Gallium nitride vertical JFET (Junction Field Effect Transistor) device with multi-layer channel and fall type super junction
By adopting a multi-layer channel and drop superjunction structure in gallium nitride vertical JFET devices, the problem that traditional devices cannot obtain high threshold voltage and large forward current at the same time is solved, and high-performance high threshold voltage and large forward current are achieved. and high pressure resistance effect.
Patent Information
- Application Number
- CN202411051783.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-01
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2044-08-01
AI Technical Summary
Traditional vertical GaN transistors cannot obtain both high threshold voltage and large forward current, limiting their performance in medium voltage and high power applications.
GaN vertical JFET device structure using multi-layer channel and drop type superjunction, by introducing drop type N-type GaN drift region and drop type P-type low-doping region into the superjunction, the doping concentration decreases from bottom to top and incrementally, a conductive region with high doping concentration is formed, and ultra-low doping and heavily doping regions are introduced in the channel region to improve carrier concentration and electric field uniformity.
It effectively improves the device's withstand voltage, on-resistance and breakdown voltage, improves the power quality factor, and makes the device safer and more reliable under extreme conditions, while meeting the requirements of high threshold voltage, large forward current and high withstand voltage.
Smart Images

Figure CN118983346A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the field of semiconductor technology, and in particular relates to a gallium nitride vertical JFET device with a multi-layer channel and a step-type super junction. Background Art
[0002] Today, lateral GaN HEMT devices are developing rapidly and maturing in RF and low-voltage power devices. Enhanced GaN HEMT based on p-GaN cap layer and enhanced GaN HEMT based on cascade structure are gradually being applied. The current commercial GaN HEMT withstand voltage level is usually below 650V, and it has advantages in switching speed in medium and low voltage applications. However, if the withstand voltage level needs to be further improved, vertical GaN will become a new focus, especially homoepitaxial GaN vertical power devices based on GaN bulk material substrates, which will become the future development direction of high voltage and high current.
[0003] Compared with lateral GaN HEMT, vertical GaN devices have the following advantages: (1) For a given chip area, they have higher breakdown voltage and current capability; (2) The electric field peak of vertical GaN devices can be transferred from the surface to the drift region, which can suppress the occurrence of surface breakdown; (3) By using GaN homoepitaxial growth, the thermal mismatch ratio between the substrate and the drift region is reduced, which is beneficial to power dissipation; (4) Since it is less dependent on surface passivation, the dynamic on-resistance is relatively stable; (5) The defect density in the homoepitaxial layer is reduced. These advantages make vertical GaN devices particularly suitable for medium voltage (600-10kV) and high power scenarios.
[0004] So far, several 1.2kV-class vertical GaN transistors have been prepared based on GaN substrates, such as: current aperture vertical electron transistor (CAVFET), junction field effect transistor (JFET), trench MOSFET and fin channel MOSFET. In the conventional structure of junction field effect transistor, since the threshold voltage and forward current are both related to the channel n-type impurity concentration, when the channel n-type impurity concentration is high, the threshold voltage is low and the forward current is large, and when the channel n-type impurity concentration is low, the threshold voltage is high and the forward current is low. In other words, the traditional vertical GaN transistor cannot obtain high threshold voltage and large forward current at the same time. Summary of the invention
[0005] In order to solve the above problems existing in the prior art, the present invention provides a gallium nitride vertical JFET device with multi-layer channels and stepped super junction. The technical problem to be solved by the present invention is achieved through the following technical solutions:
[0006] In a first aspect, the present invention provides a gallium nitride vertical JFET device with a multi-layer channel and a step-type super junction, comprising:
[0007] N++GaN substrate;
[0008] A GaN drift layer located on a surface of one side of the N++GaN substrate;
[0009] A super junction located on the surface of the GaN drift layer away from the N++GaN substrate; the super junction comprises a stepped N-type GaN drift region and a stepped P-type low-doping region, the doping concentration of the stepped N-type GaN drift region decreases from bottom to top, and the doping concentration of the stepped P-type low-doping region increases from bottom to top;
[0010] A channel region, a first P+GaN region and a second P+GaN region located on a surface of the superjunction away from the N++GaN substrate, wherein the first P+GaN region and the second P+GaN region are located on both sides of the channel region respectively;
[0011] A first gate, a source, and a second gate are respectively located on the first P+GaN region, the channel region, and the second P+GaN region on the side away from the N++GaN substrate; the channel region includes at least one layer of N--GaN region located on the side of the stepped N-type GaN drift region away from the N++GaN substrate, and at least one layer of N++GaN region located on the side of the source electrode close to the N++GaN substrate;
[0012] a passivation layer located between the first gate and the source and between the second gate and the source;
[0013] A drain electrode is located on the surface of the N++GaN substrate away from the GaN drift layer.
[0014] In one embodiment of the present invention, the stepped P-type low-doped region includes: a first P-type low-doped region and a second P-type low-doped region respectively located on both sides of the stepped N-type GaN drift region; wherein the doping concentrations of the first P-type low-doped region and the second P-type low-doped region both increase from bottom to top.
[0015] In one embodiment of the present invention, the doping concentration of the stepped N-type GaN drift region and the stepped P-type low-doping region is 0.7×10 16 ~1.1×10 18 cm -3 .
[0016] In one embodiment of the present invention, the stepped N-type GaN drift region includes three layers of N-type GaN drift regions, and the first P-type low-doped region and the second P-type low-doped region both include three layers of P-type low-doped regions, wherein the doping concentration of the same layer of P-type low-doped regions in the first P-type low-doped region and the second P-type low-doped region is the same.
[0017] In one embodiment of the present invention, in the channel region, at least one N-GaN region is included between the N--GaN region and the N++GaN region.
[0018] In one embodiment of the present invention, the doping concentration of at least one N--GaN region located on the surface of the stepped N-type GaN drift region away from the N++GaN substrate is 0.5×10 15 ~1×10 17 cm -3 The doping concentration of at least one N++GaN region located on the surface of the source electrode close to the N++GaN substrate side is 1×10 18 ~5×10 19 cm -3 .
[0019] In one embodiment of the present invention, the doping concentration of at least one N-GaN region between the N--GaN region and the N++GaN region is 3×10 17 ~5×10 19 cm -3 .
[0020] In a second aspect, the present invention provides a method for preparing a gallium nitride vertical JFET device having a multi-layer channel and a step-type super junction, comprising:
[0021] Providing an N++GaN substrate;
[0022] Depositing a GaN drift layer on one side surface of the N++GaN substrate;
[0023] A super junction consisting of a stepped N-type GaN drift region and a stepped P-type low-doped region is grown on the surface of the GaN drift layer away from the N++GaN substrate, wherein the doping concentration of the stepped N-type GaN drift region decreases from bottom to top, and the doping concentration of the stepped P-type low-doped region increases from bottom to top;
[0024] A channel region is grown on the surface of the super junction away from the N++GaN substrate, and after etching the first preset regions at both ends of the channel region, a first P+GaN region and a second P+GaN region are grown in the first preset regions at both ends of the channel region respectively;
[0025] Thinning the N++GaN substrate and forming a drain electrode on the surface thereof away from the GaN drift layer;
[0026] A source electrode is fabricated on a surface of the channel region on a side away from the N++GaN substrate, and a first gate electrode and a second gate electrode are fabricated on surfaces of the first P+GaN region and the second P+GaN region on a side away from the N++GaN substrate, respectively; wherein the channel region includes at least one layer of N--GaN region located on a surface of the stepped N-type GaN drift region on a side away from the N++GaN substrate, and at least one layer of N++GaN region located on a surface of the source electrode on a side close to the N++GaN substrate;
[0027] After a passivation layer is deposited on the surfaces of the first P+GaN region, the second P+GaN region, the first gate, the second gate and the source, holes are opened in the passivation layer on the surfaces of the source, the first gate and the second gate to lead out electrodes.
[0028] In one embodiment of the present invention, the step of growing a super junction consisting of a stepped N-type GaN drift region and a stepped P-type low-doped region on the surface of the GaN drift layer away from the N++GaN substrate comprises:
[0029] Growing multiple layers of N-type GaN drift regions in sequence on a surface of the GaN drift layer away from the N++GaN substrate, wherein the doping concentration of the multiple layers of N-type GaN drift regions decreases from bottom to top;
[0030] Etching the multi-layer N-type GaN drift region to remove the multi-layer N-type GaN drift region in the second preset regions at both ends to form a stepped N-type GaN drift region;
[0031] Multiple layers of P-type low-doped regions are sequentially grown in the second preset areas at both ends to form a stepped P-type low-doped region including a first P-type low-doped region and a second P-type low-doped region; the doping concentrations of the first P-type low-doped region and the second P-type low-doped region increase from bottom to top, and the doping concentrations of the same layer of P-type low-doped regions in the first P-type low-doped region and the second P-type low-doped region are the same.
[0032] In one embodiment of the present invention, after growing a channel region on the surface of the super junction away from the N++GaN substrate and etching the first preset regions at both ends of the channel region, the steps of growing a first P+GaN region and a second P+GaN region in the first preset regions at both ends of the channel region respectively include:
[0033] Growing a plurality of N-type GaN regions in sequence on a surface of the superjunction away from the N++GaN substrate to form a channel region;
[0034] The channel region is etched to remove a plurality of N-type GaN regions in the second preset regions at both ends of the channel region, and then a first P+GaN region and a second P+GaN region are grown in the second preset regions at both ends of the channel region respectively.
[0035] Compared with the prior art, the present invention has the following beneficial effects:
[0036] The present invention provides a gallium nitride vertical JFET device with a multi-layer channel and a step-type super junction and a preparation method thereof. The device comprises: an N++GaN substrate; a GaN drift layer located on one side surface of the N++GaN substrate; a super junction located on the side surface of the GaN drift layer away from the N++GaN substrate; a channel region, a first P+GaN region and a second P+GaN region located on the side surface of the super junction away from the N++GaN substrate, the first P+GaN region and the second P+GaN region being located on both sides of the channel region respectively; a first gate, a source electrode and a second gate electrode respectively located on the side surface of the first P+GaN region, the channel region and the second P+GaN region away from the N++GaN substrate; a passivation layer located between the first gate electrode and the source electrode and between the second gate electrode and the source electrode; and a drain electrode located on the side surface of the N++GaN substrate away from the GaN drift layer. On the one hand, since the doping concentration of the stepped N-type GaN drift region decreases from bottom to top, and the doping concentration of the stepped P-type low-doped region increases from bottom to top in the superjunction, this stepped superjunction can effectively alleviate the peak electric field at the contact position between the P-type region and the N-type drift region, and improve the device withstand voltage. Compared with the prior art, the present invention replaces the traditional drift region with a superjunction with a high doping concentration, which can increase the carrier concentration in the conductive region and reduce power loss. The forward characteristics (reduced on-resistance) and reverse characteristics (increased breakdown voltage) of the JFET device are also improved, and the power quality factor is significantly improved. In addition, making a stepped superjunction below the P-type region is conducive to improving the avalanche capability of the device, making the device safer and more reliable under extreme conditions.
[0037] On the other hand, the device channel region includes at least one N--GaN region located on the surface of the side of the stepped N-type GaN drift region away from the N++GaN substrate, and at least one N++GaN region located on the surface of the side of the source electrode close to the N++GaN substrate. By introducing ultra-low doping (N--GaN region) in the channel region, the threshold voltage of the device can be significantly improved. At the same time, the forward current is increased by increasing the doping concentration of the upper layer of the channel region (N++GaN region). The electric field voltage divider formed by the super junction makes the electric field uniformly distributed in the drift region, which is beneficial to reducing the electric field strength in the contact area between the P-type region and the N-type drift region, thereby obtaining a GaN vertical JFET that simultaneously meets high threshold voltage, large forward current and high withstand voltage.
[0038] The present invention will be further described in detail below with reference to the accompanying drawings and embodiments. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] Figure 1 It is a structural schematic diagram of a gallium nitride vertical JFET device with multi-layer channels and stepped super junction provided by an embodiment of the present invention;
[0040] Figure 2 It is a schematic flow chart of a method for preparing a gallium nitride vertical JFET device with multi-layer channels and stepped super junction provided by an embodiment of the present invention;
[0041] Figures 3a to 3j It is a schematic diagram of the preparation process of a gallium nitride vertical JFET device with multi-layer channels and stepped super junction provided by an embodiment of the present invention;
[0042] Figure 4 The transfer curves of a conventional JFET device and a GaN vertical JFET device with multi-layer channels and stepped superjunction are shown in Figure 2.
[0043] Figure 5 It is a transfer curve diagram of a conventional JFET device and a GaN vertical JFET device with multi-layer channels and stepped super junction in semi-logarithmic coordinates;
[0044] Figure 6 This is the superjunction electric field distribution diagram of a conventional JFET device;
[0045] Figure 7 This is the superjunction electric field distribution diagram of a GaN vertical JFET device with multi-layer channels and stepped superjunction;
[0046] Figure 8 This is a comparison chart of the breakdown voltage of a conventional JFET device and a GaN vertical JFET device with a multi-layer channel and a stepped superjunction. DETAILED DESCRIPTION
[0047] The present invention is further described in detail below with reference to specific embodiments, but the embodiments of the present invention are not limited thereto.
[0048] Figure 1 Schematic diagram of a structure of a gallium nitride vertical JFET device with multi-layer channels and step-type super junction provided by an embodiment of the present invention. Figure 1 The embodiment of the present invention provides a gallium nitride vertical JFET device with a multi-layer channel and a step-type super junction, comprising:
[0049] N++GaN substrate;
[0050] A GaN drift layer located on a surface of one side of an N++GaN substrate;
[0051] A superjunction located on the surface of the GaN drift layer away from the N++GaN substrate; the superjunction includes a stepped N-type GaN drift region and a stepped P-type low-doped region, the doping concentration of the stepped N-type GaN drift region decreases from bottom to top, and the doping concentration of the stepped P-type low-doped region increases from bottom to top;
[0052] A channel region, a first P+GaN region and a second P+GaN region located on a surface of a side of the superjunction away from the N++GaN substrate, wherein the first P+GaN region and the second P+GaN region are located on both sides of the channel region respectively;
[0053] A first gate, a source and a second gate are respectively located on the first P+GaN region, the channel region and the second P+GaN region on the side away from the N++GaN substrate; the channel region includes at least one layer of N--GaN region located on the side of the stepped N-type GaN drift region away from the N++GaN substrate, and at least one layer of N++GaN region located on the side of the source electrode close to the N++GaN substrate;
[0054] a passivation layer between the first gate and the source and between the second gate and the source;
[0055] The drain is located on the surface of the N++GaN substrate away from the GaN drift layer.
[0056] Specifically, in the above-mentioned GaN vertical JFET device, the surface of the N++GaN substrate away from the drain side includes a superjunction, and the superjunction structure is composed of a stepped N-type GaN drift region and a stepped P-type low-doped region. Here, "step-type" means that the doping concentration shows a changing trend from bottom to top, wherein the doping concentration of the stepped N-type GaN drift region decreases from bottom to top, and the doping concentration of the stepped P-type low-doped region increases from bottom to top. This step-type superjunction can effectively alleviate the peak electric field at the contact position between the P-type region and the N-type drift region, thereby improving the device's withstand voltage.
[0057] The surface of the super junction away from the N++GaN substrate includes a channel region, a first P+GaN region and a second P+GaN region. Figure 1 From the perspective shown, the first P+GaN region and the second P+GaN region are located on the left and right sides of the channel region, respectively. The channel region includes at least one N--GaN region at the bottom and at least one N++GaN region at the top. It should be understood that for a GaN vertical JFET device, when its gate is zero volts, because the electrons in the N-type region in the channel are one order of magnitude lower than the holes in the P-type region, the electrons in the N-type region will be depleted by the holes in the P-type region, resulting in a space charge region, and the space charge region in the N-type region is large. The two P-type regions will deplete the entire N-type region channel, preventing the drain current from flowing to the source. When the gate voltage of the GaN vertical JFET device is greater than the threshold voltage, the space charge region in the N-type region decreases and the drain current flows to the source. Since both the threshold voltage and the forward current are related to the N-type doping concentration of the channel, in a conventional JFET device, when the concentration of the N-type impurities is high, the forward current is large but the threshold voltage is low; similarly, when the concentration of the N-type impurities is low, the threshold voltage is high but the forward current is small.
[0058] This embodiment significantly improves the threshold voltage of the device by introducing ultra-low doping (N--GaN region) in the channel region, and also increases the forward current by increasing the doping concentration of the upper layer of the channel region (N++GaN region). The electric field voltage divider formed by the super junction makes the electric field uniformly distributed in the drift region, which is beneficial to reducing the electric field strength in the contact area between the P-type region and the N-type drift region, thereby obtaining a GaN vertical JFET that simultaneously meets the requirements of high threshold voltage, large forward current and high withstand voltage.
[0059] Optionally, the stepped P-type low-doped region includes: a first P-type low-doped region and a second P-type low-doped region respectively located on both sides of the stepped N-type GaN drift region; wherein the doping concentrations of the first P-type low-doped region and the second P-type low-doped region both increase from bottom to top. In this embodiment, the doping concentrations of the stepped N-type GaN drift region and the stepped P-type low-doped region are 0.7×10 16 ~1.1×10 18 cm -3 .
[0060] It should be noted that in this embodiment, both the stepped N-type GaN drift region and the stepped P-type low-doping region have a three-layer structure. Figure 1 , the stepped N-type GaN drift region includes three layers of N-type GaN drift regions, and the first P-type low-doped region and the second P-type low-doped region both include three layers of P-type low-doped regions, wherein the doping concentrations of the same layer of P-type low-doped regions in the first P-type low-doped region and the second P-type low-doped region are the same. Of course, in some other embodiments of the present application, the stepped N-type GaN drift region and the stepped P-type low-doped region may also be structures of four layers, five layers, etc., as long as the doping concentrations of each layer of N-type GaN drift region in the stepped N-type GaN drift region decrease from bottom to top, and the doping concentrations of each layer of P-type low-doped region in the stepped P-type low-doped region increase from bottom to top, and the present invention does not limit this.
[0061] Furthermore, in the channel region, at least one N-GaN region is included between the N--GaN region and the N++GaN region.
[0062] Specifically, the channel region includes multiple N-type GaN regions from bottom to top. Figure 1 From the perspective shown, the N-type GaN region located at the bottom of the channel region is the N--GaN region, i.e., N-type ultra-low doping, and the N-type GaN region located at the top of the channel region is the N++GaN region, i.e., N-type heavily doping, and there is at least one N-type GaN region between the two, which is the N-GaN region, i.e., N-type low doping. Figure 1In the figure, only the bottom N--GaN region and the top N++GaN region are illustrated in the channel region. In fact, this embodiment has no restriction on the number of layers of N--GaN region, N-GaN region and N++GaN region. That is to say, the channel region can include several layers of N--GaN region, several layers of N-GaN region and several layers of N++GaN region from bottom to top, as long as it shows a trend of ultra-low doping - low doping - heavy doping from bottom to top.
[0063] For example, the doping concentration of at least one N--GaN region located on the surface of the stepped N-type GaN drift region away from the N++GaN substrate is 0.5×10 15 ~1×10 17 cm -3 The doping concentration of at least one N++GaN region located on the surface of the source electrode close to the N++GaN substrate is 1×10 18 ~5×10 19 cm -3 , and the doping concentration of at least one N-GaN region between the N--GaN region and the N++GaN region is 3×10 17 ~5×10 19 cm -3 .
[0064] Figure 2 It is a schematic flow chart of a method for preparing a gallium nitride vertical JFET device with multi-layer channels and step-type super junction provided by an embodiment of the present invention. Figures 3a to 3j FIG. 1 is a schematic diagram of the preparation process of a gallium nitride vertical JFET device with multi-layer channels and stepped super junction provided by an embodiment of the present invention. Figure 2 and Figures 3a to 3j The embodiment of the present invention further provides a method for preparing a gallium nitride vertical JFET device having a multi-layer channel and a step-type super junction, comprising:
[0065] S1. Provide an N++GaN substrate;
[0066] S2, depositing a GaN drift layer on one side surface of the N++GaN substrate;
[0067] S3, growing a super junction consisting of a stepped N-type GaN drift region and a stepped P-type low-doped region on the surface of the GaN drift layer away from the N++GaN substrate, wherein the doping concentration of the stepped N-type GaN drift region decreases from bottom to top, and the doping concentration of the stepped P-type low-doped region increases from bottom to top;
[0068] S4, growing a channel region on the surface of the super junction away from the N++GaN substrate, and etching the first preset regions at both ends of the channel region, and then growing a first P+GaN region and a second P+GaN region in the first preset regions at both ends of the channel region respectively;
[0069] S5, thinning the N++GaN substrate, and forming a drain on the surface thereof away from the GaN drift layer;
[0070] S6. A source electrode is fabricated on a surface of a side of the channel region away from the N++GaN substrate, and a first gate electrode and a second gate electrode are fabricated on surfaces of a first P+GaN region and a second P+GaN region away from the N++GaN substrate, respectively; wherein the channel region includes at least one layer of N--GaN region located on a surface of a side of the stepped N-type GaN drift region away from the N++GaN substrate, and at least one layer of N++GaN region located on a surface of a side of the source electrode close to the N++GaN substrate;
[0071] S7. After a passivation layer is deposited on the surfaces of the first P+GaN region, the second P+GaN region, the first gate, the second gate and the source, holes are opened in the passivation layer on the surfaces of the source, the first gate and the second gate to lead out electrodes.
[0072] Specifically, Figure 3a-3b As shown, in steps S1 to S2, the N++GaN substrate is firstly ultrasonically cleaned to eliminate dangling bonds on the surface, then blow-dried and heat-treated, and then a GaN drift layer with a thickness of 1 μm to 3 μm is deposited on the surface of the N++GaN substrate using a metal organic chemical vapor deposition (MOCVD) process.
[0073] Optionally, in step S3, the step of growing a super junction consisting of a stepped N-type GaN drift region and a stepped P-type low-doped region on the surface of the GaN drift layer away from the N++GaN substrate includes:
[0074] Multilayers of N-type GaN drift regions are sequentially grown on the surface of the GaN drift layer away from the N++GaN substrate, and the doping concentration of the multilayer N-type GaN drift regions decreases from bottom to top;
[0075] Etching the multi-layer N-type GaN drift region to remove the multi-layer N-type GaN drift region in the second preset regions at both ends to form a stepped N-type GaN drift region;
[0076] Multiple layers of P-type low-doped regions are sequentially grown in the second preset areas at both ends to form a stepped P-type low-doped region including a first P-type low-doped region and a second P-type low-doped region; the doping concentrations of the first P-type low-doped region and the second P-type low-doped region increase from bottom to top, and the doping concentrations of the same layer of P-type low-doped regions in the first P-type low-doped region and the second P-type low-doped region are the same.
[0077] In this step, multiple layers of N-type GaN drift regions with a thickness of 2 μm are sequentially grown on the surface of the GaN drift layer. The doping concentration of the multiple layers of N-type GaN drift regions is 0.7×10 16 ~1.1×10 18 cm -3 And it decreases from the lower layer to the upper layer, and we get Figure 3c The epitaxial wafer shown.
[0078] Furthermore, if Figure 3d~3e As shown, the obtained epitaxial wafer is ultrasonically cleaned in acetone for 2 minutes to remove the organic matter remaining on the surface, and then ultrasonically cleaned in ethanol for 3 minutes, and the residual acetone and ethanol are washed away with deionized water, and then dried with N2; after coating, photolithography is performed by inductively coupled plasma etching (ICP), and Cl2 / N2 / O2 mixed gas is introduced to etch and remove the multi-layer N-type GaN drift region in the second preset area at both ends of the epitaxial wafer, and then a metal organic chemical vapor deposition (MOCVD) process is used to sequentially grow a multi-layer P-type low-doping region with a thickness of 2 μm in the second preset area at both ends to form a first P-type low-doping region and a second P-type low-doping region. Optionally, in the first P-type low-doping region and the second P-type low-doping region, the doping concentration increases from the lower layer to the upper layer, and the doping concentration is 0.7×10 16 ~1.1×10 18 cm -3 .
[0079] In step S4, a channel region is grown on the surface of the super junction away from the N++GaN substrate, and after etching the first preset regions at both ends of the channel region, a first P+GaN region and a second P+GaN region are grown in the first preset regions at both ends of the channel region, respectively, including:
[0080] Growing multiple N-type GaN regions in sequence on the surface of the superjunction away from the N++GaN substrate to form a channel region;
[0081] The channel region is etched to remove a plurality of N-type GaN regions in the second preset regions at both ends of the channel region, and then a first P+GaN region and a second P+GaN region are grown in the second preset regions at both ends of the channel region respectively.
[0082] Specifically, if Figure 3f As shown, a metal organic chemical vapor deposition (MOCVD) process is used to grow a channel region with a thickness of 1 μm to 3 μm on the surface of the super junction, wherein the channel region includes at least one N--GaN region below, at least one N++GaN region above, and at least one N-GaN region between the two. Optionally, the doping concentration of the N--GaN region is 0.5×10 15 ~1×10 17 cm -3, the doping concentration of the N-GaN region is 3×10 17 ~5×10 19 cm -3 , the doping concentration of the N++GaN region is 1×10 18 ~5×10 19 cm -3 .
[0083] Then, if Figure 3g~3h As shown, after the multiple N-type GaN regions in the second preset areas at both ends of the channel region are etched away by an inductively coupled plasma etching (ICP) process, a first P+GaN region and a second P+GaN region with the same thickness as the channel region are grown in the second preset areas at both ends by a metal organic chemical vapor deposition (MOCVD) process.
[0084] See also Figure 3i In steps S5 to S7, the N++GaN substrate is first thinned, and then Ti / Al / Ni / Au metal is deposited on the surface of the N++GaN substrate away from the GaN drift layer by electron beam evaporation, and then high-temperature annealing is performed in a rapid annealing furnace to form a good ohmic contact with the substrate to form a drain. Similarly, Ti / Al / Ni / Au metal is deposited on the surface of the channel region away from the N++GaN substrate by electron beam evaporation, and Ni / Au metal is deposited on the surface of the first P+GaN region and the second P+GaN region away from the N++GaN substrate. After high-temperature annealing, the source, the first gate, and the second gate are formed.
[0085] Finally, if Figure 3j As shown, a plasma chemical vapor deposition (PECVD) process is used to deposit SiNX or SiO2 with a thickness of about 50nm on the source, the first gate, the second gate, the first P+GaN region and the second P+GaN region to form a passivation layer, wherein the nitrogen (N) source is provided by ammonia (NH3) and the silicon (Si) source is provided by silane (SiH4), thereby avoiding direct contact between the first gate\the second gate and the source. A hole is opened in the passivation layer above the source, the first gate and the second gate to lead out the electrode, and the Figure 1 A GaN vertical JFET transistor with a multi-layer channel and a stepped superjunction is shown.
[0086] Figure 4 The transfer curves of conventional JFET devices and GaN vertical JFET devices with multi-layer channels and step-type super junctions are shown in Figure 2. Figure 5It is a transfer curve diagram of a conventional JFET device and a gallium nitride vertical JFET device with a multi-layer channel and a step-type super junction in a semi-logarithmic coordinate, wherein the horizontal axis represents voltage and the vertical axis represents current. It should be noted that the conventional JFET device includes, from bottom to top: a drain, a substrate located on the surface of the drain, an N-GaN drift region located on the surface of the substrate, a channel region located on the surface of the N-GaN drift region, and a first P+GaN region and a second P+GaN region located on both sides of the channel, a first gate and a second gate located on the surfaces of the first and second P+GaN regions respectively, and a source located on the surface of the channel region.
[0087] like Figure 4 As shown in Figure 2, when the threshold voltages of the conventional JFET device and the GaN vertical JFET device with multi-layer channels and step-type superjunction are both 2.8V, the electron concentration in the channel region of the conventional JFET device is 0.6×10 16 cm -3 The forward current is lower than that of the GaN vertical JFET device with multi-layer channel and step-type super junction. Figure 5 As shown in Figure 2, when the forward current of the conventional JFET device and the GaN vertical JFET device with multi-layer channel and step-type super junction is 0.6A, the channel concentration of the conventional JFET device is 2.5×10 16 cm -3 The threshold voltage is lower than that of the GaN vertical JFET device with multi-layer channel and step-type super junction.
[0088] Figure 6 This is the superjunction electric field distribution diagram of a conventional JFET device. Figure 7 This is the superjunction electric field distribution diagram of a GaN vertical JFET device with multi-layer channels and a stepped superjunction. Figures 6-7 As shown, when the voltage is 2000V, the superjunction electric field of the GaN vertical JFET device with multi-layer channels and stepped superjunction is more evenly distributed in the drift region, reducing the electric field strength in the contact area between the P-type region and the N-type drift region.
[0089] Figure 8 This is a comparison of the breakdown voltage of a conventional JFET device and a GaN vertical JFET device with a multi-layer channel and a stepped superjunction. Figure 8 As shown, the breakdown voltage of a conventional JFET device is about 1200V, and the breakdown voltage of a gallium nitride vertical JFET device with a multi-layer channel and a step-type super junction is about 2100V, which significantly improves the breakdown voltage.
[0090] It can be seen from the above embodiments that the beneficial effects of the present invention are:
[0091] The present invention provides a gallium nitride vertical JFET device with a multi-layer channel and a step-type super junction and a preparation method thereof. The device comprises: an N++GaN substrate; a GaN drift layer located on one side surface of the N++GaN substrate; a super junction located on the side surface of the GaN drift layer away from the N++GaN substrate; a channel region, a first P+GaN region and a second P+GaN region located on the side surface of the super junction away from the N++GaN substrate, the first P+GaN region and the second P+GaN region being located on both sides of the channel region respectively; a first gate, a source electrode and a second gate electrode respectively located on the side surface of the first P+GaN region, the channel region and the second P+GaN region away from the N++GaN substrate; a passivation layer located between the first gate electrode and the source electrode and between the second gate electrode and the source electrode; and a drain electrode located on the side surface of the N++GaN substrate away from the GaN drift layer. On the one hand, since the doping concentration of the stepped N-type GaN drift region decreases from bottom to top, and the doping concentration of the stepped P-type low-doped region increases from bottom to top in the superjunction, this stepped superjunction can effectively alleviate the peak electric field at the contact position between the P-type region and the N-type drift region, and improve the device withstand voltage. Compared with the prior art, the present invention replaces the traditional drift region with a superjunction with a high doping concentration, which can increase the carrier concentration in the conductive region and reduce power loss. The forward characteristics (reduced on-resistance) and reverse characteristics (increased breakdown voltage) of the JFET device are also improved, and the power quality factor is significantly improved. In addition, making a stepped superjunction below the P-type region is conducive to improving the avalanche capability of the device, making the device safer and more reliable under extreme conditions.
[0092] On the other hand, the device channel region includes at least one N--GaN region located on the surface of the side of the stepped N-type GaN drift region away from the N++GaN substrate, and at least one N++GaN region located on the surface of the side of the source electrode close to the N++GaN substrate. By introducing ultra-low doping (N--GaN region) in the channel region, the threshold voltage of the device can be significantly improved. At the same time, the forward current is increased by increasing the doping concentration of the upper layer of the channel region (N++GaN region), and the electric field voltage division formed by the super junction makes the electric field uniformly distributed in the drift region, which is conducive to reducing the electric field strength of the contact area between the P-type region and the N-type drift region, thereby obtaining a GaN vertical JFET that simultaneously satisfies high threshold voltage, large forward current and high withstand voltage. In the description of the present invention, the terms "first" and "second" are used only for descriptive purposes and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "multiple" is two or more, unless otherwise clearly and specifically defined.
[0093] The description with reference to the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine different embodiments or examples described in this specification.
[0094] The above contents are further detailed descriptions of the present invention in combination with specific preferred embodiments, and it cannot be determined that the specific implementation of the present invention is limited to these descriptions. For ordinary technicians in the technical field to which the present invention belongs, several simple deductions or substitutions can be made without departing from the concept of the present invention, which should be regarded as falling within the protection scope of the present invention.
Claims
1. A gallium nitride vertical JFET device with multi-layer channels and step-type super junction, characterized in that: include: N++GaN substrate; A GaN drift layer located on a surface of one side of the N++GaN substrate; A super junction located on the surface of the GaN drift layer away from the N++GaN substrate; the super junction comprises a stepped N-type GaN drift region and a stepped P-type low-doping region, the doping concentration of the stepped N-type GaN drift region decreases from bottom to top, and the doping concentration of the stepped P-type low-doping region increases from bottom to top; A channel region, a first P+GaN region and a second P+GaN region located on a surface of the superjunction away from the N++GaN substrate, wherein the first P+GaN region and the second P+GaN region are located on both sides of the channel region respectively; A first gate, a source, and a second gate are respectively located on the first P+GaN region, the channel region, and the second P+GaN region on the side away from the N++GaN substrate; the channel region includes at least one layer of N--GaN region located on the side of the stepped N-type GaN drift region away from the N++GaN substrate, and at least one layer of N++GaN region located on the side of the source electrode close to the N++GaN substrate; a passivation layer located between the first gate and the source and between the second gate and the source; A drain electrode is located on the surface of the N++GaN substrate away from the GaN drift layer.
2. The gallium nitride vertical JFET device with multi-layer channels and step-type super junction according to claim 1, characterized in that: The stepped P-type low-doped region includes: a first P-type low-doped region and a second P-type low-doped region respectively located on both sides of the stepped N-type GaN drift region; wherein the doping concentrations of the first P-type low-doped region and the second P-type low-doped region both increase from bottom to top.
3. The gallium nitride vertical JFET device with multi-layer channels and step-type super junction according to claim 2, characterized in that: The doping concentration of the stepped N-type GaN drift region and the stepped P-type low-doping region is 0.7×10 16 ~1.1×10 18 cm -3 .
4. The gallium nitride vertical JFET device with multi-layer channels and step-type super junction according to claim 2, characterized in that: The stepped N-type GaN drift region includes three layers of N-type GaN drift regions, and the first P-type low-doped region and the second P-type low-doped region both include three layers of P-type low-doped regions, wherein the doping concentration of the same layer of P-type low-doped regions in the first P-type low-doped region and the second P-type low-doped region is the same.
5. The gallium nitride vertical JFET device with multi-layer channels and step-type super junction according to claim 1, characterized in that: In the channel region, at least one N-GaN region is included between the N--GaN region and the N++GaN region.
6. The gallium nitride vertical JFET device with multi-layer channels and step-type super junction according to claim 5, characterized in that: The doping concentration of at least one N--GaN region located on the surface of the stepped N-type GaN drift region away from the N++GaN substrate is 0.5×10 15 ~1×10 17 cm -3 The doping concentration of at least one N++GaN region located on the surface of the source electrode close to the N++GaN substrate side is 1×10 18 ~5×10 19 cm -3 .
7. The gallium nitride vertical JFET device with multi-layer channels and step-type super junction according to claim 5, characterized in that: The doping concentration of at least one N-GaN region between the N--GaN region and the N++GaN region is 3×10 17 ~5×10 19 cm -3 .
8. A method for preparing a gallium nitride vertical JFET device with multi-layer channels and a step-type super junction, characterized in that: include: Providing an N++GaN substrate; Depositing a GaN drift layer on one side surface of the N++GaN substrate; A super junction consisting of a stepped N-type GaN drift region and a stepped P-type low-doped region is grown on the surface of the GaN drift layer away from the N++GaN substrate, wherein the doping concentration of the stepped N-type GaN drift region decreases from bottom to top, and the doping concentration of the stepped P-type low-doped region increases from bottom to top; A channel region is grown on the surface of the super junction away from the N++GaN substrate, and after etching the first preset regions at both ends of the channel region, a first P+GaN region and a second P+GaN region are grown in the first preset regions at both ends of the channel region respectively; Thinning the N++GaN substrate and forming a drain electrode on the surface thereof away from the GaN drift layer; A source electrode is fabricated on a surface of the channel region on a side away from the N++GaN substrate, and a first gate electrode and a second gate electrode are fabricated on surfaces of the first P+GaN region and the second P+GaN region on a side away from the N++GaN substrate, respectively; wherein the channel region includes at least one layer of N--GaN region located on a surface of the stepped N-type GaN drift region on a side away from the N++GaN substrate, and at least one layer of N++GaN region located on a surface of the source electrode on a side close to the N++GaN substrate; After a passivation layer is deposited on the surfaces of the first P+GaN region, the second P+GaN region, the first gate, the second gate and the source, holes are opened in the passivation layer on the surfaces of the source, the first gate and the second gate to lead out electrodes.
9. The method for preparing a gallium nitride vertical JFET device with multi-layer channels and step-type super junction according to claim 8, characterized in that: The step of growing a super junction consisting of a stepped N-type GaN drift region and a stepped P-type low-doped region on the surface of the GaN drift layer away from the N++GaN substrate comprises: Growing multiple layers of N-type GaN drift regions in sequence on a surface of the GaN drift layer away from the N++GaN substrate, wherein the doping concentration of the multiple layers of N-type GaN drift regions decreases from bottom to top; Etching the multi-layer N-type GaN drift region to remove the multi-layer N-type GaN drift region in the second preset regions at both ends to form a stepped N-type GaN drift region; Multiple layers of P-type low-doped regions are sequentially grown in the second preset areas at both ends to form a stepped P-type low-doped region including a first P-type low-doped region and a second P-type low-doped region; the doping concentrations of the first P-type low-doped region and the second P-type low-doped region increase from bottom to top, and the doping concentrations of the same layer of P-type low-doped regions in the first P-type low-doped region and the second P-type low-doped region are the same.
10. The method for preparing a gallium nitride vertical JFET device with multi-layer channels and step-type super junction according to claim 8, characterized in that: The step of growing a channel region on the surface of the super junction away from the N++GaN substrate and etching the first preset regions at both ends of the channel region, and then growing a first P+GaN region and a second P+GaN region in the first preset regions at both ends of the channel region respectively comprises: Growing a plurality of N-type GaN regions in sequence on a surface of the superjunction away from the N++GaN substrate to form a channel region; The channel region is etched to remove a plurality of N-type GaN regions in the second preset regions at both ends of the channel region, and then a first P+GaN region and a second P+GaN region are grown in the second preset regions at both ends of the channel region respectively.
Citation Information
Patent Citations
Improved vjfet devices
CN105190852A
Semiconductor device and method for manufacturing the same
CN110416317A
Silicon carbide power devices having trench-based silicon carbide charge coupling regions therein
US6313482B1
Cited By
JFET device and manufacturing method thereof
CN121194499A
Gallium nitride device and preparation method thereof
CN121398063A
A gallium nitride device and a method of fabricating the same
CN121398063B