with the bottom of the top plate (113), a movable block (1100) is provided at the bottom of the sliding plate (114), a sliding block (1102) is slidably connected to the bottom of the cavity (10), an extrusion block (1101) is provided on the top of the sliding block (1102), an electric telescopic rod (1103) is provided on the right side wall of the cavity (10), and one end of the electric telescopic rod (1103) is connected to the right side wall of the sliding block (1102).

3. The zinc alloy liquid slow cooling forming device according to claim 2, characterized in that: The left and right side walls of the cavity (10) are both provided with limiting grooves, and the left and right side walls of the sliding plate (114) and the top plate (113) are both provided with limiting blocks matching the limiting grooves.

4. The zinc alloy liquid slow cooling molding device according to claim 2, characterized in that: A guide groove is provided at the bottom of the cavity (10), and a guide block matching the guide groove is provided at the bottom of the sliding block (1102).

5. The zinc alloy liquid slow cooling molding device according to claim 2, characterized in that: The bottom of the molding cavity (3) is provided with a placement groove (111), and the stripping plate (110) matches the placement groove (111).

6. The zinc alloy liquid slow cooling molding device according to claim 2, characterized in that: The extrusion block (1101) and the movable block (1100) are both arranged in an isosceles trapezoidal shape.

7. The zinc alloy liquid slow cooling molding device according to claim 1, characterized in that: The first cooling cavity (48) and the second cooling cavity (400) are both arranged in a rectangular ring shape, and the first cooling cavity (48) and the second cooling cavity (400) are both arranged outside the molding cavity (3).

8. The zinc alloy liquid slow cooling molding device according to claim 1, characterized in that: A plurality of groups of cooling channels (49) are arranged in a rectangular ring shape inside the lower mold (2).

Citation Information

Cited By

  • Ingot casting forming system and process for zinc alloy machining

    CN119772121A