Anti-subfissure solar cell and preparation method and interconnection method thereof
By setting copper grid layers with different density on the front and back of the solar cell and interconnecting them using interconnect materials, the problems of hidden cracks and conductive silver glue spills caused by welding tape contact are solved, and the solar cell is improved power generation efficiency and production cost.
Patent Information
- Application Number
- CN202411242902.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-05
- Publication Date
- 2024-11-29
AI Technical Summary
During the interconnection process of solar cell cells, the contact and extrusion of the welding tape with the edge of the cell leads to cracking or collapse, and the spillover of conductive silver glue causes short connection of positive and negative electrodes, which increases production cost and silver consumption.
A crack-proof solar cell is designed, which has different dense copper grid layers on the front and back, and is interconnected by wrapping interconnect materials instead of traditional welding tape and conductive silver glue.
It effectively avoids the hidden cracks and edge collapse of solar cell cells, reduces the total silver consumption, improves power generation efficiency and production costs, and avoids the problems of conductive flash fracture and uneven current distribution.
Smart Images

Figure CN119050174A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of solar cell panels, and in particular to an anti-hidden crack solar cell panel and a preparation method and an interconnection method thereof. Background Art
[0002] As the production process of solar cells continues to develop, solar cells are thinned to less than 150μm. In order to connect multiple solar cells in series, the relevant technology can first weld a welding ribbon on the front of one of the solar cells, and then weld the welding ribbon to the back of another solar cell. Since the welding ribbon will contact the edge of the solar cell, when welding the welding ribbon to the back of another solar cell, the welding ribbon will squeeze the edge of the solar cell, and the thickness of the solar cell is very small. Therefore, the relevant technology has the problem of hidden cracks or broken edges of the solar cell due to the contact and squeezing of the welding ribbon with the edge of the solar cell when the two solar cells are interconnected by the welding ribbon, thereby causing the conductive grid line on the solar cell to break, and then causing the solar cell module product (such as a solar cell) to lose its power generation capacity. The related technology can also first coat the front side of one of the solar cells with conductive silver paste, and then mount the other solar cell with its back side facing downward on the conductive silver paste. Since the related technology is equivalent to completing the interconnection of two solar cells by bonding the two solar cells together with the conductive silver paste, the related technology has the problem of increasing the total silver consumption of the solar cell module product due to the need to use conductive silver paste to achieve the interconnection of multiple solar cells, thereby increasing the production cost of the solar cell module product. The related technology also has the problem of short-circuiting the positive and negative poles of the solar cell due to the overflow of the conductive silver paste to the side of the solar cell.
[0003] There is no effective technical solution to the above problems. It should be noted that the above information disclosed in this section is only used to understand the background of the present invention, and therefore may contain information that does not constitute prior art. Summary of the invention
[0004] The purpose of the present application is to provide a solar cell sheet with an anti-hidden cracking property, a preparation method thereof and an interconnection method, which can effectively solve the problems of hidden cracking or edge collapse of solar cells caused by contact and compression between the soldering ribbon and the edge of the solar cell when the soldering ribbon is used to complete the interconnection of two solar cells, the increase in the total silver consumption of solar cell module products due to the need to use conductive silver paste to achieve the interconnection of multiple solar cells, and the short circuit of the positive and negative electrodes of the solar cell due to the overflow of the conductive silver paste to the side of the solar cell.
[0005] In a first aspect, the present application provides an anti-hidden crack solar cell, comprising: A solar cell sheet, the front side of which is provided with a first copper grid layer, and the back side of which is provided with a second copper grid layer; The first copper grid layer and the second copper grid layer both include a plurality of first copper grid lines, a plurality of second copper grid lines, and interconnection materials that wrap the first copper grid lines and the second copper grid lines. The first copper grid lines are parallel to the long sides of the solar cell, the second copper grid lines are perpendicular to the first copper grid lines, the density of the first copper grid lines close to the long side edges of the solar cell is greater than the density of the first copper grid lines far from the long side edges of the solar cell, and the melting point of the interconnection material is lower than the melting points of the first copper grid lines and the second copper grid lines.
[0006] The present application provides an anti-hidden crack solar cell, which interconnects the solar cells or releases the stress generated during actual use by making the density of the first copper grid lines close to the long side edge of the solar cell greater than the density of the first copper grid lines far from the long side edge of the solar cell, and interconnects multiple solar cells by an interconnection material wrapped on the first copper grid mesh layer and the second copper grid mesh layer, that is, the present application is equivalent to using the interconnection material to replace the conductive silver glue and the welding ribbon. Therefore, the present application can effectively solve the problems of hidden cracks or edge collapse of the solar cell due to the contact and compression between the welding ribbon and the edge of the solar cell when the welding ribbon is used to complete the interconnection of two solar cells, the increase in the total silver consumption of the solar cell module product due to the need to use conductive silver glue to achieve the interconnection of multiple solar cells, and the short circuit of the positive and negative poles of the solar cell due to the overflow of the conductive silver glue to the side of the solar cell, thereby effectively solving the problems of conductive flash fracture on the solar cell due to hidden cracks or edge collapse of the solar cell, the loss of power generation capacity of the solar cell module product, and the increase in the production cost of the solar cell module product due to the increase in the total silver consumption of the solar cell module product.
[0007] Optionally, the ratio of the number of the second copper grid lines in the second copper grid mesh layer to the number of the second copper grid lines in the first copper grid mesh layer is 1:1-1.2:1.
[0008] Since the ratio of the number of second copper grid lines in the second copper grid grid layer to the number of second copper grid lines in the first copper grid grid layer is 1:1-1.2:1, the technical solution can increase the bifaciality of the solar cell by making the number of second copper grid lines on the back of the solar cell greater than the number of second copper grid lines on the front of the solar cell, thereby effectively improving the power generation efficiency of the solar cell module product.
[0009] Optionally, the width of the first copper grid line and the second copper grid line is 5-50 μm, and the thickness of the first copper grid line and the second copper grid line is 5-15 μm.
[0010] The technical solution sets the width of the first copper grid line and the second copper grid line to 5-50μm. The technical solution can effectively avoid the situation that the light energy received by the solar cell is reduced, the internal resistance of the solar cell is increased, and the production cost of the solar cell is increased due to the first copper grid line and the second copper grid line being too wide, thereby effectively avoiding the situation that the power generation efficiency of the solar cell is reduced due to the reduction of the light energy received by the solar cell, the power loss of the solar cell is increased due to the increase of the internal resistance of the solar cell, and the output power and output efficiency of the solar cell product component are reduced. The technical solution can also effectively avoid the situation that the adhesion of the first copper grid line and the second copper grid line is insufficient and the current distribution of the solar cell is insufficient due to the first copper grid line and the second copper grid line being too narrow. The uneven distribution of the first copper grid wire and the second copper grid wire can effectively avoid the situation that the first copper grid wire and the second copper grid wire fall off due to insufficient adhesion of the first copper grid wire and the second copper grid wire. The technical solution also sets the thickness of the first copper grid wire and the second copper grid wire to 5-15μm. The technical solution can also effectively avoid the situation that the production cost of the solar cell is increased due to the first copper grid wire and the second copper grid wire being too thick, too much light is blocked by the first copper grid wire and the second copper grid wire, and the conductivity of the first copper grid wire and the second copper grid wire is reduced due to the first copper grid wire and the second copper grid wire being too thin, and the mechanical strength of the first copper grid wire and the second copper grid wire is reduced, thereby effectively avoiding the situation that the power generation efficiency of the solar cell is reduced due to too much light blocked by the first copper grid wire and the second copper grid wire.
[0011] Optionally, the interconnect material is tin, tin-bismuth alloy or nickel alloy.
[0012] Optionally, the interconnect material wraps around the top surfaces of the first copper grid line and the second copper grid line, or wraps around the top surfaces and side surfaces of the first copper grid line and the second copper grid line.
[0013] In a second aspect, the present application further provides a method for preparing a solar cell sheet with an anti-hidden crack, which is used to prepare the solar cell sheet with an anti-hidden crack provided in the first aspect. The method for preparing a solar cell sheet with an anti-hidden crack comprises the following steps: S11, forming a first patterned mask on the front side of the solar cell, and forming a second patterned mask on the back side of the solar cell; S12, synchronously depositing copper material on the front and back sides of the solar cell based on the first patterned mask and the second patterned mask, and removing the first patterned mask and the second patterned mask to form a first copper grid line and a second copper grid line on the front side of the solar cell and a first copper grid line and a second copper grid line on the back side of the solar cell; S13, depositing an interconnect material on the first copper grid line and the second copper grid line to form a first copper grid mesh layer and a second copper grid mesh layer.
[0014] The present application provides a method for preparing a solar cell that is resistant to hidden cracks. The method interconnects the solar cells or releases the stress generated during actual use by making the density of the first copper grid lines close to the long side edge of the solar cell greater than the density of the first copper grid lines far from the long side edge of the solar cell, and interconnects multiple solar cells by an interconnection material wrapped on the first copper grid mesh layer and the second copper grid mesh layer. That is, the present application is equivalent to using the interconnection material to replace the conductive silver paste and the welding ribbon. Therefore, the present application can effectively solve the problems of hidden cracks or edge collapse of the solar cell due to the contact and compression between the welding ribbon and the edge of the solar cell when the welding ribbon is used to complete the interconnection of two solar cells, the increase in the total silver consumption of the solar cell module product due to the need to use conductive silver paste to achieve the interconnection of multiple solar cells, and the short circuit of the positive and negative poles of the solar cell due to the overflow of the conductive silver paste to the side of the solar cell, thereby effectively solving the problems of conductive flash fracture on the solar cell due to hidden cracks or edge collapse of the solar cell, the loss of power generation capacity of the solar cell module product, and the increase in the production cost of the solar cell module product due to the increase in the total silver consumption of the solar cell module product.
[0015] Optionally, the method for preparing a solar cell sheet with an anti-hidden crack structure further includes the following steps performed before step S11: S14, forming a first copper seed layer on the front side of the solar cell, and forming a second copper seed layer on the back side of the solar cell; Step S12 includes: S121, using a first patterned mask and a second patterned mask to simultaneously deposit copper material on the first copper seed layer and the second copper seed layer based on an electroplating process; S122, removing the first patterned mask and the second patterned mask; S123, removing the first copper seed layer outside the first copper grid mesh layer and the second copper seed layer outside the second copper grid mesh layer to form a first copper grid line and a second copper grid line on the front side of the solar cell and a first copper grid line and a second copper grid line on the back side of the solar cell.
[0016] In a third aspect, the present application further provides a method for interconnecting anti-hidden crack solar cells, which is used to interconnect a first anti-hidden crack solar cell and a second anti-hidden crack solar cell, wherein the first anti-hidden crack solar cell and the second anti-hidden crack solar cell are both anti-hidden crack solar cells provided by the first aspect above, and the method for interconnecting anti-hidden crack solar cells comprises the following steps: S21, forming a plurality of non-conductive glue dots arranged at intervals on the first copper grid layer of the first anti-hidden crack solar cell based on a glue dispensing process, and placing the second copper grid layer of the second anti-hidden crack solar cell downward on the first copper grid layer of the first anti-hidden crack solar cell, so as to fix the second anti-hidden crack solar cell on the first anti-hidden crack solar cell by using the non-conductive glue dots; S22, hot pressing the first anti-hidden crack solar cell and the second anti-hidden crack solar cell to fuse the interconnection material on the first copper grid layer of the first anti-hidden crack solar cell with the interconnection material on the second copper grid layer of the second anti-hidden crack solar cell, so as to complete the interconnection between the first anti-hidden crack solar cell and the second anti-hidden crack solar cell.
[0017] The present application provides a method for interconnecting solar cells to prevent hidden cracks. The method interconnects the solar cells or releases the stress generated during actual use by making the density of the first copper grid lines close to the long side edges of the solar cells greater than the density of the first copper grid lines far from the long side edges of the solar cells, and interconnects multiple solar cells through an interconnection material wrapped on the first copper grid mesh layer and the second copper grid mesh layer. That is, the present application is equivalent to using the interconnection material to replace the conductive silver glue and the welding ribbon. Therefore, the present application can effectively solve the problems of hidden cracks or edge collapse of solar cells caused by contact and compression between the welding ribbon and the edge of the solar cell when the welding ribbon is used to complete the interconnection of two solar cells, the increase in the total silver consumption of the solar cell module product due to the need to use conductive silver glue to achieve the interconnection of multiple solar cells, and the short circuit of the positive and negative poles of the solar cell due to the overflow of the conductive silver glue to the side of the solar cell, thereby effectively solving the problems of conductive flash fracture on the solar cell due to hidden cracks or edge collapse of the solar cell, the loss of power generation capacity of the solar cell module product, and the increase in the production cost of the solar cell module product due to the increase in the total silver consumption of the solar cell module product.
[0018] Optionally, step S21 includes: S211, placing a tinned copper foil on a region of the first copper grid layer of the first anti-hidden crack solar cell near one of the long side edges, wherein a plurality of through holes are arranged at intervals on the tinned copper foil; S212, filling the through hole with non-conductive glue; S213, placing the area of the second copper grid layer of the second anti-hidden crack solar cell close to one of the long side edges on the tinned copper foil, so as to fix the second anti-hidden crack solar cell on the first anti-hidden crack solar cell by using non-conductive glue dots.
[0019] Since the technical solution can form a large-area copper-tin-tin-copper contact by arranging a tin-plated copper foil between the first anti-hidden crack solar cell and the second anti-hidden crack solar cell to reduce conductive resistance and heat accumulation, the technical solution can effectively improve the conductive performance of the solar cell module product, and since the non-conductive adhesive is located in the through hole of the tin-plated copper foil, the technical solution can also effectively avoid the stress accumulation caused by the uneven thickness distribution of the excess non-conductive adhesive on the anti-hidden crack solar cell, and the occurrence of hidden cracks or edge collapse of the anti-hidden crack solar cell.
[0020] Optionally, a plurality of anti-overflow glue grid lines are further provided on the first copper grid layer of the first anti-hidden crack solar cell sheet, and non-conductive glue dots are arranged in the anti-overflow glue grid lines.
[0021] The anti-overflow glue grid line of this technical solution can prevent the overflow of non-conductive glue, thereby effectively avoiding the uneven thickness distribution of the non-conductive glue on the anti-hidden crack solar cell due to the overflow of the non-conductive glue, and further avoiding the stress accumulation caused by the uneven thickness distribution of the non-conductive glue on the anti-hidden crack solar cell, resulting in hidden cracks or edge collapse of the anti-hidden crack solar cell.
[0022] As can be seen from the above, the present application provides an anti-hidden crack solar cell, a preparation method thereof, and an interconnection method. The solar cells are interconnected or the stress generated during actual use is released by making the density of the first copper grid lines close to the long side edge of the solar cell greater than the density of the first copper grid lines far from the long side edge of the solar cell, and multiple solar cells are interconnected by the interconnection material wrapped on the first copper grid grid layer and the second copper grid grid layer. That is, the present application is equivalent to using the interconnection material to replace the conductive silver glue and the welding ribbon. Therefore, the present application can effectively solve the problems of hidden cracks or edge collapse of the solar cell due to the contact and compression between the welding ribbon and the edge of the solar cell when the welding ribbon is used to complete the interconnection of two solar cells, the increase in the total silver consumption of the solar cell module product due to the need to use conductive silver glue to achieve the interconnection of multiple solar cells, and the positive and negative poles of the solar cell short-circuited due to the overflow of the conductive silver glue to the side of the solar cell, thereby effectively solving the problems of conductive flash fracture on the solar cell due to hidden cracks or edge collapse of the solar cell, the loss of power generation capacity of the solar cell module product, and the increase in the production cost of the solar cell module product due to the increase in the total silver consumption of the solar cell module product. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 A schematic structural diagram of the front side of a solar cell for preventing hidden cracks provided in the first embodiment of the present application.
[0024] Figure 2 For along Figure 1 Schematic diagram of the cross-sectional structure of the AA section line.
[0025] Figure 3 A flow chart of a method for preparing a solar cell that prevents hidden cracks provided in an embodiment of the present application.
[0026] Figure 4 A schematic diagram of a method for preparing a solar cell that prevents hidden cracks provided in an embodiment of the present application.
[0027] Figure 5 A flow chart of a method for interconnecting solar cells to prevent hidden cracks provided in an embodiment of the present application.
[0028] Figure 6 A schematic diagram of the structure of a crack-proof solar cell and a tin-plated copper foil provided in an embodiment of the present application.
[0029] Figure 7 A schematic structural diagram of the front side of a solar cell for preventing hidden cracks provided in the second embodiment of the present application.
[0030] Figure 8 This is a schematic diagram of interconnecting multiple solar cells using solder ribbons in the prior art.
[0031] Figure numerals: 1, solar cell; 2, first copper grid line; 3, second copper grid line; 4, interconnection material; 5, first patterned mask; 6, second patterned mask; 7, third copper grid line; 8, tinned copper foil; 9, anti-overflow glue grid line. DETAILED DESCRIPTION
[0032] The technical solutions in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only a part of the embodiments of the present application, rather than all of the embodiments. The components of the embodiments of the present application described and shown in the drawings here can be arranged and designed in various different configurations. Therefore, the following detailed description of the embodiments of the present application provided in the drawings is not intended to limit the scope of the application claimed for protection, but merely represents the selected embodiments of the present application. Based on the embodiments of the present application, all other embodiments obtained by those skilled in the art without making creative work belong to the scope of protection of the present application.
[0033] It should be noted that similar reference numerals and letters represent similar items in the following drawings, so once an item is defined in one drawing, it does not need to be further defined and explained in subsequent drawings. At the same time, in the description of this application, the terms "first", "second", etc. are only used to distinguish the description and cannot be understood as indicating or implying relative importance.
[0034] First, as Figure 1-Figure 2 As shown, the present application provides an anti-hidden crack solar cell, which includes: A solar cell 1, with a first copper grid layer on the front side and a second copper grid layer on the back side; The first copper grid layer and the second copper grid layer both include a plurality of first copper grid lines 2, a plurality of second copper grid lines 3, and an interconnection material 4 that wraps the first copper grid lines 2 and the second copper grid lines 3. The first copper grid lines 2 are parallel to the long sides of the solar cell 1, and the second copper grid lines 3 are perpendicular to the first copper grid lines 2. The density of the first copper grid lines 2 close to the long side edge of the solar cell 1 is greater than the density of the first copper grid lines 2 far from the long side edge of the solar cell 1, and the melting point of the interconnection material 4 is lower than the melting points of the first copper grid lines 2 and the second copper grid lines 3.
[0035] Among them, this embodiment can integrate multiple anti-hidden crack solar cells provided by the present application into a solar cell assembly product (such as a solar cell and its packaging assembly), and the anti-hidden crack solar cell of this embodiment includes a solar cell 1, and the solar cell 1 is preferably a silicon wafer. The front of the solar cell 1 is provided with a first copper grid layer, and the back of the solar cell 1 is provided with a second copper grid layer. The first copper grid layer and the second copper grid layer of this embodiment both contain a plurality of first copper grid lines 2, a plurality of second copper grid lines 3, and an interconnection material 4 that wraps the first copper grid lines 2 and the second copper grid lines 3. The number of first copper grid lines 2 of the first copper grid layer of this embodiment can be the same as or different from the number of first copper grid lines 2 of the second copper grid layer, and the number of second copper grid lines 3 of the first copper grid layer of this embodiment can be the same as or different from the number of second copper grid lines 3 of the second copper grid layer. The first copper grid lines 2 of this embodiment are parallel to the long side of the solar cell 1, and the second copper grid lines 3 of this embodiment are perpendicular to the first copper grid lines 2 (that is, the second copper grid lines 3 are perpendicular to the long side of the solar cell 1), and the second copper grid lines 3 of this embodiment are equidistantly arranged on the solar cell 1. The melting point of the interconnection material 4 of this embodiment is lower than the melting points of the first copper grid line 2 and the second copper grid line 3 and is conductive. Therefore, this embodiment can be achieved by first heating the two anti-hidden crack solar cells until the interconnection material 4 thereon melts, and then placing the second copper grid layer of one of the anti-hidden crack solar cells downward on the first copper grid layer of the other solar cell 1, so that the interconnection materials 4 of the two anti-hidden crack solar cells fuse with each other, and finally cooling the two anti-hidden crack solar cells to solidify the interconnection material 4, thereby achieving the interconnection of the two anti-hidden crack solar cells. This embodiment can also be achieved by first placing the second copper grid layer of one of the anti-hidden crack solar cells downward on the first copper grid layer of the other solar cell 1, and then hot pressing the two anti-hidden crack solar cells based on the existing hot pressing process, so that the interconnection materials 4 on the two anti-hidden crack solar cells fuse into one, thereby achieving the interconnection of the two anti-hidden crack solar cells. It should be understood that the relevant technology can also achieve the interconnection of the two anti-hidden crack solar cells by welding the two ends of the welding strip to the first copper grid layer of one anti-hidden crack solar cell and the second copper grid layer of the other anti-hidden crack solar cell, respectively. It should be understood that the related technology can use silver grid lines to replace the first copper grid lines 2 and the second copper grid lines 3 of the present application. Compared with the silver grid lines, the first copper grid lines 2 and the second copper grid lines 3 of the present application have the characteristics of low cost and not easy to break after sintering. Therefore, the present application can effectively reduce the production cost of anti-hidden crack solar cells and avoid the problem of loss of power generation capacity of solar cell modules due to easy breakage of the grid lines after sintering.It should also be understood that, since the density of the first copper grid lines 2 near the long side edge of the solar cell 1 in this embodiment is greater than the density of the first copper grid lines 2 far from the long side edge of the solar cell 1, that is, this embodiment is equivalent to making the first copper grid lines 2 more densely distributed at the long side edge of the solar cell 1, when interconnecting the solar cells 1, this embodiment can use the first copper grid lines 2 more densely distributed at the long side edge of the solar cell 1 to interconnect the solar cells 1 or release the stress generated during actual use, thereby effectively reducing the occurrence of hidden cracks or edge collapse of the solar cell 1 due to excessive local stress of the solar cell 1. It should also be understood that if the solar cell 1 needs to be cut and separated, the first copper grid mesh layer and the second copper grid mesh layer are not provided at the cutting portion of the solar cell 1.
[0036] The present application provides an anti-hidden crack solar cell, which interconnects the solar cells 1 or releases the stress generated during actual use by making the density of the first copper grid lines 2 close to the long side edge of the solar cell 1 greater than the density of the first copper grid lines 2 far from the long side edge of the solar cell 1, and interconnects multiple solar cells 1 through the interconnection material 4 wrapped on the first copper grid mesh layer and the second copper grid mesh layer, that is, the present application is equivalent to using the interconnection material 4 to replace the conductive silver glue and the welding tape, so the present application can effectively solve the problem of hidden cracks or edge collapse of the solar cell 1 due to the contact and compression between the welding tape and the edge of the solar cell 1 when the welding tape is used to complete the interconnection of two solar cells 1, the increase in the total silver consumption of the solar cell module product due to the need to use conductive silver glue to achieve the interconnection of multiple solar cells 1, and the short circuit of the positive and negative poles of the solar cell 1 due to the overflow of the conductive silver glue to the side of the solar cell 1, thereby effectively solving the problem of conductive flash fracture on the solar cell 1 due to hidden cracks or edge collapse of the solar cell 1, the loss of power generation capacity of the solar cell module product, and the increase in the production cost of the solar cell module product due to the increase in the total silver consumption of the solar cell module product.
[0037] In some preferred embodiments, the ratio of the number of second copper grid lines 3 of the second copper grid layer to the number of second copper grid lines 3 of the first copper grid layer is 1:1-1.2:1. The number of second copper grid lines 3 of the second copper grid layer of this embodiment is preferably 80-150. Since the ratio of the number of second copper grid lines 3 of the second copper grid layer to the number of second copper grid lines 3 of the first copper grid layer is 1:1-1.2:1, this embodiment can increase the bifaciality of the solar cell 1 by making the number of second copper grid lines 3 on the back of the solar cell 1 greater than the number of second copper grid lines 3 on the front of the solar cell 1, thereby effectively improving the power generation efficiency of the solar cell module product. It should be understood that the prior art uses welding strips ( Figure 8 When multiple solar cells 1 are interconnected, since both ends of each welding strip can only be connected to a second copper grid line 3 (reference Figure 8 a) and a second copper grid line 3 (refer to Figure 8 b) connection in the prior art, so the number of the second copper grid lines 3 on the front side of the existing solar cell 1 needs to be the same as the number of the second copper grid lines 3 on the back side of the solar cell 1, and because the welding ribbon can only extend along one axial direction, the prior art needs to make the position of the second copper grid lines 3 on the front side of the solar cell 1 the same as the position of the second copper grid lines 3 on the back side of the solar cell 1 in order to realize the interconnection of multiple solar cells 1 by using the welding ribbon. On the other hand, the technical solution of the present application realizes the interconnection of multiple solar cells 1 by hot pressing, and the first copper grid layer of one solar cell 1 is connected to the first copper grid layer of another solar cell 1. When the second copper grid layer of the cell sheet 1 contacts, the first copper grid wire 2 and the second copper grid wire 3 of the first copper grid grid layer will form a large number of contact points with the first copper grid wire 2 and the second copper grid wire 3 of the second copper grid grid layer, that is, after hot pressing interconnection, the present application can generate enough interconnection points to achieve the effect of interconnection of the solar cell 1. Therefore, this embodiment can make the number and position of the first copper grid wire 2 of the first copper grid grid layer different from the number and position of the first copper grid wire 2 of the second copper grid grid layer, that is, compared with the prior art, this embodiment can effectively increase the bifaciality of the solar cell 1 and improve the power generation efficiency of the solar cell module product.
[0038] In some preferred embodiments, the ratio of the number of first copper grid lines 2 of the second copper grid layer to the number of first copper grid lines 2 of the first copper grid layer is 1.5:1-3:1. This embodiment is equivalent to making the number of first copper grid lines 2 on the back of the solar cell 1 greater than the number of first copper grid lines 2 on the front of the solar cell 1. This embodiment can better release stress by making the ratio of the number of first copper grid lines 2 of the second copper grid layer to the number of first copper grid lines 2 of the first copper grid layer be 1.5:1-3:1, thereby further reducing the occurrence of hidden cracks or edge collapse of the solar cell 1 due to excessive local stress of the solar cell 1.
[0039] In some preferred embodiments, the width of the first copper grid line 2 and the second copper grid line 3 is 5-50 μm, and the thickness of the first copper grid line 2 and the second copper grid line 3 is 5-15 μm. Preferably, the width of the first copper grid line 2 and the second copper grid line 3 of this embodiment is 15-25 μm, and the thickness of the first copper grid line 2 and the second copper grid line 3 of this embodiment is 5-8 μm. In this embodiment, the width of the first copper grid line 2 and the second copper grid line 3 is set to 5-50 μm. This embodiment can effectively avoid the situation that the light energy received by the solar cell 1 is reduced, the internal resistance of the solar cell 1 is increased, and the production cost of the solar cell 1 is increased due to the first copper grid line 2 and the second copper grid line 3 being too wide, thereby effectively avoiding the situation that the power generation efficiency of the solar cell 1 is reduced due to the reduction of the light energy received by the solar cell 1, and the power loss of the solar cell 1 is increased due to the increase of the internal resistance of the solar cell 1, and the output power and output efficiency of the solar cell product component are reduced. This embodiment can also effectively avoid the situation that the adhesion of the first copper grid line 2 and the second copper grid line 3 is insufficient and the current distribution of the solar cell 1 is not stable due to the first copper grid line 2 and the second copper grid line 3 being too narrow. The embodiment further sets the thickness of the first copper grid line 2 and the second copper grid line 3 to 5-15 μm, and the embodiment can effectively avoid the situation that the production cost of the solar cell 1 is increased due to the first copper grid line 2 and the second copper grid line 3 being too thick, too much light is blocked by the first copper grid line 2 and the second copper grid line 3, and the conductivity of the first copper grid line 2 and the second copper grid line 3 is reduced due to the first copper grid line 2 and the second copper grid line 3 being too thin, and the mechanical strength of the first copper grid line 2 and the second copper grid line 3 is reduced, thereby effectively avoiding the situation that the power generation efficiency of the solar cell 1 is reduced due to the excessive light blocked by the first copper grid line 2 and the second copper grid line 3.
[0040] In some preferred embodiments, the interconnection material 4 is tin, tin-bismuth alloy or nickel alloy. The thickness of the interconnection material 4 of this embodiment is preferably 1-5 μm to ensure that there is enough interconnection material 4 to fuse with each other when interconnecting multiple solar cells 1. It should be understood that the interconnection material 4 of this embodiment can also be other alloys with a melting point lower than that of copper.
[0041] In some preferred embodiments, the interconnect material 4 wraps the top surface of the first copper grid line 2 and the second copper grid line 3, or wraps the top surface and side surface of the first copper grid line 2 and the second copper grid line 3. Specifically, the top surface of the first copper grid line 2 is the outer end surface of the first copper grid line 2 facing away from the solar cell 1, and the top surface of the second copper grid line 3 is the outer end surface of the second copper grid line 3 facing away from the solar cell 1.
[0042] As can be seen from the above, the present application provides an anti-hidden crack solar cell, which interconnects the solar cells 1 or releases the stress generated during actual use by making the density of the first copper grid lines 2 close to the long side edges of the solar cells 1 greater than the density of the first copper grid lines 2 far from the long side edges of the solar cells 1, and interconnects multiple solar cells 1 through the interconnection material 4 wrapped on the first copper grid mesh layer and the second copper grid mesh layer, that is, the present application is equivalent to using the interconnection material 4 to replace the conductive silver glue and the welding ribbon, so the present application can effectively solve the problem of the welding ribbon and the solar cell 1 being connected when the welding ribbon is used to complete the interconnection of two solar cells 1. The edges of the solar cell 1 are contacted and squeezed, resulting in hidden cracks or edge collapse of the solar cell 1, the total silver consumption of the solar cell module product increases due to the need to use conductive silver glue to achieve the interconnection of multiple solar cell 1, and the positive and negative poles of the solar cell 1 are short-circuited due to the conductive silver glue overflowing to the side of the solar cell 1. This effectively solves the problems of conductive flash breakage on the solar cell 1 due to hidden cracks or edge collapse of the solar cell 1, the loss of power generation capacity of the solar cell module product, and the increase in the production cost of the solar cell module product due to the increase in the total silver consumption of the solar cell module product.
[0043] Second, as Figure 3-Figure 4 As shown, the present application also provides a method for preparing a solar cell sheet with an anti-hidden crack, which is used to prepare the solar cell sheet with an anti-hidden crack provided by the first aspect above. The method for preparing a solar cell sheet with an anti-hidden crack comprises the following steps: S11, forming a first patterned mask 5 on the front side of the solar cell 1, and forming a second patterned mask 6 on the back side of the solar cell 1; S12, based on the first patterned mask 5 and the second patterned mask 6, copper material is deposited on the front and back sides of the solar cell 1 simultaneously, and the first patterned mask 5 and the second patterned mask 6 are removed to form the first copper grid line 2 and the second copper grid line 3 on the front side of the solar cell 1 and the first copper grid line 2 and the second copper grid line 3 on the back side of the solar cell 1; S13, depositing an interconnect material 4 on the first copper grid line 2 and the second copper grid line 3 to form a first copper grid mesh layer and a second copper grid mesh layer.
[0044] The method for preparing a solar cell with anti-hidden cracks provided in the present application is used to prepare the solar cell with anti-hidden cracks provided in the first aspect. The principle of the method for preparing a solar cell with anti-hidden cracks provided in the present application is the same as the principle of the solar cell with anti-hidden cracks provided in the first aspect, and will not be discussed in detail here. Step S11 can form a first graphic mask 5 on the front of the solar cell 1 and a second graphic mask 6 on the back of the solar cell 1 based on the existing graphic mask forming process. It should be understood that the pattern of the first graphic mask 5 corresponds to the first copper grid line 2 formed in step S12, and the pattern of the second graphic mask 6 corresponds to the second copper grid line 3 formed in step S21. In step S12, copper material may be deposited on the front and back sides of the solar cell 1 using the first patterned mask 5 and the second patterned mask 6 based on an existing chemical vapor deposition process or a physical vapor deposition process, and then the first patterned mask 5 and the second patterned mask 6 may be removed based on an existing mask removal process to form the first copper grid line 2 and the second copper grid line 3 on the front side of the solar cell 1 and the first copper grid line 2 and the second copper grid line 3 on the back side of the solar cell 1. In step S13, interconnect material 4 may be deposited on the first copper grid line 2 and the second copper grid line 3 based on an existing chemical vapor deposition process or a physical vapor deposition process to form a first copper grid mesh layer and a second copper grid mesh layer.
[0045] In some preferred embodiments, the method for preparing a solar cell sheet with an anti-hidden crack structure further includes the following steps performed before step S11: S14, forming a first copper seed layer on the front side of the solar cell 1, and forming a second copper seed layer on the back side of the solar cell 1; Step S12 includes: S121, using the first patterned mask 5 and the second patterned mask 6 to simultaneously deposit copper material on the first copper seed layer and the second copper seed layer based on an electroplating process; S122, removing the first patterned mask 5 and the second patterned mask 6; S123, removing the first copper seed layer outside the first copper grid mesh layer and the second copper seed layer outside the second copper grid mesh layer to form a first copper grid line 2 and a second copper grid line 3 on the front side of the solar cell 1 and to form a first copper grid line 2 and a second copper grid line 3 on the back side of the solar cell 1.
[0046] It should be understood that if step S12 is based on an electroless deposition process to deposit copper material on the first copper seed layer and the second copper seed layer simultaneously using the first patterned mask 5 and the second patterned mask 6 using the electroplating process, then this embodiment does not need to perform step S14 and step S123.
[0047] As can be seen from the above, the present application provides a method for preparing a solar cell with an anti-hidden crack structure, which interconnects the solar cells 1 or releases the stress generated during actual use by making the density of the first copper grid lines 2 close to the long side edges of the solar cells 1 greater than the density of the first copper grid lines 2 far from the long side edges of the solar cells 1, and interconnects multiple solar cells 1 by using the interconnection material 4 wrapped on the first copper grid mesh layer and the second copper grid mesh layer, that is, the present application is equivalent to using the interconnection material 4 to replace the conductive silver glue and the soldering tape, so the present application can effectively solve the problem of the soldering tape being used to interconnect two solar cells 1. The invention can effectively solve the problems of cracking or edge collapse of the solar cell 1 caused by contact and compression with the edge of the solar cell 1, the increase in the total silver consumption of the solar cell module product due to the need to use conductive silver paste to achieve the interconnection of multiple solar cell 1, and the short circuit of the positive and negative poles of the solar cell 1 caused by the overflow of the conductive silver paste to the side of the solar cell 1, thereby effectively solving the problems of conductive flash breakage on the solar cell 1 caused by cracking or edge collapse of the solar cell 1, the loss of power generation capacity of the solar cell module product, and the increase in the production cost of the solar cell module product due to the increase in the total silver consumption of the solar cell module product.
[0048] Thirdly, Figure 5-Figure 7 As shown, the present application also provides a method for interconnecting anti-hidden crack solar cells, which is used to interconnect a first anti-hidden crack solar cell and a second anti-hidden crack solar cell, wherein the first anti-hidden crack solar cell and the second anti-hidden crack solar cell are both the anti-hidden crack solar cells provided by the first aspect above, and the method for interconnecting anti-hidden crack solar cells comprises the following steps: S21, forming a plurality of non-conductive glue dots arranged at intervals on the first copper grid layer of the first anti-hidden crack solar cell based on a glue dispensing process, and placing the second copper grid layer of the second anti-hidden crack solar cell downward on the first copper grid layer of the first anti-hidden crack solar cell, so as to fix the second anti-hidden crack solar cell on the first anti-hidden crack solar cell by using the non-conductive glue dots; S22, hot pressing the first anti-hidden crack solar cell and the second anti-hidden crack solar cell to fuse the interconnection material 4 on the first copper grid layer of the first anti-hidden crack solar cell with the interconnection material 4 on the second copper grid layer of the second anti-hidden crack solar cell, so as to complete the interconnection between the first anti-hidden crack solar cell and the second anti-hidden crack solar cell.
[0049] An embodiment of the present application provides a method for interconnecting anti-hidden crack solar cells, which is used to interconnect multiple anti-hidden crack solar cells provided by the first aspect above. The principle of the method for interconnecting anti-hidden crack solar cells provided by the embodiment of the present application is the same as the principle of the anti-hidden crack solar cell provided by the first aspect above, and will not be discussed in detail here.
[0050] The non-conductive glue points of step S21 are points obtained by dispensing non-conductive glue on the first copper grid layer based on the glue dispensing process. Since the non-conductive glue is sticky, that is, the non-conductive glue can bond different objects together, step S21 can be performed by first forming a plurality of non-conductive glue points arranged at intervals on the first copper grid layer of the first anti-hidden crack solar cell, and then fixing the second anti-hidden crack solar cell on the first anti-hidden crack solar cell by placing the second copper grid layer of the second anti-hidden crack solar cell downward on the first copper grid layer of the first anti-hidden crack solar cell. It should be understood that in order to enable the two interconnected anti-hidden crack solar cells to receive sufficient light energy, all non-conductive glues of this embodiment are preferably arranged on the area of the first copper grid layer of the first anti-hidden crack solar cell near one of the long side edges, and the area of the second copper grid layer of the second anti-hidden crack solar cell near one of the long side edges is placed on the area of the first copper grid layer of the first anti-hidden crack solar cell where the non-conductive glue is provided, that is, this embodiment is equivalent to interconnecting the solar cells 1 using the interconnection material 4 near one of the long side edges of the anti-hidden crack solar cell. Preferably, the interconnection material 4 of this embodiment is tin, and the step S22 of hot pressing the first anti-hidden crack solar cell and the second anti-hidden crack solar cell can be: heating the first anti-hidden crack solar cell and the second anti-hidden crack solar cell to 100-190°C (preferably 140-180°C) to melt the interconnection material 4 on the first anti-hidden crack solar cell and the second anti-hidden crack solar cell; applying a vertical downward force to the second anti-hidden crack solar cell to fuse the interconnection materials 4 on the first anti-hidden crack solar cell and the second anti-hidden crack solar cell; stopping heating the first anti-hidden crack solar cell and the second anti-hidden crack solar cell to solidify the interconnection materials 4 that fuse with each other. It should be understood that since the non-conductive glue of this embodiment is not conductive, even if the non-conductive glue overflows to the side of the solar cell 1, the positive and negative electrodes of the solar cell 1 will not be short-circuited due to the front and back of the solar cell 1 being connected through the overflowed glue. Preferably, the first copper grid layer of the first anti-hidden crack solar cell of this embodiment also includes a third copper grid line 7, which is perpendicular to the long side edge of the first anti-hidden crack solar cell and is distributed on the long side edge of the first anti-hidden crack solar cell provided with non-conductive glue. This embodiment can effectively increase the density of electrical contact points, thereby effectively enhancing the conductive performance of the solar cell module product.It should also be understood that, since the first copper grid layer and the second copper grid layer of the embodiment both include a first copper grid line 2 parallel to the long side edge of the solar cell 1 and a second copper grid line 3 perpendicular to the long side edge of the solar cell 1, the embodiment only needs to place the second anti-hidden crack solar cell on the first anti-hidden crack solar cell to complete the electrical connection between the first anti-hidden crack solar cell and the second anti-hidden crack solar cell, that is, when placing the second anti-hidden crack solar cell, the embodiment does not need to align the first copper grid line 2 of the second anti-hidden crack solar cell with the first copper grid line 2 of the first anti-hidden crack solar cell, and since the steps of aligning the first copper grid line 2 of the second anti-hidden crack solar cell with the first copper grid line 2 of the first anti-hidden crack solar cell are cumbersome and time-consuming, the embodiment can also effectively simplify the interconnection process of the first anti-hidden crack solar cell and the second anti-hidden crack solar cell and shorten the time required for interconnecting the first anti-hidden crack solar cell and the second anti-hidden crack solar cell.
[0051] In some preferred embodiments, step S21 includes: S211, placing a tinned copper foil 8 on a region of the first copper grid layer of the first anti-hidden crack solar cell near one of the long side edges, wherein a plurality of through holes are arranged at intervals on the tinned copper foil 8; S212, filling the through hole with non-conductive glue; S213, placing the second copper grid layer of the second anti-hidden crack solar cell near one of the long side edges on the tinned copper foil 8, so as to fix the second anti-hidden crack solar cell on the first anti-hidden crack solar cell by using non-conductive glue dots.
[0052] This embodiment is equivalent to using the tin-plated copper foil 8 as an intermediate structure for interconnecting the first anti-hidden crack solar cell with the second anti-hidden crack solar cell. Since this embodiment can form a large-area copper-tin-tin-copper contact by arranging the tin-plated copper foil 8 between the first anti-hidden crack solar cell and the second anti-hidden crack solar cell to reduce conductive resistance and heat accumulation, this embodiment can effectively improve the conductive performance of the solar cell assembly product. Moreover, since the non-conductive adhesive is located in the through hole of the tin-plated copper foil 8, this embodiment can also effectively avoid the stress accumulation caused by the uneven thickness distribution of the excess non-conductive adhesive on the anti-hidden crack solar cell, and the occurrence of hidden cracks or edge collapse of the anti-hidden crack solar cell. It should be understood that the above embodiment utilizes the interconnection material on the first anti-hidden crack solar cell and the second anti-hidden crack solar cell to realize the interconnection between the first anti-hidden crack solar cell and the second anti-hidden crack solar cell, and this embodiment utilizes the interconnection material on the first anti-hidden crack solar cell and the second anti-hidden crack solar cell and tin-plated copper foil to realize the interconnection between the first anti-hidden crack solar cell and the second anti-hidden crack solar cell. Since the interconnection material and the tin-plated copper foil of the present application are not coated with silver, the present application can make the silver consumption for interconnecting multiple solar cells 1 zero, and since the prior art needs to use conductive silver glue to realize the interconnection of multiple solar cells 1, the silver consumption for interconnecting multiple solar cells 1 in the prior art is greater than zero.
[0053] In some preferred embodiments, a plurality of anti-overflow glue grid lines 9 are further provided on the first copper grid layer of the first anti-hidden crack solar cell, and non-conductive glue dots are arranged in the anti-overflow glue grid lines 9. The anti-overflow glue grid lines 9 of this embodiment are preferably cylindrical copper grid lines, which can prevent the non-conductive glue from overflowing, thereby effectively avoiding the situation that the thickness of the non-conductive glue on the anti-hidden crack solar cell is unevenly distributed due to the overflow of the non-conductive glue, and further avoiding the situation that the stress accumulation caused by the uneven thickness distribution of the non-conductive glue on the anti-hidden crack solar cell causes the anti-hidden crack or the collapse of the edge of the anti-hidden crack solar cell.
[0054] As can be seen from the above, the present application provides a method for interconnecting solar cells to prevent hidden cracks. The solar cells 1 are interconnected or the stress generated during actual use is released by making the density of the first copper grid lines 2 close to the long side edges of the solar cells 1 greater than the density of the first copper grid lines 2 far from the long side edges of the solar cells 1, and the interconnection material 4 wrapped on the first copper grid mesh layer and the second copper grid mesh layer is used to interconnect multiple solar cells 1. That is, the present application is equivalent to using the interconnection material 4 to replace the conductive silver glue and the soldering tape. Therefore, the present application can effectively solve the problem of the soldering tape being used to complete the interconnection of two solar cells 1. The invention can effectively solve the problems of cracking or edge collapse of the solar cell 1 caused by contact and compression with the edge of the solar cell 1, the increase in the total silver consumption of the solar cell module product due to the need to use conductive silver paste to achieve the interconnection of multiple solar cell 1, and the short circuit of the positive and negative poles of the solar cell 1 caused by the overflow of the conductive silver paste to the side of the solar cell 1, thereby effectively solving the problems of conductive flash breakage on the solar cell 1 caused by cracking or edge collapse of the solar cell 1, the loss of power generation capacity of the solar cell module product, and the increase in the production cost of the solar cell module product due to the increase in the total silver consumption of the solar cell module product.
[0055] As can be seen from the above, the present application provides an anti-hidden crack solar cell and a preparation method and an interconnection method thereof, which interconnects the solar cells 1 or releases the stress generated during actual use by making the density of the first copper grid lines 2 close to the long side edge of the solar cell 1 greater than the density of the first copper grid lines 2 far from the long side edge of the solar cell 1, and interconnects multiple solar cells 1 through the interconnection material 4 wrapped on the first copper grid mesh layer and the second copper grid mesh layer, that is, the present application is equivalent to using the interconnection material 4 to replace the conductive silver glue and the welding tape, so the present application can effectively solve the problem of using the welding tape to complete the interconnection of two solar cells 1 The invention can effectively solve the problems that the conductive flash on the solar cell 1 is broken due to the cracks or edge collapse of the solar cell 1, the loss of power generation capacity of the solar cell module product, and the increase in the production cost of the solar cell module product due to the increase in the total silver consumption of the solar cell module product.
[0056] In the embodiments provided in the present application, it should be understood that, herein, relational terms such as first and second, etc. are merely used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations.
[0057] The above description is only an embodiment of the present application and is not intended to limit the protection scope of the present application. For those skilled in the art, the present application may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application shall be included in the protection scope of the present application.
Claims
1. A solar cell sheet with an anti-hidden crack feature, The anti-hidden crack solar cell sheet comprises: A solar cell sheet, the front side of which is provided with a first copper grid layer, and the back side of which is provided with a second copper grid layer; The first copper grid layer and the second copper grid layer both include a plurality of first copper grid lines, a plurality of second copper grid lines, and an interconnection material that wraps the first copper grid lines and the second copper grid lines. The first copper grid lines are parallel to the long sides of the solar cell, the second copper grid lines are perpendicular to the first copper grid lines, the density of the first copper grid lines close to the long side edges of the solar cell is greater than the density of the first copper grid lines far from the long side edges of the solar cell, and the melting point of the interconnection material is lower than the melting points of the first copper grid lines and the second copper grid lines.
2. The anti-hidden crack solar cell according to claim 1, characterized in that: The ratio of the number of the second copper grid lines of the second copper grid grid layer to the number of the second copper grid lines of the first copper grid grid layer is 1:1-1.2:
1.
3. The anti-hidden crack solar cell according to claim 1, characterized in that: The width of the first copper grid line and the second copper grid line is 5-50 μm, and the thickness of the first copper grid line and the second copper grid line is 5-15 μm.
4. The anti-hidden crack solar cell according to claim 1, characterized in that: The interconnect material is tin, tin-bismuth alloy or nickel alloy.
5. The anti-hidden crack solar cell according to claim 1, characterized in that: The interconnection material wraps around the top surfaces of the first copper grid line and the second copper grid line or wraps around the top surfaces and side surfaces of the first copper grid line and the second copper grid line.
6. A method for preparing a solar cell sheet with an anti-hidden crack structure, characterized in that: Used to prepare the anti-hidden crack solar cell according to any one of claims 1 to 5, the method for preparing the anti-hidden crack solar cell comprises the following steps: S11, forming a first patterned mask on the front side of the solar cell, and forming a second patterned mask on the back side of the solar cell; S12, synchronously depositing copper material on the front and back sides of the solar cell based on the first patterned mask and the second patterned mask, and removing the first patterned mask and the second patterned mask to form a first copper grid line and a second copper grid line on the front side of the solar cell and a first copper grid line and a second copper grid line on the back side of the solar cell; S13, depositing interconnection material on the first copper grid line and the second copper grid line to form a first copper grid mesh layer and a second copper grid mesh layer.
7. The method for preparing a solar cell sheet with an anti-hidden cracking property according to claim 6, characterized in that: The method for preparing a solar cell sheet with an anti-hidden crack structure further includes the following steps performed before step S11: S14, forming a first copper seed layer on the front side of the solar cell, and forming a second copper seed layer on the back side of the solar cell; Step S12 includes: S121, using the first patterned mask and the second patterned mask to simultaneously deposit copper material on the first copper seed layer and the second copper seed layer based on an electro-deposition process; S122, removing the first patterned mask and the second patterned mask; S123, removing the first copper seed layer outside the first copper grid mesh layer and the second copper seed layer outside the second copper grid mesh layer to form a first copper grid line and a second copper grid line on the front side of the solar cell and a first copper grid line and a second copper grid line on the back side of the solar cell.
8. A method for interconnecting solar cells to prevent hidden cracks, characterized in that: The method is used to interconnect a first anti-hidden crack solar cell and a second anti-hidden crack solar cell, wherein the first anti-hidden crack solar cell and the second anti-hidden crack solar cell are both anti-hidden crack solar cells according to any one of claims 1 to 5, and the method for interconnecting anti-hidden crack solar cells comprises the following steps: S21, forming a plurality of spaced non-conductive glue dots on the first copper grid layer of the first anti-hidden crack solar cell based on a glue dispensing process, and placing the second copper grid layer of the second anti-hidden crack solar cell downward on the first copper grid layer of the first anti-hidden crack solar cell, so as to fix the second anti-hidden crack solar cell on the first anti-hidden crack solar cell by using the non-conductive glue dots; S22, hot pressing the first anti-hidden crack solar cell and the second anti-hidden crack solar cell to fuse the interconnection material on the first copper grid layer of the first anti-hidden crack solar cell with the interconnection material on the second copper grid layer of the second anti-hidden crack solar cell to complete the interconnection between the first anti-hidden crack solar cell and the second anti-hidden crack solar cell.
9. The method for interconnecting solar cells to prevent hidden cracks according to claim 8, characterized in that: Step S21 includes: S211, placing a tinned copper foil on a region of the first copper grid layer of the first anti-hidden crack solar cell near one of the long side edges, wherein the tinned copper foil is provided with a plurality of through holes at intervals; S212, filling the through hole with non-conductive glue; S213, placing the area of the second copper grid layer of the second anti-hidden crack solar cell close to one of the long side edges on the tinned copper foil, so as to fix the second anti-hidden crack solar cell on the first anti-hidden crack solar cell by using the non-conductive glue dots.
10. The method for interconnecting solar cells to prevent hidden cracks according to claim 8, characterized in that: A plurality of anti-overflow glue grid lines are also arranged on the first copper grid layer of the first anti-hidden crack solar cell sheet, and the non-conductive glue dots are arranged in the anti-overflow glue grid lines.