Semiconductor device and tube body thereof

By designing the gradual increase in the cross-sectional area of ​​the hollow tube body and the side wall angle, the problem of uneven gas concentration and temperature in semiconductor equipment is solved, and the consistency of film thickness and uniformity of thermal budget are achieved.

CN119008472APending Publication Date: 2024-11-22SHANGHAI INTEGRATED CIRCUIT EQUIPMENT & MATERIALS INDUSTRY INNOVATION CENTER CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411204498.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-29
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

In the tube body of a semiconductor device, the gas concentration gradually decreases during the upward movement, resulting in inconsistent film thickness on the wafer, and the temperature difference in different regions affects the implantation depth and electrical properties, resulting in uneven thermal budget.

Method used

Design a hollow tube body with a cross-sectional area gradually increasing from the intake end to the gas outflow end, and the side walls form an angle with the horizontal plane. By monitoring the relationship between the thickness of the deposited film layer and the cross-sectional radius, gases in various areas of the tube body are realized. Equilibrium of concentration and temperature.

Benefits of technology

The uniform gas concentration at each position in the tube body is achieved, large-scale temperature adjustment is avoided, the thermal budgets at each position of the wafer are maintained, and the consistency of film thickness and temperature balance are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119008472A_ABST
    Figure CN119008472A_ABST
Patent Text Reader

Abstract

The invention relates to the field of semiconductors, and discloses a semiconductor device and a tube body thereof, the tube body is hollow, and the interior of the tube body is used for accommodating a wafer; the cross section area of the pipe body is gradually increased from the first end to the second end, and an included angle is formed between the side wall of the pipe body and the horizontal plane. The first end is one end through which gas enters the pipe body, the second end is one end through which the gas flows out of the pipe body, and the temperatures of all areas in the pipe body are balanced in the vertical direction of the pipe body. The area of the cross section of the pipe body is gradually reduced from the first end to the second end, gas flows at the first end quickly and is low in concentration after entering the pipe body, the gas flows towards the second end along with the gas in the pipe body, the gas flows at the second end slowly and is high in concentration, and uniform gas concentration of all areas in the vertical direction of the pipe body can be achieved; therefore, the thickness uniformity of the film layers deposited on the wafers at different positions in the tube body is improved, the temperature of different areas of the tube body does not need to be greatly adjusted, and the thermal budget of the wafers at all positions in the tube body is kept similar.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the semiconductor field, and in particular to a semiconductor device and a tube body thereof. Background Art

[0002] Semiconductor equipment, such as LPCVD (Low Pressure Chemical Vapor Deposition) machines, are widely used in semiconductor manufacturing processes. When using semiconductor equipment to deposit a film layer on a wafer, the wafer is placed in a tube body of the semiconductor equipment, the tube body has equal dimensions at the top and bottom, gas is introduced from the bottom of the tube body, and the gas is extracted from the top of the tube body. Because the wafer has a pattern, the gas is consumed more at the bottom of the tube body, and the gas concentration gradually decreases during the upward movement, resulting in a lower thickness of the film layer deposited on the upper wafer.

[0003] In order to improve the consistency of film deposition thickness on wafers at different positions in the tube, the temperature of different areas in the tube is currently adjusted, and the temperature increases from the bottom area to the top area of ​​the tube. Although this method can level the thickness difference of the film layer, due to the temperature difference in different areas (the maximum temperature difference is as high as 40°C), the thermal budget of the wafer at each position will be different, which will affect the implantation depth of the previous process IMP (Implant, also known as ion implantation), thereby affecting the electrical properties.

[0004] Therefore, how to solve the above technical problems should be the focus of technical personnel in this field. Summary of the invention

[0005] The purpose of the present application is to provide a semiconductor device and a tube body thereof, so as to balance the gas concentration in each area of ​​the tube body and the temperature in each area of ​​the tube body.

[0006] In order to solve the above technical problems, the present application provides a tube body of a semiconductor device, wherein the interior of the tube body is hollow and the interior of the tube body is used to accommodate a wafer;

[0007] The cross-sectional area of ​​the tube body gradually increases from the first end to the second end, and the side wall of the tube body has an angle with the horizontal plane, wherein the first end is the end where gas enters the tube body, and the second end is the end where gas flows out of the tube body; in the vertical direction of the tube body, the temperature of each area inside the tube body is balanced; the angle is obtained by monitoring the thickness of the deposited film layer on the wafer at the first end of the preset tube body, monitoring the thickness of the deposited film layer on the wafer at the second end of the preset tube body, the height of the tube body, and any one of the radii of the cross section of the first end of the tube body and the radius of the cross section of the second end of the tube body, and the preset tube body is a tube body with the same size at all places from the first end of the preset tube body to the second end of the preset tube body.

[0008] Optionally, the cross-section of the tube body has a circular shape.

[0009] Optionally, the radius range of the cross section of the first end of the tube body is 169±2 mm, and the radius range of the cross section of the second end of the tube body is 185±2 mm.

[0010] Optionally, the angle between the side wall of the tube body and the horizontal plane is in the range of 88°±0.2°.

[0011] Optionally, a difference between a cross-sectional dimension of the first end of the tube body and a cross-sectional dimension of the second end of the tube body is in the range of 16±2 mm.

[0012] Optionally, the tube body is an integrated structure.

[0013] Optionally, the material of the tube body includes quartz.

[0014] The present application also provides a semiconductor device, comprising any one of the tube bodies described above.

[0015] Optionally, it also includes:

[0016] The wafer carrying structure is used to carry the wafer and is located inside the tube body.

[0017] Optionally, it also includes:

[0018] A support body is used to support the tube body.

[0019] The present application provides a tube body for a semiconductor device, wherein the interior of the tube body is hollow and is used to accommodate wafers; the cross-sectional area of ​​the tube body gradually increases from the first end to the second end, and the side wall of the tube body has an angle with the horizontal plane, wherein the first end is an end where gas enters the tube body, and the second end is an end where gas flows out of the tube body; in the vertical direction of the tube body, the temperature of each area in the tube body is balanced; the angle is obtained by monitoring the thickness of the deposited film layer on the wafer at the first end of the preset tube body, monitoring the thickness of the deposited film layer on the wafer at the second end of the preset tube body, the height of the tube body, and any one of the radius of the cross section of the first end of the tube body and the radius of the cross section of the second end of the tube body, and the preset tube body is a tube body with the same size at all places from the first end of the preset tube body to the second end of the preset tube body.

[0020] It can be seen that the cross-sectional area of ​​the tube body in the present application gradually decreases from the first end to the second end, that is, the cross-sectional area of ​​the gas inlet end is the smallest, and the cross-sectional area of ​​the gas outlet end is the largest. According to the law of gas flow rate, the smaller the cross-sectional area, the greater the gas flow rate, and the larger the cross-sectional area, the smaller the gas flow rate. Therefore, after the gas enters the tube body, due to the small cross-sectional area of ​​the first end, the gas flow rate is fast and the gas concentration is low. As the gas flows to the second end in the tube body, the gas flow rate is slow at the second end and the gas concentration is high, so as to achieve uniform gas concentration in each area in the vertical direction of the tube body. That is, the present application improves the uniformity of the thickness of the film layer deposited on the wafer at different positions in the tube body by adjusting the gas concentration in the tube body. At the same time, the temperature of different areas in the tube body is balanced, so that the thermal budget of the wafer at each position in the tube body remains similar. The present application uses the difference in the thickness of the deposited film layer on the wafer monitored at the first and second ends of the preset tube body to obtain the cross-sectional area relationship at the first and second ends of the tube body, so as to determine the inclination angle of the side wall of the tube body according to the size and height of the cross-sectional area of ​​the tube body. In addition, the present application also provides a semiconductor device with the above advantages. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] In order to more clearly illustrate the embodiments of the present application or the technical solutions of the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0022] FIG1 is a schematic diagram of the structure of a tube body in the related art;

[0023] FIG2 is a schematic structural diagram of a tube body provided in an embodiment of the present application;

[0024] FIG3 is a temperature comparison diagram of various regions when using the pipe body of the present application and the pipe body in the related art;

[0025] FIG. 4 is a schematic diagram of the structure of a semiconductor device provided in an embodiment of the present application. DETAILED DESCRIPTION

[0026] In order to enable those skilled in the art to better understand the present application, the present application is further described in detail below in conjunction with the accompanying drawings and specific implementation methods. Obviously, the described embodiments are only part of the embodiments of the present application, rather than all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without making creative work are within the scope of protection of the present application.

[0027] In the following description, many specific details are set forth to facilitate a full understanding of the present invention, but the present invention may also be implemented in other ways different from those described herein, and those skilled in the art may make similar generalizations without violating the connotation of the present invention. Therefore, the present invention is not limited to the specific embodiments disclosed below.

[0028] As described in the background technology section, in the related technology, the upper and lower sizes of the tube body are equal. As shown in Figure 1, gas is introduced from the lower end of the tube body and is extracted from the top of the tube body. The concentration of the gas gradually decreases as it moves upward, resulting in a lower thickness of the film layer deposited on the upper wafer. Currently, the temperature of different areas in the tube body is adjusted to improve the consistency of the thickness of the film layer deposited on the wafer. The temperature of the tube body gradually increases from the bottom to the top. Due to the temperature difference in different areas, the thermal budget of the wafer at each position will be different.

[0029] In view of this, the present application provides a tube body of a semiconductor device. Please refer to FIG. 2 . The tube body 1 is hollow inside and is used to accommodate a wafer.

[0030] The cross-sectional area of ​​the tube body 1 gradually increases from the first end 11 to the second end 12, and the side wall of the tube body has an angle with the horizontal plane; wherein the first end 11 is the end where the gas enters the tube body 1, and the second end 12 is the end where the gas flows out of the tube body 1; in the vertical direction of the tube body, the temperature of each area in the tube body is balanced; the angle is obtained by monitoring the thickness of the deposited film layer on the wafer at the first end of the preset tube body, monitoring the thickness of the deposited film layer on the wafer at the second end of the preset tube body, the height of the tube body, and any one of the radii of the cross section of the first end of the tube body and the radius of the cross section of the second end of the tube body, and the preset tube body is a tube body with the same size at all places from the first end of the preset tube body to the second end of the preset tube body.

[0031] The interior of the tube body 1 is hollow, that is, the tube body 1 has a cavity. When a thin film is deposited on a wafer, the wafer is placed in the cavity of the tube body 1 .

[0032] The gas enters the tube body 1 from the first end 11 of the tube body 1 , flows upward, and flows out of the tube body 1 from the second end 12 of the tube body 1 .

[0033] The law of gas flow rate: the larger the tube cross section, the lower the flow rate, and the smaller the tube cross section, the higher the flow rate. In the present application, the cross-sectional area of ​​the tube body 1 gradually increases from the first end 11 to the second end 12, and the cross-sectional area of ​​the first end 11 of the tube body 1 is the smallest, so the flow rate at the first end 11 of the tube body 1 is the largest, and the gas concentration is low. The gas flow rate gradually decreases from the first end 11 to the second end 12 of the tube body 1, and the gas concentration gradually increases. Therefore, in the present application, the shape of the tube body 1 is adjusted to achieve uniform gas concentration in each area of ​​the tube body 1, so that the thickness of wafers at different positions is balanced, and large temperature adjustments in different areas of the tube body 1 are avoided, and the temperatures in different areas of the tube body 1 are basically balanced.

[0034] The tube body 1 can be divided into five areas from the first end 11 to the second end 12, namely the bottom area (Bottom), the bottom area close to the middle area (C-Bottom), the middle area (Center), the top area close to the middle area (C-Top), and the top area (Top).

[0035] The temperature balance of each area in the pipe body means that the difference between the highest and lowest temperatures in each area is no more than 5°C.

[0036] It should be pointed out that the material of the tube body 1 is not limited in this embodiment and depends on the actual situation.

[0037] As an implementation method, the material of the tube body 1 includes quartz. Quartz has high chemical stability, maintains its performance in various chemical environments, and does not react with gases; quartz also has high thermal stability, and can work for a long time at high temperatures without deformation or damage; quartz has high hardness and wear resistance, and can maintain a smooth surface during long-term use, reducing maintenance requirements and reducing costs.

[0038] It should be noted that the shape of the cross section of the tube body 1 is not limited in this embodiment and can be set at will. For example, the shape of the cross section of the tube body 1 includes but is not limited to circle, ellipse, square, rectangle, etc.

[0039] In this embodiment, the height of the tube body 1 , the size of the first end 11 , and the size of the second end 12 are not limited and can be set according to actual conditions.

[0040] Exemplarily, the height of the tube body 1 may be 504 mm.

[0041] The difference between the cross-sectional dimensions of the first end 11 of the tube body 1 and the cross-sectional dimensions of the second end 12 of the tube body 1 is not limited in this embodiment and depends on the circumstances.

[0042] As an implementation method, the difference between the cross-sectional dimensions of the first end 11 of the tube body 1 and the cross-sectional dimensions of the second end 12 of the tube body 1 is in the range of 16±2, so that when adjusting the gas concentration distribution in the tube body 1, the gas concentration in each area of ​​the tube body 1 is more uniform, thereby making the temperatures of each area closer, and minimizing the thermal budget differences of the wafers at each position.

[0043] Exemplarily, the difference between the cross-sectional dimension of the first end 11 of the tube body 1 and the cross-sectional dimension of the second end 12 of the tube body 1 may be 14 mm, 16 mm, 18 mm, etc.

[0044] The cross-sectional dimensions of the first end 11 of the tube body 1 and the cross-sectional dimensions of the second end 12 of the tube body 1 are determined according to the shape of the cross-sectional dimensions. For example, when the cross-sectional shape of the tube body 1 is circular, the cross-sectional dimensions of the first end 11 of the tube body 1 and the cross-sectional dimensions of the second end 12 of the tube body 1 may be the radius; when the cross-sectional shape of the tube body 1 is square or rectangular, the cross-sectional dimensions of the first end 11 of the tube body 1 and the cross-sectional dimensions of the second end 12 of the tube body 1 may be the side length; when the cross-sectional shape of the tube body 1 is elliptical, the cross-sectional dimensions of the first end 11 of the tube body 1 and the cross-sectional dimensions of the second end 12 of the tube body 1 may be the major axis.

[0045] In order to reduce the probability of abnormality of the tube body 1, in one embodiment of the present application, the tube body 1 is an integrated structure.

[0046] In this embodiment, the cross-sectional area of ​​the tube body 1 gradually decreases from the first end 11 to the second end 12, that is, the cross-sectional area of ​​the gas inlet end is the smallest, and the cross-sectional area of ​​the gas outlet end is the largest. According to the law of gas flow rate, the smaller the cross-sectional area, the greater the gas flow rate, and the larger the cross-sectional area, the smaller the gas flow rate. Therefore, after the gas enters the tube body 1, due to the small cross-sectional area of ​​the first end 11, the gas flow rate is fast and the gas concentration is low. As the gas flows in the tube body 1 to the second end 12, the gas flow rate is slow at the second end 12 and the gas concentration is high, so as to achieve uniform gas concentration in each area in the vertical direction of the tube body 1. That is, the present application improves the uniformity of the thickness of the film layer deposited on the wafer at different positions in the tube body 1 by adjusting the gas concentration in the tube body 1. At the same time, there is no need to make a large adjustment to the temperature of different areas of the tube body 1, and the temperature of each area of ​​the tube body 1 is balanced, so that the thermal budget of the wafer at each position in the tube body 1 remains similar.

[0047] On the basis of the above embodiments, in one embodiment of the present application, as shown in FIG. 2 , the interior of the tube body 1 of the semiconductor device is hollow, and the interior of the tube body 1 is used to accommodate a wafer;

[0048] The cross-sectional area of ​​the tube body 1 gradually increases from the first end 11 to the second end 12, and the side wall of the tube body has an angle with the horizontal plane; wherein, the first end 11 is the end where the gas enters the tube body 1, and the second end 12 is the end where the gas flows out of the tube body 1; in the vertical direction of the tube body, the temperature of each area in the tube body is balanced; the angle is obtained by monitoring the thickness of the deposited film layer on the wafer at the first end of the preset tube body, monitoring the thickness of the deposited film layer on the wafer at the second end of the preset tube body, the height of the tube body, and any one of the radii of the cross section of the first end of the tube body and the radius of the cross section of the second end of the tube body. The preset tube body is a tube body with the same size at all places from the first end of the preset tube body to the second end of the preset tube body, wherein the shape of the cross section of the tube body 1 is circular.

[0049] The shape of the wafer is circular. In this embodiment, the cross section of the tube body 1 is set to be circular to match the shape of the wafer. Moreover, after the gas is introduced into the tube body 1, the airflow is more uniform and the tube body 1 is heated more uniformly.

[0050] As an implementation method, the radius r1 of the cross section of the first end 11 of the tube body 1 is in the range of 169±2mm, and the radius r2 of the cross section of the second end 12 of the tube body 1 is in the range of 185±2mm. For example, the radius r1 of the cross section of the first end 11 of the tube body 1 can be 167mm, 168mm, 169mm, 170mm, 171mm, etc., and the radius r2 of the cross section of the second end 12 of the tube body 1 can be 183mm, 184mm, 185mm, 186mm, 187mm, etc.

[0051] The difference between the radius r1 of the cross section of the first end 11 of the tube body 1 and the radius r2 of the cross section of the second end 12 may be 16±2 mm, such as 14 mm, 16 mm, 18 mm, etc.

[0052] On the basis of any of the above embodiments, in one embodiment of the present application, the interior of the tube body 1 of the semiconductor device is hollow, and the interior of the tube body 1 is used to accommodate a wafer;

[0053] The cross-sectional area of ​​the tube body 1 gradually increases from the first end 11 to the second end 12, and the side wall of the tube body has an angle α with the horizontal plane, and the range of the angle α is 88°±0.2°; wherein, the first end 11 is the end where the gas enters the tube body 1, and the second end 12 is the end where the gas flows out of the tube body 1; in the vertical direction of the tube body, the temperature of each area in the tube body is balanced; the angle is obtained by monitoring the thickness of the deposited film layer on the wafer at the first end of the preset tube body, monitoring the thickness of the deposited film layer on the wafer at the second end of the preset tube body, the height of the tube body, and any one of the radii of the cross section of the first end of the tube body and the radius of the cross section of the second end of the tube body, and the preset tube body is a tube body with the same size at all places from the first end of the preset tube body to the second end of the preset tube body.

[0054] The angle between the side wall of the tube body 1 and the horizontal plane can be 87.8°, 87.9°, 88°, 80.1°, 80.2°, etc., which can be set according to actual conditions and is not specifically limited in this embodiment.

[0055] Monitor wafers are placed in different boat positions in a preset tube to monitor the particle count and deposited film thickness of semiconductor devices. Monitor wafers are placed evenly in different boat positions.

[0056] The angle α between the side wall of the tube body 1 and the horizontal plane can be obtained by monitoring the thickness of the deposited film layer on the wafer at the first end of the preset tube body, monitoring the thickness of the deposited film layer on the wafer at the second end of the preset tube body, the height of the tube body, and any one of the radii of the cross-section at the first end of the tube body and the radius of the cross-section at the second end of the tube body, wherein the preset tube body is a tube body with the same size at all locations from the first end of the preset tube body to the second end of the preset tube body, as shown in Figure 1.

[0057] For a preset tube body with the same upper and lower dimensions, if the temperatures of various areas in the vertical direction inside the preset tube body are set to be equal, the concentration of the gas gradually decreases as it flows from bottom to top in the preset tube body, and the thickness of the deposited film layer on the furnace-monitored wafer also becomes thinner from bottom to top.

[0058] The relationship between the gas flow rate V, the gas flow rate Q and the cross-sectional area A of the tube body 1 is V=Q / A. To balance the thickness of the deposited film layer on the monitoring wafer in each area of ​​the tube body 1, the gas flow rate must be positively correlated with the thickness of the deposited film layer on the monitoring wafer, that is, negatively correlated with the cross-sectional area of ​​the tube body 1, that is:

[0059] (1)

[0060] In the formula, A1 is the area of ​​the cross section of the first end of the tube body 1, A2 is the area of ​​the cross section of the second end of the tube body 1, r1 is the radius of the cross section of the first end of the tube body 1, r2 is the radius of the cross section of the second end of the tube body 1, D1 is the thickness required for depositing the film layer on the wafer at the first end of the tube body 1, and D2 is the thickness required for depositing the film layer on the wafer at the second end of the tube body 1.

[0061] The concentration of the gas gradually decreases as it flows from bottom to top in the preset tube, and the thickness of the deposited film layer on the monitor wafer at different positions becomes thinner from bottom to top (for example, the thickness of the deposited film layer can be 240Å→230Å→220Å→210Å→200Å from bottom to top), that is, the thickness of the deposited film layer on the monitoring wafer at the top end of the preset tube is 200Å, and the thickness of the deposited film layer on the monitoring wafer at the bottom end of the preset tube is 240Å.

[0062] Therefore, when one of the radius of the cross section at the first end of the tube body 1 and the radius of the cross section at the second end is determined, the other radius can be obtained. Assuming that the radius r1 of the cross section at the first end of the tube body 1 is 169 mm, according to formula (1), it can be obtained that:

[0063] (2)

[0064] According to formula (2), it can be obtained that the radius r2 of the cross section of the second end of the tube body 1 in the present application is 185 mm.

[0065] The relationship between the angle between the side wall of the tube body 11 and the horizontal plane, the height of the tube body 1, the radius of the first end cross section, and the radius of the second end cross section is:

[0066] (3)

[0067] Wherein, α is the angle between the side wall of the tube body 1 and the horizontal plane, and h is the height of the tube body 1.

[0068] When the height of the tube body 1 is 504 mm, the radius r1 of the cross section at the first end of the tube body 1 is 169 mm, and the radius r2 of the cross section at the second end is 185 mm, then according to formula (3), it can be determined that the angle between the side wall of the tube body 1 and the horizontal plane is 88°.

[0069] In this embodiment, the angle between the side wall of the tube body 1 and the horizontal plane is set at 88°±0.2°, so as to control the concentration uniformity of each area of ​​the tube body 1.

[0070] When the cross section of the tube body in the present application is circular, the radius of the cross section of the first end is 169mm, the radius of the cross section of the second end is 185mm, and the angle between the side wall of the tube body and the horizontal plane is 88°, when the tube body in the present application and the tube body in the related art are used to deposit a thin film on a wafer, the temperature comparison of different regions of the tube body is shown in Figure 3, where the horizontal axis is different regions of the tube body and the vertical axis is temperature. As can be seen from Figure 3, when the tube body in the related art is used, the temperature of each region is quite different, and when the tube body in the present application is used, the temperature of each region is basically equal.

[0071] The present application also provides a semiconductor device, please refer to FIG. 4 , which includes the tube body 1 described in any of the above embodiments.

[0072] As an implementation method, the semiconductor device may further include: a wafer supporting structure 2 for supporting a wafer, located inside the tube body 1 .

[0073] The wafer carrying structure 2 includes but is not limited to a tray and a wafer boat.

[0074] As an implementation method, the semiconductor device may further include: a support body, used to support the tube body to maintain the stability of the tube body 1 in the semiconductor device.

[0075] The various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.

[0076] The semiconductor device and its tube body provided by the present application are introduced in detail above. Specific examples are used in this article to illustrate the principles and implementation methods of the present application. The description of the above embodiments is only used to help understand the scheme and its core idea of ​​the present application. It should be pointed out that for ordinary technicians in this technical field, without departing from the principles of the present application, several improvements and modifications can be made to the present application, and these improvements and modifications also fall within the scope of protection of the present application.

Claims

1. A tube body of a semiconductor device, characterized in that: The interior of the tube body is hollow, and the interior of the tube body is used to accommodate the wafer; The cross-sectional area of ​​the tube body gradually increases from the first end to the second end, and the side wall of the tube body has an angle with the horizontal plane, wherein the first end is the end where gas enters the tube body, and the second end is the end where gas flows out of the tube body; in the vertical direction of the tube body, the temperature of each area in the tube body is balanced; the angle is obtained by monitoring the thickness of the deposited film layer on the wafer at the first end of the preset tube body, monitoring the thickness of the deposited film layer on the wafer at the second end of the preset tube body, the height of the tube body, and any one of the radii of the cross-section of the first end of the tube body and the radius of the cross-section of the second end of the tube body, and the preset tube body is a tube body with the same size at all places from the first end of the preset tube body to the second end of the preset tube body.

2. The semiconductor device body according to claim 1, wherein: The cross-sectional shape of the tube body includes a circle.

3. The semiconductor device body according to claim 2, characterized in that: The radius range of the cross section of the first end of the tube body is 169±2 mm, and the radius range of the cross section of the second end of the tube body is 185±2 mm.

4. The semiconductor device body according to claim 3, characterized in that: The angle between the side wall of the tube body and the horizontal plane is in the range of 88°±0.2°.

5. The semiconductor device body according to claim 1, wherein: The difference between the cross-sectional dimension of the first end of the tube body and the cross-sectional dimension of the second end of the tube body is in the range of 16±2 mm.

6. The semiconductor device body according to claim 1, wherein: The tube body is an integrated structure.

7. The semiconductor device body according to claim 1, wherein: The material of the tube body includes quartz.

8. A semiconductor device, characterized in that: Comprising a tube body as claimed in any one of claims 1 to 7.

9. The semiconductor device according to claim 8, wherein: Also includes: The wafer carrying structure is used to carry the wafer and is located inside the tube body.

10. The semiconductor device according to claim 8, wherein Also includes: A support body is used to support the tube body.