Clothes ironing sizing aerosol and preparation method thereof

Through the combination of hydroxyethyl starch and biquaternary ammonium salt-modified dimethylsiloxane and polyethylene glycol-400, the problem of flatness, stiffness and flexibility after ironing of clothes is solved, and the flatness of clothes is achieved. Clever and smooth styling, and improves wrinkle resistance and safety.

CN118979385APending Publication Date: 2024-11-19GUANGDONG WESLEY CHEM TECH CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202411046629.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-01
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

Existing clothing ironing agents are difficult to make the clothing achieve a flat, stiff and not easily deformed shaping effect, and local deposition and brittle cracking are prone to ironing of high-plant fiber clothing.

Method used

Hydroxyethyl starch is used to cross-link dimethylsiloxane with biquaternary ammonium salt to reduce film formation hardness, and polyethylene glycol-400 is added to uniform penetration and diffusion, combining specific proportions of corrosion inhibitors and solubilizers , forming a soft and tough film to ensure that the clothes are smooth, crisp and smooth.

Benefits of technology

It achieves the flat, stiff and smooth shaping effects of the clothes, avoids brittle cracks and local deposition, improves the overall stiffness and wrinkle resistance of the clothes, and has the effect of sterilization, anti-mold and anti-static.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004973657630000071
    Figure BDA0004973657630000071
  • Figure BDA0004973657630000081
    Figure BDA0004973657630000081
  • Figure HDA0004973657640000011
    Figure HDA0004973657640000011
Patent Text Reader

Abstract

The invention relates to the field of clothes ironing, and particularly discloses a sizing aerosol for clothes ironing and a preparation method thereof. The clothing ironing sizing aerosol comprises the following components: hydroxyethyl starch, biquaternary ammonium salt modified dimethyl siloxane, polyethylene glycol-400, a corrosion inhibitor, a solubilizer, an aromatic, a propellant and water. After the sizing aerosol for ironing the clothes is sprayed on the surface of the clothes and is ironed at high temperature, a layer of soft thin film with high toughness can be formed on the surface of a fabric, brittle rupture is not prone to occurring, and therefore the clothes can keep a smooth and stiff shaping effect, and the clothes can be ironed at high temperature. And the construction problem that the hydroxyethyl starch is easy to locally deposit and difficult to uniformly spread is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of ironing, and in particular to a clothing ironing sizing aerosol and a preparation method thereof. Background Art

[0002] Clothes are prone to wrinkles during production, transportation, and storage. A lot of wrinkles not only damage the appearance and texture of the clothes, but may also weaken their functionality. For example, wrinkles may reduce the breathability and waterproofness of sports or waterproof fabrics. Therefore, wrinkled clothes need to be properly handled and maintained.

[0003] Clothes ironing agent is an additive used to spray on the surface of clothes to help eliminate wrinkles on clothes, which is beneficial to improve the overall appearance of clothes. Clothes ironing agents on the market often use cationic surfactants as the main anti-wrinkle ingredient. By forming a thin layer of cationic film on the surface of clothes, it reduces the friction between fibers and reduces the generation of static electricity, thereby effectively reducing the formation of wrinkles. However, the use of antistatic agents can only reduce the generation of wrinkles on clothes, and cannot make clothes achieve a stiff shaping effect.

[0004] As a technical improvement, a patent application with publication number CN102978916A and name "A fabric finishing slurry and its preparation method" adopts hydroxyethyl starch in its technical solution, which can be shaped and film-formed on the fabric surface, so that the fabric has a smooth and stiff effect; however, the inventor found through a large number of experiments that due to the molecular structure characteristics of hydroxyethyl starch, although it can solidify into a film on the fabric surface and have a certain shaping effect, its film hardness is relatively high and it is prone to brittle cracking, so it cannot maintain the smoothness and stiffness of the clothes; on the other hand, for clothes with a high plant fiber content, hydroxyethyl starch itself has viscosity. When applied to the surface of clothing fibers, it will quickly adhere to and deposit on local clothing fibers during the process of high-temperature ironing and solidification into a film, making it difficult to penetrate and evenly spread on the entire clothing fibers, thereby greatly reducing the overall stiffness of the clothing. The shaping effect is also not conducive to construction operations such as spraying and ironing. Summary of the invention

[0005] In order to make the clothes after ironing have the shaping effect of being flat, stiff, soft and not easy to deform, the present application provides a clothes ironing starch aerosol.

[0006] In a first aspect, the present application provides a clothing ironing and starching aerosol, which adopts the following technical solution: A clothing ironing and starching aerosol, comprising the following components in percentage by mass: Hydroxyethyl starch 4-5%; Diquaternary ammonium salt modified dimethylsiloxane 0.18-0.22%; Polyethylene glycol-400 1.7-2.3%; Corrosion inhibitor 0.2-0.3%; Solubilizer 0.14-0.16%; Aromatherapy agent 0.25-0.35%; Propellant 9-11%; The balance is water.

[0007] The conception principle of the present invention is as follows: The inventors have found through research that hydroxyethyl starch is a natural polysaccharide. Although it can solidify into a film on the surface of fabrics and play a certain shaping effect, its film hardness is relatively high and it is easy to crack, and it cannot achieve the effect of making clothes smooth and stiff. On the other hand, hydroxyethyl starch itself has viscosity. When applied to the surface of clothing fibers, it will quickly adhere to and deposit on local clothing fibers during the process of high-temperature ironing and solidification into a film, making it difficult to penetrate and evenly spread on the entire clothing fibers, thereby greatly reducing the overall stiff shaping effect of the clothing. In order to solve the above technical problems, the present invention introduces diquaternary ammonium salt modified dimethyl siloxane to undergo a cross-linking reaction with hydroxyethyl starch, thereby The invention discloses a novel method for modifying the modified hydroxyethyl starch to reduce the hardness of the film. When the aerosol is sprayed on the surface of the clothing and then ironed at high temperature, a soft and tough film can be formed on the surface of the fabric without cracking, thereby maintaining a flat and stiff shaping effect on the clothing. On the other hand, the invention introduces polyethylene glycol-400, which has a lubricating effect, so that the modified hydroxyethyl starch can be uniformly infiltrated and diffused to the entire fabric surface during high-temperature ironing, thereby solving the construction problem that the hydroxyethyl starch is easily deposited locally and difficult to be evenly spread. When in use, the aerosol is sprayed on the surface of the clothing, and then gently ironed back and forth, so that the entire clothing can achieve a shaping effect of being flat, crisp, smooth, and not easy to deform.

[0008] In addition, the hydroxyethyl starch in the formula is a plant ingredient, which is easy to grow mold when sprayed on clothes. The diquaternary ammonium salt modified dimethyl siloxane has bactericidal and mildew-proof effects, which can effectively prevent the hydroxyethyl starch from mold and fungus, thereby improving the safety of the aerosol, and no additional bactericides need to be added to the formula, saving costs. At the same time, the diquaternary ammonium salt modified dimethyl siloxane itself is a cationic antistatic agent, and also has antistatic and anti-wrinkle effects.

[0009] Preferably, the corrosion inhibitor includes one or more of sodium benzoate, sodium tartrate, triethanolamine, and sodium tripolyphosphate.

[0010] By adopting the above technical solution, a corrosion inhibitor is added to the clothing ironing sizing aerosol, and the corrosion inhibitor can form a protective layer between clothing fibers, reduce the friction between the fibers, and enable the clothing structure to maintain a certain integrity.

[0011] Preferably, the corrosion inhibitor is composed of sodium benzoate and triethanolamine in a mass ratio of (1-2):1.

[0012] By adopting the above technical solution and using sodium benzoate and triethanolamine in a specific proportion as corrosion inhibitors, the friction between fibers can be reduced, thereby achieving the effect of maintaining the integrity of the clothing structure; in addition, sodium benzoate and triethanolamine can work together to react with hydroxyl groups and alkaline substances in clothing fibers to form stable ester bonds and salts, so that the clothing remains crisp during the ironing process while having good softness and better wrinkle resistance.

[0013] Preferably, the solubilizer includes one or more of PEG-40 hydrogenated castor oil, polysorbate-20, and polyoxyethylene lauryl ether.

[0014] By adopting the above technical solution and using one or more of the above substances as solubilizers, the solubility and fluidity of each component in the aerosol can be effectively enhanced, so that the aerosol can be more evenly dispersed on the surface of the clothes during ironing, thereby improving the flatness.

[0015] Preferably, the solubilizer is composed of PEG-40 hydrogenated castor oil and polysorbate-20 in a mass ratio of 1:(0.4-0.6).

[0016] By adopting the above technical scheme, using a specific proportion of PEG-40 hydrogenated castor oil and polysorbate-20 as solubilizers, it is beneficial to enhance the fluidity of the aerosol and enable the aerosol to be evenly dispersed on the surface of clothing; at the same time, the molecular structure of PEG-40 hydrogenated castor oil and polysorbate-20 contains a large amount of long-chain fatty acids, which can form a thin film on the surface of clothing, reduce excessive contact between hydroxyethyl starch and clothing fibers, and thus help to further improve the softness of clothing ironing.

[0017] Preferably, the fragrance is essence.

[0018] By adopting the above technical solution, essence is used as a fragrance in the aerosol, which can effectively remove the odor on the clothes and make the ironed clothes have a certain special fragrance.

[0019] Preferably, the propellant includes one or more of propane, propane-butane, butane and isobutane.

[0020] By adopting the above technical solution, using the gas with stable physical and chemical properties and not easy to react with other effective ingredients in the aerosol as a propellant, a certain thrust can be provided for the aerosol without adversely affecting the effectiveness of the components in the aerosol.

[0021] In a second aspect, the present application provides a method for preparing a clothing ironing sizing aerosol, which adopts the following technical scheme: A method for preparing a clothing ironing sizing aerosol, comprising the following steps: S1, adding hydroxyethyl starch, diquaternary ammonium salt modified dimethyl siloxane, polyethylene glycol, corrosion inhibitor, solubilizer, fragrance, and water into a container, stirring evenly to obtain a premix; S2, putting the premix into an aerosol can, and charging the propellant into the aerosol can to obtain the clothes ironing and starching aerosol.

[0022] By adopting the above technical scheme and preparing the clothing ironing and sizing aerosol according to the above steps, it is helpful to prepare the clothing ironing and sizing aerosol with good compatibility and good quality; at the same time, this method is simple to operate, the preparation process is fast, and it is easy to implement on a large scale.

[0023] In summary, this application has the following beneficial effects: 1. Hydroxyethyl starch has a high hardness after film formation, and is prone to brittle cracking, which makes it impossible to make clothes smooth and stiff. In order to solve this problem, the present invention introduces diquaternary ammonium salt modified dimethyl siloxane, which undergoes a cross-linking reaction with hydroxyethyl starch, thereby modifying hydroxyethyl starch and reducing its film hardness. When the aerosol is sprayed on the surface of clothing and ironed at high temperature, a soft and tough film can be formed on the surface of the fabric, and it is not easy to crack, so that the clothing can maintain a smooth and stiff shaping effect. In addition, the hydroxyethyl starch in the formula is a plant ingredient, which is easy to grow mold when sprayed on clothing, and the diquaternary ammonium salt modified dimethyl siloxane has the effect of sterilization and mildew resistance, which can effectively prevent hydroxyethyl starch from growing mold and bacteria, improve the safety of the aerosol, and no additional bactericides need to be added in the formula, saving costs; at the same time, the diquaternary ammonium salt modified dimethyl siloxane itself is a cationic antistatic agent, which also has the effects of antistatic and wrinkle resistance.

[0024] 2. In order to solve the problem that hydroxyethyl starch is difficult to spread evenly and is easy to deposit and adhere to local clothing fibers during high-temperature curing film formation, thereby reducing the overall shaping effect of clothing, the present invention introduces polyethylene glycol-400, so that the modified hydroxyethyl starch can be evenly penetrated and diffused to the entire fabric surface during high-temperature ironing, thereby solving the construction problem that hydroxyethyl starch is easy to be locally deposited and difficult to spread evenly. When in use, the aerosol is sprayed onto the surface of the clothing, and then gently ironed back and forth, and the entire clothing can achieve a shaping effect of being flat, crisp, smooth and not easy to deform.

[0025] 3. By using sodium benzoate and triethanolamine as corrosion inhibitors in a specific proportion, sodium benzoate and triethanolamine can work together to react with hydroxyl groups and alkaline substances in clothing fibers to form stable ester bonds and salts, making the clothes softer and smoother during ironing, that is, maintaining crispness while having good softness and better wrinkle resistance; in addition, by using PEG-40 hydrogenated castor oil and polysorbate-20 as solubilizers in a specific proportion, it is beneficial to enhance the fluidity of the aerosol, so that the aerosol can be evenly dispersed on the surface of the clothing and improve the flatness; at the same time, the molecular structure of PEG-40 hydrogenated castor oil and polysorbate-20 contains a large amount of long-chain fatty acids, which can form a film on the surface of clothing, reduce excessive contact between hydroxyethyl starch and clothing fibers, and thus help to further improve the softness of clothing ironing. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 This is a cotton piece sample picture; Figure 2 This is a cotton piece sample picture; Figure 3 This is a diagram showing the effect of the cotton sheet being stiffened after ironing in Example 3; Figure 4 This is a picture showing the softening effect of the cotton sheet after ironing in Example 3. DETAILED DESCRIPTION

[0027] The present application is further described in detail below with reference to the embodiments.

[0028] The raw materials of the following examples and comparative examples are all commercially available, as follows: Hydroxyethyl starch was purchased from Shanghai Yuanye Biotechnology Co., Ltd.; Diquaternary ammonium salt-modified dimethylsiloxane was purchased from Guangzhou Tuoxin Chemical Technology Co., Ltd., model number REWOQUATSQ 1; CAS number of corn starch is 2567-51-3; Polyquaternium-7 was purchased from Shandong Xinquansheng Chemical Technology Co., Ltd., model M550; The CAS number of fatty alcohol polyoxyethylene ether AEO9 is 68213-23-0; The CAS number of polyethylene glycol-400 is 25322-68-3; The CAS number of sodium benzoate is 532-32-1; The CAS number of triethanolamine is 102-71-6; The CAS number of polysorbate-20 is 9005-64-5; The CAS number of triethanolamine is 527-07-1; The CAS number of sodium tartrate is 6106-24-7; The CAS number of PEG-40 hydrogenated castor oil is 61788-85-0.

[0029] Example 1 A clothes ironing and starching aerosol, comprising the following components: Hydroxyethyl starch 4g; diquaternary ammonium salt modified dimethyl siloxane 0.18g; polyethylene glycol-400 1.7g; corrosion inhibitor 0.2g; solubilizer 0.14g; fragrance 0.25g; propellant 9g; water 84.53g.

[0030] The corrosion inhibitor is a mixture of 1g sodium benzoate and 1g triethanolamine; the solubilizer is a mixture of 1g PEG-40 hydrogenated castor oil and 0.4g polysorbate-20; the fragrance is essence; and the propellant is propane-butane.

[0031] A method for preparing a clothes ironing and starching aerosol, which is specifically as follows: S1, adding hydroxyethyl starch, diquaternary ammonium salt modified dimethyl siloxane, polyethylene glycol, corrosion inhibitor, solubilizer, fragrance, and water into a stirrer, and stirring at a speed of 100 r / min for 20 minutes to obtain a premix; S2, putting the premix into an aerosol can, and charging the propellant into the aerosol can to obtain the clothes ironing and starching aerosol.

[0032] Example 2 A clothes ironing and starching aerosol, comprising the following components: 5g hydroxyethyl starch; 0.22g diquaternary ammonium salt modified dimethylsiloxane; 2.3g polyethylene glycol-400; 0.3g corrosion inhibitor; 0.16g solubilizer; 0.35g fragrance; 11g propellant; 80.67g water.

[0033] The corrosion inhibitor is a mixture of 2g sodium benzoate and 1g triethanolamine; the solubilizer is a mixture of 1g PEG-40 hydrogenated castor oil and 0.6g polysorbate-20; the fragrance is essence; and the propellant is propane-butane.

[0034] A method for preparing a clothes ironing and starching aerosol, which is specifically as follows: S1, adding hydroxyethyl starch, diquaternary ammonium salt modified dimethyl siloxane, polyethylene glycol, corrosion inhibitor, solubilizer, fragrance, and water into a stirrer, and stirring at a speed of 100 r / min for 20 minutes to obtain a premix; S2, putting the premix into an aerosol can, and charging the propellant into the aerosol can to obtain the clothes ironing and starching aerosol.

[0035] Example 3 A clothes ironing and starching aerosol, comprising the following components: 4.5g hydroxyethyl starch; 0.2g diquaternary ammonium salt modified dimethylsiloxane; 2.0g polyethylene glycol-400; 0.25g corrosion inhibitor; 0.15g solubilizer; 0.3g fragrance; 10g propellant; 82.6g water.

[0036] The corrosion inhibitor is a mixture of 1.5 g sodium benzoate and 1 g triethanolamine; the solubilizer is a mixture of 1 g PEG-40 hydrogenated castor oil and 0.5 g polysorbate-20; the fragrance is essence; and the propellant is propane-butane.

[0037] A method for preparing a clothes ironing and starching aerosol, which is specifically as follows: S1, adding hydroxyethyl starch, diquaternary ammonium salt modified dimethyl siloxane, polyethylene glycol, corrosion inhibitor, solubilizer, fragrance, and water into a stirrer, stirring at a speed of 100 r / min for 20 minutes to obtain a premix; S2, putting the premix into an aerosol can, and charging the propellant into the aerosol can to obtain the clothes ironing and starching aerosol.

[0038] Example 4 The difference from Example 3 is that sodium benzoate is replaced by an equal amount of sodium tartrate.

[0039] Example 5 The difference from Example 3 is that triethanolamine is replaced by an equal amount of sodium tartrate.

[0040] Example 6 The difference from Example 3 is that an equal amount of lauryl alcohol polyoxyethylene ether is used to replace PEG-40 hydrogenated castor oil.

[0041] Example 7 The difference from Example 3 is that an equal amount of lauryl alcohol polyoxyethylene ether is used to replace polysorbate-20.

[0042] Comparative Example 1 The difference from Example 3 is that the diquaternary ammonium salt-modified dimethyl siloxane and polyethylene glycol-400 are not contained, and the reduced amount is replaced by an equal amount of water.

[0043] Comparative Example 2 The difference from Example 3 is that the diquaternary ammonium salt-modified dimethylsiloxane is replaced by an equal amount of polyquaternium-7.

[0044] Comparative Example 3 The difference from Example 3 is that an equal amount of fatty alcohol polyoxyethylene ether AEO9 is used to replace polyethylene glycol-400.

[0045] Experiment 1: Flatness Test The cotton cloth was cut into a cotton sheet with a length and width of 15*20 cm respectively, folded in half 4 times, and lightly tied with a rubber band for 30 minutes to make obvious creases appear on the cotton sheet to obtain a cotton sheet sample; the clothing ironing sizing aerosol prepared in the above embodiments and comparative examples was sprayed once on the diagonal center of the cotton sheet sample, and ironed 2 times from the spraying point to each of the four sides using a household ironing machine, and the cotton sheet was cooled to room temperature to obtain the ironed cotton sheet. The change in the flatness of the cotton sheet surface within 3 minutes was observed and recorded to judge the overall shaping effect of the cotton sheet, and the recorded results are shown in Table 1.

[0046] Experiment 2: Aerosol dispersion performance test (1) Cut the cotton cloth into a cotton sheet with a length and width of 15*20 cm respectively, fold it in half 4 times, and then lightly tie it with a rubber band for 30 minutes to make obvious creases appear on the cotton sheet to obtain a cotton sheet sample; spray the clothing ironing sizing aerosol prepared in the above embodiments and comparative examples once on the diagonal center of the cotton sheet sample, and use a household ironing machine to iron the cotton sheet twice from the spraying point to each of the four sides in sequence, and wait for the cotton sheet to cool to room temperature to obtain the ironed cotton sheet. After spraying the aerosol, observe whether the aerosol is deposited during the high-temperature ironing process to judge the dispersion performance of the aerosol, and record the results in Table 1; Experiment 3: Smoothness test Take the ironed cotton sheet of Experiment 1 and fold it twice naturally, and press it lightly to make the folded parts of the cotton sheet fit together. After 30 seconds, unfold the cotton sheet and observe whether there are creases on the cotton sheet and the clarity of the creases. Use this to judge the softness of the cotton sheet. The clearer the creases, the lower the softness and the lower the wrinkle resistance. The recorded results are shown in Table 1.

[0047] Table 1 According to the data comparison of Example 3 and Comparative Examples 1-3 in Table 1, it can be obtained that the cotton sheet of Example 3 is flat and crisp without obvious wrinkles. This is because in addition to hydroxyethyl starch as a setting agent, the aerosol also contains diquaternary ammonium salt-modified dimethyl siloxane as a modifier of hydroxyethyl starch, and polyethylene glycol-400 as an auxiliary ironing agent, which not only solves the problem of brittle cracking of hydroxyethyl starch film formation, but also avoids the construction problem of hydroxyethyl starch being easily deposited locally and difficult to spread evenly, thereby maintaining the setting effect of the clothes being flat, crisp and not easy to deform.

[0048] Comparative Example 1 contains hydroxyethyl starch, but does not use diquaternary ammonium salt-modified dimethyl siloxane and polyethylene glycol-400. Although the prepared aerosol can solidify into a film on the surface of the fabric and play a certain shaping effect, the hydroxyethyl starch film has a high hardness and is prone to brittle cracking. Therefore, the cotton sheet is flat after initial ironing, but the maintenance time is short. Obvious wrinkles appear again within 3 minutes, and the hardness is uneven. Some areas collapse. After folding in half, slight creases appear in the collapsed area, so the clothes cannot maintain the flat and stiff effect. On the other hand, hydroxyethyl starch itself has viscosity. After high-temperature ironing and curing into a film, it will quickly adhere to and deposit on local clothing fibers. It is difficult to penetrate and evenly spread on the entire clothing fiber. Therefore, Comparative Example 1 shows that the aerosol is locally deposited after spraying and is difficult to spread.

[0049] In Comparative Example 2, an equal amount of polyquaternium-7 was used to replace the diquaternary ammonium salt-modified dimethyl siloxane. The flatness test result was the same as that of Comparative Example 1, but no deposition occurred after ironing after the aerosol was sprayed. This shows that although the diquaternary ammonium salt-modified dimethyl siloxane is a cationic antistatic agent, it can react with hydroxyethyl starch by cross-linking when applied to the aerosol, thereby improving the film hardness of the hydroxyethyl starch and preventing it from being easily brittle. Therefore, other cationic quaternary ammonium salts cannot be used as modifiers for hydroxyethyl starch, and the shaping effect of keeping the clothes flat and stiff cannot be achieved.

[0050] Comparative Example 3: An equal amount of fatty alcohol polyoxyethylene ether AEO9 was used to replace polyethylene glycol-400. After spraying with aerosol, ironing was performed, and local deposition was observed, which was difficult to spread. However, the cotton sheet after ironing was uneven in hardness and softness, and some areas collapsed without obvious wrinkles. This indicates that the lack of polyethylene glycol-400 as an auxiliary ironing agent will cause hydroxyethyl starch to adhere to local clothing fibers during the high-temperature curing film formation process, making it difficult to spread evenly, thereby reducing the overall shaping effect of the clothing.

[0051] On the other hand, according to the softness test results, by comparing the data of Example 3 and Examples 4-5 in Table 1, it can be obtained that by using a specific ratio of sodium benzoate and triethanolamine as corrosion inhibitors, they can react with hydroxyl groups and alkaline substances in clothing fibers to form stable ester bonds and salts, making the clothes softer and smoother during the ironing process, that is, they remain crisp while having good softness and better wrinkle resistance.

[0052] According to the data comparison between Example 3 and Examples 6-7 in Table 1, it can be obtained that by using a specific ratio of PEG-40 hydrogenated castor oil and polysorbate-20 as a solubilizer, on the one hand, it is beneficial to enhance the fluidity of the aerosol and make it more evenly dispersed on the surface of clothing; on the other hand, the molecular structure of PEG-40 hydrogenated castor oil and polysorbate-20 contains a large amount of long-chain fatty acids, which can form a film on the surface of clothing, reduce excessive contact between hydroxyethyl starch and clothing fibers, and thus help to further improve the softness of clothing.

[0053] This specific embodiment is merely an explanation of the present application and is not a limitation of the present application. After reading this specification, those skilled in the art may make modifications to the present embodiment without any creative contribution as needed, but such modifications are protected by the patent law as long as they are within the scope of the claims of the present application.

Claims

1. A clothing ironing and starching aerosol, characterized in that: The following components are included in mass percentage: Hydroxyethyl starch 4-5%; Diquaternary ammonium salt modified dimethylsiloxane 0.18-0.22%; Polyethylene glycol-400 1.7-2.3%; Corrosion inhibitor 0.2-0.3%; Solubilizer 0.14-0.16%; Aromatherapy agent 0.25-0.35%; Propellant 9-11%; The balance is water.

2. The clothing ironing and starching aerosol according to claim 1, characterized in that: The corrosion inhibitor includes one or more of sodium benzoate, sodium tartrate, triethanolamine and sodium tripolyphosphate.

3. The clothing ironing and starching aerosol according to claim 2, characterized in that: The corrosion inhibitor is composed of sodium benzoate and triethanolamine in a mass ratio of (1-2):

1.

4. The clothing ironing and starching aerosol according to claim 1, characterized in that: The solubilizing agent includes one or more of PEG-40 hydrogenated castor oil, polysorbate-20, and lauryl alcohol polyoxyethylene ether.

5. The clothing ironing and starching aerosol according to claim 4, characterized in that: The solubilizer is composed of PEG-40 hydrogenated castor oil and polysorbate-20 in a mass ratio of 1:(0.4-0.6).

6. The clothing ironing and starching aerosol according to claim 1, characterized in that: The aromatic agent is essence.

7. The clothing ironing and starching aerosol according to claim 1, characterized in that: The propellant includes one or more of propane, propane-butane, butane and isobutane.

8. A method for preparing a clothing ironing sizing aerosol according to any one of claims 1 to 7, characterized in that: The following steps are involved: S1, adding hydroxyethyl starch, diquaternary ammonium salt modified dimethyl siloxane, polyethylene glycol, corrosion inhibitor, solubilizer, fragrance, and water into a container, stirring evenly to obtain a premix; S2, putting the premix into an aerosol can, and charging the propellant into the aerosol can to obtain the clothes ironing and starching aerosol.

Citation Information

Patent Citations

  • Fabric finishing pulp and preparation method thereof

    CN102978916A