Coating method for double-layer coating single-texture mobile phone rear cover with ceramic effect
By heating and curing on the back cover of the mobile phone and adding double-layer coating technology of nano-alumina and silicon carbide, the coating peeling problem in the existing technology is solved, the wear resistance and corrosion resistance are improved, and the ceramic effect and usage experience are improved. .
Patent Information
- Application Number
- CN202411035701.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-11-22
AI Technical Summary
The double-layer coating on the back cover of the existing mobile phone is prone to fall off after a long time of use, and the second coating has poor wear resistance and strength, which affects the user experience.
The coating method of the mobile phone back cover with single texture is adopted. The first layer is heated and cured to improve adhesion. The second layer of coating is added with nano alumina and silicon carbide, and the sputtering coating technology is used to make it The material is evenly attached, the two coatings are fused in the heating box, and finally polished.
The second coating is effectively prevented from falling off, strengthening the hardness, wear resistance and corrosion resistance of the coating, improving the ceramic effect, and ensuring the uniformity and adhesion of the coating.
Smart Images

Figure CN118996348A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of ceramic effect mobile phone back cover coating, in particular to a coating method for a double-layer coated single-textured ceramic effect mobile phone back cover. Background Art
[0002] Existing mobile phone back cover sheets are generally made of plastic. In order to make the texture of the mobile phone back cover sheet more colorful, the mobile phone back cover is usually coated.
[0003] At present, the double-layer coating and ceramic effect on the back cover of the mobile phone are all achieved through coating equipment. The first layer of coating is applied to the back cover of the mobile phone, and then the second layer of coating is applied after the coating is completed. However, the second layer of coating is currently directly coated on the surface of the first layer of coating. With the long-term use of the mobile phone, the second layer of coating on the back cover of the mobile phone is prone to fall off. The wear resistance and strength of the second layer of coating are relatively poor, which affects the user experience. For this reason, we propose a coating method for a double-layer coating single-texture ceramic effect mobile phone back cover. Summary of the invention
[0004] The purpose of the present invention is to provide a coating method for a double-layer coated single-textured ceramic effect mobile phone back cover to solve the problems raised in the above background technology.
[0005] To achieve the above object, the present invention provides the following technical solution: a coating method for a double-layer coated single-textured ceramic effect mobile phone back cover, the coating method for a double-layer coated single-textured ceramic effect mobile phone back cover comprising the following specific steps: S1. Preparation: Use anhydrous alcohol to wipe the back cover of the mobile phone to remove dust, oil and impurities attached to its surface; S2. Prepare the first layer of coating, select a coating material with a ceramic texture, and debug and calibrate the coating equipment to ensure uniformity and thickness control of the coating; S3, applying the first layer of coating, placing the back cover of the mobile phone on the coating equipment, ensuring the position is accurate, after adjusting the position of the back cover of the mobile phone, start the coating equipment, and use the sputtering coating method to make the coating material evenly adhere to the back cover of the mobile phone to form the first layer of coating; S4, curing of the first coating layer. Carefully place the back cover of the mobile phone after the first coating layer is placed in a heating box for heating to cure the first coating layer, which can effectively improve the adhesion and stability of the first coating layer. S5. Preparation for the second coating layer: Select a coating material with a ceramic texture, and mix nano-aluminum oxide and silicon carbide into the coating material and mix them evenly, which can effectively enhance the hardness, wear resistance and corrosion resistance of the coating and effectively improve the ceramic effect; S6, applying the second coating layer, placing the mobile phone back cover coated with the first coating layer on the coating equipment, adjusting the position of the mobile phone back cover, starting the coating equipment, and using the sputtering coating method to evenly attach the coating material to the mobile phone back cover to form the second coating layer; S7, the second coating layer is cured, the coated mobile phone back cover is placed in a heating box for heating and curing to ensure that the two coating layers are well fused; S8, grinding and polishing, remove the back cover of the mobile phone after curing, use a microscope to observe the uniformity, thickness, adhesion and appearance of the coating, and use grinding equipment to grind and polish it.
[0006] Preferably, the debugging and calibration of the coating equipment in S2 includes the following specific steps: S2.1. Check all parts of the coating equipment, such as spray gun, evaporation source, and rotating table, to ensure that all parts are in normal working condition without damage or looseness; S2.2. According to the coating material, the heating temperature of the coating equipment is set, and the evaporation source power is adjusted according to the evaporation characteristics of the material, which can effectively control the evaporation rate of the coating material; S2.3. Adjust the rotation speed of the rotating table to ensure that the back cover of the mobile phone can evenly receive the coating material during the coating process; S2.4. Turn on the vacuum pump and evacuate the coating chamber to achieve the required vacuum degree. Use a vacuum gauge to monitor the vacuum degree in the coating chamber in real time to ensure that the process requirements are met. During the evacuation process, check the sealing of the equipment to prevent air leakage from affecting the vacuum degree. S2.5. Move the spray gun of the coating equipment to a suitable position so that it maintains a proper distance and angle with the back cover of the mobile phone to ensure the uniformity of the coating. Control the spray amount of the coating material by adjusting the gas flow and liquid flow of the spray gun; S2.6. Before formal coating, select a sample for trial coating. After the trial coating, use a film thickness measuring instrument to check the coating thickness of the test-plated sample to determine whether it meets the requirements, and observe the coating uniformity of the sample through a microscope; S2.7. Based on the test plating results, if the coating thickness meets the requirements, formal coating will be carried out. If it does not meet the requirements, the evaporation source power, spray gun position, rotation rate, and the spray gun spray coating material spray amount will be readjusted, and the test plating operation will be carried out again until the test plating results meet the requirements.
[0007] Preferably, in S3, after the back cover of the mobile phone is fixed, the process parameters of the sputtering coating, such as sputtering power, sputtering time and working gas flow rate, are set, and according to the set parameters, the sputtering power supply is turned on to generate plasma on the surface of the target material, and the sputtered coating material particles fly to the surface of the back cover of the mobile phone. The working gas is ionized under the action of the electric field to form plasma, which promotes the sputtering and deposition of the coating material. At the same time, the rotating table rotates to ensure that the coating material is evenly attached to the back cover of the mobile phone.
[0008] Preferably, the working gas is argon.
[0009] Preferably, during the coating process, the display instrument on the equipment is observed to monitor the sputtering power, gas flow and vacuum degree in real time to ensure that they are stable near the set values to avoid affecting the normal coating. The coating condition of the back cover of the mobile phone is checked regularly to observe the uniformity and color changes of the coating. If any abnormality is found, stop and make adjustments in time.
[0010] Preferably, in S3, when the preset sputtering time is reached, the sputtering power supply and the working gas supply are turned off, and the equipment is allowed to cool naturally to avoid adverse effects of high temperature on the back cover and the coating of the mobile phone.
[0011] Preferably, when the back cover of the mobile phone is placed in the heating box for heating in S4 and S7, it is necessary to ensure that the back cover of the mobile phone is placed horizontally and has a certain distance between it and the placement bracket in the heating box to ensure uniform heat conduction.
[0012] Preferably, in S7, the coated back cover of the mobile phone is placed in a heating box for heating and curing, and the temperature of the heating box is set at 150°C-200°C.
[0013] Preferably, the time for heating and curing the back cover of the mobile phone in S7 is 8-16 minutes. After the curing time is over, the heating function of the heating box is turned off, and the back cover of the mobile phone is allowed to cool naturally in the heating box to avoid adverse effects on the coating quality due to rapid temperature changes.
[0014] Compared with the prior art, the present invention provides a coating method for a double-layer coated single-textured ceramic effect mobile phone back cover, which has the following beneficial effects: 1. The coating method of the double-layer coating single-texture ceramic effect mobile phone back cover, when performing the second layer coating, by adding nano alumina and silicon carbide to the second layer coating material, and mixing the added nano alumina and silicon carbide evenly, the hardness, wear resistance and corrosion resistance of the coating can be effectively enhanced, the ceramic effect can be improved, and by performing a curing treatment, it is ensured that the two layers of coating are well fused, and the second layer of coating is effectively prevented from falling off after long-term use.
[0015] 2. The coating method of the double-layer coated single-textured ceramic effect mobile phone back cover can make the coating material evenly adhere to the mobile phone back cover to form a coating by using a sputtering coating method, thereby improving the coating effect.
[0016] 3. For the coating method of the double-layer coated single-textured ceramic effect mobile phone back cover, after the curing time is over, the heating function of the heating box is turned off, and the mobile phone back cover is allowed to cool naturally in the heating box to avoid adverse effects on the coating quality due to rapid temperature changes. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a schematic diagram of the structure of the present invention; Figure 2 It is a schematic diagram of the structure of the present invention. DETAILED DESCRIPTION
[0018] like Figure 1-Figure 2 As shown, the present invention provides a technical solution: a coating method for a double-layer coated single-textured ceramic effect mobile phone back cover, the coating method for a double-layer coated single-textured ceramic effect mobile phone back cover comprises the following specific steps: S1. Preparation: Use anhydrous alcohol to wipe the back cover of the mobile phone to remove dust, oil and impurities attached to its surface; S2. Prepare the first layer of coating, select a coating material with a ceramic texture, and debug and calibrate the coating equipment to ensure uniformity and thickness control of the coating; S3, applying the first layer of coating, placing the back cover of the mobile phone on the coating equipment, ensuring the position is accurate, after adjusting the position of the back cover of the mobile phone, start the coating equipment, and use the sputtering coating method to make the coating material evenly adhere to the back cover of the mobile phone to form the first layer of coating; S4, curing of the first coating layer. Carefully place the back cover of the mobile phone after the first coating layer is placed in a heating box for heating to cure the first coating layer, which can effectively improve the adhesion and stability of the first coating layer. S5. Preparation for the second coating layer: Select a coating material with a ceramic texture, and mix nano-aluminum oxide and silicon carbide into the coating material and mix them evenly, which can effectively enhance the hardness, wear resistance and corrosion resistance of the coating and effectively improve the ceramic effect; S6, applying the second coating layer, placing the mobile phone back cover coated with the first coating layer on the coating equipment, adjusting the position of the mobile phone back cover, starting the coating equipment, and using the sputtering coating method to evenly attach the coating material to the mobile phone back cover to form the second coating layer; S7, the second coating layer is cured, the coated mobile phone back cover is placed in a heating box for heating and curing to ensure that the two coating layers are well fused; S8, grinding and polishing, remove the back cover of the mobile phone after curing, use a microscope to observe the uniformity, thickness, adhesion and appearance of the coating, and use grinding equipment to grind and polish it.
[0019] The commissioning and calibration of the coating equipment in S2 includes the following specific steps: S2.1. Check all parts of the coating equipment, such as spray gun, evaporation source, and rotating table, to ensure that all parts are in normal working condition without damage or looseness; S2.2. According to the coating material, the heating temperature of the coating equipment is set, and the evaporation source power is adjusted according to the evaporation characteristics of the material, which can effectively control the evaporation rate of the coating material; S2.3. Adjust the rotation speed of the rotating table to ensure that the back cover of the mobile phone can evenly receive the coating material during the coating process; S2.4. Turn on the vacuum pump and evacuate the coating chamber to achieve the required vacuum degree. Use a vacuum gauge to monitor the vacuum degree in the coating chamber in real time to ensure that the process requirements are met. During the evacuation process, check the sealing of the equipment to prevent air leakage from affecting the vacuum degree. S2.5. Move the spray gun of the coating equipment to a suitable position so that it maintains a proper distance and angle with the back cover of the mobile phone to ensure the uniformity of the coating. Control the spray amount of the coating material by adjusting the gas flow and liquid flow of the spray gun; S2.6. Before formal coating, select a sample for trial coating. After the trial coating, use a film thickness measuring instrument to check the coating thickness of the test-plated sample to determine whether it meets the requirements, and observe the coating uniformity of the sample through a microscope; S2.7. Based on the test plating results, if the coating thickness meets the requirements, formal coating will be carried out. If it does not meet the requirements, the evaporation source power, spray gun position, rotation rate, and the spray gun spray coating material spray amount will be readjusted, and the test plating operation will be carried out again until the test plating results meet the requirements.
[0020] In S3, after the back cover of the mobile phone is fixed, the process parameters of the sputtering coating are set, such as sputtering power, sputtering time and working gas flow rate. According to the set parameters, the sputtering power supply is turned on to generate plasma on the surface of the target material, and the sputtered coating material particles fly to the surface of the back cover of the mobile phone. The working gas is argon. The argon is ionized under the action of the electric field to form plasma, which promotes the sputtering and deposition of the coating material. At the same time, the rotating table rotates to ensure that the coating material is evenly attached to the back cover of the mobile phone.
[0021] During the coating process, observe the display instruments on the equipment, monitor the sputtering power, gas flow and vacuum degree in real time to ensure that they are stable near the set values to avoid affecting the normal coating. Regularly check the coating condition of the back cover of the mobile phone to observe the uniformity and color changes of the coating. If there is any abnormality, stop and make adjustments in time.
[0022] In S3, when the preset sputtering time is reached, the sputtering power supply and working gas supply are turned off, and the equipment is allowed to cool naturally to avoid adverse effects of high temperature on the back cover and coating of the mobile phone.
[0023] When placing the back cover of the mobile phone in the heating box for heating in S4 and S7, it is necessary to ensure that the back cover of the mobile phone is placed horizontally and has a certain distance between it and the placement bracket in the heating box to ensure uniform heat conduction.
[0024] In S7, the coated mobile phone back cover is placed in a heating box for heating and curing, and the temperature of the heating box is set at 150℃-200℃.
[0025] The heating and curing time of the back cover of the mobile phone in S7 is 8-16 minutes. After the curing time is over, the heating function of the heating box is turned off, and the back cover of the mobile phone is allowed to cool naturally in the heating box to avoid adverse effects on the coating quality due to rapid temperature changes.
[0026] The above generally describes the present invention in detail, but it is obvious to a person skilled in the art that some modifications or improvements can be made to the present invention. Therefore, modifications or improvements that do not depart from the spirit of the present invention are within the scope of protection of the present invention.
Claims
1. A coating method for a double-layer coated single-textured ceramic effect mobile phone back cover, characterized in that: The coating method of the double-layer coated single-textured ceramic effect mobile phone back cover comprises the following specific steps: S1. Preparation: Use anhydrous alcohol to wipe the back cover of the mobile phone to remove dust, oil and impurities attached to its surface; S2. Prepare the first layer of coating, select a coating material with a ceramic texture, and debug and calibrate the coating equipment to ensure uniformity and thickness control of the coating; S3, applying the first layer of coating, placing the back cover of the mobile phone on the coating equipment, ensuring the position is accurate, after adjusting the position of the back cover of the mobile phone, start the coating equipment, and use the sputtering coating method to make the coating material evenly adhere to the back cover of the mobile phone to form the first layer of coating; S4, curing of the first coating layer. Carefully place the back cover of the mobile phone after the first coating layer is placed in a heating box for heating to cure the first coating layer, which can effectively improve the adhesion and stability of the first coating layer. S5. Preparation for the second coating layer: Select a coating material with a ceramic texture, and mix nano-aluminum oxide and silicon carbide into the coating material and mix them evenly, which can effectively enhance the hardness, wear resistance and corrosion resistance of the coating and effectively improve the ceramic effect; S6, applying the second coating layer, placing the mobile phone back cover coated with the first coating layer on the coating equipment, adjusting the position of the mobile phone back cover, starting the coating equipment, and using the sputtering coating method to evenly attach the coating material to the mobile phone back cover to form the second coating layer; S7, the second coating layer is cured, the coated mobile phone back cover is placed in a heating box for heating and curing to ensure that the two coating layers are well fused; S8, grinding and polishing, remove the back cover of the mobile phone after curing, use a microscope to observe the uniformity, thickness, adhesion and appearance of the coating, and use grinding equipment to grind and polish it.
2. The coating method of a double-layer coated single-textured ceramic effect mobile phone back cover according to claim 1, characterized in that: The debugging and calibration of the coating equipment in S2 includes the following specific steps: S2.
1. Check all parts of the coating equipment, such as spray gun, evaporation source, and rotating table, to ensure that all parts are in normal working condition without damage or looseness; S2.
2. According to the coating material, the heating temperature of the coating equipment is set, and the evaporation source power is adjusted according to the evaporation characteristics of the material, which can effectively control the evaporation rate of the coating material; S2.
3. Adjust the rotation speed of the rotating table to ensure that the back cover of the mobile phone can evenly receive the coating material during the coating process; S2.
4. Turn on the vacuum pump and evacuate the coating chamber to achieve the required vacuum degree. Use a vacuum gauge to monitor the vacuum degree in the coating chamber in real time to ensure that the process requirements are met. During the evacuation process, check the sealing of the equipment to prevent air leakage from affecting the vacuum degree. S2.
5. Move the spray gun of the coating equipment to a suitable position so that it maintains a proper distance and angle with the back cover of the mobile phone to ensure the uniformity of the coating. Control the spray amount of the coating material by adjusting the gas flow and liquid flow of the spray gun; S2.
6. Before formal coating, select a sample for trial coating. After the trial coating, use a film thickness measuring instrument to check the coating thickness of the test-plated sample to determine whether it meets the requirements, and observe the coating uniformity of the sample through a microscope; S2.
7. Based on the test plating results, if the coating thickness meets the requirements, formal coating will be carried out. If it does not meet the requirements, the evaporation source power, spray gun position, rotation rate, and the spray gun spray coating material spray amount will be readjusted, and the test plating operation will be carried out again until the test plating results meet the requirements.
3. The coating method of a double-layer coated single-textured ceramic effect mobile phone back cover according to claim 1, characterized in that: In the step S3, after the back cover of the mobile phone is fixed, the process parameters of the sputtering coating are set, such as the sputtering power, the sputtering time and the working gas flow rate. According to the set parameters, the sputtering power supply is turned on to generate plasma on the surface of the target material. The sputtered coating material particles fly to the surface of the back cover of the mobile phone. The working gas is ionized under the action of the electric field to form plasma, which promotes the sputtering and deposition of the coating material. At the same time, the rotating table rotates to ensure that the coating material is evenly attached to the back cover of the mobile phone.
4. The coating method of a double-layer coated single-textured ceramic effect mobile phone back cover according to claim 3, characterized in that: The working gas is argon.
5. The coating method of a double-layer coated single-textured ceramic effect mobile phone back cover according to claim 3, characterized in that: During the coating process, observe the display instruments on the equipment, monitor the sputtering power, gas flow and vacuum degree in real time to ensure that they are stable near the set values to avoid affecting the normal coating. Regularly check the coating condition of the back cover of the mobile phone to observe the uniformity and color changes of the coating. If there is any abnormality, stop and make adjustments in time.
6. The coating method of a double-layer coated single-textured ceramic effect mobile phone back cover according to claim 3, characterized in that: In the above-mentioned S3, when the preset sputtering time is reached, the sputtering power supply and the working gas supply are turned off, and the equipment is allowed to cool down naturally to avoid adverse effects of high temperature on the back cover and the coating of the mobile phone.
7. The coating method of a double-layer coated single-textured ceramic effect mobile phone back cover according to claim 1, characterized in that: When the back cover of the mobile phone is placed in the heating box for heating in the S4 and S7, it is necessary to ensure that the back cover of the mobile phone is placed horizontally and has a certain distance between it and the placement bracket in the heating box to ensure uniform heat conduction.
8. The coating method of a double-layer coating single-texture ceramic effect mobile phone back cover according to claim 1, characterized in that: In the step S7, the coated mobile phone back cover is placed in a heating box for heating and curing, and the temperature of the heating box is set at 150° C.-200° C.
9. The coating method of a double-layer coated single-textured ceramic effect mobile phone back cover according to claim 1, characterized in that: The time for heating and curing the back cover of the mobile phone in S7 is 8-16 minutes. After the curing time is over, the heating function of the heating box is turned off, and the back cover of the mobile phone is allowed to cool naturally in the heating box to avoid adverse effects on the coating quality due to rapid temperature changes.