Monitoring and fixing device used during meltallizing of generic semiconductor parts

By using robotic arms and infrared structures to monitor coating parameters in real time during the melting process of pan-semiconductor components, and using the fixing mechanism of clamping and springs to stabilize the clamping of parts, the problems of inaccurate monitoring technology and part movement are solved, achieving high Quality coating and safe production.

CN118996316AActive Publication Date: 2024-11-22ANHUI FULLERDE TECH DEV CO LTD

Patent Information

Application Number
CN202411143742.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-20
Publication Date
2024-11-22
Estimated Expiration
2044-08-20

AI Technical Summary

Technical Problem

In the prior art, monitoring technology during the melting process of the pan-semiconductor parts cannot reflect the real situation of the coating surface in real time and accurately, resulting in uneven coating and unstable quality, and the parts are prone to move or fall off during the melting process, affecting the Equipment safety and production efficiency.

Method used

A monitoring fixture including a robotic arm, infrared structure and fixing mechanism is designed. The coating roughness and thickness are monitored in real time by controlling the molten metal wire and infrared structure. The fixing mechanism uses clamps and springs to achieve stable clamping of parts. , ensure uniform deposition of coatings and safe equipment.

Benefits of technology

Real-time online monitoring and detection of coating parameters is realized to ensure that it is within a predetermined range, improve coating quality and production efficiency, avoid coating uneven coating and equipment damage, and ensure safety at the production site.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118996316A_ABST
    Figure CN118996316A_ABST
Patent Text Reader

Abstract

The invention discloses a monitoring and fixing device during meltallizing of a generic semiconductor part, and relates to the technical field of part meltallizing, the monitoring and fixing device comprises a monitoring mechanism and a fixing mechanism, the monitoring mechanism further comprises a mechanical arm, a meltallizing metal wire is arranged in the top end of the mechanical arm, and the front end of the mechanical arm is fixedly connected with a spraying tail end structure; the top end of the mechanical arm is fixedly connected with an infrared structure, and the meltallizing metal wire, the infrared structure and the spraying tail end structure are used for meltallizing the surface of a part and detecting parameters such as roughness and thickness of a meltallizing coating. By means of the mechanical arm, the meltallizing metal wire, the infrared structure and the spraying tail end structure, the effect of monitoring and detecting parameters such as roughness and thickness of a meltallizing coating on line in real time is achieved, the detection result is fed back to a control system of the meltallizing machine in real time, corresponding adjustment is made, and needed meltallizing parameters are met. And real-time monitoring and detection are carried out, so that the roughness, thickness and other parameters of the coating can be always kept in a preset range.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of parts spraying, and in particular to a monitoring and fixing device for spraying pan-semiconductor parts. Background Art

[0002] The surface of the components in the pan-semiconductor cavity is treated by spraying, mainly to improve the corrosion resistance, wear resistance, hardness and other properties of the components, so as to adapt to the extreme environment of high temperature and strong corrosion in the semiconductor manufacturing process, thereby improving the service life and performance of the parts. Spraying technology, also known as thermal spraying technology, is a process that heats the material to a molten or semi-molten state and sprays it onto the surface of the substrate through a high-speed airflow to form a coating.

[0003] In existing thermal spraying devices, the monitoring technology cannot accurately reflect the actual situation of the coating surface in real time, and may be interfered by environmental factors and produce errors, which will cause the coating surface to be uneven, affecting the aesthetics and overall quality of the coating. Moreover, if the surface roughness or thickness of the coating after thermal spraying does not meet the requirements, additional processing steps are required to correct these problems.

[0004] In order to solve the problem that the monitoring technology in the existing technology cannot reflect the real situation of the coating surface in real time and accurately, an infrared device is installed on the spraying device to meet the online real-time monitoring and detection of parameters such as the roughness and thickness of the sprayed coating, and the control system of the spraying machine is fed back in real time according to the detection results to make corresponding adjustments to meet the required spraying parameters.

[0005] However, in the process of spraying semiconductor parts, since most parts are placed in a certain place for spraying and are not fixed during spraying, the parts will move or rotate due to the force generated by the spraying during the spraying process, resulting in the spraying material not being evenly and stably deposited on the surface of the parts. Moreover, if the parts move violently or fall off during the spraying process, it may also damage the spraying equipment. Summary of the invention

[0006] The purpose of the present invention is to solve the shortcomings existing in the prior art, and a monitoring and fixing device for the melt spraying of pan-semiconductor components is proposed. The main problem it solves is that the monitoring technology in the prior art cannot reflect the actual situation of the coating surface in real time and accurately.

[0007] In order to achieve the above object, the present invention adopts the following technical solutions: A monitoring and fixing device for the spraying of pan-semiconductor parts, comprising a monitoring mechanism and a fixing mechanism, the monitoring mechanism also comprises a mechanical arm, a spraying wire is arranged inside the top of the mechanical arm, a spraying end structure is fixedly connected to the front end of the mechanical arm, an infrared structure is fixedly connected to the top of the mechanical arm, the spraying wire, the infrared structure and the spraying end structure are used to spray the surface of the parts and detect the roughness and thickness of the sprayed coating. Therefore, the adhesion between the coating and the substrate can be effectively improved by appropriately increasing the roughness of the coating, and the thickness of the coating directly affects its resistance to the external environment.

[0008] As a further improvement of the present invention, a transmission line is fixedly connected to one side of the mechanical arm away from the spraying end structure, a power control system is fixedly connected to one end of the transmission line away from the mechanical arm, a transmission system is rotatably provided at the middle of the top of the power control system, two transmission systems are provided, the other transmission system is rotatably connected to the top of the mechanical arm, the spraying metal wire is wound around the outer surfaces of the two transmission systems, and the bottom end of the mechanical arm is fixedly connected to the base 1. Thus, the effect of melting the metal material and spraying it can be achieved.

[0009] As a further improvement of the present invention, the fixing mechanism includes a fixing body, the bottom end of the fixing body is fixedly connected to the second base, the outer surface of the fixing body close to the mechanical arm is fixedly connected to a connecting column, the bottom end of the connecting column is fixedly connected to a horizontal clamping plate, two horizontal clamping plates are provided, and two vertical clamping plates are symmetrically provided in the middle of the two horizontal clamping plates. Therefore, the parts can be fixed by the horizontal clamping plate and the vertical clamping plate.

[0010] As a further improvement of the present invention, the bottom end of the horizontal clamping plate below is evenly fixedly connected with a plurality of telescopic rods 1, the bottom ends of the telescopic rods 1 are fixedly connected to the top of the base 2, the outside of the telescopic rods 1 is provided with a spring 1, the two ends of the spring 1 are respectively fixedly connected to the bottom end of the horizontal clamping plate below and the top of the base 2, and the fixed body is symmetrically fixedly connected to two connecting rods 1 on one side close to the mechanical arm. Thus, the parts can be automatically closed and fixed after being placed.

[0011] As a further improvement of the present invention, a wiping cotton is fixedly connected to the middle of the first connecting rod, two baffles are symmetrically fixedly connected to the two sides of the lower horizontal clamping plate, the two baffles are fixedly connected to the two springs and the two telescopic rods on the sides close to each other, and the two springs and the two telescopic rods on both sides are fixedly connected to the sides of the two vertical clamping plates at their ends away from the baffles. Thus, the wiping cotton can achieve a wiping effect on the surface of the parts.

[0012] As a further improvement of the present invention, the horizontal clamping plates are symmetrically provided with two horizontal grooves on one side close to each other, the vertical clamping plates are symmetrically provided with two longitudinal grooves on one side close to each other, the bottom ends of the vertical clamping plates are symmetrically fixed with two sliding blocks, the bottom ends of the horizontal clamping plates below are symmetrically provided with four sliding grooves, and the four sliding blocks are slidably connected inside the four sliding grooves, respectively. Thus, the parts can be clamped all around.

[0013] As a further improvement of the present invention, the side of the lower horizontal clamping plate away from the mechanical arm is symmetrically fixedly connected with two connecting rods 2, the middle of the connecting rods 2 is fixedly connected with a handle, and the bottom of the handle is fixedly connected with a round block, so that the user can pull the horizontal clamping plate downwards conveniently.

[0014] As a further improvement of the present invention, the middle part of the round block is rotatably connected with a clamping block, the middle part of the fixed body is symmetrically provided with two movable grooves, the two connecting rods are respectively arranged inside the two movable grooves, and a clamping groove is provided on the side of the fixed body away from the mechanical arm. This ensures that the clamping can be performed when the horizontal clamp is pulled to the bottom.

[0015] Compared with the prior art, the present invention has the following beneficial effects: 1. Through the robotic arm, the spraying wire, the infrared structure and the spraying end structure, the robotic arm controls the spraying end structure to align with the surface of the part. Then the infrared structure is used to accurately adjust the position of the spraying end structure, so that the spraying wire can accurately spray the surface of the part through the spraying end structure, which will achieve the effect of online real-time monitoring and detection of parameters such as roughness and thickness of the spraying coating, and feedback to the control system of the spraying machine in real time according to the test results, and make corresponding adjustments to meet the required spraying parameters. Real-time monitoring and detection can ensure that parameters such as roughness and thickness of the coating are always kept within the predetermined range, thereby avoiding instability in coating quality. Moreover, the real-time monitoring system can quickly feed back the test results to the control system, and the control system can immediately make corresponding adjustments based on the feedback information, thereby shortening the production cycle and improving production efficiency. Accurately controlling the thickness and roughness of the coating can also avoid material waste caused by excessively thick or thin coatings.

[0016] 2. Through the horizontal clamping plate, vertical clamping plate, spring 1 and spring 2, under the elastic action of telescopic rod 1 and spring 2, the horizontal clamping plate and the vertical clamping plate can be brought close to each other. When the part is located in the middle of the horizontal clamping plate and the vertical clamping plate, it will be clamped under the action of spring 1 and spring 2. Clamping the parts can prevent them from moving or deforming due to external forces during the spraying process, thereby ensuring that the coating can be deposited evenly and stably on the surface of the parts. This helps to avoid problems such as uneven coating thickness and excessive surface roughness, and improve the overall quality of the coating. In addition, clamping the parts can ensure their stability during the spraying process and reduce the adjustment time required due to part movement or deformation. This helps to improve production efficiency and shorten production cycles. Clamping parts can also prevent parts from flying out or other accidents due to loss of control during the spraying process. This helps to ensure the safety of the production site and protect the life and property of operators.

[0017] 3. After the parts are fixed by the horizontal and vertical clamps, the spring 1 is used to rebound so that the surface of the part that needs to be sprayed will contact the wiping cotton. At this time, the wiping cotton will wipe the surface of the part that needs to be sprayed. Cleaning the surface of the part is conducive to the fusion of metal powder with the surface of the part during the spraying process, forming a stronger metallurgical bond. This helps to improve the overall quality of the coating. In addition, the clean surface also helps the metal powder to be evenly distributed during the spraying process, forming a coating with uniform thickness and smooth surface, which helps to improve the overall quality and use effect of the coating. Spraying on a clean surface can more accurately control the spraying process parameters, such as spraying distance, spraying speed, and spraying temperature, which helps to achieve a more stable spraying process and improve production efficiency and product quality. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a schematic diagram of the structure of the present invention.

[0019] Figure 2 It is a structural schematic diagram of the present invention from another angle.

[0020] Figure 3 It is a schematic diagram of the structure of the monitoring mechanism in the present invention.

[0021] Figure 4 It is a structural schematic diagram of the fixing mechanism in the present invention.

[0022] Figure 5 It is a schematic diagram of the structure of the horizontal clamping plate, the vertical clamping plate and the baffle in the present invention.

[0023] Figure 6 It is a schematic structural diagram of the vertical clamping plate, the longitudinal groove and the sliding block in the present invention.

[0024] Figure 7It is a schematic structural diagram of the transverse clamping plate, the second connecting rod and the fixing block in the present invention.

[0025] In the figure: 100, monitoring mechanism; 101, transmission system; 102, power control system; 103, transmission line; 104, robotic arm; 105, spraying wire; 106, infrared structure; 107, spraying terminal structure; 108, base one; 200, fixing mechanism; 201, fixing body; 202, base two; 203, connecting column; 204, horizontal clamping plate; 205, vertical clamping plate; 206, wiping cotton; 207, connecting rod one; 208, telescopic rod one; 209, spring one; 210, baffle; 211, spring two; 212, telescopic rod two; 213, horizontal groove; 214, longitudinal groove; 215, sliding block; 216, sliding groove; 217, connecting rod two; 218, handle; 219, round block; 220, fixing block; 221, moving groove; 222, fixing groove. DETAILED DESCRIPTION

[0026] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the specific embodiments of the present invention are described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth to facilitate a full understanding of the present invention. However, the present invention can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the present invention, so the present invention is not limited by the specific implementation disclosed below.

[0027] It should be noted that when an element is referred to as being "fixed to" another element, it may be directly on the other element or there may be a central element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. The terms "vertical", "horizontal", "left", "right" and similar expressions used herein are for illustrative purposes only and do not represent the only implementation method.

[0028] like Figure 1-3As shown, the present invention provides a monitoring and fixing device for the melt spraying of pan-semiconductor parts, including a monitoring mechanism 100 and a fixing mechanism 200. The monitoring mechanism 100 also includes a robotic arm 104. A melt spraying wire 105 is arranged inside the top of the robotic arm 104. A spraying end structure 107 is fixedly connected to the front end of the robotic arm 104. An infrared structure 106 is fixedly connected to the top of the robotic arm 104. The melt spraying wire 105, the infrared structure 106 and the spraying end structure 107 are used to melt spray the surface of the part and detect parameters such as the roughness and thickness of the melt sprayed coating. A transmission line 103 is fixedly connected to one side of the mechanical arm 104 away from the spraying end structure 107, and a power control system 102 is fixedly connected to one end of the transmission line 103 away from the mechanical arm 104. A transmission system 101 is rotatably connected to the middle of the top of the power control system 102. Two transmission systems 101 are provided, and the other transmission system 101 is rotatably connected to the top of the mechanical arm 104. The spraying metal wire 105 is wound around the outer surface of the two transmission systems 101, and a base 108 is fixedly connected to the bottom of the mechanical arm 104. In this way, the parameters such as the roughness and thickness of the spraying coating can be monitored and detected online in real time, and the control system of the spraying machine is fed back in real time according to the detection results, so that corresponding adjustments can be made to meet the required spraying parameters.

[0029] like Figure 4-5 As shown, the fixing mechanism 200 includes a fixing body 201, the bottom end of the fixing body 201 is fixedly connected to a base 202, the outer surface of the fixing body 201 close to the mechanical arm 104 is fixedly connected to a connecting column 203, the bottom end of the connecting column 203 is fixedly connected to a horizontal clamping plate 204, two horizontal clamping plates 204 are provided, and two vertical clamping plates 205 are symmetrically provided in the middle of the two horizontal clamping plates 204. The bottom end of the lower horizontal clamping plate 204 is evenly fixedly connected to a plurality of telescopic rods 1 208, the bottom ends of the telescopic rods 1 208 are all fixedly connected to the top of the base 202, the outside of the telescopic rods 1 208 is all provided with a spring 1 209, the two ends of the spring 1 209 are respectively fixedly connected to the bottom end of the lower horizontal clamping plate 204 and the top of the base 202, and the side of the fixing body 201 close to the mechanical arm 104 is symmetrically fixedly connected to two connecting rods 1 207. The middle of the connecting rod 1 207 is fixedly connected with a wiping cotton 206, and two baffles 210 are symmetrically fixedly connected to the two sides of the lower horizontal clamping plate 204. The two baffles 210 are fixedly connected with spring 211 and telescopic rod 212 on the sides close to each other, and the ends of the spring 211 and telescopic rod 212 on both sides away from the baffle 210 are respectively fixedly connected to the sides of the two vertical clamping plates 205. Thus, the parts can be clamped by the elastic effect of the spring 1 209 and the spring 211, and the surface of the side of the part that needs to be sprayed can be cleaned.

[0030] like Figure 2-7As shown, two horizontal grooves 213 are symmetrically provided on the side where the horizontal clamps 204 are close to each other, and two longitudinal grooves 214 are symmetrically provided on the side where the vertical clamps 205 are close to each other. The bottom ends of the vertical clamps 205 are symmetrically fixedly connected with two sliding blocks 215. Four sliding grooves 216 are symmetrically provided at the bottom end of the lower horizontal clamp 204. The four sliding blocks 215 are respectively slidably connected inside the four sliding grooves 216. Two connecting rods 217 are symmetrically fixedly connected on the side of the lower horizontal clamp 204 away from the mechanical arm 104. A handle 218 is fixedly connected to the middle part of the connecting rod 217. A round block 219 is fixedly connected to the bottom end of the handle 218. A fixing block 220 is rotatably connected to the middle part of the round block 219. Two movable grooves 221 are symmetrically provided through the middle part of the fixed body 201. The two connecting rods 217 are respectively arranged inside the two movable grooves 221. A fixing groove 222 is provided on the side of the fixed body 201 away from the mechanical arm 104. Thereby, when the parts need to be placed, the horizontal clamping plate 204 will not rebound upward.

[0031] The effect achieved by the entire device is as follows: first, the operator pulls the handle 218 downward. Since the connecting rod 217 fixedly connected at both ends of the handle 218 is fixedly connected to the lower cross clamp 204, and since the connecting rod 217 is arranged inside the spring 211, the downward pulling of the handle 218 will cause the lower cross clamp 204 to move downward along the moving groove 221. Since the bottom end of the lower cross clamp 204 is fixedly connected with the telescopic rod 1 208 and the spring 1 209, at this time, the telescopic rod 1 208 will be telescoped and the spring 1 209 will be elastically deformed. When the cross clamp 204 moves to the bottom end, the fixing block 220 rotatably connected to the round block 219 fixedly connected to the bottom end of the handle 218 is controlled to rotate, so that the fixing block 220 rotates to a position where it is fixed with the fixing groove 222. At this time, the cross clamp 204 will not rebound under the fixing effect. When the spring 1 209 does not rebound during the clamping process, it means that the parts can be fixed more stably. This helps to reduce vibration or displacement caused by the rebound of spring 209, thereby improving the accuracy and stability of clamping.

[0032] Then, since the sliding blocks 215 fixedly connected to the bottom ends of the vertical clamping plates 205 are respectively slidably connected to the sliding grooves 216 opened at the top ends of the horizontal clamping plates 204, the operator can slide the vertical clamping plates 205 away from each other along the surface of the horizontal clamping plates 204. The movement of the vertical clamping plates 205 will cause the telescopic rod 212 to be telescoped and the spring 211 to be elastically deformed. At this time, the parts are placed in the slotted transverse grooves 213 at the top ends of the horizontal clamping plates 204, and then the vertical clamping plates 205 are released. At this time, the vertical clamping plates 205 will move toward the center under the effect of the rebound of the spring 211, so that the parts are moved by the longitudinal grooves opened on one side of the vertical clamping plates 205. The parts are fixed to the groove 214. When the parts are fixed, the clamping block 220 is rotated away from the clamping groove 222. At this time, the horizontal clamping plate 204 will move upward under the effect of the rebound of the spring 209. Since the parts are set to exit the surface state of the horizontal clamping plate 204, when the horizontal clamping plate 204 drives the parts to move upward, the surface of the parts that need to be sprayed will contact the wiping cotton 206 fixedly connected to the middle of the connecting rod 207, so that the effect of wiping the parts is achieved when the surface of the parts contacts the wiping cotton 206. Cleaning the surface of the parts is conducive to the fusion of the metal powder with the surface of the parts during the spraying process, forming a more solid metallurgical bond. This helps to improve the overall quality of the coating. In addition, the clean surface also helps the metal powder to be evenly distributed during the spraying process, forming a coating with uniform thickness and smooth surface, which helps to improve the overall quality and use effect of the coating.

[0033] When the parts collide with the slotted transverse groove 213 of the top transverse clamping plate 204 driven by the rebound of the transverse clamping plate 204, the parts will be fixed and clamped around to prevent them from moving or deforming due to external forces during the spraying process, thereby ensuring that the coating can be deposited evenly and stably on the surface of the parts. Finally, when the parts are completely clamped, the power control system 102 is started to transmit a signal to the mechanical arm 104 through the transmission line 103 so that the mechanical arm 104 moves to a suitable spraying position, and then the spraying metal wire 105 is heated, melted and sprayed through the spraying end structure 107, and the transmission system 101 is always started to push the spraying metal wire 105 forward, and then the surface of the parts is continuously detected through the infrared structure 106, so as to achieve the effect of online real-time monitoring and detection of parameters such as roughness and thickness of the spraying coating, and the control system of the spraying machine is fed back in real time according to the detection results, and corresponding adjustments are made to meet the required spraying parameters. Real-time monitoring and detection can ensure that parameters such as coating roughness and thickness always remain within the predetermined range, thereby avoiding unstable coating quality.

[0034] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A monitoring and fixing device for a pan-semiconductor component during thermal spraying, comprising a monitoring mechanism (100) and a fixing mechanism (200), characterized in that: The monitoring mechanism (100) further comprises a mechanical arm (104), a top end of which is internally provided with a spraying metal wire (105), a front end of which is fixedly connected to a spraying end structure (107), and a top end of which is fixedly connected to an infrared structure (106), wherein the spraying metal wire (105), the infrared structure (106) and the spraying end structure (107) are used to spray the surface of a part and detect parameters such as roughness and thickness of the sprayed coating.

2. A monitoring and fixing device for the melting and spraying of pan-semiconductor parts according to claim 1, characterized in that: A transmission line (103) is fixedly connected to one side of the robot arm (104) away from the spraying end structure (107), and a power control system (102) is fixedly connected to one end of the transmission line (103) away from the robot arm (104). A transmission system (101) is rotatably connected to the middle of the top of the power control system (102). Two transmission systems (101) are provided, and the other transmission system (101) is rotatably connected to the top of the robot arm (104). The sprayed metal wire (105) is wound around the outer surfaces of the two transmission systems (101), and the bottom end of the robot arm (104) is fixedly connected to a base 1 (108).

3. The monitoring and fixing device for the melt spraying of pan-semiconductor parts according to claim 1 is characterized in that: The fixing mechanism (200) comprises a fixing body (201), the bottom end of the fixing body (201) being fixedly connected to a second base (202), the outer surface of the fixing body (201) close to the mechanical arm (104) being fixedly connected to a connecting column (203), the bottom end of the connecting column (203) being fixedly connected to a horizontal clamping plate (204), two horizontal clamping plates (204) being provided, and two vertical clamping plates (205) being symmetrically provided in the middle of the two horizontal clamping plates (204).

4. The monitoring and fixing device for the melt spraying of pan-semiconductor parts according to claim 3 is characterized in that: The bottom end of the lower horizontal clamp (204) is evenly and fixedly connected to a plurality of telescopic rods (208), the bottom ends of the telescopic rods (208) are fixedly connected to the top of the base (202), the outside of the telescopic rods (208) is provided with springs (209), the two ends of the springs (209) are respectively fixedly connected to the bottom end of the lower horizontal clamp (204) and the top of the base (202), and the fixed body (201) is symmetrically fixedly connected to two connecting rods (207) on one side close to the mechanical arm (104).

5. The monitoring and fixing device for the melt spraying of pan-semiconductor parts according to claim 4 is characterized in that: A wiping cotton (206) is fixedly connected to the middle of the connecting rod 1 (207), and two baffles (210) are symmetrically fixedly connected to the two sides of the horizontal clamping plate (204) below. The two baffles (210) are fixedly connected to the sides close to each other with spring 2 (211) and telescopic rod 2 (212), and the ends of the spring 2 (211) and telescopic rod 2 (212) on both sides away from the baffle (210) are respectively fixedly connected to the sides of the two vertical clamping plates (205).

6. The monitoring and fixing device for the melt spraying of pan-semiconductor parts according to claim 5 is characterized in that: Two transverse grooves (213) are symmetrically provided on one side of the transverse clamping plate (204) close to each other, two longitudinal grooves (214) are symmetrically provided on one side of the vertical clamping plate (205) close to each other, two sliding blocks (215) are symmetrically fixedly connected to the bottom ends of the vertical clamping plates (205), and four sliding grooves (216) are symmetrically provided on the bottom end of the lower transverse clamping plate (204), and the four sliding blocks (215) are slidably connected to the inside of the four sliding grooves (216), respectively.

7. The monitoring and fixing device for the melt spraying of pan-semiconductor parts according to claim 6 is characterized in that: Two second connecting rods (217) are symmetrically fixedly connected to one side of the lower horizontal clamping plate (204) away from the mechanical arm (104), a handle (218) is fixedly connected to the middle of the second connecting rod (217), and a round block (219) is fixedly connected to the bottom end of the handle (218).

8. The monitoring and fixing device for the melt spraying of pan-semiconductor parts according to claim 7 is characterized in that: The middle part of the round block (219) is rotatably connected to a fixing block (220), the middle part of the fixed body (201) is symmetrically provided with two movable grooves (221), the two connecting rods (217) are respectively arranged inside the two movable grooves (221), and a fixing groove (222) is provided on a side of the fixed body (201) away from the robot arm (104).

Citation Information

Patent Citations

  • Thermal spraying equipment for empennage product

    CN116288117A

  • Automatic temperature measuring device in laser cladding process

    CN214621489U

  • Meltallizing rotating device

    CN217646712U

  • Rotary clamping mechanism for thermal spraying

    CN219385290U

  • Thermal spraying apparatus and thermal spraying system, and thermal spraying technique thereof

    US20190262854A1