Material suitable for high-strength automobile inner door panel and preparation process thereof
Through the combination of modified PP resin, titanium dioxide, talc powder, and carbon fiber crystal powder and specific process processing, the wear resistance and strength problems of automotive interior door panel materials are solved, extending service life and maintaining surface flatness under high temperature environments .
Patent Information
- Application Number
- CN202411110314.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-14
- Publication Date
- 2024-11-29
AI Technical Summary
The existing automotive interior door panel materials have poor wear resistance and low strength, resulting in short service life, especially in high temperature environments, which affects aesthetics and functionality.
Using a combination of modified PP resin, titanium dioxide, talc powder, carbon fiber crystal powder, expanded flame retardant, plasticizer and lubricant, a high-strength car interior is prepared through specific processes such as high-temperature and high-pressure reaction and vacuum drying. Door panel panel material.
It improves the wear resistance and strength of the material, extends the service life, and maintains surface flatness and strength under high temperature environments.
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of automobile door panel materials, and in particular relates to a material suitable for a high-strength automobile inner door panel and a preparation process thereof. Background Art
[0002] Automobile interior door panels refer to the plates or panels installed inside the car doors. They are used to decorate and protect the internal structure of the door as well as provide functionality and convenience. In the manufacturing process, injection molds are usually used for injection molding.
[0003] In the prior art, most of the automobile interior door panels are made of PP or PVC materials. The resulting automobile interior door panels have poor wear resistance. In addition, during the production, transportation and use, there is a problem that the surface of the PP products is uneven due to friction, which in turn affects the service life of the plastic products. In the automotive industry, especially in the summer when the temperature is relatively high, after a long period of exposure to the road, the surface of the automobile interior door panels will swell, the strength will decrease and age, which will seriously affect the aesthetics and service life of the interior. Summary of the invention
[0004] In view of this, the technical problem to be solved by the present invention is to provide a material suitable for high-strength automobile inner door panel and its preparation process, so as to avoid the trouble of poor strength and low wear resistance of previous automobile door panel materials.
[0005] In order to solve the above technical problems, the present invention discloses a material suitable for high-strength automobile inner door panel, comprising: 70-90 parts of modified PP resin, 20-25 parts of titanium dioxide, 1-15 parts of talc, 20-35 parts of carbon fiber crystal powder, 1-5 parts of masterbatch, 2-5 parts of intumescent flame retardant, 20-40 parts of plasticizer, and 10-15 parts of lubricant.
[0006] According to one embodiment of the present invention, the mixture includes 70 parts of modified PP resin, 20 parts of titanium dioxide, 3 parts of talc, 20 parts of carbon fiber crystal powder, 2 parts of masterbatch, 2 parts of intumescent flame retardant, 20 parts of plasticizer and 10 parts of lubricant.
[0007] According to one embodiment of the present invention, the mixture includes 90 parts of modified PP resin, 25 parts of titanium dioxide, 15 parts of talc, 35 parts of carbon fiber crystal powder, 5 parts of masterbatch, 5 parts of intumescent flame retardant, 40 parts of plasticizer and 15 parts of lubricant.
[0008] According to one embodiment of the present invention, the mixture includes 80 parts of modified PP resin, 22 parts of titanium dioxide, 7 parts of talc, 28 parts of carbon fiber crystal powder, 3 parts of masterbatch, 4 parts of intumescent flame retardant, 30 parts of plasticizer and 12 parts of lubricant.
[0009] The present invention also discloses a preparation process of a material suitable for a high-strength automobile inner door panel, comprising: Step a. Add modified PP resin, titanium dioxide, talcum powder, carbon fiber powder, masterbatch, intumescent flame retardant, plasticizer and lubricant into the reactor according to the mass fraction, keep the temperature at 70°C for 30 minutes, start stirring at 150 r / min, heat the temperature in the reactor from 70°C to 210°C within 90 minutes, and start the pressure relief after the pressure in the reactor rises to 1.8-2.0MPa for 120 minutes; Step b. Allow the pressure in the autoclave to drop to normal pressure over 30 minutes, then raise the temperature to 230°C and keep warm for 30 minutes. Slowly open the vacuum system to gradually reduce the pressure in the autoclave to -0.05MPa and maintain for 30 minutes; Step c. The discharged material is cooled and pelletized, and then extracted in 100°C boiling water for 36 hours; Step d. Finally, take out and introduce high-purity nitrogen at 150° C. to dry for 36 hours to obtain the product material.
[0010] Compared with the prior art, the present invention can achieve the following technical effects: The automotive interior door panel material is prepared by modifying PP resin with titanium dioxide, talcum powder and carbon fiber crystal powder to ensure toughness. At the same time, the strength is improved by adding carbon fiber crystal powder, and titanium dioxide and talcum powder improve wear resistance and extend service life.
[0011] Of course, any product implementing the present invention does not necessarily need to achieve all of the above-mentioned technical effects at the same time. DETAILED DESCRIPTION
[0012] The following will describe the implementation methods of the present invention in detail with reference to examples, so that the implementation process of how the present invention applies technical means to solve technical problems and achieve technical effects can be fully understood and implemented accordingly.
[0013] The present invention discloses a material suitable for a high-strength automobile inner door panel, comprising: 70-90 parts of modified PP resin, 20-25 parts of titanium dioxide, 1-15 parts of talc, 20-35 parts of carbon fiber crystal powder, 1-5 parts of masterbatch, 2-5 parts of intumescent flame retardant, 20-40 parts of plasticizer, and 10-15 parts of lubricant.
[0014] Among them, modified PP resin is the main material, titanium dioxide and talcum powder are plastic fillers, carbon fiber crystal powder can enhance the strength of PP material and improve durability, and masterbatch is used for color adjustment.
[0015] Example 1 includes 70 parts of modified PP resin, 20 parts of titanium dioxide, 3 parts of talcum powder, 20 parts of carbon fiber crystal powder, 2 parts of masterbatch, 2 parts of intumescent flame retardant, 20 parts of plasticizer, and 10 parts of lubricant.
[0016] The process is as follows: Step a. Add modified PP resin, titanium dioxide, talcum powder, carbon fiber powder, masterbatch, intumescent flame retardant, plasticizer and lubricant into the reactor according to the mass fraction, keep the temperature at 70°C for 30 minutes, start stirring at 150 r / min, heat the temperature in the reactor from 70°C to 210°C within 90 minutes, and start the pressure relief after the pressure in the reactor rises to 1.8-2.0MPa for 120 minutes; Step b. Allow the pressure in the autoclave to drop to normal pressure over 30 minutes, then raise the temperature to 230°C and keep warm for 30 minutes. Slowly open the vacuum system to gradually reduce the pressure in the autoclave to -0.05MPa and maintain for 30 minutes; Step c. The discharged material is cooled and pelletized, and then extracted in 100°C boiling water for 36 hours; Step d. Finally, take out and introduce high-purity nitrogen at 150° C. to dry for 36 hours to obtain the product material.
[0017] Example 2 includes 90 parts of modified PP resin, 25 parts of titanium dioxide, 15 parts of talc, 35 parts of carbon fiber crystal powder, 5 parts of masterbatch, 5 parts of intumescent flame retardant, 40 parts of plasticizer, and 15 parts of lubricant.
[0018] The process is as follows: Step a. Add modified PP resin, titanium dioxide, talcum powder, carbon fiber powder, masterbatch, intumescent flame retardant, plasticizer and lubricant into the reactor according to the mass fraction, keep the temperature at 70°C for 30 minutes, start stirring at 150 r / min, heat the temperature in the reactor from 70°C to 210°C within 90 minutes, and start the pressure relief after the pressure in the reactor rises to 1.8-2.0MPa for 120 minutes; Step b. Allow the pressure in the autoclave to drop to normal pressure over 30 minutes, then raise the temperature to 230°C and keep warm for 30 minutes. Slowly open the vacuum system to gradually reduce the pressure in the autoclave to -0.05MPa and maintain for 30 minutes; Step c. The discharged material is cooled and pelletized, and then extracted in 100°C boiling water for 36 hours; Step d. Finally, take out and introduce high-purity nitrogen at 150° C. to dry for 36 hours to obtain the product material.
[0019] Example 3 includes 80 parts of modified PP resin, 22 parts of titanium dioxide, 7 parts of talc, 28 parts of carbon fiber crystal powder, 3 parts of masterbatch, 4 parts of intumescent flame retardant, 30 parts of plasticizer, and 12 parts of lubricant.
[0020] The process is as follows: Step a. Add modified PP resin, titanium dioxide, talcum powder, carbon fiber powder, masterbatch, intumescent flame retardant, plasticizer and lubricant into the reactor according to the mass fraction, keep the temperature at 70°C for 30 minutes, start stirring at 150 r / min, heat the temperature in the reactor from 70°C to 210°C within 90 minutes, and start the pressure relief after the pressure in the reactor rises to 1.8-2.0MPa for 120 minutes; Step b. Allow the pressure in the autoclave to drop to normal pressure over 30 minutes, then raise the temperature to 230°C and keep warm for 30 minutes. Slowly open the vacuum system to gradually reduce the pressure in the autoclave to -0.05MPa and maintain for 30 minutes; Step c. The discharged material is cooled and pelletized, and then extracted in 100°C boiling water for 36 hours; Step d. Finally, take out and introduce high-purity nitrogen at 150° C. to dry for 36 hours to obtain the product material.
[0021] The bumper material products of the above three embodiments were respectively injection molded into finished bumpers of uniform specifications, and then subjected to bumper strength tests. In the bumper tests, the vehicle was subjected to frontal and rear-end collisions with obstacles in the shape of vehicle bumpers at a speed of 9.7 km / h, and to collisions with the front and rear corners of obstacles at a speed of 4.8 km / h. It was found that the bumper material of embodiment 3 had the lowest damage and the highest strength.
[0022] In summary, the present invention prepares automobile interior door panel materials by combining modified PP resin with titanium dioxide, talcum powder and carbon fiber crystal powder to ensure toughness, while adding carbon fiber crystal powder to improve strength, and titanium dioxide and talcum powder improve wear resistance and enhance service life.
[0023] The above description shows and describes several preferred embodiments of the present invention, but as mentioned above, it should be understood that the present invention is not limited to the form disclosed herein, and should not be regarded as excluding other embodiments, but can be used in various other combinations, modifications and environments, and can be modified within the scope of the invention concept described herein through the above teachings or the technology or knowledge of the relevant field. Changes and variations made by those skilled in the art do not depart from the spirit and scope of the present invention, and should be within the scope of protection of the claims attached to the present invention.
Claims
1. A material suitable for high-strength automotive inner door panel, characterized in that: include: 70-90 parts of modified PP resin, 20-25 parts of titanium dioxide, 1-15 parts of talc, 20-35 parts of carbon fiber crystal powder, 1-5 parts of masterbatch, 2-5 parts of intumescent flame retardant, 20-40 parts of plasticizer, and 10-15 parts of lubricant.
2. The material suitable for high-strength automobile inner door panel according to claim 1, characterized in that: include: 70 parts of modified PP resin, 20 parts of titanium dioxide, 3 parts of talc, 20 parts of carbon fiber crystal powder, 2 parts of masterbatch, 2 parts of intumescent flame retardant, 20 parts of plasticizer, and 10 parts of lubricant.
3. The material suitable for high-strength automobile inner door panel according to claim 1, characterized in that: include: 90 parts of modified PP resin, 25 parts of titanium dioxide, 15 parts of talc, 35 parts of carbon fiber crystal powder, 5 parts of masterbatch, 5 parts of intumescent flame retardant, 40 parts of plasticizer, and 15 parts of lubricant.
4. The material suitable for high-strength automobile inner door panel according to claim 1, characterized in that: include: 80 parts of modified PP resin, 22 parts of titanium dioxide, 7 parts of talc, 28 parts of carbon fiber crystal powder, 3 parts of masterbatch, 4 parts of intumescent flame retardant, 30 parts of plasticizer, and 12 parts of lubricant.
5. A process for preparing the material suitable for high-strength automobile inner door panel according to claim 1, characterized in that: include: Step a. Add modified PP resin, titanium dioxide, talcum powder, carbon fiber powder, masterbatch, intumescent flame retardant, plasticizer and lubricant into the reactor according to the mass fraction, keep the temperature at 70°C for 30 minutes, start stirring at 150 r / min, heat the temperature in the reactor from 70°C to 210°C within 90 minutes, and start the pressure relief after the pressure in the reactor rises to 1.8-2.0MPa for 120 minutes; Step b. The pressure in the autoclave is reduced to normal pressure after 30 min, and then the temperature is raised to 230 ° C and kept warm for 30 min; the vacuum system is slowly opened to gradually reduce the pressure in the autoclave to -0.05 MPa and maintained for 30 min; Step c. The discharged material is cooled and pelletized, and then extracted in 100°C boiling water for 36 hours; Step d. Finally, take out and introduce high-purity nitrogen at 150° C. to dry for 36 hours to obtain the product material.