Manufacturing method of carved groove wallboard
By first applying surface primer and engraving grooves in the manufacturing of trench wall panels, and then printing and coating with digital equipment and soft rollers, the paint stacking problem is solved, and the uniformity and aesthetics of the product are improved. Reduced costs.
Patent Information
- Application Number
- CN202411135511.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-19
- Publication Date
- 2024-11-22
AI Technical Summary
In the existing trench wall panel manufacturing technology, paint is easy to accumulate in the trench, affecting the use effect and increasing costs.
First coat the surface primer on the substrate surface, then carve the grooves in the grooves, and use digital equipment to print the topcoat. Combined with the use of soft rollers and coating hard rollers, a protective layer and a uniform topcoat layer are formed. , reduce paint buildup and application times.
It improves the uniformity of the topcoat, reduces the accumulation of paint in the groove, reduces the amount of paint and the number of times of application, reduces production costs, and improves product quality and aesthetics.
Smart Images

Figure CN118988692A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of wallboard manufacturing, in particular to a method for manufacturing a grooved wallboard. Background Art
[0002] At present, the grooved wall panels on the market are mainly painted with UV roller coating. In order to ensure uniform paint in the groove, not only multiple roller coatings are required, but also a large amount of paint is used, which easily leads to paint accumulation at the edge of the groove during the rolling process. Sanding is also required to remove excess paint on the surface of the substrate, and the sanding process will cause dust accumulation in the groove that is difficult to remove. Summary of the invention
[0003] The object of the present invention is to provide a method for manufacturing a grooved wallboard to solve the technical problem in the prior art that paint is accumulated in the grooves, which affects the use effect of the wallboard and increases the cost.
[0004] An embodiment of the present invention provides a method for manufacturing a grooved wallboard, which comprises the following steps:
[0005] The premixed slurry is extruded by an extruder to form a substrate;
[0006] In a dust-free environment, the paint is rolled on the surface of the substrate and the paint is cured to form a surface primer layer on the surface of the substrate;
[0007] engraving a groove on the side of the substrate coated with the surface primer layer;
[0008] Apply the groove primer in the groove using a soft roller;
[0009] Using digital equipment to print on the surface of the surface primer and the groove primer to form a topcoat layer, wherein the printing ink volume of the digital equipment is 5-15g / m2 and the printing speed is 10-20m / min;
[0010] A protective layer is formed by coating the surface of the substrate having a surface primer layer using a coating hard roller.
[0011] Furthermore, before using an extruder to extrude the premixed slurry to form a substrate, the method further comprises:
[0012] Mixing resin, filler, chain extender, lubricant, and plasticizer to form a mixed liquid;
[0013] The mixed solution is fully stirred to form a premixed slurry.
[0014] Furthermore, the ratio of resin, filler, chain extender, lubricant and plasticizer is (2-2.5):(7-8):(1-5):(0.1-0.5):(1-5).
[0015] Furthermore, before rolling the primer on the surface of the substrate in a dust-free environment and curing the primer, the method further comprises:
[0016] Sand the substrate.
[0017] Further, the substrate is sanded including:
[0018] A plurality of sandpapers are used to grind the surface of the substrate in sequence according to a preset sequence, wherein the mesh numbers of the plurality of sandpapers are increased in sequence according to the preset sequence, and the mesh numbers of the plurality of sandpapers are 120-320 meshes.
[0019] Further, in a dust-free environment, rolling paint on the surface of the substrate and curing the paint to form a surface primer layer on the surface of the substrate includes:
[0020] The base material is coated with primer by roller coating for 2-3 times, and each coat of oil needs to be cured with UV lamp, and the coating amount is 20-40g / m2.
[0021] Furthermore, before engraving the groove on the side of the substrate coated with the primer, the method further comprises:
[0022] The substrate is first separated and chamfered after being coated with a surface primer.
[0023] Further, applying the groove primer in the groove using a soft roller includes:
[0024] Use a 20-30° soft roller to coat the substrate, with a coating amount of 6-12g / m 2 After coating, use UV lamp for curing. The UV lamp curing energy is 150-400mj / cm 2 .
[0025] Further, forming a protective layer by coating a surface of a substrate having a surface primer layer with a coating hard roller includes:
[0026] Use a coating hard roller to coat the printed substrate with a coating amount of 10-20g / m 2 .
[0027] Furthermore, when a groove is engraved on the side of the substrate coated with the primer, the groove depth is 0.3-1 mm and the groove width is 0.5-5 mm.
[0028] The invention provides a method for manufacturing a grooved wallboard, which first applies a surface primer, then forms grooves, applies a groove primer in the grooves, and finally prints a topcoat on the surface of the substrate by printing, thereby effectively improving the uniformity of the topcoat and improving the product quality. It also reduces the accumulation of paint in the grooves, reduces the number of coatings and the amount of paint used, and thus reduces costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0030] Figure 1 A flow chart of a method for manufacturing a grooved wallboard provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0031] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Generally, the components of the embodiments of the present invention described and shown in the drawings here can be arranged and designed in various different configurations.
[0032] In the description of the present invention, it should be noted that the terms "upper", "lower", "inside", "outside", etc. indicate directions or positional relationships based on the directions or positional relationships shown in the accompanying drawings, or are directions or positional relationships in which the product of the invention is usually placed when in use. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore should not be understood as a limitation on the present invention.
[0033] Some embodiments of the present invention are described in detail below in conjunction with the accompanying drawings. In the absence of conflict, the following embodiments and features in the embodiments can be combined with each other.
[0034] Example 1
[0035] Please refer to Figure 1 As shown, this embodiment provides a method for manufacturing a grooved wallboard, which includes the following steps:
[0036] S100: Use an extruder to extrude the premixed slurry into a substrate. In this embodiment, resin, filler, chain extender, lubricant, plasticizer and other materials are mixed in a certain proportion, and after sufficient stirring and kneading, a twin-screw extruder is used to extrude to form a plate-like substrate. Forming a plate by mixed numerical extrusion is a prior art, and the specific operation steps are not limited here. Any extrusion molding method disclosed in the market can be used to achieve substrate extrusion molding. A twin-screw extruder can be used for extrusion, and other extrusion equipment can also be selected for processing according to the production environment and cost.
[0037] S200: In a dust-free environment, the paint is rolled on the surface of the substrate and cured to form a surface primer layer on the surface of the substrate. The surface primer layer can be a colored primer, such as white, gray primer, etc. The surface primer is applied to the surface of the substrate to cover the original base color of the substrate and improve the aesthetics of the substrate. The coating can be carried out in a dust-free workshop to prevent dust from adhering to the surface of the substrate and affecting the coating effect.
[0038] S300: Carve a groove on the side of the substrate coated with primer. According to the use requirements and design patterns, grooves are opened on the surface of the substrate. Traditional grooved wall panels are processed by first grooving and then painting. This method not only affects the efficiency and effect of painting, but also leads to increased costs. The present embodiment adopts the operating steps of first applying the surface primer and then opening the grooves. On the one hand, when the surface primer is applied on a substrate with a flat surface, the coating is more uniform and the coating efficiency is higher. On the other hand, it avoids the accumulation of paint in the grooves or at the edges of the grooves when applying the surface primer, thereby ensuring the aesthetics of the substrate and the grooves and the accuracy of the grooves. It can also avoid the accumulation of paint in the grooves when painting, reduce the amount of paint used, and save costs.
[0039] S400: Use a soft roller to apply the groove primer in the groove. When the groove is opened, the surface primer applied on the substrate will be removed, and the groove needs to be coated separately. When coating, a soft roller is used to apply the groove primer along the groove. The size of the soft roller is adapted to the groove to ensure that the paint can be evenly applied to the inner wall of the groove during coating, avoiding paint accumulation, saving costs while ensuring the coating effect of the paint and improving the aesthetics of the substrate.
[0040] S500: Use digital equipment to print on the surface of the surface primer and the groove primer to form a topcoat layer, wherein the printing ink volume of the digital equipment is 5-15g / m2 and the printing speed is 10-20m / min. After the surface primer and the groove primer are dried, the ink is printed on the surface of the substrate to form a pattern. During the process, the paint can be accurately, evenly and stably printed in the groove. There are many color choices in the groove, and different colors can be printed according to different needs. The printed pattern in the groove has good adhesion and will not fall off due to scratching.
[0041] S600: Use a coating hard roller to coat the surface of the substrate with a surface primer layer to form a protective layer. The coating of the protective layer can protect the substrate and improve the scratch resistance of the substrate surface. At the same time, the protective layer covers the surface primer, which can adjust the color and gloss of the substrate and improve the aesthetics of the grooved wallboard.
[0042] The grooved wallboard manufacturing method in this embodiment adopts the method of first applying a surface primer, then opening the grooves, and using digital printing to form the wallboard by inkjet in the grooves, thereby avoiding paint accumulation in the grooves, saving costs, and improving operating efficiency and the aesthetics of the finished product.
[0043] Optionally, in some implementations of the present embodiment, the resin, filler, chain extender, lubricant, and plasticizer are first mixed to form a mixed solution, wherein the ratio of the resin, filler, chain extender, lubricant, and plasticizer is (2-2.5):(7-8):(1-5):(0.1-0.5):(1-5). The mixed solution is then fully stirred to form a premixed slurry, and the premixed slurry is added to an extruder for extrusion to form a substrate. By mixing the above materials in the above proportions to form a premixed slurry, the substrate is extruded to form a substrate with high strength, long service life, and convenient for subsequent groove opening. After the substrate is produced, it is easy to adsorb with the paint, and the paint will not fall off, and the use effect is good.
[0044] Optionally, in some implementations of this embodiment, before rolling the primer on the surface of the substrate in a dust-free environment and curing the primer, the substrate is sanded.
[0045] In this embodiment, after the substrate is extruded and left to harden, the surface of the substrate is sanded to eliminate defects such as burrs or protrusions generated during extrusion, to ensure the flatness of the substrate surface, to facilitate the subsequent application of a surface primer to the substrate surface, and to improve the uniformity and adhesion of the surface primer after application.
[0046] Optionally, in some implementations of this embodiment, sanding the substrate includes: using multiple sandpapers to grind the surface of the substrate in sequence according to a preset order, wherein the mesh sizes of the multiple sandpapers increase in a preset order, and the mesh sizes of the multiple sandpapers are 120-320.
[0047] In this embodiment, by sanding the substrate surface, on the one hand, it is possible to eliminate defects such as burrs and protrusions generated when the substrate is extruded, ensure the overall flatness of the base groove surface, facilitate the subsequent coating of the surface primer, and avoid uneven surface primer layer. The polished substrate is also more uniform when the surface primer is coated. On the other hand, the surface of the polished substrate forms a frosted texture, which is convenient for paint adhesion and avoids problems such as paint falling off during use. During polishing, according to the actual situation of the substrate, sandpaper is used for multiple polishing, and the mesh number of the sandpaper is gradually increased each time to ensure the polishing effect.
[0048] Optionally, in some implementations of this embodiment, in a dust-free environment, paint is rolled on the surface of the substrate and the paint is cured to form a surface primer layer on the surface of the substrate, including: coating the substrate with primer by rolling, the number of coatings is 2-3 times, and each coat of oil needs to be cured with a UV lamp, and the coating amount is 20-40g / m2.
[0049] In this embodiment, the surface primer layer adopts UV curing paint (UV paint for short). UV curing paint has the effect of preventing pollution and saving energy, and has excellent chemical and physical properties of coating and fast curing characteristics. It is widely used in the production of plastics, vacuum plating, PVC floors, shadow masks, car headlights, wooden floors, cabinet panels, etc. It is an ideal coating for wall panel primer. In addition, UV curing paint has the advantages of not containing volatile organic compounds, less pollution to the environment, fast curing speed, saving energy, good performance of cured products, and being suitable for high-speed automated production. However, traditional coatings are volatile and have slow curing speeds, which are not conducive to environmental protection. The embodiment of the present application adopts UV paint, and the number of coatings is 2-3 times. After each coating, UV is used for curing. The next coating is carried out after the UV paint is completely cured to ensure the coating effect and avoid paint falling off. Multiple coatings are used to ensure the uniformity of coating. The coating amount of UV paint is 20-40g / m 2 , to ensure the covering effect and uniformity of the surface primer layer. It is understandable that when the coating amount of UV paint is too small, the thickness of the surface primer layer is too thin, unable to cover the color of the substrate, affecting the subsequent topcoat printing; on the contrary, when the coating amount is too large, the surface primer layer is too thick, not only the cost is high, but also the primer is prone to unevenness, affecting the aesthetics of the finished product.
[0050] Optionally, in some implementations of this embodiment, before engraving the groove on the side of the substrate coated with the primer, the substrate coated with the surface primer is first separated and edge-cut.
[0051] In this embodiment, a larger substrate plate is formed by extrusion processing with an extruder. Since the surface primer is applied first and then the grooves are opened, the substrate is relatively flat when the surface primer is applied, and a large area can be directly coated, thereby improving coating efficiency and uniformity. After the surface primer is completely dry, the substrate is cut as needed, and the edges are processed after cutting to ensure that the edges are completely aligned when the wall panels are spliced, which can effectively reduce the height difference and seam problems after splicing.
[0052] Optionally, in some implementations of this embodiment, applying the groove primer in the groove using a soft roller includes: coating the substrate with a 20-30° soft roller, with a coating amount of 6-12 g / m 2 After coating, use UV lamp for curing. The UV lamp curing energy is 150-400mj / cm 2 .
[0053] In this embodiment, when applying the groove primer, the groove primer can be applied along the designed grooves. A 20-30° soft roller is used to apply the primer, ensuring that the paint fully enters the grooves and forms a coating effect in the grooves, avoiding paint accumulation and ensuring the uniformity of the groove primer. The inner area of the groove is small and in a sunken state. The coating amount is 6-12g / m 2After coating, UV lamp is used for curing. Since the groove has a certain depth, the UV lamp curing energy is 150-400mj / cm 2 , to ensure that the curing effect meets the requirements.
[0054] It should be noted that, in some other embodiments, depending on the color of the primer and the color of the substrate, the amount of paint applied can be selectively adjusted according to the actual coating effect.
[0055] Optionally, in some implementations of this embodiment, the protective layer is formed by coating the surface of the substrate having the surface primer layer with a coating hard roller, including the steps of: coating the printed substrate with a coating hard roller, with a coating amount of 10-20 g / m 2 .
[0056] In this embodiment, a coating hard roller is used to coat the printed substrate, and the coating amount is 10-20g / m 2 After forming a protective film, it protects the substrate and the surface primer, enhances the scratch resistance of the substrate surface, and improves the glossiness of the substrate surface. Using a hard roller will not allow the coating oil to enter the grooves, which can control its appearance and affect the overall aesthetics.
[0057] Optionally, in some implementations of the embodiments, when a groove is engraved on the side of the substrate coated with the primer, the groove depth is 0.3-1 mm and the groove width is 0.5-5 mm.
[0058] In this embodiment, the processing thickness of the substrate is 4-12mm. According to the usage scenario and requirements, the extrusion thickness of the substrate is adjusted during production. When opening the groove, the engraving size and style of the groove can be freely designed, including but not limited to square, hexagonal, relief, etc. Due to the difference in substrate thickness, the groove depth range is controlled within 0.3-1mm, and the groove width range is controlled within 0.5-5mm. The groove can be formed without affecting the strength of the substrate, avoiding cracking or breaking of the substrate, and ensuring the service life of the substrate.
[0059] Example 2
[0060] This embodiment provides a grooved wallboard, which is manufactured using the grooved wallboard manufacturing method provided in the above embodiment.
[0061] The grooved wallboard provided in this embodiment has high groove opening accuracy, no paint accumulation in the grooves, low cost and high aesthetics.
[0062] In summary, the present invention provides a method for manufacturing a grooved wallboard, which comprises the following steps:
[0063] S100: using an extruder to extrude the premixed slurry into a substrate;
[0064] S200: rolling paint on the surface of the substrate and curing the paint to form a surface primer layer on the surface of the substrate;
[0065] S300: grooves are engraved on the side of the substrate coated with a surface primer layer;
[0066] S400: Apply groove primer in the groove using a soft roller;
[0067] S500: using a digital device to print on the surface of the surface primer and the groove primer to form a topcoat layer, wherein the printing ink volume of the digital device is 5-15g / m2 and the printing speed is 10-20m / min;
[0068] S600: A protective layer is formed by coating the surface of the substrate having the surface primer layer using a coating hard roller.
[0069] The grooved wallboard manufacturing method provided in the present application adopts the method of first applying a surface primer, then opening grooves, and inkjet forming the wallboard in the grooves in combination with digital printing, thereby avoiding paint accumulation in the grooves, saving costs, and improving operating efficiency and the aesthetics of the finished product.
[0070] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A method for manufacturing a grooved wallboard, characterized in that: include: The premixed slurry is extruded by an extruder to form a substrate; In a dust-free environment, rolling paint on the surface of the substrate, and curing the paint to form a surface primer layer on the surface of the substrate; Carving a groove on the side of the substrate coated with the surface primer layer; Applying a groove primer in the groove using a soft roller; Using a digital device to print on the surface of the surface primer and the groove primer to form a topcoat layer, wherein the printing ink amount of the digital device is 5-15g / m2 and the printing speed is 10-20m / min; A protective layer is formed by coating the surface of the substrate having the surface primer layer with a coating hard roller.
2. The method for manufacturing a grooved wallboard according to claim 1, characterized in that: Before the premixed slurry is extruded by an extruder to form a substrate, the method further comprises: Mixing resin, filler, chain extender, lubricant, and plasticizer to form a mixed liquid; The mixed solution is fully stirred to form the premixed slurry.
3. The method for manufacturing a grooved wallboard according to claim 2, characterized in that: The ratio of the resin, filler, chain extender, lubricant and plasticizer is (2-2.5):(7-8):(1-5):(0.1-0.5):(1-5).
4. The method for manufacturing a grooved wallboard according to claim 1, characterized in that: In the dust-free environment, before rolling the primer on the surface of the substrate and curing the primer, the method further comprises: The substrate is subjected to sanding treatment.
5. The method for manufacturing a grooved wallboard according to claim 4, characterized in that: The sanding treatment of the substrate comprises: A plurality of sandpapers are used to polish the surface of the substrate in sequence according to a preset sequence, wherein the mesh sizes of the plurality of sandpapers are increased in sequence according to the preset sequence, and the mesh sizes of the plurality of sandpapers are 120-320.
6. The method for manufacturing a grooved wallboard according to claim 1, characterized in that: The method of rolling paint on the surface of the substrate in a dust-free environment and curing the paint to form a surface primer layer on the surface of the substrate comprises: The base material is coated with primer by roller coating for 2-3 times, and each coat of oil needs to be cured with UV lamp, and the coating amount is 20-40g / m2.
7. The method for manufacturing a grooved wallboard according to claim 1, characterized in that: Before engraving the groove on the side of the substrate coated with the primer, the method further comprises: The substrate is first separated and chamfered after being coated with a surface primer.
8. The method for manufacturing a grooved wallboard according to claim 1, characterized in that: The method of applying the groove primer in the groove by using a soft roller comprises: The substrate is coated with a 20-30° soft roller, with a coating amount of 6-12 g / m2. After coating, a UV lamp is used for curing, and the UV lamp curing energy is 150-400 mj / cm2.
9. The method for manufacturing a grooved wallboard according to claim 1, characterized in that: The method of forming a protective layer by coating the surface of the substrate having a surface primer layer with a coating hard roller comprises: Use a coating hard roller to coat the printed substrate with a coating amount of 10-20g / m 2 .
10. The method for manufacturing a grooved wallboard according to claim 1, characterized in that: The groove is engraved on the side of the substrate coated with the primer, the groove depth is 0.3-1mm, and the groove width is 0.5-5mm.