Welding auxiliary component

By designing the guide groove, avoidance groove and welding hole of welding auxiliary components, combined with the cooling air duct, the problems of not being tightly bonded to the skeleton and filter membrane and uneven welding heat during the welding process of the spiral filter element are solved, and the strength of the filter element is significantly improved and Service life ensures its reliability in demanding environments.

CN119035893AActive Publication Date: 2024-11-29SICHUAN YIJUWEI TECHNOLOGY CO LTD
View PDF 14 Cites 0 Cited by

Patent Information

Application Number
CN202411526608.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-30
Publication Date
2024-11-29
Estimated Expiration
2044-10-30

AI Technical Summary

Technical Problem

The existing spiral filter element welding process has quality defects caused by the incomplete bonding of the frame and the filter membrane and the uneven welding heat control, which affects the strength and service life of the filter element.

Method used

A welding auxiliary component is designed, including a guide groove, a first avoidance groove and a welding hole, to ensure that the filter element maintains stability and flexibility during the welding process, to accurately dock the welding electrode, and to improve welding quality with the cooling air duct.

Benefits of technology

It effectively solves the quality defects in the welding process, improves the overall strength and service life of the filter element, and ensures its reliable filtration performance in high-demand environments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119035893A_ABST
    Figure CN119035893A_ABST
Patent Text Reader

Abstract

The invention provides a welding auxiliary component, and relates to the technical field of filter element production, the welding auxiliary component comprises a component body, the component body is provided with a guide groove and a first avoiding groove, the guide groove is used for being matched with the peripheral wall of a leading-out roller to form a material channel, and the material channel is used for allowing a formed spiral filter element to pass through; the first avoiding groove is formed in the guide groove, and the first avoiding groove partially coincides with a spiral moving path of a framework of the spiral filter element on the lead-out roller so as to avoid the framework; and a welding hole is formed in the first avoiding groove and is used for realizing the matching of a welding electrode on the lead-out roller and a welding electrode on the bonding pad so as to weld the framework and the filter membrane. Compared with the prior art, the spiral filter element forming device has the advantage that the problem of quality defects after spiral filter elements are formed can be solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of filter element production, and in particular to a welding auxiliary component. Background Art

[0002] Spiral filter elements are widely used in industries such as oil and gas, agriculture, medical treatment, aerospace and navigation, chemical industry, and food processing, and are mainly used in pipelines, filtration systems, and high-precision equipment. These fields have strict requirements on the strength, corrosion resistance, filtration accuracy, and durability of spiral filter elements, and the market demand is growing.

[0003] The spiral filter element is generally manufactured by a related welding device. In the related technology, the welding device has a lead-out roller and a welding pad. After the filter membrane and the frame are spirally wound and formed, the frame and the filter membrane of the formed spiral filter element need to be welded to improve the forming stability of the frame and the filter membrane. In the process of realizing the present invention, the applicant found that the quality of the spiral filter element after welding has quality defects. Summary of the invention

[0004] In order to solve the problem of quality defects after the spiral filter element is formed, the present application provides a welding auxiliary component.

[0005] In a first aspect, the present application provides a welding auxiliary component, which adopts the following technical solution: A welding auxiliary component includes a component body, wherein the component body has a guide groove and a first avoidance groove, wherein the guide groove is used to cooperate with the peripheral wall of a lead-out roller to form a material channel, and the material channel is used for a formed spiral filter element to pass through; the first avoidance groove is arranged in the guide groove, and the first avoidance groove partially overlaps with the spiral moving path of the skeleton of the spiral filter element on the lead-out roller to achieve avoidance of the skeleton; a welding hole is arranged in the first avoidance groove, and the welding hole is used to achieve the cooperation between the welding electrode on the lead-out roller and the welding electrode on the welding pad to weld the skeleton to the filter membrane.

[0006] Preferably, the component body further comprises a cooling air duct for introducing cooling air flow, and an air outlet of the cooling air duct is arranged on the inner wall of the welding hole.

[0007] Preferably, the cooling air duct includes an axially connected insertion section and a guide section, the insertion section is used for inserting an external air duct, and one end of the guide section away from the insertion section opens toward the mating position of the welding electrode on the lead-out roller and the welding electrode on the welding pad; the inner diameter of the insertion section is larger than the inner diameter of the guide section to limit the external air duct from entering the guide section.

[0008] Preferably, the matching position of the welding electrode on the welding pad and the welding electrode on the lead-out roller is a welding point, and the extension path of the cooling air duct is tangent to the outer peripheral contour line of the welding pad at the welding point.

[0009] Preferably, the lowest point of the bottom wall of the first avoidance groove is below the extension path of the cooling air duct, so that part of the cooling air flow blown out from the cooling air duct enters the first avoidance groove and flows along the first avoidance groove following the skeleton.

[0010] Preferably, a second avoidance groove is provided on the side of the component body away from the first avoidance groove, the second avoidance groove is used for partial embedding of the welding pad, the first avoidance groove and the second avoidance groove are connected through a welding hole, and the welding point is located in the welding hole.

[0011] Preferably, the highest point of the inner bottom wall of the second avoidance groove is located above the extension path of the cooling air duct, so that part of the cooling air flow blown out from the cooling air duct enters the second avoidance groove and flows along the second avoidance groove; and / or, the connecting junction between the first avoidance groove and the second avoidance groove is located on the extension path of the cooling air duct.

[0012] Preferably, a surface of the component body facing away from the guide groove is a mounting surface, and the mounting surface is detachably connected to the frame at a position avoiding the second avoidance groove.

[0013] Preferably, the mounting surface is a curved surface.

[0014] Preferably, the component body is provided with an escape notch near the inlet end of the guide groove, and the escape notch is used to escape the conveyor belt wound on the lead-out roller.

[0015] The present invention has the following advantages and beneficial effects: During the production of the spiral filter element, the formed filter element first moves through the material channel, which is formed by the cooperation of the guide groove and the peripheral wall of the lead-out roller. The design of the guide groove ensures that the filter element can maintain stability during movement and prevents welding errors caused by position offset. In this process, the friction between the filter element and the lead-out roller is reduced, allowing the filter element to pass smoothly, while reducing the interference of external forces on the welding position, thereby ensuring the consistency and accuracy of the welding process.

[0016] When the filter element passes through the material channel, the first avoidance groove allows the frame to adjust itself during the welding process. Specifically, during welding, if the frame fails to fit the filter membrane completely, the avoidance groove provides the necessary space, allowing the frame to make slight adjustments during movement to avoid gaps or misalignment. This flexibility ensures a close fit between the frame and the filter membrane, reduces possible structural defects during welding, and thus improves the overall strength after welding.

[0017] In addition, the welding hole in the first avoidance groove ensures the precise docking between the welding electrode on the lead-out roller and the welding electrode on the welding pad. During the welding process, the design of the welding hole enables the welding electrode to accurately apply heat and pressure between the frame and the filter membrane to ensure the welding quality. This optimized electrode docking effectively reduces the risk of cold welding or uneven welding, and significantly enhances the bonding force of the welding area.

[0018] In summary, the welding auxiliary component forms an efficient welding process through the stability of the guide groove, the flexibility of the first avoidance groove and the precise matching of the welding hole. This series of designs work together to not only effectively solve the common quality defects in the spiral filter element welding process, but also significantly improve the overall strength and service life of the filter element, ensuring its reliable filtering performance in various high-demand environments. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0020] Figure 1 It is a partial installation schematic diagram for showing that a component body is installed on a frame in some embodiments of the present application; Figure 2 This is a schematic diagram of the structure of some embodiments of the present application for displaying the component body. Figure 1 ; Figure 3 It is a structural schematic diagram for showing the positional relationship between the component body and the lead-out roller in some embodiments of the present application; Figure 4 It is a partial cross-sectional view for showing the positional relationship between the component body and the lead-out roller in some embodiments of the present application; Figure 5 is a partial cross-sectional view for showing the positional relationship between the component body, the lead-out roller and the welding pad in some embodiments of the present application; Figure 6 This is a schematic diagram of the structure of some embodiments of the present application for displaying the component body Figure 2 ; Figure 7 is a partial cross-sectional view for showing a component body in some embodiments of the present application; The markings in the figure are: 100, component body; 110, guide groove; 120, first avoidance groove; 121, welding hole; 130, material channel; 140, cooling air duct; 141, insertion section; 142, guide section; 150, second avoidance groove; 160, mounting surface; 170, avoidance gap; 200, rack; 300, lead-out roller; 400, conveyor belt; 500. Solder pad. DETAILED DESCRIPTION

[0021] To make the purpose, technical solution and advantages of the present invention clearer, the technical solution of the present invention will be described in detail below. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments of the present invention, all other implementation methods obtained by ordinary technicians in this field without creative work belong to the scope of protection of the present invention.

[0022] The terms "first", "second", etc. in the specification and claims of the present application are used to distinguish similar objects, and are not used to describe a specific order or sequence. It should be understood that the data used in this way can be interchangeable under appropriate circumstances, so that the embodiments of the present application can be implemented in an order other than those illustrated or described here, and the objects distinguished by "first", "second", etc. are generally of one type, and the number of objects is not limited. For example, the first object can be one or more. In addition, "and / or" in the specification and claims represents at least one of the connected objects, and the character " / " generally indicates that the objects associated with each other are in an "or" relationship.

[0023] In the relevant technology, spiral filter elements are widely used in many industrial fields, including oil and gas transportation, agricultural irrigation, medical equipment, aerospace navigation, chemical production and food processing. These fields have extremely stringent performance requirements for spiral filter elements, especially when used for a long time, in high intensity and in corrosive environments, which puts forward extremely high standards for the strength, corrosion resistance, filtration accuracy and durability of the filter element. In order to meet these requirements, the structural design and manufacturing process of the filter element must ensure high strength and high precision, especially in terms of pressure resistance, corrosion resistance and long-term operation. The spiral filter element needs to have excellent performance. With the continuous expansion of market demand, the demand for high-performance spiral filter elements continues to grow.

[0024] The Chinese patent application with the publication number CN117862279A discloses a rigid tube blank and its skeleton structure. The manufacturing process of the spiral filter element in the application adopts a welding process. The main manufacturing process is to spirally wind the filter membrane and the supporting skeleton, and fix the skeleton and the filter membrane by welding after molding to ensure the stability of the overall structure and the stability of molding. In the prior art, the welding device generally includes a lead-out roller and a welding pad, and the molded filter element is welded by these devices during the welding process. However, the applicant found in actual production and use that this welding process has certain technical problems, resulting in quality defects in the produced spiral filter element during use, which is specifically manifested as structural instability and filter element failure.

[0025] First, the skeleton of the spiral filter element is usually made of a spiral-shaped support sheet, and the skeleton needs to fit tightly to the surface of the filter membrane after spiral winding. Ideally, the skeleton should be evenly and tightly attached to the filter membrane to form a stable spiral structure. However, in the existing manufacturing process, there may be certain deviations in the winding process, making it impossible for the skeleton and the filter membrane to maintain a complete fit. For example, due to the inconsistency of the flexibility and thickness of the skeleton and the filter membrane material, or the influence of external forces during winding, local gaps may occur between the skeleton and the filter membrane, or the skeleton may not fit strictly according to the predetermined spiral path. These gaps and deviations will directly affect the quality of subsequent welding.

[0026] Secondly, the welding process itself has certain limitations. When welding in areas where the frame and the filter membrane are not tightly fitted or are offset, due to poor contact between the two, the heat conduction during welding is uneven, the strength of the weld is difficult to meet the expected requirements, and even cold welding may occur. This leads to insufficient bonding force in the welding area, making it easy for the welded frame and filter membrane to separate or loosen under external pressure or temperature changes. In addition, poor welding may also cause local overheating of the material and damage the filter membrane, further reducing the filtration performance and durability of the filter element.

[0027] These welding defects not only affect the overall strength and structural stability of the spiral filter element, but may also cause premature failure of the filter element during actual use. Especially when used in high-pressure, high-temperature, and corrosive environments, the defective parts of the filter element can easily become stress concentration points, which in turn accelerates damage and cannot meet the strict requirements of high-precision equipment and systems for filtering performance.

[0028] Therefore, the existing spiral filter manufacturing technology has the following disadvantages: 1. It is difficult to ensure that the skeleton and the filter membrane are completely fitted during the winding process, resulting in unstable welding quality; 2. The heat control in the welding process is uneven, and the strength of the weld point is insufficient, resulting in a decrease in the overall structural strength of the filter element. An improved manufacturing process or welding method is urgently needed to ensure that the skeleton and the filter membrane of the spiral filter element are tightly fitted and to improve the welding quality, thereby improving the molding stability and service life of the spiral filter element.

[0029] Based on this, the present application provides a welding auxiliary component. The welding auxiliary component is arranged on a welding device. Figure 1 The welding device includes a frame 200, a lead-out roller 300, a conveyor belt 400 and a welding pad 500. The lead-out roller 300 is rotatably arranged on the frame 200, the conveyor belt 400 is partially wound around the inlet end of the lead-out roller 300, and the welding pad 500 is rotatably arranged on the frame 200 at the lead-out end of the lead-out roller 300. After spiral winding, the filter membrane and the skeleton are wound on the lead-out roller 300 through the conveyor belt 400, and move out from the lead-out end of the lead-out roller 300 along the length direction of the lead-out roller 300. At the same time, since the position of the welding pad 500 is close to the lead-out end of the lead-out roller 300, during the rotation process of the welding pad 500, part of its disk surface can be rotated to be located on the moving path of the filter membrane and the skeleton to form a welding point, so that the mutually attached part of the filter membrane and the skeleton during the spiral winding can pass through the welding point, and the attached part of the two is continuously welded at the lead-out end of the lead-out roller 300 to achieve the final welding forming state.

[0030] Please refer to Figure 1 to Figure 7 The welding auxiliary component includes a component body 100, which has a guide groove 110 and a first avoidance groove 120. The guide groove 110 is used to cooperate with the peripheral wall of the lead-out roller 300 to form a material channel 130, and the material channel 130 is used for the formed spiral filter element to pass through; the first avoidance groove 120 is arranged in the guide groove 110, and the first avoidance groove 120 partially overlaps with the spiral moving path of the skeleton of the spiral filter element on the lead-out roller 300 to achieve avoidance of the skeleton.

[0031] At the same time, a welding hole 121 is provided in the first avoidance groove 120, and the welding hole 121 is used to achieve the cooperation between the welding electrode on the lead-out roller 300 and the welding electrode on the welding pad 500, so as to weld the frame and the filter membrane.

[0032] On this basis, the guide groove 110 cooperates with the peripheral wall of the lead-out roller 300 to form a material channel 130, so that the formed spiral filter element can pass smoothly. This design optimizes the flow path of the material during the welding process, which is beneficial to improving the stability and consistency of the filter element during the manufacturing process. By reducing the displacement of the material and unnecessary friction, the deviation that may occur during the welding process is reduced, thereby improving the molding accuracy of the filter element.

[0033] At the same time, the first avoidance groove 120 overlaps with the frame in the spiral moving path, and the design purpose is to effectively avoid the frame. During the welding process, when the frame moves to the avoidance groove, the space in the avoidance groove allows the frame to be adjusted without being hindered, and then the frame can be accurately welded at the appropriate position during the welding process, thereby avoiding gaps or misalignments caused by improper positions, greatly reducing stress concentration in the welding area, and effectively improving welding quality.

[0034] Furthermore, the design of the welding hole 121 enables the welding electrode on the lead-out roller 300 to accurately dock with the welding electrode on the welding pad 500. Through this precise matching, uniform heat and pressure can be provided during the welding process to ensure the strength and quality of the weld. This improvement reduces the risk of cold welding or uneven welding that may occur during the welding process, makes the connection between the frame and the filter membrane more secure, and improves the stability of the overall structure.

[0035] In summary, through the comprehensive design of the guide groove 110, the first avoidance groove 120 and the welding hole 121, the welding auxiliary component effectively solves the common quality defects of the spiral filter element during the welding process. First, the design of the material channel 130 ensures the stability of the filter element during the welding process; secondly, the setting of the first avoidance groove 120 enables the skeleton to self-adjust during welding to ensure the accuracy of the welding position; finally, the optimization of the welding hole 121 realizes the precise matching of the welding electrode, thereby improving the welding quality. This series of improvement measures work together to effectively enhance the overall performance of the spiral filter element, extend its service life, and ensure its reliability and stability in high-demand environments.

[0036] Furthermore, the component body 100 is used to apply a pressure to the spiral filter element, so that the spiral filter element can offset its own elastic force when moving along the spiral path, maintain structural stability, and prevent the skeleton surface from wrinkling due to its own elastic force.

[0037] In some embodiments, reference Figure 1 , Figure 2The component body 100 also has a cooling air duct 140 for introducing a cooling air flow, and the air outlet of the cooling air duct 140 is arranged on the inner wall of the welding hole 121. In this way, the cooling air flow is introduced through the cooling air duct 140 during the welding process and blown out directly from the inner wall of the welding hole 121. This cooling effect helps to quickly reduce the temperature of the welding area and avoid material deformation or damage caused by overheating. This is crucial to maintaining the physical properties and structural integrity of the filter element material, especially when used in a high temperature environment. Lowering the welding temperature can significantly improve the stability of the welding. At the same time, during the welding process, the heat-affected zone around the weld is usually susceptible to high temperatures, resulting in reduced material properties. The introduction of cooling air flow in the cooling air duct 140 can effectively reduce the temperature gradient in the heat-affected zone, reduce thermal stress, and avoid the formation of microcracks or structural weaknesses caused by temperature changes. This effect helps to improve the overall strength and service life of the filter element after welding. Exemplary, combined Figure 3 , Figure 4 The cooling air duct 140 includes an axially connected insertion section 141 and a guide section 142. The insertion section 141 is used for inserting an external air duct, and the guide section 142 has an end away from the insertion section 141 and opens toward the matching position of the welding electrode on the lead-out roller 300 and the welding electrode on the pad 500. Furthermore, the external air duct is connected to the blower, and the wind is directly generated at the end of the external air duct through the blower.

[0038] Exemplarily, the inner diameter of the insertion section 141 is larger than the inner diameter of the guide section 142 , so as to limit the external air duct from entering the guide section 142 .

[0039] After such arrangement, since the cooling air duct 140 is a relatively closed channel, after the cooling airflow is blown out by the external air duct, the cooling airflow is not easy to carry impurities in the external ambient air into the welding point, thereby reducing the impact of impurities entering the welding point on welding. This is beneficial to improving the cleanliness of the cooling airflow and improving the welding effect.

[0040] Furthermore, the combined structure of the insertion section 141 and the guide section 142 ensures accurate guidance of the airflow. Specifically, the opening of the guide section 142 faces the mating point between the welding electrode and the pad 500, so that the cooling airflow can be accurately blown to the welding point. This design significantly improves the cooling efficiency, can quickly reduce the temperature of the welding area, and prevent welding defects caused by excessively high temperatures in local areas during welding, such as overheating deformation of the welding point or degradation of material properties.

[0041] On this basis, the inner diameter of the insertion section 141 is larger than the inner diameter of the guide section 142, so that the external air duct cannot penetrate into the guide section 142. This structural design prevents the cooling airflow from impacting the welding point area too strongly by limiting the inflow of airflow, thereby avoiding unnecessary interference with the welding process. For example, excessive airflow may cause the molten pool to be unstable during welding, uneven weld formation, and even cause cold welding. By reasonably controlling the airflow flow rate, it can be ensured that the temperature in the welding point area is steadily reduced, thereby improving the welding quality. In addition, the inner diameter of the insertion section 141 is larger than the inner diameter of the guide section 142, which can further concentrate the airflow and make the cooling airflow more concentrated on the welding point. Compared with traditional cooling methods, this airflow concentration design improves cooling efficiency, shortens cooling time, and avoids quality problems caused by uneven cooling during welding.

[0042] In some embodiments, Figure 1 , Figure 5 As shown, the matching position of the welding electrode on the pad 500 and the welding electrode on the lead-out roller 300 is the welding point, and the extension path of the cooling air duct 140 is tangent to the outer peripheral contour line of the pad 500 at the welding point. After such a setting, the cooling air flow blown out of the cooling air duct 140 can flow in a smooth and tangential direction when entering the welding area, thereby avoiding the frontal impact of the cooling air flow and the welding point to a certain extent, ensuring that the air flow can flow evenly and smoothly along the surface of the welding point. This is more conducive to taking away the heat at the welding point than the design of blowing directly vertically or radially to the welding point, because the contact area is larger when the air flow flows along the surface, and the heat transfer efficiency is higher.

[0043] At the same time, compared with the cooling airflow directly acting on the welding point, the tangential airflow path design avoids the interference of airflow on the welding process. If the airflow blows directly to the welding point, it may affect the stability of the welding pool, resulting in uneven welds or poor welding quality. Through the tangential method, the cooling airflow flows in an indirect and smooth way, which can effectively take away the heat without interfering with the formation and solidification process of the welding pool, ensuring the welding quality.

[0044] Furthermore, the cooling airflow enters the area near the welding point in a tangential manner, forming an optimal cooling path with the matching position of the welding electrode and the welding disk. The cooling airflow can focus on the high-temperature area of ​​the welding point without interfering with the work of the welding electrode, taking away the heat, and improving the controllability and welding quality of the overall welding process.

[0045] In some embodiments, reference Figure 6 , Figure 7, the lowest point of the inner bottom wall of the first avoidance groove 120 is below the extension path of the cooling air duct 140, so that part of the cooling air flow blown out from the cooling air duct 140 enters the first avoidance groove 120 and flows along the first avoidance groove 120 following the skeleton. Exemplarily, the groove line of the first avoidance groove 120 is a smooth arc. In this way, when the cooling air flow is blown out from the cooling air duct 140, since the lowest point of the first avoidance groove 120 is below the extension path of the cooling air duct 140, part of the air flow will be naturally deflected into the first avoidance groove 120. According to the Bernoulli principle in fluid mechanics, the cooling air flow has a higher pressure and a lower speed in a larger cross-section (such as at the outlet of the cooling air duct 140), and when the cooling air flow enters the first avoidance groove 120, the channel restriction of the first avoidance groove 120 will cause the air flow to accelerate and flow along the first avoidance groove 120. The bottom wall of the first avoidance groove 120 is lower than the mainstream path of the cooling airflow. This design provides a "low-pressure zone" for the cooling airflow, so that the cooling airflow is naturally guided upward into the first avoidance groove 120 and continues to flow along the direction of the spiral skeleton.

[0046] At the same time, the first avoidance groove 120 not only provides an avoidance space for the frame, but also has a "capturing" effect on the cooling airflow. The existence of the first avoidance groove 120 forms an additional cooling airflow path, so that after the cooling airflow passes through the welding hole 121, part of the cooling airflow is guided into the first avoidance groove 120 and flows along the spiral path of the frame. Since the shape of the first avoidance groove 120 partially overlaps with the spiral path of the frame, the airflow can closely follow the surface of the frame, and then contact the welded part of the frame for a longer time, thereby enhancing the cooling and heat dissipation effect.

[0047] In some embodiments, reference Figure 5 , Figure 6 A second avoidance groove 150 is provided on one side of the component body 100 away from the first avoidance groove 120. The second avoidance groove 150 is used for partially embedding the pad 500. The first avoidance groove 120 and the second avoidance groove 150 are connected through a welding hole 121, and the welding point is located in the welding hole 121. Exemplarily, the groove shape of the second avoidance groove 150 is adapted to the contour of the pad 500.

[0048] After such arrangement, the design of the second avoidance groove 150 allows the pad 500 to be partially embedded therein, thereby enhancing the fit between the pad 500 and the frame. By providing a suitable embedding space, the pad 500 can be in closer contact with the frame. This improved fit directly affects the welding quality and reduces welding defects. At the same time, during the welding process, good fit can ensure that a stable current path is formed between the welding electrode and the pad 500, thereby promoting the uniform formation of the weld. A higher fit helps to evenly distribute heat during the welding process and avoid welding defects caused by local overheating or uneven cooling.

[0049] In some embodiments, reference Figure 7 The highest point of the inner bottom wall of the second avoidance groove 150 is located above the extension path of the cooling air duct 140 , so that part of the cooling air flow blown out from the cooling air duct 140 enters the second avoidance groove 150 and flows along the second avoidance groove 150 .

[0050] After such arrangement, the second avoidance groove 150 is used to guide the cooling airflow to further flow out of the welding hole 121, so that the contact time between the welding surface of the welding pad 500 and the cooling airflow is increased, so that the cooling airflow can continue to blow on the surface of the welding pad 500 for a period of time after leaving the cooling air duct 140, thereby reducing the probability of impurities adhering to the surface of the welding pad 500. At the same time, the welding pad 500 can also be cooled to always maintain the welding effect of the welding pad 500.

[0051] Exemplarily, the connecting junction of the first avoidance groove 120 and the second avoidance groove 150 is located on the extension path of the cooling air duct 140. In this way, when the cooling airflow is ejected from the cooling air duct 140, it will be diverted when it reaches the connecting junction, so that it can effectively cover the welding area and its surrounding environment, that is, the cooling airflow can be blown into the first avoidance groove 120 and the second avoidance groove 150 at the same time, thereby enhancing the uniformity and efficiency of cooling. Specifically, when the cooling airflow enters the first avoidance groove 120, it can directly cool the skeleton and reduce its temperature; and when entering the second avoidance groove 150, it ensures that the welding pad 500 can also be cooled in time. At the same time, by reasonably distributing the airflow, the risk of local overheating is reduced, and welding defects caused by uneven airflow are avoided. This uniform cooling effect improves the overall quality and reliability of welding.

[0052] In some embodiments, reference Figure 1 , Figure 6 The surface of the component body 100 that is away from the guide groove 110 is a mounting surface 160, and the mounting surface 160 is detachably connected to the frame 200 at a position avoiding the second avoidance groove 150. Exemplarily, the mounting surface 160 can be bolted or clamped to the frame 200.

[0053] Such an arrangement allows the installation position of the component body 100 and the frame 200 to not affect the normal docking between the lead-out roller 300 and the welding pad 500, thereby improving the rationality of the installation of the component body 100 on the frame 200.

[0054] Exemplarily, the mounting surface 160 is a curved surface. With such a configuration, when the mounting surface 160 is fitted with the frame 200, the mounting surface 160 being a curved surface can further prevent the fitting portion from sliding, which is beneficial to improving the mounting stability of the component body 100 after installation.

[0055] In some embodiments, Figure 2 As shown, the component body 100 is provided with an avoidance notch 170 near the inlet end of the guide groove 110, and the avoidance notch 170 is used to avoid the conveyor belt 400 wound on the lead-out roller 300. After such arrangement, after the component body 100 is installed, the component body 100 can avoid the conveyor belt 400 by setting the avoidance notch 170, so that the installation position of the component body 100 does not affect the normal operation of the conveyor belt 400, and at the same time, the operation of the conveyor belt 400 does not affect the use of the component body 100.

[0056] The above are only specific embodiments of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can easily think of changes or substitutions within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A welding auxiliary component, It is characterized in that The component body (100) comprises a guide groove (110) and a first avoidance groove (120), wherein the guide groove (110) is used to cooperate with the peripheral wall of a lead-out roller (300) to form a material channel (130), and the material channel (130) is used to allow a formed spiral filter element to pass through; the first avoidance groove (120) is arranged in the guide groove (110), and the first avoidance groove (120) partially overlaps with a spiral moving path of a frame of the spiral filter element on the lead-out roller (300), so as to avoid the frame; A welding hole (121) is provided in the first avoidance groove (120), and the welding hole (121) is used to achieve the matching of the welding electrode on the lead-out roller (300) and the welding electrode on the welding pad (500) so as to weld the frame to the filter membrane.

2. The welding auxiliary member according to claim 1, It is characterized in that The component body (100) further comprises a cooling air duct (140) for introducing cooling air flow, and an air outlet of the cooling air duct (140) is arranged on the inner wall of the welding hole (121).

3. The welding auxiliary member according to claim 2, It is characterized in that The cooling air duct (140) comprises an axially connected insertion section (141) and a guide section (142); the insertion section (141) is used for inserting an external air duct; an end of the guide section (142) away from the insertion section (141) opens toward a matching position between a welding electrode on the lead-out roller (300) and a welding electrode on the welding pad (500); The inner diameter of the insertion section (141) is greater than the inner diameter of the flow guide section (142), so as to limit the external air duct from entering the flow guide section (142).

4. The welding auxiliary member according to claim 2, It is characterized in that The matching position of the welding electrode on the welding pad (500) and the welding electrode on the lead-out roller (300) is a welding point, and the extension path of the cooling air duct (140) is tangent to the outer peripheral contour line of the welding pad (500) at the welding point.

5. The welding auxiliary member according to claim 2, It is characterized in that The lowest point of the inner bottom wall of the first avoidance groove (120) is located below the extension path of the cooling air duct (140), so that a portion of the cooling air flow blown out from the cooling air duct (140) enters the first avoidance groove (120) and flows along the first avoidance groove (120) following the skeleton.

6. The welding auxiliary member according to claim 4, It is characterized in that A second avoidance groove (150) is provided on a side of the component body (100) facing away from the first avoidance groove (120), the second avoidance groove (150) being used for partially embedding the welding pad (500), the first avoidance groove (120) and the second avoidance groove (150) being connected via a welding hole (121), and the welding point is located in the welding hole (121).

7. The welding auxiliary member according to claim 6, It is characterized in that The highest point of the inner bottom wall of the second avoidance groove (150) is located above the extension path of the cooling air duct (140), so that a portion of the cooling air flow blown out from the cooling air duct (140) enters the second avoidance groove (150) and flows along the second avoidance groove (150); And / or, the communicating boundary between the first avoidance groove (120) and the second avoidance groove (150) is located on the extension path of the cooling air duct (140).

8. The welding auxiliary member according to claim 6, It is characterized in that A surface of the component body (100) that is away from the guide groove (110) is a mounting surface (160), and the mounting surface (160) is detachably connected to the frame (200) at a position avoiding the second avoidance groove (150).

9. The welding auxiliary member according to claim 8, It is characterized in that The mounting surface (160) is a curved surface.

10. The welding auxiliary component according to any one of claims 1 to 9, It is characterized in that The component body (100) is also provided with an avoidance notch (170) at an inlet end close to the guide groove (110), and the avoidance notch (170) is used to avoid the conveyor belt (400) wound around the lead-out roller (300).

Citation Information

Patent Citations

  • Electrochemical device and manufacturing method thereof, circuit board and housing tray

    CN102254685A

  • Liquid precise filtering device

    CN107185283A

  • Iron-aluminum-based intermetallic compound filter core and preparation method thereof

    CN111098051A

  • Turret type collector plate welding pressure head

    CN116038222A

  • Composite welding method and welding structure of T-shaped welding joint

    CN117655491A