Preparation method of electrolyte
By using dimethyl carbonate and vinyl carbonate as solvents, lithium hexafluorophosphate as solute, combined with film formation and flame retardant additives, combined with distillation, ion exchange and filtration technologies to remove impurities, the problem of impurities in electrolyte affecting conductivity is solved, and the problem of impurities in electrolytes is improved. Battery performance and safety.
Patent Information
- Application Number
- CN202410902140.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-05
- Publication Date
- 2024-11-22
AI Technical Summary
Impurities in the electrolyte hinder the migration of ions, lead to a decrease in conductivity, affecting battery performance, and the purity and quality of the electrolyte need to be improved.
Dimethyl carbonate and vinyl carbonate are used as solvents and lithium hexafluorophosphate are used as solutes to add film formation and flame retardant additives, and impurities are removed through distillation, ion exchange, precipitation filtration and adsorption filtration, etc., environmental conditions are controlled, and quality detection and storage are carried out. Preprocessing.
It improves the chemical stability and purity of the electrolyte, enhances the cycling performance and safety of the battery, and ensures the improvement of the conductivity and the normal charging and discharge of the battery.
Smart Images

Figure CN119009138A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of electrolyte preparation, and in particular to a method for preparing an electrolyte. Background Art
[0002] An electrolyte is a solution that contains substances that can produce ions. These substances will decompose into charged ions during the dissolution process, making the solution conductive. The electrolyte acts as a medium for ion conduction between the positive and negative electrodes of the battery, and is generally composed of solvents and electrolyte solutes. It can provide a channel for ion transmission for the chemical reactions inside the battery and ensure the normal charging and discharging of the battery. The electrolyte dissolved in the electrolyte contains ionic compounds, such as soluble salts, acids, and bases. These compounds will dissociate into charged cations and anions during the dissolution process. When a power source is connected, the cations move to the cathode and the anions move to the anode, thus forming an electric current.
[0003] This prior art also has the following problems when used:
[0004] The chemical stability and various properties of the electrolyte directly affect the effect of battery use. Impurities in the electrolyte will hinder the migration of ions, resulting in a decrease in conductivity and affecting the performance of batteries and other equipment. The purity and quality of the electrolyte need to be improved. Therefore, we propose a method for preparing an electrolyte to solve the above problems. Summary of the invention
[0005] In order to overcome the deficiencies of the prior art, the present invention provides a method for preparing an electrolyte, which can solve the technical problems of the existing method for preparing an electrolyte proposed in the above background technology, that the chemical stability and various properties of the electrolyte directly affect the effect of battery use, and that impurities in the electrolyte will hinder the migration of ions, resulting in a decrease in conductivity, affecting the performance of equipment such as batteries, and that the purity and quality of the electrolyte need to be improved.
[0006] In order to solve the above technical problems, the present invention provides the following technical solutions:
[0007] Step 1, preparing a solvent: preparing a dimethyl carbonate solvent and an ethylene carbonate solvent;
[0008] Step 2, preparing solute: preparing lithium salt solute;
[0009] Step 3, preparing additives: adding film-forming additives and flame retardant additives;
[0010] Step 4, mixing and stirring: the solvent, solute and additive are mixed together in a certain proportion and stirred to ensure that they are fully mixed;
[0011] Step 5, adjusting the electrolyte concentration and pH value: adjusting the electrolyte concentration and pH value according to production needs, which can be achieved by adding an appropriate amount of solvent or electrolyte;
[0012] Step 6, filtration and purification: removing impurities and insoluble substances in the solution;
[0013] Step 7, controlling environmental conditions: During the preparation process, environmental conditions such as temperature, humidity and air quality need to be controlled to avoid contamination of the electrolyte or side reactions;
[0014] Step 8, quality inspection: perform quality inspection on the prepared electrolyte to ensure that the electrolyte meets the specified standards and requirements;
[0015] Step 9, Storage: Pre-treat the packaging barrel.
[0016] As a preferred technical solution of the present invention, the step 1 is specifically:
[0017] A dimethyl carbonate solvent is mixed with an ethylene carbonate solvent, and the selected solvent is purified and treated to remove impurities and moisture. The solvent is separated by distillation according to the difference in boiling points between the electrolyte solvent and the impurities by distillation and ion exchange. The solvent is then exchanged from the mixture by utilizing the difference in ion exchange capacity of the ion exchange resin for the electrolyte solvent and the impurities.
[0018] As a preferred technical solution of the present invention, the step 2 is specifically as follows:
[0019] Lithium hexafluorophosphate is used as the solute, which has the excellent properties of high stability and good solubility.
[0020] As a preferred technical solution of the present invention, the step 4 is specifically:
[0021] In a closed environment, a circulation pipeline is set up to allow the electrolyte to circulate in the pipeline to enhance the mixing efficiency.
[0022] As a preferred technical solution of the present invention, the step 6 is specifically:
[0023] The electrolyte is purified by the method of first sedimentation filtration and then adsorption filtration. The electrolyte is filtered through a filter and filter paper to remove the sediment. A molecular sieve is used to pass the electrolyte through an adsorbent to adsorb impurities and harmful substances.
[0024] As a preferred technical solution of the present invention, the step 7 is specifically:
[0025] The ambient humidity should be controlled below 1% to avoid moisture mixing into the electrolyte that may affect its performance and cause side effects. The temperature should be controlled between 20°C and 25°C to maintain a stable temperature. Static electricity elimination measures should be taken.
[0026] As a preferred technical solution of the present invention, the step 8 is specifically:
[0027] The chemical composition, conductivity, pH, moisture content, density, impurity content and electrochemical properties of the electrolyte are tested.
[0028] As a preferred technical solution of the present invention, step 9 is specifically:
[0029] Water washing and argon replacement pretreatment processes are used to ensure that the storage container is dry and free of impurities.
[0030] Compared with the prior art, the present invention can achieve the following beneficial effects:
[0031] 1. Mix dimethyl carbonate solvent with ethylene carbonate solvent, which has the properties of both dimethyl carbonate and ethylene carbonate, making the solvent have low viscosity, low melting point, high chemical stability and better low temperature performance;
[0032] 2. After the solvent is purified and treated, it is mixed and then purified by precipitation filtration and adsorption filtration to remove impurities and moisture. The impurities are removed one by one to improve the purity of the electrolyte and the performance of the battery;
[0033] 3. Evenly mix, add film-forming additives and flame retardant additives, the battery cycle performance and stability are excellent, to a certain extent, inhibit the occurrence of electrolyte combustion or reduce the severity of combustion, and improve the safety of the battery. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Figure 1 It is a schematic diagram of the preparation method of the present invention. DETAILED DESCRIPTION
[0035] In order to make the technical means, creative features, objectives and effects of the present invention easy to understand, the present invention is further described below in conjunction with specific embodiments, but the following embodiments are only preferred embodiments of the present invention, not all. Based on the embodiments in the implementation mode, other embodiments obtained by those skilled in the art without creative work are all within the scope of protection of the present invention.
[0036] Example
[0037] See also Figure 1 , the present invention provides a technical solution: a method for preparing an electrolyte;
[0038] Step 1, preparing a solvent: preparing a dimethyl carbonate solvent and an ethylene carbonate solvent, mixing the dimethyl carbonate solvent and the ethylene carbonate solvent, purifying and treating the selected solvent to remove impurities and moisture, using a distillation method and an ion exchange method, separating the solvent by distillation according to the difference in boiling points between the electrolyte solvent and the impurities, and then using the difference in ion exchange capacity of the ion exchange resin for the electrolyte solvent and the impurities to exchange the solvent from the mixture;
[0039] Step 2, preparing the solute: preparing a lithium salt solute, using lithium hexafluorophosphate as the solute, which has excellent properties of high stability and good solubility;
[0040] Step 3, preparing additives: adding film-forming additives and flame retardant additives;
[0041] Step 4, mixing and stirring: the solvent, solute and additive are mixed together in a certain proportion and stirred to ensure that they are fully mixed and uniform. In a closed environment, a circulation pipeline is set up to allow the electrolyte to circulate in the pipeline to enhance the mixing efficiency;
[0042] Step 5, adjusting the electrolyte concentration and pH value: adjusting the electrolyte concentration and pH value according to production needs, which can be achieved by adding an appropriate amount of solvent or electrolyte;
[0043] Step 6, filtration and purification: remove impurities and insoluble substances in the solution, purify the electrolyte by first precipitation filtration and then adsorption filtration, filter through a filter and filter paper to remove the precipitate, use a molecular sieve, pass the electrolyte through an adsorbent to adsorb impurities and harmful substances;
[0044] Step 7, control environmental conditions: During the preparation process, it is necessary to control environmental conditions such as temperature, humidity and air quality to prevent the electrolyte from being contaminated or causing side reactions. The environmental humidity is controlled below 1% to prevent water from mixing into the electrolyte to affect the performance of the electrolyte and cause side effects. The temperature is controlled between 20°C and 25°C to maintain a stable temperature and take static elimination measures.
[0045] Step 8, quality inspection: Conduct quality testing on the prepared electrolyte to ensure that the electrolyte meets the specified standards and requirements, and test the chemical composition, conductivity, pH, moisture content, density, impurity content, and electrochemical properties of the electrolyte;
[0046] Step 9, Storage: Pre-treat the packaging barrels, using water washing and argon replacement pre-treatment processes to ensure that the storage container is dry and free of impurities.
[0047] Specific working principle:
[0048] like Figure 1As shown, step 1, prepare the solvent: prepare dimethyl carbonate solvent and ethylene carbonate solvent, mix the dimethyl carbonate solvent and ethylene carbonate solvent so that the solvent has the properties of both dimethyl carbonate and ethylene carbonate, improve the performance of the electrolyte, purify and treat the selected solvent to remove impurities and moisture, and use distillation and ion exchange methods to separate the solvent by distillation according to the difference in boiling points between the electrolyte solvent and the impurities. This method is suitable for solvents and impurities with large differences in boiling points, and uses the difference in ion exchange capacity of ion exchange resin for electrolyte solvents and impurities to exchange the solvent from the mixture. This method is suitable for solvents containing ionic impurities;
[0049] Step 2, preparing the solute: preparing a lithium salt solute, using lithium hexafluorophosphate as the solute, which has excellent properties of high stability and good solubility, can easily decompose lithium ions in a liquid environment, has high conductivity, and ensures the uniformity and stability of the electrolyte;
[0050] Step 3, preparing additives: adding film-forming additives and flame-retardant additives, using vinylene carbonate as a film-forming additive to form a stable solid electrolyte interface film on the electrode surface to improve the cycle performance and stability of the battery, and using trimethyl phosphate as a flame-retardant additive to inhibit the occurrence of electrolyte combustion or reduce the severity of combustion to a certain extent, thereby improving the safety of the battery;
[0051] Step 4, mixing and stirring: the solvent, solute and additive are mixed together in a certain proportion and stirred to ensure that they are fully mixed and uniform. In a closed environment, a circulation pipeline is set up to allow the electrolyte to circulate in the pipeline to enhance the mixing efficiency;
[0052] Step 5, adjusting the electrolyte concentration and pH value: adjusting the electrolyte concentration and pH value according to production needs, which can be achieved by adding an appropriate amount of solvent or electrolyte;
[0053] Step 6, filtration and purification: remove impurities and insoluble substances in the solution, purify the electrolyte by first precipitation filtration and then adsorption filtration, leave the electrolyte for a period of time to allow the impurities therein to settle to the bottom, then filter it through a filter and filter paper to remove the precipitate, and use the difference in adsorption capacity of the adsorbent for the electrolyte solvent and impurities to adsorb the solvent from the mixture, and then use a molecular sieve to pass the electrolyte through the adsorbent to adsorb the impurities and harmful substances therein;
[0054] Step 7, control environmental conditions: During the preparation process, it is necessary to control environmental conditions such as temperature, humidity and air quality to prevent the electrolyte from being contaminated or causing side reactions. The environmental humidity is controlled below 1% to prevent water from mixing into the electrolyte to affect the performance of the electrolyte and cause side effects. The temperature is controlled between 20°C and 25°C to maintain a stable temperature and take static elimination measures.
[0055] Step 8, quality inspection: Conduct quality testing on the prepared electrolyte to ensure that the electrolyte meets the specified standards and requirements, and test the chemical composition, conductivity, pH, moisture content, density, impurity content, and electrochemical properties of the electrolyte;
[0056] Step 9, storage: pre-treat the packaging barrel, use water washing and argon replacement pre-treatment procedures to ensure that the storage container is dry and free of impurities, and the above completes a series of operations of the preparation method of the electrolyte. The contents not described in detail in this specification belong to the prior art known to professional and technical personnel in this field.
[0057] The above shows and describes the basic principles, main features and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited by the above embodiments. The above embodiments and descriptions are only preferred examples of the present invention and are not intended to limit the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention. The scope of protection of the present invention is defined by the attached claims and their equivalents.
Claims
1. A method for preparing an electrolyte, characterized in that: The steps include: Step 1, preparing a solvent: preparing a dimethyl carbonate solvent and an ethylene carbonate solvent; Step 2, preparing solute: preparing lithium salt solute; Step 3, preparing additives: adding film-forming additives and flame retardant additives; Step 4, mixing and stirring: the solvent, solute and additive are mixed together in a certain proportion and stirred to ensure that they are fully mixed; Step 5, adjusting the electrolyte concentration and pH value: adjusting the electrolyte concentration and pH value according to production needs, which can be achieved by adding an appropriate amount of solvent or electrolyte; Step 6, filtration and purification: removing impurities and insoluble substances in the solution; Step 7, controlling environmental conditions: During the preparation process, environmental conditions such as temperature, humidity and air quality need to be controlled to avoid contamination of the electrolyte or side reactions; Step 8, quality inspection: perform quality inspection on the prepared electrolyte to ensure that the electrolyte meets the specified standards and requirements; Step 9, Storage: Pre-treat the packaging barrel.
2. The method for preparing an electrolyte according to claim 1, characterized in that: The step 1 is specifically as follows: A dimethyl carbonate solvent is mixed with an ethylene carbonate solvent, and the selected solvent is purified and treated to remove impurities and moisture. The solvent is separated by distillation according to the difference in boiling points between the electrolyte solvent and the impurities by distillation and ion exchange. The solvent is then exchanged from the mixture by utilizing the difference in ion exchange capacity of the ion exchange resin for the electrolyte solvent and the impurities.
3. The method for preparing an electrolyte according to claim 1, characterized in that: The step 2 is specifically as follows: Lithium hexafluorophosphate is used as the solute, which has the excellent properties of high stability and good solubility.
4. The method for preparing an electrolyte according to claim 1, characterized in that: The step 4 is specifically as follows: In a closed environment, a circulation pipeline is set up to allow the electrolyte to circulate in the pipeline to enhance the mixing efficiency.
5. The method for preparing an electrolyte according to claim 1, characterized in that: The step 6 is specifically as follows: The electrolyte is purified by the method of first sedimentation filtration and then adsorption filtration. The electrolyte is filtered through a filter and filter paper to remove the sediment. A molecular sieve is used to pass the electrolyte through an adsorbent to adsorb impurities and harmful substances.
6. The method for preparing an electrolyte according to claim 1, characterized in that: The step 7 is specifically as follows: The ambient humidity should be controlled below 1% to avoid moisture mixing into the electrolyte that may affect its performance and cause side effects. The temperature should be controlled between 20°C and 25°C to maintain a stable temperature and measures should be taken to eliminate static electricity.
7. The method for preparing an electrolyte according to claim 1, characterized in that: The step 8 is specifically as follows: The chemical composition, conductivity, pH, moisture content, density, impurity content and electrochemical properties of the electrolyte are tested.
8. The method for preparing an electrolyte according to claim 1, characterized in that: The step 9 is specifically as follows: Water washing and argon replacement pretreatment processes are used to ensure that the storage container is dry and free of impurities.