Rapid identification method for shear cracks and internal layering of thick plate product
By combining a digital micrometer and an ultrasonic thickness gauge, shear cracks and internal delamination in steel plates can be quickly identified, solving the problems of long judgment cycles and high costs in existing technologies, and achieving efficient defect identification and improved yield.
Patent Information
- Application Number
- CN202411128029.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-16
- Publication Date
- 2024-11-26
AI Technical Summary
Existing technologies have long turnaround times and high costs when identifying shear cracks and internal delamination in steel plates, and the fire cutting process may damage the quality of the steel plate, resulting in a low yield.
By combining a digital micrometer and an ultrasonic thickness gauge, shear cracks and internal delamination can be quickly identified by calibrating and measuring the thickness of the steel plate, and the type of defect can be determined by the difference in readings of the ultrasonic thickness gauge.
It enables rapid and accurate identification of steel plate defects, avoids the fire cutting process, reduces costs, increases yield, and improves logistics management efficiency.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of steel plate quality detection, and in particular to a method for quickly identifying shear cracks and internal delamination of thick plate products. Background Art
[0002] At present, in the production process of wide and thick plates, since some steel types such as Q420qD are sensitive to temperature during the shearing process, steel plates with small width margins are prone to cracks visible to the naked eye after shearing under the action of shear stress, but the depth extending to the inside of the steel plate is shallow, about 1-2mm. However, based on the morphology and distribution of the steel plate defects, it is impossible to intuitively determine whether it is a shear crack or an internal delamination defect of the steel plate. Under normal circumstances, additional flaw detection processes will be added for such defective steel plates, specifically: using automatic ultrasonic equipment to identify the flaw detection map or adding a fire cutting process to remove it and then perform penetrant flaw detection. Based on the traditional flaw detection process, on the one hand, when the steel plate has an internal delamination defect, it can be judged and identified through the flaw detection map, and when the steel plate has a shear crack defect, the flaw detection map can only show slight defects on the edge or no defects. The reason is that the defect extends to the shallower edge of the steel plate, which is difficult to cover by the equipment probe, and there is a defect judgment cycle. At the same time, the shear crack defect of the steel plate must be cleared by grinding or cutting, and the inaccurate and stable determination of the atlas recognition will lead to the flow of unqualified products to users, and there are problems in production quality control. On the other hand, since the width margin of the steel plate cut by the double-sided shear is generally about 7mm, and the upper limit of the contract width is 15mm, after the additional fire cutting process, the quality of the steel plate will be affected due to the existence of more uncertain factors, or the steel plate cannot be processed subsequently. When the steel plate has a shear crack defect, the fire cutting process can remove the defect, but it is very likely that the steel plate width will be shortened due to the fire cutting process, so that the width margin of the steel plate is not enough to be processed out of the contract. When the steel plate has an internal stratification defect, the fire cutting process cannot effectively and completely remove the defect, nor can it be determined whether the specific location of the removal has removed the defect, which is not conducive to the first-time qualitative analysis. Multiple fire cutting processes will damage the steel plate and reduce the yield rate of the steel plate. Summary of the invention
[0003] The purpose of the present invention is to provide a method for quickly identifying shear cracks and internal delamination of thick plate products, which can solve the problems of cumbersome traditional flaw detection operation methods, long defect determination cycle, and being unfavorable to logistics management and cost control.
[0004] In order to achieve the above object, the present invention adopts the following technical solution: A method for quickly identifying shear cracks and internal delamination of thick plate products comprises the following steps: Step 1: Use a digital micrometer to measure the thickness of the intact part of the steel plate; Step 2: Adjust the working mode of the ultrasonic thickness gauge to the calibration mode; Step 3: Place the probe of the ultrasonic thickness gauge on the intact part of the steel plate currently measured by the digital micrometer, and apply appropriate pressure; Step 4: Observe and record the coupling status indication and thickness reading displayed on the display screen of the ultrasonic thickness gauge; Step 5: Compare the thickness reading obtained in step 4 with the thickness reading obtained in step 1. If the thickness readings are different, press the increment button or decrement button of the ultrasonic thickness gauge to increase or decrease the thickness reading of the ultrasonic thickness gauge until it is the same as the thickness reading of the digital micrometer. Step 6: Adjust the working mode of the ultrasonic thickness gauge to the measurement mode, and record the thickness reading of the intact part of the steel plate measured by the ultrasonic thickness gauge; Step 7: Move the ultrasonic thickness gauge to the crack defect of the steel plate, and apply appropriate pressure to the ultrasonic thickness gauge. At this time, the reading of the ultrasonic thickness gauge is about half of the thickness of the steel plate. Then move the ultrasonic thickness gauge to multiple positions in the direction of the middle of the steel plate, and measure and record the thickness readings at different positions. If the multiple thickness readings are basically consistent with the thickness readings of the intact part of the steel plate and there is no obvious change, it is judged as a shear crack defect. If the multiple thickness readings are about half of the thickness of the steel plate, it is judged as an internal delamination defect.
[0005] Preferably, in step three, if the thickness reading is unstable, the position or contact pressure of the ultrasonic thickness gauge probe on the intact part of the steel plate is appropriately adjusted until the thickness reading is stable.
[0006] Preferably, in the step seven, during the multi-position movement of the ultrasonic thickness gauge toward the middle of the steel plate, the distance of each movement is 1 to 2 mm.
[0007] The beneficial effects of the present invention are as follows: the present method can quickly identify whether the crack defect in the cross section of the steel plate is caused by the stress during the shearing process or by the delamination caused by the internal quality defects of the steel plate; the present method does not require the use of a fire cutting process and will not affect the quality of the steel plate. At the same time, compared with the automatic ultrasonic equipment flaw detection pattern recognition method, the present method has higher accuracy and stability, effectively speeds up logistics management, greatly reduces costs, and improves the yield rate of steel plates. DETAILED DESCRIPTION
[0008] The technical solutions in the embodiments of the present invention are described below.
[0009] A method for quickly identifying shear cracks and internal delamination of thick plate products comprises the following steps: Step 1: Use a digital micrometer to measure the thickness of the intact part of the steel plate, where the thickness of the intact part of the steel plate is 50 mm; Step 2: Adjust the working mode of the ultrasonic thickness gauge to the calibration mode; Step 3: Place the probe of the ultrasonic thickness gauge on the intact part of the steel plate currently measured by the digital micrometer, and apply appropriate pressure; Step 4: Observe and record the coupling status indication and thickness reading displayed on the display screen of the ultrasonic thickness gauge. If the thickness reading is unstable, properly adjust the position or contact pressure of the ultrasonic thickness gauge probe on the intact part of the steel plate until the thickness reading is stable. Step 5: Compare the thickness reading obtained in step 4 with the thickness reading obtained in step 1. If the thickness readings are different, press the increment button or decrement button of the ultrasonic thickness gauge to increase or decrease the thickness reading of the ultrasonic thickness gauge until it is the same as the thickness reading of the digital micrometer. Step 6: Adjust the working mode of the ultrasonic thickness gauge to the measurement mode, and record the thickness reading of the intact part of the steel plate as 50mm; Step 7: Move the ultrasonic thickness gauge to the crack defect of the steel plate, and apply appropriate pressure to the ultrasonic thickness gauge. At this time, the reading of the ultrasonic thickness gauge is about half of the thickness of the steel plate, that is, about 25mm. Then move the ultrasonic thickness gauge to multiple positions in the direction of the middle of the steel plate, and the distance of each movement is 1-2mm. Measure and record the thickness readings at different positions. If the multiple thickness readings are basically consistent with the thickness readings of the intact part of the steel plate, that is, about 50mm, and there is no obvious change, it is judged as a shear crack defect. If the multiple thickness readings are about half of the thickness of the steel plate, that is, about 25mm, it is judged as an internal delamination defect. Among them, if the thickness reading is discontinuously displayed as 25mm, it is an internal defect. If the thickness reading is continuously displayed as 25mm, it is a delamination defect.
[0010] It should be noted that the present method can be used to quickly identify whether the crack defect of the steel plate is a shear crack defect or an internal delamination defect. If it is determined to be a shear crack defect, it can be directly removed by grinding the edge 1 to 2 mm to ensure the same width. If it is determined to be an internal delamination defect, the steel plate can be directly deconstructed and downgraded. The entire defect determination cycle is short, and effective treatment methods can be quickly adopted for the corresponding defects to prevent unqualified products from flowing to users.
Claims
1. A method for rapid identification of shear cracks and internal delamination of thick plate products, characterized in that: The following steps are involved: Step 1: Use a digital micrometer to measure the thickness of the intact part of the steel plate; Step 2: Adjust the working mode of the ultrasonic thickness gauge to the calibration mode; Step 3: Place the probe of the ultrasonic thickness gauge on the intact part of the steel plate currently measured by the digital micrometer, and apply appropriate pressure; Step 4: Observe and record the coupling status indication and thickness reading displayed on the display screen of the ultrasonic thickness gauge; Step 5: Compare the thickness reading obtained in step 4 with the thickness reading obtained in step 1. If the thickness readings are different, press the increment button or decrement button of the ultrasonic thickness gauge to increase or decrease the thickness reading of the ultrasonic thickness gauge until it is the same as the thickness reading of the digital micrometer. Step 6: Adjust the working mode of the ultrasonic thickness gauge to the measurement mode, and record the thickness reading of the intact part of the steel plate measured by the ultrasonic thickness gauge; Step 7: Move the ultrasonic thickness gauge to the crack defect of the steel plate, and apply appropriate pressure to the ultrasonic thickness gauge. At this time, the reading of the ultrasonic thickness gauge is about half of the thickness of the steel plate. Then move the ultrasonic thickness gauge to multiple positions in the direction of the middle of the steel plate, and measure and record the thickness readings at different positions. If the multiple thickness readings are basically consistent with the thickness readings of the intact part of the steel plate and there is no obvious change, it is judged as a shear crack defect. If the multiple thickness readings are about half of the thickness of the steel plate, it is judged as an internal delamination defect.
2. The method for rapid identification of shear cracks and internal delamination of thick plate products according to claim 1 is characterized in that: In the step 3, if the thickness reading is unstable, the position or contact pressure of the ultrasonic thickness gauge probe on the intact part of the steel plate is appropriately adjusted until the thickness reading is stable.
3. The method for rapid identification of shear cracks and internal delamination of thick plate products according to claim 1 is characterized in that: In the step seven, during the process of the ultrasonic thickness gauge moving to multiple positions toward the middle of the steel plate, the distance of each movement is 1 to 2 mm.