UV photocuring water-based waterproof coating and preparation method thereof
UV photocured water-based coatings prepared through specific ratios and stirring methods solve the problem of poor water-resistant boiling performance of UV cured water-based coatings in the prior art, improve the physical and chemical properties and environmental protection of the coatings, and achieve wide application prospects.
Patent Information
- Application Number
- CN202411009535.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-11-22
AI Technical Summary
Existing UV cured water-based coatings are difficult to effectively overcome the water-based boiling resistance, which seriously affects their physical and chemical properties.
15 to 25 parts of water-emulsifying reaction polyurethane acrylate, 20 to 30 parts of oily polyurethane acrylate, 1 to 3 parts of photoinitiator, 0.5 to 1 part of wetting additive, 0.3 to 0.5 parts of defoaming additive and 35 are used. ~50 parts of deionized water, UV photocurable water-resistant coating is prepared by specific stirring and dropping methods to ensure that the molecular structure contains acrylic groups and carboxylate salts, and improve the weather resistance and optical properties of the coating.
It realizes good wear resistance, adhesion, weather resistance and optical properties of UV light-cured water-based coatings, overcomes the problem of poor water-based boiling resistance, improves the adhesion, flexibility and solvent resistance of the coatings, and avoids environmental pollution. , meets market demand.
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of photocurable coatings, and in particular relates to a UV photocurable water-based water-resistant coating and a preparation method thereof. Background Art
[0002] Photocurable coatings use ultraviolet light as the energy source for coating curing. They are mainly composed of photosensitive resins, photosensitizers (photoinitiators) and diluents. At the same time, some additives are added, such as heat stabilizers. Pigments and fillers are added when preparing color paints. Traditional photocurable coatings are mainly organic solvents, which will release a large amount of volatile organic compounds (VOCs) during use, threatening human life and health and causing environmental pollution. In order to reduce environmental pollution, UV-curable water-based coatings that use water as a solvent and introduce hydrophilic groups such as carboxyl and sulfonic acid groups on the WPU macromolecular chain are currently used. UV-curable water-based coatings combine the advantages of water-based coatings and photocurable coatings. They can use relatively high molecular weight polymers to improve adhesion to certain substrates (such as metals) and improve other physical properties of the cured film. They can avoid shrinkage caused by active diluent monomers and obtain extremely thin coatings. However, the high viscosity of the organic phase can easily lead to problems such as difficulty in emulsion dispersion and low solid content, which greatly limits the promotion and application of UV-curable waterborne polyurethane coatings.
[0003] There are studies on the existing problems of UV curing waterborne coatings in the prior art, such as patent application CN117511375A - a UV curing waterborne polyurethane coating and its preparation method, which uses alkaline waterborne polyurethane emulsion as the main material to make the UV curing waterborne polyurethane coating have strong adhesion and good water resistance, solving the problems of difficult emulsion dispersion and low solid content in the current UV curing waterborne coatings. However, the existing UV curing waterborne coatings can only guarantee their application scope, but it is difficult to effectively overcome their water-based boiling resistance, which seriously affects the physical and chemical properties of UV curing waterborne coatings. Therefore, a new technical solution is needed to solve the above technical problems. Summary of the invention
[0004] The purpose of the present invention is to provide a UV light-cured water-based water-resistant coating and a preparation method to solve the problem that the current UV-cured water-based coating is difficult to effectively overcome the water-based boiling resistance, thereby seriously affecting the physical and chemical properties of the UV-cured water-based coating.
[0005] To achieve the above object, the present invention provides the following technical scheme: a method for preparing a UV light-curable water-based water-resistant coating, wherein the raw material components of the UV light-curable water-based water-resistant coating include, by weight: 15 to 25 parts of water-emulsifiable reactive polyurethane acrylate, 20 to 30 parts of oily polyurethane acrylate, 1 to 3 parts of photoinitiator, 0.5 to 1 part of wetting aid, 0.3 to 0.5 parts of defoaming aid, 0.3 to 0.8 parts of thickening aid and 35 to 50 parts of deionized water, wherein the molecular structure of the water-emulsifiable reactive polyurethane acrylate contains propylene group and carboxylate; The specific preparation steps for preparing the UV light-curing water-based water-resistant coating according to the above raw material components are as follows: firstly, water-emulsifiable reactive polyurethane acrylate, oily polyurethane acrylate, photoinitiator, wetting aid, defoaming aid and thickening aid are stirred and mixed at a temperature of 50-60° C. and a rotation speed of 800-1000 rpm for 10-30 minutes, then deionized water is uniformly added dropwise at a rotation speed of 1500-2000 rpm for 10-30 minutes for emulsification, and then emulsified and stirred at a rotation speed of 800-1000 rpm for 20-30 minutes to obtain the UV light-curing water-based water-resistant coating, wherein the water-emulsifiable reactive polyurethane acrylate is RPCUREEM001, and the oily polyurethane acrylate is RPCURE 40520, RPCURE 40160, one or more of TMPTA, HDDA, PETA, and DPHA, the photoinitiator is one or more of 1-hydroxy-cyclohexyl benzophenone, benzophenone, and diphenyl (2,4,6-trimethylbenzoyl) phosphine oxide, the wetting aid is a polyether siloxane copolymer, the defoaming aid is a mixture of one or two of modified polysiloxane or modified polyacrylic acid polymer, and the thickening aid is a polyether polyurethane associative rheological aid.
[0006] The UV light-curing water-based water-resistant coating is prepared by adopting the preparation method of the UV light-curing water-based water-resistant coating.
[0007] Compared with the prior art, the present invention has the following beneficial effects: 1. The present invention adopts a water-emulsifiable reactive polyurethane acrylate containing an propylene group and a carboxylate in its molecular structure, so that the water-emulsifiable reactive polyurethane acrylate makes up for the shortcomings of a single polyurethane aqueous emulsion, namely, poor weather resistance and poor light retention of the film, thereby making the UV light-curing water-based water-resistant coating have good abrasion resistance, adhesion, weather resistance and optical properties, and also makes the UV light-curing water-based water-resistant coating achieve good leveling and appearance in the absence of an acrylic acid monomer, thereby making the UV light-curing water-based water-resistant coating have excellent physical and chemical properties and avoiding The use of organic solvents causes environmental pollution. The problem of poor water-based boiling resistance at high temperature for a long time is overcome by uniformly dropping emulsification, so that the adhesion of the UV light-curing water-based water-resistant coating can reach 5B after 2-4 hours of boiling at 100°C. At the same time, the fullness, flexibility and solvent resistance of the UV light-curing water-based water-resistant coating are effectively improved, so that the UV light-curing water-based water-resistant coating can achieve the performance of UV solvent-based varnish and achieve the purpose of environmental protection, which can better meet the needs of the market and has broad application prospects. 2. The present invention adopts self-made RPCURE EM001 as water-emulsifiable reactive polyurethane acrylate, so that the water-emulsifiable reactive polyurethane acrylate can not only make up for the shortcomings of a single polyurethane aqueous emulsion, but also improve the leveling and appearance of the UV light-curing water-based water-resistant coating in the absence of acrylic monomers, effectively avoiding the problem of environmental pollution caused by the use of organic solvents, and also effectively overcoming the problem of poor water boiling resistance under long-term high temperature, so that the UV light-curing water-based water-resistant coating can better meet the needs of the market and has broad application prospects; 3. The present invention makes the preparation process of UV light-curing water-based water-resistant coating simpler, the reaction more gentle, and the operability stronger by stirring and mixing and emulsifying under low temperature conditions, thereby effectively reducing the production cost and improving the effect and efficiency of the preparation of UV light-curing water-based water-resistant coating, thereby ensuring the mass production of UV light-curing water-based water-resistant coating. DETAILED DESCRIPTION
[0008] The following examples are used to further illustrate the content of the present invention, but do not limit the application of the present invention. Embodiment 1:
[0009] This embodiment provides a UV light-cured water-based water-resistant coating, and the preparation method thereof comprises the following steps: First, weigh 20 parts of RPCURE EM001 (RPCURE EM001 is prepared by Jiangsu Ruipu Resin Technology Co., Ltd.) as water-emulsifiable reactive polyurethane acrylate, 30 parts of RPCURE 40520 (RPCURE 40520 is prepared by Jiangsu Ruipu Resin Technology Co., Ltd.) as oily polyurethane acrylate, 3 parts of diphenyl (2,4,6-trimethylbenzoyl) phosphine oxide as a photoinitiator, 1 part of polyether siloxane copolymer as a wetting aid, 0.5 parts of modified polysiloxane as a defoaming aid, and 0.5 parts of polyether polyurethane associative rheological aid as a thickening aid. The above parts are all weight parts; Secondly, 20 parts of RPCURE EM001, 30 parts of RPCURE 40520, 3 parts of diphenyl (2,4,6-trimethylbenzoyl) phosphine oxide, 1 part of polyether siloxane copolymer, 0.5 parts of modified polysiloxane, and 0.5 parts of polyether polyurethane associative rheological additive were added to the reactor in sequence, heated to 53°C, and stirred and mixed at 800 rpm for 15 minutes; Next, after the rotation speed is increased to 2000 rpm, 45 parts of deionized water are uniformly added dropwise for emulsification, wherein the addition time of 45 parts of deionized water is 30 minutes; Then, the rotation speed is reduced to 800 rpm and stirred for 30 minutes to obtain a UV light-cured water-based water-resistant coating; Finally, the prepared UV light-cured water-based water-resistant coating was sprayed on the sample plastic sheet, and the spray atomization was kept good during the spraying process. The wet film thickness was about 25-30 μm. The sprayed sample was placed at 60 ° C and baked for 8-10 minutes, and cured under the light of a high-pressure mercury lamp. The curing energy was not less than 500 mj / cm 2 The glossiness was measured by a three-angle gloss meter and was 101.5°. The sprayed samples were boiled in a 100°C water bath for 2h and 4h respectively, and then the adhesion performance was tested by the hundred grid method, which all reached 5B (5B means the boiling performance passed, otherwise the boiling performance failed). The flexibility was tested by the cylindrical bending method and was <2mm. Acetone was used to rub the coating on the sprayed sample, and the number of friction resistance was >500 times. The pencil hardness of the cured coating was measured by the national standard GB / T6739-1996 method (the hardness grade range is 6B~HB~6H, where 6H is the hardest and 6B is the softest) and was F. Embodiment 2:
[0010] This embodiment provides a UV light-cured water-based water-resistant coating, and the preparation method thereof comprises the following steps: First, weigh 20 parts of RPCURE EM001 as water-emulsifiable reactive polyurethane acrylate, 15 parts of RPCURE40520 and 15 parts of DPHA (dipentaerythritol hexaacrylate) as oily polyurethane acrylate, 3 parts of benzophenone as photoinitiator, 1 part of polyether siloxane copolymer as wetting aid, 0.5 parts of modified polysiloxane as defoaming aid, and 0.3 parts of polyether polyurethane associative rheological aid as thickening aid, and the above parts are all by mass; Secondly, 20 parts of RPCURE EM001, 15 parts of RPCURE 40520, 15 parts of DPHA, 3 parts of benzophenone, 1 part of polyether siloxane copolymer, 0.5 parts of modified polysiloxane, and 0.3 parts of polyether polyurethane associative rheological additive were added to the reactor in sequence, heated to 53°C, and stirred and mixed at 800 rpm for 15 minutes; Next, after the rotation speed is increased to 1800 rpm, 45.2 parts of deionized water are uniformly added dropwise for emulsification, wherein the addition time of 45.2 parts of deionized water is 20 minutes; Then, the rotation speed is reduced to 800 rpm and stirred for 30 minutes to obtain a UV light-cured water-based water-resistant coating; Finally, the prepared UV light-cured water-based water-resistant coating was sprayed on the sample plastic sheet, and the spray atomization was kept good during the spraying process. The wet film thickness was about 25-30 μm. The sprayed sample was placed at 60 ° C and baked for 8-10 minutes, and cured under the light of a high-pressure mercury lamp. The curing energy was not less than 500 mj / cm 2 The glossiness was measured by a three-angle gloss meter and was 99.6°. The sprayed samples were boiled in a 100°C water bath for 2h and 4h respectively, and then the adhesion performance was tested by the hundred grid method, which all reached 5B (5B means the boiling performance passed, otherwise the boiling performance failed). The flexibility was tested by the cylindrical bending method and was 4mm. Acetone was used to rub the coating on the sprayed sample, and the number of friction resistance was >500 times. The pencil hardness of the cured coating was measured by the national standard GB / T6739-1996 method (the hardness grade range is 6B~HB~6H, where 6H is the hardest and 6B is the softest) and was H. Embodiment 3:
[0011] This embodiment provides a UV light-cured water-based water-resistant coating, and the preparation method thereof comprises the following steps: First, weigh 25 parts of RPCURE EM001 as water-emulsifiable reactive polyurethane acrylate, 20 parts of RPCURE40520 and 10 parts of RPCURE 40160 (RPCURE 40160 is prepared by Jiangsu Ruipu Resin Technology Co., Ltd.) as oily polyurethane acrylate, 2 parts of 1-hydroxy-cyclohexyl benzophenone as a photoinitiator, 1 part of polyether siloxane copolymer as a wetting aid, 0.5 parts of modified polysiloxane as a defoaming aid, and 0.8 parts of polyether polyurethane associative rheological additive as a thickening aid. The above parts are all by mass. Secondly, 25 parts of RPCURE EM001, 20 parts of RPCURE 40520, 10 parts of RPCURE40160, 2 parts of 1-hydroxy-cyclohexyl benzophenone, 1 part of polyether siloxane copolymer, 0.5 parts of modified polysiloxane, and 0.8 parts of polyether polyurethane associative rheological additive were added to the reactor in sequence, heated to 53°C, and stirred and mixed at a speed of 1000 rpm for 20 minutes; Next, after the rotation speed is increased to 1500 rpm, 40.7 parts of deionized water are uniformly added dropwise for emulsification, wherein the addition time of 40.7 parts of deionized water is 25 minutes; Then, the rotation speed is reduced to 800 rpm and stirred for 30 minutes to obtain a UV light-cured water-based water-resistant coating; Finally, the prepared UV light-cured water-based water-resistant coating was sprayed on the sample plastic sheet, and the spray atomization was kept good during the spraying process. The wet film thickness was about 25-30 μm. The sprayed sample was placed at 60 ° C and baked for 8-10 minutes, and cured under the light of a high-pressure mercury lamp. The curing energy was not less than 500 mj / cm 2 The glossiness was measured by a three-angle gloss meter and was 100.4°. The sprayed samples were boiled in a 100°C water bath for 2h and 4h respectively, and then the adhesion performance was tested by the hundred grid method, which all reached 5B (5B means the boiling performance passed, otherwise the boiling performance failed). The flexibility was tested by the cylindrical bending method and was 6mm. Acetone was used to rub the coating on the sprayed sample, and the number of friction resistance was >500 times. The pencil hardness of the cured coating was measured by the national standard GB / T6739-1996 method (the hardness grade range is 6B~HB~6H, where 6H is the hardest and 6B is the softest) and was H.
[0012] Comparative Example 1: The UV light-curable water-based coating in this embodiment adopts conventional raw material components, to which a solvent (such as ethylene glycol butyl ether and diethylene glycol butyl ether) is added in a mass percentage of 1-5%; the prepared UV light-curable water-resistant coating is then sprayed on the sample plastic plate, and the spray atomization is maintained well during the spraying, and the wet film thickness is about 25-30 μm. The sprayed sample is placed at 60°C and baked for 8-10 minutes, and cured under the light of a high-pressure mercury lamp, and the curing energy is not less than 500mj / cm 2 The glossiness was measured by a three-angle gloss meter and was 101.3°. The sprayed sample was boiled in a 100°C water bath for 2 hours, and severe bubbling occurred in 5 minutes. The flexibility was tested by the cylindrical bending method and was 12 mm. Acetone was used to rub the coating on the sprayed sample, and the friction resistance was >500 times. The pencil hardness of the cured coating was measured by the national standard GB / T6739-1996 method (the hardness grade range is 6B~HB~6H, where 6H is the hardest and 6B is the softest) and was H.
[0013] The following is a performance comparison table of Examples 1-3 and Comparative Example 1: ; It can be seen from the above table that the UV light-cured water-based water-resistant coatings prepared by Examples 1-3 have excellent physical and chemical properties, excellent water resistance, good solvent resistance, and good flexibility, and overcome the disadvantage of poor water-based boiling resistance, so that the UV light-cured water-based water-resistant coating can reach an adhesion of 5B after boiling for 2 to 4 hours at 100°C, so that the UV light-cured water-based water-resistant coating can achieve the performance of UV solvent-based varnish and achieve the purpose of environmental protection, can better meet the needs of the market, and has broad application prospects.
Claims
1. A method for preparing a UV light-cured water-based water-resistant coating, characterized in that: The specific preparation steps are as follows: firstly, water-emulsifiable reactive polyurethane acrylate, oily polyurethane acrylate, photoinitiator, wetting aid, defoaming aid and thickening aid are stirred and mixed, then deionized water is added dropwise at a uniform speed for emulsification, and after emulsification and stirring, a UV light-cured water-based water-resistant coating is obtained, wherein the molecular structure of the water-emulsifiable reactive polyurethane acrylate contains an propylene group and a carboxylate.
2. The method for preparing a UV light-curable water-based water-resistant coating according to claim 1, characterized in that: The raw material components of the UV light-curing water-based water-resistant coating include, by mass, 15 to 25 parts of water-emulsifiable reactive polyurethane acrylate, 20 to 30 parts of oily polyurethane acrylate, 1 to 3 parts of photoinitiator, 0.5 to 1 part of wetting aid, 0.3 to 0.5 part of defoaming aid, 0.3 to 0.8 part of thickening aid and 35 to 50 parts of deionized water.
3. The method for preparing a UV light-curable water-based water-resistant coating according to claim 1 or 2, characterized in that: The water-emulsifiable reactive polyurethane acrylate is RPCURE EM001.
4. The method for preparing a UV light-curable water-based water-resistant coating according to claim 1 or 2, characterized in that: The oily polyurethane acrylate is one or more of RPCURE 40520, RPCURE 40160, TMPTA, HDDA, PETA and DPHA.
5. The method for preparing a UV light-curable water-based water-resistant coating according to claim 1 or 2, characterized in that: The photoinitiator is one or more of 1-hydroxy-cyclohexyl benzophenone, benzophenone, and diphenyl (2,4,6-trimethylbenzoyl) phosphine oxide.
6. A method for preparing a UV light-curable water-based water-resistant coating according to claim 1 or 2, characterized in that: The wetting aid is a polyether siloxane copolymer.
7. The method for preparing a UV light-curable water-based water-resistant coating according to claim 1 or 2, characterized in that: The defoaming aid is one of modified polysiloxane and modified polyacrylic acid polymer or a mixture of the two.
8. The method for preparing a UV light-curable water-based water-resistant coating according to claim 1 or 2, characterized in that: The thickening aid is a polyether polyurethane associative rheological aid.
9. The method for preparing a UV light-curable water-based water-resistant coating according to claim 1, characterized in that: The stirring and mixing temperature is 50-60°C, the stirring and mixing time is 10-30 minutes, and the stirring and mixing speed is 800-1000rpm; the stirring speed of the uniform dripping is 1500-2000rpm, and the uniform dripping time is 10-30 minutes; the emulsification stirring speed is 800-1000rpm, and the emulsification stirring time is 20-30 minutes.
10. A UV light-cured water-based water-resistant coating, characterized in that: The coating is prepared by the method for preparing a UV light-cured water-based water-resistant coating as described in claim 1, 2 or 9.
Citation Information
Patent Citations
UV-curable waterborne polyurethane coating and preparation method thereof
CN117511375A
Preparation method for cationic photo-curable water-based polyurethane emulsifier
CN110724247A
Water-based self-luminous elastic coating, and preparation method and application thereof
CN110791190A
Water-emulsifiable UV light-cured anionic resin and preparation method thereof
CN113736064A
Emulsifier capable of being subjected to UV light curing as well as preparation method and application of emulsifier
CN116410461A
Cited By
Water-based UV (ultraviolet) photocuring coating material and resin for preparing water-based UV photocuring coating material
CN119859468A