Method for improving wet etching uniformity of polycrystalline silicon
By adopting a continuous short-term etching stage in polysilicon wet etching and removing bubbles, the surface roughness caused by bubbles during wet etching is solved, and the uniformity of the wafer surface is significantly improved.
Patent Information
- Application Number
- CN202411090771.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2024-04-29
- Filing Date
- 2024-08-09
- Publication Date
- 2024-11-22
AI Technical Summary
During the wet etching process of polycrystalline silicon, the silicon tetrafluoride gas accumulates to form bubbles, resulting in roughness of the wafer surface. The etching time increases with the thickness of polycrystalline silicon, and the increased number of bubbles increases the roughness, affecting the uniformity of etching.
The wet etching process with multiple consecutive short-term wet etching stages replaced the one-time long etching process, and the bubbles on the wafer surface were removed in adjacent stages. Through cyclic soaking and removal operations, the mixing of hydrofluoric acid, nitric acid and water was employed. The solution is etched, and the number of cycles is not less than three times.
It effectively solves the problem of poor etching uniformity caused by surface bubbles and improves the wafer surface uniformity after etching.
Smart Images

Figure CN118996635A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of semiconductor manufacturing, and in particular to a method for improving the uniformity of polysilicon wet etching. Background Art
[0002] At present, the wet etching operation of polysilicon is mainly carried out in a wet etching machine using a mixed solvent of hydrofluoric acid, nitric acid and water. The etching reaction is isotropic. During the operation, the silicon tetrafluoride gas produced will gather on the surface of the wafer to form bubbles. The subsequent reaction in the area blocked by the bubbles is hindered, resulting in a rough wafer surface.
[0003] For the wet etching operation mentioned above, its duration will increase with the increase of polysilicon thickness. When the thickness of polysilicon is large, the operation time may be too long, and the number of bubbles will also increase, which will eventually aggravate the roughness of the wafer surface. Summary of the invention
[0004] The present application provides a method for improving the uniformity of polysilicon wet etching, which can improve the uniformity of the wafer surface after wet etching.
[0005] The present application provides a method for improving the uniformity of polysilicon wet etching, including: S1: Immerse the wafer in the etching solution for a predetermined unit operation time; Wherein, the wafer is a wafer with a polysilicon layer formed on the surface; S2: removing the wafer from the etching solution for a preset time to remove bubbles on the surface of the wafer; S3: cyclically executing S1-S2 for a preset number of cycles to remove the polysilicon layer on the surface of the wafer.
[0006] In some embodiments, the etching solution is a mixed solution of hydrofluoric acid, nitric acid and water.
[0007] In some embodiments, in the etching solution, the ratio of hydrofluoric acid to nitric acid is 1:50.
[0008] In some embodiments, the number of cycles is no less than three times.
[0009] In some embodiments, the method is applied to a wet etching machine, which includes a reaction pool, a lifting platform, a moving component and an exhaust component. The etching solution is placed in the reaction pool, the lifting platform for placing wafers is installed on the moving component and can enter and exit the reaction pool under the action of the moving component. The exhaust component is used to exhaust the gas in the wet etching machine.
[0010] The technical solution of this application has at least the following advantages: 1. By using multiple consecutive short wet etching stages to replace a one-time long wet etching process and removing bubbles formed on the wafer surface between adjacent wet etching stages, the problem of poor etching uniformity caused by surface bubbles can be solved and the uniformity of the wafer surface after etching can be improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] In order to more clearly illustrate the specific implementation methods of the present application or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0012] Figure 1 It is a schematic flow chart of a method for improving polysilicon wet etching uniformity provided by an exemplary embodiment of the present application; Figure 2 is a schematic diagram of a wafer that needs to be wet-etched provided by an exemplary embodiment of the present application; Figure 3 A surface diagram of a wafer having a non-uniform surface in the prior art provided by an exemplary embodiment of the present application; Figures 4A-4B is a surface image of a wafer using the method for improving polysilicon wet etching uniformity provided by the present application in accordance with an exemplary embodiment of the present application; Figure 5 It is a schematic diagram of a possible moving component provided by an exemplary embodiment of the present application. DETAILED DESCRIPTION
[0013] The following will be combined with the accompanying drawings to clearly and completely describe the technical solutions in this application. Obviously, the described embodiments are part of the embodiments of this application, not all of them. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0014] In the description of the present application, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present application. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.
[0015] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, it can also be the internal connection of two components, it can be a wireless connection, or it can be a wired connection. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0016] In addition, the technical features involved in the different embodiments of the present application described below can be combined with each other as long as they do not conflict with each other.
[0017] The present application provides a method for improving the uniformity of polysilicon wet etching, referring to Figure 1 , the method mainly includes the following contents: S1: Immerse the wafer in the etching solution for a predetermined unit operation time.
[0018] The wafer is a wafer with a polysilicon layer formed on the surface. The structure of the wafer can be as follows: Figure 2 As shown, it includes a substrate ( Figure 2 Sub in), and the oxide layer formed on the surface of the substrate in turn ( Figure 2 OX) and polysilicon layer ( Figure 2 Poly in.
[0019] Exemplarily, first, the wafer to be cleaned is immersed in an etching solution for a predetermined unit operation time. During this process, the etching solution will continue to etch the polysilicon layer on the surface. The unit operation time can be calibrated through preliminary experiments, and this application does not impose specific restrictions. For example, the surface of the sample wafer can be continuously observed during the preliminary experiment, and the time when a large number of bubbles begin to appear on the surface of the sample wafer is used as the unit operation time.
[0020] Furthermore, the etching solution mentioned above may be a mixed solution of hydrofluoric acid, nitric acid and water.
[0021] Furthermore, in the etching solution, the ratio of hydrofluoric acid to nitric acid is 1:50.
[0022] S2: The wafer is removed from the etching solution for a preset time to remove bubbles on the surface of the wafer.
[0023] For example, the wafer is removed from the etching solution and left to stand for a preset time. During this process, bubbles on the wafer surface can be removed by extracting gas, thereby eliminating the interference of bubbles on the wafer surface with the subsequent etching process. The preset time can also be calibrated by, for example, conducting preliminary experiments.
[0024] In some embodiments, the preset time length mentioned above is not less than 30 seconds.
[0025] S3: cyclically executing S1-S2 for a preset number of cycles to remove the polysilicon layer on the surface of the wafer.
[0026] Exemplarily, the above S1 and S2 can be executed cyclically until the polysilicon layer on the surface of the wafer is removed after a preset number of cycles. The preset number of cycles can also be calibrated through preliminary experiments. For example, when the existing wet etching process is used as a reference, if the duration of the existing wet etching process is A, and in step S1, the set unit operation duration is B, then the number of cycles can be obtained by dividing A by B and rounding up.
[0027] Furthermore, in some embodiments, the number of cycles mentioned above is not less than three times.
[0028] Reference Figure 3 and Figure 4, where Figure 3 The wafer surface image shows uneven etching after a one-time long-term wet etching in the prior art. Figure 4A is a surface image of a wafer after one cycle is completed using the method provided by the present application, Figure 4B Surface image of a wafer after wet etching using the method provided in the present application. It can be found that after using the method for improving the uniformity of polysilicon wet etching provided in the present application, the uniformity of the wafer surface is significantly improved.
[0029] Optionally, in some embodiments, the method for improving the uniformity of polysilicon wet etching provided in the present application can be based on a wet etching machine. The wet etching machine mainly includes a reaction tank, a lifting platform, a moving component and an exhaust component. Among them, the etching solution is placed in the reaction tank, and the wafer to be wet-etched is placed in the lifting platform. The lifting platform is installed on the moving component and can move with the moving component. The moving component can be composed of multiple cylinders, linear slides, etc. (such as Figure 5As shown), the function of driving the lifting platform to move in multiple directions can be realized. In the above steps S1 and S2, the operations of immersing the wafer in the etching solution and removing the wafer from the etching solution are completed by the moving component. The exhaust component is mainly used to exhaust the gas in the wet etching machine. Generally speaking, the exhaust component is in a normally open state. When the wafer is removed from the etching solution, the bubbles on the surface will be removed by the action of the exhaust component. Other structures such as the cleaning tank included in the wet etching machine will not be repeated in this application.
[0030] An embodiment of the present application provides a method for improving the uniformity of polysilicon wet etching, which solves the problem of poor etching uniformity caused by surface bubbles and improves the uniformity of the wafer surface after etching is completed by replacing a one-time long wet etching process with a series of short wet etching stages and removing bubbles formed on the wafer surface between adjacent wet etching stages.
[0031] Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection created by this application.
Claims
1. A method for improving the uniformity of polysilicon wet etching, characterized in that: include: S1: Immerse the wafer in the etching solution for a predetermined unit operation time; Wherein, the wafer is a wafer with a polysilicon layer formed on the surface; S2: removing the wafer from the etching solution for a preset time to remove bubbles on the surface of the wafer; S3: cyclically executing S1-S2 for a preset number of cycles to remove the polysilicon layer on the surface of the wafer.
2. The method according to claim 1, characterized in that The etching solution is a mixed solution of hydrofluoric acid, nitric acid and water.
3. The method according to claim 2, characterized in that In the etching solution, the ratio of hydrofluoric acid to nitric acid is 1:
50.
4. The method according to claim 1, characterized in that: The number of cycles is not less than three times.
5. The method according to claim 1, characterized in that The method is applied to a wet etching machine, which includes a reaction pool, a lifting platform, a moving component and an exhaust component. The etching solution is placed in the reaction pool, the lifting platform for placing wafers is installed on the moving component and can enter and exit the reaction pool under the action of the moving component, and the exhaust component is used to exhaust the gas in the wet etching machine.