Curing method of UV adhesive

By using UV glue to assist curing film in photovoltaic module production to form a sandwich structure, avoiding oxygen contact, solving the oxygen polymerization problem after UV glue curing, simplifying the process flow, reducing costs and improving component quality, and wider applicability , and the conductive wire is better wrapped.

CN119050200APending Publication Date: 2024-11-29CHANGZHOU SHICHUANG ENERGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411149215.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-21
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

Existing UV glues are prone to oxygen resistance and polymerization problems after curing in photovoltaic module production, which affects the production yield and appearance of the module. In addition, traditional processes have strict requirements on the viscosity of UV glue, high equipment costs and complex processes.

Method used

The transparent UV glue assisted curing film is used to form the cell-UV glue-UV glue sandwich structure, cure under ultraviolet light source, use the release film to avoid oxygen contact, reduce oxygen polymerization resistance, and simplify the process flow, and is suitable for low-viscosity UV glue.

Benefits of technology

It solves the problem of oxygen resistance, reduces the bonding cost after UV glue cures, improves production efficiency and component quality, has a wider applicability, and has better wrapping properties for conductive wires.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119050200A_ABST
    Figure CN119050200A_ABST
Patent Text Reader

Abstract

The invention provides a UV glue curing method, which comprises the following steps: firstly, welding a conductive wire on a battery piece, then, applying glue and distributing a film on the welded battery piece, forming a sandwich structure of battery piece-UV glue-UV glue auxiliary curing film, and then, irradiating under an ultraviolet light source to realize UV glue curing, so as to form the battery piece-UV glue-UV glue auxiliary curing film. And uncovering the UV adhesive auxiliary curing film to obtain a UV adhesive cured battery piece, and enabling the battery piece to flow to the next process.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of photovoltaics, in particular to a curing method for UV glue. Background Art

[0002] 0BB (Zero Busbar) technology refers to the design concept of removing the main grid on photovoltaic cells in the photovoltaic industry. This design can greatly reduce the silver paste consumption caused by the main grid and significantly reduce costs. As a universal cost-reduction process route, this technology has been widely promoted and applied in recent years. Many leading photovoltaic companies have also regarded it as the most cost-effective technology for mass production in the next few years, and have carried out pilot and mass production introductions.

[0003] Although 0BB is a cost-reduction technology that is gradually maturing, there are still a variety of process routes in the industry. Such as SmartWire solution, dispensing or screen printing glue solution, welding + dispensing solution or dispensing + welding solution, etc. These different process routes have their own advantages and disadvantages. The difficulty of process implementation and product yield will directly affect the performance and cost of the final product. For example, the SmartWire solution requires the conductive wire to be embedded in the organic film, and the process complexity and precision requirements are both high; the dispensing solution has limited fixing effect on the conductive wire, low lamination yield, and difficult rework; the welding + dispensing solution requires an additional dispensing process to reinforce the conductive wire after welding; the dispensing + welding solution has higher requirements for the high temperature resistance and adhesion of the UV glue.

[0004] In the above solutions, except for the SmartWire solution, UV adhesive materials are required. UV adhesive is widely used in various industrial fields due to its fast curing, excellent bonding performance and simple process. As a reinforcing material or auxiliary packaging material for photovoltaic module conductive wires, its high light transmittance, excellent weather resistance, water resistance, mechanical strength and other properties are also of concern.

[0005] However, no matter which process scheme uses UV glue, first of all, the viscosity range of UV glue is relatively narrow, and the material selection cost is relatively high. Secondly, the solution of dispensing or printing glue requires the UV glue on the battery cell to be flipped after curing before it can be connected in series. The equipment cost is high and the process is difficult. In addition, most of the UV glues currently used in mass production have oxygen inhibition problems after curing, which affects the yield of component production. Summary of the invention

[0006] The object of the present invention is to provide a curing process for UV glue in an 0BB scheme to solve the problems of UV glue application process efficiency and oxygen inhibition during curing after application in the prior art.

[0007] To achieve the above object, the present invention provides the following technical solutions: A UV glue curing method, the method comprising first welding a conductive wire on a battery cell, then applying glue and film to the welded battery cell, the glue is UV glue, the film is a transparent UV glue auxiliary curing film, forming a sandwich structure of battery cell-UV glue-UV glue auxiliary curing film, then irradiating under an ultraviolet light source to achieve UV glue curing, uncovering the UV glue auxiliary curing film, obtaining a UV glue-cured battery cell, and flowing to a downstream process.

[0008] Preferably, the UV adhesive auxiliary curing film is a high temperature resistant transparent release film.

[0009] Preferably, the high temperature resistant transparent release film is a transparent release PET film resistant to high temperatures above 120°C.

[0010] Preferably, the UV adhesive has a viscosity higher than 500cps / 25°C.

[0011] Preferably, the glue application pattern is linear or dot-shaped.

[0012] In one embodiment, the step of forming the sandwich structure includes: firstly coating the battery cell with UV glue, and then laying a UV glue auxiliary curing film on the battery cell coated with glue to form the sandwich structure.

[0013] In another embodiment, the step of forming the sandwich structure includes: firstly coating UV glue on the UV glue auxiliary curing film, and then laminating the battery cell on the coated UV glue auxiliary curing film to form the sandwich structure.

[0014] Furthermore, the method of applying the UV glue includes line coating, brush coating, dispensing, rolling coating, spraying or printing.

[0015] Compared with the prior art, the present invention has the following beneficial effects: In the UV glue curing process, we use UV glue to assist in curing the film layer, which has the following significant advantages.

[0016] 1. Simplify the traditional 0BB glue curing process and reduce equipment costs. Two adjacent battery cells can be glued and cured at the same time with one facing up and the other facing down and connected in series. Figure 7 The traditional printing glue solution requires an additional flipping action, that is, after printing glue on one side of a cell and curing it, it is flipped 180° and connected in series with another cell while the glue is printed and cured. This process solution has many steps, high positioning accuracy requirements, and low welding yield.

[0017] 2. Good process compatibility, compatible with the traditional 0BB components' commonly used processes of first gluing and then welding, or first welding and then gluing, and low transformation cost.

[0018] 3. The optional glue types and formulas for process adaptation are much more than those of traditional solutions. Because there is an auxiliary curing layer, the requirements for UV glue viscosity are greatly reduced. The traditional printing glue solution usually requires glue viscosity>15000cps / 25℃, and the upward electromagnetic spray valve dispensing solution usually requires glue viscosity>20000cps / 25℃, all to prevent the glue droplets from deforming or dripping under the action of gravity after being hit on the battery cell. Our solution does not have this risk and is also applicable to low-viscosity glue. Due to the use of release film support, as long as the glue liquid has a certain surface tension so that it can be formed on the release film, the solution of the present invention can be realized. Therefore, in principle, the viscosity and thixotropy of the glue that can be used in the present invention can be as low as 0, but in actual production, the cost of this glue with extreme performance is also high. The minimum viscosity of the glue we use in actual production is 500cps / 25℃, and the minimum thixotropy is 0.5, that is, the glue material with a viscosity higher than 500cps / 25℃ and a thixotropy higher than 0.5 is used in actual production.

[0019] 4. No oxygen inhibition problem. For the acrylic system UV glue commonly used in the industry, free radical polymerization occurs during the curing process. However, when the glue is exposed to the air for curing, the surface of the glue will become uncured and sticky, which is called oxygen inhibition. The problem of oxygen inhibition can cause the surface of the glue to be easily contaminated with dust and other impurities, affecting the appearance of the components and reducing the process yield. It can also cause adhesion between the glue surface and the film surface, and produce film wrinkles and bubbles during the lamination process. It can also cause a large number of oxidizing structures such as hydroxyl, carbonyl, and peroxy groups in the surface of the UV glue, thereby affecting the long-term stability of the UV glue. Our solution does not have oxygen inhibition problems because the surface of the UV glue does not come into contact with oxygen during the curing process.

[0020] 5. UV glue has better wrapping properties for conductive wires. In traditional glue dispensing or printing solutions, the cross-section of the conductive wire wrapped by the glue after curing is an arc-shaped surface, such as Fig. 9 and Fig.10 As shown. However, our solution wraps the conductive wire in a drum-shaped surface, which provides better protection and fixation for the conductive wire, as shown Fig.11 As shown. The same is true for different types of conductive wires, such as triangular conductive wires. Fig.12 shown.

[0021] 6. The auxiliary curing film layer may be made of, but is not limited to, high temperature resistant transparent release PET, which has low cost and good versatility. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 Schematic diagram of a cell before gluing in process example 1 of the present invention; Figure 2 is a schematic diagram of a battery cell after glue application in process embodiment 1 of the present invention, wherein the glue application pattern is linear; Figure 3 It is a schematic diagram of a cell sheet on which a UV glue auxiliary curing film is laid after glue application in process embodiment 1 of the present invention; Figure 4 Schematic diagram of a cell before glue application in process embodiment 2 of the present invention; Figure 5 Schematic diagram of the UV glue-assisted curing film after glue application in process example 2 of the present invention, wherein the glue application pattern is in the shape of dots; Figure 6 It is a schematic diagram of the structure after the battery cell and the UV glue auxiliary curing film after glue application in process embodiment 2 of the present invention are bonded; Figure 7 It is a schematic diagram of a cell with the UV glue auxiliary curing film uncovered after the UV glue is cured in process embodiment 2 of the present invention; Figure 8 It is a schematic diagram of the effect of curing two sides of two battery cells simultaneously by using the process of the present invention; Fig. 9 and Fig.10 It is a wrapping surface formed on the grid line by the prior art glue dispensing process; Fig.11 and Fig.12 It is a wrapping surface formed on the grid line by the process of the present invention; Fig.13 It is a schematic diagram of coating glue on the release film in the release film transfer process using glue in Example 3; Fig.14 Schematic diagram of using low-viscosity glue to spread over a large area on the surface of a battery cell.

[0023] In the picture: 1. Battery cell; 2. Conductive wire; 3. UV glue; 4. Release film. DETAILED DESCRIPTION

[0024] The present invention has developed a novel UV adhesive curing method. In the method of the present invention, a transparent release material is used as an auxiliary curing film layer of the UV adhesive. This material is not limited to transparent high temperature resistant release PET. This release film can be used as a protective film layer during UV adhesive curing, and can also be used as a UV adhesive transfer and auxiliary curing film layer.

[0025] In the method of the present invention, the UV glue is cured by forming a sandwich structure of a battery cell-UV glue-release film on the battery cell.

[0026] In one exemplary embodiment, UV glue is applied to the cell and then covered with a release film to form a sandwich structure. In another exemplary embodiment, UV glue is first applied to the release film and then transferred to the cell. The transfer process can be to cover the release film coated with UV glue on the cell, or to attach the cell to the release film coated with UV glue.

[0027] The release film can cover the area of ​​UV glue coating on the battery cell, or even cover the entire battery cell. For example, in a battery cell with a specification of 182*91mm, the auxiliary curing film layer can be 184*93mm in size, which is one circle larger than the battery cell and just covers the entire battery cell.

[0028] The above two methods of forming the sandwich structure can be used in combination. For example, in the process of forming a battery string, the above two methods are respectively used on two adjacent battery cells. The upper surface of one battery cell forms a structure of release film-UV glue-battery cell from top to bottom, and the lower surface of the adjacent battery cell forms a structure of battery cell-UV glue-release film from top to bottom. Then, the UV glue on the two battery cells is irradiated with a light source from top to bottom, and the adjacent battery cells are irradiated with a light source from bottom to top. Figure 8 As shown, two light sources illuminate at the same time, which not only saves the process flow, but also eliminates the need to flip the battery cell, greatly improving production efficiency.

[0029] The method of the present invention also makes the application options for glue more extensive. In the prior art, for the formation of a battery string, one method is to dispense glue and cure on the first battery cell, and then carry out the subsequent production process. However, for the second battery cell, since the UV glue is located on the lower surface of the battery cell, it is impossible to dispense glue and cure directly on the lower surface. The glue surface must be dispensed and cured upwards and then flipped to be used in series with the first battery cell. However, in the method of the present invention, because a release film is used to support the glue, it can be directly bonded and cured on the glue surface of the second battery cell, and then directly connected in series with the first battery cell. In another prior art process, in order to reduce this flipping procedure, a glue with a higher viscosity is used, and the glue is sprayed from bottom to top, and sprayed on the glue surface of the second battery cell. Because the glue has a high viscosity, it will stick to the battery cell even if it is not cured, and will not drip down due to gravity. But it is obvious that this process has a high requirement for the viscosity of the glue. In the process of the present invention, a release film is used, and the glue can be applied on the release film, and then the battery cell is laid, so a glue with a lower viscosity can be used. And after laying the battery cells, they can be cured directly without turning over the battery cells.

[0030] The method of the present invention also solves the oxygen inhibition problem existing in the prior art. In the prior art solution, due to the oxygen inhibition phenomenon, the surface of the glue becomes sticky after curing, and is easily contaminated with dust or dirt. If it is a large particle of dust or dirt, bubbles are easily generated after lamination packaging, and the appearance can be seen to be abnormal and unsightly, and the component needs to be downgraded; in addition, the surface of the glue is sticky, and when laying the film, the glue is easy to adhere to the film, so that the battery cell is easily displaced by the film, or the film is wrinkled, affecting the yield; furthermore, when oxygen inhibition occurs, the surface of the glue is actually not completely cured, and a chemical reaction may occur between the incompletely cured glue and the film, and the reliability of the glue and the reliability of the component after packaging are affected. However, by adopting the method of the present invention, the release film prevents the contact between the surface of the glue and the air, avoiding the problem of oxygen inhibition, and the glue itself is completely cured from the surface to the inside. When the glue is completely cured, the surface is also completely cured, so the surface of the cured UV glue is completely non-sticky, thereby avoiding the above-mentioned problems.

[0031] The method of the present invention also solves the problem of glue wrapping the conductive wire, thereby further improving the strength and quality of the finished product. Fig. 9 and Fig.10 When the method of the present invention is used, a drum-shaped liquid surface is generally formed, such as Fig.11 and Fig.12 As shown. This is because of the influence of the surface tension of the liquid, and the different wettability of the liquid on the surface of different materials. For example, the UV glue has better wettability on the surface of the battery cell, so the UV glue will flow wider on the surface of the battery cell, while the UV glue has poorer wettability on the release film, so the UV glue will not spread easily on the release film. Therefore, the distribution of the UV glue between the release film and the battery cell will appear narrow at the top and wide at the bottom, forming a drum-shaped liquid surface. The average thickness of the drum-shaped liquid surface wrapped around the conductive wire is thicker, especially on the upper part of the conductive wire, such as Fig. 9 and Fig.10 Compared with the thickness of the upper glue of the conductive wire of the prior art, the thickness of the upper glue of the conductive wire is obviously lower. Fig.11 and Fig.12 The method of the present invention can form a significantly thicker glue thickness on the upper part of the conductive wire. Therefore, after being cured by the method of the present invention, the wrapping, protection and fixation of the glue on the conductive wire are enhanced.

[0032] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0033] In the description of the present invention, it should be noted that the terms "upper", "lower", "inner", "outer", "front end", "rear end", "two ends", "one end", "the other end" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance.

[0034] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "provided with", "connected", etc. should be understood in a broad sense. For example, "connected" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0035] The PET fluorine release film used in the embodiment is purchased from Jinguan New Materials Co., Ltd., product number CF-S5094, size 1090*500mm, thickness 75u, release force 5-8g. The silicone oil release film used in the embodiment is purchased from Jinguan New Materials Co., Ltd., product number GC-210, size 1090*500mm, thickness 60u, release force 5-8g. Release film materials have been widely used in packaging, printing, pad printing, flexible circuit and other industries. It should be understood that although the embodiment is described with this kind of release film as an example, other release films with similar properties can also be applied to the process of the present invention, such as other halogen release films, silicone oil release films, etc., as long as they have the properties required in the process of the present invention, such as resistance to high temperatures above 120°C, having a certain transparency for UV light curing, etc., so as to achieve the effect of the process of the present invention. Example 1

[0036] The battery cells that need to be glued are as follows: Figure 1 As shown, it is characterized by no main grid, a multi-segment parallel current collection layer structure, and conductive wires have been welded on each current collection layer.

[0037] Use the dispensing process to evenly apply UV glue lines on the battery cells, such as Figure 2 The UV glue used in this embodiment has a characteristic viscosity of 6000-8000 cps / 25°C and is purchased from Shanghai Hansi Industrial Co., Ltd., product number UV03600603.

[0038] A transparent release PET film is laid on the battery cell. The transparent release PET film is a silicone oil release film with a short-term high temperature resistance of more than 120°C and a thickness of 100 microns. Figure 3 shown.

[0039] A 365nm ultraviolet light source is set up directly above the cell to irradiate until the UV glue is cured. Finally, the release film is peeled off and the cell flows to the subsequent process. Example 2

[0040] The battery cells that need to be glued are as follows: Figure 4 As shown, it is characterized by no main grid, a multi-segment parallel current collection layer structure, and conductive wires have been welded on each current collection layer.

[0041] The glue PAD dot array is printed on the UV glue auxiliary curing film layer using screen printing technology, such as Figure 5 The characteristic viscosity of the UV glue used in this embodiment is 34000-40000cps / 25°C, purchased from Shenzhen Hongjin Technology Co., Ltd., product number UV5284(-3).

[0042] Its UV glue-assisted curing film layer is a transparent fluorine-release PET film with short-term high temperature resistance of over 180°C and a thickness of 80 microns.

[0043] Keep the release film fixed, align the battery cell to be glued on the bottom surface with the glue point, and then stick it on the release film. Figure 6 As shown ( Figure 6 for bottom view).

[0044] A 365nm ultraviolet light source is set up just below the cell with the release film attached, and irradiated upward until the UV glue is cured. At the same time, another cell connected in series with this cell also completes the glue curing upward.

[0045] Finally, remove the release film from the surface of the battery cell, and the effect is as follows Figure 7 As shown, the battery strings flow to the back-end process. Example 3

[0046] The battery cells that need to be glued are as follows: Figure 1 As shown, it is characterized by no main grid, a multi-segment parallel current collection layer structure, and conductive wires have been welded on each current collection layer.

[0047] Use the dispensing process to evenly punch out UV glue lines on the UV glue auxiliary curing film layer, such as Fig.13 The UV glue used in this embodiment has a characteristic viscosity of 15000-20000 cps / 25°C and is purchased from Shenzhen Hongjin Technology Co., Ltd., product number UV5284(-4).

[0048] Its UV adhesive auxiliary curing film layer is a transparent fluorine release film with a short-term high temperature resistance of more than 180°C and a thickness of 60 microns. Figure 3 shown.

[0049] Keep the release film fixed, align the battery cell to be glued on the bottom surface with the glue line, and then stick it on the release film. Figure 3 As shown ( Figure 3 Can also be a bottom view).

[0050] A 365nm ultraviolet light source is set up just below the cell with the release film attached, and irradiated upward until the UV glue is cured. At the same time, another cell connected in series with this cell also completes the glue curing upward.

[0051] Finally, remove the release film from the surface of the battery cell, and the effect is as follows Figure 2 As shown (at this time Figure 2 The UV glue has been cured), and the battery strings flow to the subsequent process. Example 4

[0052] The battery cells that need to be glued are as follows: Figure 1 As shown, it is characterized by no main grid, a multi-segment parallel current collection layer structure, and conductive wires have been welded on each current collection layer.

[0053] Use the dispensing process to evenly apply UV glue lines on the battery cells, such as Figure 2 The UV glue used in this embodiment has a viscosity of 2000-6000 cps / 25°C and is purchased from Shenzhen Hongjin Technology Co., Ltd., product number UV5284(-9).

[0054] A transparent release PET film is laid on the battery cell. The transparent release PET film is a fluorine release film with a short-term high temperature resistance of more than 180°C and a thickness of 60 microns. Figure 3 shown.

[0055] A 365nm ultraviolet light source is set up directly above the cell to irradiate until the UV glue is cured. Finally, the release film is peeled off and the cell flows to the subsequent process. Example 5

[0056] The battery cells that need to be glued are as follows: Figure 1 As shown, it is characterized by no main grid, a multi-segment parallel current collection layer structure, and conductive wires have been welded on each current collection layer.

[0057] The UV glue dots are evenly sprayed on the battery cell by spraying. The characteristic viscosity of the UV glue used in this embodiment is 500-1500cps / 25°C, thixotropic 1, purchased from Shanghai Hansi Industrial Co., Ltd., product number UV03600609.

[0058] After spraying the glue, due to its low viscosity and thixotropy, the glue will spread over a large area on the surface of the battery cell under the influence of the capillary action of the conductive wire and the surface tension. Fig.14 As shown, the shaded part is the UV glue spread on the entire surface. Low-viscosity glue is used to form a larger coverage area, which provides better protection for the battery cell. However, in the traditional process, the low-viscosity glue has a low adhesion to the conductive wire before curing, and in addition to the difficulty in bonding and forming on the lower surface of the battery cell as mentioned above, a larger coverage area will also lead to an excessively large sticky area, an increase in the dust-adhesive surface, and difficulty in controlling the glue-coated area, resulting in a decrease in the quality of subsequent battery cells. However, by adopting the method of the present invention and using a release film for control, the glue-coated area can be well controlled, and the release film forms a shield to isolate the sticky area formed by the glue coating from the external environment, thereby avoiding exposure of the sticky area and preventing it from being contaminated by dust, thereby improving the quality of subsequent battery cells.

[0059] A transparent release PET film is laid on the battery cell. The transparent release PET film is a silicone oil release film with a short-term high temperature resistance of more than 120°C and a thickness of 60 microns.

[0060] A 365nm ultraviolet light source is set up directly above the cell to irradiate until the UV glue is cured. Finally, the release film is peeled off and the cell flows to the subsequent process.

[0061] Embodiment 1 and embodiment 2 can be combined to manufacture a battery string. Figure 8 The cross section of a battery string covered with a release film when the UV glue is cured is shown when the battery string is manufactured by combining the above two solutions.

[0062] Although the above examples 1 and 2 are described in conjunction with specific means, those skilled in the art should understand that the above means are only for illustrative purposes and should not be regarded as limiting the scope of protection of the present invention. The specific scope of protection shall be subject to the claims. For example, the above example 1 only describes the means of first applying glue to the battery cell, then coating it, and then curing it. However, the transfer method shown in example 2 can also be used in example 1. In examples 1 and 2, conductive wires under stacked grid technology are used as the current extraction structure of the battery cell, but it should be understood that any other type of current extraction structure is also applicable to the present invention, and even the main grid under the main grid structure can be fixed and protected using the solution of the present invention.

[0063] The matters not described in detail in the present invention are all known technologies to those skilled in the art.

[0064] Finally, it should be noted that the above specific implementation methods are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the embodiments, those skilled in the art should understand that the technical solution of the present invention can be modified and replaced by equivalents without departing from the spirit and scope of the technical solution of the present invention, which should be included in the scope of the claims of the present invention.

Claims

1. A UV glue curing method, characterized in that: The method comprises first welding a conductive wire on a battery cell, then applying glue and film to the welded battery cell, wherein the glue is UV glue, and the film is a transparent UV glue auxiliary curing film, to form a sandwich structure of battery cell-UV glue-UV glue auxiliary curing film, and then irradiating the battery cell under an ultraviolet light source to achieve UV glue curing, uncovering the UV glue auxiliary curing film, obtaining a battery cell cured with UV glue, and sending the battery cell to a subsequent process.

2. The UV glue curing method according to claim 1, characterized in that: The UV adhesive auxiliary curing film is a high temperature resistant transparent release film.

3. The UV glue curing method according to claim 2, characterized in that: The high temperature resistant transparent release film is a transparent release PET film resistant to high temperatures above 120°C.

4. The UV glue curing method according to claim 1, characterized in that: The UV adhesive viscosity is higher than 500cps / 25°C.

5. The UV glue curing method according to claim 1, characterized in that: The glue application pattern is linear or dotted.

6. The UV glue curing method according to claim 1, characterized in that: The steps of forming the sandwich structure include: firstly coating the battery sheet with UV glue, and then laying the UV glue auxiliary curing film on the battery sheet coated with glue to form the sandwich structure.

7. The UV glue curing method according to claim 1, characterized in that: The steps of forming the sandwich structure include: firstly coating UV glue on the UV glue auxiliary curing film, and then laminating the battery sheet on the UV glue auxiliary curing film coated with glue to form the sandwich structure.

8. The UV glue curing method according to any one of claims 6 or 7, characterized in that: Methods for applying UV glue include line coating, brushing, dispensing, rolling, spraying or printing.