Silicon nitride forming process based on plasma spraying

The silicon nitride substrate is pretreated and ionized by plasma spraying to generate Si3N4 particles, solving the problems of long molding time and poor density of traditional silicon nitride, and achieving high-density silicon nitride surface molding.

CN119020715AInactive Publication Date: 2024-11-26HENGYANG KAIXIN SPECIAL MATERIAL TECH CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202410319470.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-03-20
Publication Date
2024-11-26
Estimated Expiration
Not applicable · inactive patent

Smart Images

  • Figure CN119020715A_ABST
    Figure CN119020715A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of spraying processes, and particularly relates to a silicon nitride forming process based on plasma spraying, which comprises the following steps: S1, carrying out pretreatment such as cleaning, acid pickling, degreasing and drying on a base material, and placing the treated base material in a spraying area; s2, a base material is preheated, and surface treatment is conducted on the base material; s3, spraying a spraying base material on the base material subjected to surface treatment in S2; and S4, cleaning and detecting the base material sprayed in the step S3. According to the method, surface treatment is carried out on the base material, so that the adhesive force of the surface is improved, a foundation is provided for silicon nitride forming, silicon nitride particles are formed on the surface of the base material in an ion spraying mode, the forming speed is greatly reduced, the compactness of the formed silicon nitride surface reaches 99.85%, and the performance of a formed silicon nitride layer is effectively improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of spraying processes, and in particular relates to a silicon nitride forming process based on plasma spraying. Background Art

[0002] The most popular ultrafast sintering technology, spark plasma sintering (SPS), is mostly used to prepare nanostructured materials, amorphous materials, intermetallic compounds, metal matrices, and ceramic matrix composites. Compared with traditional sintering methods, spark plasma sintering (SPS) technology has a faster heating speed and can achieve the same sintering effect in a shorter sintering time. The rapid heating of materials prepared by spark plasma sintering (SPS) is due to the skin effect of the DC component and the AC component in the pulse current, as well as the small heat capacity of the heating system. During sintering, most of the heat is generated by the inner edge of the mold. The higher its temperature, the higher the temperature of the powder surface. In spark plasma sintering (SPS), the powder is placed in a graphite mold. While applying pressure to the powder, the current passes through the mold and the sample (if the latter is a conductive material) to heat the powder body. If the powder is a non-conductive material, the current mainly flows through the mold to generate heat. In addition to the ability to successfully prepare nanomaterials with no apparent grain growth due to lower sintering temperatures and shorter sintering times, the SPS process has the following advantages in the preparation of ceramic materials due to its unique heating system: it can clean grain boundaries, significantly increase superplasticity, reduce grain boundary segregation, enhance bonding quality, improve thermoelectric properties, and improve the ductility of alloy ceramics.

[0003] Silicon nitride-based ceramic materials have high fracture toughness and strength and excellent thermal shock resistance, corrosion resistance and wear resistance, and are widely used in the industrial field. Therefore, many researchers focus on how to use a suitable sintering method to prepare high-performance Si3N4-based ceramic materials. At present, the commonly used sintering methods for sintering silicon nitride ceramic materials are as follows: pressureless sintering, reaction sintering, gas pressure sintering (GPS), hot isostatic pressing (HIP) and hot pressing (HP) sintering. Chinese patent CN109516814A discloses a Si3N4 / SiC composite ceramic material and a preparation method thereof. The Si3N4 / SiC composite ceramic material is prepared by hot pressing sintering using Si3N4 and SiC as raw material powders, Tm2O3 and MgO as sintering aids. Although this method obtains a high-density Si3N4 / SiC ceramic material, its sintering time is long, and the surface tightness is poor after sintering. Summary of the invention

[0004] The present invention aims to provide a silicon nitride forming process based on plasma spraying to solve the technical problems of long forming time and poor surface density after forming of traditional silicon nitride.

[0005] In order to solve the above technical problems, the specific technical solutions of the present invention are as follows:

[0006] In some embodiments of the present application, a silicon nitride forming process based on plasma spraying is provided, comprising the following steps:

[0007] S1: pre-treat the substrate by cleaning, pickling, degreasing, drying, etc., and place the treated substrate in the spraying area;

[0008] S2: preheating the substrate and performing surface treatment on the substrate;

[0009] S3: spraying the spray base material on the substrate after the surface treatment in S2;

[0010] S4: Clean and inspect the substrate after spraying in S3.

[0011] In some embodiments of the present application, the pretreatment of the substrate in S1 includes the following steps:

[0012] S1.1: Place the substrate into an ultrasonic cleaner and add solvent for cleaning;

[0013] S1.2: The substrate treated in S1.1 is subjected to pickling and passivation treatment to remove the oxide scale, dirt and other impurities on the surface of the substrate and form a protective passivation film;

[0014] S1.3: Place the substrate treated in S1.2 in a degreasing solution for degreasing to remove grease from the surface of the substrate;

[0015] S1.4: Place the substrate treated in S1.3 in a drying oven to remove the attached liquid on the surface of the substrate.

[0016] In some embodiments of the present application, the surface treatment of the substrate in S2 is one or a combination of electrochemical treatment, sandblasting, application of adhesion promoter and polishing;

[0017] The temperature of the substrate pretreatment is 200-400°C.

[0018] In some embodiments of the present application, the preparation of the spray base material in S3 comprises the following steps:

[0019] S3.1: The inert gas is divided into three paths. The first path is injected into the vaporization device to carry SiCl4 into the reaction device; the second path enters from the top of the reaction device; and the third path enters from the side of the reaction device;

[0020] S3.2: heating and ionizing the inert gas entering the reaction device through the second and third paths;

[0021] S3.3: injecting the pretreated ammonia source into the reaction device to generate ammonia gas, and reacting the ammonia gas with SiCl4 to generate Si3N4 particles and HCl;

[0022] S3.4: Attach the generated Si3N4 particles to the substrate in the spraying area.

[0023] In some embodiments of the present application, in S4, the thickness, hardness, phase change and corrosion resistance of the silicon nitride layer on the surface of the substrate are detected by a scanning electron microscope, an X-ray diffractometer, etc.

[0024] In some embodiments of the present application, the pretreatment of the ammonia source in S3.3 includes: dehydration and purification.

[0025] In some embodiments of the present application, the reaction device is a combined structure, including:

[0026] A box body, wherein a spraying chamber is provided inside the box body, and an opening is provided at the top of the spraying chamber;

[0027] A reaction component, wherein the reaction component is arranged at the top of the box body, a reaction chamber is arranged inside the reaction component, and a first feed end and a second feed end are arranged on the reaction component;

[0028] The first feed end is connected to the discharge end of the gasification device;

[0029] The second feed end is used to receive ammonia gas;

[0030] A valve component, which is arranged at the opening of the spray chamber and is fixedly connected to the box body;

[0031] An ionization heating component is arranged on the top of the reaction component, the top of the ionization heating component is provided with a first air inlet end and the side of the ionization heating component is provided with a second air inlet end, and an ionization chamber is provided inside the ionization heating component;

[0032] The first air inlet end is connected to the second path, and the second air inlet end is connected to the third path;

[0033] A heating component, which is arranged in a matrix in the spray chamber and is fixedly connected to the box body;

[0034] A clamping component, which is arranged in the spraying chamber and is used to fix the position of the substrate;

[0035] The cooling component is arranged on the box body in a coiled shape and is connected to an external circulating cooling source.

[0036] In some embodiments of the present application, the ionization heating component is a combined structure, including:

[0037] A first shell, wherein the first shell is disposed on the reaction component and is fixedly connected to the reaction component, wherein a first chamber is disposed inside the first shell, and openings are disposed at the top and bottom of the first chamber;

[0038] A second shell, wherein the second shell is arranged at the opening at the top of the first shell, passes through the first shell to the first chamber, has a second chamber inside, and has a first air inlet end at the top;

[0039] The first chamber and the second chamber are interconnected to form an ionization chamber;

[0040] A second air inlet end, the second air inlet end is arranged on one side of the first shell, one end of the second air inlet end passes through the first shell to the first chamber, and the other end is connected to the third path;

[0041] A control valve component, the control valve component is arranged on the second air inlet end, and is used to control the air intake amount of the second air inlet end;

[0042] A coil component, wherein the coil component is sleeved on the first shell and is in contact with the first shell;

[0043] The radio frequency component is arranged on the first shell, and the radio frequency end of the radio frequency component passes through the first shell to the first cavity.

[0044] In some embodiments of the present application, the clamping component is a fixed structure, including:

[0045] The first driving components are arranged in a matrix in the spray chamber, are fixedly connected to the box body, and the rotation speeds of the first driving components are consistent;

[0046] A pull wire, one end of which is connected to the rotating end of the first driving component, and the other end of which is connected to the connection point of the substrate.

[0047] In some embodiments of the present application, the clamping component is a rotating structure, including:

[0048] A second driving component, which is symmetrically arranged in the spray chamber and fixedly connected to the box body;

[0049] The telescopic component is arranged on the rotating end of the second driving component, and a flexible component is also arranged on the telescopic end.

[0050] Compared with the prior art, the beneficial effect of the present invention lies in that the surface adhesion of the substrate is improved by surface treatment, and a basis is provided for silicon nitride molding. Silicon nitride particles are molded on the surface of the substrate by ion spraying, which not only greatly reduces the molding rate, but also the surface density of the silicon nitride after molding reaches 99.85%, thereby effectively improving the performance of the silicon nitride layer after molding. BRIEF DESCRIPTION OF THE DRAWINGS

[0051] Various other advantages and benefits will become apparent to those of ordinary skill in the art by reading the detailed description of the preferred embodiments below. The accompanying drawings are only for the purpose of illustrating the preferred embodiments and are not to be considered as limiting the present invention. Moreover, the same reference symbols are used throughout the accompanying drawings to represent the same components. In the accompanying drawings:

[0052] Figure 1 A schematic diagram of a process flow provided by an embodiment of the present invention;

[0053] Figure 2 A schematic diagram of the overall structure provided for an embodiment of the present invention;

[0054] Figure 3 A schematic diagram of the overall structure of a reaction device provided in an embodiment of the present invention;

[0055] Figure 4 A schematic diagram of the structure of an ionization heating component provided in an embodiment of the present invention;

[0056] Figure 5 A schematic diagram of a structure in which the clamping component provided in an embodiment of the present invention is fixed;

[0057] Figure 6 The clamping member provided in the embodiment of the present invention is a schematic structural diagram of a rotating type.

[0058] Inert gas 1, first path 101, second path 102, third path 103, vaporization device 2, reaction device 3, box 301, reaction component 4, first feed end 401, second feed end 402, valve component 5, ionization heating component 6, first air inlet end 6021, second air inlet end 6011, first shell 601, second shell 602, control valve component 603, coil component 604, radio frequency component 605, heating component 7, clamping component 8, cooling component 9, substrate 10, ammonia source 11, first drive component 801, pull wire 802, second drive component 803, telescopic component 804, flexible component 805. DETAILED DESCRIPTION

[0059] The specific implementation of the present invention is further described in detail below in conjunction with the accompanying drawings and examples. The following examples are used to illustrate the present invention, but are not intended to limit the scope of the present invention.

[0060] In order to better understand the purpose, structure and function of the present invention, the following Figure 1-6 , the present invention is further described in detail.

[0061] According to some embodiments of the present application, the following steps are included:

[0062] S1: pre-treating the substrate 10 by cleaning, pickling, degreasing, drying, etc., and placing the treated substrate 10 in a spraying area;

[0063] The pretreatment of the substrate 10 specifically includes the following steps:

[0064] S1.1: Place the substrate 10 in an ultrasonic cleaner and add a solvent for cleaning, that is, place the substrate 10 in an ultrasonic cleaner and add a solvent for the first cleaning. After cleaning for a period of time (5-10 minutes), remove the substrate 10 and remove the loose materials on the surface of the substrate 10 by a brush or the like. After removal, place the substrate 10 in an ultrasonic cleaner again and perform a second cleaning. After the second cleaning is completed, take out the substrate 10 and remove the solvent on the surface of the substrate 10 (by drying, air blowing, wiping, etc., which are not limited here);

[0065] S1.2: The substrate 10 treated by S1.1 is subjected to pickling and passivation treatment to remove scale, dirt and other impurities on the surface of the substrate 10 and form a protective passivation film, that is, the substrate 10 is placed in a container filled with an acidic solvent, and the acidic solution reacts with the surface of the substrate 10 to remove dirt such as oil, rust, scale, welding spot, etc. on the surface of the substrate 10, and a uniform and dense passivation film is formed on the surface of the substrate 10. The acidic solution can be citric acid, nitric acid, etc., and the specific type of the acidic solution is selected according to the material of the substrate 10, and is not limited here.

[0066] S1.3: Place the substrate 10 treated by S1.2 in a degreasing liquid for degreasing treatment to remove the grease on the surface of the substrate 10, that is, place the substrate 10 after the pickling and passivation treatment in a container filled with degreasing liquid, and use the degreasing liquid to dissolve, saponify or emulsify the grease on the surface of the substrate 10, so as to remove the grease components on the surface of the substrate 10. It should be noted that the degreasing liquid preferably uses an alkaline degreasing liquid. By using a degreasing liquid with an alkaline component, the acidic solution on the surface of the substrate 10 is neutralized to stop the pickling process, and at the same time, the acidic solution on the surface of the substrate 10 is prevented from affecting the effect of the degreasing treatment.

[0067] S1.4: placing the substrate 10 treated in S1.3 in a drying oven to remove the attached liquid on the surface of the substrate 10, that is, placing the substrate 10 treated in S1.3 in a drying oven to evaporate the residual degreasing liquid on the surface of the substrate 10.

[0068] S2: preheating the substrate 10 and performing surface treatment on the substrate 10, that is, placing the substrate 10 on an operating table, treating the surface of the substrate 10 by one or a combination of electrochemical treatment, sandblasting, applying an adhesion promoter, and polishing, so as to improve the adhesion of the surface of the substrate 10, and the type of specific treatment method is selected according to the material of the substrate 10. When the substrate 10 is made of metal, an electrochemical treatment method is used, the substrate 10 is placed in an electrolyte, and the substrate 10 is used as an anode. An oxide film is formed on the surface of the substrate 10 by anodization, so as to improve the adhesion of the surface of the substrate 10, wherein the metal material can also be treated by the other methods.

[0069] Quartz sand, white corundum, brown corundum, black corundum, etc. can be used as sand in the sand blasting process.

[0070] The type of accelerator may be resinous, water-soluble, polymeric, etc., and is specifically selected according to the material of the substrate 10 .

[0071] Grinding is to roughen the surface of the substrate 10 by using high-grit sandpaper or water sand.

[0072] After the surface treatment, the substrate 10 is placed in a drying oven and heated to 200-400°C, preferably to 360°C. The preheated substrate 10 is placed in a spraying area. By preheating the substrate 10, it is avoided that the spray base material directly contacts the low-temperature substrate 10, causing cracks on the surface of the substrate 10 and the problem of being unable to condense. By heating the substrate 10 to 360°C, the spray base material can condense on the surface of the substrate 10 to the greatest extent.

[0073] S3: spraying the spray base material on the substrate 10 after the surface treatment in S2, and the spray base material condenses silicon nitride on the surface of the substrate 10 by ionization convection, thereby forming a dense silicon nitride layer on the surface of the substrate 10;

[0074] S4: Clean and inspect the substrate 10 after spraying in S3, that is, inspect the thickness, hardness, phase change and corrosion resistance of the silicon nitride layer on the surface of the substrate 10 by scanning electron microscopy, X-ray diffractometer, etc.

[0075] It should be further explained that in order to further improve the wear resistance of the prepared product, a protective layer can be added to the surface of the product. The type of the protective layer can be paraffin, epoxy resin, silicone resin, etc., and the specific selection is based on actual needs.

[0076] Through the above technical solution, the technical effects produced in the embodiments of the present application are:

[0077] By pretreating the substrate 10, the cleanliness and adhesion of the surface of the substrate 10 are improved to facilitate the condensation of the spray base material on the surface of the substrate 10. By adopting the convection ionization method, the spray base material can be quickly combined with the base material to form a spray layer. The spray layer has the characteristics of dense coating and high bonding strength, which provides a basis for shortening the silicon nitride molding time and improving the surface density of silicon nitride.

[0078] The technical features in the above embodiments are adopted in the embodiments of the present application, wherein the preparation of the spray base material in S3 includes the following steps:

[0079] S3.1: The inert gas 1 is divided into three paths. The first path 101 is injected into the vaporization device 2 and carries SiCl4 into the reaction device 3. The second path 102 enters from the top of the reaction device 3. The third path 103 enters from the side of the reaction device 3. The inert gas 1 can use Ar as the gas source, but is not limited to this. The argon gas is divided into three paths. One path passes through the vaporization device 2 and carries SiCl4 into the reaction device 3.

[0080] S3.2: The inert gas 1 entering the reaction device 3 through the second path 102 and the third path 103 is heated and ionized. The second path 102 enters directly from the top of the reaction device 3, and the third path 103 enters from the side of the reaction device 3. The gases entering through the second path 102 and the third path 103 are ionized and heated through the structure inside the reaction device 3 to form a high-temperature plasma with a certain degree of ionization. The gas in the third path 103 enters periodically, which has the effect of cooling the inversion device for the gas with a temperature lower than that in the reaction device 3. It should be noted that the periodicity is controlled according to actual needs, and a control device is also provided to control the on and off of the gas in the third path 103, so as to adjust the internal temperature of the reaction device 3.

[0081] S3.3: injecting the pre-treated ammonia source 11 into the reaction device 3 to generate ammonia gas, and reacting the ammonia gas with SiCl4 to generate Si3N4 particles and HCl. The ammonia source 11 is aqueous ammonia, which generates ammonia gas by reacting with sodium hydroxide, and is dried and purified so that the generated ammonia gas does not contain impurities (including water). After entering the reaction device 3, the ammonia gas is ionized and reacts with SiCl4 to generate Si3N4 particles and HCl. The generated Si3N4 particles fall with the airflow;

[0082] S3.4: Attach the generated Si3N4 particles to the substrate 10 in the spraying area.

[0083] Through the above technical solution, the technical effects produced in the embodiments of the present application are:

[0084] The inert gas 1 is divided into three paths, one of which carries SiCl4 into the reaction device 3, and the gases of the second path 102 and the third path 103 enter the reaction device 3 to generate a high-temperature plasma with a certain degree of ionization, and the SiCl4 entering reacts with ammonia to generate Si3N4 particles and HCl. The generated Si3N4 particles descend with the airflow, and the gas of the third path 103 cools the reaction device 3 to avoid damage caused by excessive temperature of the reaction device 3, thereby improving the stability of the operation of the reaction device 3 and providing a basis for shortening the silicon nitride molding time and improving the surface density of silicon nitride.

[0085] The technical features of the above embodiments are adopted in the embodiments of the present application, wherein the reaction device 3 is a combined structure, including:

[0086] A box body 301, wherein a spraying chamber is provided inside the box body 301, and an opening is provided at the top of the spraying chamber;

[0087] The reaction component 4 is a reaction box structure, which is made of high temperature and high pressure resistant materials. The reaction component 4 is arranged on the top of the box body 301, and a reaction chamber is arranged inside it, and a first feed end 401 and a second feed end 402 are arranged on it; the first feed end 401 is connected to the discharge end of the gasification device; the second feed end 402 is used to receive ammonia, that is, the reaction chamber is used for SiCl4 and ammonia to react;

[0088] The valve component 5 is a solenoid valve structure, which is arranged at the opening of the spray chamber and is fixedly connected to the box body 301. The valve component 5 controls the on-off between the reaction chamber and the spray chamber.

[0089] The ionization heating component 6 is a quartz reactor, and the ionization heating component 6 is arranged on the top of the reaction component 4, and a first air inlet end 6021 is arranged on the top, a second air inlet end 6011 is arranged on the side, and an ionization chamber is arranged inside the ionization heating component 6; the first air inlet end 6021 is connected to the second path 102, and the second air inlet end 6011 is connected to the third path 103;

[0090] It should be noted that the ionization heating component 6 is a combined structure, including:

[0091] The first shell 601 is a hollow columnar structure with openings at both ends. The first shell 601 is disposed on the reaction component 4 and is fixedly connected to the reaction component 4. A first chamber is disposed inside the first shell 601, and openings are disposed at the top and bottom of the first chamber.

[0092] The second shell 602 is a hollow columnar structure with openings at both ends. The second shell 602 is arranged at the opening at the top of the first shell 601, and penetrates the first shell 601 to the first chamber. The second chamber is arranged inside the second shell 601, and the first air inlet end 6021 is arranged at the top of the second shell 602. The first air inlet end 6021 is connected to the second path 102, and the argon gas in the second path 102 is transferred to the second chamber and enters the first chamber.

[0093] The first chamber and the second chamber are interconnected to form an ionization chamber;

[0094] The second air inlet end 6011 is a hollow tubular structure, and the second air inlet end 6011 is disposed on one side of the first shell 601, one end of which passes through the first shell 601 to the first chamber, and the other end is connected to the third path 103;

[0095] The control valve component 603 is a valve structure that can change the cross-sectional opening area of ​​the second air inlet end 6011. The control valve component 603 is disposed on the second air inlet end 6011 and is used to control the air intake amount of the second air inlet end 6011. The air intake amount of the second air inlet end 6011 is controlled by the control valve component 603, thereby cooling the first shell 601 and the second shell 602.

[0096] The coil component 604 is a heating induction coil, which is sleeved on the first shell 601 and in contact with the first shell 601. The coil component 604 heats the gas in the ionization chamber to make the gas have a high temperature.

[0097] The RF component 605 is a RF plasma device. The RF component 605 is disposed on the first shell 601 , and its RF end penetrates the first shell 601 to the first chamber, so that plasma with a certain degree of ionization is generated in the ionization chamber.

[0098] The heating component 7 is a heating plate, which is arranged in a matrix in the spraying chamber and is fixedly connected to the box 301. It is used to generate high temperature in the spraying chamber so that the Si3N4 particles are attached to the substrate 10.

[0099] A clamping component 8 is provided in the spraying chamber and is used to fix the position of the substrate 10. The substrate 10 is clamped by the clamping component 8 to prevent the substrate 10 from shaking due to the influence of the airflow, thereby affecting the combination of the Si3N4 particles and the substrate 10;

[0100] The cooling component 9 is a circulating cold water pipe structure, which is arranged on the box body 301 in a coiled shape and connected to an external circulating cooling source, that is, the box body 301 is cooled by the cooling component 9 to prevent the box body 301 from being overheated;

[0101] It should be noted that the thickness of silicon nitride on the substrate 10 is 0.2-0.7 mm; the gas flow rate entering the first path 101, the second path 102 and the third path 103 is 1-150 L / min, the output power of the radio frequency component 605 is 7-11 Kw, preferably 11 Kw, and its frequency is 4 MHz; the purity of argon is 99%; the purity of ammonia is 99.9%; the heating component 7 is divided into three stages, when it is on the eve of spraying, its heating makes the temperature in the spraying chamber at 3 60℃; when in the spraying process, it heats the temperature in the spraying chamber to 1300-1500℃, preferably 1380℃; when the spraying is completed, it heats the temperature in the spraying chamber to 600-800℃, and then cools down after 30 minutes. The spraying chamber is heated by the heating component 7 to accelerate the combination of the substrate 10 and the Si3N4 particles, while removing NH4Cl impurities, and the substrate 10 after spraying is kept warm to make the combination more stable.

[0102] Through the above technical solution, the technical effects produced in the embodiments of the present application are:

[0103] The flow rate and spraying range of Si3N4 particles are controlled by valve component 5 so as to better combine with substrate 10. The second air inlet end 6011 is controlled by control valve component 603 to cool the first shell 601 and the second shell 602 to ensure the stability of the ionization process. The spraying chamber is heated and controlled by heating component 7 to ensure the combination of substrate 10 and Si3N4 particles and improve the stability of the combination process, thereby shortening the silicon nitride molding time and improving the surface density of silicon nitride after molding.

[0104] The embodiment of the present application adopts the technical features of the above embodiment, wherein the clamping component 8 is a fixed structure, including:

[0105] The first driving components 801 are stepping motors or servo motors. The first driving components 801 are arranged in a matrix in the spray chamber, and are fixedly connected to the box body 301. The rotation speeds of the first driving components 801 are consistent.

[0106] The pull wire 802 is a high temperature resistant linear structure. One end of the pull wire 802 is connected to the rotating end of the first driving component 801 , and the other end is connected to the connection point of the substrate 10 .

[0107] Through the above technical solution, the technical effects produced in the embodiments of the present application are:

[0108] The first driving component 801 drives the pull wire 802 to be retracted, so that the pull wire 802 is in a taut state, and then the substrate 10 is tightened and fixed so that the substrate 10 will not shake in the airflow, thereby facilitating better combination of the substrate 10 with the Si3N4 particles, thereby improving the stability and accuracy of silicon nitride molding.

[0109] The embodiment of the present application adopts the technical features of the above embodiment, wherein the clamping component 8 is a rotating structure, including:

[0110] The second driving component 803 is a stepping motor or a servo motor. The second driving component 803 is symmetrically arranged in the spraying chamber and is fixedly connected to the box body 301.

[0111] The telescopic component 804 is a telescopic cylinder or a mechanical telescopic device, which is arranged on the rotating end of the second driving component 803. A flexible component 805 (a high temperature resistant block structure, whose shape is selected according to the shape of the substrate 10) is also provided on the telescopic end.

[0112] Through the above technical solution, the technical effects produced in the embodiments of the present application are:

[0113] The substrate 10 is clamped by the telescopic component 804, so that the second driving component 803 drives the substrate 10 to rotate, so that the substrate 10 can be combined with the Si3N4 particles in all directions, avoiding the problem that the substrate 10 can only be combined with the Si3N4 particles on one side after being fixed, thereby improving the stability of silicon nitride molding and making it more applicable.

[0114] In the description of the present application, it should be understood that the terms "center", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.

[0115] The terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, unless otherwise specified, "plurality" means two or more.

[0116] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0117] In this specification, each embodiment is described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the embodiments can be referred to each other. For the device disclosed in the embodiment, since it corresponds to the method disclosed in the embodiment, the description is relatively simple, and the relevant parts can be referred to the method part.

[0118] The above description of the disclosed embodiments enables one skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A silicon nitride forming process based on plasma spraying, characterized in that: The following steps are involved: S1: pre-treat the substrate by cleaning, pickling, degreasing, drying, etc., and place the treated substrate in the spraying area; S2: preheating the substrate and performing surface treatment on the substrate; S3: spraying the spray base material on the substrate after the surface treatment in S2; S4: Clean and inspect the substrate after spraying in S3.

2. The silicon nitride forming process based on plasma spraying according to claim 1, characterized in that: The pretreatment of the substrate in S1 comprises the following steps: S1.1: Place the substrate into an ultrasonic cleaner and add solvent for cleaning; S1.2: The substrate treated in S1.1 is subjected to pickling and passivation treatment to remove the oxide scale, dirt and other impurities on the surface of the substrate and form a protective passivation film; S1.3: Place the substrate treated in S1.2 in a degreasing solution for degreasing to remove grease from the surface of the substrate; S1.4: Place the substrate treated in S1.3 in a drying oven to remove the attached liquid on the surface of the substrate.

3. The silicon nitride forming process based on plasma spraying according to claim 1, characterized in that: The surface treatment of the substrate in S2 is one or a combination of electrochemical treatment, sandblasting, application of adhesion promoter and polishing; The temperature of the substrate pretreatment is 200-400°C.

4. The silicon nitride forming process based on plasma spraying according to claim 1, characterized in that: The preparation of the spray base material in S3 comprises the following steps: S3.1: The inert gas is divided into three paths. The first path is injected into the vaporization device to carry SiCl4 into the reaction device; the second path enters from the top of the reaction device; and the third path enters from the side of the reaction device; S3.2: heating and ionizing the inert gas entering the reaction device through the second and third paths; S3.3: injecting the pretreated ammonia source into the reaction device to generate ammonia gas, and reacting the ammonia gas with SiCl4 to generate Si3N4 particles and HCl; S3.4: Attach the generated Si3N4 particles to the substrate in the spraying area.

5. The silicon nitride forming process based on plasma spraying according to claim 1, characterized in that: In the S4, the thickness, hardness, phase change and corrosion resistance of the silicon nitride layer on the surface of the substrate are detected by a scanning electron microscope, an X-ray diffractometer or the like.

6. The silicon nitride forming process based on plasma spraying according to claim 4, characterized in that: The pretreatment of the ammonia source in S3.3 includes: dehydration and purification.

7. The silicon nitride forming process based on plasma spraying according to claim 4, characterized in that: The reaction device is a combined structure, comprising: A box body, wherein a spraying chamber is provided inside the box body, and an opening is provided at the top of the spraying chamber; A reaction component, wherein the reaction component is arranged at the top of the box body, a reaction chamber is arranged inside the reaction component, and a first feed end and a second feed end are arranged on the reaction component; The first feed end is connected to the discharge end of the gasification device; The second feed end is used to receive ammonia gas; A valve component, which is arranged at the opening of the spray chamber and is fixedly connected to the box body; An ionization heating component is arranged on the top of the reaction component, the top of the ionization heating component is provided with a first air inlet end and the side of the ionization heating component is provided with a second air inlet end, and an ionization chamber is provided inside the ionization heating component; The first air inlet end is connected to the second path, and the second air inlet end is connected to the third path; A heating component, which is arranged in a matrix in the spray chamber and is fixedly connected to the box body; A clamping component, which is arranged in the spraying chamber and is used to fix the position of the substrate; The cooling component is arranged on the box body in a coiled shape and is connected to an external circulating cooling source.

8. The silicon nitride forming process based on plasma spraying according to claim 7, characterized in that: The ionization heating component is a combined structure, comprising: A first shell, wherein the first shell is disposed on the reaction component and is fixedly connected to the reaction component, wherein a first chamber is disposed inside the first shell, and openings are disposed at the top and bottom of the first chamber; A second shell, wherein the second shell is arranged at the opening at the top of the first shell, passes through the first shell to the first chamber, has a second chamber inside, and has a first air inlet end at the top; The first chamber and the second chamber are interconnected to form an ionization chamber; A second air inlet end, the second air inlet end is arranged on one side of the first shell, one end of the second air inlet end passes through the first shell to the first chamber, and the other end is connected to the third path; A control valve component, the control valve component is arranged on the second air inlet end, and is used to control the air intake amount of the second air inlet end; A coil component, wherein the coil component is sleeved on the first shell and is in contact with the first shell; The radio frequency component is arranged on the first shell, and the radio frequency end of the radio frequency component passes through the first shell to the first cavity.

9. The silicon nitride forming process based on plasma spraying according to claim 7, characterized in that: The clamping component is a fixed structure, comprising: The first driving components are arranged in a matrix in the spray chamber, are fixedly connected to the box body, and the rotation speeds of the first driving components are consistent; A pull wire, one end of which is connected to the rotating end of the first driving component, and the other end of which is connected to the connection point of the substrate.

10. The silicon nitride forming process based on plasma spraying according to claim 7, characterized in that: The clamping component is a rotating structure, comprising: A second driving component, which is symmetrically arranged in the spray chamber and fixedly connected to the box body; The telescopic component is arranged on the rotating end of the second driving component, and a flexible component is also arranged on the telescopic end.

Citation Information

Patent Citations

  • Si3N4 / SiC multiphase ceramic material and preparation method thereof

    CN109516814A

  • Corrosion resistance thermal treatment method for steel

    CN105349738A

  • Silicon nitride spraying device

    CN116197076A

  • Method for preparing silicon nitride powder by continuous ammonolysis method

    CN116693301A