Manufacturing method of rechargeable cylindrical battery main body
By designing the welding of the bent body and the shell bottom in a lithium-ion cylindrical battery, and using an isolator to isolate the current collecting disk and the shell bottom, the circuit breaking and welding problems caused by the small welding area between the current collecting disk and the steel shell bottom are solved. Improves welding reliability and battery body stability.
Patent Information
- Application Number
- CN202410950862.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2024-11-29
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The welding area between the current collecting disk and the steel shell bottom of the lithium-ion cylindrical battery is small, and it is easy to cause circuit breakage and dummy welding, which is difficult to meet market demand.
By designing the bent body of the current collecting disk and welding it with the bottom of the shell, and using an isolation body to arrange it around the bent body to isolate the current collecting disk and the bottom of the shell, ensuring local overcurrent and reducing the occurrence of dummy welding.
It effectively reduces the occurrence of dummy welding, improves the reliability and strength of welding, and ensures reliable connection of the battery body.
Smart Images

Figure CN119050491A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for manufacturing a battery used as power, and in particular to a method for manufacturing a rechargeable cylindrical battery body. Background Art
[0002] With the vigorous development of the new energy industry, a huge market is provided for the battery industry, thereby accelerating the pace of development of the battery industry.
[0003] At present, lithium-ion cylindrical batteries have gradually become the mainstream products in the new energy industry due to their advantages such as high energy density, increased charge and discharge rate, and good capacity consistency. Since full-tab / collector plate has been determined by more and more manufacturers as the preferred direction of cylindrical battery structure, the welding of the collector plate and the bottom of the steel shell is more important, but the common problems are as follows:
[0004] (1) The collector plate and the bottom of the steel shell are welded together by resistance welding. Due to the matching problem, the welding area is small, which makes it easy to break the circuit during vibration, which is difficult to meet the current market demand.
[0005] (2) After the collector plate is welded to the foil, it is easily squeezed by the winding core, causing the collector plate to fit the shell bottom. When the collector plate and the shell bottom of the steel shell are welded by resistance welding, a shunt effect occurs between the collector plate and the shell bottom, resulting in a cold weld.
[0006] Therefore, there is an urgent need for a method for manufacturing a rechargeable cylindrical battery body to overcome one or more of the above-mentioned defects. Summary of the invention
[0007] The object of the present invention is to provide a method for manufacturing a rechargeable cylindrical battery body. The rechargeable cylindrical battery body manufactured by the manufacturing method can ensure local overcurrent, so as to reduce the occurrence of cold welding during the welding process.
[0008] To achieve the above-mentioned purpose, the manufacturing method of the rechargeable cylindrical battery body of the present invention comprises the following steps:
[0009] A winding core and a current collecting plate are provided, wherein the current collecting plate comprises a current collecting plate body and a bent body bent from the end of the current collecting plate body and arranged in a layered manner and spaced apart from the current collecting plate body, and a pole ear at the first end of the winding core is welded to an end surface of the current collecting plate body facing away from the bent body;
[0010] Providing a housing and an insulating isolator, so that the isolator is arranged around the bend and covers the end surface of the collector plate body facing the bend;
[0011] The shell bottom and the bent body of the shell are welded together.
[0012] Compared with the prior art, by means of the design that "the isolator is arranged around the bending body and covers the end face of the collector body facing the bending body", the collector is welded to the shell bottom only at the position of the bending body, and the other positions of the collector are insulated and separated from the shell bottom by the isolator, so that the rechargeable cylindrical battery body made by the manufacturing method of the present invention can ensure local overcurrent, thereby reducing the occurrence of cold welding during the welding process. At the same time, since the bending body is bent out from the collector body, when the collector is a composite layer structure, such as a copper-nickel composite layer structure, the end faces of the bending body and the collector body facing each other are made of the same material, and the end faces facing each other are also made of the same material, so when the pole ear of the winding core is laser welded to the collector body, the welding high-reflection phenomenon can be avoided, thereby making the welding of the pole ear of the winding core and the collector body more reliable.
[0013] Preferably, before welding the shell bottom and the bent body together, the winding core, the current collecting plate and the isolating body are first moved into the shell, and the bent body and the shell bottom are kept in close contact.
[0014] Preferably, before welding the shell bottom of the shell and the bent body together, an external ejector pin is moved along the central channel of the winding core and the through hole of the collecting plate body to a position for pushing the bent body, so that the ejector pin keeps the bent body and the shell bottom in close contact.
[0015] Preferably, the bent body includes a first bent body bent from the end of one side of the collecting plate body and a second bent body bent from the end of the other side of the collecting plate body, and the first bent body is located between the collecting plate body and the second bent body; the external ejector pin pushes the first bent body to keep the first bent body and the second bent body and the second bent body and the shell bottom in a tight state.
[0016] Preferably, the shell bottom and the second bending body and the first bending body and the second bending body are welded together by resistance welding.
[0017] Preferably, the current collecting plate is a composite layer structure.
[0018] Preferably, the shell bottom is formed into an outer ring base for supporting the isolation body and a sunken inner ring portion sunken relative to the outer ring base through a stretching process, and the bent body and the sunken inner ring portion are welded together.
[0019] Preferably, a central through hole is opened at the central position of the insulating body, and the bent body passes through the central through hole, so that the bent body is surrounded by the insulating body.
[0020] Preferably, the isolator is a circular ring gasket.
[0021] Preferably, the separator arranged around the bent body is obtained by encapsulating the end surface of the collecting plate body facing the bent body and the first end of the winding core with rubber, and the separator is also arranged around the first end of the winding core. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 The figure shows the state when the first end of the winding core is welded to the collecting plate.
[0023] Figure 2 is Figure 1 The state diagram of the insulation obtained by encapsulation is also shown.
[0024] Figure 3 is Figure 2 A status diagram of the housing is also displayed on the base.
[0025] Figure 4 is Figure 3 The base also shows a state diagram in which the external ejector pin keeps the second bending body and the shell bottom and the first bending body and the second bending body in a close contact state.
[0026] Figure 5 is a plan view showing a rechargeable cylindrical battery main body having a structure manufactured by the manufacturing method of the present invention.
[0027] Figure 6 This is a diagram of the interior of the housing.
[0028] Figure 7 It is a three-dimensional diagram of the collecting plate.
[0029] Figure 8 yes Figure 7 The collecting plate shown is a plan view viewed in the direction indicated by the arrow above it.
[0030] Fig. 9 yes Figure 7 Floor plan viewed from top to bottom.
[0031] Fig.10 is along Fig. 9 A three-dimensional internal view cut along the CC line.
[0032] Fig.11 It is a three-dimensional diagram of the insulator formed by the encapsulation.
[0033] Fig.12 It is an internal view of a rechargeable cylindrical battery body of another structure manufactured by the manufacturing method of the present invention.
[0034] Fig.13 yes Fig.12 A stereogram of the isolate in FIG. DETAILED DESCRIPTION
[0035] Embodiments of the present invention will now be described with reference to the accompanying drawings, wherein like reference numerals represent like elements throughout the several views.
[0036] Combination Figures 1 to 5 The manufacturing method of the rechargeable cylindrical battery body of the present invention comprises the following steps:
[0037] A winding core 20 and a current collecting plate 30 are provided; wherein the current collecting plate 30 comprises a current collecting plate body 30a and a bent body 30b bent from the end of the current collecting plate body 30a and arranged in a layered manner and spaced from the current collecting plate body 30a; a pole ear (for example but not limited to a full pole ear) at the first end 22 of the winding core 20 is welded to an end surface 30a1 of the current collecting plate body 30a facing away from the bent body 30b, and the state is shown in FIG. Figure 1 As shown. Optionally, as an example, the collector plate 30 is a composite layer structure, such as but not limited to a copper-nickel composite layer structure or an aluminum-nickel composite layer structure, so that the bending body 30b and the end face 32 (30a2) of the collector plate body 30a facing each other are made of the same material; that is, the end face 32 and the end face 30a2 (see Figure 8 ) are made of the same material, and the end faces 33 (30a1) of the bend 30b and the collector plate body 30a facing each other are also made of the same material, that is, the end faces 33 and 30a1 (see Figure 8 ) The materials of the two are the same; this design can prevent the use of laser to weld the pole ear of the first end 22 of the winding core 20 with the end surface 30a1 of the collecting plate body 30a facing away from the bending body 30b, thereby generating a high-reflection welding phenomenon.
[0038] Provide a housing 10 and an insulating isolator 40, so that the isolator 40 is arranged around the bent body 30b, and the isolator 40 covers the end surface 30a2 of the collector plate body 30a facing the bent body 30b. Figure 2 Optionally, Figure 2 As an example, an isolating body 40 arranged around the bending body 30b is obtained by encapsulating the end surface 30a2 of the collecting plate body 30a facing the bending body and the first end 22 of the winding core 20, and the isolating body 40 is also arranged around the first end 22 of the winding core 20; such a design can also insulate and separate the first end 22 of the winding core 20 from the side wall 12 of the outer shell 10, thereby further reducing the effect of cold soldering.
[0039] And the shell bottom 11 of the shell 10 is welded with the bent body 30b. Figures 1 to 3 As an example, before welding the shell bottom 11 of the shell 10 and the bent body 30b together, first move the winding core 20, the collecting plate 30 and the separator 40 into the shell 10, and keep the bent body 30b and the shell bottom 11 in close contact, in preparation for welding. Figure 4As an example, before the shell bottom 11 of the shell 10 and the bent body 30b are welded together, the external ejector pin 200 is moved along the central channel 21 of the winding core 20 and the through hole 31 of the collector plate body 30a to the position of pushing the bent body 30b, so that the ejector pin 200 keeps the bent body 30b and the shell bottom 11 in a close contact state; the advantage of this design is that the ejector pin 200 and the end surface 30a1 of the collector plate body 30a facing away from the bent body 30a are made of the same material. At this time, with the help of the through hole 31, the ejector pin 200 is used to push the end face 32 of the bend 30b facing the collector plate body 30a, and the material of the end face 32 is different from the end face 30a1 of the collector plate body 30a facing away from the bend 30a. For example, when the end face 30a1 of the collector plate body 30a is a copper surface and the end face 30a2 is a nickel surface, the ejector pin 200 is pushed against the nickel surface, so the defect of material sticking to the needle (i.e., the ejector pin 200) during the welding process is effectively prevented. In addition, the defect of the collector plate 30 being too thick and having a cold solder joint is avoided. More specifically, as follows:
[0040] like Figures 1 to 5 ,as well as Figure 8 and Fig.10 As shown, as an example, the bent body 30b includes a first bent body 30b1 bent from the end of one side of the collecting plate body 30a and a second bent body 30b2 bent from the end of the other side of the collecting plate body 30a, and the first bent body 30b1 is located between the collecting plate body 30a and the second bent body 30b2; the purpose of this design is that after welding is completed, current is passed through the first bent body 30b1 and the second bent body 30b2 at the same time, so the effect of passing current is better. When the bending body 30b includes the first bending body 30b1 and the second bending body 30b2, at this time, the external ejector pin 200 pushes the first bending body 30b1 to keep the first bending body 30b1 and the second bending body 30b2 and the second bending body 30b2 and the shell bottom 11 in a close contact state, thereby meeting the need to weld the first bending body 30b1 and the second bending body 30b2 and the second bending body 30b2 and the shell bottom 11 together. Specifically, as an example, resistance welding is used to weld the shell bottom 11 and the second bending body 30b2 and the first bending body 30b1 and the second bending body 30b2 together, thereby improving the reliability and strength of welding; obviously, other welding methods can also be used according to actual needs.
[0041] like Figures 3 to 6As shown, as an example, the shell bottom 11 is formed into an outer ring base 111 for supporting the isolation body 40 and a sunken inner ring portion 112 sunken relative to the outer ring base 111 through a stretching process, and the bending body 30b (specifically the second bending body 30b2) is welded to the sunken inner ring portion 112; with the help of the design of the sunken inner ring portion 112, sufficient avoidance space is provided for the multi-layer design of the collecting plate 30, and the reliability of the welding of the bending body 30b and the shell bottom 11 is ensured.
[0042] like Fig.11 As shown, due to Fig.11 The isolating body 40 shown is formed by encapsulation, and the bending body 30 b needs to be avoided during the encapsulation process, so the isolating body 40 formed by encapsulation will have a central through hole 41 .
[0043] And Fig.12 and Fig.13 In the embodiment, since the isolating body 40 is a circular gasket, the central through hole 41 is opened at the center of the isolating body 40, so that the bent body 30b passes through the central through hole 41, so that the bent body 30b is surrounded by the isolating body 40. It should be noted that when the isolating body 40 is formed by rubber coating, the rubber coating operation is performed before the winding core 20 and the collecting plate 30 are moved into the housing 10. When the isolating body 40ˋ is a circular gasket, the isolating body 40ˋ can be firstly put on the bending body 30b, and then the isolating body 40ˋ, the winding core 20 and the collecting plate 30 can be moved into the outer shell 10 together; optionally, as an example, the winding core 20 and the collecting plate 30 can be reversed first so that the bending body 30b is arranged upward, and then the isolating body 40ˋ is put on the bending body 30b, and finally, the outer shell 10 is put on the isolating body 40ˋ, the collecting plate 30 and the winding core 20; obviously, according to actual needs, the isolating body 40ˋ, the collecting plate 30 and the winding core 20 can also be installed in the outer shell 10 in sequence.
[0044] Compared with the prior art, by virtue of the design that "the isolating body 40 (40ˋ) is arranged around the bending body 30b and covers the end surface 30a2 of the collecting plate body 30a facing the bending body 30b", the collecting plate 30 is welded to the shell bottom 11 only at the position of the bending body 30b, and the other positions of the collecting plate 30 are insulated and separated from the shell bottom 11 by the isolating body 40 (40ˋ), so that the rechargeable cylindrical battery body 100 (100ˋ) manufactured by the manufacturing method of the present invention can ensure local overcurrent, thereby reducing the occurrence of cold welding during the welding process. At the same time, since the bending body 30b is bent out from the collecting disc body 30a, when the collecting disc 30 is a composite layer structure, such as a copper-nickel composite layer structure, the end faces 32 (30a2) facing each other of the bending body 30b and the collecting disc body 30a are made of the same material, and the end faces 33 (30a1) facing each other of the bending body 30b and the collecting disc body 30a are also made of the same material. Therefore, when the pole ears of the winding core 20 and the collecting disc body 30a are laser welded, the high reflection phenomenon of welding can be avoided, thereby making the welding of the pole ears of the winding core 20 and the collecting disc body 30a more reliable.
[0045] It is worth noting that the rechargeable cylindrical battery body 100 (100ˋ) obtained by the manufacturing method of the present invention is further provided with a cover, an explosion-proof valve and an electrolyte, so as to form a complete battery product. In addition, the collector plate 30 is not limited to a disc shape, and can be a strip shape according to actual needs. Finally, Figure 8 and Fig.10 Although it is shown that there is a certain gap between the first curved body 30b1 and the second curved body 30b2, this is before the collector plate 30 is welded to the shell bottom 11. However, during the welding process, due to the top pressure of the ejector pin 200 on the first curved body 30b1, the first curved body 30b1 and the second curved body 30b2 and the second curved body 30b2 and the shell bottom 11 are kept in close contact. Figure 4 As shown, the first bending body 30b1 and the second bending body 30b2 and the second bending body 30b2 and the shell bottom 11 are welded together by resistance welding, so there is no gap between the first bending body 30b1 and the second bending body 30b2 after welding. Figure 8 and Fig.10 The gap shown in .
[0046] The above disclosure is only the preferred embodiment of the present invention, which certainly cannot be used to limit the scope of rights of the present invention. Therefore, equivalent changes made according to the scope of the patent application of the present invention are still within the scope covered by the present invention.
Claims
1. A method for manufacturing a rechargeable cylindrical battery body, It is characterized in that The steps include: A winding core and a current collecting plate are provided, wherein the current collecting plate comprises a current collecting plate body and a bent body bent from the end of the current collecting plate body and arranged in a layered manner and spaced apart from the current collecting plate body, and a pole ear at the first end of the winding core is welded to an end surface of the current collecting plate body facing away from the bent body; Providing a housing and an insulating isolator, so that the isolator is arranged around the bend and covers the end surface of the collector plate body facing the bend; The shell bottom and the bent body of the shell are welded together.
2. The method for manufacturing a rechargeable cylindrical battery body according to claim 1, It is characterized in that Before welding the shell bottom and the bent body together, first move the winding core, the current collecting plate and the isolating body into the shell, and keep the bent body and the shell bottom in close contact.
3. The method for manufacturing a rechargeable cylindrical battery body according to claim 1, It is characterized in that Before welding the shell bottom of the shell and the bent body together, the external ejector pin is moved along the central channel of the winding core and the through hole of the collecting plate body to the position of pushing the bent body, so that the ejector pin keeps the bent body and the shell bottom in close contact.
4. The method for manufacturing a rechargeable cylindrical battery body according to claim 3, It is characterized in that The bent body includes a first bent body bent from the end of one side of the current collecting plate body and a second bent body bent from the end of the other side of the current collecting plate body, and the first bent body is located between the current collecting plate body and the second bent body; the external ejector pin pushes the first bent body to keep the first bent body and the second bent body and the second bent body and the shell bottom in a close contact state.
5. The method for manufacturing a rechargeable cylindrical battery body according to claim 3, It is characterized in that The shell bottom and the second bending body as well as the first bending body and the second bending body are welded together by resistance welding.
6. The method for manufacturing a rechargeable cylindrical battery body according to claim 3, It is characterized in that The collecting plate is a composite layer structure.
7. The method for manufacturing a rechargeable cylindrical battery body according to claim 1, It is characterized in that Through the stretching process, the shell bottom is formed with an outer ring base for supporting the isolation body and a sunken inner ring portion sunken relative to the outer ring base, and the bent body and the sunken inner ring portion are welded together.
8. The method for manufacturing a rechargeable cylindrical battery body according to claim 1, It is characterized in that The central through hole is opened at the central position of the isolating body, and the bent body is passed through the central through hole, so that the bent body is surrounded by the isolating body.
9. The method for manufacturing a rechargeable cylindrical battery body according to claim 8, It is characterized in that The isolating body is a circular ring gasket.
10. The method for manufacturing a rechargeable cylindrical battery body according to claim 1, It is characterized in that The separator arranged around the bent body is obtained by encapsulating the end surface of the collecting plate body facing the bent body and the first end of the winding core. The separator is also arranged around the first end of the winding core.
Citation Information
Patent Citations
Method for assembling pole terminal of cylindrical battery
CN117855559A
Collector plate for power battery, power battery and assembly method of collector plate
CN117913469A
Cylindrical battery and battery pack
CN218498308U
Battery
CN220358203U