PU protective film and preparation process thereof

By setting up a silicon coating film on the PU protective film and improving the adhesive layer components, combined with the film-removing component design of the die-cutting machine, the problem of dust generated by the PU protective film during the die-cutting process is solved, and the film's anti-cutting performance is improved. Tidyness improves production quality.

CN119060648AInactive Publication Date: 2024-12-03SUZHOU GERUN TEXTILE TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410997098.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-24
Publication Date
2024-12-03
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The PU protective film is prone to dust during die cutting, resulting in performance and quality problems, mainly due to its structure and external dust.

Method used

A silicon coated film is provided on the base layer of the PU protective film, and an antistatic agent, hard resin and fluorine-containing hydroxyl resin are added to the glue layer to form a microporous structure, enhancing the anti-cutting performance and wear resistance, and at the same time, cutting in the die The film-removing module is designed in the machine to peel off the silicon-coated film to reduce dust adhesion and detachment.

Benefits of technology

It effectively reduces the generation of dust during die cutting, keeps the base layer clean, enhances the anti-cutting and wear resistance of the protective film, and improves production quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119060648A_ABST
    Figure CN119060648A_ABST
Patent Text Reader

Abstract

According to the technical scheme, the PU protective film is characterized by comprising a base material layer, one side of the base material layer is covered with a dustproof layer, the other side of the base material layer is provided with an adhesive layer, and a release layer is attached to the surface of the adhesive layer; the adhesive layer comprises polyurethane resin, a curing agent, an antistatic agent, hard resin, fluorine-containing hydroxyl resin, a surface wetting agent and an organic solvent; through the arrangement of the dustproof layer, external dust can be prevented from being attached to the surface of the base material layer in the die cutting process to affect machining, and all components in the adhesive layer can enhance the cutting resistance and abrasion resistance of the protective film; and the protective film with high cutting resistance is not easy to damage and generate fragments in the die cutting process, so that the generation of dust is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of PU protective films, and in particular to a PU protective film and a preparation process thereof. Background Art

[0002] PU protective film is a functional protective film made of transparent PET film as the base material, coated with polyurethane (PU) glue on one side, and a release film on the back. It is mainly used for high-temperature process protection of LCD panels, and shipment protection of ITO and glass panels.

[0003] The existing PU protective film needs to be die-cut after preparation before it can be used. However, in the PU protective film, since the chemical molecular structure of the colloid is usually relatively tight and has good adhesion, the PU protective film is prone to slight damage and breakage when subjected to external forces, such as pressure and friction during the cutting process, and is prone to produce tiny fragments or dust. These dust fragments can easily enter the adhesive layer during the die-cutting process, causing damage to the adhesive layer and having a certain impact on the performance and quality of the product. At the same time, when the PU protective film is transported to the die-cutting machine after preparation, external dust is also easily adsorbed on the surface of the PU protective film, resulting in the dust attached to the surface of the protective film being squeezed or cut during die-cutting, thereby producing smaller dust particles, affecting the production quality of the protective film. Summary of the invention

[0004] The present invention provides a PU protective film and a preparation process thereof, which solves the problem in the related art that the PU protective film generates dust during die-cutting due to its own structure and the influence of external dust.

[0005] To achieve the above-mentioned purpose, the technical solution adopted by the present invention is: a PU protective film, including a substrate layer, one side of the substrate layer is covered with a dustproof layer, the lower surface is provided with an adhesive layer, and the surface of the adhesive layer is attached with a release layer; the adhesive layer components include polyurethane resin, curing agent, antistatic agent, hard resin, fluorine-containing hydroxyl resin, surface wetting agent and organic solvent.

[0006] The present invention is further configured such that the adhesive layer components have the following proportions: 100 parts of polyurethane resin, 6-15 parts of curing agent, 1-2 parts of antistatic agent, 0.25-10 parts of hard resin, 0.5-5 parts of fluorine-containing hydroxyl resin, and 1-2 parts of surface wetting agent.

[0007] The present invention is further configured such that the dustproof layer is a silicon-coated film having a microporous structure formed on its surface.

[0008] A PU protective film preparation process, the steps are as follows:

[0009] S1, coating of silicon layer: prepare silicone oil, and coat the silicone oil on the upper surface of the substrate layer through a coating machine;

[0010] S2, curing and maturing of the silicon-coated layer: sending the substrate layer coated with silicone oil on one side in S1 into an oven or a curing furnace for curing treatment, and then placing it in a maturing chamber for maturation to obtain a substrate layer with a silicon-coated film on one side;

[0011] S3, glue solution preparation: weigh the raw materials of each component according to the formula, mix the main glue, curing agent, antistatic agent, hard resin, and fluorinated hydroxyl resin solid components in an appropriate container, and then add the solvent and surface wetting agent to stir until the glue solution is uniform and transparent;

[0012] S4, adhesive layer coating: placing the prepared substrate layer on the material rack of the coating machine, and then evenly coating the adhesive solution prepared in S3 on the lower surface of the substrate layer away from the silicon coating layer through the coating machine;

[0013] S5, adhesive layer re-curing: sending the substrate layer coated with the adhesive liquid into an oven or a curing furnace for curing treatment to obtain a substrate layer with an adhesive layer on one side and a silicon film on the other side;

[0014] S6, release layer lamination: prepare a release film, and laminate it with the base material layer obtained in S5 on the surface of the adhesive layer of the base material layer through a laminating machine;

[0015] S7, laser drilling: using a coil laser drilling machine, laser drilling is performed on the outer surface of the silicon-coated film obtained in S6 that is away from the substrate layer, forming a microporous structure on the silicon-coated film and rewinding the processed substrate layer;

[0016] S8, die-cutting: using a die-cutting machine, the protective film that has been processed and rolled up in S7 is die-cut and formed. During the die-cutting process, the silicon-coated film on the surface of the substrate layer is peeled off before cutting.

[0017] The present invention is further configured such that the die-cutting machine includes a frame provided with a control component, and a feed roller group, a feeding roller group, a cutting component and a waste winding roller group connected to the control component are sequentially arranged on the frame along the protective film conveying direction, and a discharge component is arranged between the cutting component and the waste winding roller group; a film peeling component for peeling the silicon-coated film from the substrate layer is arranged between the feed roller group and the feeding roller group.

[0018] The present invention is further configured such that the film peeling assembly includes a suction panel arranged on the frame and located between the feed roller group and the feeding roller group, the suction panel is provided with a plurality of suction holes, and a suction chamber connected to an exhaust pump is provided below the suction panel; it also includes a film peeling roller rotatably arranged on the frame, the film peeling roller is located above the suction panel, and is used for winding the silicon-coated film when the feeding roller group transports the protective film.

[0019] The present invention is further configured such that the film peeling roller includes a rotating shaft rotatably connected to the frame and connected to a motor at one end, a connecting rod located on the circumference of the rotating shaft is fixedly connected to the rotating shaft, and an abutting roller is rotatably arranged on the connecting rod.

[0020] The present invention is further configured such that the frame is elastically provided with pressure plates located on both sides of the suction panel, one end of the pressure plate extends above the suction panel, and a ball is rollingly provided on its lower surface for abutting and cooperating with the surface of the substrate layer of the protective film.

[0021] The present invention is further configured such that the cutting assembly includes a lower die base arranged on a frame and an upper die base connected to a lifting rod and sliding up and down relative to the lower die base, the upper die base is provided with a die-cutting knife, and the lower die base is provided with a discharge port located in front along the conveying direction of the protective film; the discharge assembly includes a conveyor belt which is fitted above the lower die base and arranged in the same direction as the conveying direction of the protective film, the frame is provided with a pair of transmission shafts for driving the conveyor belt to move and a driving mechanism for driving the transmission shaft to rotate, and the driving mechanism is connected to the control assembly.

[0022] The present invention is further configured such that an inclined guide plate is provided below the discharge port, a blow box is provided on one side of the discharge port, air holes are provided on the side of the blow box opposite to the discharge port, and a dustproof net is covered on the air holes; an air inlet connected to a fan is also provided on the blow box.

[0023] In summary, the beneficial effects of the present invention are:

[0024] Compared with the prior art, a silicon-coated film is provided on the surface of the substrate layer so that it can be peeled off from the substrate layer during die-cutting, thereby ensuring the neatness of the surface of the substrate layer during die-cutting; and silicone oil has an antistatic function, which can reduce the dust adsorbed by the protective film coil in the air before die-cutting, and the microporous structure provided on the surface of the silicon-coated film can fix the dust particles falling on the surface of the silicon-coated film, thereby reducing the dust from detaching from the surface of the silicon-coated film when peeling off the silicon-coated film.

[0025] The various components in the adhesive layer can enhance the cutting resistance and wear resistance of the protective film; the protective film with strong cutting resistance is not easy to be damaged or fragmented during the die-cutting process, thereby reducing the generation of dust; the protective film with good wear resistance can resist the friction and wear of the tool during the die-cutting process, reducing the dust generated by friction; through the above-mentioned improvements to the protective film layer structure and the chemical properties of the adhesive layer, the dust generated by the tool when cutting the protective film can be reduced. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 Schematic diagram of the structure of the protective film of this embodiment.

[0027] Figure 2 These are the process steps of this embodiment.

[0028] Figure 3 It is a schematic structural diagram of the die-cutting machine of this embodiment.

[0029] Figure 4 It is a cross-sectional view of this embodiment.

[0030] Figure 5 It is a partial cross-sectional view of this embodiment.

[0031] Figure 6 It is a structural diagram of the film peeling assembly of this embodiment.

[0032] Figure 7 It is a cross-sectional view of the cutting component of this embodiment.

[0033] Figure 8 2 is a structural diagram of the cutting assembly of this embodiment.

[0034] Fig. 9 It is a structural diagram of the discharging assembly of this embodiment.

[0035] Figure numerals: 1, substrate layer; 2, dustproof layer; 3, adhesive layer; 4, release layer; 5, microporous structure; 10, frame; 11, control component; 12, control panel; 13, feed roller group; 131, material rack; 14, feed roller group; 141, feed roller; 142, motor; 15, film peeling component; 151, air suction panel; 152, air suction hole; 153, air suction cavity; 154, exhaust pump; 155, film peeling Roller; 156, connecting rod; 157, abutting roller; 158, rotating shaft; 16, pressing plate; 161, ball bearing; 17, cutting assembly; 171, lower die base; 172, upper die base; 173, lifting cylinder; 18, discharging assembly; 181, discharging port; 182, conveyor belt; 183, transmission shaft; 184, guide plate; 185, blowing box; 186, fan; 19, waste winding roller group; 191, waste roller. DETAILED DESCRIPTION

[0036] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of the present invention.

[0037] like Figure 1As shown, this embodiment discloses a PU protective film, including a substrate layer 1, the upper surface of the substrate layer 1 is covered with a dustproof layer 2, the lower surface is provided with an adhesive layer 3, and the surface of the adhesive layer 3 is attached with a release layer 4; the components of the adhesive layer 3 include polyurethane resin, curing agent, antistatic agent, hard resin, fluorine-containing hydroxyl resin, surface wetting agent and organic solvent; the dustproof layer 2 is a silicon-coated film, and a microporous structure 5 is formed on its surface.

[0038] Among them, the upper surface of the substrate layer 1 is the side away from the device, and the lower surface of the substrate layer 1 is the side in contact with the device. When the user uses the protective film, the release layer 4 on the lower surface can be peeled off, and then the substrate layer 1 can be adhered to the surface of the device through the adhesive layer 3, while the upper surface of the substrate layer 1 is exposed to the outside and in contact with the air.

[0039] The silicon-coated film provided on the upper surface of the substrate layer 1 can be peeled off from the substrate layer 1 during die-cutting, thereby ensuring the cleanliness of the surface of the substrate layer 1 during die-cutting; and the silicone oil has an antistatic function, which can reduce the dust adsorbed by the protective film coil in the air before die-cutting, and the microporous structure 5 provided on the surface of the silicon-coated film can fix the dust particles falling on the surface of the silicon-coated film, thereby reducing the dust from detaching from the surface of the silicon-coated film when peeling off the silicon-coated film.

[0040] The various components in the adhesive layer 3 can enhance the cutting resistance and wear resistance of the protective film; the protective film with strong cutting resistance is not easy to be damaged or fragmented during the die-cutting process, thereby reducing the generation of dust; the protective film with good wear resistance can resist the friction and wear of the tool during the die-cutting process, reducing the dust generated by friction; through the above-mentioned improvement of the protective film layer structure and the chemical properties of the adhesive layer 3, the dust generated by the tool when cutting the protective film is reduced.

[0041] The proportions of the components of the adhesive layer 3 are as follows: 100 parts of polyurethane resin, 6-15 parts of curing agent, 1-2 parts of antistatic agent, 0.25-10 parts of hard resin, 0.5-5 parts of fluorine-containing hydroxyl resin, and 1-2 parts of surface wetting agent.

[0042] The curing agent can be an isocyanate curing agent, which can react with the main glue so that the protective film can be cured and formed after coating, thereby enhancing the strength and durability; the antistatic agent can be a quaternary ammonium salt antistatic agent, which is used to reduce the electrostatic adsorption capacity of the surface of the protective film and reduce dust adhesion; the hard resin can be an epoxy resin, which can improve the hardness and wear resistance of the protective film, thereby being able to resist the friction and wear of the tool during the die-cutting process and reduce the dust generated by friction; and the fluorine-containing hydroxyl resin can be a fluorine-containing polyurethane resin, which is used to improve the weather resistance, chemical resistance or surface properties of the protective film.

[0043] like Figure 2 As shown, the preparation process steps for preparing the above PU protective film are as follows:

[0044] S1, coating of silicon layer: prepare silicone oil, and coat the silicone oil on the upper surface of substrate layer 1 by a coating machine;

[0045] S2, curing and maturing of the silicon-coated layer: sending the substrate layer 1 with the silicone oil coated on the upper surface in S4 into an oven or a curing furnace for curing treatment, and then placing it into a maturing chamber for maturation to obtain the substrate layer 1 with the silicon-coated film on the upper surface;

[0046] After the above steps, a silicon-coated film can be formed on the upper surface of the substrate layer 1 made of PET. The silicon-coated film can cover the surface of the substrate layer 1, thereby protecting the surface of the substrate layer 1 and preventing dust impurities in the air from falling on the surface of the substrate layer 1 during storage or transportation of the protective film roll, thereby preventing the dust attached to the surface of the protective film from being squeezed or cut by the die-cutting knife during the die-cutting process, thereby generating smaller dust particles, causing the dust impurities to enter the adhesive layer 3 and affect the quality of the product.

[0047] At the same time, due to the properties of the silicon-coated film itself, it can be easily peeled off the substrate layer 1, so that it can be peeled off from the substrate layer 1 during die-cutting, thereby ensuring that the surface of the substrate layer 1 always remains clean during the die-cutting process.

[0048] S3, glue solution preparation: weigh the raw materials of each component according to the formula, mix the main glue, curing agent, antistatic agent, hard resin, and fluorinated hydroxyl resin solid components in an appropriate container, and then add the solvent and surface wetting agent to stir until the glue solution is uniform and transparent;

[0049] S4, coating of adhesive layer 3: placing the prepared substrate layer 1 on the material rack 131 of the coating machine, and then coating the adhesive solution prepared in S3 evenly on the lower surface of the substrate layer 1 relative to the silicon-coated film through the coating machine;

[0050] S5, re-curing the adhesive layer 3: sending the substrate layer 1 coated with the adhesive liquid into an oven or a curing furnace for curing treatment to obtain a substrate layer 1 with an adhesive layer 3 on the lower surface and a silicon film on the upper surface;

[0051] S6, compounding the release layer 4: prepare a release film, and compound it with the substrate layer 1 obtained in S5 on the surface of the adhesive layer 3 of the substrate layer 1 through a compounding machine;

[0052] S7, laser punching: using a coil laser puncher, the outer surface of the silicon-coated film of the substrate layer 1 obtained in S6 which is away from the substrate layer 1 is laser punched, a microporous structure 5 is formed on the silicon-coated film, and the processed substrate layer 1 is rewound; the surface of the silicon-coated film is punched by the coil laser puncher to form a microporous structure 5 on the surface of the silicon-coated film, and the microporous structure 5 can fix the dust attached to the surface of the silicon-coated film, thereby reducing the impurities attached to the surface of the silicon-coated film falling back onto the surface of the substrate layer 1 in the process of peeling the silicon-coated film off the substrate layer 1, thereby reducing the die-cutting quality of the protective film.

[0053] S8, die-cutting: using a die-cutting machine, die-cutting the protective film that has been processed and rolled up in S7. During the die-cutting process, the silicon-coated film on the surface of the substrate layer 1 is peeled off before cutting.

[0054] like Figure 3-5 As shown, the die-cutting machine includes a frame 10 provided with a control component 11 . The control component 11 is an electric control box, and a control panel 12 and a PLC module are used to control various structures provided on the frame 10 .

[0055] A feed roller group 13 connected to a control component 11 is sequentially arranged on the frame 10 along the conveying direction of the protective film. The feed roller group 13 includes a material rack 131 rotatably arranged on the frame 10, and the PU protective film that becomes a coil is placed on the material rack 131. The feed roller group 14 includes a pair of feed rollers 141 distributed up and down on the frame 10 and rotating relatively. One end of one of the feed rollers 141 is connected to a motor 142 connected to the control component 11, which can clamp the protective film and convey it forward. The transmission between the two feed rollers 141 can be gear transmission, belt transmission, or only one feed roller 141 rotates, and the other is passively rotated.

[0056] A film peeling assembly 15 for peeling the silicon-coated film from the substrate layer 1 is provided between the feed roller assembly 13 and the feed roller assembly 14. Figure 6As shown, the film peeling assembly 15 includes a suction panel 151 arranged on the frame 10 and located between the feed roller group 13 and the feeding roller group 14, a plurality of suction holes 152 are arranged on the suction panel 151, and a suction chamber 153 connected to the exhaust pump 154 ​​is arranged below the suction panel 151; it also includes a film peeling roller 155 rotatably arranged on the frame 10, the film peeling roller 155 is located above the suction panel 151, and is used to roll up the silicon-coated film when the feeding roller group 14 conveys the protective film, the film peeling roller 155 includes a rotating shaft 158 ​​which is rotatably connected to the frame 10 and one end of which is connected to the motor 142, a connecting rod 156 located on the peripheral side of the rotating shaft 158 ​​is fixedly connected to the rotating shaft 158, an abutting roller 157 is rotatably arranged on the connecting rod 156, and a plurality of abutting rollers 157 can be provided, which are evenly distributed on the peripheral side of the rotating shaft 158. In this embodiment, two abutting rollers 157 are provided.

[0057] When a pair of feeding rollers 141 convey the protective film, one end of the silicon-coated film is first peeled off so that part of it is wound around a plurality of abutting rollers 157, and the exhaust pump 154 ​​is always in operation to keep the suction chamber 153 in a suction state. When the protective film passes over the suction panel 151, the suction holes 152 will adsorb the substrate layer 1 of the protective film, so that the substrate layer 1 is always attached to the suction panel 151. At the same time, the motor 142 will control the rotation of the shaft 158, thereby driving the abutting rollers 157 distributed around the shaft 158 ​​to rotate. During the rotation process, the abutting rollers 157 can roll up the silicon-coated film, so that the silicon-coated film is pulled to the side away from the protective film, and the silicon-coated film and the substrate layer 1 are peeled off, thereby avoiding the silicon-coated film with dust attached to it being cut together and generating dust that affects the quality of the protective film after die-cutting. In addition, the film peeling component 15 automatically rolls up the silicon-coated film, which can effectively improve the die-cutting efficiency of the protective film.

[0058] In the above process, the rotating shaft 158 ​​can drive the two abutting rollers 157 to rotate along the conveying direction of the protective film, thereby generating a force on the silicon-coated film that deviates from the conveying direction of the protective film, so that the silicon-coated film can be separated from the protective film more easily, which is more suitable for die-cutting processing of the PU protective film in this application.

[0059] like Figure 6 As shown, at the same time, a pressure plate 16 is elastically arranged on the frame 10 and located on both sides of the suction panel 151. One end of the pressure plate 16 extends above the suction panel 151, and a ball 161 is rollingly arranged on its lower surface to abut against the surface of the substrate layer 1 of the protective film.

[0060] In this embodiment, the pressing plate 16 can press down and limit the part of the substrate layer 1 that has been separated from the silicon-coated film, so that the substrate layer 1 fits with the suction panel 151, thereby preventing the force generated by the silicon-coated film during the peeling process from causing the substrate layer 1 to separate from the suction panel 151 and affecting the transportation of the protective film; ensuring that the substrate layer 1 can be transported normally. Since there is no limiting structure to limit the left and right movement direction of the substrate layer 1 in the transportation direction, the relative movement direction between the substrate layer 1 and the substrate layer 1 is not fixed during the transportation process, and there may be movement in an inclined direction to one side. Therefore, in order to avoid the sliding friction between the pressing plate 16 and the substrate layer 1, which may cause wrinkles in the substrate layer 1, the ball 161 that can roll in any direction is used to convert the friction between the pressing plate 16 and the substrate layer 1 into rolling friction, thereby ensuring that when the substrate layer 1 moves in an inclined direction, the ball 161 can move in the direction of movement of the substrate layer 1, thereby preventing the substrate layer 1 from being wrinkled during the transportation process due to the sliding friction of the pressing plate 16.

[0061] like Figure 7-8 As shown, a cutting assembly 17 and a waste material winding roller assembly 19 are arranged behind the film stripping assembly 15, and a discharging assembly 18 is arranged between the cutting assembly 17 and the waste material winding roller assembly 19; Figure 7-8 As shown, the cutting assembly 17 includes a lower die base 171 arranged on the frame 10 and an upper die base 172 connected to the lifting rod and sliding up and down relative to the lower die base 171. A die cutting knife is arranged on the upper die base 172. When the protective film that has been peeled off from the silicon-coated film is sent to between the lower die base 171 and the upper die base 172 through a pair of feeding rollers 141, the upper die base 172 will be fitted with the lower die base 171 under the action of the lifting cylinder 173, so that the die cutting knife can cut and shape the protective film on the lower die base 171; and the waste remaining after cutting is wound up by the waste winding roller group 19.

[0062] like Figure 8-9 As shown, a discharge port 181 is provided in front of the lower die base 171 in the conveying direction of the protective film; the discharge assembly 18 includes a conveyor belt 182 which is fitted above the lower die base 171 and arranged in the same direction as the conveying direction of the protective film, and a pair of transmission shafts 183 for driving the conveyor belt 182 and a driving mechanism for driving the transmission shaft 183 to rotate are provided on the frame 10, and the driving mechanism is connected to the control assembly 11; when the protective film is cut and formed under the action of the die cutter, the formed protective film will be driven by the conveyor belt 182 to the discharge port 181, and then sent to the outside for sorting by the discharge port 181; as shown in FIG. Figure 4As shown, the waste winding roller group 19 includes a waste roller 191 rotatably arranged on the frame 10. Before work, one end of the waste will first be manually wound around the waste roller 191 by the staff during the debugging process. During the operation, the waste roller 191 will rotate under the drive of the motor 142, thereby realizing the winding of the waste to facilitate the subsequent collection and processing of the waste by the staff. The motor 142 connected to the waste roller 191 is also connected to the control component 11, so that its working speed can be adapted to the working speeds of the remaining components.

[0063] like Figure 8-9 A slanted guide plate 184 is provided below the discharge port 181, and the die-cut materials can be sent out to the outside through the guide plate 184, so that the staff can collect and organize the die-cut protective films conveniently; at the same time, a blow box 185 is provided on one side of the discharge port 181, and the blow box 185 is provided with air holes on the side opposite to the discharge port 181, and the air holes are covered with a dustproof net; the blow box 185 is also provided with an air inlet hole connected to the fan 186.

[0064] The blow box 185 can effectively clean the dust generated by the protective film during the die-cutting process, remove the dust attached to the surface of the protective film, and further improve the cleanliness of the product.

[0065] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the design concept of the present invention should be included in the protection scope of the present invention.

Claims

1. A PU protective film, comprising a substrate layer (1), characterized in that: The upper surface of the substrate layer (1) is covered with a dustproof layer (2), and the lower surface is provided with an adhesive layer (3), and the surface of the adhesive layer (3) is attached with a release layer (4); the components of the adhesive layer (3) include polyurethane resin, curing agent, antistatic agent, hard resin, fluorine-containing hydroxyl resin, surface wetting agent and organic solvent.

2. A PU protective film according to claim 1, characterized in that: The component proportions of the adhesive layer (3) are as follows: 100 parts of polyurethane resin, 6-15 parts of curing agent, 1-2 parts of antistatic agent, 0.25-10 parts of hard resin, 0.5-5 parts of fluorine-containing hydroxyl resin, and 1-2 parts of surface wetting agent.

3. A PU protective film according to claim 1, characterized in that: The dustproof layer (2) is a silicon-coated film, and a microporous structure (5) is formed on the surface of the film.

4. A PU protective film preparation process, used for preparing the PU protective film according to any one of claims 1 to 3, characterized in that: Here are the steps: S1, coating of a silicon layer: preparing silicone oil, and coating the silicone oil on the upper surface of the substrate layer (1) by a coating machine; S2, curing and maturing of the silicon-coated layer: sending the substrate layer (1) coated with silicone oil on one side in S1 into an oven or a curing furnace for curing treatment, and then placing it in a maturing chamber for maturation to obtain a substrate layer (1) with a silicon-coated film on one side; S3, glue solution preparation: weigh the raw materials of each component according to the formula, mix the main glue, curing agent, antistatic agent, hard resin, and fluorinated hydroxyl resin solid components in an appropriate container, and then add the solvent and surface wetting agent to stir until the glue solution is uniform and transparent; S4, coating of the adhesive layer (3): placing the prepared substrate layer (1) on the material rack (131) of the coating machine, and then evenly coating the adhesive solution prepared in S3 on the lower surface of the substrate layer (1) away from the silicon coating layer through the coating machine; S5, re-curing the adhesive layer (3): sending the substrate layer (1) coated with the adhesive liquid into an oven or a curing furnace for curing treatment to obtain a substrate layer (1) with an adhesive layer (3) on the lower surface and a silicon film on the upper surface; S6, compounding the release layer (4): prepare a release film, and compound it with the substrate layer (1) obtained in S5 on the surface of the adhesive layer (3) of the substrate layer (1) through a compounding machine; S7, laser drilling: using a coil laser drilling machine, laser drilling is performed on the outer surface of the silicon-coated film of the substrate layer (1) obtained in S6, which is away from the substrate layer (1), to form a microporous structure (5) on the silicon-coated film and rewind the processed substrate layer (1); S8, die-cutting: using a die-cutting machine, die-cutting the protective film that has been processed and rolled up in S7. During the die-cutting process, the silicon-coated film on the surface of the substrate layer (1) is peeled off before cutting.

5. A PU protective film preparation process according to claim 4, characterized in that: The die-cutting machine comprises a frame (10) provided with a control component (11); a feed roller group (13), a feeding roller group (14), a cutting component (17) and a waste winding roller group (19) connected to the control component (11) are arranged on the frame (10) in sequence along the protective film conveying direction; a discharge component (18) is arranged between the cutting component (17) and the waste winding roller group (19); and a film peeling component (15) for peeling the silicon-coated film from the substrate layer (1) is arranged between the feed roller group (13) and the feeding roller group (14).

6. A PU protective film preparation process according to claim 5, characterized in that: The film peeling assembly (15) comprises an air suction panel (151) arranged on the frame (10) and located between the feed roller group (13) and the feeding roller group (14), wherein a plurality of air suction holes (152) are arranged on the air suction panel (151), and an air suction chamber (153) connected to an exhaust pump (154) is arranged below the air suction panel (151); and further comprises a film peeling roller (155) rotatably arranged on the frame (10), wherein the film peeling roller (155) is located above the air suction panel (151) and is used for winding up the silicon-coated film when the feeding roller group (14) transports the protective film.

7. A PU protective film preparation process according to claim 6, characterized in that: The film peeling roller (155) comprises a rotating shaft (158) rotatably connected to the frame (10) and having one end connected to a motor (142); a connecting rod (156) located on the circumference of the rotating shaft (158) is fixedly connected to the rotating shaft (158); and an abutting roller (157) is rotatably provided on the connecting rod (156).

8. A PU protective film preparation process according to claim 6, characterized in that: The frame (10) is elastically provided with a pressure plate (16) located on both sides of the air suction panel (151), one end of the pressure plate (16) extends above the air suction panel (151), and a ball (161) is rollingly provided on its lower surface for abutting and cooperating with the surface of the base material layer (1) of the protective film.

9. A PU protective film preparation process according to claim 7, characterized in that: The cutting assembly (17) comprises a lower die base (171) arranged on the frame (10) and an upper die base (172) connected to a lifting rod and sliding up and down relative to the lower die base (171); a die cutting knife is arranged on the upper die base (172); a discharge port (181) is arranged in front of the lower die base (171) along the conveying direction of the protective film; the discharge assembly (18) comprises a conveyor belt (182) arranged in close contact with the upper part of the lower die base (171) and arranged in the same direction as the conveying direction of the protective film; a pair of transmission shafts (183) for driving the conveyor belt (182) to move and a driving mechanism for driving the transmission shaft (183) to rotate are arranged on the frame (10); the driving mechanism is connected to the control assembly (11).

10. A PU protective film preparation process according to claim 9, characterized in that: An inclined guide plate (184) is provided below the discharge port (181); a blow box (185) is also provided on one side of the discharge port (181); an air hole is provided on the side of the blow box (185) opposite to the discharge port (181); a dustproof net is attached to the air hole; and an air inlet hole connected to a fan (186) is also provided on the blow box (185).