Color complementing cream for leather products and preparation method of color complementing cream

By using fluorocarbon resin and crosslinking modification additives in leather products, combined with glass fiber hybrid modified graphene agent and reinforcement agent, the problem of poor stain resistance of color replenishing cream in leather products in the prior art is solved. , achieving improved wear and stain resistance and improved performance stability of the product.

CN118978836APending Publication Date: 2024-11-19GUANGZHOU ZUOLI CHEM CO LTD

Patent Information

Application Number
CN202411186587.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-28
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

The existing leather color-replenishing cream has poor interfacial properties due to the poor interface between resin raw materials and bentonite, which affects the wear resistance and use efficiency of the product.

Method used

A color replenishing cream for leather products is prepared by combining fluorocarbon resin with cross-linking modification additives, defoaming agent and ethanol solvent. .

Benefits of technology

It significantly improves the wear and stain resistance of the product, and maintains performance stability under saline and alkali conditions, and coordinates the overall effect of the product.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
Patent Text Reader

Abstract

The invention discloses color complementing cream for leather products. The color complementing cream is prepared from the following raw materials in parts by weight: 40-50 parts of fluorocarbon resin, 10-20 parts of a crosslinking modified additive, 2-5 parts of a reinforcing agent, 2-6 parts of pigment, 1-3 parts of a defoaming agent and 45-55 parts of an ethanol solvent. According to the color complementing cream, the fluorocarbon resin is matched with the cross-linking modified additive and the reinforcing agent, the pigment, the defoaming agent and the ethanol solvent are added to serve as auxiliaries, the prepared color complementing cream has excellent wear resistance and stain resistance, meanwhile, the color complementing cream and the pigment are excellent in coordination performance, and the product is excellent in performance stability under the saline-alkaline condition and has the good color complementing effect. The crosslinking modified additive is matched with the unique raw material of the crosslinking modified additive through the glass fiber hybrid modified graphene agent, so that the crosslinking modified additive and the reinforcing agent can achieve synergistic interaction, the performance effect of a product system is enhanced, and the effect stability of the product is coordinated and improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of leather products, and in particular to a color-replenishing cream for leather products and a preparation method thereof. Background Art

[0002] Leather products are practical items made entirely or mainly of leather. They include wheel tyres, harnesses, gun holsters, oil seals, leather shoes, leather clothing, suitcases, leather balls, etc. They can be used in industry, agriculture, military supplies and daily life. Leather products are durable, elastic, not easy to deform, and have good hygienic properties, so they are widely used.

[0003] Existing leather product color-repairing creams use resin raw materials combined with inorganic agents such as bentonite, which easily leads to poor interface of the raw materials, resulting in poor stain resistance of the product, thereby affecting the product's stain resistance and wear resistance coordination, and reducing the product's use efficiency. Summary of the invention

[0004] In view of the defects of the prior art, the object of the present invention is to provide a color-correcting cream for leather products and a preparation method thereof, so as to solve the problems raised in the above-mentioned background technology.

[0005] The present invention solves the technical problem by adopting the following technical solution: The present invention provides a color-replenishing cream for leather products, comprising the following raw materials in parts by weight: 40-50 parts of fluorocarbon resin, 10-20 parts of cross-linking modification additive, 2-5 parts of reinforcing agent, 2-6 parts of pigment, 1-3 parts of defoaming agent, and 45-55 parts of ethanol solvent.

[0006] Preferably, the color-replenishing cream for leather products comprises the following raw materials in parts by weight: 45 parts of fluorocarbon resin, 15 parts of cross-linking modification additive, 3.5 parts of reinforcing agent, 4 parts of pigment, 2 parts of defoaming agent, and 50 parts of ethanol solvent.

[0007] Preferably, the preparation method of the cross-linking modification additive is: S01: terephthalaldehyde, melamine and paraformaldehyde are mixed in a weight ratio of 1:4:2, and then a 5% by mass sodium hydroxide aqueous solution is added, the pH is adjusted to 7.5, and the mixture is reacted at 65-75°C for 30-40 minutes at a reaction speed of 450-550 r / min; S02: then add 15-20% of divinylbenzene, 2-5% of maleic anhydride, and 1-5% of silane coupling agent KH560 to the product, and stir; S03: Then, 1-3% of azobisisobutyronitrile and 10-20% of glass fiber hybrid modified graphene agent are added to the total amount of divinylbenzene, and the mixture is stirred for 5-10 minutes. After the stirring is completed, a cross-linked modified additive is obtained.

[0008] Preferably, the rotation speed in S02 is 300-500r / min, and the stirring speed is 10-20min.

[0009] Preferably, the preparation method of the glass fiber hybrid modified graphene agent is: Add graphene to 3-5 times of deionized water, then add hydrochloric acid to adjust the pH value to 5.5, then add chitosan (10-15%) of the total amount of graphene and sodium cellulose sulfate (1-5%), stir evenly, and obtain a graphene agent; The glass fiber is added into an ethanol solvent at a weight ratio of 1:4 and dispersed evenly, and then 10-15% of yttrium trioxide and 1-5% of silica sol are added to the total amount of the glass fiber, stirred evenly, and then washed with water and dried to obtain a glass fiber modifier; the glass fiber modifier is added into a graphene agent at a weight ratio of 1:5 and stirred sufficiently, and then washed with water and dried to obtain a glass fiber hybrid modified graphene agent.

[0010] Preferably, the aspect ratio of the glass fiber is (15-20):1.

[0011] Preferably, the pigment is a nano-dispersed pigment; and the defoaming agent is a silicon defoaming agent.

[0012] Preferably, the reinforcing agent comprises the following raw materials in parts by weight: 2-5 parts of acetaminophen, 1-3 parts of titanate coupling agent, 0.2-0.5 parts of sodium cyclohexanenate, and 0.5-1.0 parts of tocopherol acetate.

[0013] The present invention also provides a method for preparing a color-replenishing cream for leather products, comprising the following steps: The fluorocarbon resin, the cross-linking modification additive, the reinforcing agent, the pigment, the defoaming agent and the ethanol solvent are stirred and mixed in sequence until fully mixed to obtain a color-replenishing cream.

[0014] Preferably, the stirring and mixing time is 35-45 min, and the stirring speed is 650-850 r / min.

[0015] Compared with the prior art, the present invention has the following beneficial effects: The color-replenishing cream of the present invention adopts fluorocarbon resin in combination with a cross-linking modification additive and a reinforcing agent, and by adding a pigment, a defoaming agent, and an ethanol solvent as auxiliary agents, the prepared color-replenishing cream has excellent wear resistance and stain resistance, and the coordinated performance of the two is excellent, and the product has excellent performance stability under saline-alkali conditions. The cross-linking modification additive is a unique raw material of a glass fiber hybrid modified graphene agent combined with a cross-linking modification additive, which can synergize with the reinforcing agent to enhance the performance effect of the product system and coordinately improve the effect stability of the product. DETAILED DESCRIPTION

[0016] The following is a clear and complete description of the technical solutions in the embodiments of the present invention in conjunction with specific embodiments. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0017] Example 1. A color-replenishing cream for leather products according to the present embodiment comprises the following raw materials in parts by weight: 40 parts of fluorocarbon resin, 10 parts of cross-linking modification additive, 2 parts of reinforcing agent, 2 parts of pigment, 1 part of defoaming agent, and 45 parts of ethanol solvent.

[0018] The preparation method of the cross-linking modified additive of this embodiment is: S01: terephthalaldehyde, melamine and paraformaldehyde were mixed in a weight ratio of 1:4:2, and then a 5% by mass sodium hydroxide aqueous solution was added, the pH was adjusted to 7.5, and the mixture was reacted at 65°C for 30 minutes at a reaction speed of 450 r / min; S02: then add 15% of divinylbenzene, 2% of maleic anhydride and 1% of silane coupling agent KH560 to the product and stir; S03: Then, 1% of azobisisobutyronitrile and 10% of glass fiber hybrid modified graphene agent were added to the total amount of divinylbenzene, and the mixture was stirred for 5 minutes. After the stirring was completed, a cross-linked modified additive was obtained.

[0019] The rotation speed in S02 of this embodiment is 300r / min, and the stirring speed is 10min.

[0020] The preparation method of the glass fiber hybrid modified graphene agent of this embodiment is: Graphene was added to 3 times of deionized water, and then hydrochloric acid was added to adjust the pH value to 5.5, followed by adding chitosan (10% of the total amount of graphene) and sodium cellulose sulfate (1%), and stirred evenly to obtain a graphene agent; The glass fiber is added into an ethanol solvent at a weight ratio of 1:4 and dispersed evenly, and then 10% of yttrium trioxide and 1% of silica sol are added to the total amount of the glass fiber, stirred evenly, washed with water, and dried to obtain a glass fiber modifier; the glass fiber modifier is added into a graphene agent at a weight ratio of 1:5 and stirred sufficiently, and then washed with water and dried to obtain a glass fiber hybrid modified graphene agent.

[0021] The aspect ratio of the glass fiber in this embodiment is 15:1.

[0022] The pigment of this embodiment is a nano-dispersed pigment; the defoaming agent is a silicon defoaming agent.

[0023] The reinforcing agent of this embodiment includes the following raw materials in parts by weight: 2 parts of acetaminophen, 1 part of titanate coupling agent, 0.2 parts of sodium cyclohexanenate, and 0.5 parts of tocopherol acetate.

[0024] A method for preparing a color-replenishing cream for leather products in this embodiment comprises the following steps: The fluorocarbon resin, the cross-linking modification additive, the reinforcing agent, the pigment, the defoaming agent and the ethanol solvent are stirred and mixed in sequence until fully mixed to obtain a color-replenishing cream.

[0025] The stirring and mixing time in this embodiment is 35 minutes, and the stirring speed is 650 r / min.

[0026] Example 2. A color-replenishing cream for leather products according to the present embodiment comprises the following raw materials in parts by weight: 50 parts of fluorocarbon resin, 20 parts of cross-linking modification additive, 5 parts of reinforcing agent, 6 parts of pigment, 3 parts of defoaming agent, and 55 parts of ethanol solvent.

[0027] The preparation method of the cross-linking modified additive of this embodiment is: S01: terephthalaldehyde, melamine and paraformaldehyde were mixed in a weight ratio of 1:4:2, and then a 5% by mass sodium hydroxide aqueous solution was added, the pH was adjusted to 7.5, and the mixture was reacted at 75°C for 40 minutes at a reaction speed of 450-550 r / min; S02: then add 20% of divinylbenzene, 5% of maleic anhydride and 5% of silane coupling agent KH560 to the product, and stir; S03: Then, 3% of azobisisobutyronitrile and 20% of glass fiber hybrid modified graphene agent were added to the total amount of divinylbenzene, and the mixture was stirred for 10 minutes. After the stirring was completed, a cross-linked modified additive was obtained.

[0028] The rotation speed in S02 of this embodiment is 500r / min, and the stirring speed is 20min.

[0029] The preparation method of the glass fiber hybrid modified graphene agent of this embodiment is: Graphene was added to 5 times of deionized water, and then hydrochloric acid was added to adjust the pH value to 5.5, followed by adding chitosan (15% of the total amount of graphene) and sodium cellulose sulfate (5%), and stirred evenly to obtain a graphene agent; The glass fiber is added into an ethanol solvent at a weight ratio of 1:4 and dispersed evenly, and then 15% of yttrium trioxide and 5% of silica sol are added to the total amount of the glass fiber, stirred evenly, and then washed with water and dried to obtain a glass fiber modifier; the glass fiber modifier is added into a graphene agent at a weight ratio of 1:5 and stirred sufficiently, and then washed with water and dried to obtain a glass fiber hybrid modified graphene agent.

[0030] The aspect ratio of the glass fiber in this embodiment is 20:1.

[0031] The pigment of this embodiment is a nano-dispersed pigment; the defoaming agent is a silicon defoaming agent.

[0032] The reinforcing agent of this embodiment includes the following raw materials in parts by weight: 5 parts of acetaminophen, 3 parts of titanate coupling agent, 0.5 parts of sodium cyclohexanenate, and 1.0 parts of tocopherol acetate.

[0033] A method for preparing a color-replenishing cream for leather products in this embodiment comprises the following steps: The fluorocarbon resin, the cross-linking modification additive, the reinforcing agent, the pigment, the defoaming agent and the ethanol solvent are stirred and mixed in sequence until fully mixed to obtain a color-replenishing cream.

[0034] The stirring and mixing time in this embodiment is 45 minutes, and the stirring speed is 850 r / min.

[0035] Example 3. A color-replenishing cream for leather products according to the present embodiment comprises the following raw materials in parts by weight: 45 parts of fluorocarbon resin, 15 parts of cross-linking modification additive, 3.5 parts of reinforcing agent, 4 parts of pigment, 2 parts of defoaming agent, and 50 parts of ethanol solvent.

[0036] The preparation method of the cross-linking modified additive of this embodiment is: S01: terephthalaldehyde, melamine and paraformaldehyde were mixed in a weight ratio of 1:4:2, and then a 5% by mass sodium hydroxide aqueous solution was added, the pH was adjusted to 7.5, and the mixture was reacted at 70°C for 35 minutes at a reaction speed of 500 r / min; S02: then add 17.5% of divinylbenzene, 3.5% of maleic anhydride and 3% of silane coupling agent KH560 to the product, and stir; S03: Then, 2% of azobisisobutyronitrile and 15% of glass fiber hybrid modified graphene agent were added to the total amount of divinylbenzene, and the mixture was stirred for 7.5 minutes. After the stirring was completed, a cross-linked modified additive was obtained.

[0037] The rotation speed in S02 of this embodiment is 400r / min, and the stirring speed is 15min.

[0038] The preparation method of the glass fiber hybrid modified graphene agent of this embodiment is: Graphene was added to 4 times of deionized water, and then hydrochloric acid was added to adjust the pH value to 5.5, followed by adding chitosan (12.5% ​​of the total amount of graphene) and sodium cellulose sulfate (3%), and stirred evenly to obtain a graphene agent; The glass fiber is added into an ethanol solvent at a weight ratio of 1:4 and dispersed evenly, and then 12.5% ​​of yttrium trioxide and 3% of silica sol are added to the total amount of the glass fiber, stirred evenly, washed with water, and dried to obtain a glass fiber modifier; the glass fiber modifier is added into a graphene agent at a weight ratio of 1:5 and stirred sufficiently, and then washed with water and dried to obtain a glass fiber hybrid modified graphene agent.

[0039] The aspect ratio of the glass fiber in this embodiment is 17:1.

[0040] The pigment of this embodiment is a nano-dispersed pigment; the defoaming agent is a silicon defoaming agent.

[0041] The reinforcing agent of this embodiment includes the following raw materials in parts by weight: 2-5 parts of acetaminophen, 2 parts of titanate coupling agent, 0.2-0.5 parts of sodium cyclohexanenate, and 0.75 parts of tocopherol acetate.

[0042] A method for preparing a color-replenishing cream for leather products in this embodiment comprises the following steps: The fluorocarbon resin, the cross-linking modification additive, the reinforcing agent, the pigment, the defoaming agent and the ethanol solvent are stirred and mixed in sequence until fully mixed to obtain a color-replenishing cream.

[0043] The stirring and mixing time in this embodiment is 40 minutes, and the stirring speed is 700 r / min.

[0044] Example 4. A color-replenishing cream for leather products according to the present embodiment comprises the following raw materials in parts by weight: 42 parts of fluorocarbon resin, 12 parts of cross-linking modification additive, 3 parts of reinforcing agent, 3 parts of pigment, 2 parts of defoaming agent, and 46 parts of ethanol solvent.

[0045] The preparation method of the cross-linking modified additive of this embodiment is: S01: terephthalaldehyde, melamine and paraformaldehyde were mixed in a weight ratio of 1:4:2, and then a 5% by mass sodium hydroxide aqueous solution was added, the pH was adjusted to 7.5, and the mixture was reacted at 68°C for 32 minutes at a reaction speed of 460 r / min; S02: then add 18% of divinylbenzene, 3% of maleic anhydride and 2% of silane coupling agent KH560 to the product, and stir; S03: Then, 2% of azobisisobutyronitrile and 12% of glass fiber hybrid modified graphene agent were added to the total amount of divinylbenzene, and the mixture was stirred for 6 minutes. After the stirring was completed, a cross-linked modified additive was obtained.

[0046] The rotation speed in S02 of this embodiment is 320r / min, and the stirring speed is 12min.

[0047] The preparation method of the glass fiber hybrid modified graphene agent of this embodiment is: Graphene was added to 4 times of deionized water, and then hydrochloric acid was added to adjust the pH value to 5.5, followed by adding 12% of chitosan and 2% of sodium cellulose sulfate to the total amount of graphene, and stirred evenly to obtain a graphene agent; The glass fiber is added into an ethanol solvent at a weight ratio of 1:4 and dispersed evenly, and then 12% of yttrium trioxide and 2% of silica sol are added to the total amount of the glass fiber, stirred evenly, washed with water, and dried to obtain a glass fiber modifier; the glass fiber modifier is added into a graphene agent at a weight ratio of 1:5 and stirred sufficiently, and then washed with water and dried to obtain a glass fiber hybrid modified graphene agent.

[0048] The aspect ratio of the glass fiber in this embodiment is 16:1.

[0049] The pigment of this embodiment is a nano-dispersed pigment; the defoaming agent is a silicon defoaming agent.

[0050] The reinforcing agent of this embodiment includes the following raw materials in parts by weight: 3 parts of acetaminophen, 2 parts of titanate coupling agent, 0.3 parts of sodium cyclohexanenate, and 0.6 parts of tocopherol acetate.

[0051] A method for preparing a color-replenishing cream for leather products in this embodiment comprises the following steps: The fluorocarbon resin, the cross-linking modification additive, the reinforcing agent, the pigment, the defoaming agent and the ethanol solvent are stirred and mixed in sequence until fully mixed to obtain a color-replenishing cream.

[0052] The stirring and mixing time of this embodiment is 38 minutes, and the stirring speed is 700 r / min.

[0053] Comparative Example 1. The difference from Example 3 is that the cross-linking modification additive is not added to the glass fiber hybrid modified graphene agent.

[0054] Comparative Example 2. The difference from Example 3 is that no graphene agent is added to the glass fiber hybrid modified graphene agent.

[0055] Comparative Example 3. The difference from Example 3 is that yttrium trioxide is not added to the glass fiber hybrid modified graphene agent.

[0056] Comparative Example 4. The difference from Example 3 is that the glass fiber hybrid modified graphene agent is replaced by graphene.

[0057] Comparative Example 5. The difference from Example 3 is that no reinforcing agent is added.

[0058] Comparative Example 6. The difference from Example 3 is that no sodium cyclopentaneate is added to the reinforcing agent.

[0059] Comparative Example 7. The difference from Example 3 is that no acetaminophen is added to the reinforcing agent.

[0060] Comparative Example 8. The difference from Example 3 is that tocopherol acetate is not added to the reinforcing agent.

[0061] The product properties of Examples 1-4 and Comparative Examples 1-8 of the present invention are as follows

[0062] It can be seen from Examples 1-4 and Comparative Examples 1-8 that the product of the present invention has excellent wear resistance and stain resistance, and the stain resistance and wear resistance of the product can achieve a coordinated improvement effect; By adding a cross-linking modification additive to a glass fiber hybrid modified graphene agent and a reinforcing agent, the performance of the product can be coordinated and improved; at the same time, when no graphene agent or yttrium trioxide is added to the glass fiber hybrid modified graphene agent and the glass fiber hybrid modified graphene agent is replaced by graphene, the performance of the product tends to deteriorate. Only the glass fiber hybrid modified graphene agent prepared by the method of the present invention and the reinforcing agent with the component ratio of the present invention have the most significant product performance effect.

[0063] The present invention treats the product under 4% salt spray conditions for 24 hours, and further tests the performance;

[0064] It can be seen from the salt spray resistance test of the present invention that the salt spray resistance performance stability of the product of the present invention is excellent. At the same time, only when the glass fiber hybrid modified graphene agent prepared by the method of the present invention is combined with the reinforcing agent with the component ratio of the present invention, the performance stability of the product is the most excellent.

[0065] It will be apparent to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above and that the present invention can be implemented in other specific forms without departing from the spirit or essential features of the present invention. Therefore, the embodiments should be considered exemplary and non-restrictive in all respects, and the scope of the present invention is defined by the appended claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims be included in the present invention.

[0066] In addition, it should be understood that although the present specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.

Claims

1. A color-replenishing cream for leather products, characterized in that: It includes the following raw materials in parts by weight: 40-50 parts of fluorocarbon resin, 10-20 parts of cross-linking modification additive, 2-5 parts of reinforcing agent, 2-6 parts of pigment, 1-3 parts of defoaming agent, and 45-55 parts of ethanol solvent.

2. The color-replenishing cream for leather products according to claim 1, characterized in that: The color-replenishing cream for leather products comprises the following raw materials in parts by weight: 45 parts of fluorocarbon resin, 15 parts of cross-linking modification additive, 3.5 parts of reinforcing agent, 4 parts of pigment, 2 parts of defoaming agent, and 50 parts of ethanol solvent.

3. The color-replenishing cream for leather products according to claim 1, characterized in that: The preparation method of the cross-linking modification additive is: S01: terephthalaldehyde, melamine and paraformaldehyde are mixed in a weight ratio of 1:4:2, and then a 5% by mass sodium hydroxide aqueous solution is added, the pH is adjusted to 7.5, and the mixture is reacted at 65-75°C for 30-40 minutes at a reaction speed of 450-550 r / min; S02: then add 15-20% of divinylbenzene, 2-5% of maleic anhydride, and 1-5% of silane coupling agent KH560 to the product, and stir; S03: Then, 1-3% of azobisisobutyronitrile and 10-20% of glass fiber hybrid modified graphene agent are added to the total amount of divinylbenzene, and the mixture is stirred for 5-10 minutes. After the stirring is completed, a cross-linked modified additive is obtained.

4. The color-replenishing cream for leather products according to claim 3, characterized in that: The rotation speed in the S02 is 300-500r / min, and the stirring speed is 10-20min.

5. The color-correcting cream for leather products according to claim 3, characterized in that: The preparation method of the glass fiber hybrid modified graphene agent is: Add graphene to 3-5 times of deionized water, then add hydrochloric acid to adjust the pH value to 5.5, then add chitosan (10-15%) of the total amount of graphene and sodium cellulose sulfate (1-5%), stir evenly, and obtain a graphene agent; The glass fiber is added into an ethanol solvent at a weight ratio of 1:4 and dispersed evenly, and then 10-15% of yttrium trioxide and 1-5% of silica sol are added to the total amount of the glass fiber, stirred evenly, and then washed with water and dried to obtain a glass fiber modifier; the glass fiber modifier is added into a graphene agent at a weight ratio of 1:5 and stirred sufficiently, and then washed with water and dried to obtain a glass fiber hybrid modified graphene agent.

6. The color-correcting cream for leather products according to claim 5, characterized in that: The aspect ratio of the glass fiber is (15-20):

1.

7. The color-correcting cream for leather products according to claim 1, characterized in that: The pigment is a nano-dispersed pigment; the defoaming agent is a silicon defoaming agent.

8. The color-correcting cream for leather products according to claim 1, characterized in that: The reinforcing agent comprises the following raw materials in parts by weight: 2-5 parts of acetaminophen, 1-3 parts of titanate coupling agent, 0.2-0.5 parts of sodium cyclohexanenate, and 0.5-1.0 parts of tocopherol acetate.

9. A method for preparing a color-replenishing cream for leather products as claimed in any one of claims 1 to 8, comprising the following steps: The fluorocarbon resin, the cross-linking modification additive, the reinforcing agent, the pigment, the defoaming agent and the ethanol solvent are stirred and mixed in sequence until fully mixed to obtain a color-replenishing cream.

10. The method for preparing the color-correcting cream for leather products according to claim 9, characterized in that: The stirring and mixing time is 35-45 minutes, and the stirring speed is 650-850 r / min.

Citation Information

Patent Citations

  • Cross-linked furniture coating and preparation method thereof

    CN105969029A

  • Polyurethane modified asphalt, waterborne polyurethane modified asphalt emulsion, waterborne polyurethane modified asphalt waterproof coating and preparation method thereof

    CN113429886A

  • Preparation method and use method of waterproof, anticorrosive and wear-resistant composite material

    CN113736210A

  • Glass fiber reinforced polyamide material for plastic high-pressure water gun and preparation method

    CN114249980A

  • Environment-friendly ceiling and preparation method thereof

    CN114410029A

Cited By

  • Waterproof coating for preventing ceramic tiles from falling off and preparation method thereof

    CN119505617A