Coal gasification slag magnetic adsorption material and preparation method thereof
By modifying the acidizing liquid to treat the gasification slag and adding antibacterial components, the problems of magnetic particles blocking and antibacterial properties in magnetic adsorption materials are solved, the decontamination and antibacterial properties are improved, and the service life of the material is extended.
Patent Information
- Application Number
- CN202411343632.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-25
- Publication Date
- 2024-11-22
AI Technical Summary
During the preparation process of existing magnetic adsorption materials, magnetic particles are prone to block the pores, active adsorption sites are easily eluted, and microorganisms are prone to invade active adsorption sites, resulting in reduced adsorption performance and low recycling value.
The gasification slag is modified with acidification liquid, and the adsorption components and antibacterial components are added. Through the π-cationic action of imidazole structure and chitosan, combined with chemical bonding, the material's decontamination and antibacterial properties are improved, and the problem of magnetic particles is solved. and enhance antibacterial stability.
It improves the decontamination and antibacterial properties of magnetic adsorbent materials, extends the service life of the materials, and achieves antibacterial stability after multiple uses.
Smart Images

Figure SMS_1
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of comprehensive utilization of solid wastes in coal gasification industry, and more specifically, to a magnetic adsorption material for coal gasification slag and a preparation method thereof. Background Art
[0002] With the development and construction of coal chemical projects, the output of coal gasification slag is increasing. The long-term storage of coal gasification slag not only occupies a large amount of land resources, but also may cause more serious environmental and ecological problems.
[0003] Since coal gasification slag not only has a porous structure, but is also cheap and easy to obtain, it has become a hot topic for scholars to use modification technology to modify its surface, improve its adsorption performance, and then use it as an adsorbent in wastewater treatment. After the adsorption is completed, if no measures are taken to recycle and reuse it, the adsorbent becomes a new pollutant and loses the meaning of the adsorbent itself. Therefore, the prior art often uses chemical precipitation to prepare low-cost, easy-to-operate and reusable magnetic adsorption materials. However, the adsorption materials prepared by this method have problems such as magnetic particles easily clogging the pores, active adsorption sites easily being eluted, and microorganisms easily occupying active adsorption sites, resulting in reduced adsorption performance and low recycling value. Summary of the invention
[0004] In order to solve the problems of magnetic particles easily clogging pores, active adsorption sites easily being eluted and microorganisms easily occupying active adsorption sites in the preparation process of existing magnetic adsorption materials, the present application provides a coal gasification slag magnetic adsorption material with good adsorption performance and strong antibacterial performance.
[0005] The purpose of the present invention can be achieved through the following technical solutions: A method for preparing a coal gasification slag magnetic adsorption material comprises the following steps: Step S1, preparation of an acidified solution: add itaconic anhydride to deionized water at a mass ratio of 1:25-35:4, stir evenly, adjust the pH value to 8-9, then add 1-aminoethyl-3-methylimidazole bis(trifluoromethanesulfonyl)imide salt and ultrasonically treat for 0.4-0.6h, heat to 75-85°C under nitrogen, stir to react for 2-4h, and cool to room temperature to obtain an acidified solution; Step S2, preparation of adsorption components: Grind and sieve the coal gasification slag to obtain coal gasification slag particles, mix the coal gasification slag particles and the acidified liquid prepared in step S1 at a mass ratio of 1:25-35, heat to 60-80°C, stir for 1-2h, filter, wash and dry to obtain adsorption components. In the above process, the imidazole cations in the acidified liquid can form stable hydrogen bonds with the active hydroxyl groups in the coal gasification slag to obtain adsorption components with imidazole structures on the surface; Step S3, preparation of magnetic adsorption material: add adsorption component and antibacterial component into deionized water in a mass ratio of 1:40-60:22-32:2-3, stir evenly, add initiator aqueous solution dropwise while stirring, raise the temperature to 72-76°C, continue stirring and reacting for 3.5-4.5h, centrifuge and dry to obtain coal gasification slag magnetic adsorption material.
[0006] Preferably, in step S1, the coal gasification granular slag is coal gasification fine slag produced by a coal gasification furnace in Jiaozuo, Henan, and the particle size of the coal gasification granular slag is 200 meshes.
[0007] Preferably, in step S2, the initiating aqueous solution is a mixture of ammonium persulfate and deionized water in a mass ratio of 1:10-16.
[0008] Preferably, in step S2, the initiator is any one of sodium persulfate, potassium persulfate and ammonium persulfate.
[0009] Based on the characteristics of acidic functional ionized liquids, such as adjustable acidity, easy purification, easy separation, low pollution and recyclability, the present invention chemically combines itaconic anhydride and 1-aminoethyl-3-methylimidazole bis(trifluoromethanesulfonyl)imide salt to obtain an acidified liquid, and uses it to replace traditional inorganic acids, such as hydrochloric acid and sulfuric acid, to modify coal gasification slag, thereby increasing its specific surface area, improving the pore structure, and obtaining a material with better adsorption performance.
[0010] Preferably, the antibacterial component is prepared by the following method: Step A1, under nitrogen protection, add nano-magnetic ferroferric oxide to deionized water in a mass ratio of 3-5:16-28:10-16, stir evenly, then drop sodium silicate solution, maintain pH at 5.9-6.1, heat to 50-60° C., stir for 4-6 hours, filter, wash and dry to obtain magnetic particles. The stability of nano-magnetic ferroferric oxide is poor. Silicon dioxide is coated on the surface of nano-magnetic ferroferric oxide by a sol-gel method to improve its oxidation resistance and stability, so as to stabilize its magnetism; Step A2, mixing the magnetic particles and 20% ethanol aqueous solution by volume in a mass ratio of 1:15-25:0.6-0.8, adding KH-560, heating to 45-55°C, stirring for reaction for 4-6h, separating with a magnet, washing and drying to obtain modified magnetic particles; Step A3, adding the modified magnetic particles to anhydrous DMF at a mass ratio of 5:50-60:15, stirring evenly, dripping tetrabutylammonium bromide, 4,6-diamino-2-mercaptopyrimidine and anhydrous DMF mixed solution a, heating to 90-110°C, stirring for reaction for 2-3h, centrifuging the precipitate, washing and drying to obtain a pyrimidine derivative, wherein the mass ratio of tetrabutylammonium bromide, 4,6-diamino-2-mercaptopyrimidine and DMF in the mixed solution a is 0.1:1.2-1.6:15, and in the above reaction process, using tetrabutylammonium bromide as a catalyst, the epoxy group on the modified magnetic particles undergoes a ring-opening reaction with 4,6-diamino-2-mercaptopyrimidine to obtain a pyrimidine derivative; Step A4, dissolving chitosan in acetic acid solution at a mass ratio of 0.3-0.5:20-30:0.2-0.4:0.1, stirring evenly, adding cinnamaldehyde, heating to 65-75°C, stirring for reaction for 8-10h, cooling to room temperature, adding sodium borohydride, stirring for 12-16h, adjusting the pH to neutral, centrifuging and precipitating, washing and drying to obtain phenyl chitosan, in the above reaction process, using acetic acid solution as solvent, the active amino group on chitosan and the aldehyde group on cinnamaldehyde undergo Schiff condensation reaction to obtain phenyl chitosan; Step A5, adding phenyl chitosan and pyrimidine derivatives to an acetic acid solution in a mass ratio of 3: 0.2-0.4: 30-40: 0.01-0.03, ultrasonically dispersing, adding a photoinitiator, stirring evenly, and irradiating with ultraviolet light for 10-20 minutes to obtain an antibacterial component; under the catalytic action of the photocatalyst, the unsaturated double bonds on the phenyl chitosan and the thiol groups on the pyrimidine derivatives undergo a thiol-ene reaction to obtain the antibacterial component.
[0011] Preferably, in step A1, the concentration of the sodium silicate solution is 1M.
[0012] Preferably, in step A2, the silane coupling agent is KH-560.
[0013] Preferably, in step A4, the mass ratio of acetic acid to anhydrous ethanol in the acetic acid solution is 1-3:200.
[0014] Preferably, in step A5, the mass ratio of acetic acid to anhydrous ethanol in the acetic acid solution is 3-5:120.
[0015] Preferably, in step A5, the photoinitiator is dimethyl benzoate.
[0016] Preferably, the peak wavelength of the irradiation in step A5 is 365nm and the intensity is 80mw / cm 2 .
[0017] A coal gasification slag magnetic adsorption material is obtained by the above-mentioned method for preparing a coal gasification slag magnetic adsorption material.
[0018] In summary, the present application has the following beneficial effects: the present invention adds an adsorption component and an antibacterial component in the process of magnetic adsorption material, the adsorption component is coal gasification slag modified by acidification liquid, the acidification liquid is obtained by ring-opening esterification of itaconic anhydride and 1-aminoethyl-3-methylimidazole bis(trifluoromethanesulfonyl)imide salt, on the one hand, it exerts antibacterial performance, on the other hand, it exerts decontamination performance, the antibacterial performance is reflected in the quaternized imidazole structure, and the decontamination performance is reflected in the imidazole in the 1-aminopropyl-3-vinylimidazole bis(trifluoromethanesulfonyl)imide salt in the acidification liquid and the chitosan structure and benzene ring in the antibacterial component to generate π-cation reaction The use of the adsorption component to load the antibacterial component on the surface of the antibacterial component solves the problem of magnetic particles blocking the pores and improves the decontamination performance of the magnetic adsorbent material. The antibacterial component is prepared by chemically combining phenyl chitosan and pyrimidine derivatives containing thiol groups. On the one hand, it exerts antibacterial properties, and on the other hand, it exerts decontamination properties. The antibacterial properties are reflected in the chitosan structure and the pyrimidine structure, and the decontamination properties are reflected in the three-dimensional network structure obtained by free radical polymerization of double bonds. At the same time, the presence of thiol groups chemically bonds the phenyl chitosan and pyrimidine derivatives in the antibacterial component, further improving the antibacterial stability of the magnetic adsorbent after multiple uses. In summary, the present invention improves the antibacterial and decontamination properties of the magnetic adsorbent material through the combined action of the above-mentioned structures. DETAILED DESCRIPTION
[0019] The contents of the main raw materials and their components used in the examples are as follows: Table 1 Main chemical components of coal gasification slag particles% LOI <![CDATA[SiO 2 ]]> <![CDATA[Al 2 THE 3 ]]> <![CDATA[Fe 2 THE 3 ]]> CaO <![CDATA[Na 2 The]]> Others 32.00 18.26 15.57 6.80 15.93 3.5 8.00 The present application is further described in detail below with reference to the embodiments.
[0020] Preparation Examples 1-3 and Comparative Preparation Example 1 provide methods for preparing antibacterial components.
[0021] Preparation Example 1 The antibacterial component is prepared by the following method: Step A1, under nitrogen protection, add nano-magnetic ferroferric oxide to deionized water in a mass ratio of 3:16:10, stir at 400 rpm for 45 minutes until uniform, then add 1M sodium silicate solution dropwise, and control the dripping to be completed within 30 minutes, maintain the pH at 5.9 with 1M hydrochloric acid solution, heat to 50°C, stir and react for 4 hours, filter, and then wash with anhydrous ethanol and deionized water three times in sequence, and dry at 50°C to constant weight to obtain magnetic particles; Step A2, according to a mass ratio of 1:15:0.6, the magnetic particles and a 20% ethanol aqueous solution by volume were stirred at a speed of 450 rpm for 30 minutes until uniform, and then KH-560 was added, the temperature was raised to 45°C, and the reaction was stirred for 4 hours, separated by a magnet, and then washed with anhydrous ethanol and deionized water for 3 times in sequence, and dried at 45°C to constant weight to obtain modified magnetic particles; Step A3, adding the modified magnetic particles to anhydrous DMF at a mass ratio of 5:50:15, stirring at a speed of 500 rpm for 35 minutes until uniform, dripping tetrabutylammonium bromide, 4,6-diamino-2-mercaptopyrimidine and anhydrous DMF mixed solution a, and controlling the dripping to be completed within 30 minutes, maintaining the speed unchanged, heating to 110°C and stirring for 2 hours, centrifuging and precipitating, and then washing with anhydrous ethanol and deionized water for 3 times in sequence, and drying at 55°C to constant weight to obtain a pyrimidine derivative, wherein, in the mixed solution a, the mass ratio of tetrabutylammonium bromide, 4,6-diamino-2-mercaptopyrimidine and DMF is 0.1:1.2:15; Step A4, dissolving chitosan in an acetic acid solution at a mass ratio of 0.3:20:0.2:0.1, stirring at a speed of 450 rpm for 45 minutes until uniform, adding cinnamaldehyde, heating to 65°C, stirring for 8 hours, cooling to room temperature, adding sodium borohydride, continuing to stir for 12 hours, adjusting the pH to neutral with a 1M hydrochloric acid solution, centrifuging and precipitating, and then washing with anhydrous ethanol and deionized water three times in sequence, and drying at 55°C to constant weight to obtain phenyl chitosan, wherein the acetic acid solution is a mixture of acetic acid and anhydrous ethanol in a mass ratio of 1:200; Step A5: Add phenyl chitosan and pyrimidine derivatives to acetic acid solution in a mass ratio of 3:0.2:30:0.01, disperse by ultrasonic, then add benzoin dimethyl ether, stir evenly, and then place at a wavelength peak of 365nm and an intensity of 80mw / cm 2 The mixture was irradiated under ultraviolet light for 10 minutes to obtain an antibacterial component, wherein the mass ratio of acetic acid to anhydrous ethanol in the acetic acid solution was 3:120.
[0022] Preparation Example 2 Step A1, under nitrogen protection, add nano-magnetic ferroferric oxide to deionized water in a mass ratio of 4:22:13, stir at a speed of 450 rpm for 40 minutes until uniform, then add 1M sodium silicate solution dropwise, and control the dripping to be completed within 30 minutes, use 1M hydrochloric acid solution to maintain the pH at 6.0, heat to 55°C, maintain the speed unchanged, continue stirring to react for 5 hours, filter, and then wash with anhydrous ethanol and deionized water for 4 times in sequence, and dry at 55°C to constant weight to obtain magnetic particles; Step A2, according to a mass ratio of 1:20:0.7, the magnetic particles and a 20% ethanol aqueous solution were stirred at a speed of 500 rpm for 26 minutes until uniform, and then KH-560 was added, the temperature was raised to 50°C, the speed was maintained unchanged, and the stirring reaction was continued for 5 hours, separated by a magnet, and then washed with anhydrous ethanol and deionized water for 4 times in sequence, and dried at 50°C to constant weight to obtain modified magnetic particles; Step A3, adding the modified magnetic particles to anhydrous DMF at a mass ratio of 5:55:15, stirring at a speed of 550 rpm for 30 minutes until uniform, dripping tetrabutylammonium bromide, 4,6-diamino-2-mercaptopyrimidine and anhydrous DMF mixed solution a, and controlling the dripping to be completed within 30 minutes, heating to 110°C and stirring to react for 2-3 hours, centrifuging and precipitating, and then washing with anhydrous ethanol and deionized water for 4 times in sequence, and drying at 60°C to constant weight to obtain a pyrimidine derivative, wherein the mass ratio of tetrabutylammonium bromide, 4,6-diamino-2-mercaptopyrimidine and DMF in the mixed solution a is 0.1:1.4:15; Step A4, dissolving chitosan in an acetic acid solution at a mass ratio of 0.4:25:0.3:0.1, stirring at a speed of 500 rpm for 40 minutes until uniform, adding cinnamaldehyde, heating to 70°C, stirring for 9 hours, cooling to room temperature, adding sodium borohydride, continuing to stir for 14 hours, adjusting the pH to neutral, centrifuging and precipitating, and then washing with anhydrous ethanol and deionized water for 4 times in sequence, and drying at 60°C to constant weight to obtain phenyl chitosan, wherein the mass ratio of acetic acid to anhydrous ethanol in the acetic acid solution is 2:200; Step A5: Add phenyl chitosan and pyrimidine derivatives to acetic acid solution in a mass ratio of 3:0.3:35:0.02, disperse by ultrasonic, then add benzoin dimethyl ether, stir evenly, and then place at a wavelength peak of 365nm and an intensity of 80mw / cm 2 The mixture was irradiated under ultraviolet light for 15 minutes to obtain an antibacterial component, wherein the acetic acid solution was mixed with acetic acid and anhydrous ethanol in a mass ratio of 4:120.
[0023] Preparation Example 3 The antibacterial component is prepared by the following method: Step A1, under nitrogen protection, add nano-magnetic ferroferric oxide to deionized water in a mass ratio of 5:28:16, stir at a speed of 500 rpm for 35 minutes until uniform, then add 1M sodium silicate solution dropwise, and control the dripping to be completed within 30 minutes, use 1M hydrochloric acid solution to maintain the pH at 6.1, heat to 60°C, maintain the speed unchanged, continue stirring to react for 6 hours, filter, and then wash with anhydrous ethanol and deionized water for 5 times in sequence, and dry at 60°C to constant weight to obtain magnetic particles; Step A2, according to a mass ratio of 1:25:0.8, the magnetic particles and a 20% ethanol aqueous solution were stirred at a speed of 550 rpm for 22 minutes until uniform, and then KH-560 was added, the temperature was raised to 55°C, and the reaction was stirred for 6 hours, separated by a magnet, and then washed with anhydrous ethanol and deionized water for 5 times in sequence, and dried at 55°C to constant weight to obtain modified magnetic particles; Step A3, adding the modified magnetic particles to anhydrous DMF at a mass ratio of 5:60:15, stirring at a speed of 600 rpm for 25 minutes until uniform, dripping tetrabutylammonium bromide, 4,6-diamino-2-mercaptopyrimidine and anhydrous DMF mixed solution a, and controlling the dripping to be completed within 30 minutes. After the dripping is completed, the temperature is raised to 110°C and stirred for reaction for 3 hours, and the centrifugal precipitate is washed with anhydrous ethanol and deionized water for 5 times in sequence, and dried at 65°C to constant weight to obtain a pyrimidine derivative. In the mixed solution a, the mass ratio of tetrabutylammonium bromide, 4,6-diamino-2-mercaptopyrimidine and DMF is 0.1:1.6:15; Step A4, dissolving chitosan in an acetic acid solution at a mass ratio of 0.5:30:0.4:0.1, stirring at a speed of 550 rpm for 35 minutes until uniform, adding cinnamaldehyde, heating to 75°C, stirring for reaction for 10 hours, cooling to room temperature, adding sodium borohydride, continuing stirring for 16 hours, adjusting the pH to neutral, centrifuging and precipitating, and then washing with anhydrous ethanol and deionized water for 5 times in sequence, and drying at 65°C to constant weight to obtain phenyl chitosan, wherein the mass ratio of acetic acid to anhydrous ethanol in the acetic acid solution is 3:200; Step A5: Add phenyl chitosan and pyrimidine derivatives to acetic acid solution in a mass ratio of 3:0.4:40:0.03, disperse by ultrasonic, then add benzoin dimethyl ether, stir evenly, and then place at a wavelength peak of 365nm and an intensity of 80mw / cm 2 The mixture was irradiated under ultraviolet light for 20 minutes to obtain an antibacterial component, wherein the mass ratio of acetic acid to anhydrous ethanol in the acetic acid solution was 5:120.
[0024] Comparative Preparation Example 1 The antibacterial component is prepared by the following method: Step A1, under nitrogen protection, add nano-magnetic ferroferric oxide to deionized water in a mass ratio of 3:16:10, stir at 400 rpm for 45 minutes until uniform, then add 1M sodium silicate solution dropwise, and control the dripping to be completed within 30 minutes, maintain the pH at 5.9 with 1M hydrochloric acid solution, heat to 50°C, stir and react for 4 hours, filter, and then wash with anhydrous ethanol and deionized water three times in sequence, and dry at 50°C to constant weight to obtain magnetic particles; Step A2, according to a mass ratio of 1:15:0.6, the magnetic particles and a 20% ethanol aqueous solution by volume were stirred at a speed of 450 rpm for 30 minutes until uniform, and then KH-560 was added, the temperature was raised to 45°C, and the reaction was stirred for 4 hours, separated by a magnet, and then washed with anhydrous ethanol and deionized water for 3 times in sequence, and dried at 45°C to constant weight to obtain modified magnetic particles; Step A3, adding the modified magnetic particles to anhydrous DMF at a mass ratio of 5:50:15, stirring at a speed of 500 rpm for 35 minutes until uniform, dripping tetrabutylammonium bromide, 4,6-diaminopyrimidine and anhydrous DMF mixed solution a, and controlling the dripping to be completed within 30 minutes, maintaining the speed unchanged, heating to 110°C and stirring for 2 hours, centrifuging and precipitating, and then washing with anhydrous ethanol and deionized water for 3 times in sequence, and drying at 55°C to constant weight to obtain a pyrimidine derivative, wherein, in the mixed solution a, the mass ratio of tetrabutylammonium bromide, 4,6-diaminopyrimidine and DMF is 0.1:1.2:15; Step A4, dissolving chitosan in an acetic acid solution at a mass ratio of 0.3:20:0.2:0.1, stirring at a speed of 450 rpm for 45 minutes until uniform, adding cinnamaldehyde, heating to 65°C, stirring for 8 hours, cooling to room temperature, adding sodium borohydride, continuing to stir for 12 hours, adjusting the pH to neutral with a 1M hydrochloric acid solution, centrifuging and precipitating, and then washing with anhydrous ethanol and deionized water three times in sequence, and drying at 55°C to constant weight to obtain phenyl chitosan, wherein the acetic acid solution is a mixture of acetic acid and anhydrous ethanol in a mass ratio of 1:200; Step A5: Add phenyl chitosan and pyrimidine derivatives to acetic acid solution in a mass ratio of 3:0.2:30:0.01, disperse by ultrasonic, then add benzoin dimethyl ether, stir evenly, and then place at a wavelength peak of 365nm and an intensity of 80mw / cm 2 The mixture was irradiated under ultraviolet light for 10 minutes to obtain an antibacterial component, wherein the acetic acid solution was mixed with acetic acid and anhydrous ethanol in a mass ratio of 3:120.
[0025] Examples 1-3 and Comparative Examples 1-3 provide methods for preparing coal gasification slag magnetic adsorption materials.
[0026] Example 1 This embodiment provides a method for preparing a magnetic adsorption material of coal gasification slag, comprising the following steps: Step S1, preparation of an acidified solution: add itaconic anhydride to deionized water at a mass ratio of 1:25:4, stir at a speed of 450 rpm for 30 min until uniform, adjust the pH value to 8 with a 1M sodium hydroxide solution, then add 1-aminoethyl-3-methylimidazole bis(trifluoromethanesulfonyl)imide salt and perform ultrasonic treatment at an ultrasonic frequency of 30 kHz and an ultrasonic power of 400 w for 0.6 h, raise the temperature to 75° C. under nitrogen, maintain the speed unchanged, continue stirring and reacting for 2 h, and cool to room temperature to obtain an acidified solution; Step S2, preparation of adsorption component: Grind and sieve the coal gasification slag to obtain 200-mesh coal gasification slag particles, and stir the 200-mesh coal gasification slag particles and the acidified liquid prepared in step S1 at a mass ratio of 1:25 at a speed of 400 rpm for 40 minutes until uniform, heat to 60° C., stir for 1 hour, filter, wash with anhydrous ethanol and deionized water for 3 times in sequence, and dry at 50° C. to constant weight to obtain adsorption component; Step S3, preparation of magnetic adsorption material: add the adsorption component and the antibacterial component prepared in Preparation Example 1 into deionized water in a mass ratio of 1:40:22:2, stir at a speed of 300 rpm for 40 minutes until uniform, maintain the speed unchanged, add ammonium persulfate aqueous solution dropwise while stirring, and control the dripping to be completed within 30 minutes. After the dripping is completed, heat to 72°C, continue stirring to react for 4.5 hours, centrifuge and precipitate, and dry at 55°C to constant weight to obtain a coal gasification slag magnetic adsorption material, wherein the mass ratio of ammonium persulfate to deionized water in the ammonium persulfate aqueous solution is 1:12.
[0027] Example 2 This embodiment provides a method for preparing a magnetic adsorption material of coal gasification slag, comprising the following steps: Step S1, preparation of an acidified solution: add itaconic anhydride to deionized water at a mass ratio of 1:30:4, stir at a speed of 500 rpm for 25 min until uniform, adjust the pH value to 8.5 with a 1M sodium hydroxide solution, then add 1-aminoethyl-3-methylimidazole bis(trifluoromethanesulfonyl)imide salt and perform ultrasonic treatment at an ultrasonic frequency of 35 kHz and an ultrasonic power of 500 w for 0.5 h, raise the temperature to 80° C. under nitrogen, maintain the speed unchanged, continue stirring and reacting for 3 h, and cool to room temperature to obtain an acidified solution; Step S2, preparation of adsorption component: Grind and sieve the coal gasification slag to obtain 200-mesh coal gasification slag particles, and stir the coal gasification slag particles and the acidified liquid prepared in step S1 at a mass ratio of 1:30 at a speed of 450 pm for 35 minutes until uniform, heat to 70° C., stir for 1.5 hours, filter, wash with anhydrous ethanol and deionized water for 4 times in sequence, and dry at 55° C. to constant weight to obtain adsorption component; Step S3, preparation of magnetic adsorption material: add the adsorption component and the antibacterial component prepared in Preparation Example 2 to deionized water in a mass ratio of 1:50:27:2.5, stir at a speed of 355 rpm for 35 minutes until uniform, add potassium persulfate aqueous solution dropwise while stirring, and control the dripping to be completed within 30 minutes. After the dripping is completed, the temperature is raised to 74°C, and the stirring reaction is continued for 4.0 hours. Centrifugal precipitation is performed, and the gasification slag is dried to constant weight at 60°C to obtain a coal gasification slag magnetic adsorption material, wherein the mass ratio of potassium persulfate to deionized water in the potassium persulfate aqueous solution is 1:14.
[0028] Example 3 This embodiment provides a method for preparing a magnetic adsorption material of coal gasification slag, comprising the following steps: Step S1, preparation of an acidified solution: add itaconic anhydride to deionized water at a mass ratio of 1:35:4, stir at a speed of 550 rpm for 25 min until uniform, adjust the pH value to 9 with a 1M sodium hydroxide solution, add 1-aminoethyl-3-methylimidazole bis(trifluoromethanesulfonyl)imide salt, and perform ultrasonic treatment at an ultrasonic frequency of 40 kHz and an ultrasonic power of 600 w for 0.4 h, raise the temperature to 85° C. under nitrogen, maintain the speed unchanged, continue stirring and reacting for 4 h, and cool to room temperature to obtain an acidified solution; Step S2, preparation of adsorption component: Grind and sieve the coal gasification slag to obtain 200-mesh coal gasification slag particles, and stir the 200-mesh coal gasification slag particles and the acidified liquid prepared in step S1 at a mass ratio of 1:35 at a speed of 500 rpm for 30 minutes until uniform, heat to 80° C., maintain the speed unchanged, continue stirring for 2 hours, filter, wash with anhydrous ethanol and deionized water for 5 times in sequence, and dry at 60° C. to constant weight to obtain adsorption component; Step S3, preparation of magnetic adsorption material: add the adsorption component and the antibacterial component prepared in Preparation Example 3 to deionized water at a mass ratio of 1:60:32:3, stir at a speed of 400 rpm for 20 minutes until uniform, maintain the speed unchanged, and add sodium persulfate aqueous solution dropwise while stirring. After the dropwise addition, heat to 76°C, continue stirring and react for 3.5 hours, centrifuge and precipitate, and dry at 65°C to constant weight to obtain a coal gasification slag magnetic adsorption material, wherein the mass ratio of ammonium persulfate to deionized water in the sodium persulfate aqueous solution is 1:16.
[0029] Comparative Example 1 This embodiment provides a method for preparing a magnetic adsorption material of coal gasification slag, comprising the following steps: Step S1, preparation of an acidified solution: add succinic anhydride to deionized water at a mass ratio of 1:25:4, stir at a speed of 450 rpm for 30 min until uniform, adjust the pH value to 8 with a 1M sodium hydroxide solution, then add 1-aminoethyl-3-methylimidazole bis(trifluoromethanesulfonyl)imide salt and perform ultrasonic treatment at an ultrasonic frequency of 30 kHz and an ultrasonic power of 400 w for 0.6 h, raise the temperature to 75° C. under nitrogen, maintain the speed unchanged, continue stirring and reacting for 2 h, and cool to room temperature to obtain an acidified solution; Step S2, preparation of adsorption component: Grind and sieve the coal gasification slag to obtain 200-mesh coal gasification slag particles, and stir the 200-mesh coal gasification slag particles and the acidified liquid prepared in step S1 at a mass ratio of 1:25 at a speed of 400 rpm for 40 minutes until uniform, heat to 60° C., stir for 1 hour, filter, wash with anhydrous ethanol and deionized water for 3 times in sequence, and dry at 50° C. to constant weight to obtain adsorption component; Step S3, preparation of magnetic adsorption material: add the adsorption component and the antibacterial component prepared in Preparation Example 1 into deionized water in a mass ratio of 1:40:22:2, stir at a speed of 300 rpm for 40 minutes until uniform, maintain the speed unchanged, add ammonium persulfate aqueous solution dropwise while stirring, and control the dripping to be completed within 30 minutes. After the dripping is completed, heat to 72°C, continue stirring to react for 4.5 hours, centrifuge and precipitate, and dry at 55°C to constant weight to obtain a coal gasification slag magnetic adsorption material, wherein the mass ratio of ammonium persulfate to deionized water in the ammonium persulfate aqueous solution is 1:12.
[0030] Comparative Example 2 This embodiment provides a method for preparing a magnetic adsorption material of coal gasification slag, comprising the following steps: Step S1, preparation of an acidified solution: add itaconic anhydride to deionized water at a mass ratio of 1:25:4, stir at a speed of 450 rpm for 30 min until uniform, adjust the pH value to 8 with a 1M sodium hydroxide solution, add 1-(3-aminopropyl)imidazole, and perform ultrasonic treatment at an ultrasonic frequency of 30 kHz and an ultrasonic power of 400 w for 0.6 h. Raise the temperature to 75° C. under nitrogen, maintain the speed unchanged, continue stirring and reacting for 2 h, and cool to room temperature to obtain an acidified solution; Step S2, preparation of adsorption component: Grind and sieve the coal gasification slag to obtain 200-mesh coal gasification slag particles, and stir the 200-mesh coal gasification slag particles and the acidified liquid prepared in step S1 at a mass ratio of 1:25 at a speed of 400 rpm for 40 minutes until uniform, heat to 60° C., stir for 1 hour, filter, wash with anhydrous ethanol and deionized water for 3 times in sequence, and dry at 50° C. to constant weight to obtain adsorption component; Step S3, preparation of magnetic adsorption material: add the adsorption component and the antibacterial component prepared in Preparation Example 1 into deionized water in a mass ratio of 1:40:22:2, stir at a speed of 300 rpm for 40 minutes until uniform, maintain the speed unchanged, add ammonium persulfate aqueous solution dropwise while stirring, and control the dripping to be completed within 30 minutes. After the dripping is completed, heat to 72°C, continue stirring to react for 4.5 hours, centrifuge and precipitate, and dry at 55°C to constant weight to obtain a coal gasification slag magnetic adsorption material, wherein the mass ratio of ammonium persulfate to deionized water in the ammonium persulfate aqueous solution is 1:12.
[0031] Comparative Example 3 This embodiment provides a method for preparing a magnetic adsorption material of coal gasification slag, comprising the following steps: Step S1, preparation of an acidified solution: add itaconic anhydride to deionized water at a mass ratio of 1:25:4, stir at a speed of 450 rpm for 30 min until uniform, adjust the pH value to 8 with a 1M sodium hydroxide solution, then add 1-aminoethyl-3-methylimidazole bis(trifluoromethanesulfonyl)imide salt and perform ultrasonic treatment at an ultrasonic frequency of 30 kHz and an ultrasonic power of 400 w for 0.6 h, raise the temperature to 75° C. under nitrogen, maintain the speed unchanged, continue stirring and reacting for 2 h, and cool to room temperature to obtain an acidified solution; Step S2, preparation of adsorption component: Grind and sieve the coal gasification slag to obtain 200-mesh coal gasification slag particles, and stir the 200-mesh coal gasification slag particles and the acidified liquid prepared in step S1 at a mass ratio of 1:25 at a speed of 400 rpm for 40 minutes until uniform, heat to 60° C., stir for 1 hour, filter, wash with anhydrous ethanol and deionized water for 3 times in sequence, and dry at 50° C. to constant weight to obtain adsorption component; Step S3, preparation of magnetic adsorption material: add the adsorption component and the antibacterial component prepared in comparative preparation example 1 to deionized water in a mass ratio of 1:40:22:2, stir at a speed of 300 rpm for 40 minutes until uniform, maintain the speed unchanged, add ammonium persulfate aqueous solution dropwise while stirring, and control the dripping to be completed within 30 minutes. After the dripping is completed, heat to 72°C, continue stirring to react for 4.5 hours, centrifuge and precipitate, and dry at 55°C to constant weight to obtain a gasification slag magnetic adsorption material, wherein the mass ratio of ammonium persulfate to deionized water in the ammonium persulfate aqueous solution is 1:12.
[0032] Performance Testing Decontamination performance: Taking methylene blue and potassium dihydrogen phosphate solution as examples, the adsorption performance of the coal gasification slag magnetic adsorption material prepared in the present application after repeated use was simulated. Take 50 mg of the coal gasification slag magnetic adsorption material prepared in Examples 1-3 and Comparative Examples 1-3 respectively, add 50 mL, 150 mg / L, 12 ° C methylene blue solution and potassium dihydrogen phosphate solution, stir at 80 rpm until uniform, keep the speed unchanged, and sample within 3 hours, and use an ultraviolet spectrophotometer (UV-2600) to measure the concentration change of the methylene blue solution. After the adsorption is completed, the methylene blue solution adsorbed by the coal gasification slag magnetic adsorption material is washed with water, and the coal gasification slag magnetic adsorption material is recovered by magnetic separation technology. The above test process is repeated five times, and the specific test results are shown in Table 1 below: 2. Antibacterial properties Antibacterial rate: Escherichia coli and Staphylococcus aureus were used as bacterial models. The antibacterial rate of the adsorbent material after 5 uses was detected by the number of bacteria in the culture medium using the oscillation method. The test results are shown in Table 1: Table 1
[0033] It can be seen from the data shown in Table 1 above that the coal gasification slag magnetic adsorption material produced in Examples 1-3 of the present application has a higher removal rate of methylene blue and potassium dihydrogen phosphate after 5 uses. At the same time, after 5 uses, the antibacterial rate against Staphylococcus aureus and Escherichia coli can still reach more than 97%, which is higher than the national standard evaluation index for antibacterial performance and has excellent antibacterial effect.
[0034] The above contents are merely examples and explanations of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in a similar manner. As long as they do not deviate from the invention or exceed the scope defined by the claims, they shall all fall within the protection scope of the present invention.
Claims
1. A coal gasification slag magnetic adsorption material, characterized in that: The following steps are involved: Step S1, preparation of an acidified solution: add itaconic anhydride to deionized water at a mass ratio of 1:25-35:4, stir evenly, adjust the pH value to 8-9, then add 1-aminoethyl-3-methylimidazole bis(trifluoromethanesulfonyl)imide salt and ultrasonically treat for 0.4-0.6h, heat to 75-85°C under nitrogen, stir to react for 2-4h, and cool to room temperature to obtain an acidified solution; Step S2, preparation of adsorption components: Grind and sieve the coal gasification slag to obtain coal gasification slag particles, mix the coal gasification slag particles and the acidified liquid prepared in step S1 at a mass ratio of 1:25-35, heat to 60-80°C, stir for 1-2h, filter, wash and dry to obtain adsorption components; Step S3, preparation of magnetic adsorption material: add adsorption component and antibacterial component into deionized water in a mass ratio of 1:40-60:22-32:2-3, stir evenly, add initiator aqueous solution dropwise while stirring, raise the temperature to 72-76°C, continue stirring and reacting for 3.5-4.5h, centrifuge and dry to obtain coal gasification slag magnetic adsorption material.
2. The coal gasification slag magnetic adsorption material according to claim 1, characterized in that: The antibacterial component is prepared by the following method: Step A1, under nitrogen protection, add nano-magnetic ferroferric oxide to deionized water in a mass ratio of 3-5:16-28:10-16, stir evenly, then dropwise add sodium silicate solution, maintain pH at 5.9-6.1, heat to 50-60°C, stir to react for 4-6h, filter, wash and dry to obtain magnetic particles; Step A2, mixing the magnetic particles and 20% ethanol aqueous solution by volume in a mass ratio of 1:15-25:0.6-0.8, adding a silane coupling agent, heating to 45-55°C, stirring for reaction for 4-6h, separating with a magnet, washing and drying to obtain modified magnetic particles; Step A3, adding the modified magnetic particles to anhydrous DMF at a mass ratio of 5:50-60:15, stirring evenly, adding tetrabutylammonium bromide, 4,6-diamino-2-mercaptopyrimidine and anhydrous DMF mixed solution a dropwise, raising the temperature to 90-110° C., stirring for reaction for 2-3 hours, centrifuging the precipitate, washing and drying to obtain a pyrimidine derivative; Step A4, dissolving chitosan in acetic acid solution at a mass ratio of 0.3-0.5:20-30:0.2-0.4:0.1, stirring evenly, adding cinnamaldehyde, heating to 65-75°C, stirring for 8-10h, cooling to room temperature, adding sodium borohydride, stirring for 12-16h, adjusting the pH to neutral, centrifuging and precipitating, washing and drying to obtain phenyl chitosan; Step A5, adding phenyl chitosan and pyrimidine derivatives to an acetic acid solution in a mass ratio of 3: 0.2-0.4: 30-40: 0.01-0.03, ultrasonically dispersing, adding a photoinitiator, stirring evenly, and irradiating with ultraviolet light for 10-20 minutes to obtain an antibacterial component.
3. The coal gasification slag magnetic adsorption material according to claim 1, characterized in that: The particle size of the coal gasification slag particles is 200 meshes.
4. The coal gasification slag magnetic adsorption material according to claim 1, characterized in that: The initiator aqueous solution is a mixture of initiator and deionized water in a mass ratio of 1:12-16.
5. The coal gasification slag magnetic adsorption material according to claim 4, characterized in that: The initiator is any one of sodium persulfate, potassium persulfate and ammonium persulfate.
6. The coal gasification slag magnetic adsorption material according to claim 2, characterized in that: In the mixed solution a, the mass ratio of tetrabutylammonium bromide, 4,6-diamino-2-mercaptopyrimidine and DMF is 0.1:1.2-1.6:
15.
7. The coal gasification slag magnetic adsorption material according to claim 2, characterized in that: In the step A5, the photoinitiator is dimethyl benzoate.
8. The coal gasification slag magnetic adsorption material according to claim 2, characterized in that: The peak wavelength of the irradiation in step A5 is 365nm and the intensity is 80mw / cm 2 .
9. A coal gasification slag magnetic adsorption material, characterized in that: The magnetic adsorption material of coal gasification slag is obtained by the preparation method of the magnetic adsorption material of coal gasification slag according to any one of claims 1 to 8.
Citation Information
Patent Citations
Synthesizing method of fly ash magnetic bead magnetic adsorbent coated by chitosan
CN104722282A
Antibacterial chitosan dressing containing nanogold and preparation method of dressing
CN106178079A
Preparation method of modified expanded rice husk spherical adsorption material
CN107159151A
[H2Nmim][NTf2]@UiO-66-Br nanocomposite material and application thereof
CN110618224A
Coal gasification slag magnetic adsorption material and preparation method thereof
CN115178227A